一种调整材及退火炉炉辊的在线修磨方法
By designing adjustment materials with specific lengths and thicknesses, the problems of material loss and complexity in online furnace roll regrinding were solved, achieving efficient and low-cost furnace roll regrinding.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- SHOUGANG ZHIXIN QIAN AN ELECTROMAGNETIC MATERIALS CO LTD
- Filing Date
- 2024-08-22
- Publication Date
- 2026-07-17
AI Technical Summary
In existing technologies, online grinding of furnace rollers results in significant material loss, a complex grinding process, and increased grinding time, leading to higher costs.
An adjustment material is provided, comprising a transition section A, a grinding section, and a transition section B. The length of transition section A matches the annealing furnace production line and is used to replace the strip steel; the length of transition section B is 1-1.5 times that of the production line and is used to restore the temperature; the length of the grinding section is 3-4 times that of the production line and is used for grinding; the three are connected to simplify operation and reduce material loss.
By using a single roll of adjustment material to complete the furnace roller regrinding, material waste is reduced, regrinding time is shortened, costs are lowered, the operation process is simplified, and efficiency is improved.
Smart Images

Figure CN118990168B_ABST