Semi-cavity chip packaging structure and method
Patent Information
- Application Number
- CN202411012676.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-05
- Estimated Expiration
- Not applicable · inactive patent
Smart Images

Figure CN118899231A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of semiconductor packaging, and in particular to a semi-cavity chip packaging structure and method. Background Art
[0002] With the diversification of integrated circuit applications and the development of automotive electronics, smart phones, artificial intelligence, and high-performance computing, advanced packaging is moving towards system integration, high speed, high frequency, and three-dimensional directions.
[0003] In order to meet the requirements of high packaging density and low cost, silicon wafers tend to be larger in size. The increase in the number of wiring layers places higher demands on the flatness of the silicon wafers and greater demands on heat dissipation capabilities.
[0004] Therefore, it is necessary to find a packaging structure and packaging method that can simultaneously solve the warpage and heat dissipation problems of high-density fan-out packaging reconstruction wafers. Summary of the invention
[0005] To solve the above problems, the present invention provides a rationally structured semi-cavity chip packaging structure and method, thereby simultaneously solving the warping and heat dissipation problems of high-density fan-out packaging reconstructed wafers, significantly reducing the warping phenomenon, and effectively enhancing the heat dissipation effect.
[0006] The technical solution adopted by the present invention is as follows:
[0007] A semi-cavity chip packaging method, the packaging method comprising:
[0008] Taking a carrier wafer, forming an anti-reflection layer on the carrier wafer, and alternately preparing a redistribution structure on the anti-reflection layer;
[0009] connecting a functional chip on the rewiring structure;
[0010] A heat dissipation cover is buckled on the functional chip, and the functional chip is located inside the lower part of the heat dissipation cover to form a semi-cavity structure;
[0011] Encapsulating the functional chip and the heat dissipation cover to form a plastic package that encapsulates the functional chip and the heat dissipation cover;
[0012] The plastic package body is thinned to expose the heat dissipation cover;
[0013] A groove is formed on the plastic sealing body at the interval between adjacent heat dissipation covers;
[0014] removing the carrier film and the anti-reflection layer to expose the redistribution structure;
[0015] A conductive structure is formed on the exposed redistribution structure.
[0016] As a further improvement of the above technical solution:
[0017] Before forming the anti-reflection layer, a temporary bonding layer is coated on the carrier, and then the anti-reflection layer is prepared on the temporary bonding layer.
[0018] The metal lines of the uppermost and lowermost redistribution layers in the redistribution structure are metal pads, and a conductor is formed on the metal pad of the uppermost redistribution layer.
[0019] A metal bump is arranged on the bottom surface of the functional chip, and the metal bump is bonded to the rewiring structure to form wafer reconstruction.
[0020] The heat dissipation cover is a shell structure with an opening on the bottom. The opening size of the heat dissipation cover is larger than the size of the functional chip. The heat dissipation cover buckles and accommodates the functional chip inside through the opening.
[0021] The inner depth of the heat dissipation cover at the opening is greater than the height of the functional chip, and the bottom end of the circumferential edge of the heat dissipation cover extends downward beyond the bottom surface of the functional chip.
[0022] There is a spacing distance between the bottom end of the edge of the heat dissipation cover and the top surface of the redistribution structure. During packaging, the plastic encapsulation material flows into the inner side of the heat dissipation cover through the spacing distance, and the plastic encapsulation material fills the gap between the functional chip and the heat dissipation cover.
[0023] The thermal expansion coefficient of the heat dissipation cover is close to or the same as that of the functional chip; the top surface of the functional chip is provided with an adhesive layer, and the top surface of the functional chip is in contact with and adhered to the inner bottom surface of the heat dissipation cover through the adhesive layer.
[0024] A semi-cavity chip packaging structure comprises a rewiring structure, wherein the bottom surface of the rewiring structure forms a conductive structure, and the top surface of the rewiring structure is connected to a functional chip; further comprising a heat dissipation cover buckled on the functional chip, wherein the functional chip is accommodated and located on the lower inner side of the heat dissipation cover to form a semi-cavity structure; the functional chip and the heat dissipation cover are wrapped and sealed in a plastic sealing body; a groove is provided on the plastic sealing body at the interval between adjacent heat dissipation covers.
[0025] As a further improvement of the above technical solution:
[0026] The heat dissipation cover is a shell structure with an opening at the bottom, and the bottom end of the circumferential edge of the heat dissipation cover extends downward beyond the bottom surface of the functional chip; there is a spacing distance between the bottom end of the edge of the heat dissipation cover and the top surface of the redistribution structure, and the plastic package fills the gap between the functional chip and the heat dissipation cover via the spacing distance.
[0027] Compared with the prior art, the present invention has the following beneficial effects:
[0028] The provision of the heat dissipation cover in the present invention not only effectively reduces the amount of plastic packaging material used, but also reduces or even avoids the warping caused by the difference in thermal expansion coefficient. The exposure of the heat dissipation cover not only effectively enhances the heat dissipation effect, but can also be used to locate the cutting path, facilitate grooving to release the stress in the plastic packaging body to further reduce the warping phenomenon, thereby simultaneously solving the warping and heat dissipation problems of high-density fan-out packaging reconstructed wafers, significantly reducing the warping phenomenon, and effectively enhancing the heat dissipation effect.
[0029] The present invention also includes the following advantages:
[0030] By adding a heat dissipation cover, the temperature of the functional chip can be transferred upward and around, greatly reducing the internal temperature of the entire package;
[0031] The functional chip and the heat dissipation cover are encapsulated by the plastic encapsulation body, and in particular, the gap between the functional chip and the heat dissipation cover is filled by the plastic encapsulation material, so that the functional chip can be protected by the plastic encapsulation body while effectively and reliably supporting the entire reconstructed wafer. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 This is a schematic diagram of the structure presented in step S0 of the packaging method embodiment of the present invention.
[0033] Figure 2 It is a schematic diagram of the structure presented in step S1 in the packaging method embodiment of the present invention.
[0034] Figure 3 This is a schematic diagram of the structure presented in step S2 of the packaging method embodiment of the present invention.
[0035] Figure 4 Schematic diagram of the arrangement of the metal bump 601 on the functional chip of the present invention
[0036] Figure 5 This is a schematic diagram of the structure presented in step S3 of the packaging method embodiment of the present invention.
[0037] Figure 6 This is a schematic diagram of the structure presented in step S4 in the packaging method embodiment of the present invention.
[0038] Figure 7 It is a structural schematic diagram of step S5 in the packaging method embodiment of the present invention.
[0039] Figure 8 for Figure 7 Schematic diagram from top view.
[0040] Fig. 9 It is a structural schematic diagram of step S6 in the packaging method embodiment of the present invention.
[0041] Fig.10It is a structural schematic diagram of step S7 in the packaging method embodiment of the present invention.
[0042] Fig.11 It is a structural schematic diagram of step S8 in the packaging method embodiment of the present invention.
[0043] Among them: 1. Carrier; 2. Temporary bonding layer; 3. Anti-reflection layer; 4. Rewiring structure; 5. Conductor; 6. Functional chip; 7. Heat dissipation cover; 8. Plastic package; 9. Conductive structure;
[0044] 41. Rewiring layer; 42. Passivation layer;
[0045] 601. Metal bumps;
[0046] 801. Groove. DETAILED DESCRIPTION
[0047] The specific implementation of the present invention will be described below in conjunction with the accompanying drawings.
[0048] A semi-cavity chip packaging method according to this embodiment includes at least the following steps:
[0049] S1, taking a carrier wafer 1, forming an anti-reflection layer 3 on the carrier wafer 1, and alternately preparing a redistribution structure 4 on the anti-reflection layer 3;
[0050] S2, connecting the functional chip 6 to the rewiring structure 4;
[0051] S3, buckle the heat dissipation cover 7 on the functional chip 6, and the functional chip 6 is located inside the lower part of the heat dissipation cover 7 to form a semi-cavity structure;
[0052] S4, encapsulating the functional chip 6 and the heat dissipation cover 7 to form a plastic package 8 encapsulating the functional chip 6 and the heat dissipation cover 7;
[0053] S5, thinning the plastic package body 8 to expose the heat dissipation cover 7;
[0054] S6, opening a groove 801 on the plastic package body 8 at the interval between adjacent heat dissipation covers 7;
[0055] S7, removing the carrier 1 and the anti-reflection layer 3 to expose the redistribution structure 4;
[0056] S8 , forming a conductive structure 9 on the exposed redistribution structure 4 .
[0057] The provision of the heat dissipation cover 7 not only effectively reduces the amount of plastic packaging material used, but also reduces or even avoids the warping caused by the difference in thermal expansion coefficient. The exposure of the heat dissipation cover 7 not only effectively enhances the heat dissipation effect, but can also be used to locate the cutting path, facilitate grooving to release the stress in the plastic packaging body 8 to further reduce the warping phenomenon.
[0058] The semi-cavity chip packaging method of the present invention is described in detail below with reference to the accompanying drawings.
[0059] First, step S1 is performed to take a carrier wafer 1 , form an anti-reflection layer 3 on the carrier wafer 1 , and alternately prepare and form a redistribution structure 4 on the anti-reflection layer 3 .
[0060] Before forming the anti-reflection layer 3, step S0 may be performed first. Figure 1 As shown, a temporary bonding layer 2 is coated on a carrier sheet 1, and then, as shown Figure 2 As shown, an anti-reflection layer 3 is prepared on the temporary bonding layer 2.
[0061] In actual operation, a polymer such as a temporary bonding adhesive is coated on the carrier film 1 to form the temporary bonding layer 2, and the temporary bonding adhesive is cured by heating, laser or the like.
[0062] The temporary bonding layer 2 is usually a photosensitive material, which will degrade under the irradiation of laser with a specific wavelength; the provision of the temporary bonding layer 2 facilitates the subsequent debonding by laser.
[0063] The carrier sheet 1 may be selected to be transparent glass, and the thickness and thermal expansion coefficient of the carrier sheet 1 may be selected according to actual needs.
[0064] An anti-reflection layer 3 is formed on the temporary bonding layer 2 by a magnetron sputtering process. The material of the anti-reflection layer 3 can be copper, titanium, aluminum or other metals. The function of the anti-reflection layer 3 is to block the laser from damaging the rewiring structure 4 in the subsequent laser debonding process.
[0065] The redistribution structure 4 is composed of a plurality of redistribution layers 41 and a passivation layer 42 . The number of layers of the redistribution layer 41 and the passivation layer 42 is not limited.
[0066] The preparation process of the redistribution structure 4 is as follows: a first metal redistribution layer 41 is formed by the cooperation of a photolithography process and an electroplating process, and then a first PI passivation layer 42 is covered on the first metal redistribution layer 41 by a coating or lamination process, and a conductive opening is formed on the first PI passivation layer 42 by a photolithography process; in this way, other metal redistribution layers 41 and PI passivation layers 42 are alternately formed in accordance with the above steps; the metal redistribution layers 41 are electrically connected through the conductive openings. The material of the metal redistribution layer 41 can be one or a combination of two or more of titanium, copper, and aluminum.
[0067] The metal circuits of the top and bottom two redistribution layers 41 in the redistribution structure 4 are metal pads, and the metal circuits of other redistribution layers 41 in the middle are fine wiring with a line width / line spacing as small as 2μm / 2μm; a conductor 5 is formed on the metal pad of the top redistribution layer 41 to facilitate subsequent electrical connection with the flip chip.
[0068] The conductor 5 may be a solder ball formed by a ball implantation process, such as a tin ball, or may be an electroplated metal bump formed by an electroplating process.
[0069] Then execute step S2, such as Figure 3 As shown, a functional chip 6 is connected to the rewiring structure 4 .
[0070] like Figure 4 As shown, a metal bump 601 is disposed on the bottom surface of the functional chip 6 , and the metal bump 601 is bonded to the redistribution structure 4 to form wafer reconstruction.
[0071] The functional chip 6 can be bonded to the conductor 5 of the redistribution structure 4 through the metal bumps 601 below the functional chip 6 by flip-chip bonding technology, and then the wafer reconstruction can be achieved by thermal reflow.
[0072] Then execute step S3, such as Figure 5 As shown, a heat dissipation cover 7 is buckled on the functional chip 6, and the functional chip 6 is located below the heat dissipation cover 7 to form a semi-cavity structure.
[0073] In this embodiment, the heat dissipation cover 7 is a shell structure with an opening on the bottom. The opening size of the heat dissipation cover 7 is larger than the size of the functional chip 6, including that the size, length and width of the heat dissipation cover 7 are larger than the length and width of the functional chip 6. The heat dissipation cover 7 snaps the functional chip 6 into place inside through the opening.
[0074] The inner depth of the opening of the heat dissipation cover 7 is greater than the height of the functional chip 6 , and the bottom end of the circumferential edge of the heat dissipation cover 7 extends downward beyond the bottom surface of the functional chip 6 .
[0075] The thermal expansion coefficient of the heat dissipation cover 7 is close to or the same as the thermal expansion coefficient of the functional chip 6. For example, the heat dissipation cover 7 is made of materials such as alumina ceramics and graphite, which have a thermal expansion coefficient close to that of silicon.
[0076] The top surface of the functional chip 6 is provided with an adhesive layer, and the top surface of the functional chip 6 is in contact with and adhered to the inner bottom surface of the heat dissipation cover 7 via the adhesive layer; the adhesive layer can be thermal conductive silicone, DAF film (Die attach film, chip adhesive film), etc., to effectively ensure the relative fixation and relative position between the heat dissipation cover 7 and the functional chip 6, and ensure that the position of the heat dissipation cover 7 is reliable.
[0077] By adding the heat dissipation cover 7, the temperature of the functional chip 6 can be transferred upward and to the surroundings, thereby greatly reducing the internal temperature of the entire package.
[0078] Then execute step S4, such as Figure 6 As shown, the functional chip 6 and the heat dissipation cover 7 are packaged to form a plastic package 8 that encapsulates the functional chip 6 and the heat dissipation cover 7 .
[0079] There is a spacing distance between the bottom edge of the heat dissipation cover 7 and the top surface of the redistribution structure 4. During packaging, the plastic encapsulation material flows into the inner side of the heat dissipation cover 7 through the spacing distance, and the plastic encapsulation material fills the gap between the functional chip 6 and the heat dissipation cover 7, effectively ensuring the reliability of the overall structure.
[0080] In this embodiment, the functional chip 6 and the heat dissipation cover 7 are plastic-encapsulated by the plastic encapsulation body 8, and in particular, the plastic encapsulation material fills the gap between the functional chip 6 and the heat dissipation cover 7, which can protect the functional chip 6 through the plastic encapsulation body 8 while effectively and reliably supporting the entire reconstructed wafer.
[0081] Then execute step S5, such as Figure 7 As shown, the plastic package body 8 is thinned to expose the heat dissipation cover 7, which is beneficial to the heat dissipation of the functional chip 6.
[0082] like Figure 8 As shown, a distance is formed between adjacent heat dissipation covers 7 .
[0083] In actual operation, the heat dissipation cover 7 may be buckled and arranged above each single functional chip 6 , or the heat dissipation cover 7 may be buckled and arranged above two or more functional chips 6 according to actual conditions.
[0084] Then execute step S6, such as Fig. 9 As shown, a groove 801 is provided on the plastic package body 8 at the interval between adjacent heat dissipation covers 7 to release the internal stress of the plastic package body 8 and further reduce the warpage.
[0085] In this embodiment, the exposed heat dissipation covers 7 can be used to locate cutting paths according to the spacing between adjacent heat dissipation covers 7, and the grooves 801 can be formed by laser grooving or wheel cutting.
[0086] Then execute step S7, such as Fig.10 As shown, the carrier 1 and the anti-reflection layer 3 are removed to expose the redistribution structure 4.
[0087] In this embodiment, the carrier 1 can be removed by laser debonding, thermal release, chemical release or mechanical release, the temporary bonding layer 2 can be cleaned with a chemical solution, the anti-reflective layer 3 can be removed by a wet etching process, and the redistribution structure 4 can expose the bottom metal pad.
[0088] Finally, step S8 is performed. Fig.11 As shown, a conductive structure 9 is formed on the exposed redistribution structure 4 .
[0089] The conductive structure 9 may be a solder ball formed by a ball planting process, such as a tin ball, or a metal bump formed by an electroplating process. When a PCB board is mounted on the package body, the conductive structure 9 uses a solder ball formed by a ball planting process; when an organic substrate is mounted on the package body, the conductive structure 9 uses an electroplated metal bump formed by an electroplating process.
[0090] The present embodiment also proposes a semi-cavity chip packaging structure, including a rewiring structure 4, a conductive structure 9 formed on the bottom surface of the rewiring structure 4, and a functional chip 6 connected to the top surface of the rewiring structure 4; it also includes a heat dissipation cover 7 that is buckled on the functional chip 6, and the functional chip 6 is accommodated on the lower inner side of the heat dissipation cover 7 to form a semi-cavity structure; the functional chip 6 and the heat dissipation cover 7 are wrapped and sealed in a plastic sealing body 8; a groove 801 is opened on the plastic sealing body 8 at the interval between adjacent heat dissipation covers 7.
[0091] The heat dissipation cover 7 is a shell structure with an opening at the bottom, and the bottom end of the circumferential edge of the heat dissipation cover 7 extends downward beyond the bottom surface of the functional chip 6; there is a spacing distance between the bottom end of the edge of the heat dissipation cover 7 and the top surface of the redistribution structure 4, and the plastic package 8 fills the gap between the functional chip 6 and the heat dissipation cover 7 via the spacing distance.
[0092] The present invention simultaneously solves the warping and heat dissipation problems of high-density fan-out package reconstructed wafers, significantly reduces the warping phenomenon, and effectively enhances the heat dissipation effect.
[0093] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0094] The above description is an explanation of the present invention, not a limitation of the present invention. The scope of the present invention is defined in the claims. Any form of modification may be made within the scope of protection of the present invention.
Claims
1. A semi-cavity chip packaging method, characterized in that: The packaging method comprises: Taking a carrier (1), forming an anti-reflection layer (3) on the carrier (1), and alternately preparing a redistribution structure (4) on the anti-reflection layer (3); Connecting a functional chip (6) to the rewiring structure (4); The heat dissipation cover (7) is buckled onto the functional chip (6), and the functional chip (6) is located below the heat dissipation cover (7) to form a semi-cavity structure; The functional chip (6) and the heat dissipation cover (7) are packaged to form a plastic package (8) that encapsulates the functional chip (6) and the heat dissipation cover (7); The plastic package body (8) is thinned to expose the heat dissipation cover (7); A groove (801) is provided on the plastic package body (8) at the interval between adjacent heat dissipation covers (7); Removing the carrier (1) and the anti-reflection layer (3) to expose the redistribution structure (4); A conductive structure (9) is formed on the exposed redistribution structure (4).
2. A semi-cavity chip packaging method as claimed in claim 1, characterized in that: Before forming the anti-reflection layer (3), a temporary bonding layer (2) is coated on the carrier (1), and then the anti-reflection layer (3) is prepared on the temporary bonding layer (2).
3. A semi-cavity chip packaging method as claimed in claim 1, characterized in that: The metal lines of the uppermost and lowermost redistribution layers (41) in the redistribution structure (4) are metal pads, and a conductor (5) is formed on the metal pad of the uppermost redistribution layer (41).
4. A semi-cavity chip packaging method as claimed in claim 1, characterized in that: A metal bump (601) is arranged on the bottom surface of the functional chip (6), and the metal bump (601) is bonded to the rewiring structure (4) to form wafer reconstruction.
5. A semi-cavity chip packaging method as claimed in claim 1, characterized in that: The heat dissipation cover (7) is a shell structure with an opening on the bottom surface. The opening size of the heat dissipation cover (7) is larger than the size of the functional chip (6). The heat dissipation cover (7) locks and accommodates the functional chip (6) inside through the opening.
6. A semi-cavity chip packaging method as claimed in claim 5, characterized in that: The inner depth of the opening of the heat dissipation cover (7) is greater than the height of the functional chip (6), and the bottom end of the circumferential edge of the heat dissipation cover (7) extends downward beyond the bottom surface of the functional chip (6).
7. A semi-cavity chip packaging method as claimed in claim 1, 5 or 6, characterized in that: There is a spacing distance between the bottom end of the edge of the heat dissipation cover (7) and the top surface of the redistribution structure (4). During packaging, the plastic encapsulation material flows into the inner side of the heat dissipation cover (7) through the spacing distance, and the plastic encapsulation material fills the gap between the functional chip (6) and the heat dissipation cover (7).
8. A semi-cavity chip packaging method as claimed in claim 1, characterized in that: The thermal expansion coefficient of the heat dissipation cover (7) is close to or the same as the thermal expansion coefficient of the functional chip (6); the top surface of the functional chip (6) is provided with an adhesive layer, and the top surface of the functional chip (6) is in contact with and adhered to the inner bottom surface of the heat dissipation cover (7) via the adhesive layer.
9. A semi-cavity chip packaging structure, characterized in that: The invention comprises a rewiring structure (4), wherein a conductive structure (9) is formed on the bottom surface of the rewiring structure (4), and the top surface of the rewiring structure (4) is connected to a functional chip (6); the invention also comprises a heat dissipation cover (7) which is buckled onto the functional chip (6), and the functional chip (6) is accommodated on the lower inner side of the heat dissipation cover (7) to form a semi-cavity structure; the functional chip (6) and the heat dissipation cover (7) are wrapped and sealed in a plastic sealing body (8); and a groove (801) is provided on the plastic sealing body (8) at the interval between adjacent heat dissipation covers (7).
10. The semi-cavity chip packaging structure according to claim 9, characterized in that: The heat dissipation cover (7) is a shell structure with an opening at the bottom, and the bottom end of the circumferential edge of the heat dissipation cover (7) extends downward beyond the bottom surface of the functional chip (6); there is a spacing distance between the bottom end of the edge of the heat dissipation cover (7) and the top surface of the redistribution structure (4), and the plastic package (8) fills the gap between the functional chip (6) and the heat dissipation cover (7) via the spacing distance.
Citation Information
Patent Citations
Fan-out type inverted packaging structure and preparation method
CN109887890A
High-density fan-out type packaging structure and packaging method
CN116936378A
Electronic device and its manufacturing method
JP2001244404A
Electronic device and manufacturing method thereof
JP2002050721A
Semiconductor package
US20030067070A1
Cited By
Packaging structure and method for improving heat dissipation and warping of product
CN119812122A
Package structure and method for improving heat dissipation and warpage of product
CN119812122B
Packaging structure and electronic equipment
CN122458832A