Method for making a flavor carrying substrate for a heat-not-burn cigarette
By employing a double-sided injection process of phase change slow-release materials and fragrances in the fragrance carrier of heated non-combustible cigarettes, the problems of low fragrance loading and high draw resistance in the fragrance thread have been solved, achieving stable and long-lasting fragrance release and reduced draw resistance, thereby lowering production costs.
Patent Information
- Application Number
- CN202410948734.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2044-07-16
AI Technical Summary
In existing cigarette flavoring methods, the flavoring thread has a small and unstable flavoring capacity, cannot reduce draw resistance, has high equipment costs, and the flavoring release effect of phase change slow-release flavoring materials is not ideal at low temperatures.
After the phase change slow-release material is heated and melted in a water bath, fragrance is added to form a fragrance carrier material. The material is then injected into the filling holes from both ends of the fastener body through a dispensing machine. After cooling and solidification, the fragrance-added component is formed and integrated with the fastener body to form a fragrance carrier fastener for heating non-combustible cigarettes.
It improves the stability and persistence of aroma, reduces draw resistance, has low production costs, high aroma release efficiency, and enhances the smoking quality.
Smart Images

Figure CN118648723B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of cigarette technology, and more particularly to a method for manufacturing a fragrance carrier for heated non-combustible cigarettes. Background Technology
[0002] As consumers' demands for cigarettes continue to rise, most cigarettes now incorporate flavoring substances to compensate for the lack of aroma in cigarettes and to increase the richness and harmony of the aroma and smoke.
[0003] Currently, there are various methods for flavoring cigarettes. Some cigarettes use a flavoring thread inserted into a fixed part of the cigarette holder. This thread, formed by cotton thread absorbing a flavoring agent, is released during inhalation as the smoke washes away the aroma. However, because the cotton thread has a limited absorption capacity, the flavoring thread carries a relatively small amount of aroma, resulting in a short-lasting and unstable aroma. Furthermore, the flavoring thread remains within the fixed part, barely affecting the draw resistance, thus preventing a significant reduction in draw resistance and leading to a poor smoking experience. Additionally, this type of cigarette requires specialized equipment for production, which is relatively expensive.
[0004] Some cigarettes enhance their aroma by adding phase change slow-release flavoring materials to the filter rod. This involves heating and melting the phase change slow-release material, adding flavorings, and stirring thoroughly to obtain the flavoring material. The flavoring material is then embedded in the filter rod in strip, granular, or paper-coated form. During inhalation, the flavoring material melts upon heating, releasing its aroma. However, since the temperature of the smoke reaching the filter rod is generally below 40°C, while the melting point of the flavoring material is typically 40-60°C, the phase change process takes a considerable amount of time, sometimes even before the smoke is finished, resulting in a less than ideal aroma release during inhalation. Summary of the Invention
[0005] To solve the above-mentioned technical problems and achieve at least one advantage of the present invention, the present invention provides a method for manufacturing a fragrance carrier for heated non-combustible cigarettes, the method comprising:
[0006] Preparation: The phase change slow-release material is heated and melted in a water bath, and fragrance is added to the melted phase change slow-release material and stirred to form a phase change slow-release fragrance carrier material;
[0007] Double-sided injection: Molten phase change slow-release fragrance material is injected sequentially from both ends of the fastener body into its filling holes;
[0008] Molding: The phase change slow-release fragrance material in the filling hole is cooled and solidified to form a fragrance-added component that adheres to the filling hole, so as to form a fragrance-added component integrally with the fixed body for heating non-combustible cigarettes.
[0009] According to one embodiment of the present invention, the phase change sustained-release material is composed of polyethylene glycol 4000, β-cyclodextrin, carrageenan and sodium alginate, wherein polyethylene glycol 4000 is 40-80 parts, β-cyclodextrin is 5-10 parts, carrageenan is 0.5-1 part, sodium alginate is 0.5-1 part, and fragrance is 5-20 parts.
[0010] According to one embodiment of the present invention, the firmware body is made of silicone rubber.
[0011] According to one embodiment of the present invention, during the preparation of the material, the phase change slow-release material is heated in a water bath at 75-85°C.
[0012] According to one embodiment of the present invention, during double-sided injection, the firmware body is supported by the tray of the injection accessory, and the molten phase change slow-release fragrance material is injected from the top of the firmware body into the filling hole by a dispensing machine. The molten phase change slow-release fragrance material is held at one end of the filling hole and cools and solidifies. Subsequently, the firmware body is flipped so that the other end of the filling hole faces upward, and the dispensing machine injects material again. The phase change slow-release fragrance material that has been cooled and solidified sequentially forms the fragrance-added component.
[0013] According to one embodiment of the present invention, after the molten phase change slow-release fragrance material injected by the dispensing machine into one side of the firmware body cools and solidifies, the cover plate of the dispensing auxiliary is placed on top of the firmware body and the whole is flipped so that the cover plate is placed at the bottom of the firmware body and the support plate is placed at the top of the firmware body. The support plate is removed and the dispensing machine re-dispenses the material.
[0014] According to an embodiment of the present invention, during double-sided injection, the firmware body is inserted into the through hole of the array plate of the injection accessory and is successively supported by the support plate or the cover plate placed at the bottom of the array plate. There are multiple through holes, and the multiple through holes are arranged in multiple rows and columns, and the spacing between two adjacent through holes is the same. The dispensing machine can sequentially inject the firmware body in the multiple through holes into one side, and after the single-sided injection is completed and the machine is flipped, it can inject the firmware body into one side again.
[0015] According to one embodiment of the present invention, the diameter of the through hole is 1 mm larger than the diameter of the firmware body, and the thickness of the array plate is the same as the height of the firmware body.
[0016] According to one embodiment of the present invention, the phase change slow-release fragrance carrier is introduced into the dispensing machine in a molten state.
[0017] According to one embodiment of the present invention, the phase change slow-release fragrance material is cooled and solidified and then pulverized. The solidified phase change slow-release fragrance material is then heated by the dispensing machine and injected into the filling hole. Attached Figure Description
[0018] Figure 1 A schematic diagram of the structure of the fragrance carrier for heating non-combustible cigarettes according to the present invention is shown.
[0019] Figure 2 A cross-sectional view of the firmware body structure described in this invention is shown.
[0020] Figure 3 A schematic diagram of the injection fitting described in this invention is shown. Detailed Implementation
[0021] The following description is intended to disclose the present invention and enable those skilled in the art to implement it. The preferred embodiments described below are merely examples, and other obvious variations will occur to those skilled in the art. The basic principles of the invention defined in the following description can be applied to other embodiments, modifications, improvements, equivalents, and other technical solutions that do not depart from the spirit and scope of the invention.
[0022] Those skilled in the art should understand that, in the disclosure of this invention, the terms "longitudinal," "lateral," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are only for the convenience of describing this invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, the above terms should not be construed as limiting this invention.
[0023] It is understood that the term "a" should be understood as "at least one" or "one or more", that is, in one embodiment, the number of an element can be one, while in another embodiment, the number of the element can be multiple, and the term "a" should not be understood as a limitation on the number.
[0024] refer to Figures 1 to 3A preferred embodiment of the flavoring carrier for heated tobacco products according to the present invention will be described in detail below. The flavoring carrier 10 is applied to the cooling section and is integrally placed between the filter section and the smoke-generating section to form a cigarette. The flavoring carrier 10 includes a carrier body 11 and at least one flavoring element 12. The carrier body 11 has at least one filling hole 1101 for receiving the flavoring element 12. The flavoring element 12 is implemented as a phase-change slow-release flavoring material. When the smoke-generating section of the cigarette is heated and the filter section is inhaled, the flavoring component 12 melts upon heating to release aroma. Because the flavoring component 12 is fluid due to its melting, the filling hole 1101 is gradually cleared, thereby reducing draw resistance. At the same time, the smoke generated by the heating end seeps into the filling hole 1101 and flows towards the filter section together with the aroma released by the flavoring component 12. This has the effect of compensating for insufficient aroma in the cigarette. Furthermore, as the number of puffs increases, the filling hole 1101, which was blocked by the flavoring component 12, is gradually opened, increasing the amount of smoke in the later stages and improving the smoking quality.
[0025] Furthermore, by embedding the flavoring component 12 within the firmware body 11, the temperature of the flavoring firmware 10 used to heat the non-combustible cigarette increases from room temperature to 300°C from the outside to the inside during cigarette smoking. Compared to the existing method of adding the phase change slow-release flavoring material to the filter section, the flavoring firmware 10 used to heat the non-combustible cigarette is closer to the smoke-generating section, has a higher temperature, and a higher efficiency in releasing aroma. Moreover, compared to the existing method of adding flavoring thread to the firmware body 11, the cotton thread is eliminated, allowing for the use of more phase change slow-release flavoring material. The aroma produced during smoking is more stable and longer-lasting, and the draw resistance during smoking can be reduced, which is beneficial for smoking.
[0026] Preferably, the loading hole 1101 is provided and located at the center of the fastener body 11 so that the smoke and aroma are concentrated and distributed during inhalation.
[0027] Furthermore, the firmware body 11 is cylindrical and forms a plurality of air intake channels 1102. The plurality of air intake channels 1102 are spaced apart on the outer periphery of the loading hole 1101 and the air intake channels 1102 are used for flue gas circulation.
[0028] Preferably, the firmware body 11 is made of silicone rubber to avoid it absorbing fragrance.
[0029] According to another aspect of the present invention, the present invention also provides a method for manufacturing a fragrance carrier for heated non-combustible cigarettes, the method comprising the following steps:
[0030] (1) Material preparation: The phase change slow-release material is heated and melted in a water bath, and the fragrance is added to the melted phase change slow-release material and stirred to form the phase change slow-release fragrance carrier material;
[0031] (2) Double-sided injection: Molten phase change slow-release fragrance material is injected sequentially from both ends of the fastener body 11 into the filling hole 1101;
[0032] (3) Molding: The phase change slow-release fragrance material in the filling hole 1101 is cooled and solidified to form the fragrance-adding component 12 that adheres to the filling hole 1101, so as to form the fragrance-adding component 10 for heating non-combustible cigarettes integrally with the component body 11.
[0033] Preferably, the phase change sustained-release material is composed of polyethylene glycol 4000, β-cyclodextrin, carrageenan, and sodium alginate.
[0034] Preferably, the components are: polyethylene glycol 4000 (40-80 parts), β-cyclodextrin (5-10 parts), carrageenan (0.5-1 part), sodium alginate (0.5-1 part), and flavoring (5-20 parts).
[0035] Preferably, during the preparation of the material, the phase change slow-release material is heated in a water bath at 75-85°C.
[0036] Specifically, during double-sided injection, the firmware body 11 is supported by a tray 21 of an injection accessory 20. Molten phase change slow-release fragrance material is injected from the top of the firmware body 11 into the filling hole 1101 by a dispensing machine. The molten phase change slow-release fragrance material is held at one end of the filling hole 1101 and cools and solidifies. Subsequently, the firmware body 11 is flipped so that the other end of the filling hole 1101 faces upward, and the dispensing machine injects material again. The phase change slow-release fragrance material, which has cooled and solidified sequentially, integrally forms the fragrance-adding component 12. In this process, the existing dispensing machine can be used. Compared with the fragrance-adding line method of firmware body 11, no special equipment needs to be developed, resulting in lower production costs.
[0037] Furthermore, after the molten phase change slow-release fragrance material injected into the fastener body 11 by the dispensing machine cools and solidifies, the cover plate 22 of the dispensing accessory 20 is placed over the fastener body 11 and the whole assembly is flipped so that the cover plate 22 is placed at the bottom of the fastener body 11 and the support plate 21 is placed at the top of the fastener body 11. The support plate 21 is then removed, and the dispensing machine re-injects the material. During the flipping process, the two ends of the fastener body 11 are respectively abutted by the cover plate 22 and the support plate 21 to seal the filling hole 1101, preventing the cooled and solidified phase change slow-release fragrance material from not adhering tightly to the inner wall of the filling hole 1101 and thus detaching from the filling hole 1101.
[0038] Furthermore, during double-sided injection, the fastener body 11 is inserted into the through-hole 2301 of the array plate 23 of the injection accessory 20 and is successively supported by the support plate 21 or the cover plate 22 placed at the bottom of the array plate 23. Multiple through-holes 2301 are provided, arranged in multiple rows and columns, with the same spacing between adjacent through-holes 2301. The dispensing machine can sequentially inject material onto one side of the fastener body 11 within the multiple through-holes 2301, and after completing the single-sided injection and flipping the device, inject material again sequentially. During the flipping process, the two ends of each fastener body 11 abut against the support plate 21 and the cover plate 22 respectively, sealing the filling hole 1101. This prevents the phase change slow-release fragrance material, which has cooled and solidified within the filling holes 1101 of all the fastener bodies 11, from loosening and detaching from the filling holes 1101.
[0039] Preferably, the distance between two adjacent through holes 2301 is 5-10 mm.
[0040] In one embodiment, the phase change slow-release fragrance material is introduced into the dispensing machine in a molten state for dispensing by the dispensing machine.
[0041] In another embodiment, the phase change slow-release fragrance material is cooled and solidified and then pulverized for sealing and later use, and also for easy introduction into the dispensing machine. The solidified and pulverized phase change slow-release fragrance material is heated by the dispensing machine and then injected into the loading hole 1101.
[0042] Preferably, the diameter of the through hole 2301 is 1 mm larger than the diameter of the fastener body 11 to allow the fastener body 11 to be inserted into the array plate 23. The thickness of the array plate 23 is the same as the height of the fastener body 11, so that the support plate 21 and the cover plate 22 can abut against the two ends of the fastener body 11 in the through hole 2301 by abutting against the two ends of the array plate 23, thereby sealing the filling hole 1101 and facilitating the flipping and filling operation.
[0043] Preferably, the thickness of the tray 21 and the cover plate 22 is 5-10 mm.
[0044] In Example 1, the phase change sustained-release material was heated in a water bath at 80°C. The composition included 70 parts polyethylene glycol 4000, 8.5 parts β-cyclodextrin, 0.5 parts carrageenan, 1 part sodium alginate, and 20 parts L-menthol as the fragrance. The fixed body 11 had a diameter of 6.6 mm and a height of 7 mm, and the filling hole 1101 had a diameter of 2.5 mm. The array plate 23, the support plate 21, and the cover plate 22 were all 300 mm long, 195 mm wide, and 7 mm thick, and the through hole 2301 had an inner diameter of 7.6 mm. During double-sided injection, 7 mg of molten phase change sustained-release fragrance material was sequentially injected into both ends of the filling hole 1101.
[0045] In Comparative Example 1, 3.5 mg of molten phase change slow-release fragrance material was injected sequentially into both ends of the filling hole 1101, with other technical features the same as in Example 1.
[0046] In Comparative Example 2, 7 mg of the molten phase change slow-release fragrance material was injected into one end of the filling hole 1101, with other features the same as in Example 1.
[0047] In Comparative Example 3, the same amount of L-menthol flavoring was injected into the smoking section of the cigarette as in Example 1, and the flavoring component 12 was not provided.
[0048] The cigarettes produced in Example 1 and each comparative example were left open and evaluated by multiple people over several days. The evaluation results are as follows:
[0049] (1) The evaluation score of the menthol intensity of the cigarette is 0-10 points. The evaluation result is determined by calculating the average value of the cigarette. The evaluation of the change in menthol intensity of each cigarette over five days is as follows:
[0050] Example 1 Comparative Example 1 Comparative Example 2 Comparative Example 3 Day 1 10 7 7 10 the next day 9 6 6 7 Day 3 8 5 6 4 Day 4 8 5 5 3 Day 5 7 4 4 2
[0051] By comparing the data from the above embodiments and comparative examples, comparing Embodiment 1 with Comparative Example 1 shows that the amount of the flavoring component 12 formed by the cooling and solidification of the phase change slow-release flavoring material is directly proportional to the mint strength; comparing Comparative Example 1 with Comparative Example 2 shows that, based on the same size of the flavoring component 12, the mint strength of the cigarette with the flavoring component 12 formed by double-sided injection and the cigarette with the flavoring component 12 formed by single-sided injection are similar; comparing Comparative Example 1 with Comparative Example 3 shows that the mint retention effect of the cigarette with the flavoring component 12 is better than that of the cigarette with the flavoring component in the smoking section. Furthermore, the mint strength decreases to some extent with prolonged exposure time.
[0052] (2) The evaluation score for the intensity of menthol release when the cigarette is smoked is 0-10 points. The evaluation result is determined by calculating the average value of the score for the intensity of menthol release when the cigarette is smoked. The evaluation of the change in the intensity of menthol release when various types of cigarettes are smoked over five days is as follows:
[0053] Example 1 Comparative Example 1 Comparative Example 2 Comparative Example 3 Day 1 9 9 9 6 the next day 9 9 8 7 Day 3 8 9 7 4 Day 4 8 8 7 4 Day 5 8 8 8 4
[0054] By comparing the data from the above embodiments and comparative examples, comparing Embodiment 1 with Comparative Example 3, it can be seen that the cigarette with the flavoring component 12 has a better flavoring effect than the cigarette with the flavoring component injected into the smoking section; comparing Comparative Example 1 with Comparative Example 2, it can be seen that, based on the same size of the flavoring component 12, the cigarette with the flavoring component 12 formed by double-sided injection has better menthol release stability than the cigarette with the flavoring component 12 formed by single-sided injection.
[0055] Those skilled in the art should understand that the embodiments of the present invention described above and shown in the accompanying drawings are merely examples and do not limit the invention. The advantages of the present invention have been fully and effectively realized. The functional and structural principles of the present invention have been demonstrated and explained in the embodiments; any variations or modifications can be made to the implementation of the present invention without departing from these principles.
Claims
1. A method for manufacturing a fragrance carrier for heated non-combustible cigarettes, characterized in that, The method for manufacturing the fragrance carrier for heating non-combustible cigarettes includes the following steps: Preparation: The phase change slow-release material is heated and melted in a water bath, and fragrance is added to the melted phase change slow-release material and stirred to form a phase change slow-release fragrance carrier material; Double-sided injection: Molten phase change slow-release fragrance material is injected sequentially from both ends of the fastener body into its filling holes; Molding: The phase change slow-release fragrance material in the filling hole is cooled and solidified to form a fragrance-added part that adheres to the filling hole, so as to form a fragrance-added part for heating non-combustible cigarettes integrally with the fixed body; During double-sided injection, the firmware body is supported by the tray of the injection accessory. Molten phase change slow-release fragrance material is injected from the top of the firmware body into the filling hole by the dispensing machine. The molten phase change slow-release fragrance material is held at one end of the filling hole and cools and solidifies. Then the firmware body is flipped so that the other end of the filling hole faces upward, and the dispensing machine injects material again. The phase change slow-release fragrance material that has cooled and solidified successively forms the fragrance component. The phase change slow-release fragrance material is cooled, solidified, and pulverized. The solidified phase change slow-release fragrance material is then heated by the dispensing machine and injected into the filling hole. After the molten phase change slow-release fragrance material injected by the dispensing machine into one side of the firmware body cools and solidifies, the cover plate of the dispensing accessory is placed on top of the firmware body and the whole assembly is flipped over so that the cover plate is placed at the bottom of the firmware body and the support plate is placed at the top of the firmware body. The support plate is then removed and the dispensing machine re-dispenses the material.
2. The method for manufacturing the incense carrier for heated non-combustible cigarettes according to claim 1, characterized in that, The phase change sustained-release material is composed of polyethylene glycol 4000, β-cyclodextrin, carrageenan and sodium alginate, with 40-80 parts of polyethylene glycol 4000, 5-10 parts of β-cyclodextrin, 0.5-1 part of carrageenan, 0.5-1 part of sodium alginate and 5-20 parts of fragrance.
3. The method for manufacturing the incense carrier for heated non-combustible cigarettes according to claim 1, characterized in that, The firmware body is made of silicone rubber.
4. The method for manufacturing the incense carrier for heated non-combustible cigarettes according to claim 1, characterized in that, During the preparation of the material, the phase change slow-release material is heated in a water bath at 75-85°C.
5. The method for manufacturing the incense carrier for heated non-combustible cigarettes according to claim 1, characterized in that, During double-sided injection, the firmware body is inserted into the through hole of the array plate of the injection accessory and is successively supported by the support plate or the cover plate placed at the bottom of the array plate. There are multiple through holes, and the multiple through holes are arranged in multiple rows and columns, and the spacing between two adjacent through holes is the same. The dispensing machine can sequentially inject the firmware body in the multiple through holes into one side, and after the single-sided injection is completed and the machine is flipped, it can inject the firmware body into one side again.
6. The method for manufacturing the incense carrier for heated non-combustible cigarettes according to claim 5, characterized in that, The diameter of the through hole is 1 mm larger than the diameter of the firmware body, and the thickness of the array plate is the same as the height of the firmware body.
7. The method for manufacturing the incense carrier for heated non-combustible cigarettes according to claim 1, characterized in that, The phase change slow-release fragrance material is introduced into the dispensing machine in a molten state.
Citation Information
Patent Citations
Production method and application of non-continuous temperature-dependent phase change gel incense-carrying filter stick
CN107802032A
Novel heat-not-burn smoking product prepared from biological matrix and preparation method and application thereof