Glass and film removal method, vehicle

By forming side electrical connections and covering them with a coating layer in the glass edge area, combined with laser coating removal technology, the problem of coating layer oxidation and corrosion is solved, ensuring the quality and performance of the finished glass product.

CN118927730BActive Publication Date: 2026-11-20FUJIAN WANDA AUTOMOBILE GLASS IND
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411073307.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-06
Publication Date
2026-11-20
Estimated Expiration
2044-08-06

AI Technical Summary

Technical Problem

In traditional techniques, the coating layer at the glass edge is prone to oxidation and corrosion during the coating removal process, which leads to a reduction in the conductive cross-sectional area, the generation of hot spots, and affects the quality and performance of the finished glass.

Method used

A side electrical connection is formed in the glass edge area, and a coating layer is formed by magnetron sputtering to ensure that the coating layer covers the side electrical connection. The coating layer is then removed by means of laser removal to avoid exposing the edge of the coating layer and to ensure that the side electrical connection is not damaged.

Benefits of technology

It effectively avoids oxidation and corrosion at the edges of the coating layer, prevents damage to the side electrical connections, ensures that the finished glass does not have regenerated bubbles or excessive hot spot temperature, and improves the quality and performance of the glass.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118927730B_ABST
    Figure CN118927730B_ABST
Patent Text Reader

Abstract

The application relates to a glass and a film removing method and a vehicle. The glass has an edge region; the glass comprises a first electric connection part, the first electric connection part comprises a side edge electric connection part, the side edge electric connection part is arranged in the edge region; and a film coating layer is arranged on the glass surface where the first electric connection part is located, and the film coating layer at least covers the side edge electric connection part; wherein the relative position relationship between the side edge electric connection part and the film coating layer is configured to completely cover the side edge electric connection part by the film coating layer at least after film removing processing. In this way, it is ensured that the laser does not hit the side edge electric connection part during film removing processing, thereby avoiding that the side edge electric connection part is removed by one layer to expose the air hole and avoiding that the side edge electric connection part is broken to cause a short circuit problem, so that the finished product glass obtained after subsequent splicing does not have phenomena such as reborn air bubbles and excessive hot spot temperature, and the quality and use performance of the finished product glass are ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the technical field of glass, and in particular to a glass and a method for removing the film, and a vehicle. Background Technology

[0002] In automotive glass such as windshields and rear windshields, silver paste is printed onto the glass using a screen printing process, then fired. The positive and negative terminals of a power source are then connected using welding or bonding methods, allowing current to pass through the silver paste and heating the glass. Furthermore, these heated glass panes are often coated with a transparent conductive film (i.e., a coating layer), which completely covers the glass surface after forming. If the coating layer at the glass edges is not removed during subsequent processing, the edges of the coating layer will be exposed to air after the glass is laminated, leading to oxidation, discoloration, and even corrosion. This reduces the conductive cross-sectional area, creates hot spots, and may result in a series of usage risks.

[0003] However, due to factors such as unreasonable silver paste printing position and film removal design in traditional technology, the laser may easily remove a thin layer of silver paste during the film removal process, resulting in exposed pores or breakage of the silver paste, causing short circuits. This leads to problems such as regenerated bubbles and excessive hot spot temperature in the finished glass after lamination, affecting the quality and performance of the finished glass. Summary of the Invention

[0004] Therefore, it is necessary to provide a method for removing film from glass and a vehicle to address the problems of recycled bubbles and excessive hot spot temperatures in finished glass.

[0005] A first aspect of this application provides a glass glass having an edge region; the glass comprising:

[0006] A first electrical connection portion, the first electrical connection portion including a side electrical connection portion disposed within the edge region; and

[0007] A coating layer is disposed on the glass surface where the first electrical connection portion is located, and the coating layer at least covers the side electrical connection portion; wherein the relative positional relationship between the side electrical connection portion and the coating layer is configured such that, at least after the film removal process, the coating layer completely covers the side electrical connection portion.

[0008] In this glass design, the side electrical connection portion of the first electrical connection is formed by screen printing within the edge area of ​​the glass. Then, a coating layer is formed on the glass surface where the first electrical connection portion is located using processes such as magnetron sputtering. To prevent the edge portion of the coating layer from being exposed to air and oxidizing and corroding, the edge of the coating layer above the edge area needs to be de-coated (e.g., by laser de-coating, grinding wheel, etc.). After the de-coating process is completed, the coating layer can completely cover the side electrical connection portion. In this way, it is ensured that the laser will not hit the side electrical connection portion during the de-coating process, thereby avoiding the side electrical connection portion being thinned and causing pores to be exposed, and avoiding the side electrical connection portion being broken and causing short circuits. This ensures that the finished glass obtained by subsequent lamination will not have phenomena such as regenerated bubbles and excessive hot spot temperature, thus guaranteeing the quality and performance of the finished glass.

[0009] The technical solution of this application will be further described below:

[0010] In one embodiment, the coating layer includes a film-to-be-removed edge portion disposed on the surface of the edge region, and the relative positional relationship between the side electrical connection portion and the film-to-be-removed edge portion is configured such that the film-to-be-removed edge portion always completely covers the side electrical connection portion before and after the film removal process.

[0011] In one embodiment, the side electrical connection portion has a first side near the outer edge of the edge region, the distance between the first side and the outer edge of the edge region is set as a, and the edge portion to be removed has a second side near the outer edge of the edge region, the distance between the second side and the outer edge of the edge region is set as b; wherein a≧b.

[0012] In one embodiment, the side electrical connection portion has a first side near the outer edge of the edge region, the distance between the first side and the outer edge of the edge region is set as a, and the edge portion to be defilmed has a second side near the outer edge of the edge region, the distance between the second side and the outer edge of the edge region is set as b; wherein, a≧b+1mm.

[0013] In one embodiment, b ranges from 1 mm to 21 mm.

[0014] In one embodiment, the edge region extends along the outer periphery of the glass, and the side electrical connection extends circumferentially along the edge region;

[0015] The glass also includes a second electrical connection portion, which is disposed in the middle region of the glass and inside the inner edge of the edge region. The coating layer has a film removal outline, and the second electrical connection portion is disposed in a non-intersecting manner with the film removal outline.

[0016] In one embodiment, the film removal contour line has a clearance portion, the second electrical connection portion is spaced apart from the clearance portion, and the second electrical connection portion is located on the side of the clearance portion away from the edge region.

[0017] In one embodiment, the first electrical connection portion further includes an electrical connection end portion connected to the side electrical connection portion, the electrical connection end portion extending to the outside of the coating layer.

[0018] In one embodiment, the glass further includes an electrical connection element that is electrically connected to the electrical connection end.

[0019] In one embodiment, the glass includes an outer glass pane, an adhesive layer, and an inner glass pane. The outer glass pane includes a first surface and a second surface, and the inner glass pane includes a third surface and a fourth surface. The second surface and the third surface are connected by the adhesive layer, and the first electrical connection portion is disposed on the second surface or the third surface.

[0020] In one embodiment, the glass further includes an ink layer disposed on at least one of the second surface, the third surface, and the fourth surface.

[0021] A second aspect of this application also provides a method for removing the film from glass processed as described above, comprising the following steps:

[0022] A side electrical connection portion of a first electrical connection portion is formed in the edge region of the glass, and a coating layer is formed on the side of the side electrical connection portion away from the glass.

[0023] The coating layer is subjected to a film removal process at the edge of the edge region, and after the film removal process is completed, the coating layer completely covers the side electrical connection portion.

[0024] In one embodiment, the film removal process employs laser film removal.

[0025] A third aspect of this application also provides a vehicle that includes the glass described above. Attached Figure Description

[0026] The accompanying drawings, which form part of this application, are used to provide a further understanding of this application. The illustrative embodiments of this application and their descriptions are used to explain this application and do not constitute an undue limitation of this application.

[0027] To more clearly illustrate the technical solutions in the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.

[0028] Figure 1 This is a schematic diagram of the glass structure according to one embodiment.

[0029] Figure 2 This is a structural diagram showing the arrangement of the glass, the first electrical connection, the second electrical connection, and the coating layer.

[0030] Figure 3 A schematic diagram of a structure designed to allow for the avoidance of the membrane outline and the second electrical connection portion.

[0031] Figure 4 This is a partial detailed structural diagram of the glass, the first electrical connection, and the coating layer.

[0032] Figure 5 This is a flowchart illustrating the steps of a method for removing film from processed glass according to one embodiment.

[0033] Explanation of reference numerals in the attached figures:

[0034] 100. Glass; 10. Inner glass; 11. Edge region; 20. First electrical connection; 21. First side; 22. Side electrical connection; 23. Electrical connection end; 30. Coating layer; 31. Edge to be decocted; 311. Second side; 32. Decoction outline; 321. Clearance; 40. Second electrical connection; 50. Outer glass; 60. Adhesive layer; 70. Electrical connection element; 80. Ink layer. Detailed Implementation

[0035] To make the above-mentioned objectives, features, and advantages of this application more apparent and understandable, the specific embodiments of this application are described in detail below with reference to the accompanying drawings. Many specific details are set forth in the following description to provide a thorough understanding of this application. However, this application can be implemented in many other ways different from those described herein, and those skilled in the art can make similar modifications without departing from the spirit of this application. Therefore, this application is not limited to the specific embodiments disclosed below.

[0036] Furthermore, where the terms "first" and "second" appear, these terms are for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined with "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this application, where the term "multiple" appears, "multiple" means at least two, such as two, three, etc., unless otherwise explicitly specified.

[0037] In this application, unless otherwise expressly specified and limited, the terms "installation," "connection," "joining," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components, unless otherwise expressly limited. Those skilled in the art can understand the specific meaning of the above terms in this application based on the specific circumstances.

[0038] It should be noted that if a component is described as "fixed to" or "set on" another component, it can be directly on the other component or there may be an intervening component. If a component is described as "connected to" another component, it can be directly connected to the other component or there may be an intervening component.

[0039] Please see Figures 1 to 4 This application illustrates a glass 100 according to an embodiment, which includes a first electrical connection portion 20 and a coating layer 30. Depending on the actual needs, the glass 100 can be any shape, such as rectangular, sector-shaped, or triangular. The glass 100 can be single-layer glass, double-layer glass, or even multi-layer glass; no specific limitation is made here.

[0040] like Figure 1As shown, taking a rectangular glass 100 as an example, the glass 100 has an edge region 11. The edge region 11 generally refers to the entire area surrounding the main viewing area, excluding the central main viewing area. The edge region 11 at least covers at least a portion of the edges of the first electrical connection portion 20 and the coating layer 30. Specifically, the edge region 11 can be a region that extends a certain distance from the outer edge of the glass 100 towards the central area. Here, "extending a certain distance" does not mean that the edge region 11 extends inward a distance equal at every position. For example, on the left and right sides of the glass 100, the edge region 11 can extend from the edge towards the central area in the range of 5mm-200mm, while on the lower side of the glass 100, the edge region 11 can extend from the edge towards the central area in the range of 15mm-800mm. The above distance range is only an example, and this application does not impose specific limitations on it. The specific range of the edge region 11 can be selected according to actual needs.

[0041] The first electrical connection portion 20 includes a side electrical connection portion 22, which is disposed within the edge region 11, such as... Figure 1 In the embodiment shown, there are two side electrical connection portions 22, which are disposed on opposite sides of the inner glass 10 and are arranged in a generally parallel manner. The two side electrical connection portions 22 are respectively electrically connected to the positive and negative poles of the power supply.

[0042] The first electrical connection 20 can be any of the following: silver paste, copper foil, etc. Taking silver paste as an example, the silver paste is made by mixing silver powder, glass powder, and organic additives in a certain proportion. Specifically, the silver powder is used for conductivity, the glass powder is used for adhesion to the glass, and the organic additives are used for effective mixing of the silver powder and glass powder. During production, the silver paste is printed on the surface of the edge region 11 of the glass 100, and the organic additives are volatilized and bonded to the glass through pre-sintering.

[0043] A coating layer 30 is stacked on the glass surface where the first electrical connection portion 20 is located, and the coating layer 30 at least covers the side electrical connection portion 22. Specifically, the coating layer 30 can be a transparent conductive film, which includes at least one of a metal layer, a metal alloy layer, or a metal oxide layer. In some specific embodiments, the metal layer can be selected from gold (Au), silver (Ag), copper (Cu), aluminum (Al), or molybdenum (Mo). The metal alloy layer can be a silver alloy, and the metal oxide layer can be indium tin oxide, fluorine-doped tin dioxide, aluminum-doped tin dioxide, gallium-doped tin dioxide, boron-doped tin dioxide, tin-zinc oxide, or antimony-doped tin oxide, etc. For example, when the transparent conductive film includes a silver layer or a silver alloy layer, the silver layer or silver alloy layer is located between at least two dielectric layers, and the dielectric layers contain at least one of zinc oxide, tin oxide, indium oxide, titanium oxide, silicon oxide, aluminum oxide, silicon nitride, silicon carbide, aluminum nitride, or titanium metal layers. Furthermore, in some embodiments, the transparent conductive film may be selected from at least one of ITO film, ATO film, AZO film, or FTO film. The coating layer 30 may be directly deposited onto the surface of the glass 100 by chemical vapor deposition (CVD) or physical vapor deposition (PVD), for example by magnetron sputtering.

[0044] Optionally, when the glass 100 is laminated glass, it may specifically include an inner glass pane 10 and an outer glass pane 50. The outer glass pane 50 includes a first surface located near the outer side of the vehicle and a second surface located near the inner side of the vehicle. The inner glass pane 10 includes a third surface located near the outer side of the vehicle and a fourth surface located near the inner side of the vehicle. The first electrical connection portion 20 and the coating layer 30 are disposed on the second surface, or the first electrical connection portion 20 and the coating layer 30 are disposed on the third surface. The coating layer 30 can have different configurations to meet the needs of different products and applications.

[0045] The relative positional relationship between the side electrical connection portion 22 and the coating layer 30 is configured such that, at least after the film removal process, the coating layer 30 completely covers the side electrical connection portion 22.

[0046] In this solution, the glass 100 has a side electrical connection portion 22 of the first electrical connection portion 20 formed by screen printing in the edge region 11 of the inner glass 10. Then, a coating layer 30 is formed on the glass surface where the first electrical connection portion 20 is located by a process such as magnetron sputtering. In order to prevent the edge part of the coating layer 30 from being exposed to air and oxidized and corroded, the edge of the coating layer 30 located in the edge region 11 needs to be de-coated (e.g., by laser de-coating). After the de-coating is completed, the coating layer 30 can completely cover the side electrical connection portion 22. In this way, it is ensured that the laser will not hit the side electrical connection portion 22 during the de-coating process, thereby avoiding the side electrical connection portion 22 being thinned and causing pores to be exposed, and avoiding the side electrical connection portion 22 being broken and causing short circuits. This ensures that the finished glass obtained by subsequent lamination will not have phenomena such as regenerated bubbles and excessive hot spot temperature, thus ensuring the quality and performance of the finished glass.

[0047] It should be noted that the first electrical connection portion 20 in this application also includes an electrical connection end portion 23, which is connected to the side electrical connection portion 22. The electrical connection end portion 23 extends to the outside of the coating layer 30. The electrical connection end portion 23 and the side electrical connection portion 22 can be integrally formed or formed separately. Figure 1 In the illustrated embodiment, there are two electrical connection ends 23, each electrically connected to one of the two side electrical connection portions 22. In other words, before and after the film removal process, the electrical connection ends 23 are never covered by the coating layer 30, allowing the exposed electrical connection ends 23 to be easily soldered to external electrical connection elements 70 to form a power supply. For example, the electrical connection element 70 may specifically be a tongue terminal or other element that can form an electrical connection with an external power source.

[0048] Please continue reading. Figure 4 When the coating layer 30 is formed, it covers at least the edges of the inner glass 10 or the outer glass 50 on both sides. In other words, taking laminated glass as an example, if the inner glass 10 and the outer glass 10 are directly laminated, the edges of the coating layer 30 on both sides will be exposed to the air environment, causing the coating layer 10 to oxidize and corrode from the edge position inward. Therefore, a film removal process is required to ensure that the edges of the coating layer 30 are completely covered by glass or other coverings to avoid edge corrosion. The film removal process is laser film removal, specifically, the edge parts of the coating layer 30 need to be subjected to laser ablation and subtraction treatment. Specifically, in one embodiment, the coating layer 30 includes a film-to-be-removed edge 31, which is disposed on the surface of the edge region 11. The relative positional relationship between the side electrical connection part 22 and the film-to-be-removed edge 31 is configured such that the film-to-be-removed edge 31 always completely covers the side electrical connection part 22 before and after the film removal process.

[0049] In this way, it can be fully ensured that the side electrical connection portion 22 is not ablated by the laser when the coating layer 30 is laser removed, or even if the side electrical connection portion 22 is partially ablated by the laser, the side electrical connection portion 22 is always completely covered by the edge portion 31 to be removed, so there will be no problems such as the pores of the side electrical connection portion 22 being exposed or the side electrical connection portion 22 being completely broken and causing a short circuit.

[0050] Please continue reading. Figure 4 More specifically, based on any of the above embodiments, the side electrical connection portion 22 has a first side 21 near the outer edge of the edge region 11, and the distance between the first side 21 and the outer edge of the edge region 11 is set as a. The film-to-be-removed edge portion 31 has a second side 311 near the outer edge of the edge region 11, and the distance between the second side 311 and the outer edge of the edge region 11 is set as b; wherein a≧b. By setting the distance a to be greater than or equal to the distance b, it can be ensured that the first side 21 of the side electrical connection portion 22 near the edge region 11 is always located inside the second side 311 of the film-to-be-removed edge portion 31 near the edge region 11, that is, the side electrical connection portion 22 is prevented from being exposed to the outside of the film-to-be-removed edge portion 31.

[0051] Furthermore, in another embodiment, the side electrical connection portion 22 has a first side 21 near the outer edge of the edge region 11, and the distance between the first side 21 and the outer edge of the edge region 11 is set as a. The edge portion 31 to be defilmed has a second side 311 near the outer edge of the edge region 11, and the distance between the second side 311 and the outer edge of the edge region 11 is set as b. Wherein, a≧b+1mm. At this time, the second side 311 of the edge 31 to be de-coated extends at least 1 mm beyond the first side 21 of the side electrical connection 22. The extension length forms a reliable coverage margin, ensuring that regardless of whether the de-coating laser simultaneously ablates the edge 31 to be de-coated and the side electrical connection 22, the edge 31 to be de-coated will completely cover the side electrical connection 22. Problems such as exposed pores in the side electrical connection 22 or short circuits caused by the side electrical connection 22 being completely broken will not occur. This ensures that the finished glass obtained by subsequent lamination will not have phenomena such as regenerated bubbles and excessive hot spot temperature, thus guaranteeing the quality and performance of the finished glass.

[0052] Based on any of the above embodiments, the range of b is 1mm to 21mm. For example, b can be selected as 2mm, 5mm, 8mm, 14mm, 18mm, etc. The range of a is determined according to the numerical range of b (the determination method can be based on the inequality a≧b or a≧b+1mm), so as to meet the requirement that when glass 100 of various specifications and sizes is subjected to film removal processing, the coating layer 30 always completely covers the side electrical connection part 22, preventing the finished glass from having phenomena such as regenerated bubbles and hot spot temperature exceeding the standard, which would affect the quality and performance of the finished glass.

[0053] Please continue reading. Figure 2 and Figure 3 The glass 100 also includes a second electrical connection portion 40, which is disposed in the middle region of the inner glass 10 or the outer glass 50 and is located inside the inner edge of the edge region 11. The coating layer 30 has a film removal contour line 32, and the second electrical connection portion 40 is disposed in a non-intersecting manner with the film removal contour line 32. For example, the second electrical connection portion 40 can be any one of silver paste, copper foil, etc., and can be flexibly selected according to actual needs.

[0054] It should be noted that the film removal contour line 32 is a processing boundary line designed according to the heating range of the finished glass, that is, a processing trajectory line used to indicate the movement of the laser during the film removal process. After the laser moves around the film removal contour line 32, the edge of the coating layer 30 that needs to be reduced can be ablated and removed. The second electrical connection part 40 is set so as not to intersect with the film removal contour line 32, thereby avoiding the film removal laser from cutting and breaking the second electrical connection part 40 and causing a short circuit.

[0055] Specifically, based on the above embodiment, the film removal contour line 32 is provided with a clearance portion 321, and the second electrical connection portion 40 is spaced apart from the clearance portion 321, with the second electrical connection portion 40 located on the side of the clearance portion 321 away from the edge region 11. During the film removal process, the laser will not cut into the second electrical connection portion 40 when passing through the clearance portion 321, ensuring that the second electrical connection portion 40 remains intact.

[0056] Furthermore, in this application, the glass 100 includes an outer glass pane 50, an adhesive layer 60, and an inner glass pane 10. The outer glass pane 50 includes a first surface and a second surface, and the inner glass pane 10 includes a third surface and a fourth surface. The second surface and the third surface are connected by the adhesive layer 60, and a first electrical connection portion 20 is disposed on either the second surface or the third surface. Further, the glass 100 also includes an ink layer 80, which is disposed on at least one of the second, third, and fourth surfaces. The ink layer 80 helps to strengthen the glass 100 and has decorative and aesthetic functions.

[0057] The electrical connection element 70 can be a tongue terminal, copper foil, connector, or other components. The electrical connection element 70 is designed to facilitate connection with the positive and negative terminals of an external power source so that current can be passed through it to energize the first electrical connection part 20 and / or the second electrical connection part 40, thereby heating the glass 100.

[0058] The adhesive layer 60 acts as an adhesive to bond and fix the coating layer 30 to the outer glass 50. Specifically, the material of the adhesive layer 60 can be selected from one or more combinations of polycarbonate (PC), polyvinyl chloride (PVC), polyvinyl butyral (PVB), ethylene vinyl acetate (EVA), polyacrylate (PA), polymethyl methacrylate (PMMA), polyurethane (PUR), ionomer film (SGP), and polyethylene terephthalate (PET). In the embodiments of this application, the material of the adhesive layer 60 is PVB.

[0059] like Figure 5 As shown, a second aspect of this application also provides a method for removing film from the glass 100 as described above, comprising the following steps:

[0060] S10: A side electrical connection portion 22 of the first electrical connection portion 20 is formed in the edge region 11 of the inner glass 10 or the outer glass 50, and a coating layer 30 is formed on the side of the side electrical connection portion 22 away from the inner glass 10 or the outer glass 50.

[0061] S20: Perform a film removal process on the edge of the coating layer 30 located in the edge region 11, and after the film removal process is completed, make the coating layer 30 completely cover the side electrical connection portion 22.

[0062] In addition to the above, this application also provides a vehicle, which includes a body and glass 100 as described in any of the above embodiments, the glass 100 being mounted on the body. Furthermore, the glass 100 may also include edging, inserts, trim pieces, etc.

[0063] The technical features of the above embodiments can be combined in any way. For the sake of brevity, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0064] The embodiments described above are merely illustrative of several implementation methods of this application, and while the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the patent application. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of this application, and these all fall within the protection scope of this application. Therefore, the protection scope of this patent application should be determined by the appended claims.

Claims

1. A type of glass, characterized in that, The glass has an edge region; The glass comprises: A first electrical connection portion, the first electrical connection portion including a side electrical connection portion disposed within the edge region; and A coating layer is stacked on the glass surface where the first electrical connection portion is located, and the coating layer at least covers the side electrical connection portion; the coating layer includes a film-to-be-removed edge portion, the film-to-be-removed edge portion is disposed on the surface of the edge region, and the relative positional relationship between the side electrical connection portion and the film-to-be-removed edge portion is configured such that: before and after the film removal process, the film-to-be-removed edge portion always completely covers the side electrical connection portion; The side electrical connection portion has a first side near the outer edge of the edge region, and the distance between the first side and the outer edge of the edge region is set as a; the edge portion to be defilmed has a second side near the outer edge of the edge region, and the distance between the second side and the outer edge of the edge region is set as b; wherein, a≧b+1mm; The glass is manufactured using a film removal method comprising the following steps: A side electrical connection portion of a first electrical connection portion is formed in the edge region of the glass, and a coating layer is formed on the side of the side electrical connection portion away from the glass. The coating layer is subjected to a film removal process at the edge of the edge region, and after the film removal process is completed, the coating layer completely covers the side electrical connection portion.

2. The glass according to claim 1, characterized in that, The range of b is 1mm to 21mm.

3. The glass according to claim 1, characterized in that, The edge region extends along the outer periphery of the glass, and the side electrical connection portion extends circumferentially along the edge region. The glass also includes a second electrical connection portion, which is disposed in the middle region of the glass and inside the inner edge of the edge region. The coating layer has a film removal outline, and the second electrical connection portion is disposed in a non-intersecting manner with the film removal outline.

4. The glass according to claim 3, characterized in that, The film removal contour line has a clearance portion, and the second electrical connection portion is spaced apart from the clearance portion, with the second electrical connection portion located on the side of the clearance portion away from the edge region.

5. The glass according to claim 1, characterized in that, The first electrical connection portion further includes an electrical connection end, which is connected to the side electrical connection portion and extends to the outside of the coating layer.

6. The glass according to claim 5, characterized in that, The glass also includes an electrical connection element, which is electrically connected to the electrical connection end.

7. The glass according to claim 1, characterized in that, The glass includes an outer glass pane, an adhesive layer, and an inner glass pane. The outer glass pane includes a first surface and a second surface, and the inner glass pane includes a third surface and a fourth surface. The second surface and the third surface are connected by the adhesive layer, and the first electrical connection portion is disposed on the second surface or the third surface.

8. The glass according to claim 7, characterized in that, The glass further includes an ink layer disposed on at least one of the second surface, the third surface, and the fourth surface.

9. A method for removing film from glass as described in any one of claims 1 to 8, characterized in that, Includes the following steps: A side electrical connection portion of a first electrical connection portion is formed in the edge region of the glass, and a coating layer is formed on the side of the side electrical connection portion away from the glass. The coating layer is subjected to a film removal process at the edge of the edge region, and after the film removal process is completed, the coating layer completely covers the side electrical connection portion.

10. The method for removing the film from glass according to claim 9, characterized in that, The film removal process employs laser film removal.

11. A vehicle, characterized in that, Includes the glass as described in any one of claims 1 to 8.

Citation Information

Patent Citations

  • Vehicle laminated glass with inner surface coated and heated

    CN117183497A

  • Electrically conductive glass sheet

    US4778732A