Composition for optical metrology applications

By using a combination of adamantane and hydrocarbon solvents with a specific boiling point range, a thin, uniform, volatile coating is formed, which solves the problem in the prior art that it is difficult to achieve high-quality scanning on a variety of surfaces in optical measurement. This enables high-precision and high-resolution optical measurement, and the coating disappears automatically after measurement without affecting the surface quality.

CN118813082BActive Publication Date: 2026-11-24F2MB ENG UG
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410811663.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-11-02
Filing Date
2019-11-04
Publication Date
2026-11-24
Estimated Expiration
2039-11-04

AI Technical Summary

Technical Problem

Existing optical measurement technologies, especially 3D scanning technology, struggle to achieve high-quality and high-precision measurements on transparent, translucent, absorptive, reflective, or smooth surfaces. Furthermore, existing anti-reflective coating methods suffer from problems such as contamination, health risks, difficulty in removal, interaction with oil lubricants, and uneven coating thickness, all of which affect measurement accuracy and reusability.

Method used

A composition containing adamantane and hydrocarbon solvents or hydrocarbon mixtures with specific boiling point ranges is used as a volatile coating material. A thin, uniform coating is formed by spraying. The coating evaporates or sublimates naturally after measurement without the need for removal. It is suitable for various environmental conditions and supports high-quality and high-resolution scanning.

Benefits of technology

It provides the ability to form a uniform thin coating on a variety of surfaces, suitable for optical and photogrammetric methods. The coating disappears automatically after measurement without affecting surface quality. It supports high-precision and high-resolution scanning, is suitable for various environmental conditions, and requires no additional cleaning steps.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
  • Figure HDA0004906329310000011
    Figure HDA0004906329310000011
Patent Text Reader

Abstract

This invention relates to novel compositions particularly suitable for optical measurement technology applications (especially 3D scanning technology), as well as methods for manufacturing and using said compositions.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Divisional application This application is a divisional application of application number 201980087549.X, filed on November 4, 2019, entitled "Composition for optical measurement technology applications". Technical Field

[0002] This invention relates to novel compositions particularly suitable for optical measurement technology applications (especially 3D scanning technology), as well as methods for manufacturing and using said compositions. Background Technology

[0003] The quality of optical measurements largely depends on the optical properties of the object's surface. Typically, diffuse light reflection is required at the outer boundary surfaces of the object. When the surface of the object is partially or completely transparent, translucent, absorptive, reflective, smooth, or black, most currently available measurement devices struggle to achieve sufficiently high quality and accuracy for measurement / scanning. Attempts to compensate for these deficiencies by adapting the light source, sensor, and optical image to the object's characteristics, for example, have proven ineffective or insufficient in providing optimal imaging of the desired quality. Furthermore, measurement and positioning strategies to avoid erroneous measurements or reduce artifacts not only require specialized knowledge but are often time-consuming and technically demanding.

[0004] To prepare surfaces for optical 3D scanning measurements that are otherwise impossible or difficult to measure accurately, one method known in the art is to apply an anti-reflective coating to the surface to be measured, thereby making the surface opaque or matte. To obtain an optimal surface for scanning and thus achieve minimal measurement error during the scanning process, it is important to apply a coating of minimal but uniform thickness.

[0005] One such method involves applying a pigment-containing reagent (especially a whitening agent based on inorganic pigments such as titanium dioxide, chalk, or barium sulfate) to the surface to be measured / scanned. Such coatings are durable on the surface to which they are applied. However, this method of preparing a matte, opaque surface is only suitable when there are no limitations in the purity or cleanliness of the object to be coated / measured or the area or space within which the coating / measurement will take place, as the released pigments can contaminate the system, equipment (including the 3D scanning equipment itself), and the areas and laboratories where it is used. Furthermore, recent studies have confirmed that released pigment particles (such as TiO2) pose a potential health risk, as airborne particles are easily inhaled and can lodge in lung tissue, potentially causing serious health problems, including lung cancer.

[0006] Another problem with using this type of pigment-based coating is that the deposited anti-reflective layer must be removed again after measurement to restore the measured / scanned object to its original state. This poses particular problems when the measured object is valuable and / or when a simple post-measurement treatment is undesirable. Ensuring complete removal of the coating from a large, extended surface is complex and not always satisfactory, as residual coating material often remains on the surface. For sensitive and / or fragile objects (such as structural components from precision engineering fields, especially those exhibiting microcavities or open structures), applying this type of pigment-based coating inevitably leads to irreversible contamination or abrasion on the surface when attempting to remove the coating. Traditional methods for removing pigment-based coatings from scanned objects also include the use of chemical cleaners, which are generally undesirable or even incompatible with the coated object. Therefore, even when successful, these cleaning methods are often extremely cumbersome and time-consuming, making them technically or economically unattractive.

[0007] Objects subjected to 3D scanning are often components of other products, including mechanical products. Thus, the objects to be scanned are typically protected from environmental influences by the presence of coatings such as oil or lubricants, thereby inhibiting corrosion. When using pigment-based reagents, it is often impossible to apply a suitable anti-reflective coating to such objects because the pigments interact with the oil or lubricant on the object's surface, resulting in an uneven surface or even pigment / oil clumps. The disadvantages are not only the inability to form a coating suitable for scanning the object, but also the removal of the protective oil / lubricant layer, exposing the object to the environment, which is detrimental. For the manufacturer of the object, the cleaning and reapplication of the protective oil / lubricant layer by the party performing the 3D scanning operation to minimize the object's exposure time to the environment is also undesirable, especially in cases where the object is valuable or fragile.

[0008] Another drawback typically associated with using such pigment-based coatings is the potential for a relatively thick, high-grained coating. Consequently, this characteristic can introduce significant errors, distortions, and irregularities in measurements using optical microscopy and scanning techniques. Therefore, to provide optimal, high-precision measurement results, it is preferable to apply a thinner, low-grained anti-reflective coating to the surface to be measured.

[0009] To perform 3D scanning measurements, a series of adhesive dots or spots must typically be applied to the surface of the object to be scanned. These dots or spots serve as reference points for the scanner, helping it to accurately replicate the surface being measured. If the number of reference points or spots used is insufficient, additional reference points or spots must be applied to the surface to provide enough reference points for the scanner to achieve a high-quality scan. Another drawback of pigment-based sprays in this regard is that the surface is usually sprayed after the application of reference points or spots. If it is later determined that the number of applied reference points is insufficient to obtain the desired scan quality, additional reference points or spots must be applied on top of the pigment coating. This is problematic because the sprayed object needs to be handled, and during handling, the pigment can easily be removed from the surface upon contact. In fact, it is easy to remove / smear / dirty (damage) such pigment coatings from / on the surface to be scanned, which is undesirable. Even slight contact can cause more widespread problems because the object to be scanned must often be rotated or manipulated by hand to enable a full scan of the surface. Therefore, providing a product capable of forming a coating on a surface to be scanned that is sufficiently robust to withstand touch and handling without negatively impacting the quality of the scannable surface (or at least not to the point where a sufficiently high-quality scan can no longer be achieved; also known as "damage resistance") would bring significant benefits to the field. Furthermore, providing a product that exhibits the flexibility to allow the application, removal, and possible subsequent reapplication of adhesive dots or spots required by the scanner after the coating has been formed on the object to be scanned, without substantially adversely affecting the adhesion of the coated surface or the adhesive dots or spots (thus enabling its reuse), would also constitute an advantage over known prior art solutions.

[0010] Methods have been found in the art that primarily overcome the drawbacks of post-measurement coating removal associated with such pigment-based coating methods. Ideally, the antireflective coating is pigment-free, thin, low-grained, exhibits uniform diffuse reflection in all directions, and provides the scanned object in its original uncoated state after measurement without requiring the user to remove the coating by means such as cleaning or wiping the surface.

[0011] Therefore, coating materials that are volatile at room temperature or slightly above room temperature were studied. Due to their volatility, these reagents evaporate or sublimate from the coated surface in a relatively short time, leaving no residue on the surface and eliminating the need for active removal of the coating through cleaning, wiping, or washing.

[0012] One method known in the art for forming such a coating originates from the fields of archaeology and restoration and involves applying cyclododecane (e.g., this product is available under the trade name "Cyclodecan Spray" from Deffner & Johann GmbH, Germany) to the surface to be scanned by first providing a cyclododecane (commonly abbreviated as CCD or CDD) solution in a pressurized (resulting in liquefaction) propellant gas in a spray can, and then spraying the solution onto the surface to be measured. While this method overcomes some of the disadvantages associated with pigment-based sprays by forming a sublimable coating, a drawback is the significant formation of CCD crystals during application, resulting in a coarse, highly granular coating exhibiting irregular layer thickness and needle-like crystals. Such coatings are unsuitable for accurate, high-resolution optical scanning because they lead to uncorrectable measurement errors. These sprays also contain a high concentration of CCD, which can be disadvantageous from a cost perspective. Furthermore, coatings formed by such CCD sprays are easily wiped off or soiled (damaged) during handling, and the adhesion of the reference points or spots required for reliable, high-quality scanning to this coating is very poor. Removing adhesive dots or spots from a CCD-coated surface typically negatively impacts the coating quality, and these dots or spots are usually not reusable. Another drawback of CCD-based antireflective products is that they often have an odor or fragrance that the end user may find unpleasant.

[0013] In view of the foregoing, the object of the present invention is to provide a product for optical measurement technology applications (especially 3D scanning) that overcomes any (preferably more than one) of the aforementioned disadvantages associated with prior art solutions in order to provide a (anti-reflective) surface suitable for optical measurement. Particularly advantageous is the provision of a product capable of forming a coating on objects on which high-quality 3D scanning is otherwise not achievable, particularly a product capable of producing a thin, uniform coating on such objects, thereby enabling accurate, high-quality, and / or high-resolution 3D scanning of said objects. Ideally, the product should be able to restore the scanned object to an uncoated state after measurement without actively removing or cleaning the coating, and it would be advantageous if the residence time of the coating on the object to be scanned could be adjusted to suit the specific application, preferably while continuing to achieve the other desired characteristics and effects outlined herein. In this regard, the ability to extend the residence time without having to compromise between optimal coating thinness and surface uniformity would bring significant benefits to the field. Furthermore, the product's ability to form a coating that is resistant to damage / degradation during processing, and whose reference points and spots required by scanning equipment can be repeatedly applied and removed without adversely affecting surface quality or the adhesion of the reference points, is a significant advantage. From the end-user's perspective, products with a neutral or pleasant odor are also advantageous.

[0014] To ensure the broadest possible applicability, it is desirable that this product can be used directly (or in the most convenient and effortless manner) by the end user in all possible / needed situations, without the need for any specially designed devices or equipment, thus particularly allowing the coating to be applied in the field (“in situ”) rather than just in a specially constructed or equipped laboratory or area. For this purpose, it would be even more advantageous if the coating formed by said product could withstand normal and even extreme weather conditions (e.g., direct contact with water, strong winds, ultraviolet radiation, and other conditions associated with outdoor work).

[0015] A product is provided that can form a coating having one or more of the aforementioned characteristics on an object to be scanned, the surface of which has been treated with a protective coating such as oil. This coating evaporates or sublimates after measurement to provide the original object including a complete protective coating. This is particularly advantageous for 3D scanning of components that require continuous protection from environmental impacts by an oil or lubricant coating, especially those that are unsuitable for reapplying a protective oil or lubricant layer after scanning due to their fragility or high value.

[0016] Similar to its use in providing surfaces for 3D scanning measurements, the compositions of the present invention can also be used to provide surfaces for measurement using other optical measurement techniques, such as photogrammetry. Photogrammetry, an optical measurement technique, utilizes photographic images captured by a camera (e.g., a smartphone camera) to obtain reliable data from an object that is the subject of the photograph, particularly related to the surface structure and morphology of the object. For example, surveyors, architects, and engineers often use photogrammetry to create object-based morphological maps, grids, cloud points, or graphics. Photogrammetry can provide an alternative measurement technique to 3D scanning to provide 3D maps, graphics, or models of objects or surfaces. In some cases, photogrammetry may be more suitable than 3D scanning because it is often more economical and easier to use, as the required measuring equipment is simply a camera. Photogrammetry may also be superior to 3D scanning and therefore more suitable than 3D scanning when measuring larger objects such as buildings (or parts of buildings), which typically require 3D scanners for those specific applications.

[0017] In the case of optical measurement of a surface using photogrammetry, problems also exist regarding the optical properties of the object surface to be measured, especially in the case of 3D scanning. Therefore, another object of the present invention is to provide a product that overcomes any, and preferably more than one, of the disadvantages associated with the prior art, to provide a (anti-reflective) surface suitable for optical measurement (and as discussed above in the case of 3D scanning), wherein the optical measurement is performed using photogrammetry. Summary of the Invention

[0018] In view of the foregoing, the present invention relates to the following items: project 1a. A composition comprising: (i) adamantane; and (ii) a first solvent, wherein the first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point of 25°C or higher at atmospheric pressure, the boiling point range having a minimum boiling point of 25°C or higher at atmospheric pressure; and optionally... (iii) Cyclododecane; and / or optionally (iv) A second solvent, which is different from the first solvent.

[0019] 1b. A composition comprising: (i) adamantane; and (ii) A first solvent, wherein the first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point of 25°C or above at atmospheric pressure, the boiling point range having a minimum boiling point of 25°C or above at atmospheric pressure; (iii) Optionally includes cyclododecane; Also includes: (iv) a second solvent, which is different from the first solvent; and / or (v) Propellant.

[0020] 2. The composition according to any one of the preceding items, wherein the first solvent has a boiling point or boiling point range of 25°C or above, 30°C or above, 35°C or above, or 40°C or above to 50°C or below, 60°C or below, 65°C or below, 70°C or below, 75°C or below, 80°C or below, 90°C or below, 100°C or below, 110°C or below, 120°C or below, or 130°C or below at atmospheric pressure.

[0021] 3. The composition according to any one of the preceding items, wherein the first solvent has a boiling point or boiling point range of 25°C or above to 130°C or below at atmospheric pressure.

[0022] 4. The composition according to any one of the preceding items, wherein the first solvent has a boiling point or boiling point range of 30°C or above to 120°C or below at atmospheric pressure.

[0023] 5. The composition according to any one of the preceding items, wherein the first solvent has a boiling point or boiling point range of 30°C or above to 110°C or below at atmospheric pressure.

[0024] 6. The composition according to any one of the preceding items, wherein the first solvent has a boiling point or boiling point range of 30°C or above to 100°C or below at atmospheric pressure.

[0025] 7. The composition according to any one of the preceding items, wherein the first solvent has a boiling point or boiling point range of 45°C or above to 100°C or below at atmospheric pressure.

[0026] 8. The composition according to any one of the preceding items, wherein the first solvent has a boiling point or boiling point range of 50°C or above (especially 60°C or above) to 100°C or below (especially 95°C or below) at atmospheric pressure.

[0027] 9. The composition according to any one of items 1 to 6, wherein the first solvent has a boiling point or boiling point range of 30°C or above to 90°C or below at atmospheric pressure.

[0028] 10. The composition according to any one of items 1 to 6 or 9, wherein the first solvent has a boiling point or boiling point range of 30°C or above to 80°C or below at atmospheric pressure.

[0029] 11. The composition according to any one of items 1 to 6, 9 or 10, wherein the first solvent has a boiling point or boiling point range of 35°C or above to 75°C or below at atmospheric pressure.

[0030] 12. The composition according to any one of items 1 to 6, 9, 10 or 11, wherein the first solvent has a boiling point or boiling point range of 35°C or above to 70°C or below at atmospheric pressure.

[0031] 13. The composition according to any one of items 1 to 6, 9, 10, 11 or 12, wherein the first solvent has a boiling point or boiling point range of 35°C or above to 65°C or below at atmospheric pressure.

[0032] 14. The composition according to any one of items 1 to 6, 9, 10, 11, 12 or 13, wherein the first solvent has a boiling point or boiling point range of 40°C or above to 65°C or below at atmospheric pressure.

[0033] 15. The composition according to any one of items 1 to 6, 9, 10, 11, 12, 13 or 14, wherein the first solvent has a boiling point or boiling point range of 40°C or above to 60°C or below at atmospheric pressure.

[0034] 16. The composition according to any one of items 1 to 6, 9, 10, 11, 12, 13, 14 or 15, wherein the first solvent has a boiling point or boiling point range of 40°C or above to 50°C or below at atmospheric pressure.

[0035] 17. The composition according to any one of the preceding items, wherein the first solvent is selected from one or more aliphatic linear, branched, or cyclic C5-C... 10 The group consisting of hydrocarbons, wherein the hydrocarbons may be saturated or unsaturated.

[0036] 18. The composition according to any one of the preceding items, wherein the first solvent is selected from the group consisting of one or more aliphatic straight-chain, branched or cyclic C5-C8 hydrocarbons, wherein the hydrocarbons may be saturated or unsaturated.

[0037] 19. The composition according to any one of the preceding items, wherein the first solvent is selected from the group consisting of C5-hydrocarbons, C6-hydrocarbons, C7-hydrocarbons, C8-hydrocarbons, and any combination thereof.

[0038] 20. The composition according to any one of the preceding items, wherein the first solvent is selected from the group consisting of pentane, cyclopentane, hexane, cyclohexane, heptane, cycloheptane, octane, petroleum ether, petroleum ether 30-40, petroleum ether 40-60, petroleum ether 40-65, petroleum ether 60-80, petroleum ether 80-100, and any combination thereof.

[0039] 21. The composition according to any one of items 1 to 19, wherein the first solvent is selected from the group consisting of pentane, cyclopentane, hexane, cyclohexane, heptane, cycloheptane, octane, petroleum ether, petroleum ether 30-40, petroleum ether 40-60, petroleum ether 40-65, petroleum ether 60-80, petroleum ether 60-95, petroleum ether 80-100, and any combination thereof.

[0040] 22. The composition according to any one of the preceding items, wherein the first solvent is petroleum ether 40-65.

[0041] 23. The composition according to any one of items 1 to 19 or 21, wherein the first solvent is petroleum ether 60-95.

[0042] 24. The composition according to any one of items 1 to 21, wherein the first solvent is cyclopentane.

[0043] 25. The composition according to any one of items 1 to 21, wherein the first solvent is a mixture of petroleum ether 60-95 and cyclopentane.

[0044] 26. The composition according to any one of the preceding items, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 0.5 wt.% or more, 1.0 wt.% or more, 1.5 wt.% or more, 2.5 wt.% or more, 3 wt.% or more, 5 wt.% or more, or 6 wt.% or more to 10 wt.% or less, 11 wt.% or less, 12 wt.% or less, 15 wt.% or less, 20 wt.% or less, 30 wt.% or less, or 50 wt.% or less.

[0045] 27. The composition according to any one of the preceding items, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 0.5 wt.% or more to 50 wt.% or less based on the total weight of components (i) to (iv).

[0046] 28. The composition according to any one of the preceding items, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 1.0 wt.% or more to 30 wt.% or less based on the total weight of components (i) to (iv).

[0047] 29. The composition according to any one of the preceding items, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 1.5 wt.% or more to 20 wt.% or less based on the total weight of components (i) to (iv).

[0048] 30. The composition according to any one of the preceding items, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 2.5 wt.% or more to 15 wt.% or less based on the total weight of components (i) to (iv).

[0049] 31. The composition according to any one of the preceding items, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 3 wt.% or more to 12 wt.% or less based on the total weight of components (i) to (iv).

[0050] 32. The composition according to any one of the preceding items, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 5 wt.% or more to 11 wt.% or less based on the total weight of components (i) to (iv).

[0051] 33. The composition according to any one of the preceding items, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 6 wt.% or more to 10 wt.% or less based on the total weight of components (i) to (iv).

[0052] 34. The composition according to any one of the preceding items, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 10.0 wt.% or more, 12 wt.% or more, 13 wt.% or more, 15 wt.% or more, 20 wt.% or more, 25 wt.% or more, 30 wt.% or more, 35 wt.% or more, 40 wt.% or more, 45 wt.% or more, 50 wt.% or more, or 55 wt.% or more up to 90 wt.% or less, 85 wt.% or less, 80 wt.% or less, 75 wt.% or less, 70 wt.% or less, 65 wt.% or less, or 60 wt.% or less.

[0053] 35. The composition according to any one of items 1 to 30 or 34, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 10 wt.% or more to 15 wt.% or less based on the total weight of components (i) to (iv).

[0054] 36. The composition according to any one of items 1 to 30, 34 or 35, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 12 wt.% or more to 15 wt.% or less based on the total weight of components (i) to (iv).

[0055] 37. The composition according to any one of items 1 to 30, 34 or 36, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 13 wt.% or more to 15 wt.% or less based on the total weight of components (i) to (iv).

[0056] 38. The composition according to any one of items 1 to 25 or 34, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 10 wt.% or more to 55 wt.% or less based on the total weight of components (i) to (iv).

[0057] 39. The composition according to any one of items 1 to 34 or 38, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 10 wt.% or more to 50 wt.% or less based on the total weight of components (i) to (iv).

[0058] 40. The composition according to any one of items 1 to 25 or 34, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 20 wt.% or more to 90 wt.% or less based on the total weight of components (i) to (iv).

[0059] 41. The composition according to any one of items 1 to 25, 34 or 40, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 25 wt.% or more to 85 wt.% or less based on the total weight of components (i) to (iv).

[0060] 42. The composition according to any one of items 1 to 25, 34, 40 or 41, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 30 wt.% or more to 80 wt.% or less based on the total weight of components (i) to (iv).

[0061] 43. The composition according to any one of items 1 to 25, 34, or 40 to 42, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 30 wt.% or more to 75 wt.% or less based on the total weight of components (i) to (iv).

[0062] 44. The composition according to any one of items 1 to 25, 34, or 40 to 43, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 30 wt.% or more to 70 wt.% or less based on the total weight of components (i) to (iv).

[0063] 45. The composition according to any one of items 1 to 25, 34, or 40 to 44, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 30 wt.% or more to 65 wt.% or less based on the total weight of components (i) to (iv).

[0064] 46. ​​The composition according to any one of items 1 to 25, 34, or 40 to 45, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 35 wt.% or more to 60 wt.% or less based on the total weight of components (i) to (iv).

[0065] 47. The composition according to any one of items 1 to 25, 34, 38, or 40 to 46, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 35 wt.% or more to 55 wt.% or less based on the total weight of components (i) to (iv).

[0066] 48. The composition according to any one of items 1 to 25, 34, 38, or 40 to 47, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 40 wt.% or more to 55 wt.% or less based on the total weight of components (i) to (iv).

[0067] 49. The composition according to any one of items 1 to 27, 34, or 38 to 48, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 40 wt.% or more to 50 wt.% or less based on the total weight of components (i) to (iv).

[0068] 50. The composition according to any one of items 1 to 27, 34, or 38 to 49, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 45 wt.% or more to 50 wt.% or less based on the total weight of components (i) to (iv).

[0069] 50a. The composition according to any one of items 1 to 27, 34, or 38 to 45, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 30 wt.% or more to 50 wt.% or less based on the total weight of components (i) to (iv).

[0070] 50b. The composition according to any one of items 1 to 27, 34, 38 to 45 or 50a, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 30 wt.% or more to 40 wt.% or less based on the total weight of components (i) to (iv).

[0071] 50c. The composition according to any one of items 1 to 27, 34, 38 to 47 or 50a, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 35 wt.% or more to 50 wt.% or less based on the total weight of components (i) to (iv).

[0072] 50d. A composition according to any one of items 1 to 27, 34, 38 to 47, 50a or 50c, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 35 wt.% or more to 45 wt.% or less based on the total weight of components (i) to (iv).

[0073] 50e. A composition according to any one of items 1 to 27, 34, 38 to 47, 50a, 50c or 50d, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 35 wt.% or more to 40 wt.% or less based on the total weight of components (i) to (iv).

[0074] 51. The composition according to any one of the preceding items, wherein the composition does not contain any (iii) cyclododecane.

[0075] 52. The composition according to any one of the preceding items, wherein the composition does not include (iv) a second solvent.

[0076] 53. The composition according to any one of items 1 to 50 or 52, wherein the composition comprises (iii) cyclododecane.

[0077] 54. The composition according to any one of items 1 to 50, 52 or 53, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 9.0 wt.% or more to 11.0 wt.% or less, preferably 9.5 wt.% or more to 10.5 wt.% or less, based on the total weight of components (i) to (iv).

[0078] 55. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is 100:0, 95:5, 90:10, 80:20, 75:25, 2.7:1, 60:40 or 51:49 to 49:51, 40:60, 1:2.7, 25:75, 20:80, 10:90, 5:95 or 1:99.

[0079] 56. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 1:99.

[0080] 57. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 5:95.

[0081] 58. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 10:90.

[0082] 59. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 20:80.

[0083] 60. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 25:75.

[0084] 61. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 1:2.7.

[0085] 62. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 40:60.

[0086] 63. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 49:51.

[0087] 64. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is 95:5 to 5:95.

[0088] 65. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is 90:10 to 10:90.

[0089] 66. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is 80:20 to 20:80.

[0090] 67. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is 75:25 to 25:75.

[0091] 68. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is 2.7:1 to 1:2.7.

[0092] 69. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is 60:40 to 40:60.

[0093] 70. The composition according to any one of the preceding items, wherein the weight ratio of adamantane to cyclododecane is 51:49 to 49:51.

[0094] 71. The composition according to any one of items 1 to 69, wherein the weight ratio of adamantane to cyclododecane is 1.5:1 to 1:1.

[0095] 72. The composition according to any one of items 1 to 69 or 71, wherein the weight ratio of adamantane to cyclododecane is 1.5:1 to 1.25:1.

[0096] 73. The composition according to any one of items 1 to 69, 71 or 72, wherein the weight ratio of adamantane to cyclododecane is 1.4:1 to 1.3:1.

[0097] 74. The composition according to any one of the preceding items, wherein the composition comprises (iv) a second solvent, the second solvent being different from the first solvent, preferably wherein the second solvent is more polar than the first solvent.

[0098] 75. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 40°C or above, 50°C or above, 60°C or above, 64.7°C or above, 70°C or above, 75°C or above, 80°C or above, or 82°C or above to 90°C or below, 100°C or below, 110°C or below, 120°C or below, 130°C or below, 140°C or below, 150°C or below, or 160°C or below at atmospheric pressure.

[0099] 76. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 40°C or above to 160°C or below at atmospheric pressure.

[0100] 77. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 50°C or above to 150°C or below at atmospheric pressure.

[0101] 78. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 60°C or above to 140°C or below at atmospheric pressure.

[0102] 79. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 64.7 °C or above to 130 °C or below at atmospheric pressure.

[0103] 80. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 70°C or above to 120°C or below at atmospheric pressure.

[0104] 81. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 75 °C or above to 110 °C or below at atmospheric pressure.

[0105] 82. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 80°C or above to 100°C or below at atmospheric pressure.

[0106] 83. The composition according to any one of the preceding items, wherein the second solvent has a boiling point or boiling point range of 82°C or above to 90°C or below at atmospheric pressure.

[0107] 84. The composition according to any one of items 1 to 79, wherein the second solvent has a boiling point or boiling point range of 64.7°C or above to 100°C or below at atmospheric pressure.

[0108] 85. The composition according to any one of items 1 to 80 or 84, wherein the second solvent has a boiling point or boiling point range of 70°C or above to 90°C or below at atmospheric pressure.

[0109] 86. The composition according to any one of items 1 to 81, 84 or 85, wherein the second solvent has a boiling point or boiling point range of 75°C or above to 90°C or below at atmospheric pressure.

[0110] 87. The composition according to any one of items 1 to 81, 84, 85 or 86, wherein the second solvent has a boiling point or boiling point range of 75°C or above to 85°C or below at atmospheric pressure.

[0111] 88. The composition according to any one of the preceding items, wherein the second solvent is one or more alcohols, preferably wherein the second solvent is one or more alcohols selected from the group consisting of C1 to C8 alcohols (especially C1 to C8 monohydric alcohols).

[0112] 89. The composition according to any one of the preceding items, wherein the second solvent is one or more alcohols selected from the group consisting of C1 to C8 alkanols and C3 to C8 cycloalkanols, preferably, wherein the second solvent is one or more alcohols selected from methanol, ethanol, n-propanol, isopropanol, cyclopropanol, n-butanol, sec-butanol, isobutanol, tert-butanol, cyclobutanol, n-pentanol, 3-methylbut-1-ol, 2-methylbut-1-ol, 2,2-dimethylprop-1-ol, pent-3-ol, pent-2-ol, 3-methylbut-2-ol, 2-methylbut-2-ol The group consisting of alcohols including cyclopentanol, hexane-1-ol, hexane-2-ol, hexane-3-ol, 2-methylpentane-1-ol, 3-methylpentane-1-ol, 4-methylpentane-1-ol, 2-methylpentane-2-ol, 3-methylpentane-2-ol, 4-methylpentane-2-ol, 2-methylpentane-3-ol, 3-methylpentane-3-ol, 2,2-dimethylbutane-1-ol, 2,3-dimethylbutane-1-ol, 3,3-dimethylbutane-1-ol, 2,3-dimethylbutane-2-ol, 3,3-dimethylbutane-2-ol, 2-ethylbutane-1-ol, cyclohexanol, 2-heptanol, 3-heptanol, and 4-heptanol.

[0113] 90. The composition according to any one of the preceding items, wherein the second solvent is isopropanol.

[0114] 91. The composition according to any one of items 1 to 89, wherein the second solvent is ethanol.

[0115] 92. The composition according to any one of items 1 to 89, wherein the second solvent is a mixture of isopropanol and ethanol.

[0116] 93. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent to the second solvent (iv) is 99:1, 95:5, 90:10, 80:20, 70:30, 2:1, 60:40 or 55:45 to 45:55, 40:60, 1:2, 30:70, 20:80, 10:90, 5:95 or 1:99.

[0117] 94. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent to the second solvent (iv) is 99:1 to 1:99.

[0118] 95. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 95:5 to 5:95.

[0119] 96. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent to the second solvent (iv) is 90:10 to 10:90.

[0120] 97. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 80:20 to 20:80.

[0121] 98. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 3:1 to 1:3.

[0122] 99. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent to the second solvent (iv) is 70:30 to 30:70.

[0123] 100. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 2:1 to 1:2.

[0124] 101. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent (ii) to the second solvent (iv) is 60:40 to 40:60.

[0125] 102. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 45:55 to 55:45.

[0126] 102a. The composition according to any one of the preceding items, wherein the composition contains, by weight, a greater amount of the first solvent (ii) than the second solvent (iv).

[0127] 103. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 6:1 to 1:1.

[0128] 104. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent (ii) to the second solvent (iv) is 5:1 to 2:1.

[0129] 105. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 5:1 to 3:1.

[0130] 106. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 4:1.

[0131] 106a. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent (ii) to the second solvent (iv) is 3:1 to 1:1.

[0132] 107. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent (ii) to the second solvent (iv) is 3:1 to 2:1.

[0133] 108. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent (ii) to the second solvent (iv) is 1:1.

[0134] 109. The composition according to any one of the preceding items, wherein the weight ratio of the (ii) first solvent to the (iv) second solvent is 40:60 to 5:95.

[0135] 110. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent to the second solvent (iv) is 40:60 to 10:90.

[0136] 111. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent (ii) to the second solvent (iv) is 40:60 to 20:80.

[0137] 112. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent (ii) to the second solvent (iv) is 40:60 to 20:80.

[0138] 113. The composition according to any one of the preceding items, wherein the weight ratio of the first solvent (ii) to the second solvent (iv) is 40:60 to 30:70.

[0139] 114. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 3:1 to 1:3.

[0140] 115. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 2:1 to 1:2.

[0141] 116. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:1 to 1:5.

[0142] 117. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:1 to 1:4.

[0143] 118. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:1 to 1:2.

[0144] 119. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:1 to 1:1.5.

[0145] 120. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:1.1 to 1:1.4.

[0146] 121. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:1.2 to 1:1.4.

[0147] 122. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:1.3 to 1:1.4.

[0148] 123. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 3:4.

[0149] 124. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:15 to 1:3.5.

[0150] 125. The composition according to any one of the preceding items, wherein the weight ratio of (iii) cyclododecane to (iv) the second solvent is 1:2.5.

[0151] 126. The composition according to any one of the preceding items, wherein the composition further comprises one or more additives, particularly one or more additives selected from camphor, menthol and combinations thereof, wherein the content of the additives is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.25 wt.% or more to 2.5 wt.% or less, and most preferably 0.5 wt.% or more to 1.5 wt.% or less or 1.0 wt.% or less, based on the total combined weight of the additives and each of components (i) to (iv).

[0152] 127. The composition according to any one of the preceding items, wherein the composition further comprises one or more additives, particularly one or more additives selected from camphor, menthol, limonene (especially D-limonene) and combinations thereof, wherein the content of the additives is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.25 wt.% or more to 2.5 wt.% or less, and most preferably 0.5 wt.% or more to 1.5 wt.% or less or 1.0 wt.% or less, based on the total combined weight of the additives and each of components (i) to (iv).

[0153] 128. The composition according to any one of the preceding items, wherein (i) adamantane and (iii) cyclododecane (if present) and any other additives present are dissolved in (ii) a first solvent and (iv) a second solvent (if present).

[0154] 129. The composition according to any one of the preceding items, wherein the composition further comprises a propellant.

[0155] 130. The composition according to item 129, wherein the propellant is selected from butane, propane, isobutane, and any combination thereof.

[0156] 131. The composition according to any one of items 129 and 130, wherein the amount of propellant present, based on the total weight of the composition, is 15 wt.% or more to 90 wt.% or less, preferably 20 wt.% or more to 80 wt.% or less, more preferably 25 wt.% or more to 75 wt.% or less.

[0157] 132. The composition according to any one of items 129 to 131, wherein the amount of propellant present, based on the total weight of the composition, is 30 wt.% or more to 70 wt.% or less, preferably 35 wt.% or more to 60 wt.% or less, more preferably 40 wt.% or more to 50 wt.% or less.

[0158] 133. The composition according to any one of the foregoing items, wherein the composition is free of or substantially free of C 3-13 Dialkyl ketones.

[0159] 134. The composition according to any one of the foregoing items, wherein the composition does not contain C 3-13 Dialkyl ketones.

[0160] 135. The composition according to any one of the preceding items, wherein the composition is free of or substantially free of acetone.

[0161] 136. The composition according to any one of the preceding items, wherein the composition is free of acetone.

[0162] 137. The composition according to any one of the preceding items, wherein the composition is free of or substantially free of methyl ethyl ketone.

[0163] 138. The composition according to any one of the preceding items, wherein the composition is free of methyl ethyl ketone.

[0164] 139. The composition according to any one of the preceding items, wherein the composition is free of or substantially free of isopropanol.

[0165] 140. The composition according to any one of the preceding items, wherein the composition is free of isopropanol.

[0166] 141. The composition according to any one of the preceding items, wherein, based on the total weight of components (i) to (iv), the content of adamantane is less than 30 wt.

[0167] 142. The composition according to any one of the preceding items, wherein, based on the total weight of components (i) to (iv), the content of adamantane in (i) is less than 20 wt.

[0168] 143. The composition according to any one of the preceding items, wherein the content of adamantane in (i) is less than 15 wt. based on the total weight of components (i) to (iv).

[0169] 144. The composition according to any one of the preceding items, wherein the composition comprises a second solvent (iv) different from the first solvent, and the content of the second solvent (iv) different from the first solvent is 50 wt.% or less based on the total weight of components (i) to (iv).

[0170] 145. The composition according to any one of the preceding items, wherein the composition comprises a second solvent (iv) different from the first solvent, and the content of the second solvent (iv) different from the first solvent is 40 wt.% or less based on the total weight of components (i) to (iv).

[0171] 146. The composition according to any one of the preceding items, wherein the composition comprises a second solvent (iv) different from the first solvent, and the content of the second solvent (iv) different from the first solvent is 30 wt.% or less based on the total weight of components (i) to (iv).

[0172] 147. The composition according to any one of the preceding items, wherein the composition comprises less than 30 wt.% of an alcohol, particularly ethanol and / or isopropanol, based on the total weight of components (i) to (iv).

[0173] 148. The composition according to any one of the preceding items, wherein, based on the total weight of components (i) to (iv), the composition comprises less than 85 wt.%, preferably less than 50 wt.%, more preferably less than 25 wt.%, and even more preferably less than 10 wt.% of cyclohexane.

[0174] 149. The composition according to any one of the preceding items, wherein the composition is free of or substantially free of cyclohexane.

[0175] 150. The composition according to any one of the preceding items, wherein the composition is free of or substantially free of isopentane.

[0176] 151. The composition according to any one of the preceding items, wherein the composition comprises substantially the components expressly listed herein.

[0177] 152. The composition according to any one of the preceding items, wherein the composition comprises the components expressly listed herein.

[0178] 153. Use of the composition according to any one of the preceding items in 3D scanning applications.

[0179] 154. Use of the composition according to any one of items 1 to 152 in the preparation of an object surface for 3D scanning measurement.

[0180] 155. Use of the composition according to any one of items 1 to 152 in improving the 3D scanning quality and / or resolution of an object.

[0181] 156. Use of the composition according to any one of items 1 to 152 in improving the light reflectivity of a surface on which the composition is applied.

[0182] 157. Use of the composition according to any one of items 1 to 152 in improving the 3D scannability of a surface.

[0183] 158. A method for improving the 3D scannability of a surface, the method comprising the step of applying a composition according to any one of items 1 to 152 to the surface to be scanned.

[0184] 159. A method for preparing an object surface for 3D scanning measurement, the method comprising the step of applying a composition according to any one of items 1 to 152 to the surface to be scanned.

[0185] 160. A method for performing 3D scanning of an object, the method comprising the steps of: 1) applying a composition according to any one of items 1 to 152 to the surface of the object to be scanned, and 2) performing 3D scanning measurements.

[0186] 161. Use of the composition according to any one of items 1 to 152 in photogrammetry.

[0187] 162. Use of the composition according to any one of items 1 to 152 in the preparation of an object surface for photogrammetric optical measurement.

[0188] 163. Use of the composition according to any one of items 1 to 152 in improving the scanning quality and / or resolution of an object, wherein the scanning is performed using photogrammetry.

[0189] 164. Use of the composition according to any one of items 1 to 152 in improving the photogrammetric scanability of a surface.

[0190] 165. A method for improving the photogrammetric scanability of a surface, the method comprising the step of applying a composition according to any one of items 1 to 152 to a surface to be scanned by photogrammetry.

[0191] 166. A method for preparing an object surface for photogrammetric scanning, the method comprising the step of applying a composition according to any one of items 1 to 152 to the surface to be scanned.

[0192] 167. A method for performing photogrammetric scanning of an object, the method comprising the steps of: 1) applying a composition according to any one of items 1 to 152 to the surface of the object to be scanned, and 2) performing photogrammetric scanning measurement.

[0193] 168. Use of the composition according to any one of items 1 to 152 in reducing the intensity of light reflection on a surface to which the composition is applied.

[0194] 169. Use of the composition according to any one of items 1 to 152 as a matting agent.

[0195] 170. Use of the composition according to any one of items 1 to 152 in improving the opacity of a surface on which the composition is applied.

[0196] 171. Use of the composition according to any one of items 1 to 152 in forming a protective coating on a surface on which the composition is applied, in particular, wherein the protective coating is a temporary protective coating, preferably wherein the temporary protective coating sublimates over time. Attached Figure Description

[0197] Figure 1 The visual representation of the coated surface of Example 1 is shown.

[0198] Figure 2 The visual representation of the coated surface of Example 2 is shown.

[0199] Figure 3 The visual representation of the coated surface of Example 3 is shown.

[0200] Figure 4 The visual representation of the coated surface in Comparative Example 1 is shown.

[0201] Figure 5 The visual representation of the coated surface in Comparative Example 2 is shown.

[0202] Figure 6 The visual representation of the coated surface in Comparative Example 3 is shown. Detailed Implementation

[0203] Unless otherwise specified herein, atmospheric pressure shall be understood as 101.325 kPa. Unless otherwise specified herein, room temperature or ambient temperature shall be understood as 21 ± 1 °C. Unless otherwise stated, all measurements and procedures disclosed herein shall be understood as being performed at atmospheric pressure and room temperature. Unless otherwise stated, all boiling point values ​​referred to herein shall be understood as boiling point values ​​measured at atmospheric pressure. Unless otherwise stated, all weight percentage values ​​(wt.%) specified herein shall be understood as weight percentages relative to the total weight of the composition.

[0204] The compositions of the present invention are intended to achieve one or more of the objectives outlined above by overcoming one or more disadvantages associated with known prior art solutions for preparing object surfaces for 3D scanning measurements (in particular by providing the object with an anti-reflective coating that enables improved 3D scanning measurements of said object).

[0205] In this respect, the present invention relates to a composition comprising: (i) adamantane; and (ii) a first solvent, wherein the first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point of 25°C or higher at atmospheric pressure, the boiling point range having a minimum boiling point of 25°C or higher at atmospheric pressure; and optionally... (iii) Cyclododecane; and / or optionally (iv) A second solvent, which is different from the first solvent.

[0206] In this context, the invention also relates to a composition comprising: (i) adamantane; and (ii) A first solvent, wherein the first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point of 25°C or above at atmospheric pressure, the boiling point range having a minimum boiling point of 25°C or above at atmospheric pressure; (iii) Optionally includes cyclododecane; Also includes: (iv) a second solvent, which is different from the first solvent; and / or (v) Propellant.

[0207] The inventors have discovered that solutions formed using adamantane dissolved in a first solvent or a mixture of the first and second solvents can overcome one or more of the problems outlined above. As demonstrated by experimental data in this application, a direct comparison of the compositions of the present invention with prior art alternatives also using sublimable coatings in 3D scanning applications shows that the compositions of the present invention can form coatings with significantly improved thinness, uniformity, and surface quality, thereby enabling for the first time accurate, high-quality, and high-resolution 3D scanning of surfaces and objects to which such sublimable compositions have been applied. Furthermore, the compositions of the present invention using adamantane dissolved in at least the first solvent have been found to exhibit a number of other advantages over prior art compositions using CCDs dissolved only in propellant gas (i.e., known prior art solutions for providing sublimable coatings in the field of 3D scanning), as surfaces exhibiting particularly excellent damage resistance, adhesive point adhesion, adhesive point removal and reapplication tolerance, and residence time characteristics are obtained. Additionally, using adamantane instead of a CCD has the added advantage of not subjecting the user to unpleasant or pungent odors from the composition or coated object. Although the coating formed by the compositions of the present invention is thin, it exhibits a high level of durability and adhesion against direct contact with running water, thus demonstrating excellent weather resistance. It is also capable of forming a coating exhibiting all the aforementioned advantages on oily / lubricated surfaces, which remain oily / lubricated after sublimation, thereby protecting them from environmental influences. The requirement for reapplication of oil / lubricant is reduced compared to prior art compositions; in fact, it is generally no longer required. The compositions disclosed herein exhibit all these advantages, making a valuable contribution to the field. The excellent balance achieved among such a wide range of properties, as demonstrated herein, further enhances the value of the contributions of the compositions of the present invention.

[0208] In this invention and disclosure, adamantane refers to adamantane (C) as known in the art. 10 H 16 The compositions of the present invention are compounds that do not contain any other adamantane-containing materials, such as, for example, polyadamantane (also known as diadamantoids) comprising two or more adamantane units in a single molecule, or substituted adamantane. Therefore, the compositions of the present invention are preferably substantially free of or completely free of such polyadamantanes and substituted adamantanes, and if any such compounds are present, their presence is due to impurities contained in commercially available adamantane, and their content will in no way affect the advantageous properties of the compositions of the present invention described herein.

[0209] The compositions of the present invention may optionally include a second sublimable hydrocarbon in the form of cyclododecane (also referred to in the art as CCD or CDD). In addition to adamantane, the advantage of using a CCD is the increased residence time of the coating on the coated surface. Depending on the specific application and the size, shape, and / or type of the object to be 3D scanned, a shorter or longer residence time of the applied coating may be required. Therefore, if a longer scanning time is anticipated, or a longer period exists between the application of the composition / coating to the surface to be scanned and the 3D scan itself, achieving a longer residence time (enough time for the coating to remain on the surface for successful scanning measurement) may be advantageous. Thus, the use of a mixture of adamantane and CCD in the compositions of the present invention can provide coatings exhibiting one or more of the aforementioned advantages, while providing coatings that remain on the surface to be scanned for a longer time compared to coatings formed from compositions containing adamantane as the sole sublimable material. Therefore, by increasing or decreasing the CCD content relative to adamantane, the residence time of the coating can be customized to the user's specific needs without sacrificing other desired properties, such as coating thinness and uniformity, achievable 3D scan quality, damage resistance, adhesive point adhesion, etc. In fact, contrary to what has been observed with prior art compositions employing CCD, the use of a mixture of CCD and adamantane allows for a coating with improved thinness compared to coatings employing adamantane alone. Regarding residence time, a shorter residence time, as understood in this invention, can be considered as a residence time of less than 45 minutes. A medium residence time can be considered as a period of 45 minutes or more up to 24 hours or less. A longer residence time can be considered as a period of more than 24 hours. Therefore, the object of this invention is to provide a product that can be customized to provide a coating exhibiting any of these residence times while simultaneously providing excellent performance in one or more (preferably all) of the aforementioned characteristics. The residence times mentioned above were measured at room temperature and atmospheric pressure.

[0210] The compositions of the present invention can be, and preferably are, solutions. When the compositions of the present invention are solutions, all sublimable components (adamantane, cyclododecane, and any other sublimable components or additives present) in a given composition are completely dissolved in a first solvent or a mixture of the first and second solvents present in the composition, such that the resulting composition is a solution at room temperature.

[0211] In the presence of cyclododecane in the composition of the present invention, preferably, a second solvent different from the first solvent is also present in the composition.

[0212] Based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) in the compositions of the present invention can be 0.5 wt.% or more, 1.0 wt.% or more, 1.5 wt.% or more, 2.5 wt.% or more, 3 wt.% or more, 5 wt.% or more, or from 6 wt.% or more to 10 wt.% or less, 11 wt.% or less, 12 wt.% or less, 15 wt.% or less, 20 wt.% or less, 30 wt.% or less, or 50 wt.% or less. Within these ranges, the compositions of the present invention can particularly have a lower limit of 1.5 wt.% or more. Within these ranges, the compositions of the present invention preferably have a lower limit of 2.5 wt.% or more. Within these ranges, the compositions of the present invention more preferably have a lower limit of 3 wt.% or more. In these ranges, the compositions of the present invention more preferably have a lower limit of 5 wt.% or more. In these ranges, the compositions of the present invention most preferably have a lower limit of 6 wt.% or more. In these ranges, the compositions of the present invention particularly may have an upper limit of 20 wt.% or less. In these ranges, the compositions of the present invention preferably have an upper limit of 15 wt.% or less. In these ranges, the compositions of the present invention more preferably have an upper limit of 12 wt.% or less. In these ranges, the compositions of the present invention more preferably have an upper limit of 11 wt.% or less. In these ranges, the compositions of the present invention most preferably have an upper limit of 10 wt.% or less. The compositions of the present invention exhibiting these weight ranges may be free of (iii) cyclododecane. The compositions of the present invention exhibiting these weight ranges may contain (i) adamantane and (iii) cyclododecane.

[0213] Preferably, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) in the composition of the present invention is 1.5 wt.% or more, or 3 wt.% or more to 10 wt.% or less, 11 wt.% or less, 12 wt.% or less, 15 wt.% or less, 20 wt.% or less, 30 wt.% or less, or 50 wt.% or less. More preferably, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) in the composition of the present invention is 3 wt.% or more to 20 wt.% or 15 wt.% or less. More preferably, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) in the compositions of the present invention is 3 wt.% or more to 12 wt.% or less, or 11 wt.% or less, or even 5 wt.% or more to 11 wt.% or 10 wt.% or less. Compositions of the present invention exhibiting these weight ranges may be free of (iii) cyclododecane. Compositions of the present invention exhibiting these weight ranges may contain (i) adamantane and (iii) cyclododecane. Compositions of the present invention exhibiting these weight ranges may be free of (iii) cyclododecane and (iv) a second solvent, and in this case, preferably composed of (i) adamantane and (ii) a first solvent. Compositions of the present invention exhibiting these weight ranges may contain (i) adamantane and (iii) cyclododecane and (iv) a second solvent.

[0214] In a particularly preferred embodiment of the invention, the composition is free of (iii) cyclododecane and (iv) a second solvent. In a particularly preferred embodiment of the invention, the composition is free of (iii) cyclododecane and (iv) a second solvent, and the total amount of (i) adamantane is 3 wt.% or more to 20 wt.% or 15 wt.% or less, preferably 5 wt.% or more to 15 wt.% or less or 12 wt.% or less, based on the total weight of components (i) to (iv). In this embodiment, the total content of (i) adamantane is particularly preferably 6 wt.% or more to 10 wt.% or less. In this case, in one embodiment, the amount of (i) adamantane present may be 6.25 wt.% based on the total weight of components (i) to (iv). In this case, in one embodiment, the amount of (i) adamantane present may be 10 wt.% based on the total weight of components (i) to (iv). In these embodiments, the composition of the present invention may consist essentially of or comprise (i) adamantane and (ii) a first solvent, i.e., the composition does not contain any (iii) cyclododecane, (iv) a second solvent, or any other additives or components. In these embodiments, the composition of the present invention may consist essentially of or comprise (i) adamantane, (ii) a first solvent, and a propellant, i.e., the composition does not contain any (iii) cyclododecane, (iv) a second solvent, or any other additives or components.

[0215] In a further, particularly preferred embodiment of the invention, the composition comprises (iii) cyclododecane, and the total combined amount of (i) adamantane and (iii) cyclododecane is 3 wt.% or more to 20 wt.% or 15 wt.% or less, preferably 5 wt.% or more to 15 wt.% or less or 12 wt.% or less, based on the total weight of components (i) to (iv). In this embodiment, the total combined amount of (i) adamantane and (iii) cyclododecane is particularly preferably 6 wt.% or more to 11 wt.% or less. In this case, in one embodiment, the combined amount of (i) adamantane and (iii) cyclododecane may be 7 wt.% or more to 11 wt.% or less, based on the total weight of components (i) to (iv). In this case, in one embodiment, the combined amount of (i) adamantane and (iii) cyclododecane present, based on the total weight of components (i) to (iv), may be 9 wt.% or more to 11 wt.% or less, and even more preferably, the combined amount present, based on the total weight of components (i) to (iv), is 10 wt%. In this case, the composition of the present invention preferably further includes (iv) a second solvent. In this case, in an even more preferred embodiment, the composition of the present invention further comprises camphor and / or menthol (preferably camphor), and the content of camphor and / or menthol is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.5 wt.% or more to 2.5 wt.% or less, based on the total combined weight of the camphor and / or menthol and each of components (i) to (iv).

[0216] In a further preferred embodiment of the invention, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) in the composition of the invention may be 10.0 wt.% or more, 12 wt.% or more, 13 wt.% or more, 15 wt.% or more, 20 wt.% or more, 25 wt.% or more, 30 wt.% or more, 35 wt.% or more, 40 wt.% or more, 45 wt.% or more, 50 wt.% or more, or 55 wt.% or more up to 90 wt.% or less, 85 wt.% or less, 80 wt.% or less, 75 wt.% or less, 70 wt.% or less, 65 wt.% or less, or 60 wt.% or less. In this case, in one aspect, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) may be 10 wt.% or more to 15 wt.% or less. In this aspect, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is preferably 12 wt.% or more to 15 wt.% or less. More preferably, in this aspect, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is more preferably 13 wt.% or more to 15 wt.% or less. In this aspect, the composition preferably does not contain (iii) cyclododecane. Still in this context, in another (second) aspect, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) in the composition of the present invention may be 10 wt.% or more to 55 wt.% or less. More preferably, in this (second) aspect, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) in the composition of the present invention is 10 wt.% or more to 50 wt.% or less. Still in this case, in yet another (third) aspect, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) may be 20 wt.% or more to 90 wt.% or less, 25 wt.% or more to 85 wt.% or less, 30 wt.% or more to 80 wt.% or less, 30 wt.% or more to 75 wt.% or less, 30 wt.% or more to 70 wt.% or less, or 30 wt.% or more to 65 wt.% or less.Preferably, in this (third) aspect, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 35 wt.% or more to 60 wt.% or less, especially 35 wt.% or more to 55 wt.% or less, more especially 40 wt.% or more to 55 wt.% or less, more preferably 40 wt.% or more to 50 wt.% or less, and most preferably 45 wt.% or more to 50 wt.% or less. In this (third) aspect, a composition is also preferred in which the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 30 wt.% or more to 50 wt.% or less, or to 40 wt.% or less, or 35 wt.% or more to 50 wt.% or less, or to 45 wt.% or less, preferably 35 wt.% or more to 40 wt.% or less. In this (third) aspect, the composition of the invention preferably comprises (iii) cyclododecane. In this embodiment (i.e., including each individual aspect), the composition preferably comprises (iv) a second solvent different from the first solvent. The (iv) second solvent is preferably ethanol.

[0217] In the compositions of the present invention, and in the context of the foregoing preferred embodiments and other parts thereof, the weight ratio of adamantane to cyclododecane can be 100:0, 95:5, 90:10, 80:20, 75:25, 2.7:1, 60:40, or 51:49 to 49:51, 40:60, 1:2.7, 25:75, 20:80, 10:90, 5:95, or 1:99. A 100:0 ratio, i.e., a composition without cyclododecane, may be suitable when a particularly short residence time (less than 45 minutes) of the coating on the surface to be scanned is desired. Generally, increasing the cyclododecane content relative to adamantane results in a particularly long residence time. The weight ratio of adamantane to cyclododecane can be from 100:0 to 5:95 or 1:99. In particular, the weight ratio of adamantane to cyclododecane can be from 100:0 to 20:80 or 10:90. Preferably, the weight ratio of adamantane to cyclododecane can be from 100:0 to 25:75. Most preferably, the weight ratio of adamantane to cyclododecane in the composition of the present invention can be from 100:0 to 1:2.7.

[0218] When a longer residence time of the coating is required, the weight ratio of adamantane to cyclododecane is preferably 95:5 to 5:95 or 90:10 to 10:90. When a moderate residence time (45 minutes or longer to 24 hours or less) is required and the composition includes cyclododecane, a particularly attractive balance of properties can be obtained using a weight ratio of adamantane to cyclododecane of 80:20 to 20:80 (especially 75:25 to 25:75). Most preferably, in this case, the weight ratio of adamantane to cyclododecane can be 2.7:1 to 1:2.7. The weight ratio of adamantane to cyclododecane can also be 60:40 to 40:60 or 51:49 to 49:51. In cases where a moderate dwell time (45 minutes or longer to 24 hours or less) and other desirable properties described herein are particularly attractively balanced, and the composition includes cyclododecane, it is especially preferred to use adamantane and cyclododecane in the composition of the invention, with a weight ratio of adamantane to cyclododecane of 1:1 to 1:4, particularly 1:1 to 1:3, more particularly 1:2 to 1:3, and most particularly 1:2.7. Furthermore, in this case, the composition of the invention may also contain more adamantane than cyclododecane (by weight). In this case, the weight ratio of adamantane to cyclododecane may preferably be 1.5:1 to 1:1, more preferably 1.5:1 to 1.25:1, and most preferably 1.4:1 to 1.3:1.

[0219] Therefore, in this case, in a further particularly preferred embodiment of the invention, the composition comprises (iii) cyclododecane, and the total combined amount of (i) adamantane and (iii) cyclododecane is 3 wt.% or more to 20 wt.% or 15 wt.% or less, preferably 5 wt.% or more to 15 wt.% or less or 12 wt.% or less, based on the total weight of components (i) to (iv). In this embodiment, the total combined amount of (i) adamantane and (iii) cyclododecane is particularly preferably 6 wt.% or more to 11 wt.% or less. In this case, in one embodiment, the combined amount of (i) adamantane and (iii) cyclododecane may be 7 wt.% or more to 11 wt.% or less, based on the total weight of components (i) to (iv). In this embodiment, the combined amount of (i) adamantane and (iii) cyclododecane, based on the total weight of components (i) to (iv), can be 9 wt.% or more to 11 wt.% or less, and even more preferably, the combined amount of components (i) to (iv) is 10 wt.%. In this case, the weight ratio of adamantane to cyclododecane is preferably 1:1 to 1:4, more preferably 1:1 to 1:3, even more preferably 1:2 to 1:3, and most particularly 1:2.7. In this case, the composition of the present invention preferably further includes (iv) a second solvent. In this case, the composition of the present invention preferably further includes camphor and / or menthol (preferably camphor), and the content of camphor and / or menthol is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.5 wt.% or more to 2.5 wt.% or less, and most preferably 0.5 wt.% or more to 1.0 wt.% or less, based on the total combined weight of the camphor and / or menthol and each of components (i) to (iv).

[0220] Therefore, in this case, in a further particularly preferred embodiment of the invention, the composition comprises (iii) cyclododecane, and based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane is 20 wt.% or more to 90 wt.% or less, preferably 25 wt.% or more to 85 wt.% or less, or 30 wt.% or more to 75 wt.% or less, 70 wt.% or less, or 65 wt.% or less. In a first aspect of this embodiment, the total combined amount of (i) adamantane and (iii) cyclododecane is particularly preferably 35 wt.% or more to 60 wt.% or less. In the case of this first aspect, based on the total weight of components (i) to (iv), the combined amount of (i) adamantane and (iii) cyclododecane may be 35 wt.% or more to 55 wt.% or less, or 40 wt.% or more to 55 wt.% or less. In this first aspect, based on the total weight of components (i) to (iv), the combined amount of (i) adamantane and (iii) cyclododecane is preferably 40 wt.% or more to 50 wt.% or less, and even more preferably, based on the total weight of components (i) to (iv), the combined amount of (i) adamantane and (iii) cyclododecane is 45 wt.% or more to 50 wt.% or less. Alternatively, in another (second) aspect of this embodiment, based on the total weight of components (i) to (iv), the combined amount of (i) adamantane and (iii) cyclododecane is 30 wt.% or more to 50 wt.% or less, or to 40 wt.% or less, or 35 wt.% or more to 50 wt.% or less, or to 45 wt.% or less, preferably 35 wt.% or more to 40 wt.% or less. In this embodiment, the weight ratio of adamantane to cyclododecane is preferably 1.5:1 to 1:1, more preferably 1.5:1 to 1.25:1, and most preferably 1.4:1 to 1.3:1. In this embodiment, the composition of the invention preferably further includes (iv) a second solvent as defined elsewhere herein. In this case, if present, (iv) the second solvent is preferably ethanol. In this embodiment, the composition of the invention may also include additives as defined elsewhere herein, particularly camphor and / or menthol (preferably camphor), the content of which, based on the total combined weight of the camphor and / or menthol and each of components (i) to (iv), is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.5 wt.% or more to 2.5 wt.% or less, and most preferably 0.5 wt.% or more to 1.0 wt.% or less.

[0221] The compositions of the present invention include a first solvent. The first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point range of 25°C or higher at atmospheric pressure, wherein the boiling point range has a lowest boiling point of 25°C or higher at atmospheric pressure (i.e., the lowest boiling point component of the hydrocarbon mixture has a boiling point of 25°C or higher). The first solvent may be a hydrocarbon or a composition of hydrocarbons having a boiling point or boiling point range of 25°C or higher, 30°C or higher, 35°C or higher, or 40°C or higher to 50°C or lower, 60°C or lower, 65°C or lower, 70°C or lower, 75°C or lower, 80°C or lower, 90°C or lower, 100°C or lower, 110°C or lower, 120°C or lower, or 130°C or lower at atmospheric pressure. In particular, the boiling point or boiling point range of the first solvent at atmospheric pressure can be 30°C or above, or 35°C or above to 50°C or below, 60°C or below, 65°C or below, 70°C or below, 75°C or below, 80°C or below, 90°C or below, 100°C or below, 110°C or below, 120°C or below, or 130°C or below. Preferably, the boiling point or boiling point range of the first solvent at atmospheric pressure can be 35°C or above, or 40°C or above to 50°C or below, 60°C or below, 65°C or below, 70°C or below, 75°C or below, 80°C or below, 90°C or below, 100°C or below, 110°C or below, 120°C or below, or 130°C or below. More preferably, the boiling point or boiling point range of the first solvent is 35°C or higher to 100°C or lower, especially 90°C or lower, preferably 80°C or lower, more preferably 75°C or lower, and most preferably 70°C or lower. In a particularly preferred embodiment, the boiling point or boiling point range of the first solvent is 40°C or higher to 65°C or lower. In other particularly preferred embodiments, the boiling point or boiling point range of the first solvent is 45°C or higher to 100°C or lower, and may be 50°C or higher to 100°C or lower, or 60°C or higher to 95°C or lower. In the above cases, the first solvent may be, and preferably, an aliphatic hydrocarbon or a mixture of aliphatic hydrocarbons.

[0222] The first solvent can be selected from one or more aliphatic linear, branched, or cyclic C5-C solvents. 10 The group consisting of hydrocarbons, wherein the hydrocarbons may be saturated or unsaturated. The first solvent may be selected from the group consisting of one or more aliphatic straight-chain, branched, or cyclic C5-C8 hydrocarbons, wherein the hydrocarbons may be saturated or unsaturated. Examples of saturated or unsaturated aliphatic straight-chain or branched C5-C8 hydrocarbons include pentane, cyclopentane, pentene, cyclopentene, hexane, cyclohexane, hexene, cyclohexene, heptane, cycloheptane, heptene, cycloheptene, octane, cyclooctane, octene, and cyclooctene. References to heptene and octene should be understood to cover all isomers of these compounds.

[0223] The first solvent can be selected from the group consisting of pentane, cyclopentane, hexane, cyclohexane, heptane, cycloheptane, octane, petroleum ether, petroleum ether 30-40, petroleum ether 40-60, petroleum ether 40-65, petroleum ether 60-80, petroleum ether 80-100, and any combination thereof. Alternatively, the first solvent can be selected from the group consisting of pentane, cyclopentane, hexane, cyclohexane, heptane, cycloheptane, octane, petroleum ether, petroleum ether 30-40, petroleum ether 40-60, petroleum ether 40-65, petroleum ether 60-80, petroleum ether 60-95, petroleum ether 80-100, and any combination thereof. As used herein, pentane should be understood to include n-pentane, isopentane, and neopentane, and preferably n-pentane. As used herein, pentene should be understood to include 1-pentene, cis-2-pentene, and trans-2-pentene. As used herein, hexane should be understood to include n-hexane, 2-methylpentane, 3-methylpentane, 2,3-dimethylbutane, and 2,2-dimethylbutane, preferably n-hexane. As used herein, hexene should be understood to include 1-hexene, trans-2-hexene, cis-2-hexene, trans-3-hexene, and cis-3-hexene. As used herein, heptane should be understood to include n-heptane, 2-methylhexane, 3-methylhexane, 2,2-dimethylpentane, 2,3-dimethylpentane, 2,4-dimethylpentane, 3,3-dimethylpentane, 3-ethylpentane, and 2,2,3-trimethylbutane, preferably n-heptane. As used herein, heptene should be understood to include 1-heptene and all other isomers of heptene. As used herein, octane is to be understood to include n-octane, 2-methylheptane, 3-methylheptane, 4-methylheptane, 3-ethylhexane, 2,2-dimethylhexane, 2,3-dimethylhexane, 2,4-dimethylhexane, 2,5-dimethylhexane, 3,3-dimethylhexane, 3,4-dimethylhexane, 3-ethyl-2-methylpentane, 3-ethyl-3-methylpentane, 2,2,3-trimethylpentane, 2,2,4-trimethylpentane, 2,3,4-trimethylpentane, and 2,2,3,3-tetramethylbutane, and preferably n-octane. As used herein, octene is to be understood to include 1-octene and all other isomers of octene.

[0224] The term petroleum ether is widely used and understood by those skilled in the art. Petroleum ether is a distillation fraction of petroleum, consisting of or substantially composed of aliphatic hydrocarbons. Different fractions may be collected during petroleum distillation, resulting in different products defined by the temperature range of petroleum distillation at atmospheric pressure, within which these products are collected. For example, petroleum ether 40-65 refers to a petroleum distillation fraction collected between 40°C and 65°C, meaning that the hydrocarbon compounds contained therein have a boiling point range of 40°C to 65°C at atmospheric pressure. Synonyms for "petroleum ether" in the art include "wundbenzin," "petroleum spirit," "lignoin," "naphtha," and "petroleum volatile oil."

[0225] The first solvent can be selected from the group consisting of C5-hydrocarbons, C6-hydrocarbons, C7-hydrocarbons, C8-hydrocarbons, or any combination thereof, wherein the solvent or solvent mixture has a boiling point as defined above. The first solvent is preferably selected from the group consisting of pentane, cyclopentane, hexane, cyclohexane, heptane, cycloheptane, octane, petroleum ether, petroleum ether 30-40, petroleum ether 40-60, petroleum ether 40-65, petroleum ether 60-80, petroleum ether 60-95, petroleum ether 80-100, or any combination thereof. In this case, the first solvent can be selected from the group consisting of cyclopentane, hexane, cyclohexane, heptane, cycloheptane, octane, petroleum ether, petroleum ether 30-40, petroleum ether 40-60, petroleum ether 40-65, petroleum ether 60-80, petroleum ether 60-95, petroleum ether 80-100, or any combination thereof. In some embodiments, the first solvent is not pentane. In some embodiments, the first solvent may contain pentane, but is not limited to pentane. Most preferably, the first solvent is petroleum ether 40-65 or petroleum ether 60-95 or cyclopentane or a mixture of petroleum ether 60-95 and cyclopentane. In the most preferred embodiment, the first solvent comprises cyclopentane. The above disclosures relating to the definition or specific characteristics of the first solvent can be combined with any disclosures provided herein regarding the definition or characteristics of any other component and combination thereof of the compositions disclosed herein (including disclosures relating to their respective amounts in the compositions of the invention).

[0226] The compositions of the present invention optionally include a second solvent different from the first solvent. In particular, in the case of the presence of cyclododecane in the compositions of the present invention, preferably, a second solvent different from the first solvent is also present in the composition. The polarity of the second solvent is preferably greater than that of the first solvent. In the context of the present invention, greater polarity means having a higher dielectric constant (ε) at a given temperature (e.g., at room temperature or 25°C).

[0227] The boiling point or boiling point range of the second solvent at atmospheric pressure can be 40°C or above, 50°C or above, 60°C or above, 64.7°C or above, 70°C or above, 75°C or above, 80°C or above, 82°C or above to 90°C or below, 100°C or below, 110°C or below, 120°C or below, 130°C or below, 140°C or below, 150°C or below, or 160°C or below. Preferably, the boiling point or boiling point range of the second solvent at atmospheric pressure is 50°C or above, or 60°C or above to 90°C or below, 100°C or below, 110°C or below, 120°C or below, 130°C or below, 140°C or below, 150°C or below, or 160°C or below. More preferably, the boiling point or boiling point range of the second solvent at atmospheric pressure is 64.7°C or higher, or 70°C or higher to 90°C or lower, 100°C or lower, 110°C or lower, 120°C or lower, 130°C or lower, 140°C or lower, 150°C or lower, or 160°C or lower. Even more preferably, the boiling point or boiling point range of the second solvent at atmospheric pressure is 75°C or higher, or 80°C or higher to 90°C or lower, 100°C or lower, 110°C or lower, 120°C or lower, 130°C or lower, 140°C or lower, 150°C or lower, or 160°C or lower. Particularly preferably, the boiling point or boiling point range of the second solvent at atmospheric pressure is 60°C or higher to 90°C or lower, or 100°C or lower. Most preferably, the second solvent has a boiling point or boiling point range of 64.7°C or higher to 100°C or lower at atmospheric pressure, particularly 70°C or higher to 90°C or lower, more particularly 75°C or higher to 90°C or lower, and most particularly 75°C or higher to 85°C or lower. In the above-described case, the second solvent is preferably one or more alcohols, preferably one or more alcohols selected from the group consisting of C1-C8 alcohols, particularly one or more alcohols selected from the group consisting of C1-C8 monohydric alcohols, most preferably one or more monohydric alcohols selected from the group consisting of C1-C8 alkanols and C3-C8 cycloalkanols.

[0228] In the compositions of the present invention, when the second solvent is selected from the group consisting of one or more C1-C8 alkanols and C3-C8 cycloalkanols, the second solvent is preferably selected from methanol, ethanol, n-propanol, isopropanol, cyclopropanol, n-butanol, sec-butanol, isobutanol, tert-butanol, cyclobutanol, n-pentanol, 3-methylbut-1-ol, 2-methylbut-1-ol, 2,2-dimethylprop-1-ol, pent-3-ol, pent-2-ol, 3-methylbut-2-ol, 2-methylbut-2-ol, cyclopentanol, hex-1-ol, hex-2-ol. The second solvent is selected from the group consisting of hexane-3-ol, 2-methylpentane-1-ol, 3-methylpentane-1-ol, 4-methylpentane-1-ol, 2-methylpentane-2-ol, 3-methylpentane-2-ol, 4-methylpentane-2-ol, 2-methylpentane-3-ol, 3-methylpentane-3-ol, 2,2-dimethylbutane-1-ol, 2,3-dimethylbutane-1-ol, 3,3-dimethylbutane-1-ol, 2,3-dimethylbutane-2-ol, 3,3-dimethylbutane-2-ol, 2-ethylbutane-1-ol, cyclohexanol, 2-heptanol, 3-heptanol, and 4-heptanol. More preferably, the second solvent is selected from members of this group whose boiling point or boiling point range at atmospheric pressure is 60°C or higher to 90°C or lower, or 100°C or lower. Most preferably, the second solvent is selected from members of this group whose boiling point or boiling point range at atmospheric pressure is 75°C or higher to 85°C or lower. Most preferably, the second solvent is isopropanol or ethanol or a mixture of isopropanol and ethanol, with ethanol being the most preferred.

[0229] The second solvent may be ethanol-free. The second solvent may be benzyl alcohol-free. The second solvent may be both ethanol and benzyl alcohol-free. The compositions of the present invention may be ethanol-free. The compositions of the present invention may be benzyl alcohol-free. The compositions of the present invention may be both ethanol and benzyl alcohol-free.

[0230] The compositions of the present invention may be free of (iv) the second solvent. Where the compositions of the present invention simultaneously include (ii) a first solvent and (iv) a second solvent different from the first solvent (each solvent as defined above), there is no particular limitation on the weight ratio of said (ii) first solvent to said (iv) second solvent, and the most important function of the second solvent is to ensure that the composition is a solution rather than, for example, a suspension. For example, for non-technical reasons (e.g., to comply with specific regulatory standards and requirements of a given jurisdiction), it may also be necessary to vary the content of the second solvent relative to the first solvent. This ratio can be varied extensively without negatively impacting the desired coating properties described elsewhere herein. Therefore, in the case where the composition of the present invention simultaneously comprises (ii) a first solvent and (iv) a second solvent different from the first solvent (each solvent as defined above), the weight ratio of said (ii) first solvent to said (iv) second solvent may be 99:1, 95:5, 90:10, 80:20, 70:30, 3:1, 2:1, 60:40 or 55:45 to 45:55, 40:60, 1:2, 1:3, 30:70, 20:80, 10:90, 5:95 or 1:99. In any composition disclosed herein comprising (ii) a first solvent and (iv) a second solvent different from the first solvent, the weight ratio of said (ii) first solvent to said (iv) second solvent may be from 99:1 to 1:99. In any composition disclosed herein comprising (ii) a first solvent and (iv) a second solvent different from the first solvent, the weight ratio of said (ii) first solvent to said (iv) second solvent may be from 95:1 to 1:95. In any composition disclosed herein comprising (ii) a first solvent and (iv) a second solvent different from the first solvent, the weight ratio of said (ii) first solvent to said (iv) second solvent may be from 90:10 to 10:90. In any composition disclosed herein comprising (ii) a first solvent and (iv) a second solvent different from the first solvent, the weight ratio of said (ii) first solvent to said (iv) second solvent may preferably be from 80:20 to 20:80. In any composition disclosed herein comprising (ii) a first solvent and (iv) a second solvent different from the first solvent, the weight ratio of said (ii) first solvent to said (iv) second solvent may more preferably be from 3:1 to 1:3. The weight ratio of said (ii) first solvent to said (iv) second solvent may be from 70:30 to 30:70. The weight ratio of the first solvent to the second solvent in (ii) can be from 2:1 to 1:2.

[0231] The weight ratio of (ii) the first solvent to (iv) the second solvent can also be 60:40 to 40:60 or 55:45 to 45:55. As demonstrated herein, an excellent balance of desired coating properties can be found by simultaneously employing (ii) the first solvent and (iv) the second solvent in the compositions of the present invention (with a weight ratio of (ii) the first solvent to (iv) the second solvent of 6:1 to 1:1, especially 5:1 to 2:1, more especially 5:1 to 3:1, and most especially 4:1). Where a shorter residence time is required, preferably neither (iii) cyclododecane nor (iv) the second solvent is used.

[0232] However, as outlined above, it may be necessary to change the relative amounts of the two solvents so that, for example, there is a weight ratio of about 1:1, or even an excess of the second solvent relative to the first solvent by weight. Therefore, in the case where the composition of the present invention simultaneously comprises (ii) a first solvent and (iv) a second solvent different from the first solvent (each solvent as defined above), the weight ratio of said (ii) first solvent to said (iv) second solvent can be 55:45, 1:1, or 45:55 to 40:60, 1:2, 30:70, 20:80, 10:90, 5:95, or 1:99. In this case, the weight ratio of said (ii) first solvent to said (iv) second solvent can be 1:1, 45:55, or 40:60 to 5:95, for example 40:60 to 5:95, or preferably 40:60 to 10:90. In this case, the weight ratio of said (ii) first solvent to said (iv) second solvent can more preferably be 40:60 to 20:80.

[0233] In compositions excluding (iii) cyclododecane, the weight ratio of the first solvent (ii) to the second solvent (iv) is particularly preferably 3:1 to 2:1. In compositions containing (iii) cyclododecane, the weight ratio of the first solvent (ii) to the second solvent (iv) is particularly preferably 3:1 to 1:1.

[0234] Therefore, when the compositions disclosed herein include (ii) a first solvent and (iv) a second solvent, the second solvent may be particularly preferably selected from methanol, ethanol, n-propanol, isopropanol, cyclopropanol, n-butanol, sec-butanol, isobutanol, tert-butanol, cyclobutanol, n-pentanol, 3-methylbut-1-ol, 2-methylbut-1-ol, 2,2-dimethylprop-1-ol, pent-3-ol, pent-2-ol, 3-methylbut-2-ol, 2-methylbut-2-ol, cyclopentanol, hex-1-ol, hex-2-ol, hex-3-ol, 2-methylpent-1-ol, 3-methylpent-1-ol, 4-methylpent-1-ol, 2-methylpent-2-ol, 3-methylpent-2-ol, 4-methylpent-2-ol, 2-methylpent-3-ol, 3-methylpent-3-ol, 2,2-dimethylprop-1 ...2,2-dimethylprop-1-ol, 2-methylprop-2-ol, 2-methylpent-3-ol, 2,2-dimethylprop-1-ol, 2-methylprop-2-ol, 2-methylprop-2-ol, 2-methylprop-2-ol, 2-methylprop-2-ol, 2-methylprop-2-ol, 2-methylprop-2-ol, 2-methylprop-2-ol, 2-methylprop-2-ol, 2-methylprop-2-ol, 2-methylprop- The first solvent is selected from the group consisting of methylbutanol, 2,3-dimethylbutanol, 3,3-dimethylbutanol, 2,3-dimethylbutanol, 3,3-dimethylbutanol, 2-ethylbutanol, cyclohexanol, 2-heptanol, 3-heptanol, and 4-heptanol, more preferably from the group consisting of members of the group whose boiling point or boiling point range at atmospheric pressure is 60°C or above to 90°C or below or 100°C or below (more preferably 75°C or above to 85°C or below), and most preferably, the second solvent is isopropanol, ethanol, or a mixture of isopropanol and ethanol, with ethanol being the most preferred; and the weight ratio of the first solvent to the second solvent is 6:1 to 1:1, especially 5:1 to 2:1, preferably 5:1 to 3:1, and most preferably 4:1. In this case, in the composition excluding (iii) cyclododecane, the weight ratio of the first solvent (ii) to the second solvent (iv) is particularly preferably 3:1 to 2:1. In this case, in the composition containing (iii) cyclododecane, the weight ratio of the first solvent (ii) to the second solvent (iv) is particularly preferably 3:1 to 1:1.

[0235] In the composition of the present invention containing (i) adamantane, (ii) a first solvent, (iii) cyclododecane and (iv) a second solvent different from the first solvent, the weight ratio of (i) to (ii) is particularly preferred to be 1:5 to 1:50, most preferably 1:20 to 1:30, or 5:1 to 1:5 or 3:1 to 1:2, most preferably 3:1 to 1:1, and the weight ratio of (iii) to (iv) is 1:1 to 1:5, most preferably 1:2.5 or 1:4.

[0236] In a further, particularly preferred embodiment of the invention, the composition comprises (iii) cyclododecane, and the total combined amount of (i) adamantane and (iii) cyclododecane is 3 wt.% or more to 20 wt.% or 15 wt.% or less, preferably 5 wt.% or more to 15 wt.% or less or 12 wt.% or less, based on the total weight of components (i) to (iv). In this embodiment, the total combined amount of (i) adamantane and (iii) cyclododecane is particularly preferably 6 wt.% or more to 11 wt.% or less. In this case, in one embodiment, the combined amount of (i) adamantane and (iii) cyclododecane may be 7 wt.% or more to 11 wt.% or less, based on the total weight of components (i) to (iv). In this embodiment, the combined amount of (i) adamantane and (iii) cyclododecane, based on the total weight of components (i) to (iv), can be 9 wt.% or more to 11 wt.% or less, and even more preferably, the combined amount of components (i) to (iv) is 10 wt.%. In this embodiment, the composition of the invention preferably further includes (iv) a second solvent, and the second solvent is isopropanol as defined elsewhere herein. In this embodiment, the weight ratio of (ii) the first solvent to (iv) the second solvent can be 99:1, 95:5, 90:10, 80:20, 70:30, 2:1, 60:40, or 55:45 to 45:55, 40:60, 1:2, 30:70, 20:80, 10:90, 5:95, or 1:99, preferably 90:10 or 80:20 to 30:70 or 20:80. In this case, in even more preferred embodiments, the composition of the present invention further comprises camphor and / or menthol (preferably camphor), and the content of camphor and / or menthol is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.5 wt.% or more to 2.5 wt.% or less, based on the total combined weight of the camphor and / or menthol and each of components (i) to (iv).

[0237] In this case, in a further particularly preferred embodiment of the invention, the composition comprises (iii) cyclododecane, and the total combined amount of (i) adamantane and (iii) cyclododecane is 3 wt.% or more to 20 wt.% or 15 wt.% or less, preferably 5 wt.% or more to 15 wt.% or less or 12 wt.% or less, based on the total weight of components (i) to (iv). In this embodiment, the total combined amount of (i) adamantane and (iii) cyclododecane is particularly preferably 6 wt.% or more to 11 wt.% or less. In this case, in one embodiment, the combined amount of (i) adamantane and (iii) cyclododecane may be 7 wt.% or more to 11 wt.% or less, based on the total weight of components (i) to (iv). In this embodiment, the combined amount of (i) adamantane and (iii) cyclododecane, based on the total weight of components (i) to (iv), can be 9 wt.% or more to 11 wt.% or less, and even more preferably, the combined amount of components (i) to (iv) is 10 wt.%. In this case, the weight ratio of adamantane to cyclododecane is preferably 1:1 to 1:4, more preferably 1:1 to 1:3, even more preferably 1:2 to 1:3, and most particularly 1:2.7. In this case, the composition of the present invention preferably further includes (iv) a second solvent, and the second solvent is isopropanol as defined elsewhere herein. In this case, the weight ratio of (ii) the first solvent to (iv) the second solvent can be 99:1, 95:5, 90:10, 80:20, 70:30, 2:1, 60:40 or 55:45 to 45:55, 40:60, 1:2, 30:70, 20:80, 10:90, 5:95 or 1:99, preferably 90:10 or 80:20 to 30:70 or 20:80. In this case, the composition of the present invention preferably further includes camphor and / or menthol (preferably camphor), and the content of camphor and / or menthol is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.5 wt.% or more to 2.5 wt.% or less, and most preferably 0.5 wt.% or more to 1.0 wt.% or less, based on the total combined weight of the camphor and / or menthol and each of components (i) to (iv).

[0238] In a further, particularly preferred embodiment of the invention, the composition comprises (iii) cyclododecane, and the total combined amount of (i) adamantane and (iii) cyclododecane is 20 wt.% or more to 90 wt.% or less, preferably 25 wt.% or more to 85 wt.% or less, or 30 wt.% or more to 75 wt.% or less, 70 wt.% or less, or 65 wt.% or less, based on the total weight of components (i) to (iv). In a first aspect of this embodiment, the total combined amount of (i) adamantane and (iii) cyclododecane is particularly preferably 35 wt.% or more to 60 wt.% or less. In the case of this first aspect, the combined amount of (i) adamantane and (iii) cyclododecane present, based on the total weight of components (i) to (iv), can be 35 wt.% or more to 55 wt.% or less, or 40 wt.% or more to 55 wt.% or less. In this first aspect, based on the total weight of components (i) to (iv), the combined amount of (i) adamantane and (iii) cyclododecane is preferably 40 wt.% or more to 50 wt.% or less, and even more preferably, based on the total weight of components (i) to (iv), the combined amount is 45 wt.% or more to 50 wt.% or less. Alternatively, in another (second) aspect of this embodiment, based on the total weight of components (i) to (iv), the combined amount of (i) adamantane and (iii) cyclododecane is 30 wt.% or more to 50 wt.% or less or to 40 wt.% or less, or 35 wt.% or more to 50 wt.% or less or to 45 wt.% or less, preferably 35 wt.% or more to 40 wt.% or less. In this embodiment, the weight ratio of adamantane to cyclododecane is preferably 1.5:1 to 1:1, more preferably 1.5:1 to 1.25:1, and most preferably 1.4:1 to 1.3:1. In this embodiment, the composition of the invention preferably further includes (iv) a second solvent as defined elsewhere herein. In this case, if present, (iv) the second solvent is preferably ethanol. In this embodiment, the weight ratio of (ii) the first solvent to (iv) the second solvent can be 99:1, 95:5, 90:10, 80:20, 70:30, 2:1, 60:40, or 55:45 to 45:55, 40:60, 1:2, 30:70, 20:80, 10:90, 5:95, or 1:99, preferably 3:1 or 2:1 to 1:3 or 1:2, and most preferably 3:1 to 1:1.In this embodiment, the composition of the present invention may further include camphor and / or menthol (preferably camphor), and the content of camphor and / or menthol is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.5 wt.% or more to 2.5 wt.% or less, and most preferably 0.5 wt.% or more to 1.0 wt.% or less, based on the total combined weight of the camphor and / or menthol and each of components (i) to (iv).

[0239] Although there is no particular limitation on the content of the second solvent, in order to ensure an excellent distribution of the desired coating properties outlined herein, independent of residence time, it may be preferred that the weight ratio of (iii) to (iv) is 1:1 to 1:5, more preferably 1:1.15 to 1:3.5, when (iii) cyclododecane and (iv) the second solvent are present in the composition of the present invention.

[0240] In addition to components (i) to (iv), the compositions of the present invention may also include one or more additives. Additives can be used to provide any amount of the performance and standards required in the field of 3D scanning spray products. In particular, the compositions of the present invention may also include odor masking agents. Such odor masking agents are particularly useful in the compositions of the present invention containing CCDs, which are compounds that the end user may perceive as having an unpleasant odor. Therefore, the compositions of the present invention may include additives capable of masking the odor of CCDs. Examples of such additives include camphor and menthol. Therefore, the compositions of the present invention may include camphor, menthol, or combinations thereof as additives. Another example of such additives is limonene, especially D-limonene. Therefore, the compositions of the present invention may include limonene as an additive, especially D-limonene. Therefore, the compositions of the present invention may include camphor, menthol, limonene (especially D-limonene), or any combination thereof as additives. In this case, based on the total combined weight of the additives and each of components (i) to (iv), one or more additives may be present in the composition of the present invention at any amount required to mask the CCD odor (especially at 0.1 wt.% or more, 0.25 wt.% or more, or 0.5 wt.% or more to 1.0 wt.% or less, 1.5 wt.% or less, 2.5 wt.% or less, or 5 wt.% or less). Preferably, based on the total combined weight of the additives and each of components (i) to (iv), one or more additives are present in an amount of 0.1 wt.% or more to 5 wt.% or less, more preferably 0.25 wt.% or more to 2.5 wt.% or less, even more preferably 0.5 wt.% or more to 1.5 wt.% or less, and most preferably 0.5 wt.% or more to 1.0 wt.% or less. In this case, the weight ratio of camphor and / or menthol (preferably camphor) to the CCD is particularly suitable from 1:5 to 1:20, preferably 1:8. In this case, the weight ratio of camphor, menthol, limonene (especially D-limonene) or any combination thereof (preferably camphor) to the CCD is even more particularly suitable from 1:5 to 1:20, preferably 1:8.

[0241] There are no particular limitations on the types of surfaces on which the compositions of the present invention can be used to provide coatings exhibiting the properties and advantages described herein. Therefore, the compositions of the present invention can be used in particular to form coatings on glass surfaces, metal surfaces, polymer surfaces, acrylic surfaces, wood surfaces, enamel surfaces, textile surfaces (e.g., fabric, nonwoven, or leather), ceramic surfaces, and any other type of surface that may require improvement in the ability to achieve high-quality 3D scanning. Particularly important are surfaces that are transparent, translucent, light-absorbing, reflective, and / or glossy. Typically, such surfaces can be surfaces of parts (including mechanical components) (especially metal parts) used in precision engineering. As summarized above, ideally, an object prepared for optical scanning by applying a coating based on the compositions of the present invention should return to its original, unchanged, uncoated state after measurement, especially without requiring actions such as cleaning or wiping the surface to remove the coating. Therefore, ideally, the compositions of the present invention should not cause any changes to the object to which they are applied, such as structural changes or surface-related changes. Therefore, ideally, the components of the compositions of the present invention should be chemically inert to the surface to which the compositions are applied. Therefore, when applied to, for example, polymers or acrylic materials, it is important that the components do not react with or dissolve the surface of the material or otherwise damage it. Consequently, the compositions of the present invention preferably do not contain components that may damage the surface of polymers or acrylic materials, such as solvents that may harm the surface of polymers or acrylic materials. Examples of such solvents include ketones, such as C3- 13 Dialkyl ketones (i.e., ketones with alkyl groups on both sides of the carbonyl group, containing a total of 3 to 13 carbon atoms), especially acetone and methyl ethyl ketone. Therefore, the compositions of this technology are preferably free of (or substantially free of) acetone and / or methyl ethyl ketone, more preferably free of (or substantially free of) acetone and methyl ethyl ketone. By omitting such compounds / solvents from the compositions of the present invention, the versatility of the compositions in terms of compatibility with different types of scannable objects is improved. "Substantially free of" means that the substance may be present in a small amount that does not affect the desired properties associated with the compositions of this technology as taught herein (e.g., as an impurity in other components of the present composition—commercial solvents may, for example, contain small amounts of excess acetone or methyl ethyl ketone impurities). Therefore, in this case, "substantially free of" can mean that the amount of the substance substantially free of the composition in question can be 1000 ppm or less, 750 ppm or less, 500 ppm or less, 300 ppm or less, 200 ppm or less, 100 ppm or less, 50 ppm or less, or 10 ppm or less. Preferably, the compositions of this technology are free of C3- 13Dialkyl ketones. Preferably, the compositions of this technology are acetone-free. Preferably, the compositions of this technology are methyl ethyl ketone-free.

[0242] The compositions of the present invention can be used to provide a thin (e.g., 50 μm or less, 20 μm or less, 10 μm or less, or even 5 μm or less), highly uniform, scannable coating on the surface of an object, particularly to provide a surface capable of enabling accurate, high-quality, high-resolution 3D scanning of the object. Therefore, the compositions of the present invention can be used in 3D scanning applications (particularly for preparing object surfaces for 3D scanning measurements and / or facilitating 3D scanning measurements and / or enabling 3D scanning of objects). Thus, particularly in the 3D scanning of objects, the compositions of the present invention can be used to improve the scannability, scan quality, scan accuracy, and / or scan resolution of the object. Scannability refers to the ability of an object to be reliably 3D scanned. The compositions can achieve this and are therefore used to improve the diffuseness of light reflected from the object (particularly the diffuseness of light reflected from the object to be 3D scanned), thereby improving scannability, scan accuracy, scan quality, and / or scan resolution. The compositions of the present invention can be further used to provide any other advantages associated with the teachings herein. For example, the compositions of the present invention can be used to prepare object surfaces for scanning measurements (particularly 3D scanning measurements). Furthermore, the compositions of the present invention can be used to provide coated surfaces that exhibit, in particular, excellent resistance to damage, adhesion to reference points required for 3D scanning measurements, the ability to remove and re-adhere these reference points without significantly reducing surface quality, and / or weather resistance (e.g., durability against direct contact with running water). The compositions of the present invention can be used to prepare surfaces for 3D scanning measurements that have been protected or coated with, for example, a film of oil or lubricant.

[0243] Therefore, the present invention also relates to a method for preparing an object surface for 3D scanning measurements, the method comprising the step of applying any composition according to the invention to the surface to be scanned. The method may further comprise the step of allowing (ii) a first solvent and (iv) a second solvent (if present) to evaporate at least partially and preferably completely to form a coating on the surface. Preferably, the coating is non-liquid and / or non-solution. Preferably, the coating forms a surface that exhibits higher opacity relative to a corresponding uncoated surface, and most preferably is opaque. Preferably, the coating is solid at room temperature. Preferably, the coating primarily comprises (i) adamantane and (iii) cyclododecane (if present) (and any other additives used in the composition), but may also include the balance of (ii) the first solvent and (iv) the second solvent (if present in the composition of the invention). Based on the total weight of the coating, the balance refers to less than 10 wt.%, more preferably less than 5 wt.%, even more preferably less than 2 wt.%, and most preferably less than 1 wt.%. Preferably, the coating is substantially free of the balance solvent. The present invention also relates to a method for 3D scanning an object. The method includes the steps described above or the step of preparing an object surface for 3D scanning measurement, as well as additional subsequent steps of performing 3D scanning measurement on the object.

[0244] The compositions of the present invention can be applied to the surface to be coated by any means known and / or standard to those skilled in the art, thereby creating a surface for 3D scanning measurements. In particular, the compositions of the present invention can be applied to the respective surfaces by, for example, spraying (with or without propellant or aerosol), immersing an object or surface in the composition, or applying the composition to the surface using suitable tools known in the art (e.g., a brush).

[0245] Particularly preferred is the application of the composition of the invention to the surface to be coated by spraying. Spray coating can be performed using any standard method known in the art to apply a coating to the surface, thereby preparing a surface for 3D scanning measurements. For example, the composition can be applied using a spray gun technique or by pressurizing the composition (to the pressure standards in the art for such products) in a spray can or container used for this type of coating and using the propellant gas to carry / propel the composition to the surface to be coated as it is ejected from the spray can or container. These are methods well known to those skilled in the art. For example, spray coating can typically be performed at a distance of 30 cm (or even 15 cm to 20 cm) from the surface to be coated. The type of "spray nozzle" ("Sprühkopf") used in the spray can, spray container, or spray gun can be selected from those commonly available and used in the art and can be matched to any specific requirements of the spraying operation and / or the type of object to be sprayed. Most preferably, the spray gun or nozzle exhibits the size and performance of the spray gun or nozzle used in the experimental procedures disclosed herein. For example, the nozzle diameter of the "spray head" is 0.51 (+ / -0.02) mm, or the nozzle diameter of the spray gun is 0.8 mm. Alternatively, a "spray head" with a larger nozzle diameter (e.g., 4 mm) can be used. Preferably, the "spray head" used in the case of the invention sprays a continuous amount upon startup. Preferably, the "spray head" used in the case of the invention is compatible with both BOV and vertical valve types. In addition to those used in the experimental procedures disclosed herein, another example of a coating system suitable for applying the compositions of the invention is an aerosol can (e.g., a 400 ml aerosol can with a diameter of 65 mm and a height of 157 mm) equipped with a ball valve stem (e.g., a 4 mm diameter Ariane ball valve stem, for example) and a "spray head" (e.g., a "spray head" with a nozzle diameter of 4 mm). The spray head can have a "fit-in" neck finish, is compatible with BOV and vertical valves, and sprays a continuous amount. In this regard, where commercial product names or trademarks are used herein to describe these or any other products, the performance, size, dimensions, composition, etc. of the products shall be understood as the performance, size, dimensions, composition, etc. of the corresponding products provided under the names or trademarks as of the filing date of this application (the applicable priority date).

[0246] Therefore, the compositions of the present invention may further include a propellant. In the context of the use of the term "additive" in this invention, the propellant should not be considered an "additive." The propellant can be any propellant known in the art for use in aerosol sprays. Such propellants are well known to those skilled in the art. Preferably, the propellant can be selected from the group consisting of butane, propane, isobutane, and any combination thereof. In this case, a typical propellant is a mixture of butane, propane, and isobutane in a weight ratio of 74:23:3. When a propellant is present in the compositions of the present invention, it can be used in any amount sufficient to propel the composition to the desired surface relative to the other components of the composition. In particular, when the compositions of the present invention include a propellant, the amount of propellant present in the composition can be 30 wt.% or more, 35 wt.% or more, or 40 wt.% or more up to 50 wt.% or less, 60 wt.% or less, or 70 wt.% or less, based on the total weight of the composition. In this case, based on the total weight of the composition, the amount of propellant present is preferably 30 wt.% or more up to 70 wt.% or less, more preferably 35 wt.% or more up to 60 wt.% or less, and most preferably 40 wt.% or more up to 50 wt.% or less.

[0247] Carbon dioxide can be used as a substitute for the propellants listed above. Therefore, carbon dioxide can be used as a propellant in the compositions of the present invention in the amounts specified in the preceding paragraph. Alternatively, pressurized air can be used as a propellant in the compositions of the present invention, and can be used in the amounts specified in the preceding paragraph.

[0248] The compositions of the present invention can also be applied to the surface to be coated without the use of propellants or pressurized gas. For example, the composition can be applied using a spray bottle (e.g., a spray bottle equipped with a manual atomizer / sprayer / nozzle).

[0249] Besides 3D scanning technology, the optical measurement applications to which the compositions of this technology are applicable also include photogrammetry. Therefore, in one embodiment, the compositions of this technology are used in photogrammetry to, for example, prepare an object surface for photogrammetric optical measurement. The compositions of this technology can be used to improve the scanning quality and / or resolution of an object, wherein the scanning is performed using photogrammetry. The compositions of this technology can be used to improve the photogrammetric scanability of a surface (i.e., the sensitivity of the surface to allowing photogrammetric scanning). Therefore, the present invention relates to a method for improving the photogrammetric scanability of a surface, the method comprising the step of applying the compositions of this technology to a surface to be scanned by photogrammetry. The present invention also relates to a method for preparing an object surface for photogrammetric scanning measurement, the method comprising the step of applying the compositions according to this technology to the surface to be scanned. The present invention also relates to a method for realizing photogrammetric scanning of an object, the method comprising the steps of: 1) applying the compositions according to this technology to the surface of the object to be scanned, and 2) performing photogrammetric scanning measurement.

[0250] The compositions of the present invention can be used to provide a thin (e.g., 50 μm or less, 20 μm or less, 10 μm or less, or even 5 μm or less), highly uniform, scannable coating on the surface of an object, particularly to provide a surface capable of enabling accurate, high-quality, high-resolution photogrammetric scanning of the object. Therefore, the compositions of the present invention can be used in photogrammetric (scanning) applications, particularly in preparing object surfaces for photogrammetric (scanning) measurements and / or facilitating photogrammetric (scanning) measurements and / or enabling photogrammetric scanning of objects. Thus, particularly in the photogrammetric scanning of objects, the compositions of the present invention can be used to improve the scannability, scan quality, scan accuracy, and / or scan resolution of the object. "Scannability" refers to the object's ability to achieve its reliable photogrammetric scanning. The compositions can achieve this and can therefore be used to improve the diffuseness of light reflected from the object (particularly the diffuseness of light reflected from the object to be photogrammetrically measured / scanned), thereby improving scannability, scan accuracy, scan quality, and / or scan resolution. The compositions of the present invention can be further used to provide any other advantages associated with the teachings herein. For example, the compositions of the present invention can be used to prepare object surfaces for scanning measurements (especially photogrammetric (scanning) measurements). Furthermore, the compositions of the present invention can be used to provide coated surfaces that exhibit, in particular, excellent resistance to damage, adhesion to reference points required for photogrammetric (scanning) measurements by measuring devices (e.g., cameras), the ability to remove and re-adhere these reference points without significantly reducing surface quality, and / or weather resistance (e.g., durability against direct contact with running water). The compositions of the present invention can be used to prepare surfaces for photogrammetric (scanning) measurements that have been protected or coated with, for example, a film of oil or lubricant.

[0251] Therefore, the present invention also relates to a method for preparing an object surface for photogrammetric (scanning) measurement, the method comprising the step of applying any composition according to the invention to the surface to be measured / scanned. The method may further comprise the step of allowing (ii) a first solvent and (iv) a second solvent (if present) to evaporate at least partially and preferably completely to form a coating on the surface. Preferably, the coating is non-liquid and / or non-solution. Preferably, the coating forms a surface that exhibits greater opacity relative to a corresponding uncoated surface, and most preferably is opaque. Preferably, the coating is solid at room temperature. Preferably, the coating primarily comprises (i) adamantane and (iii) cyclododecane (if present) (and any other additives used in the composition), but may also include the balance of (ii) the first solvent and (iv) the second solvent (if present in the composition of the invention). Based on the total weight of the coating, the balance refers to less than 10 wt.%, more preferably less than 5 wt.%, even more preferably less than 2 wt.%, and most preferably less than 1 wt.%. Preferably, the coating is substantially free of the balance solvent. The present invention also relates to a method for photogrammetric scanning / measuring an object, the method comprising the steps described above or the step of preparing an object surface for photogrammetric scanning / measuring, and additional subsequent steps of photogrammetric scanning / measuring the object.

[0252] The compositions of the present invention can be applied to the surface to be coated by any means known and / or standard to those skilled in the art, thereby creating a surface for photogrammetric scanning / measuring. In particular, the compositions of the present invention can be applied to the respective surfaces by, for example, spraying (with or without propellant or aerosol), immersing an object or surface in the composition, or applying the composition to the surface using suitable tools known in the art (e.g., a brush).

[0253] Particularly preferred is the application of the composition of the invention to the surface to be coated by spraying. Spray coating can be performed using any standard method known in the art to apply a coating to the surface, thereby preparing a surface for photogrammetric scanning / measuring. For example, the composition can be applied using a spray gun technique or by pressurizing the composition (to the pressure standards in the art for such products) in a spray can or container used for this type of coating and using the propellant gas to carry / propel the composition to the surface to be coated as it is ejected from the spray can or container. These are methods well known to those skilled in the art. For example, spray coating can typically be performed at a distance of 30 cm (or even 15 cm to 20 cm) from the surface to be coated. The type of "spray nozzle" ("Sprühkopf") used in the spray can, spray container, or spray gun can be selected from those commonly available and used in the art and can be matched to any specific requirements of the spraying operation and / or the type of object to be sprayed. Most preferably, the spray gun or nozzle exhibits the size and performance of the spray gun or nozzle used in the experimental procedures disclosed herein. For example, the nozzle diameter of the "spray head" is 0.51 (+ / -0.02) mm, or the nozzle diameter of the spray gun is 0.8 mm. Alternatively, a "spray head" with a larger nozzle diameter (e.g., 4 mm) can be used. Preferably, the "spray head" used in the case of the invention sprays a continuous amount upon startup. Preferably, the "spray head" used in the case of the invention is compatible with both BOV and vertical valve types. In addition to those used in the experimental procedures disclosed herein, another example of a coating system suitable for applying the compositions of the invention is an aerosol can (e.g., a 400 ml aerosol can with a diameter of 65 mm and a height of 157 mm) equipped with a ball valve stem (e.g., a 4 mm diameter Ariane ball valve stem, for example) and a "spray head" with a nozzle diameter of 4 mm. The spray head can have an "insertion" caliber, can be compatible with BOV and vertical valves, and sprays a continuous amount. In this regard, where commercial product names or trademarks are used herein to describe these or any other products, the performance, size, dimensions, composition, etc. of the products shall be understood as the performance, size, dimensions, composition, etc. of the corresponding products provided under the names or trademarks as of the filing date of this application (the applicable priority date).

[0254] The compositions of this technology can be used in a variety of other applications. These applications include: providing general (temporary) marking such as on walls, baseboards, roads, pavements, sidewalks, ground, etc. (e.g., in the fields of construction, road engineering, or forensic science); temporary blocking of optical fibers; white balance adjustment in the fields of photography and film; reducing surface reflectivity, for example, in the fields of photography and film; especially as a coating in the automotive and aerospace industries to facilitate the identification of surface deformations or inconsistencies (e.g., dents) on surfaces such as metallic surfaces; as a carrier medium for (composite) lubricants and oils; in the dental industry, particularly in promoting tooth and gingival replication for potential use in the manufacture of dental restorations such as dentures, dental implants, crowns, bridges, etc.; in OMV (on-machine measurement); for (temporarily) disabling photoelectric sensors, optical / optical barriers, etc.; for preparing surfaces for dynamic measurements such as real-time deformation measurements (e.g., by laser Doppler velocimetry, Aramis, Argus, Pontus, etc.); in laser holography; as a protective coating; in the field of archaeology as a coating (for protection and for optimizing surfaces for optical measurements); and in wood restoration. Other applications include: temporarily highlighting touch / marking scratches in (sheet) metal welding (in automatic and manual marking processes), ensuring a perfect surface fit in die-spotting / blueing of (functional) surfaces, and acting as a release agent during demolding.

[0255] In the context of this invention, a compound is sublimable if, particularly at room temperature and atmospheric pressure, it transforms directly from a solid phase to a gas phase without passing through an intermediate liquid phase.

[0256] The compositions of this technology may be free of endotrimethylenenorbornene. The compositions of this technology may be free of glycol ethers. The compositions of this technology may be free of alkyl ethers of alkylene glycols, especially monoalkyl and dialkyl ethers of alkylene glycols. The compositions of this technology may and preferably are free of conventional rust inhibitors, especially morpholine, diisopropylamine, dicyclohexylamine, diisobutylamine, piperidine, propargyl alcohol, 2-butyn-1-ol, or any combination thereof. Preferably, the compositions of this technology are free of all of the above compounds.

[0257] As used herein, the term “comprising” should be understood to also encompass alternatives to the products / methods / uses in which the term “comprising” may also consist “only” of the elements described subsequently.

[0258] As used herein, the term “comprising” should be understood to also encompass the products / methods / uses in which the term “comprising” is used, or alternatives that may consist “substantially” of the elements subsequently described.

[0259] Where numerical ranges are disclosed herein, such ranges are continuous, including the maximum and minimum values ​​of the range, and every value between these maximum and minimum values. Furthermore, where the range refers to integers, it includes every integer between the minimum and maximum values ​​of the range. Additionally, where multiple ranges are provided to describe a feature or characteristic, these ranges may be combined. That is, unless otherwise stated, all ranges disclosed herein should be understood to include any and all subranges contained therein. For example, a specified range from “1 to 10” should be considered to include any and all subranges between the minimum value 1 and the maximum value 10, including the values ​​1 and 10. Exemplary subranges of the range 1 to 10 include, but are not limited to, 1 to 6.1, 3.5 to 7.8, and 5.5 to 10. It should be understood that the upper and lower limits of quantities, ranges, and ratios defined herein can be combined independently. Similarly, each element or feature of the invention taught to exist in a given range or quantity may be combined with other elements of the corresponding embodiment in the respective implementation, which also exist in the ranges or quantities taught herein for those other elements. All ranges and quantities of one element of an embodiment may be combined with all ranges and quantities of other elements in the embodiment. Therefore, a range or value taught for one element or component of the invention (e.g., a preferred, more preferred, or most preferred range or value) can be combined with any range or quantity taught for another element or component of the said embodiment, regardless of whether the range or quantity taught for that other element refers to a preferred, more preferred, or most preferred (or simply disclosed in the absence of any such designation or reference) range or quantity.

[0260] Since all figures, values, and / or expressions regarding the specified amounts of material, composition, reaction conditions, boiling points, molecular weights, number of carbon atoms, etc., used herein and in the appended claims are subject to various measurement uncertainties encountered in obtaining these values, unless otherwise stated, all of them should be understood to be modified by the term "about" in all cases. As used herein, the term "about" in conjunction with a numerical value should be understood to refer to the degree of error of an instrument commonly used by a person of ordinary skill in the art to measure the value under the circumstances of this disclosure, and more specifically, to the range of said numerical value where the identifiable function or performance is not affected, and thus the function or performance precisely exhibited at said numerical value will not differ. The term "about" in conjunction with a numerical value may refer to ±20% of the value. The term "about" in conjunction with a numerical value may refer to ±10% of the value. The term "about" in conjunction with a numerical value may refer to ±5% of the value. The term "about" in conjunction with a numerical value may refer to ±1% of the value. The term "about" in conjunction with a numerical value may refer to ±0.5% of the value.

[0261] A particularly preferred embodiment of the invention relates to a composition comprising (i) adamantane, (ii) petroleum ether 40 / 65, (iii) cyclododecane and (iv) isopropanol, wherein the weight ratio of (i):(ii):(iii):(iv) is 3.3:87.9:8.8:22.

[0262] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane, (ii) petroleum ether 40 / 65, (iii) cyclododecane and (iv) isopropanol, wherein the weight ratio of (i):(ii):(iii):(iv) is 3.3:87.9:8.8:22.

[0263] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane, (ii) petroleum ether 40 / 65, (iii) cyclododecane, (iv) isopropanol and camphor, wherein the weight ratio of (i):(ii):(iii):(iv):camphor is 3.3:87.9:8.8:22:1.1.

[0264] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane, (ii) petroleum ether 40 / 65, (iii) cyclododecane, (iv) isopropanol and camphor, wherein the weight ratio of (i):(ii):(iii):(iv):camphor is 3.3:87.9:8.8:22:1.1.

[0265] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, the first composition comprising (i) adamantane, (ii) petroleum ether 40 / 65, (iii) cyclododecane, (iv) isopropanol and camphor, wherein the weight ratio of (i):(ii):(iii):(iv):camphor is 3.3:87.9:8.8:22:1.1; wherein the weight ratio of the first composition to the propellant is 49:51 to 51:49. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3.

[0266] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, the first composition being composed of (i) adamantane, (ii) petroleum ether 40 / 65, (iii) cyclododecane, (iv) isopropanol, and camphor, wherein the weight ratio of (i):(ii):(iii):(iv):camphor is 3.3:87.9:8.8:22:1.1; wherein the weight ratio of the first composition to the propellant is 49:51 to 51:49. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3.

[0267] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane, (ii) cyclopentane, (iii) cyclododecane and (iv) ethanol in a weight ratio of (i):(ii):(iii):(iv) of 4:4:3:4.

[0268] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane, (ii) cyclopentane, (iii) cyclododecane and (iv) ethanol, wherein the weight ratio of (i):(ii):(iii):(iv) is 4:4:3:4.

[0269] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, the first composition comprising (i) adamantane, (ii) cyclopentane, (iii) cyclododecane, and (iv) ethanol in a weight ratio of (i):(ii):(iii):(iv) of 4:4:3:4; wherein the weight ratio of the first composition to the propellant is 1:1.6 to 1:1.8. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3. Alternatively, the propellant may be propane.

[0270] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, the first composition being composed of (i) adamantane, (ii) cyclopentane, (iii) cyclododecane, and (iv) ethanol in a weight ratio of (i):(ii):(iii):(iv) of 4:4:3:4; wherein the weight ratio of the first composition to the propellant is 1:1.6 to 1:1.8. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3. Alternatively, the propellant may be propane.

[0271] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane, (ii) (a) cyclopentane, (ii) (b) petroleum ether 60-95, (iii) cyclododecane and (iv) ethanol, wherein the weight ratio of (i):(ii)(a):(ii)(b):(iii):(iv) is 4:4:3:3:4.

[0272] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane, (ii) (a) cyclopentane, (ii) (b) petroleum ether 60-95, (iii) cyclododecane and (iv) ethanol, wherein the weight ratio of (i):(ii)(a):(ii)(b):(iii):(iv) is 4:4:3:3:4.

[0273] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, the first composition comprising (i) adamantane, (ii) (a) cyclopentane, (ii) (b) petroleum ether 60-95, (iii) cyclododecane, and (iv) ethanol, wherein the weight ratio of (i):(ii)(a):(ii)(b):(iii):(iv) is 4:4:3:3:4; wherein the weight ratio of the first composition to the propellant is 1:1.4 to 1:1.8. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3. Alternatively, the propellant may be propane.

[0274] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, the first composition comprising (i) adamantane, (ii) (a) cyclopentane, (ii) (b) petroleum ether 60-95, (iii) cyclododecane, and (iv) ethanol, wherein the weight ratio of (i):(ii)(a):(ii)(b):(iii):(iv) is 4:4:3:3:4; wherein the weight ratio of the first composition to the propellant is 1:1.4 to 1:1.8. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3. Alternatively, the propellant may be propane.

[0275] A particularly preferred embodiment of the invention relates to a composition comprising (i) adamantane, (ii) (a) cyclopentane, (ii) (b) petroleum ether 60-95 and (iv) ethanol, wherein the weight ratio of (i):(ii)(a):(ii)(b):(iv) is 25:93:25:42.

[0276] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane, (ii) (a) cyclopentane, (ii) (b) petroleum ether 60-95 and (iv) ethanol, wherein the weight ratio of (i):(ii) (a):(ii) (b):(iv) is 25:93:25:42.

[0277] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, the first composition comprising (i) adamantane, (ii) (a) cyclopentane, (ii) (b) petroleum ether 60-95, and (iv) ethanol, wherein the weight ratio of (i):(ii)(a):(ii)(b):(iv) is 25:93:25:42; wherein the weight ratio of the first composition to the propellant is 2.2:1 to 1.2:1. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3. Alternatively, the propellant may be propane.

[0278] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, the first composition being composed of (i) adamantane, (ii) (a) cyclopentane, (ii) (b) petroleum ether 60-95, and (iv) ethanol, wherein the weight ratio of (i):(ii)(a):(ii)(b):(iv) is 25:93:25:42; wherein the weight ratio of the first composition to the propellant is 2.2:1 to 2:1. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3. Alternatively, the propellant may be propane.

[0279] As used above, the designations (ii)(a) and (ii)(b) are used only to indicate that, in the cases where these designations are used, a solvent of a more broad definition belonging to the first solvent of (ii) of the present invention is used. These solvents are then designated (ii)(a) and (ii)(b) in turn, solely for the purpose of making the current composition as clear as possible. For example, if the composition of the present invention comprises two different solvents belonging to the more broad definition of the first solvent of (ii) used elsewhere herein (therefore designated (ii)(a) and (ii)(b)) and in that case further refers to, for example, the weight ratio of (ii) to (iv), then the combined weight of (ii)(a) and (ii)(b) will represent the total weight of (ii) used to calculate the weight ratio from (ii) to (iv).

[0280] A particularly preferred embodiment of the invention relates to a composition comprising (i) adamantane and (ii) petroleum ether 40 / 65, wherein the weight ratio of (i):(ii) is 1:9.

[0281] A particularly preferred embodiment of the present invention relates to a composition comprising (i) adamantane and (ii) petroleum ether 40 / 65, wherein the weight ratio of (i):(ii) is 1:9.

[0282] A particularly preferred embodiment of the invention relates to a composition comprising (i) adamantane and (ii) petroleum ether 40 / 65, wherein (i) adamantane is present at 6.25 wt.% based on the total weight of the composition.

[0283] A particularly preferred embodiment of the invention relates to a composition comprising (i) adamantane and (ii) petroleum ether 40 / 65, wherein (i) adamantane is present at 6.25 wt.% based on the total weight of the composition.

[0284] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, wherein the first composition comprises (i) adamantane and (ii) petroleum ether 40 / 65, wherein (i) adamantane is present at 6.25 wt.% based on the total weight of the first composition; and wherein the weight ratio of the first composition to the propellant is 49:51 to 51:49. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3.

[0285] A particularly preferred embodiment of the invention relates to a composition comprising a first composition and a propellant, wherein the first composition consists of (i) adamantane and (ii) petroleum ether 40 / 65, wherein (i) adamantane is present at 6.25 wt.% based on the total weight of the first composition; and wherein the weight ratio of the first composition to the propellant is 49:51 to 51:49. The propellant may be a mixture of butane:propane:isobutane, preferably a mixture of butane:propane:isobutane in a weight ratio of 74:23:3.

[0286] Example Unless otherwise stated, all synthesis procedures and parameter measurements should be understood as being performed at room temperature / ambient temperature (i.e., 21 ± 1 °C) and atmospheric pressure. Unless otherwise stated, all reagents are laboratory grade.

[0287] The embodiments described below are for illustrative purposes only and are not intended to limit the scope of the invention as claimed and described elsewhere herein.

[0288] The following mixtures (mixtures 1 to 3) according to the invention are prepared by adding adamantane, along with CCD and camphor (if present) in specified amounts to a solvent (petroleum ether (“Wundbenzin” 40 / 65 and isopropanol (if present)) and mixing / stirring together at room temperature to form a solution. The resulting solution is filtered through a high-density filter (paper funnel with nylon insert, 125µm; available from carparts GmbH, Cologne, Germany, product name Car System Multi-stretch Farbsieb VE 125µm; product number V146957-VE) to form the final mixtures 1 to 3.

[0289]

[0290] Example 1 Using standard industrial equipment and techniques for filling aerosol cans (aerosol cans filled by Pamasol-Swiss-Aerosol-Solutions, Switzerland), Mixture 1 is pumped into a 400ml industrial standard aerosol can (65mm diameter, 157mm height, 400ml filling volume, 520ml full volume, 15bar, cylindrical can, available from G. Staehle GmbH u.Co. KG, Germany). The aerosol can is then weighed to determine the amount of Mixture 1 contained within, before the valve is installed, crimped, and sealed according to standard procedures. The aerosol can is then pressurized with a liquid propellant (butane:propane:isobutane, 74:23:3), and the final weight of the aerosol can is measured to determine the amount of propellant contained. Finally, a nozzle (“Sprühkopf”) (nozzle diameter 0.51 (+ / -0.02) mm; available from Deutsche Präzisions-Ventil GmbH, Germany) is installed on the aerosol can to activate the valve, thereby spraying the composition upon pressing. The final composition of Example 1 consisted of 87.9 g of petroleum ether 40 / 65, 22 g of isopropanol, 8.8 g of cyclododecane, 3.3 g of adamantane, 1.1 g of camphor, and 122.3 g of propellant.

[0291] Example 2 Using standard industrial equipment and techniques for filling aerosol cans (aerosol cans filled by Pamasol-Swiss-Aerosol-Solutions of Switzerland), Mixture 2 is pumped into a 400ml industrial standard aerosol can (65mm diameter, 157mm height, filling volume 400ml, full volume 520ml, 15bar, cylindrical can, available from G.Staehle GmbH u.Co. KG of Germany). The aerosol can is then weighed to determine the amount of Mixture 2 contained within, before the valve is installed, crimped, and sealed according to standard procedures. The aerosol can is then pressurized with a liquid propellant (butane:propane:isobutane 74:23:3), and the final weight of the aerosol can is measured to determine the amount of propellant contained. Finally, the necessary nozzle (“Sprühkopf”) (nozzle diameter 0.51 (+ / -0.02) mm; available from Deutsche Präzisions-Ventil GmbH, Germany) is installed on the aerosol can to activate the valve, thereby spraying the composition upon pressing. The final composition of Example 2 consisted of 120 g of petroleum ether 40 / 65, 8 g of adamantane, and 122.3 g of propellant.

[0292] Example 3 The mixture 3 prepared as described above is transferred to a plastic container that can be fitted with a spray gun so that the mixture can be subsequently applied to the object to be coated.

[0293] Comparative Examples 1-3 The embodiments of the present invention were tested against a series of prior art, commercial and non-prior art products. Comparative Example 1 (a non-prior art product) was a petroleum ether 40 / 65 (73 g) solution of cyclododecane (4.6 g), pressurized in an aerosol spray can using 64.5 g of propellant (following the pressurization and aerosol can preparation processes of Examples 1 and 2 above). Comparative Example 2 was a commercially available aerosol cyclododecane spray, available from Deffner & Johann GmbH, Germany, under the product name "Cyclododecan Spray" (product number: 2062 400). According to available data, this product contains 25% to less than 50% by weight of cyclododecane, 25% to less than 50% by weight of propane, 25% to less than 50% by weight of butane, and 10% to less than 12.5% ​​by weight of isobutane, and is used as a pressurized aerosol spray in a standard 400 ml spray can. Comparative Example 3 is a commercially available TiO2-containing pigment-based aerosol spray for 3D scanning manufactured by Helling GmbH in Germany. The product name is "3-D Laserscanning Entspiegelungsspray" (product number: 119.990.001; 119.990.004), which also contains isopropanol and n-butane, propane and isobutane propellants.

[0294] Apply coating The compositions of each of Examples 1-3 and Comparative Examples 1-3 were applied manually to the test substrate (a transparent and colorless solid glass sphere with a diameter of 127.1 mm) from a distance of approximately 300 mm, using a single, uniform coating. In each of the following Tests 1-3, the necessary adhesive reference points (3 mm in diameter) provided by the scanner manufacturer were applied to the test substrate according to the scanner manufacturer's instructions before applying the coating. Spraying was stopped when the glass surface of the sphere was no longer visible.

[0295] In Examples 1 and 2 and Comparative Examples 1 to 3, this includes simply spraying the composition from the respective spray can by pressing the nozzle (thus opening the valve) and applying the coating to the glass sphere as described above.

[0296] In Example 3, the composition does not contain a propellant, so a spray gun (Tectake HVLPLackierpistole, available from Tectake GmbH, Germany; air pressure 1.5 bar, nozzle diameter 0.8 mm) is used to spray the composition onto the glass sphere.

[0297] test The following tests were then performed on each coated glass sphere: 1) whether the coating formed a scannable surface; 2) the quality of the formed coating surface; 3) damage resistance; 4) the adhesion of reference points / spots to the coating; 5) the ability to remove reference points / spots without negatively impacting surface quality; 6) the ability to re-adhere reference points / spots after removal; 7) coating residence time; 8) coating formation on oily surfaces; and 9) the coating's resistance to water flow. Each of these properties was measured according to the following test procedure: 1) Scannability In this test, the ability of the coated surface to enable the scanner to perform 3D scanning of the test object was evaluated. The scanner used was an ATOS Triple Scan 16M Plus 29M / SO (available from GOM GmbH, Germany), installed within a Scanbox 5120 (also available from GOM GmbH, Germany), and scanning was performed according to the instructions and workflow specified by the scanner manufacturer in the scanner software (ATOS Professional 2018, Hotfix 1, Rev. 111729, build 2018-08-22). In this case, the scanner was calibrated before any scanning measurements were performed. Calibration scans were performed according to the calibration scheme specified in the aforementioned software, using the ATOS Triple Scan 16 M Plus 29M / SO sensor and a measurement cavity (“Messvolumen”) of MV170 (170mm × 130mm × 130mm). The calibration object was a calibration plate (Triple Scan; CP40-170-41739s). The number of calibration points was 3657, and the calibration temperature was 23.2℃. The following calibration settings were applied: camera lens 50.00mm, focal length (projector) 60.00mm, recording mode multi-recording mode ("Mehrfachaufnahme"), and Eclipse quality 0.4.

[0298] The coated object (coated glass sphere) to be scanned is prepared as described above, and the scanner is positioned directly in front of the specific sphere to be measured. By aligning the scanner's focal point with the center of the sphere to be scanned, the sphere is ensured to be precisely positioned in the center of the scanner's measurement cavity.

[0299] Then, scan the corresponding sphere according to the scheme specified in the scanner software. After a successful scan, reposition the scanner at a different angle to cover new areas of the sphere's surface. Then scan again. Repeat this process until the entire surface of the sphere has been scanned. Use the scanner software to process the scan data.

[0300] In the table below, "Yes" means the scanner can perform 3D scanning of the coated object. "Barely" means it can scan less than 50% of the surface.

[0301] 2) Surface quality The quality of the coating surface is reflected by thickness, smoothness, and uniformity. The coating thickness was determined using the Alicona G5 surface characterization device (available from Alicona Imaging GmbH, Germany; product number: A201015018, Alicona IF-frame SN: 076201502516, Alicona IF-SensorC100 Instrument G1Vb4 SN: 074201502516, Alicona IF-C100 ElectronicsUnit Va2 SN: 081027011915; Software-MeasureSuite 5.3.1), and the coating thickness for each embodiment is recorded in the table below. The same Alicona G5 device and software were used to visually represent the coating surface, allowing for the evaluation of surface uniformity and smoothness. Figures 1 to 6 The visual representation of the coated surface for each embodiment is described and summarized in the table below. A rating of 1 (excellent uniformity) to 5 (very poor uniformity) is given based on the observed degree of uniformity.

[0302] 3) Damage resistance Glass spheres coated with the corresponding compositions of Examples 1-3 and Comparative Examples 1-3 were prepared as described above and placed on a flat surface. Each sphere was then lifted off the surface by grasping it with the fingers of one hand and held for 5 seconds. The sphere was then placed back on the surface and released. Each sphere was then visually inspected and given a "rating" of 1 to 5 based on the damage to the surface coating relative to its initial post-coating state.

[0303] Rating: 1 = No stains on the coating during processing, and no further processing is required before scanning; 3 = Some stains during processing, but the coating remains intact to some extent; 5 = The coating is immediately soiled / removed during processing, and the surface quality is compromised.

[0304] 4) Adhesion of reference point / spot As described above, a coating of each corresponding composition was applied to a glass sphere, except that a reference point was not applied to the sphere before applying the coating composition. Instead, after the composition was applied and allowed to dry to form the desired coating, a reference point was applied to the coating surface. The applied reference point was then observed for 30 minutes, and any changes in the initial adhesion / initial adhesion quality of the reference point to the coating surface and the degree of adhesion over time were recorded.

[0305] Rating: 1 = The reference point adheres very well to the coated surface and remains adhered until actively removed; 2 = The reference point adheres well to the coated surface; 3 = The reference point exhibits average adhesion to the coated surface; 4 = The reference point shows minimal adhesion to the coated surface and detaches after a short time without further interference; 5 = The reference point does not adhere to the coated surface at all.

[0306] 5) The impact of removing reference points / spots on surface quality As described in test 4) above, apply reference points to the surface of the coated glass sphere. Then manually remove these reference points, being careful not to damage the surface coating with your hands. Visually inspect the surface area of ​​the coating with the reference points removed and assign a "rating" of 1 to 5 to reflect the quality of the remaining coating.

[0307] score: 1. The quality of the coated surface showed no significant deterioration; 5 = The quality of the coated surface is significantly impaired when the reference point is removed.

[0308] 6) Re-adhesion ability of reference point / spot The reference point application and removal process is performed according to tests 4) and 5) above. The removed reference points are then reapplied to the coated surface where they have been removed, and the adhesion of these reference points is tested according to the process outlined in test 4) above.

[0309] score: 1= After reapplication, the reference point adheres very well to the coated surface and remains adhered until it is actively removed; 2= ​​After reapplication, the reference point adheres well to the coated surface; 3= After reapplication, the adhesion of the reference point to the coated surface is generally poor; 4= After reapplication, the reference point showed the least adhesion to the coated surface and detached after a short time without further interference; 5= After reapplying, the reference point cannot adhere to the coated surface at all.

[0310] 7) Duration of stay After coating the glass spheres with the corresponding compositions outlined above, the time required for sufficient coating to remain on the surface to allow for successful scanning measurements according to the scanning procedure described above was determined. The results for each composition are listed in the table below. In this regard, "shorter" results correspond to residence times of less than 45 minutes, "medium" results correspond to residence times of 45 minutes to 24 hours or less, and "longer" results correspond to residence times of more than 24 hours.

[0311] 8) In Forming a coating on an oily surface The coating of the corresponding composition was applied to the metal (steel) gear with the lubricating oil protective coating in the manner described above for the glass sphere, and scanning measurements were performed according to the scheme of Test 1 outlined above.

[0312] In the table below, a "good" result means that a coating of sufficient quality to achieve a high-quality scan was formed, and that the coating subsequently sublimated to keep the underlying protective oil layer intact. A "medium" result means that a coating of sufficient quality to achieve a high-quality scan was formed, but after sublimation, the underlying protective oil layer was no longer intact and had to be recoated. A "poor" result means that a coating of sufficient quality to achieve a high-quality scan could not be formed.

[0313] 9) Water resistance of the coating Glass spheres coated with each corresponding composition were prepared as described above. The coated spheres were then held under a running tap of cold water, allowing the water to flow over the coated surface for 10 seconds. The spheres were then removed from the water flow path and allowed to air dry for 20 seconds. The coated surface was then visually evaluated to determine if the coating was damaged.

[0314] Ratings (see table below): Yes = It has water resistance (the coating quality is still sufficient to achieve high-quality scanning of the coated object according to the process outlined in Experiment 1).

[0315] No = No water resistance (the coating quality is no longer sufficient to achieve high-quality scanning of the coated object according to the process outlined in Experiment 1).

[0316]

[0317] A coating can be formed on it, but the surface coating coverage is very poor. The surface portion has good uniformity (see...). Figure 4 ) These figures were generated by the aforementioned scanner software (described in Test 2 above; Alicona G5 surface characterization device; Software-MeasureSuite 5.3.1), and in particular show the surface quality (including smoothness and uniformity) obtained when glass spheres were coated with the corresponding compositions of Examples 1-3 and Comparative Examples 1-3 according to the coating process outlined above.

[0318] 1. A composition comprising: (i) adamantane; and (ii) a first solvent, wherein the first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point of 25°C or higher at atmospheric pressure, the boiling point range having a minimum boiling point of 25°C or higher at atmospheric pressure; and optionally... (iii) Cyclododecane; and / or optionally (iv) A second solvent, which is different from the first solvent.

[0319] 2. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 25°C or above, 30°C or above, 35°C or above, or 40°C or above to 50°C or below, 60°C or below, 65°C or below, 70°C or below, 75°C or below, 80°C or below, 90°C or below, 100°C or below, 110°C or below, 120°C or below, or 130°C or below at atmospheric pressure.

[0320] 3. The composition according to 1 or 2, wherein the first solvent is selected from the group consisting of pentane, cyclopentane, hexane, cyclohexane, heptane, cycloheptane, octane, petroleum ether, petroleum ether 30-40, petroleum ether 40-60, petroleum ether 40-65, petroleum ether 60-80, petroleum ether 80-100, and any combination thereof.

[0321] 4. The composition according to any one of 1 to 3, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 0.5 wt.% or more, 1.0 wt.% or more, 1.5 wt.% or more, 2.5 wt.% or more, 3 wt.% or more, 5 wt.% or more, or 6 wt.% or more to 10 wt.% or less, 11 wt.% or less, 12 wt.% or less, 15 wt.% or less, 20 wt.% or less, 30 wt.% or less, 50 wt.% or less; preferably, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 1.5 wt.% or more to 20 wt.% or less based on the total weight of components (i) to (iv); more preferably, wherein the total combined amount of (i) adamantane and (iii) cyclododecane (if present) is 3 wt.% or more to 12 wt.% or less based on the total weight of components (i) to (iv).

[0322] 5. The composition according to any one of 1 to 4, wherein the weight ratio of adamantane to cyclododecane is 100:0, 95:5, 90:10, 80:20, 3:1, 2.7:1, 60:40 or 51:49 to 49:51, 40:60, 1:2.7, 1:3, 20:80, 10:90, 5:95 or 1:99; more preferably, wherein the weight ratio of adamantane to cyclododecane is 100:0 to 10:90; even more preferably, wherein the weight ratio of adamantane to cyclododecane is 100:0 to 20:80; most preferably, wherein the weight ratio of adamantane to cyclododecane is 100:0 to 1:2.7.

[0323] 6. The composition according to any one of 1 to 5, wherein the composition does not contain any (iii) cyclododecane; preferably, the composition does not contain any (iii) cyclododecane, nor does it contain (iv) a second solvent.

[0324] 7. The composition according to any one of 1 to 5, wherein the composition comprises (iii) cyclododecane; preferably, wherein the total combined amount of (i) adamantane and (iii) cyclododecane is 9.0 wt.% or more to 11.0 wt.% or less, more preferably 9.5 wt.% or more to 10.5 wt.% or less, based on the total weight of components (i) to (iv).

[0325] 8. The composition according to any one of 1 to 5 or 7, wherein the weight ratio of adamantane to cyclododecane is 95:5 to 5:95, especially 90:10 to 10:90, preferably 80:20 to 20:80, and most preferably 2.7:1 to 1:2.7.

[0326] 9. The composition according to any one of 1 to 8, wherein the composition comprises (iv) a second solvent different from the first solvent; preferably, wherein the second solvent is more polar than the first solvent; more preferably, wherein the second solvent is more polar than the first solvent, and the second solvent has a boiling point or boiling point range at atmospheric pressure of 40°C or above, 50°C or above, 60°C or above, 64.7°C or above, 70°C or above, 75°C or above, 80°C or above, or 82°C or above to 90°C or below, 100°C or below, 110°C or below, 120°C or below, 130°C or below, 140°C or below, 150°C or below, or 160°C or below.

[0327] 10. The composition according to any one of 1 to 9, wherein the second solvent is one or more alcohols; preferably, wherein the second solvent is one or more alcohols selected from the group consisting of C1 to C8 alcohols, particularly selected from the group consisting of C1 to C8 monohydric alcohols; more preferably, wherein the second solvent is one or more alcohols selected from the group consisting of C1 to C8 alkanols and C3 to C8 cycloalkanols; most preferably, wherein the second solvent is selected from methanol, ethanol, n-propanol, isopropanol, cyclopropanol, n-butanol, sec-butanol, isobutanol, tert-butanol, cyclobutanol, n-pentanol, 3-methylbut-1-ol, 2-methylbut-1-ol, 2,2-dimethylprop-1-ol, pent-3-ol, The group consisting of pentyl-2-ol, 3-methylbut-2-ol, 2-methylbut-2-ol, cyclopentanol, hex-1-ol, hex-2-ol, hex-3-ol, 2-methylpentyl-1-ol, 3-methylpentyl-1-ol, 4-methylpentyl-1-ol, 2-methylpentyl-2-ol, 3-methylpentyl-2-ol, 4-methylpentyl-2-ol, 2-methylpentyl-3-ol, 3-methylpentyl-3-ol, 2,2-dimethylbut-1-ol, 2,3-dimethylbut-1-ol, 3,3-dimethylbut-1-ol, 2,3-dimethylbut-2-ol, 3,3-dimethylbut-2-ol, 2-ethylbut-1-ol, cyclohexanol, 2-heptanol, 3-heptanol, 4-heptanol, and any combination thereof.

[0328] 11. The composition according to any one of 1 to 10, wherein the weight ratio of the first solvent to the second solvent (iv) is 99:1, 95:5, 90:10, 80:20, 70:30, 2:1, 60:40, or 55:45 to 45:55, 40:60, 1:2, 30:70, 20:80, 10:90, 5:95, or 1:99; in particular, wherein the weight ratio of the first solvent to the second solvent (iv) is 90:10 to 10:90; preferably, wherein the weight ratio of the first solvent to the second solvent (iv) is 80:20 to 20:80.

[0329] 12. The composition according to any one of 1 to 11, wherein the composition further comprises one or more additives, particularly one or more additives selected from camphor, menthol and combinations thereof, wherein the content of the additives is preferably 0.1 wt.% or more to 5 wt.% or less, more preferably 0.25 wt.% or more to 2.5 wt.% or less, and most preferably 0.5 wt.% or more to 1.5 wt.% or less or 1.0 wt.% or less, based on the total combined weight of the additives and each of components (i) to (iv).

[0330] 13. The composition according to any one of 1 to 12, wherein the composition further comprises a propellant; in particular, wherein the amount of the propellant present, based on the total weight of the composition, is 20 wt.% or more to 80 wt.% or less, preferably 30 wt.% or more to 70 wt.% or less, more preferably 35 wt.% or more to 60 wt.% or less, and most preferably 40 wt.% or more to 50 wt.% or less.

[0331] 14. Use of the composition according to any one of 1 to 13 in 3D scanning applications.

[0332] 15. A method for performing 3D scanning of an object, the method comprising the steps of: 1) applying a composition according to any one of 1 to 13 to the surface of the object to be scanned, and 2) performing 3D scanning measurements.

Claims

1. A composition comprising: (i) adamantane; as well as (ii) A first solvent, wherein the first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point of 25°C or above at atmospheric pressure, the boiling point range having a minimum boiling point of 25°C or above at atmospheric pressure; (iii) Optionally includes cyclododecane; Also includes: (iv) A second solvent, which is different from the first solvent, and is selected from methanol, ethanol, n-propanol, isopropanol, cyclopropanol, n-butanol, sec-butanol, isobutanol, cyclobutanol, n-pentanol, 3-methylbut-1-ol, 2-methylbut-1-ol, 2,2-dimethylprop-1-ol, pent-3-ol, pent-2-ol, 3-methylbut-2-ol, 2-methylbut-2-ol, cyclopentanol, hex-1-ol, hex-2-ol, hex-3-ol, 2-methylpentanol, 3-methyl The group consisting of pentyl-1-ol, 4-methylpentyl-1-ol, 2-methylpentyl-2-ol, 3-methylpentyl-2-ol, 4-methylpentyl-2-ol, 2-methylpentyl-3-ol, 3-methylpentyl-3-ol, 2,2-dimethylbut-1-ol, 2,3-dimethylbut-1-ol, 3,3-dimethylbut-1-ol, 2,3-dimethylbut-2-ol, 3,3-dimethylbut-2-ol, 2-ethylbut-1-ol, cyclohexanol, 2-heptanol, 3-heptanol, 4-heptanol, and any combination thereof; and / or (v) Propellant; Based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is greater than 0.5 wt% to less than 50 wt%.

2. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 25°C to 130°C at atmospheric pressure.

3. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 30°C to 120°C at atmospheric pressure.

4. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 30°C to 110°C at atmospheric pressure.

5. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 30°C to 100°C at atmospheric pressure.

6. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 45°C to 100°C at atmospheric pressure.

7. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 50°C to 100°C at atmospheric pressure.

8. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 60°C to 95°C at atmospheric pressure.

9. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 30°C to 90°C at atmospheric pressure.

10. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 30°C to 80°C at atmospheric pressure.

11. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 35°C to 75°C at atmospheric pressure.

12. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 35°C to 70°C at atmospheric pressure.

13. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 35°C to 65°C at atmospheric pressure.

14. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 40°C to 65°C at atmospheric pressure.

15. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 40°C to 60°C at atmospheric pressure.

16. The composition according to claim 1, wherein the first solvent has a boiling point or boiling point range of 40°C to 50°C at atmospheric pressure.

17. The composition according to claim 1, wherein the first solvent is selected from the group consisting of pentane, cyclopentane, hexane, cyclohexane, heptane, cycloheptane, octane, petroleum ether, and any combination thereof.

18. The composition according to claim 17, wherein the petroleum ether is petroleum ether 30-40, petroleum ether 40-60, petroleum ether 40-65, petroleum ether 60-80, or petroleum ether 80-100.

19. The composition according to claim 1, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is greater than 1.0 wt% to less than 30 wt%.

20. The composition according to claim 1, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is greater than 1.5 wt% to less than 20 wt%.

21. The composition according to claim 1, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is greater than 2.5 wt% to less than 15 wt%.

22. The composition according to claim 1, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is greater than 3 wt% to less than 12 wt%.

23. The composition according to claim 1, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is greater than 5 wt% to less than 11 wt%.

24. The composition according to claim 1, wherein, based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is greater than 6 wt% to less than 10 wt%.

25. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 100:0 to 1:

99.

26. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 5:

95.

27. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 100:0 to 10:

90.

28. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 20:

80.

29. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 25:

75.

30. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 1:2.

7.

31. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 40:

60.

32. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is from 100:0 to 49:

51.

33. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 95:5 to 5:

95.

34. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 90:10 to 10:

90.

35. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 80:20 to 20:

80.

36. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 75:25 to 25:

75.

37. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 2.7:1 to 1:2.

7.

38. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 60:40 to 40:

60.

39. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 51:49 to 49:

51.

40. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 1.5:1 to 1:

1.

41. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 1.5:1 to 1.25:

1.

42. The composition according to any one of claims 1-24, wherein the weight ratio of adamantane to cyclododecane is 1.4:1 to 1.3:

1.

43. The composition according to any one of claims 1-24, wherein the composition does not contain any (iii) cyclododecane.

44. The composition according to any one of claims 1-24, wherein the composition does not contain any (iii) cyclododecane, nor does it contain (iv) a second solvent.

45. The composition according to any one of claims 1-18, wherein the composition comprises (iii) cyclododecane; wherein the total combined amount of (i) adamantane and (iii) cyclododecane is greater than 9.0 wt% and less than 11.0 wt% based on the total weight of components (i) to (iv).

46. ​​The composition according to any one of claims 1-18, wherein the composition comprises (iii) cyclododecane; wherein the total combined amount of (i) adamantane and (iii) cyclododecane is greater than 9.5 wt% and less than 10.5 wt% based on the total weight of components (i) to (iv).

47. The composition according to any one of claims 1-24, wherein the second solvent is more polar than the first solvent.

48. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 40°C to 160°C at atmospheric pressure.

49. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 50°C to 150°C at atmospheric pressure.

50. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 60°C to 140°C at atmospheric pressure.

51. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 64.7°C to 130°C at atmospheric pressure.

52. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 70°C to 120°C at atmospheric pressure.

53. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 75°C to 110°C at atmospheric pressure.

54. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 80°C to 100°C at atmospheric pressure.

55. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 82°C to 90°C at atmospheric pressure.

56. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 64.7°C to 100°C at atmospheric pressure.

57. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 70°C to 90°C at atmospheric pressure.

58. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 75°C to 90°C at atmospheric pressure.

59. The composition according to any one of claims 1-24, wherein the second solvent has a boiling point or boiling point range of 75°C to 85°C at atmospheric pressure.

60. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 99:1 to 1:

99.

61. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 95:5 to 5:

95.

62. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 90:10 to 10:

90.

63. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 80:20 to 20:

80.

64. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 3:1 to 1:

3.

65. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 70:30 to 30:

70.

66. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 2:1 to 1:

2.

67. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 60:40 to 40:

60.

68. The composition according to any one of claims 1-24, wherein the weight ratio of the first solvent to the second solvent (iv) is 45:55 to 55:

45.

69. The composition according to any one of claims 1-24, wherein the composition further comprises one or more additives selected from camphor, menthol, and combinations thereof.

70. The composition according to claim 69, wherein the content of the additive is from 0.1 wt% to 5 wt% based on the total combined weight of the additive and each of components (i) to (iv).

71. The composition according to claim 69, wherein the content of the additive is from 0.25 wt% to 2.5 wt% based on the total combined weight of the additive and each of components (i) to (iv).

72. The composition according to claim 69, wherein the content of the additive is from 0.5 wt% to 1.5 wt% based on the total combined weight of the additive and each of components (i) to (iv).

73. The composition according to claim 69, wherein the content of the additive is from 0.5 wt% to 1.0 wt% based on the total combined weight of the additive and each of components (i) to (iv).

74. The composition according to any one of claims 1-24, wherein the amount of propellant present is from 20 wt% to 80 wt% based on the total weight of the composition.

75. The composition according to any one of claims 1-24, wherein the amount of propellant present is from 30 wt% to 70 wt% based on the total weight of the composition.

76. The composition according to any one of claims 1-24, wherein the propellant is present in an amount of 35 wt% to 60 wt% based on the total weight of the composition.

77. The composition according to any one of claims 1-24, wherein the propellant is present in an amount of 40 wt% to 50 wt% based on the total weight of the composition.

78. Use of the composition according to any one of claims 1-77 in optical measurement technology applications.

79. Use of the composition according to any one of claims 1-77 in 3D scanning applications.

80. A method of implementing a 3D scan of an object, the method comprising the steps of: 1) Applying the composition according to any one of claims 1 to 77 to the surface of the object to be scanned, and 2) Performing 3D scanning measurements.

81. The use of the composition of any one of claims 1 to 77, or a composition comprising any of the following, for providing a temporary label: (i) adamantane; and (ii) a first solvent, wherein the first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point of 25°C or higher at atmospheric pressure, the boiling point range having a minimum boiling point of 25°C or higher at atmospheric pressure; and optionally... (iii) Cyclododecane; and / or (iv) A second solvent, which is different from the first solvent; Based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is 0.5 wt% to 50 wt%.

82. A method for performing 3D scanning or photogrammetric scanning of an object, the method comprising the following steps: 1) Apply the composition to the surface of the object to be scanned, and 2) Perform 3D scanning measurement or photogrammetry. The composition is the composition according to any one of claims 1 to 77 or a composition comprising the following: i) adamantane; and (ii) a first solvent, wherein the first solvent is a hydrocarbon or a mixture of hydrocarbons having a boiling point of 25°C or higher at atmospheric pressure, the boiling point range having a minimum boiling point of 25°C or higher at atmospheric pressure; and optionally... (iii) Cyclododecane; and / or (iv) A second solvent, which is different from the first solvent; Based on the total weight of components (i) to (iv), the total combined amount of (i) adamantane and (iii) cyclododecane, if present, is 0.5 wt% to 50 wt%.

Citation Information

Patent Citations

  • Use of a means for the reversible, volatile matting or proofing of optically difficult or impossible-to-measure objects

    DE102017010280A1