TMCP cooling plate shape control method suitable for steel plates with different widths

By using the MULPIC rapid cooling device to adjust cooling parameters and shielding measures in the TMCP process, the problem of buckling deformation caused by uneven cooling of the steel plate is solved, uniform cooling and plate shape stability of the steel plate are achieved, and the competitiveness of the product is improved.

CN118744162APending Publication Date: 2024-10-08WUHAN IRON & STEEL GRP ECHENG IRON & STEEL CO LTD
View PDF -1 Cites 0 Cited by

Patent Information

Application Number
CN202411190042.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-10-08

AI Technical Summary

Technical Problem

In the TMCP process, as the cooling rate of the steel plate increases, uneven cooling of the steel plate leads to the interaction between thermal stress and phase transformation stress, leading to serious buckling deformation problems, especially in the production of steel plates for bridge structures. The temperature drops rapidly at the head, tail and edges, resulting in unstable board shape.

Method used

The MULPIC rapid cooling device is used to manually adjust the upper and lower water ratio of the header, the water volume and the roller speed, and the head and tail shielding, edge shielding, side spray and other functions are used to ensure uniform cooling of the steel plate. By adjusting the lower/upper header water ratio and The edge shielding width controls the cooling rate and cooling area to ensure straight cooling of the steel plate.

Benefits of technology

It effectively improves the cooling uniformity of the steel plate, reduces residual stress and uneven deformation, and ensures the stability of the plate shape. The unevenness of the produced steel plate is ≤5mm/(1000mm), which is better than the national standard and improves the market competitiveness of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118744162A_ABST
    Figure CN118744162A_ABST
Patent Text Reader

Abstract

The invention discloses a TMCP cooling plate shape control method suitable for steel plates with different widths. Comprising the following steps: (1) smelting in a converter and continuously casting into a blank; (2) the heating and tapping temperature of a continuous casting billet is 1130-1170 DEG C; (3) double-rack two-stage rolling is adopted in the rolling process, and the finish rolling temperature of the steel plate is controlled to be 800-860 DEG C; (4) cooling process: the steel plate is straightened by a pre-straightening machine to ensure that the steel plate enters an MUPLIC device to be cooled to be straight, and the initial cooling temperature range of the steel plate is 730-780 DEG C; the roller speed is 0.9-1.3 m / s, header partition spraying is adopted, the water ratio of a lower header to an upper header is 0.9-1.3, the cooling rate is 9-15 DEG C / s, the final cooling temperature is 450-500 DEG C, the edge shielding width is 50-80 mm, and the head and tail shielding length is 0.9-1 m; according to the method, cooling process parameters are optimized, the cooling effect of the steel plates is guaranteed, meanwhile, the cooling uniformity of the steel plates is improved, the plate shape problem existing in the TMCP cooling process of the steel plates with different widths is solved, the plate shape is stably controlled within 5 mm / 1000 mm and is better than the requirement of the national standard GB / T 709-2019, and the market competitiveness of corresponding products is greatly improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of steel plate shape control, in particular to a method suitable for TMCP cooling shape control of steel plates with different widths. Background Art

[0002] TMCP is a general term for the technology of air cooling, controlled cooling and accelerated cooling based on controlled rolling with controlled heating temperature, rolling temperature and reduction during hot rolling. Since the TMCP process produces high-strength and high-toughness steel without adding too many alloy elements and without complicated subsequent heat treatment, it is considered to be a process that saves alloys and energy and is environmentally friendly. Therefore, since its development in the 1980s, it has become an indispensable technology for the production of low-alloy high-strength wide and thick plates. As the market demand for TMCP steel continues to increase, the TMCP process itself is also constantly developing in applications. From the research work in recent years, the focus is on controlled cooling, especially accelerated cooling. By accelerating the cooling rate after rolling, not only can the growth of grains be suppressed, but also the ultrafine ferrite or bainite structure required for high strength and toughness can be obtained, and even the martensite structure can be obtained. However, as the cooling rate of the steel plate increases, the uneven cooling of the steel plate is aggravated, especially the temperature drop at the head, tail and edge of the steel plate is faster. The interaction of thermal stress and phase transformation stress caused by uneven cooling will cause serious buckling deformation of the steel plate. Summary of the invention

[0003] The purpose of the present invention is to produce bridge structure steel using the TMCP process with a thickness of 16 to 40 mm, a width of 2000 to 3800 mm, and a yield strength of 345 to 500 MPa. As the cooling rate of the steel plate increases, the uneven cooling of the steel plate becomes more severe, especially the temperature drop at the head, tail and edges of the steel plate is faster. The interaction between the thermal stress and phase change stress caused by the uneven cooling can lead to severe buckling and deformation of the steel plate. A method for TMCP cooling plate shape control suitable for steel plates of different widths is provided.

[0004] The present invention is a method for TMCP cooling shape control of steel plates with different widths, which uses a MULPIC rapid cooling device to manually adjust the upper and lower water ratios, water volume and roller speed of the header, and uses head and tail shielding, edge shielding, side spraying and other functions to ensure that the steel plate is cooled evenly and has a qualified shape; specifically, the following steps are included: (1) Converter smelting and continuous casting into billets; (2) The continuous casting billet heating furnace temperature is 1130~1170℃; (3) The rolling process adopts double-stand two-stage rolling, and the final rolling temperature of the steel plate is controlled at 800-860°C; (4) Cooling process: The steel plate is straightened by the pre-straightening machine to ensure that the steel plate is straight when entering the MUPLIC device for cooling. The steel plate cooling temperature range is 730-780℃; the roller speed is 0.9-1.3m / s, the manifold partition spraying is adopted, the lower / upper manifold water ratio is 0.9-1.3, the cooling rate is 9-15℃ / s, the final cooling temperature is 450-500℃, the edge shielding width is 50-80mm, and the head and tail shielding length is 0.9-1m; among them, for steel plates of different widths, the lower / upper manifold water ratio is set differently, and the specific settings are as follows: ① For steel plates with a width of 2000-2500mm, the lower / upper header water ratio is set at 1.1-1.3, and the edge shielding width is 50-65mm; ② For steel plates with a width of 2500-3200mm, the lower / upper header water ratio is set at 1.0-1.25, and the edge shielding width is 60-75mm; ③ For steel plates with a width of 3200-3800 mm, the lower / upper header water ratio is set at 0.9-1.2, and the edge shielding width is 65-80 mm; In the above cooling process, in order to ensure cooling efficiency, a cooling fan device is used to ensure that the cooling water temperature is ≤28°C.

[0005] The method of the invention is suitable for plate shape control of steel for bridge structure produced by TMCP process with a steel plate thickness of 16 to 40 mm, a width of 2000 to 3800 mm, and a yield strength of 345 to 500 MPa. The unevenness of the produced steel plate is ≤5 mm / (1000 mm).

[0006] The MUPLIC rapid cooling device used in the method of the present invention adopts a variable flow water pillow cooling header with edge shielding and water convexity control, with 24 headers arranged at the top and bottom, divided into 4 zones A, B, C, and D, each zone is 6 meters, and the total length is 24 meters. The process parameters such as the cooling area, the water volume of each header, the upper and lower water ratio, and the roller speed can be set according to the performance requirements of each steel grade.

[0007] The process principle of the present invention is: During the cooling process of the steel plate after rolling, the cooling process parameters are adjusted to achieve the refinement of the microstructure grains, and the strength and comprehensive mechanical properties are further improved without reducing the toughness of the steel. As the cooling rate increases, the strength of the steel plate increases, and the uneven cooling of the steel plate is aggravated. In order to reduce the large residual stress and uneven deformation caused by the rapid cooling of the steel plate, the ratio of cooling water in the upper and lower headers is adjusted to evenly cool the entire steel plate. The temperature drop at the head, tail and edge of the steel plate is relatively fast. The use of head and tail shielding and edge shielding can reduce the amount of cooling water at the head, tail and edge, reduce the cooling rate, ensure uniform cooling of the entire plate, and prevent the steel plate from cooling and deformation; at the same time, as the width of the steel plate increases, the lateral cooling area increases, the lower / upper header water ratio decreases accordingly, and the edge shielding width increases accordingly to ensure the control of the lateral unevenness of the steel plate.

[0008] The present invention improves the cooling uniformity of the steel plate while ensuring the cooling effect of the steel plate by optimizing the cooling process parameters, solves the plate shape problem existing in the TMCP cooling process of steel plates of different widths, and significantly improves the curvature of TMCP process steel plates with a diameter of 16 to 40 mm, a width of 2000 to 3800 mm, and a yield strength of 345 to 500 MPa. The plate shape is stably controlled at 5 mm / (1000 mm), which is better than the requirements of the national standard GB / T 709-2019, and greatly increases the market competitiveness of the corresponding products. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 This is a photograph of the unevenness measurement of the steel plate produced in Example 7 of the present invention. DETAILED DESCRIPTION

[0010] In order to better explain the technical solution of the present invention, the technical solution of the present invention is further described below in conjunction with specific embodiments. The following embodiments are merely exemplary of the technical solution of the present invention and do not limit the present invention in any form. The serial numbers of the following embodiments are only for description and do not represent the advantages and disadvantages of the embodiments.

[0011] Table 1 is a list of main production process parameters and unevenness measurement results of steel plates in various embodiments of the present invention.

[0012] A method for TMCP cooling shape control of steel plates of different widths in various embodiments of the present invention is to use a MULPIC rapid cooling device to manually adjust the upper and lower water ratio, water volume and roller speed of the header, and use head and tail shielding, edge shielding, side spraying and other functions to ensure uniform cooling of the steel plate and qualified plate shape; specifically, the following steps are included: (1) Converter smelting and continuous casting into billets; (2) The continuous casting billet heating furnace temperature is 1130~1170℃; (3) The rolling process adopts double-stand two-stage rolling, and the final rolling temperature of the steel plate is controlled at 800-860°C; (4) Cooling process: The steel plate is straightened by the pre-straightening machine to ensure that the steel plate is straight when entering the MUPLIC device for cooling. The steel plate cooling temperature range is 730-780℃; the roller speed is 0.9-1.3m / s, the manifold partition spraying is adopted, the lower / upper manifold water ratio is 0.9-1.3, the cooling rate is 9-15℃ / s, the final cooling temperature is 450-500℃, the edge shielding width is 50-80mm, and the head and tail shielding length is 0.9-1m; among them, for steel plates of different widths, the lower / upper manifold water ratio is set differently, and the specific settings are as follows: ① For steel plates with a width of 2000-2500mm, the lower / upper header water ratio is set at 1.1-1.3, and the edge shielding width is 50-65mm; ② For steel plates with a width of 2500-3200mm, the lower / upper header water ratio is set at 1.0-1.25, and the edge shielding width is 60-75mm; ③For steel plates with a width of 3200-3800mm, the lower / upper header water ratio is set at 0.9-1.2, and the edge shielding width is 65-80mm; to ensure cooling efficiency, cooling fan equipment is used to ensure that the cooling water temperature is ≤28℃.

[0013] The method of the invention is suitable for plate shape control of steel for bridge structure produced by TMCP process with a steel plate thickness of 16 to 40 mm, a width of 2000 to 3800 mm, and a yield strength of 345 to 500 MPa. The unevenness of the produced steel plate is ≤5 mm / (1000 mm).

[0014] The MUPLIC rapid cooling device used in the method of the present invention adopts a variable flow water pillow cooling header with edge shielding and water convexity control, with 24 headers arranged at the top and bottom, divided into 4 zones A, B, C, and D, each zone is 6 meters, and the total length is 24 meters. The process parameters such as the cooling area, the water volume of each header, the upper and lower water ratio, and the roller speed can be set according to the performance requirements of each steel grade.

[0015] Table 1 List of main production process parameters and roughness measurement results of steel plates in various embodiments of the present invention

[0016] It can be seen from the above table that the steel plates produced by the TMCP process of the present invention have good plate shape, and the maximum unevenness of the steel plates is 5mm / 1000mm, which indicates that the present invention has good control over the plate shape of steel plates of different widths.

[0017] Figure 1 This is a photo of the unevenness measurement of a 28 mm (thickness) × 3200 mm (width) steel plate prepared in Example 7 of the present invention. It can be seen from the photo that the unevenness of the steel plate is ≤3 mm / 1000 mm.

[0018] The above embodiments are only specific examples for explaining the present invention and do not limit the present invention in any form. Any non-substantial changes made by anyone based on the above contents and forms without departing from the protection scope of the claims of the present invention shall be deemed to fall within the protection scope of the claims of the present invention. The present invention is not limited to the above specific implementation examples.

Claims

1. A method for TMCP cooling shape control of steel plates of different widths, which uses a MULPIC rapid cooling device to manually adjust the upper and lower water ratios, water volume and roller speed of the header, and uses head and tail shielding, edge shielding, side spraying and other functions to ensure uniform cooling of the steel plate and qualified shape; it is characterized by The steps include: (1) Converter smelting and continuous casting into billets; (2) The continuous casting billet heating furnace temperature is 1130~1170℃; (3) The rolling process adopts double-stand two-stage rolling, and the final rolling temperature of the steel plate is controlled at 800-860°C; (4) Cooling process: The steel plate is straightened by the pre-straightening machine to ensure that the steel plate is straight when entering the MUPLIC device for cooling. The steel plate cooling temperature range is 730-780℃; the roller speed is 0.9-1.3m / s, the manifold partition spraying is adopted, the lower / upper manifold water ratio is 0.9-1.3, the cooling rate is 9-15℃ / s, the final cooling temperature is 450-500℃, the edge shielding width is 50-80mm, and the head and tail shielding length is 0.9-1m; among them, for steel plates of different widths, the lower / upper manifold water ratio is set differently, and the specific settings are as follows: ① For steel plates with a width of 2000-2500mm, the lower / upper header water ratio is set at 1.1-1.3, and the edge shielding width is 50-65mm; ② For steel plates with a width of 2500-3200mm, the lower / upper header water ratio is set at 1.0-1.25, and the edge shielding width is 60-75mm; ③ For steel plates with a width of 3200-3800 mm, the lower / upper header water ratio is set at 0.9-1.2, and the edge shielding width is 65-80 mm; In the above cooling process, in order to ensure cooling efficiency, a cooling fan device is used to ensure that the cooling water temperature is ≤28°C.

2. A method for TMCP cooling shape control of steel plates of different widths according to claim 1, characterized in that: The method described in claim 1 is suitable for plate shape control of steel for bridge structures produced by TMCP process with a steel plate thickness of 16 to 40 mm, a width of 2000 to 3800 mm, and a yield strength of 345 to 500 MPa. The unevenness of the produced steel plate is ≤5 mm / 1000 mm.

3. The method for controlling the cooling shape of TMCP steel plates of different widths according to claim 1, characterized in that: The MUPLIC rapid cooling device used in the method of claim 1 uses a variable flow water pillow cooling manifold with edge shielding and water convexity control, with 24 pipes arranged above and below, divided into 4 zones A, B, C, and D, each zone is 6m long, with a total length of 24m.