A wetting agent for oil-based drilling fluid, and a preparation method and application thereof

By compounding N,N′-bis(alkyl)-acyldiamine diacetic acid, alkanolamide-terminated polyoxyethylene ether, and fatty acid wetting agents, the problem of wetting agent failure in oil-based drilling fluids at high temperatures was solved, achieving good wetting properties and temperature resistance, and improving the stability and demulsification voltage of the drilling fluid.

CN118879287BActive Publication Date: 2026-11-20JINGZHOU XUECHENG IND CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202410902945.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-07-08
Publication Date
2026-11-20
Estimated Expiration
2044-07-08

AI Technical Summary

Technical Problem

Existing oil-based drilling fluid wetting agents are prone to failure at high temperatures, leading to a decrease in drilling fluid demulsification voltage and poor wettability, thus affecting the stability of the drilling fluid.

Method used

A compound wetting agent consisting of N,N′-bis(alkyl)acyldiamine diacetic acid, alkanolamide-terminated polyoxyethylene ether, and fatty acids is used. Through the unique twin structure and the synergistic effect of multiple polar groups, the adsorption strength and emulsification performance of the wetting agent at high temperatures are improved.

Benefits of technology

At 150℃, 180℃, and 210℃, the wetting agent exhibited good wetting and temperature resistance, improved the stability and demulsification voltage of the drilling fluid, reduced water loss under high temperature and high pressure, and enhanced the high temperature resistance of oil-based drilling fluids.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004931494980000101
    Figure BDA0004931494980000101
  • Figure BDA0004931494980000111
    Figure BDA0004931494980000111
  • Figure BDA0004931494980000112
    Figure BDA0004931494980000112
Patent Text Reader

Abstract

The application provides a wetting agent for oil-based drilling fluid and a preparation method and application thereof, and particularly relates to the technical field of drilling fluid. The wetting agent for oil-based drilling fluid provided by the application comprises, in mass parts, 25-45 parts of N,N'-dihydrocarbylacyl diamine diacetic acid, 25-55 parts of alkylol amide-terminated polyoxyethylene ether and 15-45 parts of fatty acid; the number of C atoms of the hydrocarbyl in the N,N'-dihydrocarbylacyl diamine diacetic acid is 18-46; and the number of ethylene oxide polymerization monomers in the alkylol amide-terminated polyoxyethylene ether is 2-6. The wetting agent provided by the application contains strong polar groups, gemini structures and multiple hydrophilic polar groups in one molecule, and these polar groups and special structures can be firmly adsorbed on the surface of cuttings and barite; meanwhile, multiple surfactants synergistically act, so that the wetting agent is more firmly adsorbed, can be better wetted and is not easy to desorb at high temperatures.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of drilling fluid technology, specifically relating to a wetting agent for oil-based drilling fluid, its preparation method, and its application. Background Technology

[0002] Compared to water-based drilling fluids, oil-based drilling fluids typically have lower shear stress. Therefore, when hydrophilic drill cuttings and barite, among other solid particles, are present in oil-based drilling fluids, sedimentation can occur, compromising the fluid's stability. To prevent sedimentation, wetting agents are added to oil-based drilling fluids. Wetting agents are surfactants with an amphiphilic structure; the hydrophilic end of the wetting agent molecule has a strong affinity and can bind to solid surfaces. When a wetting agent molecule binds to a solid surface, it directs its oleophilic end towards the oil phase, transforming the originally hydrophilic solid surface into an oleophilic one—a process known as wetting reversal. With the increasing popularity of oil-based drilling fluids, especially in high-density systems, the use of wetting agents is becoming more frequent and in larger quantities, playing an increasingly important role.

[0003] Currently, there are various wetting agents on the market, most of which use oleic acid, Span, alkyl polyethers, etc. However, certain problems have occurred during their use, especially at high temperatures, such as wetting failure, large drop in drilling fluid demulsification voltage after addition, and weak wetting. Summary of the Invention

[0004] In view of this, the purpose of this invention is to provide a wetting agent for oil-based drilling fluids, its preparation method, and its application. The oil-based drilling fluid provided by this invention has high temperature resistance, good wetting effect, and minimal impact on drilling fluid performance.

[0005] To solve the above-mentioned technical problems, the present invention provides the following technical solution:

[0006] This invention provides a wetting agent for oil-based drilling fluids, comprising, by weight parts, 25-45 parts of N,N′-bis(alkyl)acyldiamine diacetic acid, 25-55 parts of alkanolamide-terminated polyoxyethylene ether, and 15-45 parts of fatty acid;

[0007] The N,N′-bis(alkyl)acyldiamine diacetic acid has 18 to 46 carbon atoms in its hydrocarbon group;

[0008] The number of ethylene oxide monomers in the alkanolamide-terminated polyoxyethylene ether is 2 to 6.

[0009] Preferably, the N,N′-bis(alkyl)acyldiamine diacetic acid is one or more of the following: N,N′-bispalmitoylethylenediamine diacetic acid, N,N′-bislauroylethylenediamine diacetic acid, N,N′-bisoleylethylenediamine diacetic acid, N,N′-bistalloylethylenediamine diacetic acid, N,N′-bispalmitoylpropylenediamine diacetic acid, N,N′-bisoleylpropylenediamine diacetic acid, N,N′-bistalloylpropylenediamine diacetic acid, N,N′-bispalmitoylbutyldiamine diacetic acid, N,N′-bislauroylbutyldiamine diacetic acid, N,N′-bisoleylbutyldiamine diacetic acid, and N,N′-bistalloylbutyldiamine diacetic acid.

[0010] Preferably, the preparation method of the N,N′-bis(alkyl)acyldiamine diacetic acid includes the following steps:

[0011] By mass, 35-65 parts of diamine and 55-65 parts of water are mixed, and 25-55 parts of chloroacetic acid aqueous solution are added to the resulting mixture. The mixture is heated, and the pH of the heating system is adjusted to 9-11 to produce an acid-base reaction, thereby obtaining diamine diacetic acid.

[0012] The diamine diacetic acid, 25-55 parts of hydrocarbon acyl chloride, and 1-3 parts of the first catalyst are mixed and subjected to an amidation reaction to obtain N,N′-bis-hydrocarbonyl diamine diacetic acid.

[0013] Preferably, the first catalyst is an alkaline solution, wherein the alkali in the alkaline solution is sodium hydroxide and / or potassium hydroxide; and the concentration of the alkaline solution is 15-25 wt%.

[0014] Preferably, the method for preparing the alkanolamide-terminated polyoxyethylene ether includes the following steps:

[0015] By mass, 10-20 parts of diethanolamine and 0.2-1.2 parts of a second catalyst are mixed and heated. 3-12 parts of ethylene oxide are added to the resulting hot mixture to carry out a polycondensation reaction. 85-97 parts of an alkanolamide capping agent are added to the resulting polycondensation product to carry out a capping reaction. The pH of the resulting capping product is adjusted to 6-7 to obtain an alkanolamide-capped polyoxyethylene ether.

[0016] Preferably, the alkanolamide-terminated polyoxyethylene ether contains one or two of the following: coconut oil diethanolamide 6501, coconut oil diethanolamide 6502, coconut oil diethanolamide 6503, and oleic acid diethanolamide.

[0017] Preferably, the second catalyst is an alkaline solution, wherein the alkali in the alkaline solution is sodium hydroxide and / or potassium hydroxide; and the concentration of the alkaline solution is 15-25 wt%.

[0018] Preferably, the fatty acid includes one of tall oleic acid, soybean oleic acid, and coconut oleic acid.

[0019] The present invention also provides a method for preparing the wetting agent for oil-based drilling fluid described in the above technical solution, comprising the following steps;

[0020] By weight, 25-45 parts of N,N′-bis(alkyl)acyldiamine diacetic acid, 25-55 parts of alkanolamide-terminated polyoxyethylene ether, and 15-45 parts of fatty acid are mixed and heated to obtain the oil-based drilling fluid wetting agent.

[0021] The present invention also provides the application of the wetting agent for oil-based drilling fluid described in the above technical solution or the wetting agent for oil-based drilling fluid prepared by the preparation method described in the above solution in oil-based drilling fluid.

[0022] This invention provides a wetting agent for oil-based drilling fluids, comprising, by weight, 25-45 parts of N,N′-bis(alkyl)acyldiamine diacetic acid, 25-55 parts of alkanolamide-terminated polyoxyethylene ether, and 15-45 parts of fatty acid; wherein the N,N′-bis(alkyl)acyldiamine diacetic acid has 18-46 carbon atoms in its hydrocarbon group; and the alkanolamide-terminated polyoxyethylene ether has 2-6 ethylene oxide monomers. In this invention, N,N′-bis(alkyl)acyldiamine diacetic acid contains a unique twin structure, with two long-chain hydrocarbon groups and two polar carboxylic acid groups in one molecule. This structure allows for easier formation of an adsorption layer on a solid surface with nonpolar groups facing the gas and polar groups facing the solid, enabling better adsorption onto the surface of barite and rock cuttings, as well as better dispersion in oil-based drilling fluids. Furthermore, the twin structure contains both two amide groups and two carboxyl groups, resulting in more robust adsorption onto the surface of barite and rock cuttings, providing not only good wettability but also better temperature resistance. The alkanolamide-terminated polyoxyethylene ether utilizes existing alkanolamide... Alcohol amides, with several ethylene oxide chains attached and end-capped with alkanolamines, are made more polar and have more adsorption groups, enabling them to be more firmly adsorbed onto the surface of barite and rock cuttings, thus giving them good wettability and temperature resistance. A combination of multiple surfactants, through controlled proportions, produces a synergistic effect, resulting in denser and more robust adsorption on solid surfaces in oil-based drilling fluids, further enhancing the wetting effect of the wetting agent. It also improves the wetting agent's high-temperature resistance, preventing desorption at high temperatures. Furthermore, the various polar groups in the compounded wetting agent, such as amine, carboxyl, and amide groups, generate hydrogen bonds in the drilling fluid, enhancing the stability of the oil-based drilling fluid.

[0023] Meanwhile, the hydrophilic groups of this wetting agent contain a large number of amine, carboxyl, and amide groups, as well as a certain length of lipophilic chain, giving it emulsifying properties. Therefore, when added to oil-based drilling fluids, it can enhance the emulsification of the system to a certain extent without reducing the demulsification voltage, and has little impact on the oil-based drilling fluid. It also has high temperature resistance, preventing desorption at high temperatures. Furthermore, it possesses multiple polar groups, resulting in good wettability. Test results show that the temperature-resistant oil-based drilling fluid wetting agent obtained in this invention has a sedimentation volume of less than 3.4 at 150℃, 180℃, and 210℃, indicating that it has good wettability and temperature resistance. When applied to drilling fluid systems, the demulsification voltage increases while the structure remains unchanged, although the plastic viscosity decreases slightly. High-temperature and high-pressure water loss is reduced, and the static stability at 180℃ is good.

[0024] The present invention also provides a method for preparing a wetting agent for oil-based drilling fluids. Because the molecular weights used in this wetting agent are all relatively small, it has good low-temperature fluidity, is easy to use in the field, and is beneficial to industrial production. Detailed Implementation

[0025] This invention provides a wetting agent for oil-based drilling fluids, comprising, by weight parts, 25-45 parts of N,N′-bis(alkyl)acyldiamine diacetic acid, 25-55 parts of alkanolamide-terminated polyoxyethylene ether, and 15-45 parts of fatty acid;

[0026] The N,N′-bis(alkyl)acyldiamine diacetic acid has 18 to 46 carbon atoms in its hydrocarbon group;

[0027] The number of ethylene oxide polymerizable monomers in the alkanolamide-terminated polyoxyethylene ether is 2 to 6.

[0028] In this invention, unless otherwise specified, all raw materials and equipment used are commercially available products well known in the art.

[0029] The wetting agent for oil-based drilling fluid prepared by the present invention comprises 25 to 45 parts of N,N′-bis(alkyl)-acyldiamine diacetic acid, preferably 28 to 42 parts, and more preferably 30 to 40 parts by weight. In this invention, the N,N′-bis(alkyl)acyldiamine diacetic acid is preferably N,N′-bispalmitoylethylenediamine diacetic acid, N,N′-bislauroylethylenediamine diacetic acid, N,N′-bisoleylethylenediamine diacetic acid, N,N′-bistalloylethylenediamine diacetic acid, N,N′-bispalmitoylpropylenediamine diacetic acid, N,N′-bislauroylpropylenediamine diacetic acid, N,N′-bisoleylpropylenediamine diacetic acid, N,N′-bistalloylpropylenediamine diacetic acid, N,N′-bispalmitoylbutyldiamine diacetic acid, N,N′-bislauroylbutyldiamine diacetic acid, or N,N′-bisoleylbutyldiamine diacetic acid. It is one or more of N,N′-bis-tyloleylbutanediamine diacetic acid, more preferably one or more of N,N′-bispalmitoylethylenediamine diacetic acid, N,N′-bislauroylethylenediamine diacetic acid, N,N′-bisoleylethylenediamine diacetic acid, N,N′-bispalmitoylpropylenediamine diacetic acid, N,N′-bislauroylpropylenediamine diacetic acid, N,N′-bispalmitoylbutanediamine diacetic acid and N,N′-bislauroylbutanediamine diacetic acid, and more preferably N,N′-bispalmitoylethylenediamine diacetic acid, N,N′-bispalmitoylpropylenediamine diacetic acid or N,N′-bislauroylbutanediamine diacetic acid.

[0030] In this invention, the number of C atoms in the hydrocarbon group of the N,N′-bis(alkyl)acyldiamine diacetic acid is 18 to 46, preferably 20 to 45, and more preferably 22 to 40.

[0031] In this invention, the preparation method of the N,N′-bis(alkyl)acyldiamine diacetic acid preferably includes the following steps:

[0032] By mass, 35-65 parts of diamine and 55-65 parts of water are mixed, and 25-55 parts of chloroacetic acid aqueous solution are added to the resulting mixture. The mixture is heated, and the pH of the heating system is adjusted to 9-11 to produce an acid-base reaction, thereby obtaining diamine diacetic acid.

[0033] The diamine diacetic acid, 25-55 parts of hydrocarbon acyl chloride, and 1-3 parts of the first catalyst are mixed and subjected to an amidation reaction to obtain N,N′-bis-hydrocarbonyl diamine diacetic acid.

[0034] By mass fraction, the present invention mixes 35-65 parts of diamine and 55-65 parts of water, adds 25-55 parts of chloroacetic acid aqueous solution to the resulting mixture, heats, adjusts the pH of the heating system to 9-11, and causes an acid-base reaction to obtain diamine diacetic acid.

[0035] Based on parts by weight, the present invention uses 35 to 65 parts of diamine, preferably 38 to 62 parts, and more preferably 40 to 60 parts. In the present invention, the diamine preferably includes one or more of ethylenediamine, propylenediamine, and butanediamine, and more preferably ethylenediamine, propylenediamine, or butanediamine.

[0036] Based on the mass fraction of the diamine, this invention uses 55-65 parts of water, preferably 58-62 parts, and more preferably 60 parts. This invention does not have special requirements for the mixing method; commonly used techniques in the art can be employed to mix the substances evenly. For example, stirring, shaking, etc. In this invention, the mixing temperature is preferably 25-30°C.

[0037] Based on the mass fraction of the diamine, the present invention uses 25-55 parts of an aqueous chloroacetic acid solution, preferably 28-51 parts, more preferably 30-50 parts. The concentration of the aqueous chloroacetic acid solution is preferably 35-45 wt%, more preferably 38-42 wt%, and even more preferably 40 wt%. In the present invention, the aqueous chloroacetic acid solution is preferably added dropwise.

[0038] In this invention, the heating temperature is preferably 48-53°C, more preferably 50°C.

[0039] In this invention, the pH value of the heating system is preferably adjusted using an alkaline solution, wherein the alkaline solution is preferably sodium hydroxide and / or potassium hydroxide, more preferably sodium hydroxide; the concentration of the alkaline solution is preferably 15-25 wt%, more preferably 20 wt%. In this invention, the pH value of the heating system is adjusted to 9-11, preferably 10. During the pH adjustment process, the alkaline reacts with the hydrogen chloride generated during the dropwise addition of the chloroacetic acid aqueous solution, promoting the reaction to proceed, thereby obtaining diamine diacetic acid.

[0040] After obtaining diamine diacetic acid, the present invention mixes the diamine diacetic acid, 25-55 parts of hydrocarbon acyl chloride and 1-3 parts of the first catalyst, and carries out an amidation reaction to obtain N,N′-bis-hydrocarbonyl diamine diacetic acid.

[0041] Based on the mass fraction of the diamine used in the preparation of the diamine diacid, the present invention uses 25 to 55 parts of hydrocarbon acyl chloride, preferably 28 to 52 parts, and more preferably 30 to 50 parts. In the present invention, the hydrocarbon acyl chloride is preferably one or more of palmitoyl chloride, lauroyl chloride, oleic acid acyl chloride, and talluloyl chloride.

[0042] Based on the mass fraction of the diamine used in the preparation of the diamine-diacid, the present invention uses 1 to 3 parts of the first catalyst, preferably 2 parts. In the present invention, the first catalyst is preferably an alkaline solution, wherein the alkaline solution is preferably sodium hydroxide and / or potassium hydroxide, more preferably sodium hydroxide; the concentration of the alkaline solution is preferably 15 to 25 wt%, more preferably 18 to 22 wt%, and even more preferably 20 wt%.

[0043] The present invention does not have any special requirements for the mixing; the mixing methods commonly used in the art can be used to mix the substances evenly.

[0044] In this invention, the temperature of the amidation reaction is preferably 48-53°C, more preferably 50°C, and the time is preferably 4-6 hours, more preferably 5 hours.

[0045] In this invention, after the amidation reaction is completed, the resulting material is preferably further concentrated and purified to obtain N,N′-bis(alkyl)acyldiamine diacetic acid. This invention does not have special requirements for the concentration and purification method; commonly used techniques in the art are sufficient.

[0046] In this invention, the acid-base reaction and amidation reaction are preferably carried out in a closed environment.

[0047] The N,N′-dialkylacyldiamine diacetic acid obtained by this invention contains two long chains of alkylacyl groups and two carboxyl groups. This unique twin structure can more easily form an adsorption layer on the solid surface with nonpolar groups facing the gas and polar groups facing the solid, so that one end can be well adsorbed on the surface of barite and rock cuttings, and the other end can be dispersed in oil-based drilling fluids, exhibiting good wettability.

[0048] Based on the mass fraction of the N,N′-dialkyl acyl diamine diacetic acid, the wetting agent for oil-based drilling fluids prepared according to the present invention comprises 25-55 parts, preferably 28-52 parts, and more preferably 30-50 parts, of alkanolamide-terminated polyoxyethylene ether. In the present invention, the alkanolamide-terminated polyoxyethylene ether contains 2-6 ethylene oxide monomers, preferably 3-5.

[0049] In this invention, the method for preparing the alkanolamide-terminated polyoxyethylene ether preferably includes the following steps:

[0050] By mass, 10-20 parts of diethanolamine and 0.2-1.2 parts of a second catalyst are mixed and heated. 3-12 parts of ethylene oxide are added to the resulting hot mixture to carry out a polycondensation reaction. 85-97 parts of an alkanolamide capping agent are added to the resulting polycondensation product to carry out a capping reaction. The pH of the resulting capping product is adjusted to 6-7 to obtain an alkanolamide-capped polyoxyethylene ether.

[0051] The present invention uses 10 to 20 parts by weight of diethanolamine, preferably 12 to 18 parts.

[0052] Based on the mass fraction of the diethanolamine, the present invention uses 0.2 to 1.2 parts of the second catalyst, preferably 0.5 to 1.0 parts. In the present invention, the second catalyst is preferably an alkaline solution, wherein the alkaline solution preferably contains sodium hydroxide and / or potassium hydroxide, more preferably sodium hydroxide; the concentration of the alkaline solution is preferably 15 to 25 wt%, more preferably 18 to 22 wt%, and even more preferably 20 wt%.

[0053] In this invention, the heating temperature is preferably 90–110°C, more preferably 95–100°C. In this invention, the heating process preferably also includes vacuuming. Through heating and vacuuming, the solvent in the second catalyst is removed.

[0054] Based on the mass fraction of the diethanolamine, the present invention uses 3 to 12 parts of ethylene oxide, preferably 5 to 10 parts.

[0055] In this invention, the temperature of the polycondensation reaction is preferably 90-110°C, more preferably 95-100°C, the time is preferably 0.5-1.5h, more preferably 1h, and the pressure is preferably 0.05-0.1MPa, more preferably 0.08MPa.

[0056] Based on the mass fraction of the diethanolamine, the present invention uses 85-97 parts of the end-capping agent alkanolamide, preferably 88-95 parts. In the present invention, the end-capping agent alkanolamide in the alkanolamide-terminated polyoxyethylene ether is preferably one or two of coconut oil diethanolamide 6501, coconut oil diethanolamide 6502, coconut oil diethanolamide 6503, and oleic acid diethanolamide, more preferably coconut oil diethanolamide 6501, coconut oil diethanolamide 6502, or coconut oil diethanolamide 6503.

[0057] In this invention, the temperature of the end-capping reaction is preferably 90-110°C, more preferably 95-100°C, the time is preferably 1-3 hours, more preferably 2 hours, and the pressure is preferably 0.05-0.1 MPa, more preferably 0.08 MPa.

[0058] In this invention, the process after the capping reaction preferably includes concentrating and purifying the resulting material to obtain alkanolamide-capped polyoxyethylene ether. This invention does not have special requirements for the concentration and purification process; well-known techniques in the art can be used. In a specific embodiment of this invention, vacuum distillation is employed.

[0059] In this invention, the pH value of the obtained end-capping product is preferably adjusted to 6-7 using an acid solution; the acid solution is preferably an aqueous solution of sulfuric acid and / or an aqueous solution of hydrochloric acid, more preferably an aqueous solution of sulfuric acid, and the concentration of the acid solution is preferably 0.2-2 mol / L, more preferably 0.5-1 mol / L.

[0060] The alkanolamide-terminated polyoxyethylene ether obtained by this invention contains several ethylene oxide chains and alkanolamines, has a large number of polar groups, and has a small molecular weight, which allows it to be firmly adsorbed onto the surface of barite and rock fragments.

[0061] Based on the mass fraction of the N,N′-dialkyl acyl diamine diacetic acid, the wetting agent for oil-based drilling fluids prepared according to the present invention comprises 15-45 parts of fatty acids, preferably 18-42 parts, and more preferably 20-40 parts. In the present invention, the fatty acids preferably include one of tall oleic acid, soybean oleic acid, and coconut oleic acid.

[0062] The wetting agent for oil-based drilling fluid obtained by this invention contains N,N′-dialkyl acyl diamine diacetic acid, alkanolamide-terminated polyoxyethylene ether, and fatty acid. The three are compounded together and produce a synergistic effect, making the adsorption of oil-based drilling fluid on solid surfaces more dense and firm, improving its high-temperature resistance and avoiding desorption at high temperatures. At the same time, the compounded wetting agent contains a large number of hydrophilic groups such as amine, carboxyl, and amide groups, as well as lipophilic chains of a certain length. After being added to oil-based drilling fluid, it can enhance the emulsification of the system to a certain extent without reducing the demulsification voltage of the system, and has little impact on oil-based drilling fluid.

[0063] The present invention also provides a method for preparing the wetting agent for oil-based drilling fluid described in the above technical solution, comprising the following steps;

[0064] By weight, 25-45 parts of N,N′-bis(alkyl)acyldiamine diacetic acid, 25-55 parts of alkanolamide-terminated polyoxyethylene ether, and 15-45 parts of fatty acid are mixed and heated to obtain the oil-based drilling fluid wetting agent.

[0065] The present invention does not have any special requirements for the mixing; any technical solution known in the art can be used to make the substances uniform.

[0066] In this invention, the heating temperature is preferably 45-60°C, more preferably 50-55°C, and the heating time is preferably 1-3 hours, more preferably 2 hours.

[0067] The present invention also provides the application of the wetting agent for oil-based drilling fluid described in the above technical solution in oil-based drilling fluid.

[0068] The present invention does not have special requirements for the specific implementation of the application; any implementation method well known in the art can be used. In a specific embodiment of the present invention, 1 wt% of oil-based drilling fluid wetting agent is mixed with the base slurry.

[0069] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions of the present invention will be clearly and completely described below in conjunction with specific embodiments. The described embodiments are only some embodiments of the present invention, and not all embodiments. Any modifications, equivalent substitutions, improvements, etc., made to the embodiments of the present invention based on the technical essence and general principles of the present invention without creative effort should be within the protection scope of the present invention.

[0070] Example 1

[0071] Add 40 parts of ethylenediamine and 60 parts of water to a reactor, heat to 30°C and stir until uniformly mixed. Raise the temperature to 50°C, add 50 parts of 40wt% chloroacetic acid aqueous solution dropwise, then add 20wt% sodium hydroxide aqueous solution to adjust the pH of the solution to 10. React for 5 hours, concentrate and purify to obtain concentrated ethylenediamine diacetic acid solution. Add 40 parts of palmitoyl chloride and 2 parts of 20wt% sodium hydroxide aqueous solution, and react at 30°C for 5 hours to obtain N,N'-bispalmitoylethylenediamine diacetic acid.

[0072] 12 parts of diethanolamine and 0.4 parts of 20wt% sodium hydroxide aqueous solution were added to a reaction vessel, heated to 95°C, and vacuumed to -0.08 MPa to remove the solvent from the sodium hydroxide aqueous solution. While maintaining the vacuum, 5 parts of ethylene oxide were added and reacted for 1 hour. Under the same conditions, 95 parts of coconut oil diethanolamide 6501 were added and reacted for 2 hours. The mixture was then subjected to vacuum distillation, and 0.5 mol / L sulfuric acid solution was added to adjust the pH to 7 to obtain oleic acid diethanolamide polyoxyethylene ether.

[0073] 40 parts of N,N'-bispalmitoylethylenediamine diacetic acid, 30 parts of oleic acid diethanolamide polyoxyethylene ether, and 30 parts of tall oleic acid were mixed and heated to 50°C for 2 hours to obtain a temperature-resistant oil-based drilling fluid wetting agent.

[0074] Example 2

[0075] Add 50 parts of propylenediamine and 60 parts of water to a reactor, heat to 30°C and stir until uniformly mixed. Add 40 parts of 40wt% chloroacetic acid aqueous solution dropwise, raise the temperature to 50°C, add 20wt% sodium hydroxide aqueous solution to adjust the pH of the solution to 10, react for 5 hours and concentrate and purify to obtain propylenediamine diacetic acid concentrate. Add 40 parts of palmitoyl chloride and 2 parts of 20wt% sodium hydroxide aqueous solution, react at 30°C for 5 hours to obtain N,N'-bispalmitoylpropylenediamine diacetic acid.

[0076] 14 parts of diethanolamine and 0.7 parts of 20wt% sodium hydroxide aqueous solution were added to a reaction vessel, heated to 95°C, and vacuumed to -0.08 MPa to remove the solvent from the sodium hydroxide aqueous solution. While maintaining the vacuum, 7.5 parts of ethylene oxide were added, and the reaction was carried out for 1 hour. Under the same conditions, 92.5 parts of coconut oil diethanolamide 6502 were added, and the reaction was carried out for 2 hours. The mixture was then subjected to vacuum distillation, and 0.5 mol / L sulfuric acid solution was added to adjust the pH to 7 to obtain oleic acid diethanolamide polyoxyethylene ether.

[0077] 30 parts of N,N'-bispalmitoylpropylenediamine diacetic acid, 50 parts of oleic acid diethanolamide polyoxyethylene ether, and 20 parts of soybean oleic acid were mixed and heated to 50°C for 2 hours to obtain a temperature-resistant wetting agent for oil-based drilling fluids.

[0078] Example 3

[0079] Add 60 parts of butanediamine and 60 parts of water to a reactor, heat to 30°C and stir until uniformly mixed. Add 30 parts of 40wt% chloroacetic acid aqueous solution dropwise, raise the temperature to 50°C, add 20wt% sodium hydroxide aqueous solution to adjust the pH of the solution to 10, react for 5 hours and concentrate and purify to obtain a concentrated butanediamine diacetic acid solution. Add 50 parts of lauroyl chloride and 2 parts of 20wt% sodium hydroxide aqueous solution, react at 30°C for 5 hours to obtain N,N'-bispalmitoylbutanediamine diacetic acid.

[0080] 16 parts of ethanolamine and 1.0 part of 20wt% sodium hydroxide aqueous solution were added to a reaction vessel, heated to 95°C, and vacuumed to -0.08 MPa to remove the solvent from the sodium hydroxide aqueous solution. While maintaining the vacuum, 10 parts of ethylene oxide were added and reacted for 1 hour. Under the same conditions, 90 parts of coconut oil diethanolamide 6503 were added and reacted for 2 hours. The mixture was then subjected to vacuum distillation, and the pH was adjusted to 7 by adding 0.5 mol / L sulfuric acid solution to obtain oleic acid diethanolamide polyoxyethylene ether.

[0081] 35 parts of N,N'-bispalmitoylbutanediamine diacetic acid, 35 parts of oleic acid diethanolamide polyoxyethylene ether, and 30 parts of coconut oil acid were mixed and heated to 50°C for 2 hours to obtain a temperature-resistant wetting agent for oil-based drilling fluids.

[0082] Comparative Example 1

[0083] 12 parts of diethanolamine and 0.4 parts of 20wt% sodium hydroxide aqueous solution were added to a reaction vessel, heated to 95°C, and vacuumed to -0.08 MPa to remove the solvent from the sodium hydroxide aqueous solution. While maintaining the vacuum, 5 parts of ethylene oxide were added and reacted for 1 hour. Then, 95 parts of coconut oil diethanolamide 6501 were added and reacted for 2 hours. The mixture was then subjected to vacuum distillation, and the pH was adjusted to 7 by adding 0.5 mol / L sulfuric acid solution to obtain oleic acid diethanolamide polyoxyethylene ether.

[0084] 70 parts of oleic acid diethanolamide polyoxyethylene ether and 30 parts of tall oleic acid were mixed and heated to 50°C for 2 hours to obtain a temperature-resistant wetting agent for oil-based drilling fluid.

[0085] Comparative Example 2

[0086] 40 parts of ethylenediamine and 60 parts of water were added to a reactor and heated to 30°C. The mixture was stirred until homogeneous. 50 parts of 40wt% chloroacetic acid aqueous solution were added dropwise. The temperature was then raised to 50°C. 20wt% sodium hydroxide aqueous solution was added to adjust the pH of the solution to 10. The reaction was carried out for 5 hours, and the solution was concentrated and purified to obtain ethylenediamine diacetic acid concentrate. 40 parts of palmitoyl chloride and 2 parts of 20wt% sodium hydroxide aqueous solution were added, and the reaction was carried out at 30°C for 5 hours to obtain N,N'-bispalmitoylethylenediamine diacetic acid.

[0087] 70 parts of N,N'-bispalmitoylethylenediamine diacetic acid and 30 parts of tall oil acid were mixed and heated to 50°C for 2 hours to obtain a temperature-resistant wetting agent for oil-based drilling fluids.

[0088] Comparative Example 3

[0089] Add 40 parts of ethylamine and 60 parts of water to a reactor, heat to 30°C and stir until uniformly mixed. Add 50 parts of 40wt% chloroacetic acid aqueous solution dropwise, raise the temperature to 50°C, add 20wt% sodium hydroxide aqueous solution to adjust the pH of the solution to 10, react for 5 hours and concentrate and purify to obtain concentrated ethylamine diacetic acid solution. Add 40 parts of palmitoyl chloride and 2 parts of 20wt% sodium hydroxide aqueous solution, react at 30°C for 5 hours to obtain N,N'-bispalmitoylethylamine diacetic acid.

[0090] 12 parts of diethanolamine and 0.4 parts of 20wt% sodium hydroxide aqueous solution were added to a reaction vessel, heated to 95°C, and vacuumed to -0.08 MPa to remove the solvent from the sodium hydroxide aqueous solution. While maintaining the vacuum, 5 parts of ethylene oxide were added and reacted for 1 hour. Under the same conditions, 95 parts of coconut oil diethanolamide 6501 were added and reacted for 2 hours. The mixture was then subjected to vacuum distillation, and 0.5 mol / L sulfuric acid solution was added to adjust the pH to 7 to obtain oleic acid diethanolamide polyoxyethylene ether.

[0091] 40 parts of N,N'-bispalmitoyl ethylamine diacetic acid, 30 parts of oleic acid diethanolamide polyoxyethylene ether, and 30 parts of tall oleic acid were mixed and heated to 50°C for 2 hours to obtain a temperature-resistant wetting agent for oil-based drilling fluids.

[0092] Comparative Example 4

[0093] 40 parts of ethylenediamine and 60 parts of water were added to a reactor and heated to 30°C. The mixture was stirred until homogeneous. 50 parts of 40wt% chloroacetic acid aqueous solution were added dropwise. The temperature was then raised to 50°C. 20wt% sodium hydroxide aqueous solution was added to adjust the pH of the solution to 10. The reaction was carried out for 5 hours, and the solution was concentrated and purified to obtain ethylenediamine diacetic acid concentrate. 40 parts of palmitoyl chloride and 2 parts of 20wt% sodium hydroxide aqueous solution were added, and the reaction was carried out at 30°C for 5 hours to obtain N,N'-bispalmitoylethylenediamine diacetic acid.

[0094] 40 parts of N,N'-bispalmitoylethylenediamine diacetic acid, 30 parts of coconut oil diethanolamide 6501 and 30 parts of tall oil acid were mixed and heated to 50°C for 2 hours to obtain a temperature-resistant oil-based drilling fluid wetting agent.

[0095] The performance of the temperature-resistant oil-based drilling fluids prepared in Examples 1-3 and Comparative Examples 1-4 was compared using wetting agents. The specific steps are as follows:

[0096] (1) Comparison of wettability by sedimentation volume: When barite settles in a surfactant white oil solution, it forms capillary channels. The wetting agent converts the barite surface into oil wettability, reducing the resistance of the oil phase in the capillary channels, thereby reducing the amount of oil phase contained in the barite volume, and ultimately reducing the volume of stable barite. Therefore, the smaller the sedimentation volume of barite, the better its wettability. Based on this principle, 200 mL of No. 3 white oil and 20 g of temperature-resistant oil-based drilling fluid wetting agent were mixed and stirred at high speed for 10 min. Then, 80 g of barite was added and stirred at 12000 rpm for 1 h. The mixture was aged at different temperatures for 16 h. After cooling and stirring evenly, the mixture was quickly poured into 20 mL centrifuge tubes and allowed to stand for 24 h. The sedimentation volume was then recorded, and the wettability of the wetting agent was determined based on the amount of sedimentation volume. The results are shown in Table 1.

[0097] Table 1. Comparison of the wettability of the wetting agents for temperature-resistant oil-based drilling fluids prepared in Examples 1-3 and Comparative Examples 1-4.

[0098]

[0099]

[0100] As can be seen from Table 1, after adding the wetting agent, the sedimentation volume decreased after aging at different temperatures for both the examples and comparative examples. However, the sedimentation volume increased at higher temperatures. The sedimentation volumes of Examples 1-3 at 150℃, 180℃, and 210℃ were all less than 3.4, indicating that the temperature-resistant wetting agent for oil-based drilling fluids obtained by this invention has good wetting and temperature resistance. The sedimentation volumes of Comparative Examples 1-4 were significantly larger than those of Example 1, indicating that the wetting properties of Comparative Examples 1-4 were not as good as those of Example 1, and the effect was worse at higher temperatures. This shows that the twin structure of N,N′-bis(alkyl)acyldiamine diacetic acid, the alkanolamide-terminated polyoxyethylene ether, and the grafting structure of the alkanolamide-terminated polyoxyethylene ether obtained by this invention are all of great significance to the wetting properties of the wetting agent.

[0101] (2) Take the drilling mud from well Yang 101H36-3 in the Sichuan block. The mud density is 2.20 g / cm³. 3 Different wetting agents (1 wt%) were added, stirred at high temperature for 20 min, and aged at 180℃ for 16 h. The plastic viscosity, dynamic shear force, initial shear, final shear, demulsification voltage, and high-temperature high-pressure filtration loss of the drilling fluid were tested according to Part B / T16783.2. The 1-day settling stability of the drilling mud was also tested to compare the effects of the wetting agents. The test results are shown in Table 2. In the table, the Xinchuangneng wetting agent is OW, an oil-based drilling fluid wetting agent from Sichuan Xinchuangneng Petroleum Engineering Technology Co., Ltd., and the Henan Longxiang wetting agent is LXWET, an oil-based drilling fluid wetting agent from Henan Longxiang Petroleum Additives Co., Ltd.

[0102] Table 2 Performance tests of different systems composed of wetting agents for temperature-resistant oil-based drilling fluids prepared in Example 1 and Comparative Examples 1-4.

[0103]

[0104]

[0105] As shown in Table 2, compared with the base slurry, the system composed of the wetting agent and base slurry in Example 1 showed an increased demulsification voltage, unchanged dynamic shear force, but slightly decreased plastic viscosity, reduced high-temperature and high-pressure water loss, and significantly improved static stability at 180°C. Compared with the systems formed by the wetting agents obtained in Comparative Examples 1-4, the demulsification voltage, viscosity, and water loss were reduced, and although the stability at 180°C was slightly enhanced compared to the base slurry, it was still worse than that of Example 1. The addition of Xinchuangneng wetting agent and Henan Longxiang wetting agent resulted in a slight decrease in plastic viscosity, a significant decrease in dynamic shear force, a significant reduction in demulsification, an increase in water loss, and virtually no improvement in settling stability. This indicates that the temperature-resistant oil-based drilling fluid wetting agent prepared in this invention has minimal impact on system performance, improves system stability, reduces water loss, and exhibits good high-temperature resistance, demonstrating excellent performance.

[0106] The temperature-resistant oil-based drilling fluid wetting agent prepared in this invention solves the problems of wetting failure at high temperatures, significant drop in drilling fluid demulsification voltage after addition, and weak wetting, avoiding the problem of reducing the system's demulsification voltage during the wetting process. This temperature-resistant oil-based drilling fluid wetting agent is composed of three surfactants. The product contains strongly polar groups such as -O-, -CONH-, -NH-, and -COOH, as well as a twin structure and multiple hydrophilic polar groups within a single molecule. These polar groups and special structures can firmly adsorb onto the surface of rock cuttings and barite. Furthermore, due to the synergistic effect between multiple surfactants, the adsorption is even stronger, resulting in better wetting performance and no desorption at high temperatures. Additionally, the interaction between polar groups enhances the emulsification performance of the system to a certain extent, with minimal impact on the system.

[0107] The above description is only a preferred embodiment of the present invention. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.

Claims

1. A wetting agent for oil-based drilling fluids, characterized in that, It consists of 25-45 parts by mass of N,N′-bis(alkyl)acyldiamine diacetic acid, 25-55 parts of alkanolamide-terminated polyoxyethylene ether, and 15-45 parts of fatty acid; The N,N′-bis(alkyl)acyldiamine diacetic acid is one of N,N′-bispalmitoylethylenediamine diacetic acid, N,N′-bispalmitoylpropylenediamine diacetic acid, and N,N′-bispalmitoylbutyldiamine diacetic acid; The preparation method of the alkanolamide-terminated polyoxyethylene ether includes the following steps: By mass, 10-20 parts of diethanolamine and 0.2-1.2 parts of the second catalyst are mixed and heated. 3-12 parts of ethylene oxide are added to the resulting hot mixture to carry out a polycondensation reaction. 85-97 parts of the end-capping agent alkanolamide are added to the resulting polycondensation product to carry out an end-capping reaction. The pH value of the resulting end-capping product is adjusted to 6-7 to obtain alkanolamide-terminated polyoxyethylene ether. The capping agent alkanolamide is one or two of coconut oil diethanolamide 6501, coconut oil diethanolamide 6502, coconut oil diethanolamide 6503, and oleic acid diethanolamide.

2. The wetting agent for oil-based drilling fluid according to claim 1, characterized in that, The preparation method of the N,N′-bis(alkyl)acyldiamine diacetic acid includes the following steps: By mass, 35-65 parts of diamine and 55-65 parts of water are mixed, and 25-55 parts of chloroacetic acid aqueous solution are added to the resulting mixture. The mixture is heated, and the pH of the heating system is adjusted to 9-11 to produce an acid-base reaction, thereby obtaining diamine diacetic acid. The diamine diacetic acid, 25-55 parts of hydrocarbon acyl chloride, and 1-3 parts of the first catalyst are mixed and subjected to an amidation reaction to obtain N,N′-bis-hydrocarbonyl diamine diacetic acid.

3. The wetting agent for oil-based drilling fluid according to claim 2, characterized in that, The first catalyst is an alkaline solution, wherein the alkali in the alkaline solution is sodium hydroxide and / or potassium hydroxide; the concentration of the alkaline solution is 15~25wt%.

4. The wetting agent for oil-based drilling fluid according to claim 1, characterized in that, The second catalyst is an alkaline solution, wherein the alkali in the alkaline solution is sodium hydroxide and / or potassium hydroxide; the concentration of the alkaline solution is 15~25wt%.

5. The wetting agent for oil-based drilling fluid according to claim 1, characterized in that, The fatty acids include one of tall oleic acid, soybean oleic acid, and coconut oleic acid.

6. A method for preparing the wetting agent for oil-based drilling fluid according to any one of claims 1 to 5, characterized in that, Includes the following steps; By weight, 25-45 parts of N,N′-bis(alkyl)-acyldiamine diacetic acid, 25-55 parts of alkanolamide-terminated polyoxyethylene ether, and 15-45 parts of fatty acid are mixed and heated to obtain the wetting agent for oil-based drilling fluid.

7. The application of the wetting agent for oil-based drilling fluid according to any one of claims 1 to 5 or the wetting agent for oil-based drilling fluid prepared by the preparation method according to claim 6 in oil-based drilling fluid.

Citation Information

Patent Citations

  • Emulsive wetting agent for high-temperature resistant oil-based drilling well liquid, as well as preparation method and application of emulsive wetting agent

    CN104388062A

  • Superfine oil-base drilling fluid used for high temperature high temperatur high pressure superdeep well and preparation method thereof