Diffusion welding and quenching method for tin bronze and structural steel

CN119017009APending Publication Date: 2024-11-26SUZHOU FEIWO AVIATION TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411035940.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-31
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

There are problems such as mismatch between welding materials, unstable melt pool, risk of thermal cracks, interface reactions and welding deformation in the diffusion welding and quenching process of tin bronze and structural steel, resulting in unstable welding quality and degradation, especially during the quenching process. It is prone to cracks and deterioration, affecting the strength and toughness of the parts.

Method used

After the electroless nickel plating is used to treat structural steel, sub-temperature quenching is performed during vacuum diffusion welding, and the welding and heat treatment processes are combined. The cooling process is controlled through air-cooled quenching to avoid the impact of secondary heating on the welded joints, and in the welding temperature gradient Perform quenching to ensure that the matrix is ​​completely austenitized.

Benefits of technology

It improves welding quality and efficiency, avoids cracking and performance degradation of welded joints, shortens the process cycle, saves costs and resources, improves the strength and toughness of welded parts, and the pass rate reaches 75%.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119017009A_ABST
    Figure CN119017009A_ABST
Patent Text Reader

Abstract

The invention relates to a diffusion welding and quenching method for tin bronze and structural steel. The method comprises the following steps: firstly, carrying out chemical nickel plating on the surface of the structural steel to be processed, and wiping the nickel-plated structural steel and tin bronze with alcohol before assembly; the obtained treated tin bronze and structural steel are folded, in a vacuum diffusion welding furnace, the temperature is increased to 870 + / -10 DEG C from the room temperature at a constant speed, and first-time heat preservation and pressure maintaining are conducted; raising the temperature to 900 + / -10 DEG C at a constant speed, and carrying out heat preservation and pressure preservation for the second time; quenching at a subcritical quenching temperature to obtain a welding part; and performing rough machining, semi-finish machining, post-welding inspection, finish machining and size inspection on the obtained welding part, and warehousing after the welding part is qualified. According to the method, the machining cost is saved, the period is shortened, grain coarsening, caused by secondary heating, of a welding joint is successfully avoided, meanwhile, joint element homogenization is promoted, and the welding quality is directly improved.