A high directivity optical fiber transducer based on a hollow optical fiber and a manufacturing method thereof
By welding hollow optical fibers to quartz optical fibers and filling them with composite PDMS material, the problems of complex structure and poor directionality of optical fiber transducers in the field of photoacoustic technology have been solved, achieving high-directional photoacoustic response and fast propagation, making it suitable for a variety of special environments.
Patent Information
- Application Number
- CN202411154910.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2044-08-22
AI Technical Summary
Existing fiber optic transducers in the field of photo-induced ultrasound suffer from problems such as complex structure, cumbersome manufacturing process, high equipment requirements, high cost, poor directionality, and insufficient stability.
The method employs the welding of hollow optical fiber and quartz optical fiber, with the interior filled with composite PDMS material. The hollow optical fiber tube wall guides the propagation of sound waves, simplifying the optical path design, enhancing directivity, and achieving photothermal conversion and thermoacoustic conversion through a simple fabrication process.
It achieves high-directional photoacoustic response with fast speed, low loss, and applicability to various special environments, reducing maintenance costs and enhancing sound wave propagation distance and signal acquisition capabilities.
Smart Images

Figure CN118988694B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of photo-induced ultrasound technology, specifically relating to a highly directional fiber optic transducer based on hollow optical fiber and its fabrication method. Background Technology
[0002] Photoacousticization involves a complex energy conversion mechanism, primarily comprising two consecutive stages: photothermal conversion and thermoacoustic conversion. In this process, the photoacoustic effect first relies on photothermal conversion, where light energy is absorbed by a light-absorbing material and converted into heat energy. Subsequently, the heat energy further generates ultrasonic waves through thermoacoustic conversion. Fiber optic ultrasonic transducers possess many advantages over non-fiber optic platforms, such as high sensitivity, wide bandwidth distribution, excellent long-range transmission capability, and lightweight design. These characteristics have led to the widespread application of fiber optic ultrasonic transducers in numerous fields, including medical imaging, structural health monitoring, industrial process control, acoustic sensing, and marine exploration.
[0003] Currently, domestic and international patents have proposed photo-induced ultrasonic transducers with different structures, each with its own advantages and disadvantages in terms of structure and design.
[0004] For example, in the existing technology "Optomechanical Effects Occurring in a Hybrid Metal-Halide Perovskite Single Crystal Based on Photoinduced Resonant Ultrasound Spectroscopy," Tisdale Jeremy T et al. from the University of Tennessee used RUS (Resonant Ultrasound Spectroscopy) to measure photoinduced ultrasonic effects in a hybrid metal halide perovskite single crystal under CW (Continuous Wave) laser irradiation. However, the RUS measurement technique in this study requires high-precision instruments and complex data analysis, increasing the difficulty and cost of the experiment. In contrast, the experimental setup process described in this patent is simple and inexpensive.
[0005] For example, in the existing technology "Hybrid optical fiber for light-induced superconductivity," Evgeny Sedov et al. from Vladimir University, Russia, designed a light-induced superconducting fiber mediated by exciton-polariton Bose-Einstein condensate. However, the stability and durability of the new material used in practical applications still need to be verified, and it may face environmental impacts and degradation issues during long-term use. The fiber material in this patent is mature and suitable for measurement applications in various extreme environments such as underwater and high-altitude areas.
[0006] Furthermore, based on a search of relevant technologies, the following is found:
[0007] Firstly, Chinese patent application CN116299837B utilizes micro-nano optics technology to etch the fiber core on the fiber end face, forming a 45° tilted grating. It then employs sputtering and dip-coating methods to fabricate an FP resonant cavity on the fiber end face to detect photoinduced ultrasonic echo signals. A graphene array and polystyrene composite material are coated onto the pulsed laser emission point of the multimode fiber tilted grating as a photoinduced ultrasonic transducer, generating photoinduced ultrasonic signals for endoscopic imaging. This design involves multiple complex processes such as fiber core etching, sputtering, and dip-coating, making the manufacturing process cumbersome and requiring advanced equipment and processes. In contrast, the fiber connection operation in this patent is simple and does not easily damage the fiber structure.
[0008] Secondly, Chinese patent application CN107050673A provides a focused photo-induced ultrasound material, its preparation method, and an endoscopic photo-induced ultrasound probe. However, the 3D printing technology based on mask image projection stereolithography in this design is complex, and the high-precision 3D printing equipment and preparation process require high precision and stability, increasing manufacturing and maintenance costs. In contrast, the design in this patent is simple and reduces usage and maintenance costs.
[0009] Based on various studies, the main structures for optical fiber applications in photosonography include air chambers formed by chemical etching and annular cavities covered with thick coatings of composite PDMS material. Each of these methods has its own drawbacks. For example, chemical etching for air chambers is complex and results in structural instability after welding; directly filling annular cavities with composite PDMS material leads to poor directionality and significant heat loss.
[0010] In comparison, the hollow fiber structure for highly directional photoacoustic effects proposed in this invention achieves significant improvements in fiber optic transducer design and functionality. The internal cavity of the hollow fiber facilitates the filling of composite materials, providing space for photoacoustic conversion. The hollow fiber's walls naturally guide the propagation direction of the generated ultrasound, enhancing the directionality of ultrasound transmission and enabling it to propagate over longer distances in a specified direction. Furthermore, the method of fabricating the fiber optic transducer utilizes the welding of hollow fiber to silica fiber, further enhancing the system's structural directionality. The hollow fiber also protects the internal composite PDMS material from detaching in complex underwater environments. The overall fabrication process is simple, making it more suitable for photoacoustic applications requiring low loss and high directionality. Summary of the Invention
[0011] The purpose of this invention is to provide a highly directional fiber optic transducer based on hollow fiber and its fabrication method, which simplifies optical path design, has low loss, high directionality, fast photoacoustic response speed, is simple to prepare, and is suitable for various special environments.
[0012] The specific technical solution adopted by this invention is as follows:
[0013] A highly directional fiber optic transducer based on hollow optical fiber includes a quartz optical fiber with a hollow optical fiber fixed at one end. The hollow optical fiber is filled with a composite PDMS material, with a gap between the composite PDMS material and the quartz optical fiber. During operation, the quartz optical fiber transmits optical signals, and the composite PDMS material fills the air cavity inside the hollow optical fiber for photothermal and thermoacoustic conversion. Compared with traditional thermistor materials and thermistor circuits, it has a rapid response, high photoacoustic conversion efficiency, good mechanical properties, obvious sound frequency vibration, and easy signal acquisition. The outer wall of the hollow optical fiber plays a certain guiding role in the transmission process after the sound wave is generated, making the sound wave propagation direction more concentrated, thereby enhancing the effective propagation distance.
[0014] The quartz optical fiber is either a single-mode fiber or a multimode fiber.
[0015] The quartz optical fiber includes an outer sheath and a fiber core located inside the outer sheath.
[0016] The outer sheath has a diameter of 60–2000 μm, and the fiber core has a diameter greater than 5 μm.
[0017] The composite PDMS material is filled inside the hollow optical fiber with a thickness of 40–200 μm.
[0018] A method for fabricating a highly directional fiber optic transducer based on hollow fiber includes the following steps:
[0019] S1: Mix MWCNT, 1-pyrenebutyric acid and thionyl chloride, transfer the mixed solution to a round-bottom flask, and reflux at 100°C for 30 min to obtain pyrenebutyryl chloride and remove unreacted thionyl chloride;
[0020] Next, the product, from which unreacted thionyl chloride has been removed, was left to stand overnight in tetrahydrofuran with oleylamine and triethylamine.
[0021] Then, the product was washed with diethyl ether to remove unreacted tetrahydrofuran, sodium sulfate was added to the washed product, and the product was placed in a vacuum drying oven to dry MWCNT to constant weight to obtain pyrene-butyryl-functionalized MWCNT product.
[0022] Functionalized MWCNTs were dissolved in xylene, stirred evenly, and then subjected to ultrasonic oscillation to obtain a stable MWCNT / xylene solution.
[0023] S2: Mix the PDMS prepolymer with the PDMS crosslinking agent, and weigh xylene as a solvent. Pour the mixed PDMS prepolymer and crosslinking agent mixture into the solvent and stir until the PDMS is completely dissolved in the xylene to form a homogeneous solution.
[0024] S3: Take the MWCNT / xylene solution obtained in step S1, mix it with the PDMS / xylene solution obtained in step S2, and treat it with ultrasonic vibration to obtain a composite PDMS material;
[0025] S4: After filling the hollow optical fiber cavity with the composite PDMS material, heat the composite PDMS material to solidify it.
[0026] S5: The hollow optical fiber filled with the composite PDMS material is fixedly connected to the quartz optical fiber.
[0027] In step S1, MWCNT, 1-pyrenebutyric acid, and thionyl chloride are mixed in a mass ratio of 1:3:5, and oleylamine and triethylamine are mixed in a mass ratio of 35:71.
[0028] In step S1, the ultrasonic oscillator is used to treat the device with ultrasonic oscillation at 1 kHz and 5 W for 1 hour.
[0029] In step S2, the prepolymer and PDMS crosslinking agent are mixed in a mass ratio of 10:1.
[0030] In step S5, the fixed connection is achieved by using an optical fiber welding component to connect the quartz optical fiber and the hollow optical fiber together by fusion welding.
[0031] In step S5, the fixed connection is achieved by using PI adhesive to connect the quartz optical fiber and the hollow optical fiber together by fusion welding.
[0032] The technical effects achieved by this invention are as follows:
[0033] The present invention provides a highly directional fiber optic transducer based on hollow fiber, which simplifies optical path design, has low loss, high directionality, fast photoacoustic response speed, is simple to manufacture, and is suitable for a variety of special environments.
[0034] The present invention discloses a highly directional fiber optic transducer based on hollow fiber. The outer wall of the hollow fiber plays a guiding role in the propagation process after the sound wave is generated, making the sound wave propagation direction more concentrated, thereby enhancing the effective propagation distance.
[0035] The present invention discloses a method for fabricating a highly directional fiber optic transducer based on hollow fiber. The method involves welding single-mode fiber to hollow fiber to form a relatively sealed air chamber, thereby providing a certain degree of physical protection for the internal composite PDMS material, further preventing material detachment, exhibiting strong anti-interference capabilities, and being flexibly applicable to special extreme environments, while reducing maintenance costs.
[0036] The present invention discloses a method for fabricating a highly directional fiber optic transducer based on hollow optical fiber. The method involves filling an air chamber with composite PDMS material for photothermal and thermoacoustic conversion. Compared with traditional thermistor materials and thermistor circuits, the transducer has a rapid response, high photoacoustic conversion efficiency, good mechanical properties, obvious sound frequency vibration, and easy signal acquisition.
[0037] The present invention discloses a method for fabricating a highly directional fiber optic transducer based on hollow optical fiber. By combining PDMS material with a high absorbency material, the photosensitive and thermosensitive properties of PDMS material are improved, the photoacoustic conversion efficiency of the material is enhanced, and its mechanical properties are optimized so that it can perform photoacoustic energy conversion better. Attached Figure Description
[0038] Figure 1 This is a cross-sectional view of a highly directional fiber optic transducer based on hollow fiber according to Embodiment 1 of the present invention;
[0039] Figure 2 This is a flowchart illustrating the preparation process of the composite PDMS material according to Embodiment 2 of the present invention;
[0040] Figure 3 This is a schematic diagram of the capillary process filling composite PDMS material in Embodiment 2 of the present invention;
[0041] Figure 4 This is a welding schematic diagram of a highly directional fiber optic transducer based on hollow fiber according to Embodiment 2 of the present invention;
[0042] Figure 5 This is a schematic diagram of the bonding of a highly directional fiber optic transducer based on hollow fiber according to Embodiment 4 of the present invention;
[0043] Figure 6 This is a schematic diagram of the hollow optical fiber with reserved air cavity in Embodiment 5 of the present invention.
[0044] The attached diagram lists the components represented by each number as follows:
[0045] 1. Quartz optical fiber; 2. Hollow optical fiber; 3. Composite PDMS material; 4. Optical fiber welded parts; 5. PI adhesive parts. Detailed Implementation
[0046] To make the objectives and advantages of this invention clearer, the invention will be specifically described below with reference to embodiments. It should be understood that the following text is merely used to describe one or more specific embodiments of the invention and does not strictly limit the scope of protection specifically claimed by the invention.
[0047] Example 1:
[0048] like Figure 1As shown, a highly directional fiber optic transducer based on hollow fiber includes a quartz fiber 1, with a hollow fiber 2 fixed to one end of the quartz fiber 1. The hollow fiber 2 is filled with a composite PDMS material 3, and a gap is left between the composite PDMS material 3 and the quartz fiber 1. During operation, the quartz fiber 1 transmits optical signals, and the composite PDMS material 3 fills the air chamber inside the hollow fiber 2 for photothermal and thermoacoustic conversion. Compared with traditional thermistor materials and thermistor circuits, it has a rapid response, high photoacoustic conversion efficiency, good mechanical properties, obvious sound frequency vibration, and easy signal acquisition. The outer wall of the hollow fiber 2 plays a certain guiding role in the transmission process after the sound wave is generated, making the sound wave propagation direction more concentrated, thereby enhancing the effective propagation distance.
[0049] like Figure 1 As shown, the quartz optical fiber 1 is a single-mode or multi-mode optical fiber. When working, it can transmit multiple sets of optical signals and change the photothermal conversion and thermoacoustic conversion rate of the composite PDMS material 3.
[0050] like Figure 1 As shown, the quartz optical fiber 1 includes an outer sheath and a fiber core located inside the outer sheath. The diameter of the outer sheath is 60 to 2000 μm, and the diameter of the fiber core is greater than 5 μm. The use of a thicker outer sheath tightly protects the fiber core and reduces the occurrence of fiber core damage.
[0051] like Figure 1 As shown, the composite PDMS material 3 is filled inside the hollow optical fiber 2 with a thickness of 40-200 μm. The cross-sectional area of the composite PDMS material 3 is much larger than that of the fiber core, which can transmit as much of the optical signal as possible from the fiber core.
[0052] Example 2:
[0053] like Figure 2 As shown, a method for fabricating a highly directional fiber optic transducer based on hollow fiber is described in step S1: The functionalization of MWCNT pyrenebutyryl by pyrenebutyric acid is as follows: 1g MWCNT, 3g 1-pyrenebutyric acid and 5g thionyl chloride are mixed, and the mixed solution is transferred to a 25ml round bottom flask and refluxed at 100℃ for 30min to obtain pyrenebutyryl chloride and remove unreacted thionyl chloride.
[0054] Next, the product was placed in 15 ml of tetrahydrofuran with 3.5 mg oleylamine and 7.1 mg triethylamine and allowed to stand overnight.
[0055] Then, wash the product with 20 ml of diethyl ether to remove unreacted tetrahydrofuran, add sodium sulfate to the washed product, and place the product in a vacuum drying oven to dry MWCNT at 60 °C to constant weight to obtain pyrene-butyryl-functionalized MWCNT product.
[0056] Functionalized MWCNTs were dissolved in 90g xylene, stirred evenly, and then placed in an ultrasonic oscillator and subjected to ultrasonic oscillation at 1kHz and 5W for 1h to obtain a stable MWCNT / xylene solution.
[0057] Step S2: In the process of preparing the composite material, MWCNT is uniformly dispersed in the PDMS material by mixing PDMS and functionalized MWCNT in a xylene solution;
[0058] Mix 10 mg of PDMS prepolymer with 1 mg of PDMS crosslinking agent at a ratio of 10:1, and weigh 89 g of xylene as a solvent. Pour the weighed PDMS prepolymer and crosslinking agent mixture into the xylene solution and stir with a magnetic stirrer until the PDMS is completely dissolved in the xylene to form a homogeneous solution.
[0059] Step S3: Take 90g of the MWCNT / xylene solution obtained in step S1, mix it with the PDMS / xylene solution obtained in step S2, and then treat it with ultrasonic vibration.
[0060] After ultrasonic oscillation, the solution was stirred for another 10 minutes using a high-speed stirrer to ensure that MWCNT was uniformly dispersed in the PDMS xylene solution and to further improve the uniformity.
[0061] If air bubbles are present in the solution during stirring, the mixed solution can be placed in a vacuum degassing device for degassing treatment;
[0062] During the operation, it is necessary to check the distribution of MWCNTs in the solution to ensure that they are evenly dispersed;
[0063] Step S4: Based on the hollow optical fiber 2, the composite PDMS material solution 3 should be filled into the hollow cavity of the hollow optical fiber to clean the hollow optical fiber and ensure that the inside of the optical fiber is clean, free of dust and impurities; use ethanol or other suitable solvents to clean the hollow optical fiber.
[0064] After allowing it to stand and dry, place the prepared liquid composite PDMS material 3 into a clean reagent tube; gently insert one end of the hollow optical fiber 2 directly into the solution, such as... Figure 3 As shown, due to capillary action, the liquid will naturally fill the cavity of the hollow optical fiber 2 along the hollow optical fiber 2. After a certain amount of liquid is introduced into the hollow optical fiber 2, the hollow optical fiber 2 is immediately lifted to observe the height of the composite PDMS material 3 entering the cavity of the hollow optical fiber 2. Usually, the photo-ultrasound efficiency of the polymer composite PDMS material 3 with a thickness between 40 and 200 μm is the best. Therefore, it is necessary to repeatedly use capillary action to allow the liquid composite PDMS material 3 to enter the cavity inside the hollow optical fiber 2 until the hollow optical fiber 2 is filled to the predetermined length.
[0065] Next, the position of the composite PDMS material 3 was adjusted so that the material end was 30-50 μm away from the hollow fiber 2 end. The hollow fiber 2 was then placed horizontally in a high-temperature drying oven and heated at 80°C for 40 min to cure the composite PDMS material 3 and form a composite PDMS material layer.
[0066] Step S5: Connect the hollow optical fiber 2 filled with composite PDMS material 3 and the quartz optical fiber 1 by fusion splicing to achieve high-precision alignment and low-loss connection. Place the two optical fibers at both ends in a precision fiber optic cutter to cut them, ensuring that the cut surface is flat and smooth without gaps or bevels.
[0067] After cutting, use a high-powered microscope to inspect the fiber cross-section to ensure it is perfectly flat to guarantee welding quality. Place the fiber in the fixed slot of the fiber fusion splicer, align it with the fiber core center axis, and start the fusion splicer to perform the splicing.
[0068] During fusion splicing, the end faces of the optical fibers are melted by electric arc heating, and the two ends of the optical fibers are then joined together in the molten state. Figure 4 As shown, the fiber optic welding component 4 is coated at the welding position, wherein the fiber optic welding component 4 can be made of 353ND fiber optic curing adhesive;
[0069] After the fusion splicing is completed, the tensile test of the splice point is performed using the strength test function built into the fusion splicer to ensure that the connection is firm, thus completing the fabrication of a composite PDMS material-filled air gap dual-core optical fiber for triggering highly directional photo-ultrasonic effects.
[0070] The ingredient quantities used in this method are shown in Table 1 below:
[0071] Ingredient Quantity Table 1
[0072]
[0073]
[0074] Example 3:
[0075] The design and production process is the same as in Example 2. For similarities, please refer to Example 2. Figure 2 As shown, the difference lies in the following: After preparing composite PDMS material 3 in step S3, an additional 0.5 mg of powdered AuNP material is added, and the AuNP is dispersed in the composite material solution by ultrasonic oscillation at 1 kHz and 5 W for 30 min to form a composite.
[0076] PDMS-MWCNT-AuNP material;
[0077] The introduction of AuNP materials further enhances the absorption efficiency of the composite PDMS material for specific wavelength bands of light. The size of AuNPs is usually between 1 and 100 nm and can have different shapes, such as spherical, rod-shaped, and star-shaped. Changes in shape and size will lead to changes in the local surface LSPR (plasma resonance) effect. The LSPR of spherical AuNPs usually appears in the visible light range. As the particle size increases, the LSPR peak redshifts, further enhancing the absorption efficiency in this wavelength band, thereby further improving the photo-ultrasound efficiency of the system.
[0078] Example 4:
[0079] The design and production process is the same as in Example 2. For similarities, please refer to Example 2. Figure 5 As shown, the difference is that in step S5, the method of connecting the single-mode fiber and the hollow fiber is to use PI adhesive 5 (polyimide) to bond the fiber. Before connecting the single-mode fiber and the hollow fiber, the fiber end face is cut with a fiber optic cleaver to make it flat and smooth. The fiber end face is cleaned with alcohol and a lint-free cloth to ensure that there is no dirt or grease.
[0080] Preferably, 0.5mg PI adhesive 5 is uniformly coated on the end faces of single-mode optical fiber and hollow optical fiber, and then aligned with the end faces of the optical fiber again after coating.
[0081] Then perform initial drying on the welded joint, controlling the temperature of the bonding joint at 80-120℃ and the drying time at 30 minutes, so that the PI film gradually hardens.
[0082] The temperature at the bonding area was increased to 150–200℃, and the pre-curing time was 20 min. The temperature at the bonding area was then increased to 300–500℃, and the complete curing time was 2 h. The performance of the PI adhesive part 5 was further enhanced through the complete curing process. After cooling, the fiber bonding was verified, as well as the mechanical properties and light transmission of the fiber bonding area.
[0083] Since composite PDMS materials may decompose at high temperatures, and the temperature of the welding tip of an optical fiber welding machine is 1500–1700°C, directly using an optical fiber welding machine for welding poses a potential problem of altering the composition of the composite PDMS material.
[0084] Therefore, in Example 4, PI adhesive 5 is selected for bonding single-mode optical fiber and hollow optical fiber. The curing temperature of PI adhesive 5 is 700℃, which does not cause the composite PDMS material to decompose or denature. In addition, PI adhesive 5 is resistant to aging, solvents, and has stable chemical properties, and can be used for bonding silicon-based materials.
[0085] Example 5:
[0086] The design and manufacturing process is the same as in Example 2, and the similarities can be referred to in Example 2. The difference lies in step S4: during the process of introducing composite PDMS material into the hollow optical fiber using capillary action, an air chamber is reserved at the end, such as... Figure 6 As shown;
[0087] After introducing composite PDMS material into the hollow optical fiber using capillary action, a micro-injection pump is used to blow the composite PDMS material inside the hollow optical fiber into the other end face of the hollow optical fiber until an air cavity with a width of 40μm is reserved at the welding end face of the hollow optical fiber, and then the composite PDMS material is cured.
[0088] Example 6:
[0089] like Figure 5 As shown, the design and manufacturing process is the same as in Example 2, except that in steps S1, S2 and S3: the composite PDMS material is prepared by mixing PDMS material solution with 0.1 mg of spherical AuNP material.
[0090] Add 0.5 mg of powdered AuNP material and use an ultrasonic oscillator at 1 kHz and 5 W for 30 min to disperse AuNP in the composite material solution.
[0091] Example 7:
[0092] like Figure 5 As shown, the design and manufacturing process is the same as in Example 2, except that in steps S1, S2 and S3: the composite PDMS material is prepared by mixing 10 ml of PDMS material solution with Sudan Red solution. In this example, Sudan Red Type II is preferred.
[0093] For detailed explanation, the applicant has provided the following Table 2:
[0094] Table 2
[0095] Sudan Red dye parameter Preferred or range Example of Reference Dosage Sudan I 0.625–10 (ng / mL) 5.00ml 6ml Sudan II 0.625–10 (ng / mL) 8.00ml 8ml Sudan III 0.625–10 (ng / mL) 10.00ml 10ml Sudan IV 0.625–10 (ng / mL) 10.00ml 10ml 2-AA 0.75–10 (ng / mL) 8.00ml 8ml
[0096] When using:
[0097] The experimental procedure is the same as in Example 2, except that 10g of PDMS prepolymer and 1g of crosslinking agent are weighed and added to 89g of xylene.
[0098] Then use a magnetic stirrer to stir until the PDMS is completely dissolved and a homogeneous solution is formed;
[0099] Subsequently, 8 ml of Sudan II material was added to the solution. After the addition, the mixed solution was placed in an ultrasonic oscillator and treated with ultrasonic vibration at 1 kHz and 5 W for 30 min until a homogeneous and stable solution was formed, thus forming the composite PDMS material.
[0100] The above description is merely a preferred embodiment of the present invention. It should be noted that those skilled in the art can make various improvements and modifications without departing from the principles of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention. Structures, devices, and operating methods not specifically described or explained in this invention are implemented according to conventional methods in the art unless otherwise specified or limited.
Claims
1. A highly directional fiber optic transducer based on hollow fiber, characterized in that: Includes a quartz optical fiber (1), one end of which is fixed with a hollow optical fiber (2), the hollow optical fiber (2) is filled with a composite PDMS material (3), and a gap is left between the composite PDMS material (3) and the quartz optical fiber (1). It also includes a method for fabricating highly directional fiber optic transducers, the method comprising the following steps: S1: Mix MWCNT, 1-pyrenebutyric acid and thionyl chloride, transfer the mixed solution to a round-bottom flask, and reflux at 100°C for 30 min to obtain pyrenebutyryl chloride and remove unreacted thionyl chloride; Next, the product, from which unreacted thionyl chloride has been removed, was left to stand overnight in tetrahydrofuran with oleylamine and triethylamine. Then, the product was washed with diethyl ether to remove unreacted tetrahydrofuran, sodium sulfate was added to the washed product, and the product was placed in a vacuum drying oven to dry MWCNT to constant weight to obtain pyrene-butyryl-functionalized MWCNT product. Functionalized MWCNTs were dissolved in xylene, stirred evenly, and then subjected to ultrasonic oscillation to obtain a stable MWCNT / xylene solution. S2: Mix the PDMS prepolymer with the PDMS crosslinking agent, and weigh xylene as a solvent. Pour the mixed PDMS prepolymer and crosslinking agent mixture into the solvent and stir until the PDMS is completely dissolved in the xylene to form a homogeneous solution. S3: Take the MWCNT / xylene solution obtained in step S1, mix it with the PDMS / xylene solution obtained in step S2, and treat it with ultrasonic vibration to obtain composite PDMS material (3). S4: After filling the cavity of the hollow optical fiber (2) with the composite PDMS material (3), heat the composite PDMS material (3) to solidify it; S5: The hollow optical fiber (2) filled with the composite PDMS material (3) is fixedly connected to the quartz optical fiber (1).
2. The highly directional fiber optic transducer based on hollow fiber according to claim 1, characterized in that: The quartz optical fiber (1) is a single-mode optical fiber or a multimode optical fiber.
3. A highly directional fiber optic transducer based on hollow fiber according to claim 1, characterized in that: The quartz optical fiber (1) includes an outer sheath and a fiber core located inside the outer sheath; The outer sheath has a diameter of 60–2000 μm, and the fiber core has a diameter greater than 5 μm.
4. A highly directional fiber optic transducer based on hollow fiber according to claim 1, characterized in that: The composite PDMS material (3) is filled inside the hollow optical fiber (2) with a thickness of 40 to 200 μm.
5. A highly directional fiber optic transducer based on hollow fiber according to claim 1, characterized in that: In step S1, MWCNT, 1-pyrenebutyric acid, and thionyl chloride are mixed in a mass ratio of 1:3:5, and oleylamine and triethylamine are mixed in a mass ratio of 35:
71.
6. A highly directional fiber optic transducer based on hollow fiber according to claim 1, characterized in that: In step S1, the ultrasonic oscillator is used to treat the device with ultrasonic oscillation at 1 kHz and 5 W for 1 hour.
7. A highly directional fiber optic transducer based on hollow fiber according to claim 1, characterized in that: In step S2, the prepolymer and PDMS crosslinking agent are mixed in a mass ratio of 10:
1.
8. A highly directional fiber optic transducer based on hollow fiber according to claim 1, characterized in that: In step S5, the fixed connection is achieved by using an optical fiber welding component (4) to connect the quartz optical fiber (1) and the hollow optical fiber (2) together by fusion welding.
9. A highly directional fiber optic transducer based on hollow fiber according to claim 1, characterized in that: In step S5, the fixed connection is achieved by using PI adhesive (5) to connect the quartz optical fiber (1) and the hollow optical fiber (2) together by fusion welding.
Citation Information
Patent Citations
Focusing photoinduced ultrasound material, preparation method thereof and endoscopic photoinduced ultrasound probe
CN107050673A
A method for preparing an all-optical lateral photo-induced ultrasound self-generating and self-retracting fiber optic endoscope
CN116299837B
Sensitivity-enhanced composite multi-cavity FPI temperature sensor, preparation method and application
CN115638894A