Preparation method of Ni-Co nanoflower hydrotalcite adsorbent based on microwave assistance

The microwave-assisted synthesis of Ni-Co nanoflower hydrotalcite adsorbent solves the problem of low energy utilization efficiency in traditional methods, achieves efficient and environmentally friendly hydrotalcite preparation, improves the adsorption performance and reaction speed, and provides opportunities for water treatment. Efficient dye removal solution.

CN118718976APending Publication Date: 2024-10-01SHANDONG UNIV +1

Patent Information

Application Number
CN202410942006.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-15
Publication Date
2024-10-01

Smart Images

  • Figure CN118718976A_ABST
    Figure CN118718976A_ABST
Patent Text Reader

Abstract

The invention discloses a preparation method of a Ni-Co nanoflower hydrotalcite adsorbent based on microwave assistance, and belongs to the technical field of adsorbents. Hydrotalcite is synthesized by adopting a microwave assistance method, microwave energy directly acts on reactants, energy loss in the conduction process is reduced, the energy utilization efficiency is improved, and the energy utilization rate is increased. The reaction system is heated more uniformly, and the reaction time is shortened. Green chemistry is effectively realized, and the chemical industry is promoted to develop towards a more sustainable direction. Nickel salt, cobalt salt, urea and deionized water are mixed and then placed in a microwave reactor, reactants are directly heated through a microwave radiation method, and therefore the efficient and uniform heating process is achieved. The microwave-assisted method obviously improves the synthesis efficiency and greatly shortens the reaction time. The prepared Ni-Co nanoflower hydrotalcite has a relatively large specific surface area, a rich porous structure and a relatively large interlayer spacing, and is endowed with excellent adsorption capacity. An efficient and environment-friendly solution is provided for the field of water treatment.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of adsorbents, and specifically relates to a method for preparing a Ni-Co nano-flower hydrotalcite adsorbent based on microwave assistance. Background Art

[0002] Dye wastewater is one of the most polluted types of wastewater due to its high chemical oxygen demand, heavy color, high pH and low biodegradability. Due to the wide application of dyes in industrial production, its excessive discharge will have a negative impact on aquatic organisms, human health and the ecological environment. At present, some technologies have been developed to remove dyes from water, such as precipitation, degradation, adsorption, catalysis, reverse osmosis and flocculation. Among them, adsorption is regarded as a suitable, economical and convenient method for removing dyes from water because of its advantages such as high efficiency, low cost, simple operation and environmental friendliness. The effect of the adsorption process depends on the properties of the adsorbate. The ideal adsorbent has the characteristics of high efficiency, low cost, high stability and environmental protection. As a double-layer hydroxide, hydrotalcite has a structure composed of alternating positively charged metal hydroxide layers and negatively charged anion and water molecule layers. The layered structure, anion exchange capacity, high charge density, high specific surface area, high stability and adjustable structure of hydrotalcite make hydrotalcite have good adsorption capacity for dye organic molecules in water. The layered structure and large specific surface area of ​​hydrotalcite also facilitate its application in water treatment. Nano-flower hydrotalcite with highly branched and stacked nanosheets can significantly increase the specific surface area of ​​hydrotalcite and form a porous network. By regulating the interlayer gap of hydrotalcite, the pore structure of the adsorbent can be regulated, which helps to provide more adsorption sites, promote the movement of dye molecules inside the adsorbent, and improve its adsorption performance. At the same time, the controllable synthesis and surface modification of hydrotalcite also provide more possibilities for its application in dye adsorption in water.

[0003] However, the common hydrotalcite synthesis method cannot directly apply energy to the reactants, which increases the energy loss in the conduction process, affects the energy utilization efficiency, and makes the overall reaction time longer. Summary of the invention

[0004] The purpose of the present invention is to provide a method for preparing a Ni-Co nano-flower hydrotalcite adsorbent based on microwave assistance in order to solve the above-mentioned problems.

[0005] The technical solution adopted by the present invention is as follows: a method for preparing a Ni-Co nano-flower hydrotalcite adsorbent based on microwave assistance, the preparation method comprising the following steps:

[0006] S1: adding nickel salt, cobalt salt, urea and deionized water into the microwave cavity of a microwave chemical reactor;

[0007] Wherein: the molar ratio of nickel salt to cobalt salt is 1:1-4; the molar ratio of the total amount of nickel salt and cobalt salt to urea is 1:2-6

[0008] S2: heating the reaction under microwave irradiation,

[0009] S3: filtering, washing and drying the obtained solid to obtain a Ni-Co nano-flower hydrotalcite adsorbent;

[0010] S4: The obtained nano-flower hydrotalcite adsorbent is collected, preserved and packaged, thereby completing the entire preparation process of the microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent.

[0011] In a preferred embodiment, in step S1, the nickel salt is one or more of nickel chloride, nickel nitrate, nickel sulfate, nickel acetate or their hydrates.

[0012] In a preferred embodiment, in step S1, the cobalt salt is one or more of cobalt chloride, cobalt nitrate, cobalt sulfate, cobalt acetate or their hydrates.

[0013] In a preferred embodiment, in step S2, the heating method is a microwave method.

[0014] In a preferred embodiment, in step S2, the reaction temperature is 50-150° C., the microwave radiation power is 200-500 W, and the reaction time is 10-30 min.

[0015] In a preferred embodiment, in step S3, the solvents used for washing are water and ethanol, the drying temperature is 60-100° C., and the drying time is 12-24 hours.

[0016] In a preferred embodiment, in step S3, the nano-flower hydrotalcite adsorbent has a three-dimensional nano-flower structure with a specific surface area of ​​100-200 m 2 / g.

[0017] In a preferred embodiment, the application method of the nano-flower hydrotalcite adsorbent is: dispersing the Ni-Co nano-flower hydrotalcite adsorbent in an aqueous solution containing a dye, stirring, and taking the suspension at fixed time intervals to measure the dye concentration; after the adsorption is completed, filtering, drying, and calcining the hydrotalcite adsorbent to achieve adsorbent regeneration.

[0018] In a preferred embodiment, the adsorbent addition amount is 0.1-1 g / L, the dye concentration is 20-500 mg / L, and the dye used is methyl orange.

[0019] In summary, due to the adoption of the above technical solution, the beneficial effects of the present invention are:

[0020] In the present invention, microwave-assisted hydrotalcite synthesis is adopted, microwave energy can be directly applied to reactants, energy loss in the conduction process is reduced, energy utilization efficiency is improved, rapid heating can be achieved, the reaction system is heated more evenly, and the reaction time is greatly reduced. This efficient, energy-saving and green and environmentally friendly hydrotalcite synthesis method can effectively realize green chemistry and promote the chemical industry to develop in a more sustainable direction. By mixing nickel salt, cobalt salt, urea and deionized water and placing them in a microwave reactor, the reactants are directly heated by microwave radiation, thereby realizing an efficient and uniform heating process. Compared with the traditional hydrothermal method, the microwave-assisted method significantly improves the synthesis efficiency and greatly shortens the reaction time. The prepared Ni-Co nano-flower hydrotalcite has a large specific surface area, rich porous structure and larger interlayer spacing, giving it excellent adsorption capacity. Especially in the application of removing dyes in water, this adsorbent not only has a high adsorption rate and a large adsorption amount, but also has good recovery performance, providing a kind of efficient and environmentally friendly solution for the field of water treatment. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 This is the SEM image of the Ni-Co nano-flower hydrotalcite adsorbent prepared in Example 1;

[0022] Figure 2 This is the XRD pattern of the Ni-Co nano-flower hydrotalcite adsorbent prepared in Example 1;

[0023] Figure 3 This is a nitrogen adsorption and desorption curve of the Ni-Co nano-flower hydrotalcite adsorbent prepared in Example 1;

[0024] Figure 4 This is a graph showing the amount of dye adsorbed by the Ni-Co nano-flower hydrotalcite adsorbent prepared in Example 1-2;

[0025] Figure 5 Flow chart of the method in the present invention. DETAILED DESCRIPTION

[0026] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.

[0027] Reference Figure 1-5 ,

[0028] A method for preparing a Ni-Co nano-flower hydrotalcite adsorbent based on microwave assistance, the preparation method comprising the following steps:

[0029] S1: adding nickel salt, cobalt salt, urea and deionized water into the microwave cavity of a microwave chemical reactor;

[0030] Wherein: the molar ratio of nickel salt to cobalt salt is 1:1-4; the molar ratio of the total amount of nickel salt and cobalt salt to urea is 1:2-6

[0031] S2: heating the reaction under microwave irradiation,

[0032] S3: filtering, washing and drying the obtained solid to obtain a Ni-Co nano-flower hydrotalcite adsorbent;

[0033] S4: The obtained nano-flower hydrotalcite adsorbent is collected, preserved and packaged, thereby completing the entire preparation process of the microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent.

[0034] In step S1, the nickel salt is one or more of nickel chloride, nickel nitrate, nickel sulfate, nickel acetate or their hydrates.

[0035] In step S1, the cobalt salt is one or more of cobalt chloride, cobalt nitrate, cobalt sulfate, cobalt acetate or their hydrates.

[0036] In step S2, the heating method is microwave method.

[0037] In step S2, the reaction temperature is 50-150° C., the microwave radiation power is 200-500 W, and the reaction time is 10-30 min.

[0038] In step S3, the solvents used for washing are water and ethanol, the drying temperature is 60-100° C., and the drying time is 12-24 hours.

[0039] In step S3, the nano-flower hydrotalcite adsorbent has a three-dimensional nano-flower structure with a specific surface area of ​​100-200m 2 / g.

[0040] The application method of the nano-flower hydrotalcite adsorbent is as follows: the Ni-Co nano-flower hydrotalcite adsorbent is dispersed in an aqueous solution containing a dye, stirred, and the suspension is taken at fixed time intervals to measure the dye concentration; after the adsorption is completed, the hydrotalcite adsorbent is filtered, dried, and calcined to achieve adsorbent regeneration.

[0041] The adsorbent addition amount is 0.1-1 g / L, the dye concentration is 20-500 mg / L, and the dye used is methyl orange.

[0042] Example 1

[0043] (1) Ni(NO3)2·6H2O:Co(NO3)2·6H2O:urea in a molar ratio of 1:2:12 was dissolved in deionized water and stirred evenly. The obtained solution was transferred to the microwave cavity of a microwave reactor and reacted for 30 min at 120°C and a microwave power of 300 W to obtain a solid product. The obtained solid product was filtered, washed three times with water and ethanol, and dried at 80°C for 24 h to obtain a Ni-Co nanoflower hydrotalcite adsorbent with a specific surface area of ​​128.5 m 2 / g.

[0044] (2) Disperse 0.1 g of the Ni-Co nano-flower hydrotalcite adsorbent obtained in step (1) into 100 mL of a 200 mg / L methyl orange aqueous solution, stir at room temperature, and take samples every 20 min. Use an ultraviolet spectrophotometer to measure the concentration of methyl orange dye until adsorption saturation is reached, and the saturated adsorption amount is 194 mg / L.

[0045] Example 2

[0046] The adsorbent in step (2) of Example 1 was filtered out and dried at 80°C for 24 hours. The dried adsorbent was calcined at 600°C for 4 hours for regeneration. The specific surface area of ​​the regenerated adsorbent was 117.6 m 2 / g; the regenerated adsorbent was subjected to dye adsorption under the same conditions as step (2) of Example 1, and the saturated adsorption capacity was 187 mg / L.

[0047] It can be known from the above experimental results that in the present invention, microwave-assisted hydrotalcite synthesis can directly act on the reactant with microwave energy, reduce the energy loss in the conduction process, improve the energy utilization efficiency, can be quickly heated, the reaction system is heated more evenly, and the reaction time is greatly reduced. This efficient, energy-saving and green and environmentally friendly hydrotalcite synthesis method can effectively realize green chemistry and promote the chemical industry to develop in a more sustainable direction. By mixing nickel salt, cobalt salt, urea and deionized water and placing them in a microwave reactor, the reactant is directly heated by microwave radiation, thereby achieving an efficient and uniform heating process. Compared with the traditional hydrothermal method, the microwave-assisted method significantly improves the synthesis efficiency and greatly shortens the reaction time. The prepared Ni-Co nano-flower hydrotalcite has a large specific surface area, rich porous structure and larger interlayer spacing, giving it excellent adsorption capacity. Especially in the application of removing dyes in water, this adsorbent not only has a high adsorption rate and a large adsorption amount, but also has good recovery performance, providing an efficient and environmentally friendly solution for the field of water treatment.

[0048] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the term "comprise" or any other variant thereof is intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.

[0049] The above description enables those skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but will conform to the widest scope consistent with the principles and novel features disclosed herein.

Claims

1. A method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent, characterized in that: The preparation method comprises the following steps: S1: adding nickel salt, cobalt salt, urea and deionized water into the microwave cavity of a microwave chemical reactor; Wherein: the molar ratio of nickel salt to cobalt salt is 1:1-4; the molar ratio of the total amount of nickel salt and cobalt salt to urea is 1:2-6 S2: heating the reaction under microwave irradiation, S3: filtering, washing and drying the obtained solid to obtain a Ni-Co nano-flower hydrotalcite adsorbent; S4: The obtained nano-flower hydrotalcite adsorbent is collected, preserved and packaged, thereby completing the entire preparation process of the microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent.

2. The method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent according to claim 1, characterized in that: In step S1, the nickel salt is one or more of nickel chloride, nickel nitrate, nickel sulfate, nickel acetate or their hydrates.

3. The method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent according to claim 1, characterized in that: In step S1, the cobalt salt is one or more of cobalt chloride, cobalt nitrate, cobalt sulfate, cobalt acetate or their hydrates.

4. The method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent according to claim 1, characterized in that: In the step S2, the heating method is a microwave method.

5. The method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent according to claim 1, characterized in that: In step S2, the reaction temperature is 50-150° C., the microwave radiation power is 200-500 W, and the reaction time is 10-30 min.

6. The method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent according to claim 1, characterized in that: In step S3, the solvents used for washing are water and ethanol, the drying temperature is 60-100° C., and the drying time is 12-24 hours.

7. The method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent according to claim 1, characterized in that: In step S3, the nano-flower hydrotalcite adsorbent has a three-dimensional nano-flower structure with a specific surface area of ​​100-200 m 2 / g.

8. The method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent according to any one of claims 1 to 7, characterized in that: The application method of the nano-flower hydrotalcite adsorbent is as follows: the Ni-Co nano-flower hydrotalcite adsorbent is dispersed in an aqueous solution containing a dye, stirred, and the suspension is taken at fixed time intervals to measure the dye concentration; after the adsorption is completed, the hydrotalcite adsorbent is filtered, dried, and calcined to achieve adsorbent regeneration.

9. The method for preparing a microwave-assisted Ni-Co nano-flower hydrotalcite adsorbent according to claim 8, characterized in that: The adsorbent addition amount is 0.1-1 g / L, the dye concentration is 20-500 mg / L, and the dye used is methyl orange.

Citation Information

Patent Citations

  • Nickel-cobalt layered bimetallic hydroxide flowering-on-nanosheet and preparation method thereof

    CN109650465A

Cited By

  • Preparation method and application of Y2O3-Co (OH) 2 particles

    CN120550812A

  • Preparation method of y2o3-co (oh) 2 particles and application thereof

    CN120550812B

  • Five-element co-doped porous CoFeCuMnNi-LDH nano material as well as preparation method and application thereof

    CN121819864A

  • Porous co-doped cofe cumn ni-lDH nanomaterials, methods of making and applications thereof