PEEK composite material as well as preparation method and application thereof

CN118895033AInactive Publication Date: 2024-11-05ZHEJIANG DEQING CONCEPTFE PLASTIC PROD

Patent Information

Application Number
CN202411356474.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-27
Publication Date
2024-11-05
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure CN118895033A_ABST
    Figure CN118895033A_ABST
Patent Text Reader

Abstract

The invention discloses a PEEK composite material and a preparation method and application thereof, and the preparation method comprises the following steps: (1) carrying out plasma treatment on carbon fibers to obtain modified carbon fibers; (2) respectively preparing sulfonated PEEK and carboxylated PEEK; (3) mixing the sulfonated PEEK, the modified carbon fiber and a silane coupling agent for reaction to obtain a modified PEEK component I; (4) mixing the carboxylated PEEK, the modified carbon fiber and a silane coupling agent for reaction to obtain a modified PEEK component II; and (5) uniformly mixing at least one of the modified PEEK component I and the modified PEEK component II with N, N '-carbonyldiimidazole in a feeding mechanism of a granulator, and granulating in the granulator to obtain the PEEK composite material. The PEEK composite material has excellent tensile strength, compression strength, creep resistance and high temperature resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of polymer materials, and particularly relates to a PEEK composite material and a preparation method and application thereof. Background Art

[0002] PEEK is an aromatic crystalline thermoplastic polymer material. Its outstanding comprehensive physical, chemical, mechanical, electrical and thermal properties combined with typical thermoplastic molding and processing adaptability make it one of the most outstanding members of the special engineering plastic system. Carbon fiber is a one-dimensional material with corrosion resistance, high strength and high modulus. After mixing PEEK with carbon fiber, the mechanical properties of the composite material can be improved by several times.

[0003] However, there is a poor interface bonding between PEEK and carbon fiber, which makes the bonding strength between the two low. Therefore, in order to make the composite material of PEEK and carbon fiber have good mechanical properties, it is usually necessary to surface modify PEEK and carbon fiber.

[0004] For example, a Chinese invention patent with announcement number CN118105538B discloses a modified fiber-reinforced PEEK bone scaffold material and a preparation method thereof. The preparation method first uses concentrated sulfuric acid to sulfonate PEEK fibers, grafts sulfonic acid groups on the PEEK molecular chain, and obtains sulfonated PEEK; then uses N, N'-carbonyldiimidazole to activate the sulfonic acid groups on the sulfonated PEEK and reacts with 1-(3-aminopropyl) imidazole, so that the imidazole groups are grafted on the PEEK molecular chain to obtain component one; at the same time, the carbon fiber is heat-treated with a hydrochloric acid solution to obtain a carbon fiber with a hydroxyl-rich surface, and then the carbon fiber is aldehyde-formylated with NaIO4; finally, 1,4-butanesulfonic acid lactone is reacted with the aldehyde group on the surface of the carbon fiber, and the sulfonic acid lactone group is grafted on the surface of the carbon fiber to obtain a modified carbon fiber; finally, the polyetheretherketone grafted with imidazole groups on the molecular chain is reacted with the carbon fiber grafted with sulfonic acid lactone groups on the surface to obtain a modified PEEK.

[0005] The modified PEEK is designed to be used to make bone scaffold materials for human body, which has great additional requirements on the biocompatibility and antibacterial properties of the product, so the modification process is relatively complicated. If PEEK materials need to be applied in industrialization, it is necessary to develop an appropriate modification process. Summary of the invention

[0006] The object of the present invention is to provide a PEEK composite material and a preparation method and application thereof. The PEEK composite material has excellent tensile strength, compressive strength, creep resistance and high temperature resistance, and is suitable for conventional industrial applications.

[0007] To achieve the above-mentioned object of the invention, the technical solution of the present invention is as follows: A method for preparing a PEEK composite material, the preparation method comprising the following steps: (1) Plasma treatment of carbon fiber to obtain modified carbon fiber; (2) preparing sulfonated PEEK and carboxylated PEEK respectively; (3) mixing sulfonated PEEK, modified carbon fiber and silane coupling agent to obtain modified PEEK component 1; (4) mixing and reacting the carboxylated PEEK, the modified carbon fiber and the silane coupling agent to obtain a modified PEEK component 2; (5) Mixing at least one of the modified PEEK component 1 and the modified PEEK component 2 with N, N'-carbonyldiimidazole in a feeding mechanism of a granulator, and then granulating in the granulator to obtain the PEEK composite material.

[0008] The present invention first performs plasma treatment on the carbon fiber, on the one hand, etching marks are formed on the surface of the carbon fiber to increase the surface roughness, and on the other hand, C free radicals are formed on the surface of the carbon fiber, both of which can achieve the purpose of improving the hydrophilicity of the carbon fiber; at the same time, the present invention respectively prepares sulfonated PEEK and carboxylated PEEK, and under the action of a silane coupling agent, the sulfonated PEEK and the carboxylated PEEK are interfacially bonded with the modified carbon fiber respectively to obtain a modified PEEK component one and a modified PEEK component two; under the action of N, N'-carbonyldiimidazole, the modified PEEK component one and the modified PEEK component two are further cross-linked, so that in the obtained PEEK composite material, not only does the interface bonding between PEEK and the carbon fiber not exist, but also there is cross-linking bonding between the carbon fibers and between the PEEK fibers, so that the PEEK composite material has excellent strength performance, creep resistance and high temperature resistance.

[0009] Furthermore, the cross-linking of the modified PEEK component one and the modified PEEK component two occurs during the granulation process, thus achieving two goals at one stroke.

[0010] Preferably, in step (1) of the method for preparing the PEEK composite material, the carbon fiber is treated with oxygen plasma at 70-90 W for 2-5 min to obtain the modified carbon fiber.

[0011] Preferably, in step (2) of the above-mentioned method for preparing the PEEK composite material, the preparation process of the sulfonated PEEK comprises: (a) PEEK fiber was added to concentrated sulfuric acid at a weight-to-volume ratio of 1:(60-80) and reacted at 50-60°C for 20-30 h; (b) After the reaction is completed, the reactants are washed with ice water and the precipitated polymer is dried to obtain the sulfonated PEEK; The preparation process of the carboxylated PEEK comprises: (i) PEEK fibers were first treated with argon plasma at 280-350 W for 2-5 min; (ii) The PEEK fibers were then treated with acrylic acid plasma at 40-60 W for 2-5 min.

[0012] Preferably, in step (4) of the preparation method of the above-mentioned PEEK composite material, sulfonated PEEK or carboxylated PEEK and modified carbon fiber are added to a silane coupling agent ethanol hydrolyzate having a volume fraction of 1-5% in a mass ratio of (2-4):1, and after being fully mixed, refluxed at 40-60°C for 1-2 h to obtain the modified PEEK component one or modified PEEK component two; The silane coupling agent is gamma-aminopropyltriethoxysilane.

[0013] If the content of sulfonated PEEK or carboxylated PEEK is excessive, the modified PEEK component 1 or the modified PEEK component 2 still contains active sulfonic acid groups or carboxyl groups, which facilitates the cross-linking in step (5).

[0014] Preferably, in step (5) of the method for preparing the above-mentioned PEEK composite material, the mass ratio of the modified PEEK component one, the modified PEEK component two and N, N'-carbonyldiimidazole is 1:1:(2-5).

[0015] Preferably, in step (5) of the above-mentioned method for preparing the PEEK composite material, the feeding mechanism comprises at least two feeding hoppers fixed on the feeding frame and arranged in a straight line and a mixing hopper simultaneously connected to the lower part of each feeding hopper, a first control structure for controlling the front and rear opening size of the feeding outlet is provided on the feeding outlet of the feeding hopper, and a second control structure for simultaneously controlling the left and right opening size of each feeding outlet is provided between the plurality of feeding outlets; The first control structure includes a discharge baffle plate slidably connected to the lower end of the upper hopper via a first sliding structure, and a limiting structure for maintaining the current opening is provided between the discharge baffle plate and the upper hopper; The second control structure includes a horizontally arranged and serrated switch baffle, which is slidably connected to the feeding frame through a second sliding structure, and the switch baffle has a material blocking surface and a discharge port arranged at intervals along the distribution direction of the feeding hopper, and the discharge port corresponds to the feeding outlet one by one. A switch driving structure is provided between the switch baffle and the feeding frame for driving the switch baffle to slide left and right to simultaneously open or close all feeding outlets.

[0016] Among them, each feeding hopper is used to put in different raw materials (modified PEEK component one, modified PEEK component two or N,N'-carbonyldiimidazole) respectively, and the mixing hopper is used to mix various raw materials evenly. The first control mechanism on each feeding outlet is used to independently control the opening size of the feeding outlet, and the second control structure is used to simultaneously control the switch and opening size of the feeding outlet. In the present invention, the feeding outlet connected to the mixing hopper is rectangular, and the first control mechanism adjusts the width of the feeding outlet. Adjusting the size relationship of each width can achieve the size relationship of each raw material input rate, which can effectively control the mixing ratio of each raw material; the second control mechanism is used to adjust the length of the feeding outlet, and the second control mechanism controls each length synchronously, which reduces the control cost and does not affect the mixing ratio of each raw material. The product of the length and the width can characterize the rate of material discharge.

[0017] As a further preference, in the preparation method of the above-mentioned PEEK composite material, the mixing hopper is Y-shaped, comprising an integrally connected bucket-shaped upper part and a tubular lower part, the bucket-shaped upper part is butted directly below all the feeding outlets, and the tubular lower part is provided with an inclined plate mixing structure and / or a spiral mixing structure; The inclined plate mixing structure comprises at least three inclined material plates distributed up and down and inclined downward, the upper ends and sides of the inclined material plates are detachably connected to the inner side walls of the tubular lower part, a material passage is provided between the lower ends and the inner side walls of the tubular lower part, and the inclined directions of adjacent inclined material plates are opposite; The spiral mixing structure comprises a spiral mixing plate, the spiral mixing plate and the inner side wall of the mixing channel are detachably connected, and a spiral mixing channel is formed between the spiral mixing plate and the inner side wall of the tubular lower part.

[0018] Among them, the bucket-shaped upper part is mainly used to receive the discharge from each feeding outlet and guide it to the tubular lower part. The tubular lower part specifically mixes the raw materials through the inclined plate mixing structure and / or the spiral mixing structure. The tubular lower part finally transports the evenly mixed raw materials to the granulator below.

[0019] The inclined plate mixing structure is composed of multiple inclined material plates. A material passing channel is formed between the lower end of the inclined material plate and the inner side wall of the tubular lower part. The other three sides are fixedly connected. The inclined directions of adjacent inclined material plates are opposite, so that the raw materials are transported downward in a broken line between the inclined material plates. During the transportation process, especially when falling from the material passing channel to the next inclined material plate, the raw materials are mixed. The structure is simple. The spiral mixing structure is realized by a spiral mixing plate. The plate surface of the spiral mixing plate spirals downward, and multiple raw materials are mixed in the process of spiraling downward.

[0020] Both the inclined plate mixing structure and the spiral mixing structure achieve mixing of raw materials through gravity and corresponding inclined surfaces, do not require additional driving mechanisms, have simple structures, and are detachably connected to the tubular lower part, making disassembly and assembly convenient. The specific detachability can be achieved through a bolt structure.

[0021] Preferably, in step (5) of the above-mentioned method for preparing a PEEK composite material, the granulator is a twin-screw granulator, the screw diameter of the twin-screw granulator is 25-35 mm, the aspect ratio is (40-45):1, and the twin-screw speed is 500-1500 rpm; the feeding zone temperature is 290-300°C, the compression, mixing and homogenization zone temperature is 300-310°C, and the melting zone temperature is 320-330°C; the twin-screw granulator adopts a three-hole die head, the die hole diameter is 4.5-5.5 mm, and the die head temperature is 320-330°C.

[0022] The present invention also provides a PEEK composite material, which is prepared by adopting the above-mentioned preparation method.

[0023] The present invention also provides application of the above-mentioned PEEK composite material in preparing a pole frame.

[0024] Traditional hydrogen production pole frames are made of metal materials, which have the problems of high processing cost, low efficiency, poor corrosion resistance, heavy weight, etc. The present invention uses a special PEEK composite material to prepare a special engineering plastic pole frame through injection molding, which can not only conveniently process more complex sealing structures and forms, but also make the pole frame have better structural sealing effect, which is conducive to greatly improving the efficiency of hydrogen production; and the pole frame has the advantages of corrosion resistance, light weight (single product weight is reduced by 6 times), good thermal stability, excellent insulation performance, creep resistance, etc., and has a longer service life.

[0025] Compared with the prior art, the technical effects of the present invention are embodied in: (1) The present invention first performs plasma treatment on the carbon fiber, on the one hand, forming etching marks on the surface of the carbon fiber to increase the surface roughness, and on the other hand, forming C free radicals on the surface of the carbon fiber, both of which can achieve the purpose of improving the hydrophilicity of the carbon fiber; at the same time, the present invention respectively prepares sulfonated PEEK and carboxylated PEEK, and under the action of a silane coupling agent, the sulfonated PEEK and the carboxylated PEEK are interfacially bonded with the modified carbon fiber to obtain a modified PEEK component one and a modified PEEK component two; under the action of N, N'-carbonyldiimidazole, the modified PEEK component one and the modified PEEK component two are further cross-linked, so that in the obtained PEEK composite material, not only does there exist poor interface bonding between PEEK and carbon fiber, but also there are cross-linking bonds between carbon fiber and carbon fiber, and between PEEK fiber and PEEK fiber, so that the PEEK composite material has excellent strength performance, creep resistance and high temperature resistance.

[0026] (2) In the present invention, the cross-linking of the modified PEEK component 1 and the modified PEEK component 2 occurs during the granulation process, thus achieving two goals at one stroke.

[0027] (3) The present invention designs a new type of feeding mechanism for the granulator, which can not only use the feeding hoppers, the first control mechanism and the second control mechanism to effectively control the mixing ratio of the raw materials (modified PEEK component one, modified PEEK component two and N, N'-carbonyldiimidazole); but also use the inclined plate mixing structure and the spiral mixing structure to promote the modified PEEK component one, modified PEEK component two and N, N'-carbonyldiimidazole to be fully mixed before granulation; and the inclined plate mixing structure and the spiral mixing structure both achieve the mixing of the raw materials through gravity and the corresponding inclined surfaces, without the need for an additional driving mechanism, and have a simple structure. Moreover, the inclined material plate and the spiral mixing plate are both detachably connected to the tubular lower part, and are easy to disassemble and assemble.

[0028] (4) The present invention adopts a special PEEK composite material to prepare a special engineering plastic pole frame by injection molding, which can not only conveniently process more complex sealing structures and forms, so that the pole frame has a better structural sealing effect, which is beneficial to greatly improve the hydrogen production efficiency; but also the pole frame has the advantages of corrosion resistance and chemical corrosion, light weight (the weight of a single product is reduced by 6 times), good thermal stability, excellent insulation performance, creep resistance, etc., and has a longer service life. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 It is a schematic diagram of the cooperation between the granulator and the feeding mechanism provided by the present invention; Figure 2 It is a structural schematic diagram of the feeding mechanism provided by the present invention; Figure 3 It is a top view schematic diagram of the feeding mechanism provided by the present invention; Figure 4 yes Figure 3 Schematic diagram of the cross section at AA in the middle; Figure 5 yes Figure 3 Schematic diagram of the cross section at the middle BB; Figure 6 yes Figure 2 A magnified detail of point C in FIG. Figure 7 It is a simplified schematic diagram of the switch baffle provided by the present invention.

[0030] In the figure, a granulator 1, a feeding mechanism 2, a feeding hopper 21, a mixing hopper 22, a feeding outlet 23, a strip notch 24, a bucket-shaped upper part 25, a tubular lower part 26, a first control structure 3, a first sliding structure 31, a discharge baffle 32, a limiting structure 33, a slide groove 34, a rib 35, a limiting platform 36, a limiting screw 37, a second control structure 4, a switch baffle 41, a baffle surface 42, a discharge port 43, an inclined plate mixing structure 5, an inclined material plate 51, a material transfer channel 52, a spiral mixing structure 6, a spiral mixing plate 61, a spiral mixing channel 62, an ash and dust removal mechanism 7, a transition pipe 71, a material receiving port 72, an air inlet 73, an air outlet 74, and a partition plate 75. DETAILED DESCRIPTION

[0031] The technical solution of the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0032] Example 1 This embodiment provides a PEEK composite material, and the preparation method of the PEEK composite material comprises the following steps: (1) Plasma treatment of carbon fiber to obtain modified carbon fiber; Specifically, the length of the carbon fiber used in this embodiment is between 1.0 and 1.5 cm. If necessary, it is soaked in acetone for 24 hours before use to remove the oily lubricant on the surface of the carbon fiber, and then washed and dried for use; Then, the carbon fiber was treated with oxygen plasma at a vacuum degree of 25 Pa, a power of 70 W, and a temperature of 20°C for 5 min to obtain modified carbon fiber. (2) preparing sulfonated PEEK and carboxylated PEEK respectively; The length of the PEEK fiber used in this embodiment is also between 1.0 and 1.5 cm. If necessary, the fiber is soaked in acetone for 24 hours before use to remove the oily lubricant on the surface of the carbon fiber, and then washed and dried for later use. Among them, the preparation process of sulfonated PEEK includes: (a) PEEK fiber was added into concentrated sulfuric acid (95% by volume) at a weight-to-volume ratio of 1:60 and reacted at 60 °C for 20 h. (b) After the reaction is completed, the reactants are washed with ice water and the precipitated polymer is dried to obtain sulfonated PEEK; The preparation process of the carboxylated PEEK comprises: (i) PEEK fibers were first treated with argon plasma at a vacuum of 30 Pa, a power of 280 W, and 20 °C for 5 min; (ii) PEEK fiber was treated with acrylic acid plasma at a vacuum degree of 18 Pa, a power of 60 W, and a temperature of 20 °C for 2 min to obtain carboxylated PEEK; (3) mixing sulfonated PEEK, modified carbon fiber and silane coupling agent to obtain modified PEEK component 1; Specifically, sulfonated PEEK and modified carbon fiber were mixed in a mass ratio of 2:1 and added into a 75% ethanol hydrolyzate of γ-aminopropyltriethoxysilane with a volume fraction of 2%. After being fully mixed, the mixture was refluxed at 40°C for 2 h and vacuum dried to obtain modified PEEK component 1. (4) mixing and reacting the carboxylated PEEK, the modified carbon fiber and the silane coupling agent to obtain a modified PEEK component 2; Specifically, carboxylated PEEK and modified carbon fiber were mixed in a mass ratio of 4:1 and added into a 75% ethanol hydrolyzate of γ-aminopropyltriethoxysilane with a volume fraction of 5%, and then fully mixed, refluxed at 60°C for 1 h and vacuum dried to obtain modified PEEK component 2; (5) mixing at least one of the modified PEEK component 1 and the modified PEEK component 2 with N, N'-carbonyldiimidazole in a feeding mechanism of a granulator, and then granulating in the granulator to obtain the PEEK composite material of this embodiment; like Figures 1 to 7 As shown, the feeding mechanism of this embodiment includes three feeding hoppers 21 fixed on the feeding frame and arranged in a straight line, and a mixing hopper 22 simultaneously connected to the bottom of the three feeding hoppers 21. A first control structure 3 for controlling the front and rear opening size of the feeding outlet 23 is provided on the feeding outlet 23 of the feeding hopper 21, and a second control structure 4 for simultaneously controlling the left and right opening size of each feeding outlet 23 is provided between the multiple feeding outlets 23.

[0033] Specifically, the feeding mechanism 2 is used to feed the granulator 1, wherein each feeding hopper 21 is used to feed different raw materials respectively, and the mixing hopper 22 is used to mix various raw materials uniformly, and the first control mechanism on each feeding outlet 23 is used to independently control the opening size of the feeding outlet 23, and the second control structure 4 is used to simultaneously control the switch and opening size of the feeding outlet 23. In other words, the feeding outlet 23 actually connected to the mixing hopper 22 is rectangular, and the first control mechanism adjusts the width of the feeding outlet 23. Adjusting the size relationship of each width can achieve the size relationship of each raw material input rate, which can effectively control the mixing ratio of each raw material; the second control mechanism is used to adjust the length of the feeding outlet 23, and the second control mechanism controls each length synchronously, which reduces the control cost and does not affect the mixing ratio of each raw material. The product of the length and the width can represent the rate of feeding.

[0034] like Figure 2 , Figure 3 , Figure 4 and Figure 6 As shown, the first control structure 3 includes a discharge baffle 32 slidably connected to the lower end of the upper hopper 21 through a first sliding structure 31, and a limit structure 33 for maintaining the current opening is provided between the discharge baffle 32 and the upper hopper 21. A strip-shaped notch 24 is provided at the lower end of the rear side wall of the upper material outlet 23, and the discharge baffle 32 is inserted into the strip-shaped notch 24. The first sliding structure 31 includes a slide groove 34 and a convex rib 35 respectively provided between the left and right side walls of the upper material outlet 23 and the side wall of the discharge baffle 32. The thickness of the discharge baffle 32 is adapted to the height of the strip-shaped notch 24, the upper end surface of the discharge baffle 32 is in sliding contact with the upper end of the strip-shaped notch 24, and the lower end surface is flush with the lower end of the upper material outlet 23. A gripper is also provided at the rear end of the discharge baffle 32, and an indicator scale for indicating the opening size is provided on the discharge baffle 32 along the telescopic direction.

[0035] In this embodiment, the limiting structure 33 includes a limiting platform 36 arranged on the outer wall of the upper hopper 21, and a screw hole is provided on the limiting platform 36, and a limiting screw 37 is screwed into the screw hole. A resistance increasing layer is provided at the lower end of the limiting screw 37, and the resistance increasing layer is in tight pressure contact with the upper end surface of the discharge baffle 32.

[0036] Specifically, the discharge baffle 32 is arranged horizontally and can slide in the horizontal direction. A passage for allowing raw materials to pass through is formed between the front end of the discharge baffle 32 and the inner wall of the upper hopper 21. By adjusting the position of the discharge baffle 32 on the upper hopper 21, the size of the passage can be adjusted. The limiting structure 33 is used to limit the sliding of the discharge baffle 32 so that it maintains the current material blocking state. The structure is simple and easy to operate. The strip notch 24 is arranged on one side of the lower end of the upper material outlet 23, and the discharge baffle 32 is inserted into the upper material outlet 23 horizontally from the strip notch 24. The first sliding structure 31 is realized in the form of a slide groove 34 and a convex rib 35, which is easy to disassemble and assemble and has a simple structure.

[0037] The upper end surface of the discharge baffle 32 is in contact with the upper end of the strip notch 24, and the lower end is flush with the lower end of the loading outlet 23, eliminating the space between the lower end surfaces of the discharge baffle 32 and the loading outlet 23, reducing the possibility of raw materials being caught therein. The gripper at the rear end of the discharge baffle 32 is operated by the operator, and the indicator scale is used to indicate the degree of opening of the discharge baffle 32 to the loading outlet 23, which helps to control the mixing ratio of the raw materials.

[0038] A limit screw 37 is engaged in the screw hole of the limit platform 36, and the lower end of the limit screw 37 is pressed against the discharge baffle 32 to limit the movement of the discharge baffle 32, and the resistance increasing layer is used to increase the friction between the limit screw 37 and the discharge baffle 32 to improve the limiting effect.

[0039] like Figure 3 , Figure 5 and Figure 7 As shown, the second control structure 4 includes a horizontally arranged and serrated switch baffle 41, which is slidably connected to the loading frame through a second sliding structure, and the switch baffle 41 has blocking surfaces 42 and discharge ports 43 arranged at intervals along the distribution direction of the loading hopper 21, and the discharge ports 43 correspond to the loading outlets 23 one by one. A switch driving structure is provided between the switch baffle 41 and the loading frame for driving the switch baffle 41 to slide left and right to simultaneously open or close all the loading outlets 23.

[0040] Specifically, a discharge port 43 is arranged at intervals on one side of the switch baffle 41, and a material blocking surface 42 is formed between adjacent discharge ports 43. The spacing between each discharge port 43 is adapted to the spacing between each feeding outlet 23. The switch baffle 41 can slide horizontally through the second sliding structure, and the switch driving structure is used to drive the sliding movement of the switch baffle 41 to achieve the effect of controlling the size and opening and closing of each feeding outlet 23, and the control effect is synchronous for the control of each feeding outlet 23, reducing the setting cost of the switch driving structure. The switch driving structure includes a drive cylinder assembly, which is arranged on the feeding frame, and the movement control of the switch baffle 41 is directly achieved through the extension and retraction of its output end.

[0041] like Figure 2 , Figure 4 and Figure 5As shown, the mixing hopper 22 is Y-shaped, including an integrally connected bucket-shaped upper part 25 and a tubular lower part 26, the bucket-shaped upper part 25 is butted directly below all the feed outlets 23, and an inclined plate mixing structure 5 and a spiral mixing structure 6 are arranged in the tubular lower part 26. The inclined plate mixing structure 5 includes three inclined material plates 51 distributed up and down and inclined downward, the upper end and the side of the inclined material plate 51 are detachably connected to the inner side wall of the tubular lower part 26, and a material passage 52 is arranged between the lower end and the inner side wall of the tubular lower part 26, and the inclination directions of adjacent inclined material plates 51 are opposite; the spiral mixing structure 6 is located below the inclined plate mixing structure 5, including a spiral mixing plate 61, the spiral mixing plate 61 and the inner side wall of the mixing channel are detachably connected, and a spiral mixing channel 62 is formed between the spiral mixing plate 61 and the inner side wall of the tubular lower part 26.

[0042] Specifically, the bucket-shaped upper part 25 is mainly used to receive the discharge of each feeding outlet 23, and guide and collect it into the tubular lower part 26. The tubular lower part 26 specifically realizes the mixing of each raw material through the inclined plate mixing structure 5 and the spiral mixing structure 6. The tubular lower part 26 finally conveys the mixed raw materials to the granulator 1 below. The inclined plate mixing structure 5 is composed of a plurality of inclined material plates 51. A material passing channel 52 is formed between the lower end of the inclined material plate 51 and the inner side wall of the tubular lower part 26. The other three sides are fixedly connected. The inclined directions of adjacent inclined material plates 51 are opposite, so that the raw materials are conveyed downward in a broken line between each inclined material plate 51. In the conveying process, especially when falling from the material passing channel 52 to the next inclined material plate 51, the effect of mixing each raw material is achieved. The structure is simple. The spiral mixing structure 6 is realized by a spiral mixing plate 61. The plate surface of the spiral mixing plate 61 is spirally downward, and multiple raw materials are mixed in the process of spiral downward. The inclined plate mixing structure 5 and the spiral mixing structure 6 both achieve mixing of raw materials through gravity and corresponding inclined surfaces, without the need for an additional driving mechanism, and have a simple structure. Moreover, the inclined material plate 51 and the spiral mixing plate 61 are both detachably connected to the tubular lower part 26, making disassembly and assembly convenient. The specific detachable method can be achieved through a bolt structure.

[0043] As an optimization of this embodiment, ash retaining grooves extending in the width direction are distributed along the inclined direction on the inclined material plate 51. The width of the ash retaining grooves is smaller than the size of the raw material. When the raw material passes through, fine dust impurities mixed in the raw material remain therein, thereby improving the quality of the composite material.

[0044] like Figure 2 and Figure 5As shown, a dust removal mechanism 7 is also provided between the mixing hopper 22 and the loading hopper 21. The dust removal mechanism 7 includes a transition pipe 71 fixed transversely on the loading frame. The upper end of the transition pipe 71 is provided with a material receiving port 72 that docks with the loading outlet 23. The lower end is open and docks with the mixing hopper 22. The two opposite sides of the transition pipe 71 are provided with an air inlet 73 and an air outlet 74, respectively. A negative pressure suction component is connected to the air outlet 74. A partition plate 75 is vertically fixed in the transition pipe 71. The partition plate 75 is located between adjacent loading outlets 23. Each outlet corresponds to a group of negative pressure suction components. A material blocking net is provided on the air outlet 74 to prevent the raw materials from running out. A filter screen is provided on the air inlet 73 to prevent the entry of debris from the external environment.

[0045] Specifically, the ash and dust removal mechanism 7 is used to further remove fine dust impurities mixed in the raw materials. The main body is a transition pipe 71. The upper and lower ends of the transition pipe 71 are respectively connected to the feeding outlet 23 and the mixing hopper 22. The air inlet 73 and the air outlet 74 on the side of the transition pipe 71 are provided with a device for generating a transverse airflow. The device can be specifically a negative pressure suction component. In the process of the raw materials falling in the transition pipe 71, the transverse airflow can bring out the dust impurities with smaller volume and lighter weight, thereby achieving the effect of ash and dust removal and improving the quality of the composite material obtained by the blending and modification of the granulator 1. The partition plate 75 separates the transition pipe 71 into a plurality of separate channels, each channel corresponds to each feeding outlet 23, and a group of negative pressure suction components are respectively provided on the side wall of each channel, which are used to realize the ash and dust removal treatment of each raw material respectively. Since the volume and density of different raw materials are not necessarily the same, each negative pressure suction component can generate a corresponding strength of lateral airflow to ensure the effect of effectively conveying the raw materials downward without affecting the effect. Even when facing powdered raw materials or additives, the corresponding ash and dust removal mechanism 7 can choose not to work. The material retaining net is used to prevent the raw materials from being sucked out, and the filter is used to prevent external impurities from being sucked in. In addition, the air inlet 73 can also be used as an observation port to facilitate the observation of the conveying status of the materials therein.

[0046] For illustration, the attached drawings are brief schematic diagrams of the main parts. The second sliding connection structure, filter screen, material blocking net, switch drive structure, loading rack, negative pressure suction component, indicator scale and injection molding machine are common knowledge and are not specifically shown in the drawings.

[0047] The working principle of the feeding mechanism is as follows: in the initial state, the switch baffle 41 and the feeding baffle are both in a completely closed state, and the modified PEEK component 1, the modified PEEK component 2 and N, N'-carbonyldiimidazole are added to each feeding hopper 21, and each feeding baffle is pulled out to a corresponding distance according to the indicator scale, so that the mass ratio of the modified PEEK component 1, the modified PEEK component 2 and N, N'-carbonyldiimidazole is 1:1:2. When feeding is required, the switch baffle 41 moves horizontally, and the raw material is conveyed downward from the discharge port 43 into the transition pipe 71, and the lateral airflow generated by the negative pressure suction component sucks out the fine dust mixed in the raw material. After that, each raw material and additive enters the bucket-shaped upper part 25, and then enters the tubular lower part 26 after being guided. Each raw material is conveyed downward in a zigzag shape between the inclined material plates 51 to complete the initial mixing, and then passes through the spiral mixing plate 61 for secondary mixing.

[0048] The mixed raw materials enter the granulator 1. The granulator 1 of this embodiment uses a twin-screw granulator 1. The screw diameter of the twin-screw granulator is 25 mm, the aspect ratio is 40:1, and the twin-screw speed is 500 rpm; the feeding zone temperature is 290°C, the compression, mixing and homogenization zone temperature is 300°C, and the melting zone temperature is 330°C; the twin-screw granulator adopts a three-hole die head with a die hole diameter of 5.0 mm and a die head temperature of 320°C.

[0049] Example 2 This embodiment provides a PEEK composite material, and the preparation method of the PEEK composite material comprises the following steps: (1) Plasma treatment of carbon fiber to obtain modified carbon fiber; Specifically, the length of the carbon fiber used in this embodiment is between 1.0 and 1.5 cm. If necessary, it is soaked in acetone for 24 hours before use to remove the oily lubricant on the surface of the carbon fiber, and then washed and dried for use; Then, the carbon fiber was treated with oxygen plasma at a vacuum degree of 20 Pa, a power of 90 W, and a temperature of 20°C for 2 min to obtain modified carbon fiber. (2) preparing sulfonated PEEK and carboxylated PEEK respectively; The length of the PEEK fiber used in this embodiment is also between 1.0 and 1.5 cm. If necessary, the fiber is soaked in acetone for 24 hours before use to remove the oily lubricant on the surface of the carbon fiber, and then washed and dried for later use. Among them, the preparation process of sulfonated PEEK includes: (a) PEEK fiber was added into concentrated sulfuric acid (95% by volume) at a weight-to-volume ratio of 1:80 and reacted at 50 °C for 30 h. (b) After the reaction is completed, the reactants are washed with ice water and the precipitated polymer is dried to obtain sulfonated PEEK; The preparation process of the carboxylated PEEK comprises: (i) PEEK fibers were first treated with argon plasma at a vacuum of 35 Pa, a power of 350 W, and a temperature of 20 °C for 2 min; (ii) PEEK fiber was treated with acrylic acid plasma at a vacuum degree of 20 Pa, a power of 40 W, and a temperature of 20 °C for 5 min to obtain carboxylated PEEK; (3) mixing sulfonated PEEK, modified carbon fiber and silane coupling agent to obtain modified PEEK component 1; Specifically, sulfonated PEEK and modified carbon fiber were mixed in a mass ratio of 4:1 and added into a 75% ethanol hydrolyzate of γ-aminopropyltriethoxysilane with a volume fraction of 5%. After being fully mixed, the mixture was refluxed at 50°C for 1.5 h and vacuum dried to obtain modified PEEK component 1. (4) mixing and reacting the carboxylated PEEK, the modified carbon fiber and the silane coupling agent to obtain a modified PEEK component 2; Specifically, carboxylated PEEK and modified carbon fiber were mixed in a mass ratio of 2:1 and added into a 75% ethanol hydrolyzate of γ-aminopropyltriethoxysilane with a volume fraction of 5%, and then fully mixed, refluxed at 50°C for 1.5 h and vacuum dried to obtain modified PEEK component 2; (5) mixing at least one of the modified PEEK component 1 and the modified PEEK component 2 with N, N'-carbonyldiimidazole in a feeding mechanism of a granulator, and then granulating in the granulator to obtain the PEEK composite material of this embodiment; Specifically, the raw materials (the mass ratio of modified PEEK component one, modified PEEK component two and N, N'-carbonyldiimidazole is 1:1:5) are mixed in the same feeding mechanism as in Example 1, and granulated in the same granulator as in Example 1.

[0050] Example 3 This embodiment provides a PEEK composite material, and the preparation method of the PEEK composite material comprises the following steps: (1) Plasma treatment of carbon fiber to obtain modified carbon fiber; Specifically, the length of the carbon fiber used in this embodiment is between 1.0 and 1.5 cm. If necessary, it is soaked in acetone for 24 hours before use to remove the oily lubricant on the surface of the carbon fiber, and then washed and dried for use; Then, the carbon fiber was treated with oxygen plasma at a vacuum degree of 20 Pa, a power of 80 W, and a temperature of 20°C for 2 min to obtain modified carbon fiber. (2) preparing sulfonated PEEK and carboxylated PEEK respectively; The length of the PEEK fiber used in this embodiment is also between 1.0 and 1.5 cm. If necessary, the fiber is soaked in acetone for 24 hours before use to remove the oily lubricant on the surface of the carbon fiber, and then washed and dried for later use. Among them, the preparation process of sulfonated PEEK includes: (a) PEEK fiber was added into concentrated sulfuric acid (95% by volume) at a weight-to-volume ratio of 1:70 and reacted at 55 °C for 30 h. (b) After the reaction is completed, the reactants are washed with ice water and the precipitated polymer is dried to obtain sulfonated PEEK; The preparation process of the carboxylated PEEK comprises: (i) PEEK fibers were first treated with argon plasma at a vacuum of 35 Pa, a power of 320 W, and a temperature of 20 °C for 3 min; (ii) PEEK fiber was treated with acrylic acid plasma at a vacuum degree of 20 Pa, a power of 50 W, and a temperature of 20 °C for 5 min to obtain carboxylated PEEK; (3) mixing sulfonated PEEK, modified carbon fiber and silane coupling agent to obtain modified PEEK component 1; Specifically, sulfonated PEEK and modified carbon fiber were mixed in a mass ratio of 3:1 and added into a 75% ethanol hydrolyzate of γ-aminopropyltriethoxysilane with a volume fraction of 4%. After being fully mixed, the mixture was refluxed at 50°C for 2 h and vacuum dried to obtain modified PEEK component 1. (4) The modified PEEK component 1 and N, N'-carbonyldiimidazole are mixed in a feeding mechanism of a granulator, and then granulated in the granulator to obtain the PEEK composite material of this embodiment; Specifically, the raw materials were mixed in the same feeding mechanism as in Example 1 (the mass ratio of the modified PEEK component 1 to N, N'-carbonyldiimidazole was 2:5), and granulated in the same granulator as in Example 1.

[0051] Example 4 This embodiment provides a PEEK composite material, and the preparation method of the PEEK composite material comprises the following steps: (1) Plasma treatment of carbon fiber to obtain modified carbon fiber; Specifically, the length of the carbon fiber used in this embodiment is between 1.0 and 1.5 cm. If necessary, it is soaked in acetone for 24 hours before use to remove the oily lubricant on the surface of the carbon fiber, and then washed and dried for use; Then, the carbon fiber was treated with oxygen plasma at a vacuum degree of 20 Pa, a power of 80 W, and a temperature of 20°C for 4 min to obtain modified carbon fiber. (2) preparing sulfonated PEEK and carboxylated PEEK respectively; The length of the PEEK fiber used in this embodiment is also between 1.0 and 1.5 cm. If necessary, the fiber is soaked in acetone for 24 hours before use to remove the oily lubricant on the surface of the carbon fiber, and then washed and dried for later use. Among them, the preparation process of sulfonated PEEK includes: (a) PEEK fiber was added into concentrated sulfuric acid (95% by volume) at a weight-to-volume ratio of 1:60 and reacted at 60 °C for 20 h. (b) After the reaction is completed, the reactants are washed with ice water and the precipitated polymer is dried to obtain sulfonated PEEK; The preparation process of the carboxylated PEEK comprises: (i) PEEK fibers were first treated with argon plasma at a vacuum of 40 Pa, a power of 300 W, and a temperature of 20 °C for 3 min; (ii) PEEK fiber was treated with acrylic acid plasma at a vacuum degree of 22 Pa, a power of 50 W, and a temperature of 20 °C for 5 min to obtain carboxylated PEEK; (3) mixing and reacting the carboxylated PEEK, the modified carbon fiber and the silane coupling agent to obtain a modified PEEK component 2; Specifically, carboxylated PEEK and modified carbon fiber were mixed in a mass ratio of 3:1 and added into a 75% ethanol hydrolyzate of γ-aminopropyltriethoxysilane with a volume fraction of 4%. After being fully mixed, the mixture was refluxed at 50°C for 2 h and vacuum dried to obtain modified PEEK component 2. (4) The modified PEEK component 2 and N, N'-carbonyldiimidazole are mixed in a feeding mechanism of a granulator, and then granulated in the granulator to obtain the PEEK composite material of this embodiment; Specifically, the raw materials were mixed in the same feeding mechanism as in Example 1 (the mass ratio of the modified PEEK component 2 to N, N'-carbonyldiimidazole was 2:5), and granulated in the same granulator as in Example 1.

[0052] Embodiment 5-8 The PEEK composite material prepared in Examples 1-4 was injection molded to prepare an electrode frame for hydrogen production by electrolysis.

[0053] The PEEK composite materials prepared in Examples 1-4 were made into test samples in the same manner as in Examples 5-8, and the physical properties of each test sample were tested, wherein the tensile strength was tested according to GB / T 1040.1-2018, the compressive strength was tested according to GB / T 1041-2008, the creep rate was tested according to GB / T41061-2021, and the relative temperature index was tested according to UL746B. The test results are shown in Table 1.

[0054] Table 1 Tensile Strength Compression strength Creep rate Relative Temperature Index Example 1 287 MPa 146 MPa 1% 269℃ Example 2 291 MPa 153 MPa 1% 277℃ Example 3 273 MPa 138 MPa 2% 258℃ Example 4 265 MPa 134 MPa 2% 257℃ It can be seen from Table 1 that the PEEK composite materials prepared in the present invention have excellent strength, creep resistance and high temperature resistance.

Claims

1. A method for preparing a PEEK composite material, characterized in that: The following steps are involved: (1) Plasma treatment of carbon fiber to obtain modified carbon fiber; (2) preparing sulfonated PEEK and carboxylated PEEK respectively; (3) mixing sulfonated PEEK, modified carbon fiber and silane coupling agent to obtain modified PEEK component 1; (4) mixing and reacting the carboxylated PEEK, the modified carbon fiber and the silane coupling agent to obtain a modified PEEK component 2; (5) Mixing at least one of the modified PEEK component 1 and the modified PEEK component 2 with N, N'-carbonyldiimidazole in a feeding mechanism of a granulator, and then granulating in the granulator to obtain the PEEK composite material.

2. The method for preparing the PEEK composite material according to claim 1, characterized in that: In step (1), the carbon fiber is treated with oxygen plasma at 70-90W for 2-5 min to obtain the modified carbon fiber.

3. The method for preparing the PEEK composite material according to claim 1, characterized in that: In step (2), the preparation process of sulfonated PEEK includes: (a) PEEK fiber was added to concentrated sulfuric acid at a weight-to-volume ratio of 1:(60-80) and reacted at 50-60°C for 20-30 h; (b) After the reaction is completed, the reactants are washed with ice water and the precipitated polymer is dried to obtain the sulfonated PEEK; The preparation process of the carboxylated PEEK comprises: (i) PEEK fibers were first treated with argon plasma at 280-350 W for 2-5 min; (ii) The PEEK fibers were then treated with acrylic acid plasma at 40-60 W for 2-5 min.

4. The method for preparing the PEEK composite material according to claim 1, characterized in that: In step (4), sulfonated PEEK or carboxylated PEEK and modified carbon fiber are added to a silane coupling agent ethanol hydrolyzate having a volume fraction of 1-5% in a mass ratio of (2-4):1, and after being fully mixed, refluxed at 40-60°C for 1-2 h and vacuum dried to obtain the modified PEEK component one or modified PEEK component two; The silane coupling agent is gamma-aminopropyltriethoxysilane.

5. The method for preparing the PEEK composite material according to claim 1, characterized in that: In step (5), the mass ratio of modified PEEK component 1, modified PEEK component 2 and N, N'-carbonyldiimidazole is 1:1:(2-5).

6. The method for preparing the PEEK composite material according to claim 1, characterized in that: In step (5), the feeding mechanism comprises at least two feeding hoppers (21) fixed on a feeding frame and arranged in a straight line, and a mixing hopper (22) simultaneously connected to the lower side of each feeding hopper (21), a first control structure (3) for controlling the front and rear opening size of the feeding outlet (23) is provided on the feeding outlet (23) of the feeding hopper (21), and a second control structure (4) for simultaneously controlling the left and right opening size of each feeding outlet (23) is provided between the plurality of feeding outlets (23); The first control structure (3) comprises a discharge baffle (32) slidably connected to the lower end of the upper hopper (21) via a first sliding structure (31), and a limiting structure (33) for maintaining a current opening is provided between the discharge baffle (32) and the upper hopper (21); The second control structure (4) comprises a horizontally arranged and serrated switch baffle (41), wherein the switch baffle (41) is slidably connected to the feeding frame via a second sliding structure, wherein the switch baffle (41) has a material blocking surface (42) and a material discharge port (43) arranged at intervals along the distribution direction of the feeding hopper (21), wherein the material discharge port (43) corresponds to the feeding outlet (23) one by one, and a switch driving structure for driving the switch baffle (41) to slide left and right to simultaneously open or close all the feeding outlets (23) is provided between the switch baffle (41) and the feeding frame.

7. The method for preparing the PEEK composite material according to claim 6, characterized in that: The mixing hopper (22) is Y-shaped, comprising an integrally connected hopper-shaped upper portion (25) and a tubular lower portion (26), wherein the hopper-shaped upper portion (25) is connected to the bottom of all the feed outlets (23), and the tubular lower portion (26) is provided with an inclined plate mixing structure (5) and / or a spiral mixing structure (6); The inclined plate mixing structure (5) comprises at least three inclined material plates (51) distributed vertically and inclined downwardly, the upper ends and sides of the inclined material plates (51) are detachably connected to the inner side walls of the tubular lower part (26), a material transfer channel (52) is provided between the lower ends and the inner side walls of the tubular lower part (26), and the inclined directions of adjacent inclined material plates (51) are opposite; The spiral mixing structure (6) comprises a spiral mixing plate (61), the spiral mixing plate (61) and the inner wall of the mixing channel are detachably connected, and a spiral mixing channel (62) is formed between the spiral mixing plate (61) and the inner wall of the tubular lower part (26).

8. The method for preparing the PEEK composite material according to claim 1, characterized in that: In step (5), the granulator is a twin-screw granulator, the screw diameter of the twin-screw granulator is 25-35 mm, the aspect ratio is (40-45):1, the twin-screw speed is 500-1500 rpm; the feeding zone temperature is 290-300°C, the compression, mixing and homogenization zone temperature is 300-310°C, and the melting zone temperature is 320-330°C; the twin-screw granulator adopts a three-hole die head, the die hole diameter is 4.5-5.5 mm, and the die head temperature is 320-330°C.

9. A PEEK composite material, characterized in that: The method is prepared according to any one of claims 1 to 8.

10. Use of the PEEK composite material as claimed in claim 9 in preparing a pole frame.

Citation Information

Patent Citations

  • Modified fiber reinforced PEEK bone scaffold material and preparation method thereof

    CN118105538A

  • Novel organic fertilizer automatic batching device

    CN213725845U

  • Automatic powder mixing equipment

    CN219505077U

Cited By

  • Preparation method of phosphoric acid doped melamine modified sulfonated polyetheretherketone composite membrane

    CN120737403A

  • Wear-resistant PEEK composite material and application of wear-resistant PEEK composite material in reversing valve for air bag pump