Mask plate tensioning manufacturing method and mask plate
By combining frames, mesh surfaces, and metal strips in a mesh-stretching method, the problem of ensuring accuracy in splicing small-sized sheets was solved, enabling high-precision and high-efficiency production of large-sized photomasks.
Patent Information
- Application Number
- CN202410941950.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-15
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2044-07-15
AI Technical Summary
In the existing technology, the raw material sheet size of metal photomask is small, which cannot meet the production needs of large-size photomasks, and it is difficult to guarantee the accuracy of the mesh opening or pattern after splicing multiple small-size sheets.
By employing a combination of a frame, multiple mesh surfaces, reinforcing metal strips, and extending metal strips, and through methods such as stretching the mesh, splicing, and removing the extending metal strips, the mesh surfaces are ensured to be omnidirectionally tensioned and fixed, forming a high-precision metal mask plate.
This technology enables high-precision mesh morphology features for large-size photomasks, improving manufacturing efficiency and product quality.
Smart Images

Figure CN118951603B_ABST
Abstract
Description
Technical Field
[0001] This disclosure relates to the technical field of OLED manufacturing, and more specifically, to a method for fabricating a photomask and a photomask. Background Technology
[0002] Metal masks are important tools in the manufacturing process of OLED (organic light-emitting diode) display panels. They are mainly used to limit the deposition area of film materials during the evaporation of organic materials or the formation of encapsulation layers.
[0003] Depending on the type of film layer deposited, metal masks can be categorized into several types, including precision metal masks (FMM), general-purpose metal masks (CMM), and CVD masks (encapsulation layer metal masks). Currently, the common method for fabricating metal masks is to etch the raw material into a single patterned mesh, and then use specialized mesh stretching equipment for processes such as stretching, adjusting, and welding to complete the fabrication.
[0004] With the continuous iteration of display panel production lines, the demand for larger metal photomasks is also increasing. The existing raw material sheets for metal photomasks are too small to meet the production requirements of large-size photomasks. If multiple small sheets are spliced together, it is difficult to guarantee the accuracy of the mesh openings or patterns after splicing. Summary of the Invention
[0005] To address or improve the aforementioned problems in the prior art, this disclosure provides a method for fabricating a photomask and a photomask.
[0006] The mask sheet fabrication method provided in this embodiment specifically includes:
[0007] It provides a frame, multiple mesh panels, at least one reinforcing metal strip, and multiple extending metal strips;
[0008] The frame prefabrication is formed by tensioning and fixing the reinforcing metal strips across the frame. The reinforcing metal strips are set at the preset splicing positions of multiple mesh surfaces on the frame.
[0009] To form a prefabricated mesh panel, one end of one or more extended metal strips is fixed to the splicing end of the mesh panel with other mesh panels, and the other end of the strip extends away from the mesh panel.
[0010] Tension the mesh by clamping and pulling the extended metal strips, the joint between the mesh and the frame.
[0011] Splicing, maintaining the stretched state, fixing the splicing ends of the mesh to other mesh to the reinforcing metal strip, and fixing the splicing ends of the mesh to the frame to the frame, wherein adjacent meshes are fixed to the same reinforcing metal strip;
[0012] Remove the extension metal strip.
[0013] In the aforementioned technical solution, the use of extended metal strips to connect the mesh surface allows for the application of tension in directions where the mesh surface cannot be clamped and stretched in existing technical solutions. During the mesh stretching step, the extended metal strips can be used to adjust the morphological features of the mesh surface. Therefore, the metal mask plate formed by this solution has high precision in the morphological features of the mesh surface and high manufacturing efficiency.
[0014] This solution also includes a reinforcing metal strip between the two spliced mesh surfaces, which is used to weld and fix the spliced parts of the mesh after the mesh has been adjusted.
[0015] Optionally, the mesh may include openwork openings or patterns, and ribs surrounding the openings or patterns;
[0016] Furthermore, forming a mesh prefabricated component includes fixing one end of an extended metal strip to a rib, wherein the fixed extended metal strip and the rib are parallel.
[0017] In the above-mentioned alternative solutions, the metal strip is extended and connected to the parallel rib to avoid the tension of the extended metal strip causing a deterioration effect on the opening morphology on the mask.
[0018] Optionally, forming a prefabricated mesh includes fixing two sets of equal numbers of extended metal strips to opposite ends of the mesh.
[0019] Optionally, the tensioning net includes clamping two sets of extended metal strips respectively and applying tension in opposite directions to each.
[0020] Among the above-mentioned alternative solutions, the metal strip can be extended to apply tension to both ends of the mesh surface. This is especially suitable for mesh surfaces where both ends are spliced with other mesh surfaces and their edges cannot be directly clamped.
[0021] Optionally, a prefabricated mesh surface is formed, including setting a mesh surface end groove at the end of the mesh surface, and embedding one end of an extended metal strip into the mesh surface end groove and fixing it to the mesh surface.
[0022] After the splicing of the mesh and the mesh surface is completed, the aforementioned extension metal strip needs to be removed. To avoid the residual extension metal strip affecting the flatness of the mesh surface, a mesh surface end groove is set, and the end of the extension metal strip that is fixed to the mesh surface is embedded in the groove. The other parts can be removed in subsequent steps.
[0023] Optionally, the extended metal strip may be provided with a semi-etched line or a dashed through-etched line;
[0024] The removal of the extension metal strip includes breaking the extension metal strip along a half-etched line or through an etched line.
[0025] Optionally, the extension metal strip can be removed, including by directly cutting off the portion of the extension metal strip that is not embedded in the end groove of the mesh surface using a laser.
[0026] Optionally, forming a prefabricated mesh includes setting a preset cutting area on the mesh surface and fixing one end of an extended metal strip to the preset cutting area;
[0027] Removing the extension metal strip includes cutting off the pre-cut area along with the extension metal strip fixed therein.
[0028] Optionally, the extended metal strips can be staggered in different mesh prefabricated components. This is to avoid interference caused by the clamping of the extended metal strips on different mesh surfaces.
[0029] Optionally, the net can be stretched, including adjusting the openings or patterns on the net surface.
[0030] Optionally, the fixing in the aforementioned technical solution can specifically be laser welding.
[0031] This disclosure also provides a mask plate, which is manufactured by the mask plate mesh fabrication method described in any of the foregoing embodiments.
[0032] In summary, the mask sheet fabrication method provided in this embodiment can achieve the clamping of the mask sheet surface around the perimeter during sheet stretching and splicing, and can adjust the pattern of multiple spliced mesh surfaces in the mask sheet to achieve the set accuracy requirements, thereby improving the overall manufacturing accuracy of the product. Attached Figure Description
[0033] To more clearly illustrate the technical solutions in the embodiments or background art of this disclosure, the accompanying drawings used in the embodiments or background art of this disclosure will be described below.
[0034] Figure 1 This is a flowchart illustrating the net-making method in an embodiment of this disclosure;
[0035] Figure 2 This is a schematic diagram of the frame prefabricated component formed by the netting manufacturing method in this embodiment of the present disclosure;
[0036] Figure 3 This is a schematic diagram (style 1) of the precast mesh formed by the mesh fabrication method in this embodiment of the present disclosure;
[0037] Figure 4 This is a schematic diagram of the net-stretching and splicing steps in the net-stretching method of this disclosure embodiment, and shows the tension direction used to maintain the net-stretching state;
[0038] Figure 5 This is a cross-sectional schematic diagram of the combination of reinforcing metal strips, frame, and mesh in an embodiment of this disclosure;
[0039] Figure 6This illustrates one connection method between reinforcing metal strips and mesh.
[0040] Figure 7 Another connection method for reinforcing metal strips and mesh is shown;
[0041] Figure 8 This is a schematic diagram (style 2) of the precast mesh formed by the mesh fabrication method in this embodiment of the present disclosure;
[0042] Figure 9 This illustrates a connection method between a prefabricated mesh component and an extended metal strip;
[0043] Figure 10 The preset removal area and its preset boundary are shown on the mesh surface;
[0044] Figure 11 Two structural forms are shown to facilitate the breaking of extended metal strips;
[0045] Figure 12 This illustration shows one splicing configuration (3 mesh surfaces) of the netting manufacturing method in an embodiment of this disclosure;
[0046] Figure 13 Another splicing form (2 mesh surfaces) of the netting manufacturing method in this embodiment is shown;
[0047] Figure 14 Several splicing methods for achieving large-size photomasks are illustrated for reference.
[0048] Figure 15 A schematic diagram illustrating the application of tension force on a mesh preform and an extended metal strip is shown for reference.
[0049] The image is labeled as follows:
[0050] 10 prefabricated frame components;
[0051] 11 frames, 111 frame slots;
[0052] 12 reinforced metal strips;
[0053] 20 precast mesh panels;
[0054] 21 mesh surface, 211 mesh surface preset boundary, 212 mesh surface end groove;
[0055] 22 Extended metal strip, 221 Half-etched line, 222 Through-etched line. Detailed Implementation
[0056] In this specification, it will also be understood that when an element is referred to as being "connected" to other elements relative to them, such as "connected to" other elements, the element may be directly connected to or directly coupled to the element, or there may be an intervening third element; in addition, in embodiments of this disclosure, "connection" is primarily a mechanical connection, especially a fixed connection such as a weld.
[0057] The present disclosure will now be described more fully below with reference to the accompanying drawings. However, the present disclosure may be implemented in many different ways and should not be construed as limited to the embodiments set forth herein. Rather, these embodiments are provided herein to make the disclosure more detailed and complete, and to fully convey the scope of the disclosure to those skilled in the art. The same reference numerals denote the same objects throughout the drawings.
[0058] In some embodiments of this disclosure, for ease of explanation, reference directions such as "first direction" and "second direction" are introduced. Figure 4 The reference coordinate axes shown are used as a baseline. Furthermore, the arrows in the accompanying drawings indicate the direction of the forces acting on the various components of the mask plate when the mesh is stretched / tensioned to adjust the mesh surface.
[0059] The "mask tension" described in the embodiments is, explanatoryly, explained in the OLED manufacturing process, when performing physical vapor deposition (such as evaporation) or chemical vapor deposition (such as forming an encapsulation film), tension needs to be applied to the mask to make it taut and adhere to the substrate. In order to ensure that the deformation of each component of the mask is consistent at this time, the assembly of each component of the mask needs to be carried out in a tensioned state, that is, assembled under the tension corresponding to that applied during use.
[0060] To more clearly illustrate the technical ideas that differ from the prior art in the embodiments of this disclosure, the following is an exemplary description of the method of the prior art to solve the technical problem of "small size of metal mask raw material sheet".
[0061] Method 1, such as Figure 14 As shown in Figure a, in the prior art, a large-size mesh surface is divided into two or more smaller-size mesh surfaces and then spliced together. Figure 14 As shown by the tension arrow in Figure a, tension cannot be applied at the joints of the mesh. The mesh stretching and morphological adjustments made through tension can only affect the three edges of the mesh, making it difficult to guarantee mesh accuracy. Alternatively, to compensate for the aforementioned problems, design compensation (special compensation for the edges that cannot bear force) can be used. However, considering the numerous holes or complex patterns on the mesh, this may exceed the computational capabilities or resolution of existing calculation tools (such as finite element analysis software). Designing compensation is difficult, inaccurate, and not easy to implement.
[0062] Method 2, such as Figure 14As shown in b, the entire mesh surface is divided into multiple smaller mesh surfaces with patterns (openings) along its long axis, and these smaller mesh surfaces are arranged sequentially, with each end welded to the long side of the frame. From... Figure 14 As shown by the tension arrow in Figure b, during splicing, the mesh surface can only withstand tension in the direction parallel to the short side of the frame, and this method cannot effectively guarantee the morphological accuracy of the mesh surface.
[0063] Method 3, such as Figure 14 As shown in Figure c, the desired opening / pattern is formed by interlacing multiple metal strips (without patterns or openings) in the warp / weft direction. This method is complex, has low precision, and can only produce products with large openings, such as encapsulation layer masks, while it is difficult to apply to products with complex or tiny patterns, such as FMM masks.
[0064] In summary, all existing methods suffer from poor precision or low production efficiency. The root cause lies in the inability to apply tension to the joints of adjacent meshes during splicing, preventing each mesh from being omnidirectionally stretched. This can only be compensated for through methods such as compensation calculations. Precision is a core key indicator for metal mask products, and its quality directly affects the product specifications and performance. The aforementioned methods are all detrimental to the final display panel product quality.
[0065] Considering the various shortcomings of existing technologies and not wanting to be bound by any theories, this disclosure provides a method for fabricating a photomask by stretching multiple small-sized mesh surfaces. The method aims to enable multiple small-sized mesh surfaces to be stretched omnidirectionally and accurately, and then spliced together in the stretched state to form a large-sized photomask, effectively ensuring the morphological accuracy of the mesh surfaces, thereby improving the product quality of the final display panel.
[0066] Therefore, this disclosure provides a method for manufacturing a photomask mesh, including as follows: Figure 1 The overall steps shown are as follows:
[0067] S1. Provides a frame 11, multiple sheets 21, at least one reinforcing metal strip 12, and multiple extension metal strips 22.
[0068] S2a. Form a frame prefabricated component 10, tension the reinforcing metal strip 12 and fix it across the frame 11, with the reinforcing metal strip 12 set at the preset splicing positions of multiple mesh surfaces 21 on the frame 11.
[0069] like Figure 13 As shown, this includes two mesh surfaces 21, one above the other. Taking the upper mesh surface as an example, its left, right, and upper ends are all splicing ends with the frame 11, allowing for unobstructed clamping and pulling to stretch the mesh. However, the lower end of this mesh surface is splicing end with other mesh surfaces; if clamped, the grippers would damage the lower mesh surface, thus preventing direct clamping. To optimize this problem, the embodiment includes the following steps:
[0070] S2b. Forming the precast mesh 20 includes fixing one end of one or more extended metal strips 22 to the splicing end of the mesh 21 with other mesh surfaces, and extending the other end of the extended metal strips away from the mesh 21. This step allows tension to be indirectly applied to the splicing end with other mesh surfaces during the meshing process by clamping the extended metal strips 22.
[0071] Steps S2a and S2b can be performed in any order.
[0072] For example, the frame prefabricated component 10 formed in step S2a is as follows: Figure 2 As shown in the figure, the arrows represent the tension force applied to the reinforcing metal strip, which is applied to both ends of the reinforcing metal strip 12 that are fixedly connected to the frame 11.
[0073] The mesh prefabricated component 20 formed in step S2b can specifically be of two styles, including, for example... Figure 3 The style shown is 1 and as shown Figure 8 Style 2 is shown. (As shown) Figure 3 As shown, one end of the mesh surface 21 of style 1 is fixedly connected to multiple extended metal strips 22, and as... Figure 8 As shown, the two opposite ends of the mesh surface 21 of style 2 (both of which are preset splicing ends with other mesh surfaces) are provided with multiple extended metal strips 22 in opposite directions.
[0074] In this embodiment, the mesh prefabricated component 20 of style 2 is particularly suitable for being placed between two mesh prefabricated components 20 of style 1. Since both ends are connected to other mesh surfaces, the mesh surface in the mesh prefabricated component 20 at this position can only rely on the two sides of the adjacent frame to apply tension. In this embodiment, by using multiple extended metal strips 22 in opposite directions, all four sides of the mesh surface can be subjected to tension, so that the mesh surface can be accurately stretched and then fixed in the frame.
[0075] by Figure 12 Taking the mask plate shown as an example, it is formed by splicing together three mesh surfaces: upper, middle, and lower. The upper and lower mesh surfaces are formed based on the mesh surface prefabricated parts of style 1 mentioned above, while the middle mesh surface, with both ends connected to other mesh surfaces, is formed based on the mesh surface prefabricated parts of style 2 mentioned above.
[0076] Although the accompanying drawings show two extended metal strips 22 on one side, the embodiments of this disclosure are not limited to this, and there may be any number of extended metal strips 22. It should be noted that the extended metal strips 22 need to be connected within the range of the ribs parallel to them, including but not limited to the portion of the mesh edge in the rib extension direction. Preferably, the number of extended metal strips 22 is equal to the number of ribs in that direction, and preferably the connection point is the intersection of the rib center lines extending around the mesh pattern / opening.
[0077] In a typical embodiment, such as Figure 4 As shown, the extension direction of each rib is parallel to the first direction and the second direction, respectively, and the major axis of each extended metal strip 22 is parallel to the second direction. The first direction is defined as the direction of the seam between adjacent mesh surfaces, and is also the direction of the major axis of the reinforcing metal strip 12; the second direction is perpendicular to the first direction.
[0078] In another typical embodiment, the extension direction of the aforementioned ribs is not limited to, for example... Figure 4 The directions shown are parallel to the first and second directions, respectively, as shown in the figure. Figure 15 As shown, the metal strips can also have a certain angle (0-180°) with the first and second directions. Furthermore, the multiple extended metal strips 22 fixed on the same mesh surface can also have angles with each other and with the first and second directions.
[0079] Step S3. Spread the net, as follows Figure 4 As shown, the splicing ends of the extension metal strip 22, the mesh surface 21 and the frame 11 are clamped and pulled respectively to make the mesh surface 21 taut.
[0080] In a typical embodiment, such as Figure 4 As shown, the tension in the first and second directions applied to the mesh surface in the mesh preform 20, and the tension in the second direction applied to the extension metal strip 22, are tension forces parallel to the first and second directions applied directly to the mesh surface and the extension metal strip 22 by the mesh tensioning device.
[0081] In another typical embodiment, the tension in the first and second directions applied to the mesh surface in the mesh preform 20 can be interpreted as the resultant force of the tensile forces acting at that location or edge of the mesh surface, which is substantially along the first and second directions. The tension in the second direction applied to the extension metal strip 22 can be interpreted as the resultant force of the tensile forces applied to different extension metal strips 22 fixed at a location on the same side of the mesh surface, which is substantially along the second direction.
[0082] For example, such as Figure 15 As shown, in the stretched state, tension F1 and tension F2 are applied to the right side of the mesh surface in the mesh preform 20, and the resultant force of F1 and F2 forms a tension substantially along the first direction; and in the stretched state, tension F1′ and tension F2′ are applied to the two extended metal strips 22 on the lower side of the mesh surface in the mesh preform 20, and the resultant force of F1′ and F2′ forms a tension substantially along the second direction.
[0083] like Figure 4As shown in the figure, the edges of the two mesh surfaces that connect with the frame can be directly clamped and stretched. At the junction of the two mesh surfaces, tension is applied by extending the metal strip 22. Thus, tension is applied to all four edges of each mesh surface, which can stretch the mesh surface completely. The shape of the mesh surface can be corrected by adjusting the tension of the four edges.
[0084] When tension is applied to both opposite ends of the mesh surface via the extended metal strip 22, for example... Figure 8 The mesh surface 21 in the mesh prefabricated component shown in the figure has its tension in the second direction entirely derived from the clamping and pulling of the extended metal strip 22.
[0085] When tension is applied to one end of the mesh surface via an extended metal strip 22, and the other end is clamped directly to the edge without an extended metal strip, for example... Figure 4 The tension in the second direction of the two mesh surfaces shown in the figure comes from the clamping and pulling of the extended metal strip 22.
[0086] S4. Splicing: Maintaining the tensioned state of step S3, fix the splicing end of the mesh surface 21 to the reinforcing metal strip 12, and fix the splicing end of the mesh surface 21 to the frame 11 to the frame 11, wherein adjacent mesh surfaces are fixed to the same reinforcing metal strip 12.
[0087] For example, the fastening in the steps can be welding or bonding with adhesive, etc.
[0088] S5. Remove the extended metal strip 22 to obtain the mask plate.
[0089] In a preferred embodiment, the length of the extended metal strip 22 is defined. The length of the extended metal strip 22 must be set to ensure that the clamping mechanism can clamp it correctly. Preferably, since it is necessary to avoid the clamping device contacting / damaging the mesh surface as much as possible, Figure 4 As shown, the end of the extended metal strip 22 needs to extend to the frame 10.
[0090] In a preferred embodiment, the end of the extended metal strip 22 needs to extend beyond the outer edge of the frame 10.
[0091] In a preferred embodiment, such as Figure 3 or Figure 8 As shown, the mesh surface 21 includes openings or patterns (cells) for forming the mesh pattern, and ribs surrounding the openings; in the step of forming the mesh preform 20, one end of the extended metal strip 22 is fixed to the rib; the fixed extended metal strip 22 and the rib are parallel.
[0092] In a preferred embodiment, such as Figure 8As shown, in the step of forming the mesh preform 20, two sets of equal numbers of extended metal strips 22 are respectively fixed to opposite ends of the mesh. More preferably, the extended metal strips 22 at different ends are staggered.
[0093] In a preferred embodiment, the net stretching step includes clamping two sets of extended metal strips 22 at both ends of the net surface and applying tension in opposite directions.
[0094] In an optional embodiment, the openings / patterns on each mesh surface can be the same, such as... Figure 13 Alternatively, each mesh surface can have different openings / patterns, such as... Figure 12 According to the actual production process, different mesh surfaces used in different processes can be integrated into the same mask frame using the method in this embodiment, which helps to improve production efficiency and reduce production costs.
[0095] In an optional embodiment, the sizes of the mesh surfaces can be the same or different. Typically, the mesh surfaces are oriented along the short side of the mask frame (e.g., ...). Figure 4 The dimensions in the first direction are the same, while those in the long side direction of the mask frame (e.g.) are different. Figure 4 The dimensions may vary in the second direction of the mesh. To ensure that the tension of the mesh can be maintained in all directions, each mesh must completely fill the entire opening of the mask frame after splicing. All edges of each spliced mesh must be fixed to the prefabricated frame components (including the frame or reinforcing metal strips).
[0096] In a preferred embodiment, such as Figure 4 As shown, the extended metal strips 22 in the different mesh prefabricated components 20 are arranged in an alternating manner.
[0097] In a preferred embodiment, during the step of forming the frame prefabrication, the reinforcing metal strip 12 is stretched across and fixed to the frame 11, specifically including: as follows Figure 5 As shown, a frame groove 111 is formed on the frame 11. The depth of the frame groove 111 is the same as the thickness of the reinforcing metal strip 12. The end of the reinforcing metal strip 12 that connects to the frame 11 is placed in the frame groove, and the bottom of the reinforcing metal strip 12 is fixedly connected to the bottom of the frame groove 111. In this embodiment, by setting the frame groove 111, the reinforcing metal strip 12 can be embedded in the frame 11. Preferably, its top surface is flush with the top surface of the frame (the surface connecting the mesh surface), so that the height of the connection between the mesh surface and the frame, and the connection between the mesh surface and the reinforcing metal strip 12, is flush. This ensures the flatness of the mesh surface and avoids incorrect gaseous material deposition or shadow formation at the opening edge when the mask is used.
[0098] like Figure 4As shown, the mask plate formed in the aforementioned embodiment maintains the tension at the splicing point of the mesh surface through the reinforcing metal strip 12 between adjacent mesh surfaces, resulting in better mesh surface flatness.
[0099] The method of fixing the reinforcing metal strip 12 directly to the mesh surface can be, for example... Figure 6 As shown, the mesh surface 21 is positioned above the reinforcing metal strip 12, and its bottom is welded to the top of the reinforcing metal strip 12.
[0100] In another preferred embodiment, such as Figure 7 As shown, two "L"-shaped grooves are formed at the two edges of the top of the reinforcing metal strip 12, and the mesh 21 is embedded and fixed in the "L"-shaped grooves. In this scheme, the bottom of the mesh 21 is welded to the top of the reinforcing metal strip 12, and the end of the mesh 21 is welded to the side wall of the "L"-shaped groove. This makes the mesh 21 and the reinforcing metal strip 12 have more welding points, which makes the mask plate better able to withstand the stress in the second direction and avoids the warping of the end of the mesh 21 (where it is connected to the reinforcing metal strip 12) due to tension.
[0101] In a preferred embodiment, in the step of forming the mesh preform, such as Figure 9 As shown, a mesh end groove 212 is provided at the end of the mesh surface 21, and one end of the extended metal strip 22 is embedded in the mesh end groove 212 and fixed to the mesh surface 21. The upper surface of the extended metal strip 22 is flush with the upper surface of the mesh surface 21. This arrangement allows the remaining portion (welded end) of the extended metal strip 22 after removal in step S5 to be accommodated in the mesh end groove 212, avoiding affecting the flatness of the mesh surface.
[0102] Regarding the method for removing the extension metal strip 22 in step S5, in a preferred embodiment, such as... Figure 11 As shown, the extended metal strip 22 is provided with a half-etched line 221 or a dashed through-etched line 222, making the metal strip easy to break at this point; when it is necessary to remove the extended metal strip 22, the extended metal strip 22 is broken along the half-etched line 221 or the through-etched line 222.
[0103] Optionally, the semi-etched line 221 can be set on one surface of the extended metal strip 22, or it can be set on two surfaces opposite each other (e.g., Figure 11 ).
[0104] In a preferred embodiment, the method for removing the extension metal strip 22 in step S5 involves using a laser to cut off the portion of the extension metal strip 22 that is not embedded in the aforementioned mesh end groove 212.
[0105] In another typical embodiment, such as Figure 10 As shown, a preset cutting area is set on the mesh surface, for example... Figure 10The area below the preset boundary 211 of the mesh surface. And one end of the extended metal strip 22 is fixed to the preset cutting area; when it is necessary to remove the extended metal strip 22, the preset cutting area and the extended metal strip 22 thereon are cut off together.
[0106] The finished mask plate, after splicing and removal of the extension metal strip, is as follows: Figure 12 , Figure 13 As shown.
[0107] In a preferred embodiment, the wire mesh stretching step further includes: adjusting the wire mesh prefabricated component, which involves adjusting the wire mesh prefabricated component 20 using a wire mesh stretching device so that the opening shape of the wire mesh surface in the wire mesh prefabricated component 20 meets the requirements.
[0108] In this embodiment, when the accuracy requirement is relatively low, multiple prefabricated mesh components can be assembled by sequentially tensioning and splicing the mesh.
[0109] When high precision is required, the prefabricated mesh components on both sides of the reinforcing metal strip need to be stretched and spliced simultaneously to avoid the reinforcing metal strip being pulled to one side and deformed after welding on one side, which would adversely affect the precision of the final product. In the embodiment of simultaneous stretching and splicing, the extended metal strips on different mesh surfaces and the extended metal strips at different ends of the same mesh surface need to be staggered to avoid interference from the clamps.
[0110] In the foregoing embodiments, preferably, the fixing is specifically laser welding.
[0111] This disclosure also provides a mask plate, which is formed by the mask plate mesh fabrication method described in any of the foregoing embodiments or their preferred or optional embodiments. It has all the structural features described in the foregoing method embodiments, and due to space limitations, it will not be repeated in this disclosure.
[0112] The above description is only a partial embodiment of this disclosure, but the scope of protection of this disclosure is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the technical scope disclosed in the embodiments of this disclosure should be included within the scope of protection of this disclosure. Therefore, the scope of protection of this disclosure should be determined by the scope of the claims.
Claims
1. A method for manufacturing a photomask mesh, characterized in that, include: Provides a frame (11), multiple mesh panels (21), at least one reinforcing metal strip (12), and multiple extending metal strips (22); A frame prefabricated component (10) is formed, and the reinforcing metal strip (12) is tensioned and fixed across the frame (11). The reinforcing metal strip (12) is set at the preset splicing position of the plurality of mesh surfaces (21) on the frame (11). Form a prefabricated mesh (20), fix one end of one or more of the extended metal strips (22) to the splicing end of the mesh (21) and other meshes, and extend the other end away from the mesh (21); The net is used to clamp and pull the splicing ends of the extended metal strip (22), the mesh surface (21), and the frame (11) respectively, so that the mesh surface (21) is taut; Splicing, maintaining the stretched net state, fixing the splicing end of the net surface (21) and other net surfaces to the reinforcing metal strip (12), fixing the splicing end of the net surface (21) and the frame (11) to the frame (11), wherein adjacent net surfaces are fixed to the same reinforcing metal strip (12); Remove the extended metal strip (22).
2. The method for manufacturing a mask plate mesh according to claim 1, characterized in that, The mesh (21) includes openwork openings or patterns, and ribs surrounding the openings or patterns; The formation of the mesh preform (20) includes fixing one end of the extended metal strip (22) to the rib, wherein the fixed extended metal strip (22) and the rib are parallel.
3. The method for manufacturing a mask plate according to claim 1, characterized in that, The formation of the prefabricated mesh (20) includes fixing two sets of extended metal strips (22) of the same number to the two splicing ends of the mesh and other mesh surfaces respectively. The tension net includes clamping the two sets of extended metal strips (22) respectively and applying tension in opposite directions to each.
4. The method for manufacturing a mask plate according to claim 1, characterized in that, The prefabricated mesh (20) includes a mesh end groove (212) provided at the end of the mesh (21), and one end of the extended metal strip (22) is embedded in the mesh end groove (212) and fixedly connected to the mesh (21).
5. The method for manufacturing a mask plate according to claim 4, characterized in that, The extended metal strip (22) is provided with a half-etched line (221) or a dashed through-etched line (222); The removal of the extension metal strip (22) includes breaking the extension metal strip (22) along the half-etched line (221) or through-etched line (222).
6. The method for manufacturing a mask plate according to claim 4, characterized in that, The removal of the extension metal strip (22) includes cutting off the portion of the extension metal strip (22) that is not embedded in the mesh end groove (212) by laser.
7. The method for manufacturing a mask plate according to claim 1, characterized in that, The formation of the prefabricated mesh (20) includes setting a preset cutting area on the mesh surface and fixing one end of the extended metal strip (22) to the preset cutting area; The removal of the extended metal strip (22) includes cutting off the preset cutting area.
8. The method for manufacturing a mask plate according to claim 1, characterized in that, In the different mesh prefabricated components (20), the extended metal strips (22) are arranged in an alternating pattern.
9. The method for manufacturing a mask plate according to claim 1, characterized in that, The netting includes adjusting the openings or patterns on the netting surface.
10. A photomask, characterized in that, The mask plate is manufactured by the mask plate mesh fabrication method according to any one of claims 1 to 9.
Citation Information
Patent Citations
Manufacturing method of mask plate and mask plate
CN107740041A
Mask plate and preparation method thereof
CN110629156A