Paint composition

By combining fly ash with titanium dioxide and a particle size of less than 4.0 μm in the paint composition, the particle size distribution is optimized, the performance of the paint is improved, and the problem of fly ash waste disposal is solved, achieving a win-win situation for environmental protection and economic benefits.

CN118891331APending Publication Date: 2024-11-01VECOR IP HLDG

Patent Information

Application Number
CN202380028046.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-08-15
Filing Date
2023-02-14
Publication Date
2024-11-01

Smart Images

  • Figure BDA0005044825750000381
    Figure BDA0005044825750000381
  • Figure BDA0005044825750000401
    Figure BDA0005044825750000401
  • Figure BDA0005044825750000411
    Figure BDA0005044825750000411
Patent Text Reader

Abstract

The present invention relates to a paint composition wherein the composition comprises fly ash, TiOz and a polymeric binder material, and wherein the fly ash has a d50 particle size of less than 4.0 [mu] m.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Reflective thermal-insulation exterior wall coating

    CN103555102A

  • Sun-proof and aging-resistant exterior wall coating and preparation method thereof

    CN108276840A

  • Heat shield matte coating material composition and method for forming heat shield matte coating film

    JP2014196401A

  • Surface-coating compositions and composite materials

    WO1992004297A1

  • Materials and methods for the efficient dispersion of nanoparticles

    WO2021189049A1

Cited By

  • Oil paint composition and its preparation method

    TWI923467B