System and method for fixing CO2 in gas
Patent Information
- Application Number
- CN202411011659.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-05
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure CN118892738A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of carbon neutrality technology, and in particular to a system and method for fixing CO2 in gas. Background Art
[0002] Since the Industrial Revolution, the average temperature of the earth has continued to rise due to the emission of greenhouse gases. The current global average temperature is 1.1℃ higher than before industrialization, and a series of ecological and environmental problems have arisen. At present, the global annual carbon dioxide emissions exceed 30 billion tons, and the international community has taken a series of measures to meet the challenges of climate change. According to the "Direct Air Carbon Capture 2022" report released by the International Energy Agency (IEA), in order to achieve global net zero emissions, more than 85 million tons of CO2 need to be captured from the air by 2030, and 980 million tons of CO2 need to be captured by 2050.
[0003] At present, the methods for capturing carbon dioxide widely used internationally mainly include liquid chemical absorption and solid amine physical adsorption, both of which have low efficiency in capturing carbon dioxide but high energy consumption. And because the raw materials used to capture carbon dioxide need to be recycled, the captured carbon dioxide is produced in a high-purity state and needs to be used or sealed, which further causes energy consumption. Therefore, the development of an efficient system and method for directly capturing carbon dioxide from the air is of great significance for controlling the carbon dioxide content in the atmosphere and responding to climate change.
[0004] In view of this, the present invention is proposed. Summary of the invention
[0005] The object of the present invention is to provide a system and method for fixing CO2 in gas, which can be used to efficiently absorb CO2 in fixed gas, and the system has a simple structure, an easily controllable operation process, and is convenient for engineering scale-up and industrial production.
[0006] According to a first aspect of the present invention, a system for fixing CO2 in gas is provided, comprising: a reactor body, in which a plurality of layers of loading trays are arranged in sequence from top to bottom; the plurality of layers of loading trays include: a first loading tray arranged on both sides of the reactor body and a second loading tray arranged in the middle of the reactor body, the first loading tray and the second loading tray being arranged alternately from top to bottom; a first distributor is arranged on the first loading tray, and a second distributor is arranged on the second loading tray.
[0007] In the present invention, the number of layers and quantity of the material loading trays are not strictly limited and can be reasonably set according to the actual CO2 absorption amount and device conditions.
[0008] Preferably, the number of the first material loading trays in each layer is two, the two first material loading trays are distributed on both sides of the reactor body, and a first distributor is arranged above each of the first material loading trays.
[0009] Preferably, the number of the second material loading trays in each layer is two, the two second material loading trays are distributed in the middle of the reactor body, and a second distributor is arranged above each of the second material loading trays.
[0010] Preferably, a vibrator is disposed at the bottom of each of the first loading tray and the second loading tray.
[0011] Preferably, a ramp is provided above the first distributor and the second distributor.
[0012] In the present invention, there is no strict restriction on the form of the reactor body. Preferably, the reactor body is a frame structure, and the frame structure is in open contact with the gas, so as to facilitate the direct capture of carbon dioxide from the gas.
[0013] Preferably, a raw material inlet is provided at the upper part of the reactor body, and the raw material inlet is connected to a material storage tank through a conveying device, and the material storage tank stores mineralized raw materials; a raw material outlet is provided at the lower part of the reactor body; and a plurality of layers of loading trays are arranged in sequence from top to bottom between the raw material inlet and the raw material outlet.
[0014] A second aspect of the present invention provides a method for fixing CO2 in gas, wherein the method uses the above-mentioned system for fixing CO2 in gas to fix CO2 in gas, comprising the following steps:
[0015] S1, the mineralized raw materials enter the reactor body and are transported to the first loading tray;
[0016] S2, the mineralized raw material is spread on the first loading tray by the first distributor, and after the mineralized raw material reacts with CO2 in the gas for a certain period of time, the first distributor pushes the mineralized raw material from both sides to the middle to the second loading tray;
[0017] S3, the mineralized raw material is spread on the second loading tray by the second distributor, and after the mineralized raw material reacts with CO2 in the gas for a certain period of time, the second distributor pushes the mineralized raw material from the middle to both sides to the first loading tray of the next layer;
[0018] S4. After steps S1-S3 are repeated multiple times, the mineralized raw materials are discharged from the reactor body.
[0019] Preferably, the mineralized raw materials are divided into multiple batches and enter the reactor body, each batch of mineralized raw materials is processed according to steps S1-S4, and each batch of mineralized raw materials enters the reactor body after the previous batch of mineralized raw materials completes step S2.
[0020] Preferably, in step S2, after the mineralized raw material is spread on the first loading tray by the first distributor, the vibrator is turned on, and after the mineralized raw material reacts with CO2 in the gas for a certain time, the vibrator is turned off; in step S3, after the mineralized raw material is spread on the second loading tray by the second distributor, the vibrator is turned on, and after the mineralized raw material reacts with CO2 in the gas for a certain time, the vibrator is turned off.
[0021] In the present invention, the mineralized raw material is any material that can react with carbon dioxide, preferably calcium-containing materials (carbide slag, fly ash, phosphate tailings, etc.), magnesium-containing materials (forsterite, serpentine, etc.), silicates (steel slag, waste concrete, etc.) or any other natural or industrial materials.
[0022] In the present invention, carbon dioxide can come from air with a concentration of less than 0.1%, or from other gases released into the atmosphere produced by human or biological activities with a carbon dioxide concentration greater than or equal to 0.1%, such as farms, factories, etc.
[0023] Beneficial effects:
[0024] The present invention enables the CO2-containing gas to fully contact with any natural or industrial material that can absorb carbon dioxide by alternately arranging the first loading tray and the second loading tray on both sides and in the middle of the reactor body from top to bottom, thereby achieving efficient absorption of ultra-low concentration CO2 and greatly improving the absorption and utilization rate of low-concentration CO2. In addition, the present invention adopts gas-solid phase mixing, the system structure is simple, the operation process is easy to control, and only a small amount of mechanical energy is consumed without additional heat energy, which is convenient for engineering scale-up and industrial application. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0026] Figure 1 This is a schematic diagram of the system structure for fixing CO2 in gas provided by the present invention.
[0027] Figure 2 This is a side view of the first loading tray and the first distributor provided by the present invention.
[0028] Explanation of the reference numerals: 1. Reactor body; 2. Raw material inlet; 31. First loading tray; 32. Second loading tray; 41. First distributor; 42. Second distributor; 5. Vibrator; 6. Raw material outlet; 7. Conveying device; 8. Material storage tank; 9. Ramp plate. DETAILED DESCRIPTION
[0029] The technical solution of the present invention will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0031] In addition, the terms "first" and "second" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, "multiple" means two or more, unless otherwise clearly and specifically defined. In addition, the terms "installed", "connected" and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal connection of two components. For those of ordinary skill in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0032] Example 1
[0033] like Figures 1 to 2As shown, this embodiment provides a system for fixing CO2 in gas, including: a reactor body 1, in which several layers of loading trays are arranged in sequence from top to bottom, for containing mineralized raw materials; the several layers of loading trays include: a first loading tray 31 arranged on both sides of the reactor body 1 and a second loading tray 32 arranged in the middle of the reactor body 1, and the first loading tray 31 and the second loading tray 32 are arranged alternately from top to bottom; a first distributor 41 is arranged on the first loading tray 31, and a second distributor 42 is arranged on the second loading tray 32, and the first distributor 41 and the second distributor 42 are used to distribute or convey the mineralized raw materials. In this embodiment, the number of the first loading tray 31 in each layer is two, and the two first loading trays 31 are distributed on both sides of the reactor body 1, and a first distributor 41 is arranged above each first loading tray 31. By alternately arranging the first loading tray 31 and the second loading tray 32 on both sides and in the middle of the reactor body 1 from top to bottom, the CO2-containing gas is fully in contact with the mineralized raw material, so that efficient absorption of ultra-low concentration CO2 can be achieved, and the absorption and utilization rate of low concentration CO2 is greatly improved; in addition, by adopting gas-solid phase mixing, the system structure is simple, the operation process is easy to control, and only a small amount of mechanical energy is consumed without additional heat energy, which is convenient for engineering scale-up and industrial application.
[0034] In this embodiment, the number of the second material loading trays in each layer is two, the two second material loading trays 32 are distributed in the middle of the reactor body 1 , and a second distributor 42 is disposed above each second material loading tray 32 .
[0035] The distributor (first distributor 41 and second distributor 42) can be placed on the loading tray (first loading tray 31 and second loading tray 32) without gaps, or can be adjusted to be placed above the loading tray according to needs. When the distributor is placed on the loading tray without gaps, the distributor can push the raw materials from the upper loading tray to the lower layer. When the distributor is adjusted to a certain height and placed above the loading tray (the distance between it and the loading tray is d>0m), it can spread a certain thickness of raw materials on the loading tray according to needs.
[0036] There is no limitation on the fixing method of the distributor. In the present embodiment, the distributor can slide on the loading tray horizontally via a slide rail and can move up and down vertically via a telescopic rod to be close to or maintain a certain height with the loading tray.
[0037] In this embodiment, vibrators 5 are provided at the bottom of the first loading tray 31 and the second loading tray 32. When a certain thickness of raw materials are spread on the loading trays, the corresponding vibrators 5 are turned on to maintain a certain fluffiness between the raw materials, thereby improving the CO2 absorption efficiency of the raw materials through vibration.
[0038] In this embodiment, a ramp 9 is disposed above the first distributor 41 and the second distributor 42 to prevent the mineralized raw materials from falling into a dead corner when the mineralized raw materials fall from the upper loading tray to the lower loading tray.
[0039] Specifically, the shape of the reactor body 1 can be flexibly set. In this embodiment, it is a frame structure, which can be welded by transverse and longitudinal beams. The frame structure is convenient for open contact with the gas.
[0040] There is no limitation on the fixing method of the loading tray. In this embodiment, the first loading tray 31 can be welded or clamped on the beam of the frame structure, and the second loading tray 32 can be connected to the first loading tray 31 through a connecting rod.
[0041] There is no restriction on the size of the reactor body 1, and it can be flexibly set according to actual needs. In the present embodiment, the reactor body 1 is 6 meters long, 1 meter wide and 6 meters high. There are eight layers of loading trays, which are distributed in the reactor body 1 from top to bottom in the form of two sides, middle and two sides, and the spacing between each layer of loading trays is 0.6 meters. The length of the monomer loading tray is 2 meters and the width is 1 meter. The loading tray in the middle is connected to two monomer loading trays, that is, the total length is 4 meters. The first layer of loading trays is 1 meter apart from the top of the reactor body 1 frame, and the eighth layer of loading trays is 0.8 meters apart from the bottom of the reactor body 1 frame. Raw material inlets 2 are set on both sides of the top of the reactor body 1 frame, and the spacing between the raw material inlet 2 and the first layer of loading trays is 0.6 meters. Raw material outlets 6 are set on both sides of the bottom of the reactor body 1 frame, and the outlet height is 0.4 meters.
[0042] In this embodiment, a raw material inlet 2 is provided at the upper part of the reactor body 1, and the raw material inlet 2 is connected to a material storage tank 8 through a conveying device 7. The material storage tank 8 stores mineralized raw materials, and the mineralized raw materials are transported from the material storage tank 8 to the raw material inlet 2 through the conveying device 7; a raw material outlet 6 is provided at the lower part of the reactor body 1; and a plurality of layers of loading trays 3 are sequentially arranged from top to bottom between the raw material inlet 2 and the raw material outlet 6.
[0043] This embodiment also provides a method for fixing CO2 in gas, using the above-mentioned system for fixing CO2 in gas to fix CO2 in gas, including the following steps:
[0044] S1, the mineralized raw material enters the reactor body 1 from the raw material inlet 2 and is then transported to the first loading tray 31;
[0045] S2, the mineralized raw material is spread on the first loading tray 31 by the first distributor 41, and after the mineralized raw material reacts with CO2 in the gas for a certain period of time, the first distributor 41 pushes the mineralized raw material from both sides to the middle to the second loading tray 32;
[0046] S3, the mineralized raw material is spread on the second loading tray 32 by the second distributor 42, and after the mineralized raw material reacts with CO2 in the gas for a certain period of time, the second distributor 42 pushes the mineralized raw material from the middle to both sides to the first loading tray 31 of the next layer;
[0047] S4. After steps S1-S3 are repeated for multiple times, the mineralized raw material falls into the raw material outlet 6 and then is discharged from the reactor body 1.
[0048] In this embodiment, after the mineralized raw materials are spread on the loading tray, the distributor returns to its original position.
[0049] In this embodiment, the main active ingredient of the mineralized raw material is calcium hydroxide.
[0050] In this embodiment, the mineralized raw materials are divided into multiple batches and enter the reactor body 1. Each batch of mineralized raw materials is processed according to steps S1-S4. Each batch of mineralized raw materials enters the reactor body 1 after the previous batch of mineralized raw materials completes step S2. The mineralized raw materials are added in batches at intervals to facilitate full contact between the mineralized raw materials and the CO2-containing gas, thereby improving the conversion rate of the mineralized raw materials.
[0051] In this embodiment, in step S2, after the mineralized raw materials are spread on the first loading tray 31 through the first distributor 41, the vibrator 5 is turned on, and after reacting with CO2 in the gas for a certain time, the vibrator 5 is turned off; in step S3, after the mineralized raw materials are spread on the second loading tray 32 through the second distributor 42, the vibrator 5 is turned on, and after reacting with CO2 in the gas for a certain time, the vibrator 5 is turned off.
[0052] The following is a detailed description of the working process of fixing CO2 in the air in the reactor with eight layers of loading trays (i.e., four layers of first loading trays 31 and four layers of second loading trays 32) in this embodiment:
[0053] The first batch of pretreated mineralized raw materials enter the reactor body 1 from the raw material inlet 2 and accumulate on both sides of the first layer of loading tray. After the feeding is completed, the first layer distributor starts from both sides of the loading tray to spread the raw materials on the loading tray with a thickness of 4 cm and then returns to both sides of the loading tray, and turns on the vibrator. After 3 hours, the vibrator is turned off, and the first layer distributor is close to the loading tray and slowly pushes the raw materials to the second layer of loading tray and then returns to both sides of the first layer of loading tray. The second batch of pretreated mineralized raw materials enter the reactor body 1 through the raw material inlet 2 and accumulate on both sides of the first layer of loading tray. After the feeding is completed, the first layer distributor starts from both sides of the first layer of loading tray to spread the second batch of raw materials on the first layer of loading tray with a thickness of 4 cm and then returns to both sides of the loading tray. At the same time, the two distributors of the second layer start from the center line, and spread the first batch of raw materials on the second layer of loading tray with a thickness of 4 cm to the left and right sides respectively, and then return to the center line of the loading tray. The first and second layer vibrators are turned on at the same time, and the vibrators are turned off after 3 hours. The second layer distributor is close to the second layer loading tray and slowly pushes the first batch of raw materials to the third layer loading tray and then returns to the center line of the second layer loading tray. Then the first layer distributor is close to the first layer loading tray and slowly pushes the second batch of raw materials to the second layer loading tray and then returns to both sides of the first layer loading tray. The distributor returns to its original position after each distribution. The third batch of pre-treated mineralized raw materials enters the reactor body 1 through the raw material inlet 2. After the feeding is completed, the above operation is repeated, and the first, second and third layers of three batches of raw materials are spread on the loading tray with a thickness of 4 cm. Turn on the vibrator, turn off the vibrator after 3 hours, and push the three layers of raw materials to the next layer loading tray in order from bottom to top. Repeat the process of feeding a new batch of raw materials, distributing, and turning on the vibration. After 3 hours, the raw materials are sent to the next layer loading tray from bottom to top. When the first batch of mineralized raw materials is fixed with CO2 for 3 hours on the eighth layer loading tray, the distributor pushes the raw materials to the two raw material outlets 6 at the bottom. After pushing each layer of raw materials from bottom to top, the ninth batch of mineralized raw materials can enter the reactor body 1.
[0054] According to the test, the conversion rate of the mineralized raw materials collected from the raw material outlet was 72%, that is, the conversion rate of calcium hydroxide into calcium carbonate.
[0055] Example 2
[0056] This embodiment is the same as Embodiment 1 except for the following differences.
[0057] In this example, the mineralized raw material whose main active ingredient is calcium hydroxide is also selected. The raw material is spread on the loading plate with a thickness of 4 cm, and the vibrator is turned on. The residence time on each layer of the loading plate is 5 hours. After the mineralized raw material stays on each layer in turn, it is pushed to the raw material outlet, and the mineralized raw material is collected. The conversion rate is 85% after detection.
[0058] Example 3
[0059] This embodiment is the same as Embodiment 1 except for the following differences.
[0060] In this example, the mineralized raw material whose main active ingredient is calcium hydroxide is also selected. The raw material is spread on the loading plate with a thickness of 3 cm, and the vibrator is turned on. The residence time on each layer of the loading plate is 3 hours. After the mineralized raw material stays on each layer in turn, it is pushed to the raw material outlet, and the mineralized raw material is collected. The conversion rate is 88% after detection.
[0061] Comparison Example
[0062] Instead of using the system of fixing CO2 in the gas of the present invention, the mineralized raw material whose main active ingredient is calcium hydroxide after activation is spread with a thickness of 4 cm on a tabletop 1 meter above the ground, 1 meter wide and 2 meters long, and placed in an outdoor open space with air circulation. After 24 hours, samples are collected for testing, and the conversion rate of calcium hydroxide is 1.75%.
[0063] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A system for fixing CO2 in gas, characterized in that: include: A reactor body (1), wherein a plurality of layers of material loading trays are sequentially arranged in the reactor body (1) from top to bottom; The plurality of layers of material loading trays include: first material loading trays (31) arranged on both sides of the reactor body (1) and second material loading trays (32) arranged in the middle of the reactor body (1), wherein the first material loading trays (31) and the second material loading trays (32) are arranged alternately from top to bottom; The first material loading tray (31) is provided with a first material distributor (41), and the second material loading tray (32) is provided with a second material distributor (42).
2. The system according to claim 1, characterized in that The number of the first material loading trays (31) in each layer is two, and the two first material loading trays (31) are distributed on both sides of the reactor body (1), and a first distributor (41) is arranged above each of the first material loading trays (31).
3. The system according to claim 1, characterized in that The number of the second material loading trays in each layer is two, the two second material loading trays (32) are distributed in the middle of the reactor body (1), and a second distributor (42) is arranged above each of the second material loading trays (32).
4. The system according to claim 1, characterized in that A vibrator (5) is provided at the bottom of each of the first material loading tray (31) and the second material loading tray (32).
5. The system according to claim 1, characterized in that A ramp (9) is provided above the first material distributor (41) and the second material distributor (42).
6. The system according to claim 1, characterized in that The reactor body (1) is a frame structure, and the frame structure is in open contact with the gas.
7. The system according to claim 1, characterized in that The reactor body (1) is provided with a raw material inlet (2) at the top, and the raw material inlet (2) is connected to a material storage tank (8) through a conveying device (7), and the material storage tank (8) stores mineralized raw materials; the reactor body (1) is provided with a raw material outlet (6) at the bottom; and a plurality of layers of loading trays (3) are arranged in sequence from top to bottom between the raw material inlet (2) and the raw material outlet (6).
8. A method for fixing CO2 in gas, characterized in that: The system for fixing CO2 in gas according to any one of claims 1 to 7 is used to fix CO2 in gas, comprising the following steps: S1, the mineralized raw material enters the reactor body (1) and is transported to the first loading tray (31); S2, the mineralized raw material is spread on the first loading tray (31) by the first distributor (41), and after the mineralized raw material reacts with CO2 in the gas for a certain period of time, the first distributor (41) pushes the mineralized raw material from both sides to the middle to the second loading tray (32); S3, the mineralized raw material is spread on the second loading tray (32) through the second distributor (42), and after the mineralized raw material reacts with CO2 in the gas for a certain period of time, the second distributor (42) pushes the mineralized raw material from the middle to both sides to the first loading tray (31) of the next layer; S4. After steps S1-S3 are repeated multiple times, the mineralized raw materials are discharged from the reactor body (1).
9. The method according to claim 8, characterized in that The mineralized raw materials are divided into multiple batches and enter the reactor body (1). Each batch of mineralized raw materials is processed according to steps S1-S4. Each batch of mineralized raw materials enters the reactor body (1) after the previous batch of mineralized raw materials completes step S2.
10. The method according to claim 8, characterized in that In step S2, after the mineralized raw material is spread on the first loading tray (31) by the first distributor (41), the vibrator (5) is turned on, and after the mineralized raw material reacts with CO2 in the gas for a certain period of time, the vibrator (5) is turned off; in step S3, after the mineralized raw material is spread on the second loading tray (32) by the second distributor (42), the vibrator (5) is turned on, and after the mineralized raw material reacts with CO2 in the gas for a certain period of time, the vibrator (5) is turned off.
Citation Information
Patent Citations
Automatically-adjusted continuous multi-bed decarburization system
CN114191965A
Isobaric moving bed continuous gas purifier
CN1154261A
Baffle plate type movable bed plate string device for HF (hydrogen fluoride) recovery
CN115608110A
Mineralization system for directly mineralizing CO2 in air
CN117839419A
A fixed bed reaction device with inclined baffles
CN220940621U
Cited By
Method for realizing direct mineralization of carbon dioxide in air by using natural ore
CN120325065A