Semiconductor element and forming method thereof

By weakening the covalent bonds between chalcogen atoms and transition metal atoms on the two-dimensional material layer of semiconductor components to form metallic bonds, the complexity issues caused by size reduction in semiconductor component manufacturing are solved, and current performance and production efficiency are improved. .

CN118762999APending Publication Date: 2024-10-11TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410025658.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-06-13
Filing Date
2024-01-08
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

In semiconductor component manufacturing, as component dimensions shrink, forming reliable semiconductor components becomes more complex, and there are challenges in finding a balance between maintaining high performance and improving production efficiency.

Method used

By forming a two-dimensional material layer on a substrate, containing transition metal atoms and chalcogen atoms, and forming a gate structure and source/drain contacts thereon, the bonds between chalcogen atoms and transition metal atoms are weakened through chemical molecular reactions. Covalent bonds, thus forming metallic bonds to improve contact quality.

Benefits of technology

It improves the current performance and production efficiency of semiconductor components, reduces contact resistance, and increases the contact area of ​​components, thus improving overall performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118762999A_ABST
    Figure CN118762999A_ABST
Patent Text Reader

Abstract

The invention discloses a semiconductor element and a forming method thereof. The method includes forming a two-dimensional material layer on a substrate, wherein the two-dimensional material layer includes transition metal atoms and chalcogenide atoms; forming a gate structure above the two-dimensional material layer; providing chemical molecules to the two-dimensional material layer such that atoms of the chemical molecules react with portions of the chalcogen atoms to weaken covalent bonds between the portions of the chalcogen atoms and the transition metal atoms; and forming a source / drain contact over the two-dimensional material layer, wherein contact metal atoms of the source / drain contact and transition metal atoms of the two-dimensional material layer form metal bonds.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to semiconductor devices and methods of forming the same. Background Art

[0002] The semiconductor integrated circuit (IC) industry has experienced exponential growth. Technological advances in IC materials and design have created generations of ICs, each with smaller and more complex circuits than the previous one. As ICs have evolved, functional density (i.e., the number of interconnected components per chip) has increased, while component size (i.e., the smallest component that can be manufactured by a process) has decreased. Processes that shrink in size generally provide increased production efficiency and reduced associated waste. Reductions in size also increase process and production complexity. Therefore, forming reliable semiconductor components is a challenge as size decreases. Summary of the invention

[0003] According to some embodiments of the present disclosure, a method for forming a semiconductor element includes forming a two-dimensional material layer on a substrate, wherein the two-dimensional material layer includes transition metal atoms and chalcogenide atoms; forming a gate structure above the two-dimensional material layer; providing chemical molecules to the two-dimensional material layer so that atoms of the chemical molecules react with parts of the chalcogenide atoms to weaken the covalent bonds between parts of the chalcogenide atoms and the transition metal atoms; and forming source / drain contacts above the two-dimensional material layer, wherein contact metal atoms of the source / drain contacts form metal bonds with transition metal atoms of the two-dimensional material layer.

[0004] According to some embodiments of the present disclosure, a method for forming a semiconductor element includes forming a two-dimensional material layer on a substrate, wherein the two-dimensional material layer includes transition metal atoms and chalcogen atoms; forming a gate structure above the two-dimensional material layer; removing a portion of the chalcogen atoms from the two-dimensional material layer to expose a portion of the transition metal atoms of the two-dimensional material layer; and forming a source / drain contact above the two-dimensional material layer, wherein the contact metal atoms of the source / drain contact and the portion of the transition metal atoms of the two-dimensional material layer form a metal bond.

[0005] According to some embodiments of the present disclosure, a semiconductor device includes a substrate; and a first transistor located above the substrate. The first transistor includes a first two-dimensional material channel layer, a first gate structure, and a first source / drain contact. The first two-dimensional material channel layer is made of transition metal dichalcogenide. The first gate structure surrounds the first two-dimensional material channel layer. The first source / drain contact contacts and is located at opposite ends of the first two-dimensional material channel layer, wherein there is no chalcogen atom between the metal atoms of the first source / drain contact and the transition metal atoms of the first two-dimensional material channel layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0006] The aspects of the present disclosure are best understood from the following detailed description when read in conjunction with the accompanying drawings. Note that, in accordance with standard practice in the industry, various features are not drawn to scale. In fact, the dimensions of the various features may be arbitrarily increased or reduced for clarity of discussion.

[0007] Figures 1A to 5 Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0008] Figures 6 to 8 Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0009] Figures 9 to 12 Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0010] Figures 13 to 17 Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0011] FIG. 18A to FIG. 22 Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0012] Fig.23A , Fig. 23B , Fig.23C , Fig.23D , Fig.23E The crystal structure of the two-dimensional material layer and the metal contact of some embodiments of the present disclosure;

[0013] Fig.24 The simulation results of the current under a fixed voltage for some embodiments of the present disclosure;

[0014] Fig.25A , Fig.25B , Fig.25C The crystal structure of the two-dimensional material layer and the metal contact of some embodiments of the present disclosure;

[0015] Fig.26 The simulation results of the current under a fixed voltage for some embodiments of the present disclosure;

[0016] Fig.27A and Fig.27B The crystal structure of the two-dimensional material layer of some embodiments of the present disclosure;

[0017] Fig.28A , Fig.28B , Fig.28C , Fig.28D The crystal structure of the two-dimensional material layer and the metal contact of some embodiments of the present disclosure;

[0018] Fig.29The simulation results of the current under a fixed voltage for some embodiments of the present disclosure;

[0019] Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The crystal structure of the two-dimensional material layer and the metal contact of some embodiments of the present disclosure;

[0020] Fig.31 The simulation results of the current under a fixed voltage for some embodiments of the present disclosure;

[0021] Fig.32A , Fig.32B , Fig.32C , Fig.32D The crystal structure of the two-dimensional material layer and the metal contact of some embodiments of the present disclosure;

[0022] Fig.33 The simulation results of the current under a fixed voltage for some embodiments of the present disclosure;

[0023] Fig.34A , Fig.34B , Fig.34C The crystal structure of the two-dimensional material layer and the metal contact of some embodiments of the present disclosure;

[0024] Fig.35 The simulation results of the current under a fixed voltage for some embodiments of the present disclosure;

[0025] Fig.36A , Fig.36B , Fig.36C , Fig.36D The crystal structure of the two-dimensional material layer and the metal contact of some embodiments of the present disclosure;

[0026] Fig.37 The simulation results of the current under a fixed voltage for some embodiments of the present disclosure;

[0027] FIG. 38A to FIG. 38B Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0028] FIG. 39A to FIG. 39C Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0029] FIG. 40A to FIG. 40C Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0030] FIG. 41A to FIG. 41C Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0031] FIG. 42A to FIG. 42B Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0032] FIG. 43A to FIG. 43B Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0033] FIG. 44A to FIG. 44C Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0034] FIG. 45A to FIG. 45B Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure;

[0035] Fig.46 The present invention discloses a semiconductor device according to some embodiments of the present invention.

[0036]

Explanation of symbols

[0037] 100:Substrate

[0038] 105: Gate dielectric layer

[0039] 110: Two-dimensional material layer / TMD layer

[0040] 110A, 110B: 2D material layer

[0041] 110CH: Channel area

[0042] 110SD: Source / Drain Region

[0043] 110SD_1: Part 1

[0044] 110SD_2: Part 2

[0045] 110E: Etching part

[0046] 120: passivation layer

[0047] 130: Source / drain contact

[0048] 135,135A,135B,135C:Metal

[0049] 140: Gate electrode

[0050] 150: Gate structure

[0051] 200:Substrate

[0052] 215: Spacer

[0053] 230: Source / drain contact

[0054] 230A, 230B: Metal layer

[0055] 240: Gate structure

[0056] 300:Substrate

[0057] 315: Spacer

[0058] 340: Gate structure

[0059] 340A: Gate dielectric layer

[0060] 340B: Gate electrode

[0061] A1, A2, A3, A4, A5: Situation

[0062] B1,B2,B3,B4: Situation

[0063] C1,C2,C3,C4: Situation

[0064] D1,D2,D3,D4,D5,D6: Situation

[0065] E11, E12: Curve

[0066] F1,F2,F3,F4: Situation

[0067] G1, G2, G3: Situation

[0068] H1,H2,H3,H4: Situation

[0069] CA: Chalcogen Atom

[0070] CMA: Metal Atom

[0071] CT, CT1, CT2: Contact

[0072] E1, E2, E3, E4, E5, E6: Etching process

[0073] LC1,LC2,LC3: lattice constants

[0074] MA: Metal Atom

[0075] ML: Single Layer

[0076] MP: Precursor

[0077] IO:Ion

[0078] HA: Atom

[0079] O1, O2, O3, O4: Open

[0080] P1, P2: Patterning process

[0081] TR1,TR2: Transistor DETAILED DESCRIPTION

[0082] The following disclosure provides many different embodiments or examples for implementing the different features of the subject matter provided. Specific examples of components and configurations are described below to simplify the disclosure. Of course, these are only examples and are not intended to be limiting. For example, in the following description, the formation of a first feature above or on a second feature may include an embodiment in which the first and second features are formed in direct contact, and may also include an embodiment in which additional features may be formed between the first and second features so that the first and second features may not be in direct contact. In addition, in various examples, the disclosure may repeat reference numbers and / or letters. This repetition is for the purpose of simplicity and clarity, and does not itself define the relationship between the various embodiments and / or configurations discussed.

[0083] Additionally, for ease of description, spatially relative terms such as "beneath," "below," "lower," "above," and "upper," and the like, may be used herein to describe the relationship of one element or feature to another element or feature as illustrated in the figures. The various spatially relative terms are intended to encompass different orientations of the elements in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (rotated 90 degrees or at other orientations), and the spatially relative descriptors used herein likewise interpreted accordingly.

[0084] Figures 1A to 5 The present invention discloses different stages of a method for forming a semiconductor device according to some embodiments of the present invention. Figures 1A to 5 This is a method used as an example. Figures 1A to 5 The structure shown is not limited to being formed by this method and can be formed independently of this method. Figures 1A to 5 It is described by a series of operations or steps, but it should be understood that these operations are not intended to be limiting, and in other embodiments, the order of these operations can be adjusted, and the method can also be applied to other structures. In other embodiments, some of the operations drawn or described can be omitted in whole or in part.

[0085] refer to Figure 1A and Figure 1B ,in Figure 1A A cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Figure 1B is a crystal structure of a single two-dimensional material layer according to some exemplary embodiments. The figure shows a substrate 100. In general, Figure 1AThe illustrated substrate 100 may include a bulk semiconductor substrate. Bulk semiconductors typically include crystalline semiconductor material silicon, but may also include one or more other semiconductor materials, such as germanium, silicon-germanium alloys, compound semiconductors (e.g., GaAs, AlAs, InAs, GaN, AlN, etc.), or alloys thereof (e.g., Ga x Al 1-x As、Ga x Al 1-x N、In x Ga 1-x As, etc.), oxide semiconductors (e.g., ZnO, SnO 2 、TiO 2 , Ga 2 O 3 The semiconductor material may be doped. Other substrates may be used including multilayer substrates, gradient substrates, or substrates with mixed crystal orientations. In some other embodiments, the substrate 100 may include sapphire (e.g., crystalline Al 2 O 3 ), such as sapphire with large grains or a single crystal layer or a sapphire coating. In another example, the substrate 100 can be a sapphire substrate, such as a sapphire substrate, such as a transparent sapphire substrate, such as a sapphire substrate containing α-Al 2 O 3 Other elemental semiconductors such as germanium may also be used for the substrate 100 .

[0086] In some embodiments where the substrate 100 is a doped substrate 100, the dopant concentration may be about 1×10 20 cm -3 About 1x10 21 cm -3 In some embodiments, the substrate 100 may serve as a gate structure (ie, Figure 5 Therefore, if the dopant concentration of the substrate 100 is too low (e.g., much lower than about 1×10 20 cm -3 ), the substrate 100 may not provide sufficient conductivity. On the other hand, if the dopant concentration of the substrate 100 is too high (e.g., much higher than about 1×10 21 cm -3 ), the performance of the component will not be significantly improved.

[0087] The gate dielectric layer 105 is deposited over the substrate 100. In more detail, the gate dielectric layer 105 is deposited on the front side of the substrate 100. The gate dielectric layer 105 includes, for example, an oxide, such as silicon oxide (SiO 2 ), aluminum oxide (Al 2 O 3). In some other embodiments, the gate dielectric layer 105 may include a high-k dielectric material, such as a metal oxide (e.g., oxides of Hf, Al, Zr, La, Mg, Ba, Ti, and other metals), the like, or a combination thereof, or a multilayer thereof. In some embodiments, the gate dielectric layer 105 may be deposited by a suitable deposition process, such as thermal evaporation, a chemical vapor deposition (CVD) process, a physical vapor deposition (PVD) process, an atomic layer deposition (ALD) process, or other suitable deposition processes.

[0088] The two-dimensional material layer 110 is formed above the gate dielectric layer 105. In some embodiments, the two-dimensional material layer 110 is in direct contact with the top surface of the gate dielectric layer 105. Therefore, the two-dimensional material layer 110 is vertically separated from the substrate 100 by the gate dielectric layer 105. In some embodiments, the two-dimensional material layer 110 can be patterned, for example, by a photolithography process, so that a portion of the top surface of the gate dielectric layer 105 is exposed.

[0089] As used herein, consistent with the generally accepted definition in the field of solid-state materials, "two-dimensional material (2-D material)" may refer to a crystalline material composed of a single layer of atoms. As widely accepted in the art, "two-dimensional material" may also be referred to as a "monolayer" material. In the present disclosure, "two-dimensional material" and "monolayer" material may be used interchangeably, with no difference in meaning unless otherwise specifically noted. The two-dimensional material layer 110 may be a two-dimensional material of suitable thickness. In some embodiments, the two-dimensional material includes a single layer of atoms in each of its single-layer structures, and thus the thickness of the two-dimensional material refers to the number of single layers of the two-dimensional material, which may be one single layer or more than one single layer. The coupling between two adjacent single layers of a two-dimensional material is through van der Waals forces, which are weaker than the chemical bonds between atoms within each single layer.

[0090] In some embodiments, the two-dimensional material layer 110 can be a two-dimensional semiconductor material, which can be a single layer or a stack of several layers of strong bonding layers, and attract each other through weak interlayer van der Waals forces, so that these layers can be mechanically or chemically peeled into separate atomic thin layers. Two-dimensional semiconductor materials are candidate materials for transistor channels, sources, and drains. Examples of two-dimensional semiconductor materials include transition metal dichalcogenides (TMDs), graphene, layered III-VI chalcogenides, hexagonal boron nitride (h-BN), black phosphorus, etc. In some embodiments, the two-dimensional semiconductor can include one or more layers and can have a thickness in the range of about 0.5-100 nm. The advantage of several layers of two-dimensional semiconductors is that they have high electron mobility values.

[0091] Figure 1B is a crystal structure of a single layer ML of an exemplary TMD according to some exemplary embodiments. Figure 1BIn the embodiment, a one-molecule-thick TMD material layer includes transition metal atoms MA and chalcogenide atoms CA. The transition metal atoms MA may form a layer in the middle region of the one-molecule-thick TMD material layer, and the chalcogenide atoms CA may form a top layer above the middle layer of the transition metal atoms MA and a bottom layer below the middle layer of the transition metal atoms MA. The transition metal atoms MA may be W atoms, Mo atoms, or Pt atoms, and the chalcogenide atoms CA may be S atoms, Se atoms, or Te atoms. Figure 1B In some embodiments, each transition metal atom MA is bonded (e.g., by polar covalent bonds) to six chalcogen atoms CA, and each chalcogen atom CA is bonded (e.g., by polar covalent bonds) to three chalcogen atoms CA. Throughout the description, a cross-bound layer of a transition metal atom MA and two chalcogen atoms CA may be referred to as a TMD monolayer ML. In some embodiments, a TMD monolayer ML may be a WS 2 ,WSe 2 、WTe 2 、MoS 2 、MoSe 2 、MoTe 2 , PtS 2 , PtSe 2 , PtTe 2 wait.

[0092] Reference Figure 1A , a passivation layer 120 is deposited on the two-dimensional material layer 110. In some embodiments, the passivation layer 120 may be an insulating dielectric material. The passivation layer 120 may include silicon oxide (SiO 2 ), silicon nitride (Si 3 N 4 ), silicon oxynitride (SiON), phosphosilicate glass (PSG), borosilicate glass (BSG), boron-doped phosphosilicate glass (BPSG), undoped silicate glass (USG), low dielectric constant (low-k) dielectrics such as fluorosilicate glass (FSG), silicon oxycarbide (SiOCH), carbon-doped oxide (CDO), flowable oxide or porous oxide (e.g., xerogel / aerogel), etc., or a combination thereof. The dielectric material of the passivation layer 120 can be deposited using any suitable method, such as CVD, physical vapor deposition (PVD), ALD, PEALD, PECVD, SACVD, FCVD, spin coating, and / or the like. Or a combination thereof.

[0093] refer to Figure 2 ,in Figure 21 is a cross-sectional view of an intermediate stage of manufacturing a semiconductor device. The passivation layer 120 is subjected to a patterning process P1 to form an opening O1 in the passivation layer 120. In detail, the opening O1 extends through the passivation layer 120 and exposes the two-dimensional material layer 110. In some embodiments, the patterning process P1 can be performed by a suitable photolithography process. For example, a mask layer (e.g., a photoresist) is deposited over the passivation layer 120, the mask layer is patterned to form an opening that exposes an unwanted portion of the passivation layer 120, an etching process is performed to remove the unwanted portion of the passivation layer through the opening of the mask layer, and then the mask layer is removed.

[0094] After the patterning process P1 is completed, a source / drain region 110SD may be formed in the two-dimensional material layer 110 through the opening O1 of the passivation layer 120. In some embodiments, the source / drain region 110SD is a doped region in the two-dimensional material layer 110. For example, an ion implantation process may be performed on the portion of the two-dimensional material layer 110 that is not covered by the passivation layer 120 to implant n-type or p-type dopants (e.g., As, P, B, In, etc.) into the source / drain region 110SD to form a doped region; or a dopant source layer may be first deposited over the source / drain region 110SD of the two-dimensional material layer 110, and then the dopant may be diffused from the dopant source layer into the two-dimensional material layer 110 by annealing. In some embodiments, the portion of the two-dimensional material layer 110 between the source / drain regions 110SD will serve as a channel region of the transistor and may be referred to as a channel region 110CH.

[0095] refer to Figure 3A and Figure 3B ,in Figure 3A A cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Figure 3B is a crystal structure of a single two-dimensional material layer according to some exemplary embodiments. The two-dimensional material layer 110 is subjected to an etching process E1 through the opening O1 of the passivation layer 120. In some embodiments, the source / drain region 110SD of the two-dimensional material layer 110 is subjected to an etching process E1. In some embodiments, an accelerated etching process (H 2 ) plasma performs the etching process E1 at a combination of its energy power, flow rate, pressure and temperature, which results in the incident kinetic energy range of each plasma ion being (Just above the dissociation energy of each bond within the TMD).

[0096] like Figure 3BAs shown, when the two-dimensional material layer 110 is made of TMD, an etching process E1 is performed to remove the chalcogen atoms CA of the TMD layer 110 exposed by the passivation layer 120. As described above, the TMD layer 110 may include transition metal atoms MA located in the middle region, top chalcogen atoms CA located above the transition metal atoms MA in the middle region, and bottom chalcogen atoms CA located below the transition metal atoms MA in the middle region. The etching process E1 may remove only the chalcogen atoms CA in the top layer through the opening O1 of the passivation layer 120, while leaving the transition metal atoms MA in the middle layer and the chalcogen atoms CA in the bottom layer substantially intact. In some embodiments, the bond (e.g., polar covalent bond) between the chalcogen atoms CA and the transition metal atoms MA in the top layer may be broken during the thermal cracking process caused by the etching process E1. Therefore, after the etching process E1 is completed, the transition metal atoms MA of the TMD layer 110 may be exposed through the opening O1 of the passivation layer 120.

[0097] In some embodiments, the etching process E1 is a vapor phase etching process, which will not damage the basal plane of the intermediate layer transition metal atoms MA. Figure 3B As shown, after the etching process E1 is completed, the middle layer of the transition metal atoms MA is basically intact. That is, the etching process E1 only removes the chalcogen atoms CA on the top layer of the TMD layer 110, but does not remove the transition metal atoms MA of the TMD layer 110. In addition, only part of the chalcogen atoms CA on the top layer exposed by the opening O1 of the passivation layer 120 is removed, while the other part of the top chalcogen atoms CA covered by the passivation layer 120 is still bonded to the transition metal atoms MA after the etching process E1 is completed. Moreover, since the bottom layer of the TMD layer 110 is covered by the middle layer of the transition metal atoms MA, the chalcogen atoms CA on the bottom layer of the TMD layer 110 will not be removed by the etching process E1. In other words, the etching process E1 only removes the exposed part of the chalcogen atoms CA on the top layer, and the etching process E1 does not etch through the TMD layer 110.

[0098] refer to Figure 4A and Figure 4B ,in Figure 4A A cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Figure 4B is a crystal structure of a single two-dimensional material layer according to some exemplary embodiments. After the etching process E1 is completed, the opening O1 of the passivation layer 120 (see Figure 3A and Figure 3B), and the source / drain contact 130 is in contact with the source / drain region 110SD of the two-dimensional material layer 110. In some embodiments, the source / drain contact 130 can be formed by, for example, depositing a metal layer to fill the opening O1 of the passivation layer 120, and then performing a patterning process to pattern the metal layer. In some embodiments, the source / drain contact 130 may include Pt, Au, Ag, Cu, Ni, Al, W, or other suitable contact metals. The source / drain contact 130 may be deposited by any suitable method, such as CVD, PECVD, PVD, ALD, PEALD, chemical plating, etc.

[0099] In some embodiments where the two-dimensional material layer 110 is made of TMD, as described above, the TMD layer 110 undergoes Figure 3A and Figure 3B The etching process E1 described in the embodiment includes removing the chalcogenide atoms CA of the two-dimensional material layer 110 exposed by the opening O1 of the passivation layer 120 to expose the transition metal atoms MA of the two-dimensional material layer 110. The contact metal atoms CMA of the source / drain contact 130 can form a metal bond with the transition metal atoms MA of the two-dimensional material layer 110. In other embodiments, the contact metal atoms CMA of the source / drain contact 130 also form a chemical bond with the adjacent chalcogenide atoms CA of the two-dimensional material layer 110. In some embodiments, there is no chalcogenide atom CA of the two-dimensional material layer 110 between the transition metal atom MA of the two-dimensional material layer 110 and the contact metal atom CMA of the source / drain contact 130. In some embodiments, Figure 4B The crystal structure of the crystalline structure can be obtained by a suitable technique, such as a high resolution transmission electron microscope (HRTEM), a scanning tunneling microscope (STM), and the like.

[0100] In some embodiments, because the transition metal atoms MA of the two-dimensional material layer 110 at the source / drain region 110SD of the two-dimensional material layer 110 are bonded to the contact metal atoms CMA of the source / drain contact, while the transition metal atoms MA of the two-dimensional material layer 110 at the channel region 110CH of the two-dimensional material layer 110 are still bonded to the chalcogen atoms CA of the two-dimensional material layer 110. Therefore, the binding energy of the transition metal atoms MA at the source / drain region 110SD of the two-dimensional material layer 110 may be different from the binding energy of the transition metal atoms MA at the channel region 110CH of the two-dimensional material layer 110. For example, the binding energy of the transition metal atoms MA at the source / drain region 110SD of the two-dimensional material layer 110 is less than half of the binding energy of the transition metal atoms MA at the channel region 110CH of the two-dimensional material layer 110. In some embodiments, the two-dimensional material layer 110 may be measured by X-ray photoelectron spectroscopy (XPS).

[0101] Since the contact metal atoms CMA of the source / drain contact 130 can directly form metal bonds with the transition metal atoms MA of the two-dimensional material layer 110, the contact resistance between the source / drain contact 130 and the corresponding source / drain region 110SD of the two-dimensional material layer 110 can be reduced. Therefore, the performance of the device can be improved. However, if the chalcogenide atoms CA of the two-dimensional material layer 110 are not as Figure 3A and Figure 3B The source / drain contacts 130 can only be connected to the two-dimensional material layer 110 by van der Waals force, rather than forming a metal bond with the two-dimensional material layer 110. In this case, the performance of the device may be unsatisfactory.

[0102] refer to Figure 5 ,in Figure 5 1 is a cross-sectional view of an intermediate stage of manufacturing a semiconductor device. A gate electrode 140 is formed on the back side of the substrate 100. In more detail, the gate electrode 140 is disposed on a side of the substrate 100 opposite to the gate dielectric layer 105, the two-dimensional material layer 110, the passivation layer 120, and the source / drain contacts 130. In some embodiments, the gate electrode 140 may be formed by, for example, flipping the substrate 100. Figure 4A The structure of the substrate 100 is such that the back side of the substrate 100 faces upward, and then a metal layer is deposited over the back side of the substrate 100 to form a gate electrode 140. The gate electrode 140 can be deposited by any suitable method, such as CVD, PECVD, PVD, ALD, PEALD, chemical plating, etc. In some embodiments, the gate electrode 140 may include a metal such as Cu, Al, W, Co, Ru, etc., or a combination thereof, or a multilayer thereof. In some embodiments, a chemical mechanical polishing (CMP) process may be selectively performed on the back side of the substrate 100 to reduce the thickness of the substrate 100.

[0103] In some embodiments, the gate electrode 140, the substrate 100, the gate dielectric layer 105, the two-dimensional material layer 110 and the source / drain contacts 130 are combined to form a transistor. In some embodiments, the gate electrode 140, the substrate 100 and the gate dielectric layer 105 together serve as a gate structure 150 of the transistor. The two-dimensional material layer 110 serves as a channel layer of the transistor. In some embodiments, since the gate structure 150 is disposed below the channel layer (two-dimensional material layer 110) of the transistor, the transistor may also be referred to as a "bottom-gate" transistor.

[0104] Figures 6 to 8 The following are different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. It should be noted that Figures 6 to 8 Some components can be similar to Figures 1A to 5 In the description, these components have the same reference numerals and the relevant details will not be repeated for simplicity.

[0105] Please refer to Figure 6 , Figure 6 and Figure 1A The difference between the two-dimensional material layer 110 and the two-dimensional material layer 110 is that before forming the passivation layer 120, a patterned mask 170 is formed to cover the two-dimensional material layer 110. The patterned mask 170 includes an opening O2 that exposes a portion of the two-dimensional material layer 110. Then, an etching process E2 is performed on the two-dimensional material layer 110. In some embodiments where the two-dimensional material layer 110 is made of TMD, the top chalcogen atoms of the portion of the two-dimensional material layer 110 exposed by the opening O2 of the patterned mask 170 are removed by the etching process E2. The etching process E2 is similar to Figure 3A and Figure 3B The etching process E1 discussed in the above description will not be repeated for the sake of simplicity. After the etching process E2 is completed, the two-dimensional material layer 110 includes an etched portion 110E. Here, the "etched portion" of the two-dimensional material layer 110 may represent a portion of the two-dimensional material layer 110 from which the chalcogen atoms are removed.

[0106] refer to Fig. 7A and Figure 7B ,in Fig. 7A is a cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Figure 7B The crystal structure of the single-layer two-dimensional material layer and the metal contact disclosed in the present invention. Figure 6 After the etching process E2, the patterned mask 170 is removed. Next, a passivation layer 120 is formed to cover the two-dimensional material layer 110, and source / drain contacts 130 are formed in the passivation layer 120. In some embodiments, each source / drain contact 130 is wider than the etched portion 110E of the two-dimensional material layer 110 below. In other words, the source / drain contact 130 of the two-dimensional material layer 110 can be connected to the unetched portion 110E of the two-dimensional material layer 110. Figure 6 The etching process E2 described above etches a portion of the contact. In some embodiments, the source / drain contact 130 may be formed by, for example, patterning the passivation layer 120 to form a Figure 6 The opening O2 of the patterned mask 170 is made wider, a metal layer is deposited in the opening of the passivation layer 120, and then the metal layer is patterned.

[0107] like Figure 7B As shown, some of the contact metal atoms CMA of the source / drain contact 130 can be connected to the Figure 6 The transition metal atoms MA of the two-dimensional material layer 110 exposed by the etching process E2 form a metal bond. On the other hand, because the source / drain contact 130 is wider than the etched portion 110E of the two-dimensional material layer 110, some of the contact metal atoms CMA of the source / drain contact 130 may vertically overlap the chalcogenide atoms CA. That is, a portion of the contact metal atoms CMA of the source / drain contact 130 may be vertically separated from the transition metal atoms MA of the two-dimensional material layer 110 by the chalcogenide atoms CA of the two-dimensional material layer 110. This is because Figure 6 During the described etching process E2 , these parts of the chalcogen atoms CA are not removed.

[0108] In some embodiments, a portion of the transition metal atoms MA at the source / drain region 110SD of the two-dimensional material layer 110 is bonded to the contact metal atoms CMA of the source / drain contact 130, while another portion of the transition metal atoms MA at the source / drain region 110SD of the two-dimensional material layer 110 is still bonded to the chalcogen atoms CA of the two-dimensional material layer 110. Figure 7B As shown, the binding energy of the transition metal atoms MA of the two-dimensional material layer 110 at the first portion 110SD_1 of the source / drain region 110SD may be different from the binding energy of the transition metal atoms MA of the two-dimensional material layer 110 at the second portion 110SD_2 of the source / drain region 110SD. In some embodiments, the binding energy of the transition metal atoms MA of the two-dimensional material layer 110 may be measured by X-ray photoelectron spectroscopy (XPS).

[0109] refer to Figure 8 , a gate electrode 140 is formed on the back side of the substrate 100. The gate electrode 140, the substrate 100, the gate dielectric layer 105, the two-dimensional material layer 110 and the source / drain contacts 130 together form a transistor. In some embodiments, the gate electrode 140, the substrate 100 and the gate dielectric layer 105 together serve as a gate structure 150 of the transistor. The two-dimensional material layer 110 serves as a channel layer of the transistor. In some embodiments, since the gate structure 150 is disposed below the channel layer (two-dimensional material layer 110) of the transistor, the transistor may also be referred to as a "bottom gate" transistor.

[0110] Figures 9 to 12 The following are different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. It should be noted that Figures 9 to 12 Some components can be similar to Figures 1A to 5 In the description, these components have the same reference numerals and the relevant details will not be repeated for simplicity.

[0111] Please refer to Fig. 9 , Fig. 9 and Figure 2 Similarly, the passivation layer 120 is subjected to a patterning process P2 to form an opening O3 in the passivation layer 120 . Fig. 9 The patterning process P2 and Figure 2 The difference of patterning process P1 is that Fig. 9 The patterning process P2 is performed so that each opening O3 exposes the edge of the corresponding two-dimensional material layer 110. In addition, the opening O3 may expose a portion of the gate dielectric layer 105 that is not covered by the two-dimensional material layer 110. In some embodiments, the source / drain region 110SD may be formed in the two-dimensional material layer 110 through the opening O3 of the passivation layer 120. In some embodiments, the source / drain region 110SD is a doped region in the two-dimensional material layer 110.

[0112] refer to Fig. 10A and Fig. 10B ,in Fig. 10A A cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Fig. 10B is a crystal structure of a single two-dimensional material layer in some exemplary embodiments. The two-dimensional material layer 110 is subjected to an etching process E3. In some embodiments where the two-dimensional material layer 110 is made of TMD, the portion of the top chalcogen atoms CA of the two-dimensional material layer 110 exposed by the opening O3 of the passivation layer 120 is removed by the etching process E3, such as Fig. 10B As shown. Etching process E3 is similar to Figure 3A and Figure 3B The etching process E1 is discussed in detail above, so for the sake of simplicity, the relevant details will not be repeated.

[0113] refer to Fig.11A and Fig. 11B ,in Fig.11A A cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Fig. 11B The crystalline structure of the single-layer two-dimensional material layer and the metal contact in some embodiments. After the etching process E3 is completed, the opening O3 of the passivation layer 120 (see Fig. 10A and Fig. 10B ) is formed in the gate dielectric layer 105, and the source / drain contact 130 is in contact with the source / drain region 110SD of the two-dimensional material layer 110.

[0114] like Fig. 11B As shown, in some embodiments where the two-dimensional material layer 110 is made of TMD, some contact metal atoms CMA of the source / drain contact 130 form metal bonds with transition metal atoms MA of the two-dimensional material layer 110. These transition metal atoms MA are due to Fig. 10A and Fig. 10B On the other hand, some of the contact metal atoms CMA of the source / drain contact 130 can form chemical bonds with the adjacent chalcogen atoms CA at the top layer of the single layer ML. In addition, some of the contact metal atoms CMA of the source / drain contact 130 can also form chemical bonds with the chalcogen atoms CA at the bottom layer of the single layer ML. This is because the opening O3 extends to a position flush with the bottom surface of the two-dimensional material layer 110, which will expose part of the chalcogen atoms CA at the bottom layer of the single layer ML at the edge of the two-dimensional material layer 110.

[0115] In some embodiments, because the contact metal atom CMA is connected to the transition metal atom MA of the two-dimensional material layer 110, the vertical distance (e.g., along the Y direction) between the contact metal atom CMA and the transition metal atom MA is substantially equal to the lattice constant LC1 of the contact metal atom CMA along the vertical direction (e.g., the Y direction), which is greater than the lattice constant LC2 of the two-dimensional material layer 110 along the vertical direction (e.g., the Y direction). If the chalcogenide atom CA is not removed from the two-dimensional material layer 110, the contact metal atom CMA will cover the chalcogenide atom CA, so that the vertical distance (e.g., along the Y direction) between the contact metal atom CMA and the transition metal atom MA will be greater than the lattice constant of the contact metal atom CMA along the vertical direction (e.g., the Y direction). In addition, the lateral distance (e.g., along the X direction) between the contact metal atom CMA and the transition metal atom MA is substantially equal to the lattice constant LC3 of the contact metal atom CMA along the lateral direction (e.g., the X direction).

[0116] refer to Fig.12 , a gate electrode 140 is formed on the back side of the substrate 100. The gate electrode 140, the substrate 100, the gate dielectric layer 105, the two-dimensional material layer 110 and the source / drain contacts 130 together form a transistor. In some embodiments, the gate electrode 140, the substrate 100 and the gate dielectric layer 105 together serve as a gate structure 150 of the transistor. The two-dimensional material layer 110 serves as a channel layer of the transistor. In some embodiments, since the gate structure 150 is disposed below the channel layer (two-dimensional material layer 110) of the transistor, the transistor may also be referred to as a "bottom gate" transistor.

[0117] Figures 13 to 17 The following are different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. It should be noted that Figures 13 to 17 Some components can be similar to Figures 1A to 5 In the description, these components have the same reference numerals and the relevant details will not be repeated for simplicity.

[0118] Please refer to Fig.13 , Fig.13 and Fig. 9 Similarly, the passivation layer 120 is subjected to a patterning process P2 to form an opening O3 in the passivation layer 120. In some embodiments, Fig.13 The patterning process P2 is performed so that each opening O3 exposes the edge of the corresponding two-dimensional material layer 110. In addition, the opening O3 may expose a portion of the gate dielectric layer 105 that is not covered by the two-dimensional material layer 110. In some embodiments, the source / drain region 110SD may be formed in the two-dimensional material layer 110 via the opening O3 of the passivation layer 120. In some embodiments, the source / drain region 110SD is a doped region in the two-dimensional material layer 110. The patterning process P2 may include an etching process for removing an unnecessary portion of the passivation layer 120. In some embodiments, as shown in the figure, the etchant used in the etching process of the patterning process P2 has a higher etching rate for the passivation layer 120 than for the two-dimensional material layer 110 and the gate dielectric layer 105. That is, the etching rate for the two-dimensional material layer 110 and the gate dielectric layer 105 is higher. The gate dielectric layer 105 has a higher etching resistance to the etching process of the patterning process P2 than the passivation layer 120.

[0119] refer to Fig.14 , performing an etching process E4 to remove a portion of the gate dielectric layer 105 through the opening O3 of the passivation layer 120, so that the opening O3 extends downward into the gate dielectric layer 105. In more detail, the etching process E4 may remove a portion of the gate dielectric layer 105 vertically located below the two-dimensional material layer 110, so that the bottom surface of the two-dimensional material layer 110 is exposed to the opening O3 after the etching process E4 is completed. In some embodiments, the etching process E4 may include Fig.13 The etchant used in the etching process of the patterning process P2 is different from the etchant used in the etching process E4. In some embodiments, the etchant used in the etching process E4 has a higher etching rate for the gate dielectric layer 105. That is, the two-dimensional material layer 110 and the passivation layer 120 may include a higher etching resistance than the gate dielectric layer 105 to the etching process E4. In some embodiments, after the etching process E4 is completed, the source / drain region 110SD of the two-dimensional material layer 110 is suspended above the substrate 100. That is, due to the etching process E4, at least three sides of the two-dimensional material layer 110 are exposed to the opening O3 of the passivation layer 120.

[0120] refer to Fig.15A and Fig. 15B ,in Fig.15A is a cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Fig. 15B The crystalline structure of the single-layer two-dimensional material layer and the metal contact disclosed in the present invention. The two-dimensional material layer 110 is subjected to an etching process E5 through the opening O3 of the passivation layer 120. In some embodiments, the source / drain region 110SD of the two-dimensional material layer 110 is subjected to an etching process E5. In some embodiments, an accelerated etching process (H 2 ) The plasma performs the etching process E5 under the combination of its energy power, flow rate, pressure and temperature, so that the incident kinetic energy range of each plasma ion is (just above the dissociation energy of each bond in the TMD). In some embodiments, the etchant of etching process E5 is different from Fig.14 The etchant of the etching process E4 described in the above embodiment.

[0121] like Fig. 15B As shown, when the two-dimensional material layer 110 is made of TMD, an etching process E5 is performed to remove the chalcogen atoms CA of the TMD layer 110 exposed through the opening O3 of the passivation layer 120. As described above, the TMD layer 110 may include transition metal atoms MA located in the middle region, top chalcogen atoms CA located above the transition metal atoms MA, and bottom chalcogen atoms CA located below the transition metal atoms MA. The etching process E5 can remove the chalcogen atoms CA in the top layer through the opening O3 of the passivation layer 120, and can also remove the chalcogen atoms CA in the bottom layer through the opening O3 of the passivation layer 120. This is because Fig.14 The etching process E5 is performed, and the surface and bottom surface of the two-dimensional material layer 110 are exposed. In some embodiments, the bonding (e.g., polar covalent bonding) between the chalcogen atoms CA at the top bottom layer and the transition metal atoms MA can be destroyed by thermal decomposition (e.g., etching process E5). Therefore, after the etching process E5 is completed, the top side and bottom side of the transition metal atoms MA of the TMD layer 110 can be exposed through the opening O3 of the passivation layer 120.

[0122] In some embodiments, the etching process E5 is a vapor phase etching process that does not damage the base surface of the transition metal atoms MA. Fig. 15B As shown, after the etching process E5 is completed, the intermediate layer of the transition metal atoms MA is substantially intact. That is, the etching process E5 only removes the chalcogen atoms CA of the TMD layer 110, but does not remove the transition metal atoms MA of the TMD layer 110. In addition, part of the TMD layer 110 is covered by the passivation layer 120 and the gate dielectric layer 105 during the etching process E5. Therefore, the etching process E5 only removes the exposed part of the chalcogen atoms CA, while the etching process E5 does not remove the chalcogen atoms CA covered by the passivation layer 120 and the gate dielectric layer 105.

[0123] refer to Fig.16A and Fig. 16B ,in Fig.16Ais a cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Fig. 16B The crystal structure of the single-layer two-dimensional material layer and the metal contact disclosed in the present invention. After completing the etching process E5 (see Fig.15A and Fig. 15B ) after that, in the opening O3 of the passivation layer 120 (see Fig.15A and Fig. 15B ), and the source / drain contact 130 is in contact with the source / drain region 110SD. In some embodiments, the source / drain contact 130 may extend from the top surface of the two-dimensional material layer 110, through the sidewall of the two-dimensional material layer 110, and reach the bottom surface of the two-dimensional material layer 110. That is, a portion of the source / drain contact 130 may extend to a position perpendicular to the substrate 100 and the two-dimensional material layer 110. The source / drain contact 130 may contact the two-dimensional material layer 110, the sidewall of the gate dielectric layer 105, and the top surface of the substrate 100.

[0124] In some embodiments where the two-dimensional material layer 110 is made of TMD, as described above, the TMD layer 110 undergoes Fig.15A and Fig. 15B The etching process E5 described in . The chalcogenide atoms CA of the two-dimensional material layer 110 exposed by the opening O3 of the passivation layer 120 are removed to expose the transition metal atoms MA of the two-dimensional material layer 110. The contact metal atoms CMA of the source / drain contact 130 may form a metal bond with the transition metal atoms MA of the two-dimensional material layer 110. In some embodiments, the contact metal atoms CMA may form a metal bond with the transition metal atoms MA via the top side of the transition metal atom MA layer, and form a metal bond with the transition metal atoms MA via the bottom side of the transition metal atom MA layer. In some other embodiments, the contact metal atoms CMA of the source / drain contact 130 may also form a chemical bond with the adjacent chalcogenide atoms CA of the two-dimensional material layer 110. In some embodiments, the contact metal atoms CMA may form a chemical bond with the chalcogenide atoms CA of the top layer of the monolayer ML of the two-dimensional material layer 110 and a chemical bond with the chalcogenide atoms CA of the bottom layer of the monolayer ML.

[0125] refer to Fig.17 , a gate electrode 140 is formed on the back side of the substrate 100. The gate electrode 140, the substrate 100, the gate dielectric layer 105, the two-dimensional material layer 110 and the source / drain contacts 130 together form a transistor. In some embodiments, the gate electrode 140, the substrate 100 and the gate dielectric layer 105 together serve as a gate structure 150 of the transistor. The two-dimensional material layer 110 serves as a channel layer of the transistor. In some embodiments, since the gate structure 150 is disposed below the channel layer (two-dimensional material layer 110) of the transistor, the transistor may also be referred to as a "bottom gate" transistor.

[0126] FIG. 18A to FIG. 22 The following are different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. It should be noted that FIG. 18A to FIG. 22 Some components can be similar to Figures 1A to 5 In the description, these components have the same reference numerals and the relevant details will not be repeated for simplicity.

[0127] refer to Fig.18A and Fig.18B ,in Fig.18A is a cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Fig.18B The crystal structure of the single-layer two-dimensional material layer and the metal contact disclosed in this invention can be Figure 2 The structure shown in FIG. 1 is subjected to an etching process E6 to remove the Figure 2 ) exposes a portion of the two-dimensional material layer 110. In some embodiments, the etching process E6 etches through the two-dimensional material layer 110 to form an opening O4 exposing the gate dielectric layer 105. In some embodiments, the etching process E6 may be a plasma dry etching process using Ar plasma.

[0128] like Fig.18B As shown, when the two-dimensional material layer 110 is made of TMD, the TMD layer 110 may include transition metal atoms MA located in the middle region, top chalcogen atoms CA located above the transition metal atoms MA in the middle layer, and bottom chalcogen atoms CA located below the transition metal atoms MA in the middle layer. In some embodiments, the etching process E6 may remove the transition metal atoms MA formed by the opening O1 (see Figure 2 ) vertically exposed chalcogenide atoms CA and transition metal atoms MA. In more detail, part of the chalcogenide atoms CA in the top layer and the bottom layer of the monolayer ML and the transition metal atoms MA in the middle region of the monolayer ML are etched away. Therefore, some chalcogenide atoms CA in the top layer, some chalcogenide atoms CA in the bottom layer, and some transition metal atoms MA in the monolayer ML in the middle region are exposed to the opening O4.

[0129] refer to Fig.19A and Fig.19B ,in Fig.19A is a cross-sectional view of an intermediate stage in the manufacture of a semiconductor device. Fig.19B The crystal structure of the single-layer two-dimensional material layer and the metal contact disclosed in the present invention. Some exemplary embodiments. After the etching process E6 is completed (see Fig.18A and Fig.18B), depositing a first metal layer 230A in the opening O4. The first metal layer 230A may be deposited by any suitable method, such as CVD, PECVD, PVD, ALD, PEALD, electrochemical plating (ECP), chemical plating, etc. In some embodiments, the first metal layer 230A may include Pt, Au, Ag, Cu, Ni, Al, W, Mo, or other suitable contact metals. In some embodiments where the two-dimensional material layer 110 is made of TMD, the first metal layer 230A may include the same metal as the transition metal of the two-dimensional material layer 110. For example, if the two-dimensional material layer 110 is made of WS 2 ,WSe 2 or WTe 2 If the two-dimensional material layer 110 is made of MoS 2 、MoSe 2 or MoTe 2 If the two-dimensional material layer 110 is made of PtS 2 , PtSe 2 or PtTe 2 The first metal layer 230A may include Pt.

[0130] refer to Fig.19B As described above, the TMD layer 110 undergoes Fig.18A and Fig.18B The contact metal atoms CMA of the first metal layer 230A may form a metal bond with the transition metal atoms MA of the two-dimensional material layer 110. In some other embodiments, the contact metal atoms CMA130 of the first metal layer 230A may also form a metal bond with the transition metal atoms MA of the two-dimensional material layer 110. Fig.18A and Fig.18B ) form chemical bonds between the chalcogen atoms CA at the top and bottom layers of the monolayer ML.

[0131] refer to Fig. 20 . The second metal layer 230B is deposited in the opening O4 and above the first metal layer 230A. The second metal layer 230B may be deposited by any suitable method, such as CVD, PECVD, PVD, ALD, PEALD, electrochemical plating (ECP), chemical plating, etc. In some embodiments, the second metal layer 230B may include Pt, Au, Ag, Cu, Ni, Al, W, Mo, or other suitable contact metals. In some embodiments where the two-dimensional material layer 110 is made of TMD, the first metal layer 230A may include a metal that is the same as the transition metal of the two-dimensional material layer 110, and the second metal layer 230B may include a metal that is different from the transition metal of the two-dimensional material layer 110. For example, if the two-dimensional material layer 110 is made of WS 2 ,WSe2 or WTe 2 If the two-dimensional material layer 110 is made of MoS 2 、MoSe 2 or MoTe 2 If the two-dimensional material layer 110 is made of PtS 2 , PtSe 2 or PtTe 2 The second metal layer 230B may include a metal different from Pt. In some embodiments, the second metal layer 230B may include a work function value higher than the work function value of the first metal layer 230A and the work function value of the transition metal of the two-dimensional material layer 110 .

[0132] refer to Fig.21 The first metal layer 230A and the second metal layer 230B are patterned to form source / drain contacts 230. In some embodiments, each source / drain contact 230 includes a remaining portion of the first metal layer 230A and the second metal layer 230B. In some embodiments, the first metal layer 230A and the second metal layer 230B may be patterned by, for example, forming a patterned mask, wherein the patterned mask has openings exposing unwanted portions of the first metal layer 230A and the second metal layer 230B, performing an etching process to remove unwanted portions of the first metal layer 230A and the second metal layer 230B, and then removing the patterned mask.

[0133] refer to Fig. 22 , a gate electrode 140 is formed on the back side of the substrate 100. The gate electrode 140, the substrate 100, the gate dielectric layer 105, the two-dimensional material layer 110 and the source / drain contacts 130 together form a transistor. In some embodiments, the gate electrode 140, the substrate 100 and the gate dielectric layer 105 together serve as a gate structure 150 of the transistor. The two-dimensional material layer 110 serves as a channel layer of the transistor. In some embodiments, since the gate structure 150 is disposed below the channel layer (two-dimensional material layer 110) of the transistor, the transistor may also be referred to as a "bottom gate" transistor.

[0134] Fig.23A , Fig. 23B , Fig.23C , Fig.23D , Fig.23E The crystal structure of the two-dimensional material layer and the metal contact of some embodiments disclosed herein. In more detail, Fig.23A , Fig. 23B , Fig.23C , Fig.23D , Fig.23EThe crystal relationship between the TMD layer and the contact at the atomic scale is shown respectively. Fig.24 The simulation results of the current under a fixed voltage are shown in FIG.

[0135] Fig.23A is an example in which the contact CT is disposed on the top side of the TMD monolayer ML, wherein the chalcogenide atoms CA of the TMD monolayer ML are not removed, and thus the contact metal atoms CMA are connected to the chalcogenide atoms CA by van der Waals forces.

[0136] Fig. 23B This is an example of setting the contact CT at the edge side of the TMD monolayer ML, wherein the chalcogen atom CA of the TMD monolayer ML is not removed, and the contact metal atom CMA can form a metallic bond with the transition metal atom MA exposed at the edge side of the TMD monolayer ML.

[0137] Fig.23C is an example where the contact CT is placed on the top side of the TMD monolayer ML, e.g. Figures 1A to 5 and Figures 6 to 8 In such an embodiment, some of the chalcogen atoms CA of the TMD monolayer ML are removed and can be replaced with contact metal atoms CMA. Thus, the contact metal atoms CMA can form metallic bonds with the transition metal atoms MA exposed through the top side of the TMD monolayer ML. Note that Fig.23C In the process, the contact metal atoms CMA can form a ratio with the exposed transition metal atoms MA. Fig. 23B More metal bonds.

[0138] Fig.23D is an example in which the contact CT is disposed on the top side of the TMD monolayer ML and extends to the edge side of the TMD monolayer ML, e.g. Figures 9 to 12 In such an embodiment, some chalcogen atoms CA of the TMD monolayer ML are removed and can be replaced with contact metal atoms CMA. Therefore, the contact metal atoms CMA can form metallic bonds with the transition metal atoms MA exposed from the top side of the TMD monolayer ML and from the edge side of the TMD monolayer ML. Note that in Fig.23D In the process, the contact metal atoms CMA can form a ratio with the exposed transition metal atoms MA. Fig.23C More metal bonds.

[0139] Fig.23E is an example in which the contact CT is disposed on the top side of the TMD monolayer ML and extends to the edge side and the bottom side of the TMD monolayer ML, e.g. Figures 13 to 17In such an embodiment, some chalcogen atoms CA of the TMD monolayer ML are removed from the top and bottom sides of the TMD monolayer ML and can be replaced with contact metal atoms CMA. Thus, the contact metal atoms CMA can form metallic bonds with the transition metal atoms MA exposed from the top, edge, and bottom sides of the TMD monolayer ML. Note that in Fig.23E In the process, the contact metal atoms CMA can form a ratio with the exposed transition metal atoms MA. Fig.23D More metal bonds.

[0140] like Fig.24 As shown, the figure shows the simulated current of five cases A1, A2, A3, A4, and A5 under a fixed voltage, among which cases A1, A2, A3, A4, and A5 are respectively Fig.23A , Fig. 23B , Fig.23C , Fig.23D , Fig.23E In case A3, the chalcogenide atom CA is replaced by the contact metal atom CMA on one side of the TMD monolayer ML. The simulated current of case A3 is higher than that of cases A1 and A2. In addition, the structure of case A4 ( Fig.23D ) has a structure that is larger than that of case A3 by contacting the edge side of the TMD monolayer ML ( Fig.23C ) larger contact area. Therefore, the current of case A4 is substantially equal to the sum of the currents of cases A2 and A3. In addition, the structure of case A5 ( Fig.23E ) has a larger contact area with the TMD single layer ML than that of the structure of case A4 ( Fig.23D ) is larger (greater than twice). Therefore, the current of case A5 is twice higher than the current of case A4. Therefore, it can be seen that when the chalcogenide atoms CA of the TMD monolayer ML are replaced by the contact metal atoms CMA of the contact CT, the current can be increased. Moreover, when the contact CT contacts the TMD monolayer ML on more sides, the contact area between the contact CT and the TMD monolayer ML will increase, and the current can be increased.

[0141] Fig.25A , Fig.25B , Fig.25C The crystal structure of the two-dimensional material layer and the metal contact according to some embodiments of the present disclosure. Fig.26 The simulation results of the current under a fixed voltage are shown in FIG.

[0142] Fig.25A The left side of FIG. 4 shows the crystal structure of the TMD monolayer ML, in which two columns of chalcogen atoms CA of the TMD monolayer ML are removed. Fig.25AThe right side of FIG. 1 shows a cross-sectional view, in which a contact CT is formed over the TMD monolayer ML and the removed chalcogen atom CA of the TMD monolayer ML is replaced by one contact metal atom CMA (or one column of contact metal atoms CMA). In some embodiments, the contact length between the contact CT and the TMD monolayer ML can be about 3.0×10 -4 μm to about 3.25x10 -4 μm, for example, 3.125x10 -4 μm.

[0143] Fig.25B The left side of FIG. 4 shows the crystal structure of a TMD monolayer ML, in which four columns of chalcogen atoms CA of the TMD monolayer ML are removed. Fig.25B The right side of FIG. 1 shows a cross-sectional view, in which a contact CT is formed over the TMD monolayer ML and the removed chalcogen atoms CA of the TMD monolayer ML are replaced by two contact metal atoms CMA (or two columns of contact metal atoms CMA). In some embodiments, the contact length between the contact CT and the TMD monolayer ML can be about 6.0×10 -4 μm to about 6.5x10 -4 μm, for example, 6.25x10 -4 μm.

[0144] Fig.25C The left side of FIG. 4 shows the crystal structure of a TMD monolayer ML, in which an infinite column (eg, a macroscopic number of columns) of chalcogen atoms CA of the TMD monolayer ML is removed. Fig.25C The right side of shows a cross-sectional view, where a contact CT is formed over the TMD monolayer ML and the removed chalcogen atoms CA of the TMD monolayer ML are replaced by contact metal atoms CMA.

[0145] like Fig.26 As shown, the simulated currents of four cases B1, B2, B3, and B4 under a fixed voltage are shown, where case B1 is Fig. 23B The simulation results of the structure (side contact only) are shown in Figure 2. Cases B2, B3, and B4 are Fig.25A , Fig.25B , Fig.25C The results show that when more chalcogen atoms CA of the TMD monolayer ML are replaced by contact metal atoms CMA of the contact CT, the current increases. That is, when the contact length between the contact metal atom CMA and the transition metal atom MA increases, the current will increase accordingly. In addition, cases B1 and B2 have substantially the same current value, which is because the structures of the two cases (e.g., Fig. 23B and Fig.25AIn the structure of ), the contact metal atom CMA and the transition metal atom MA have substantially the same contact area. The results further show that when the contact area between the contact metal atom CMA and the transition metal atom MA increases, the current increases.

[0146] Fig.27A and Fig.27B The crystal structure of the two-dimensional material layer of some embodiments disclosed herein. Fig.27A A side view showing the crystal structure of a TMD monolayer ML ( Fig.27A ) and top view ( Fig.27A ), where the chalcogen atoms CAML are removed from the top and bottom sides of the TMD monolayer, as Figures 13 to 17 The embodiment discussed. Fig.27B A side view of the crystal structure of a TMD monolayer ML is shown when a contact is formed over the TMD monolayer ML ( Fig.27B ) and top view ( Fig.27B ), such as Figures 13 to 17 The embodiment discussed. Note that for the sake of brevity, Fig.27B The contacting metal atoms are not shown in FIG.

[0147] exist Fig.27A and Fig.27B In an embodiment, the chalcogen atoms CA are removed from the top and bottom sides of the TMD monolayer ML, which can reduce the contact resistance between the TMD monolayer ML and the contact formed on the TMD monolayer ML. This is because the transition metal atoms MA exposed by the TMD monolayer ML will reconstruct and relax during the contact formation. For example, if the contact is made of Pt and the TMD monolayer ML is made of WS 2 The exposed W atoms (transition metal atoms MA) will be Fig.27A The direction of the arrow changes its arrangement. Fig.27B In the case of W, the exposed W atoms will be dragged by the Pt metal to align with the Pt atoms, as shown in Fig.27B This is because after the W atom loses the WS bond, the exposed W atom in the TMD monolayer ML may fall into the lattice position of the Pt metal.

[0148] Fig.28A , Fig.28B , Fig.28C , Fig.28D The crystal structure of the two-dimensional material layer and the metal contact according to some embodiments of the present disclosure. Fig.29 The simulation results of the current under a fixed voltage are shown in FIG.

[0149] Fig.28A , Fig.28B, Fig.28C , Fig.28D is an example of contacting CT with the top, edge, and bottom sides of a TMD monolayer ML, e.g. Figures 13 to 17 The embodiment discussed. Fig.28A , Fig.28B , Fig.28C , Fig.28D The difference is that the contact length between the contact metal atom CMA and the transition metal atom MA increases with Fig.28A , Fig.28B , Fig.28C , Fig.28D That is, as Fig.28A , Fig.28B , Fig.28C , Fig.28D , the contact metal atom CMA bonds with more transition metal atoms MA.

[0150] like Fig.29 As shown, the simulated currents of C1, C2, C3, and C4 in four cases under a fixed voltage are shown, where C1, C2, C3, and C4 are Fig.28A , Fig.28B , Fig.28C , Fig.28D The results show that when the contact length between the contact metal atom CMA and the transition metal atom MA increases, the current will increase. In addition, when the contact length approaches infinity (for example, Fig.28D ), the current will converge to a stable current.

[0151] Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The crystal structure of the two-dimensional material layer and the metal contact of some embodiments disclosed herein. In more detail, Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The left side of Figure 2 shows the side view of the crystal structure of the TMD monolayer ML and the contact CT in different cases. Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The right side shows the top view of the crystal structure of TMD monolayer ML under different conditions. Fig.31 The simulation results of the current under a fixed voltage are shown in FIG.

[0152] Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The TMD monolayer ML is made of the same material, for example, WS in some embodiments. 2 .However, Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The contact CT is made of different materials. For example, Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The contact CT can be Pt, Ni, Al, Au, Cu, Ag, respectively, where these metals all have a face-centered cubic (FCC) crystal structure. As shown on the right side of the figure. Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E As shown, after relaxation, the exposed W atoms can reorganize and relax and fall into the crystal structure of these metals (e.g., Pt, Ni, Al, Au, Cu). Fig.30F As shown on the right, the exposed W atoms do not fall into the crystal structure of the metal (eg, Ag).

[0153] like Fig.31 As shown, the simulated currents of six cases D1, D2, D3, D4, D5, and D6 under a fixed voltage are shown, where the cases D1, D2, D3, D4, D5, and D6 are respectively Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The results show that after the transition metal atom MA is bonded to the contact metal atom CMA, the current can only be improved if the transition metal atom MA is effectively twisted into a crystal arrangement similar to that of the contact metal atom CMA, for example Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E Example.

[0154] Fig.31 Further curves E11 and E12 are shown. Curve E11 is the work function value of the transition metal (such as W in such an embodiment) of the TMD monolayer. On the other hand, curve E12 is Fig. 30A , Fig. 30B , Fig. 30C , Fig.30D , Fig.30E , Fig.30F The work function trend of the contact metal, such as Pt, Ni, Al, Au, Cu, Ag. It can be seen that when the work function value of the contact metal is greater than the work function value of the TMD monolayer transition metal, the current can be significantly improved, such as case D1. Results, return to reference Figures 1A to 22 If the source / drain contacts 130 (or the second metal layer 230B) include a metal having a work function value higher than the work function value of the transition metal of the two-dimensional material layer 110 , the current of the transistor may be improved.

[0155] Fig.32A , Fig.32B , Fig.32C , Fig.32D The crystal structure of the two-dimensional material layer and the metal contact according to some embodiments of the present disclosure. Fig.33 The simulation results of the current under a fixed voltage are shown in FIG.

[0156] Fig.32A , Fig.32B , Fig.32C , Fig.32D The contacts CT are made of the same material, for example, Pt in some embodiments. However, Fig.32A , Fig.32B , Fig.32C , Fig.32D The TMD monolayer ML is made of different materials. For example, Fig.32A , Fig.32B , Fig.32C , Fig.32D The TMD single layer ML is composed of WS 2 ,WSe 2 、MoSe 2 and MoS 2 It is noteworthy that the exposed W atoms and exposed Se atoms of the TMD monolayer ML will fall into the crystal arrangement as the contacting metal atoms (Pt).

[0157] like Fig.33 As shown, the simulated currents of four cases F1, F2, F3, and F4 under fixed voltage are shown, where cases F1, F2, F3, and F4 are respectively Fig.32A , Fig.32B , Fig.32C , Fig.32D. Comparing cases F1 and F2, the currents of cases F1 and F2 are substantially the same. Similarly, comparing cases F3 and F4, the currents of cases F3 and F4 are substantially the same. Therefore, it can be seen that the materials based on the same transition metal (e.g., W or Mo) and the chalcogen atom CA (e.g., S or Se) do not significantly affect.

[0158] Fig.34A , Fig.34B , Fig.34C The crystal structure of the two-dimensional material layer and the metal contact according to some embodiments of the present disclosure. Fig.35 The simulation results of the current under a fixed voltage are shown in FIG.

[0159] Fig.34A , Fig.34B , Fig.34C The TMD monolayer ML is made of the same material, for example, WS in some embodiments. 2 .However, Fig.34A , Fig.34B , Fig.34C The contacts are different. For example, Fig.34A In the embodiment, the contact CT1 is connected to the TMD single layer ML via a side contact, wherein the contact CT1 may include a first metal, such as Pt. Fig.34B In the embodiment, the contact CT2 is connected to the TMD monolayer ML via a side contact, wherein the contact CT2 may include a second metal, such as W, wherein the second metal is different from the first metal of the contact CT1. In some embodiments, the second metal may be the same as the transition metal of the TMD monolayer ML, such as W. Fig.34C In FIG. 5 , multiple metal contacts are connected to the TMD single layer ML, wherein contact CT2 is connected to the TMD single layer ML, and contact CT1 is connected to contact CT2.

[0160] like Fig.35 As shown, the simulated currents of three cases G1, G2 and G3 under fixed voltage are shown, where cases G1, G2 and G3 are Fig.34A , Fig.34B , Fig.34C Simulation results of the structure of . Comparing cases G1 and G2, it can be seen that when the contact metal (e.g., CT2) is the same as the transition metal of the TMD monolayer ML, the current can be improved. In addition, comparing cases G1, G2, and G3, it can be seen that the current of case G3 (e.g., about 1536 μA / μm) is greater than the sum of the current of case C1 (e.g., about 428 μA / μm) and the current of case C2 (e.g., about 1052 μA / μm). That is, when using multi-metal contacts, the contact resistance can be reduced and the current can be further increased.

[0161] Fig.36A , Fig.36B , Fig.36C , Fig.36D The crystal structure of the two-dimensional material layer and the metal contact according to some embodiments of the present disclosure. Fig.37 The simulation results of the current under a fixed voltage are shown in FIG. Fig.36A , Fig.36B , Fig.36C , Fig.36D The left side shows the side view of the crystal structure of TMD monolayer and contact in different cases. Fig.36A , Fig.36B , Fig.36C , Fig.36D The right side shows perspective views of the crystal structures of TMD monolayers and contacts for different cases.

[0162] Fig.36A , Fig.36B , Fig.36C , Fig.36D 1 shows a structure in which the TMD single layer ML is first etched to form an opening extending through the TMD single layer ML, then the contact CT2 is filled in the opening, and the contact CT1 is formed over the contact CT2. Fig.36A , Fig.36B , Fig.36C , Fig.36D Examples and FIG. 18A to FIG. 22 For example, contact CT2 may be similar to FIG. 18A to FIG. 22 The first metal layer 230A discussed in the above, while the contact CT1 may be similar to FIG. 18A to FIG. 22 The second metal layer 230B discussed in . Fig.36A , Fig.36B , Fig.36C , Fig.36D The difference is that the length of contact CT2 increases with Fig.36A , Fig.36B , Fig.36C , Fig.36D The contact area between contact CT2 and contact CT1 increases as Fig.36A , Fig.36B , Fig.36C , Fig.36D In some embodiments, Fig.36A is an example of removing two rows of chalcogen atoms from a TMD monolayer ML, Fig.36B is an example of removing 4 columns of chalcogen atoms from a TMD monolayer ML, Fig.36C is an embodiment of removing 6 columns of chalcogen atoms of the TMD monolayer ML, Fig.36D is an embodiment of removing an infinite number of columns (eg, a macroscopic number of columns) of chalcogen atoms of a TMD monolayer ML.

[0163] like Fig.37As shown, the simulated currents of three cases H1, H2, H3 and H4 under fixed voltage are shown, where cases H1, H2, H3 and H4 are Fig.36A , Fig.36B , Fig.36C , Fig.36D It can be seen that when the contact area between the contact CT2 and the contact CT1 increases, the current can be improved.

[0164] FIG. 38A to FIG. 38B The following are different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. It should be noted that: FIG. 38A to FIG. 38B Some elements described are similar to those described above, these elements are labeled with the same reference numerals, and the relevant details will not be repeated for the sake of brevity.

[0165] exist Fig.38A In FIG. 1 , a two-dimensional material layer 110 is shown. In some embodiments, although Fig.38A Not shown in FIG. 1 is a gate structure (ie, Figure 5 The gate structure 150) may contact the two-dimensional material layer 110. Fig.38B In the method, source / drain contacts 130 are formed on opposite ends of the two-dimensional material layer 110. In more detail, the method includes replacing non-metal atoms, such as chalcogenide or nitrogen, with metal atoms so that the metal atoms directly bond with the metal atoms of the two-dimensional material layer 110 and serve as the source / drain contacts 130 of the transistor.

[0166] In some embodiments, the removal of non-metal atoms from the two-dimensional material layer 110 can be achieved by atomic-layer-etching (ALE) or dry etching. The ALE process can use chemical adsorption species such as Cl 2 , BCl 3 CF 4 and WF 6 The dry etching process may include plasma etching using Ar or He ions. The process temperature window of the chemically adsorbed species is below 400° C., for example, about 25° C. to 400° C. The kinetic energy of the Ar or He ions is above 20 eV, for example, about 20 eV to 50 eV. The operating pressure is in the range of about 0.1 mtorr to about 10 mtorr.

[0167] FIG. 39A to FIG. 39C Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. FIG. 39A to FIG. 39C The method of forming source / drain contacts 130 on opposite ends of the two-dimensional material layer 110 is shown. It can be understood that FIG. 39A to FIG. 39C The method described in is suitable for forming Figures 1A to 5 , Figures 6 to 8 , Figures 9 to 12 , Figures 13 to 17 The source / drain contacts 130 and FIG. 18A to FIG. 22 Source / drain contacts 230 are provided.

[0168] exist Fig.39A In, such as BCl 3 or CF 4 Chemical molecules such as chemisorbed species are supplied to the two-dimensional material layer 110 to weaken the bonding between the chalcogenide atoms CA (non-metal atoms) and the metal atoms MA. This is because the atoms HA of the chemisorbed species, such as halogen atoms (i.e., chlorine (Cl) or fluorine (F)), can bond with the chalcogenide atoms CA of the two-dimensional material layer 110, so that the covalent bond between the chalcogenide atoms CA and the metal atoms MA is weakened (or broken).

[0169] exist Fig.39B In the embodiment, after providing the chemically adsorbed substance, ion bombardment (i.e., plasma etching) is performed by using Ar or He ions IO to remove the chalcogen atoms CA bonded to the atoms HA of the chemically adsorbed substance in the two-dimensional material layer 110. As described above, the covalent bonds between the chalcogen atoms CA and the metal atoms MA are weakened (or broken) due to the atoms HA of the chemically adsorbed substance. Therefore, the chalcogen atoms CA can be easily removed during the ion bombardment, and the metal atoms MA of the two-dimensional material layer 110 are exposed.

[0170] exist Fig.39C , a deposition process is performed to form the source / drain contact 130. As described above, a portion of the chalcogenide atoms CA of the two-dimensional material layer 110 is removed to expose the metal atoms MA of the two-dimensional material layer 110. Therefore, the contact metal atoms CMA of the source / drain contact 130 may form a metal bond with the metal atoms MA of the two-dimensional material layer 110. In some embodiments, there is no chalcogenide atom CA of the two-dimensional material layer 110 between the metal atoms MA of the two-dimensional material layer 110 and the contact metal atoms CMA of the source / drain contact 130.

[0171] FIG. 40A to FIG. 40C Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. FIG. 40A to FIG. 40C The method of forming source / drain contacts 130 on opposite ends of the two-dimensional material layer 110 is shown. It can be understood that FIG. 40A to FIG. 40C The method described in is suitable for forming Figures 1A to 5 , Figures 6 to 8 , Figures 9 to 12 , Figures 13 to 17 The source / drain contacts 130 and FIG. 18A to FIG. 22 Source / drain contacts 230 are provided.

[0172] Fig.40AIn the case of chemical adsorption, such as H 2 , free radical H atom, BCl 3 or CF 4 is supplied to the two-dimensional material layer 110 to weaken (or break) the covalent bond between the chalcogenide atom CA (non-metal atom) and the metal atom MA. This is because the atoms HA of the chemically adsorbed substance, such as the halogen atoms (i.e., chlorine (Cl) or fluorine (F)) or hydrogen (H) atoms of the chemically adsorbed substance, can react with the chalcogenide atom CA of the two-dimensional material layer 110, so that the covalent bond between the chalcogenide atom CA and the metal atom MA is weakened (or broken). In some embodiments, the atoms HA of the chemically adsorbed substance can react with the chalcogenide atom CA of the two-dimensional material layer 110 to form a diffusible sulfide (e.g., HS-).

[0173] exist Fig.40B In the process, a deposition process is performed to form the source / drain contacts 130. As described above, part of the chalcogen atoms CA of the two-dimensional material layer 110 reacts with the halogen atoms or the hydrogen (H) atoms to form diffusible sulfides, and the metal deposition process can drive away the diffusible non-metal atoms of the two-dimensional material layer 110. Therefore, the contact metal atoms CMA of the source / drain contacts 130 can form metal bonds with the metal atoms MA of the two-dimensional material layer 110.

[0174] exist Fig.40C In the process, the deposition process is performed until all the diffusible non-metal atoms (i.e., chalcogen atoms CA) of the two-dimensional material layer 110 are driven away. Therefore, there are no chalcogen atoms CA of the two-dimensional material layer 110 between the metal atoms MA of the two-dimensional material layer 110 and the contact metal atoms CMA of the source / drain contact 130.

[0175] FIG. 41A to FIG. 41C Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. FIG. 41A to FIG. 41C The method of forming source / drain contacts 130 on opposite ends of the two-dimensional material layer 110 is shown. It can be understood that FIG. 41A to FIG. 41C The method described in is suitable for forming Figures 1A to 5 , Figures 6 to 8 , Figures 9 to 12 , Figures 13 to 17 The source / drain contacts 130 and FIG. 18A to FIG. 22 Source / drain contacts 230 are provided.

[0176] Fig.41A Similar to Fig.40A , where chemically adsorbed species such as H 2 , free radical H atom, BCl 3 or CF 4is supplied to the two-dimensional material layer 110 to weaken (or destroy) the bond between the chalcogenide atoms CA (non-metal atoms) and the metal atoms MA, thereby forming diffusive sulfides.

[0177] Fig.41B Similar to Fig.40B , a deposition process is performed to form the source / drain contacts 130. As described above, part of the chalcogen atoms CA of the two-dimensional material layer 110 reacts with the halogen to form diffusible sulfides, and the metal deposition process can drive away the diffusible non-metal atoms of the two-dimensional material layer 110. Therefore, the contact metal atoms CMA of the source / drain contacts 130 can form metal bonds with the metal atoms MA of the two-dimensional material layer 110.

[0178] exist Fig.41C In the embodiment, an annealing process is performed to accelerate the removal of non-metal atoms (i.e., chalcogen atoms CA) of the two-dimensional material layer 110. Therefore, there are no chalcogen atoms CA of the two-dimensional material layer 110 between the metal atoms MA of the two-dimensional material layer 110 and the contact metal atoms CMA of the source / drain contact 130. In some embodiments, the annealing process may include thermal annealing, microwave annealing, laser annealing, or rapid thermal annealing. In some embodiments, the annealing process may be performed to accelerate the removal of non-metal atoms (i.e., chalcogen atoms CA) of the two-dimensional material layer 110. Therefore, there are no chalcogen atoms CA of the two-dimensional material layer 110 between the metal atoms MA of the two-dimensional material layer 110 and the contact metal atoms CMA of the source / drain contact 130. Fig.41B The annealing process is performed during or after the deposition process. In some embodiments, the temperature of the annealing process is in a range of about 150° C. to about 450° C.

[0179] FIG. 42A to FIG. 42B Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. FIG. 42A to FIG. 42B The method of forming source / drain contacts 130 on opposite ends of the two-dimensional material layer 110 is shown. It can be understood that FIG. 42A to FIG. 42B The method described in is suitable for forming Figures 1A to 5 , Figures 6 to 8 , Figures 9 to 12 , Figures 13 to 17 The source / drain contacts 130 and FIG. 18A to FIG. 22 Source / drain contacts 230 are provided.

[0180] exist Fig.42A In the process, the metal precursor MP of the source / drain contact 130, such as WF 6 , HfCl 4 and InCl 3Provided to the two-dimensional material layer 110, the metal precursor MP undergoes a redox reaction with the two-dimensional material layer 110. In more detail, the bond between the chalcogen atom CA and the metal atom MA can be weakened (or destroyed), and the non-metal atom (i.e., the chalcogen atom CA) of the two-dimensional material layer 110 can react with the atom HA (i.e., Cl, F, etc.) of the metal precursor, and the reacted non-metal atom of the two-dimensional material layer 110 is replaced by the metal atom CMA of the precursor (i.e., W, Hf, In, etc.), and the metal atom CMA of the precursor forms a metal bond with the metal atom MA of the two-dimensional material layer 110. The metal atom CMA of the precursor forms the source / drain contact 130, and the metal atom CMA of the precursor can also be referred to as the contact metal atom CMA of the source / drain contact 130.

[0181] exist Fig.42B In the process, a metal precursor is provided until there are no chalcogenide atoms CA of the two-dimensional material layer 110 between the metal atoms MA of the two-dimensional material layer 110 and the contact metal atoms CMA of the source / drain contacts 130 .

[0182] FIG. 43A to FIG. 43B Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. FIG. 43A to FIG. 43B The method of forming source / drain contacts 130 on opposite ends of the two-dimensional material layer 110 is shown. It can be understood that FIG. 43A to FIG. 43B The method described in is suitable for forming Figures 1A to 5 , Figures 6 to 8 , Figures 9 to 12 , Figures 13 to 17 The source / drain contacts 130 and FIG. 18A to FIG. 22 Source / drain contacts 230 are provided.

[0183] exist Fig.43A In some embodiments, the source / drain contact 130 includes a metal alloy including at least two different metal elements. For example, the source / drain contact 130 may include a low melting point metal element and a high melting point metal element. In some embodiments, the low melting point metal element has a melting point lower than about 650°C and may include Bi, In, Sn, Sb, etc. The high melting point metal element has a melting point higher than about 650°C and may include Al, Pt, Ti, W, Mo, etc. In some embodiments, after forming the source / drain contact 130, a portion of the chalcogen atoms CA of the two-dimensional material layer 110 may be located between the metal atoms MA of the two-dimensional material layer 110 and the contact metal atoms CMA of the source / drain contact 130. In some embodiments, the low melting point material is easy to react with the chalcogen atoms CA of the two-dimensional material layer 110, and the high melting point material is used to improve the thermal stability of the source / drain contact 130.

[0184] exist Fig.43B In the embodiment, an annealing process is performed to remove a portion of the non-metal atoms (i.e., chalcogenide atoms CA) of the two-dimensional material layer 110 between the metal atoms MA of the two-dimensional material layer 110 and the contact metal atoms CMA of the source / drain contacts 130. For example, the annealing process can weaken (or destroy) the covalent bonds between the chalcogenide atoms CA and the metal atoms MA of the two-dimensional material layer 110 to form a diffusive chalcogenide. The chalcogenide atoms CA are diffused and driven away via the annealing process, so that the contact metal atoms CMA of the source / drain contacts 130 can form a metallic bond with the metal atoms MA of the two-dimensional material layer 110. In some embodiments, there is no chalcogenide atom CA of the two-dimensional material layer 110 between the metal atoms MA of the two-dimensional material layer 110 and the contact metal atoms CMA of the source / drain contacts 130. In some embodiments, the annealing process can include thermal annealing, microwave annealing, laser annealing, or rapid thermal annealing. In some embodiments, the annealing process can be performed at a temperature of 1000 ℃ and a temperature of 1000 ℃. Fig.43A The annealing process is performed during or after the deposition process of the source / drain contact 130. In some embodiments, the temperature of the annealing process is in the range of about 150° C. to about 450° C. In some embodiments, the contact metal atoms CMA of the source / drain contact 130 may be the same as the metal atoms MA of the two-dimensional material layer 110, or may be different from the metal atoms MA of the two-dimensional material layer 110.

[0185] FIG. 44A to FIG. 44C The following are different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure. It should be noted that: FIG. 44A to FIG. 44C Some elements described are similar to those described above, these elements are labeled with the same reference numerals, and the relevant details will not be repeated for the sake of brevity.

[0186] exist Fig.44A In FIG. 1 , a two-dimensional material layer 110 is shown. In some embodiments, although Fig.44A Not shown in FIG. 1 is a gate structure (ie, Figure 5 The gate structure 150) may contact the two-dimensional material layer 110. Fig.44B In the method, source / drain contacts 130 are formed on opposite ends of the two-dimensional material layer 110. In more detail, the method includes replacing non-metal atoms, such as chalcogenide or nitrogen, with metal atoms so that the metal atoms directly bond with the metal atoms of the two-dimensional material layer 110 and serve as the source / drain contacts 130 of the transistor.

[0187] exist Fig.44CIn the embodiment, metal 135 is formed over source / drain contacts 130, respectively. In some embodiments, metal 135 may be formed using electroplating, and thus metal 135 may be selectively formed on the metal surface of source / drain contacts 130. In some embodiments, metal 135 may include Pt, Au, Ag, Cu, Ni, Al, W, or other suitable contact metals.

[0188] FIG. 45A to FIG. 45B Different stages of a method for forming a semiconductor device according to some embodiments of the present disclosure.

[0189] exist Fig.45A , a gate all around (GAA) component is shown. The GAA component includes a substrate 200. The substrate 200 may be similar to the substrate 100 described above. A two-dimensional material layer 110 is formed over the substrate 200, and a gate structure 240 is formed to surround the two-dimensional material layer 110. The two-dimensional material layer 110 may also be referred to as a two-dimensional material channel layer. Spacers 215 are formed on opposite sides of the gate structure 240. Source / drain contacts 130 are formed on opposite ends of the two-dimensional material layer 110. The source / drain contacts 130 may be formed using FIG. 39A to FIG. 39C , FIG. 40A to FIG. 40C , FIG. 41A to FIG. 41C , FIG. 42A to FIG. 42B and FIG. 43A to FIG. 43B The method described in .

[0190] In some embodiments, the gate structure 240 may include a gate dielectric layer and a gate electrode located above the gate dielectric layer. The gate dielectric layer may include a high-k dielectric. Examples of high-k dielectric materials include HfO 2 、HfSiO、HfSiON、HfTaO、HfTiO、HfZrO、zirconia、alumina、titanium oxide、hafnium dioxide-alumina (HfO 2 -Al 2 O 3 ) alloys, other suitable high-k dielectric materials, and / or combinations thereof. The gate electrode may include a work function metal layer and a fill metal. The work function metal layer may be an n-type or p-type work function layer. Exemplary p-type work function metals include TiN, TaN, Ru, Mo, Al, WN, ZrSi 2 、MoSi 2 、TaSi 2 、NiSi 2, WN, other suitable p-type work function materials or combinations thereof. Exemplary n-type work function metals include Ti, Ag, TaAl, TaAlC, TiAlN, TaC, TaCN, TaSiN, Mn, Zr, other suitable n-type work function materials or combinations thereof. The work function layer may include multiple layers. The fill metal may include tungsten (W), aluminum (Al), copper (Cu) or other suitable conductive materials. The spacer 215 may be formed of silicon oxide, silicon nitride, silicon oxynitride, or combinations thereof.

[0191] exist Fig.45B In the embodiment, metal 135 is formed over source / drain contacts 130, respectively. In some embodiments, metal 135 may be formed using electroplating, and thus metal 135 may be selectively formed on the metal surface of source / drain contacts 130. In some embodiments, metal 135 may include Pt, Au, Ag, Cu, Ni, Al, W, or other suitable contact metals.

[0192] Fig.46 Semiconductor devices of some embodiments of the present disclosure. A complementary field effect transistor (CFET) device is shown, which includes a first transistor TR1 and a second transistor TR2 vertically stacked above the first transistor TR1. The CFET device includes a substrate 300. The substrate 300 can be similar to the substrate 100 described above. A two-dimensional material layer 110A is formed above the substrate 300, and a two-dimensional material layer 110B is formed above the two-dimensional material layer 110A and is vertically separated from the two-dimensional material layer 110A. A gate structure 340 is formed surrounding the two-dimensional material layers 110A and 110B. The two-dimensional material layers 110A and 110B can also be referred to as two-dimensional material channel layers. Spacers 315 are formed on opposite sides of the gate structure 340. Source / drain contacts 130A are formed on opposite ends of the two-dimensional material layer 110A, and source / drain contacts 130B are formed on opposite ends of the two-dimensional material layer 110A. The source / drain contacts 130A and 130B can be used FIG. 39A to FIG. 39C , FIG. 40A to FIG. 40C , FIG. 41A to FIG. 41C , FIG. 42A to FIG. 42B and FIG. 43A to FIG. 43B The method described in .

[0193] The gate structure 340, the two-dimensional material layer 110A and the source / drain contact 130A may collectively serve as a first transistor TR1. The gate structure 340, the two-dimensional material layer 110B and the source / drain contact 130B may collectively serve as a second transistor TR2. In some embodiments, the first transistor TR1 is a P-type element, and the second transistor TR2 is an N-type element.

[0194] In some embodiments, the gate structure 340 may include a gate dielectric layer 340A and a gate electrode 340B on the gate dielectric layer 340A. The materials of the gate dielectric layer 340A and the gate electrode 340B are formed on the upper Fig.45A and Fig.45B The relevant details will not be repeated.

[0195] Metal 135 is formed over source / drain contacts 130A and 130B, respectively. Metal 135 may include metal 135A in contact with a first of source / drain contacts 130A, metal 135B in contact with a first of source / drain contacts 130B, wherein metal 135A is vertically spaced apart from metal 135B. Metal 135 also includes metal 135C in contact with a second of source / drain contacts 130A and a second of source / drain contacts 130B. In some embodiments, metal 135A may be used as a power supply terminal Vdd of a CFET element, metal 135B may be used as a power supply terminal Vss of a CFET element, and metal 135c may be used as an output terminal Vout of a CFET element.

[0196] According to the aforementioned embodiments, it can be seen that the present disclosure provides advantages for manufacturing integrated circuits. However, it should be understood that other embodiments can provide additional advantages, and not all advantages must be disclosed herein, and not all embodiments require specific advantages. One advantage is to remove chalcogen atoms from the source / drain region of the TMD channel layer before forming the source / drain contact, so that the metal atoms of the source / drain contact can form metal bonds with the transition metal atoms of the TMD channel layer, which will increase the contact area between the source / drain contact and the source / drain region of the TMD channel layer, thereby increasing the current of the transistor. Another advantage is that when more chalcogen atoms are removed from the side of the TMD channel layer, the contact area between the source / drain contact and the source / drain region of the TMD channel layer will increase, which can reduce the current of the transistor. Another advantage is that when the work function value of the metal atoms of the source / drain contact is greater than the work function value of the transition metal atoms of the TMD channel layer, the current of the transistor can be increased. Another advantage is that when the metal atoms of the source / drain contact are the same as the transition metal atoms of the TMD channel layer, the current of the transistor can be increased. Another advantage is that when the source / drain contacts are a multi-metal structure, the current of the transistor can be increased.

[0197] According to some embodiments of the present disclosure, a method includes forming a two-dimensional material layer on a substrate, wherein the two-dimensional material layer includes transition metal atoms and chalcogenide atoms; forming a gate structure above the two-dimensional material layer; providing chemical molecules to the two-dimensional material layer so that the atoms of the chemical molecules partially react with some chalcogenide atoms to weaken the covalent bonds between some chalcogenide atoms and the transition metal atoms; and forming a source / drain contact above the two-dimensional material layer, wherein the contact metal atoms of the source / drain contact form metal bonds with the transition metal atoms of the two-dimensional material layer.

[0198] In some embodiments, the method further includes performing an ion bombardment on a portion of the chalcogen atoms before forming the source / drain contacts.

[0199] In some embodiments, forming the source / drain contacts includes performing a metal deposition process, wherein the metal deposition process drives off portions of the chalcogen atoms.

[0200] In some embodiments, the metal deposition process is performed until a portion of the chalcogen atoms in the two-dimensional material layer is completely removed from the two-dimensional material layer.

[0201] In some embodiments, an annealing process is further performed to partially diffuse and drive away the chalcogen atoms.

[0202] In some embodiments, the annealing process is performed after the metal deposition process.

[0203] In some embodiments, the chemical molecule comprises BCl 3 or CF 4 .

[0204] In some embodiments, the chemical molecule comprises WF 6 , HfCl 4 or InCl 3 , wherein the chemical molecule and the portion of the chalcogen atom undergo a redox reaction to weaken the covalent bond between the portion of the chalcogen atom and the transition metal atom.

[0205] In some embodiments, metal atoms in the chemical molecule and transition metal atoms in the two-dimensional material layer form metal bonds to form source / drain contacts.

[0206] According to some embodiments of the present disclosure, a method includes forming a two-dimensional material layer on a substrate, wherein the two-dimensional material layer includes transition metal atoms and chalcogen atoms; forming a gate structure above the two-dimensional material layer; removing a portion of the chalcogen atoms from the two-dimensional material layer to expose a portion of the transition metal atoms of the two-dimensional material layer; and forming a source / drain contact above the two-dimensional material layer, wherein the contact metal atoms of the source / drain contact and the portion of the transition metal atoms of the two-dimensional material layer form a metallic bond.

[0207] In some embodiments, removing the chalcogen atoms from the two-dimensional material layer includes performing an annealing process.

[0208] In some embodiments, the annealing process is performed after forming source / drain contacts.

[0209] In some embodiments, before removing the portion of the chalcogenide atoms from the two-dimensional material layer, the portion of the chalcogenide atoms is located between the contact metal atoms of the source / drain contacts and the transition metal atoms of the two-dimensional material layer.

[0210] In some embodiments, each of the source / drain contacts is a metal alloy including a first metal element and a second metal element different from the first metal element.

[0211] In some embodiments, removing the portion of chalcogen atoms from the two-dimensional material layer includes providing a metal precursor for source / drain contacts, wherein the metal precursor and the portion of chalcogen atoms undergo a redox reaction to weaken the covalent bond between the portion of chalcogen atoms and the transition metal atom.

[0212] In some embodiments, removing the chalcogen atoms from the two-dimensional material layer comprises providing a 3 or CF 4 chemical molecules.

[0213] According to some embodiments of the present disclosure, a device includes a substrate; and a first transistor located above the substrate. The first transistor includes a first two-dimensional material channel layer, a first gate structure, and a first source / drain contact. The first two-dimensional material channel layer is made of transition metal dichalcogenide. The first gate structure surrounds the first two-dimensional material channel layer. The first source / drain contact contacts and is located at opposite ends of the first two-dimensional material channel layer, wherein there is no chalcogen atom between the metal atoms of the first source / drain contact and the transition metal atoms of the first two-dimensional material channel layer.

[0214] In some embodiments, a second transistor is further included above the first transistor. The second transistor includes a second two-dimensional material channel layer, a second gate structure, and a second source / drain contact. The second two-dimensional material channel layer is made of transition metal dichalcogenide. The second gate structure surrounds the second two-dimensional material channel layer. The second source / drain contact contacts and is located at opposite ends of the second two-dimensional material channel layer, wherein there is no chalcogen atom between the metal atom of the second source / drain contact and the transition metal atom of the second two-dimensional material channel layer.

[0215] In some embodiments, the metal atoms of the first source / drain contacts include a metal element different from the transition metal atoms of the first two-dimensional material channel layer.

[0216] In some embodiments, the metal atoms of the first source / drain contacts include a metal element that is the same as the transition metal atoms of the first two-dimensional material channel layer.

[0217] The foregoing summarizes the features of several embodiments so that those skilled in the art may better understand the aspects of the present disclosure. Those skilled in the art will appreciate that they may readily use the present disclosure as a basis for designing or modifying other processing procedures and structures for carrying out the same purposes and / or achieving the same advantages of the embodiments described herein. Those skilled in the art will also appreciate that such equivalent constructions do not depart from the spirit and scope of the present disclosure, and that they may be variously modified, substituted, and altered without departing from the spirit and scope of the present disclosure.

Claims

1. A method for forming a semiconductor element, characterized in that: Include: forming a two-dimensional material layer on a substrate, wherein the two-dimensional material layer comprises a plurality of transition metal atoms and a plurality of chalcogen atoms; forming a gate structure above the two-dimensional material layer; providing a plurality of chemical molecules to the two-dimensional material layer so that a plurality of atoms of the plurality of chemical molecules react with a plurality of portions of the plurality of chalcogen atoms to weaken covalent bonds between the plurality of portions of the plurality of chalcogen atoms and the plurality of transition metal atoms; as well as A plurality of source / drain contacts are formed above the two-dimensional material layer, wherein a plurality of contact metal atoms of the plurality of source / drain contacts and the plurality of transition metal atoms of the two-dimensional material layer form metal bonds.

2. The method according to claim 1, characterized in that The method further includes performing an ion bombardment on the plurality of portions of the plurality of chalcogen atoms before forming the plurality of source / drain contacts.

3. The method according to claim 1, characterized in that Wherein forming the plurality of source / drain contacts comprises performing a metal deposition process, wherein the metal deposition process drives away the plurality of portions of the plurality of chalcogen atoms from the two-dimensional material layer.

4. The method according to claim 1, characterized in that Wherein the plurality of chemical molecules comprises BCl3 or CF4.

5. The method according to claim 1, characterized in that The plurality of chemical molecules include WF6, HfCl4 or InCl3, wherein the plurality of chemical molecules and the plurality of portions of the plurality of chalcogen atoms undergo a redox reaction to weaken covalent bonds between the plurality of portions of the plurality of chalcogen atoms and the plurality of transition metal atoms.

6. A method for forming a semiconductor element, characterized in that: Include: forming a two-dimensional material layer on a substrate, wherein the two-dimensional material layer comprises a plurality of transition metal atoms and a plurality of chalcogen atoms; forming a gate structure above the two-dimensional material layer; removing portions of the plurality of chalcogen atoms from the two-dimensional material layer to expose portions of the plurality of transition metal atoms in the two-dimensional material layer; as well as A plurality of source / drain contacts are formed over the two-dimensional material layer, wherein a plurality of contact metal atoms of the plurality of source / drain contacts and the plurality of portions of the plurality of transition metal atoms of the two-dimensional material layer form metallic bonds.

7. The method according to claim 6, characterized in that Wherein removing the portions of the chalcogen atoms from the two-dimensional material layer comprises performing an annealing process.

8. The method according to claim 6, characterized in that Wherein removing the multiple portions of the multiple chalcogen atoms from the two-dimensional material layer includes providing a metal precursor for the multiple source / drain contacts, wherein the metal precursor and the multiple portions of the multiple chalcogen atoms undergo a redox reaction to weaken the covalent bonds between the multiple portions of the multiple chalcogen atoms and the multiple transition metal atoms.

9. A semiconductor element, characterized in that: Include: a substrate; and A first transistor, located above the substrate, comprises: a first two-dimensional material channel layer, wherein the first two-dimensional material channel layer is made of transition metal dichalcogenide; A first gate structure surrounds the first two-dimensional material channel layer; and A plurality of first source / drain contacts are in contact with and located at opposite ends of the first two-dimensional material channel layer, wherein there are no chalcogen atoms between the plurality of metal atoms of the plurality of first source / drain contacts and the plurality of transition metal atoms of the first two-dimensional material channel layer.