Preparation method for realizing multi-effect pattern
Patent Information
- Application Number
- CN202411099618.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-26
Smart Images

Figure CN119019885A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of pigment printing, and in particular to a method for preparing a pattern with multiple effects. Background Art
[0002] With the advancement of technology and the needs of the anti-counterfeiting market, optical color-changing anti-counterfeiting technology has evolved from the original simple color change to an effect that combines color change with angle and dynamic changes in light and dark. This type of magnetic optical change is also called optical color-changing anti-counterfeiting technology. The pattern printed by optical color-changing technology will show changing colors when observed from different angles, and as the observation angle changes, a moving bright light band can be seen on the pattern. The principle of optical color-changing is that the magnetic pigment particles in the magnetic optically variable ink are transformed from a disordered state to an ordered arrangement state after being magnetized and oriented, thereby showing a special optical effect.
[0003] In the prior art, magnetic optically variable ink is used and magnetized and oriented by a specific fixed magnetic device after printing to form a corresponding pattern. Although it has an excellent optically variable effect as the angle changes, careful observation reveals that the edge of the light will basically present a relatively obvious dark area, and the light and dark will alternate as the observation angle changes. Therefore, no matter from which angle you observe, you will see light bands and dark sides, which affects the presentation of the pattern.
[0004] In order to change the existing technical problems, more than two significant features can be set on the image, each of which is reflected on a separate coating to form an image effect, and when one of the images moves in one direction, the two images presented by at least two coatings move together, but have different shapes, so that the pattern can present a more complete visual effect at multiple angles. However, the above effect needs to be produced through multiple printings and multiple fixed magnetic superpositions, which is not conducive to the control of production costs, and also increases the complexity of the production process and reduces the product yield. Summary of the invention
[0005] In order to solve the above technical problems, the present application provides a method for preparing a multi-effect pattern, the preparation method comprising:
[0006] Preparing varnish, magnetic pigment and transparent optically variable pigment, and mixing the varnish, magnetic pigment and transparent optically variable pigment to obtain ink;
[0007] Uniformly coating the ink on a substrate, and subjecting the substrate coated with the ink to a magnetization operation to form a pattern on the substrate;
[0008] The substrate with the pattern formed thereon is dried and cured to form a multiple effect pattern on the substrate.
[0009] Wherein, the mass of the pigment mixture formed by the magnetic pigment and the transparent optically variable pigment is 3% to 40% of the mass of the ink.
[0010] Wherein, the average particle size of the magnetic pigment is 5 to 100 μm, and the average particle size of the transparent optically variable pigment is 5 to 100 μm.
[0011] The mass of the magnetic pigment accounts for more than 1% of the mass of the ink, and the mass of the transparent optically variable pigment accounts for more than 2% of the mass of the ink.
[0012] Wherein, the light band transmittance of the transparent optically variable pigment is greater than or equal to 60%.
[0013] The mass of the varnish is 60% to 97% of the mass of the ink.
[0014] Wherein, the step of mixing the varnish, the magnetic pigment and the transparent optically variable pigment to obtain ink comprises:
[0015] Mixing the varnish, the magnetic pigment and the transparent optically variable pigment to obtain a mixture;
[0016] The mixture is dispersed at a low speed to obtain the ink, wherein the time for dispersing the mixture at a low speed is 10 to 40 minutes.
[0017] Wherein, the substrate comprises one of paper, metal, PET film, glass and wood.
[0018] Among them, the method of uniformly coating the ink on the substrate includes one of offset printing, gravure printing, flexographic printing, screen printing, letterpress printing, spraying and roller coating.
[0019] The method of performing drying and curing operation on the substrate forming the pattern includes at least one of UV curing method, LED curing method, electron beam curing method, oxidative polymerization drying method and physical drying method.
[0020] Beneficial effects of the present application: Different from the prior art, the preparation method for realizing a multi-effect pattern provided by the present application includes: preparing varnish, magnetic pigment and transparent optically variable pigment, mixing varnish, magnetic pigment and transparent optically variable pigment to obtain ink; uniformly coating the ink on the substrate, and performing a magnetization operation on the substrate coated with the ink to form a pattern on the substrate; performing a drying and curing operation on the substrate with the pattern formed to form a multi-effect pattern on the substrate. In the present application, due to the presence of the transparent optically variable pigment, it is ensured that the color of the magnetic pigment in the coating is not affected after magnetization orientation, the transparent optically variable pigment will not cover the magnetic pigment too much, and the transparent optically variable pigment can appear in the dark area of the magnetic pigment when the user changes the angle of viewing the image, thereby increasing the brightness of the dark area and ensuring the complete presentation of the image. Furthermore, the ink in the present application contains a transparent optically variable pigment, so that the multi-effect pattern can be obtained by only printing the ink once and magnetizing once, which simplifies the user's process of pattern manufacturing while ensuring the dynamic optical effect, reduces the manufacturing cost of the pattern, and improves the user's experience of the preparation method provided by the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0022] in:
[0023] Figure 1 It is a schematic diagram of a process of an embodiment of a preparation method provided in the present application;
[0024] Figure 2 is a flow chart of an embodiment of step S1;
[0025] Figure 3 is a schematic diagram of a first embodiment of a pattern obtained by the preparation method of the present application;
[0026] Figure 4 is a schematic diagram of a second embodiment of a pattern obtained by the preparation method of the present application;
[0027] Figure 5 is a schematic diagram of a third embodiment of a pattern obtained by the preparation method of the present application;
[0028] Figure 6 is a schematic diagram of a fourth embodiment of a pattern obtained by the preparation method of the present application;
[0029] Figure 7 is a schematic diagram of a fifth embodiment of a pattern obtained by the preparation method of the present application;
[0030] Figure 8 is a schematic diagram of a sixth embodiment of a pattern obtained by the preparation method of the present application;
[0031] Fig. 9 is a schematic diagram of a seventh embodiment of a pattern obtained by the preparation method of the present application;
[0032] Fig.10 is a schematic diagram of a first embodiment of a pattern obtained by an existing preparation method;
[0033] Fig.11 is a schematic diagram of an eighth embodiment of a pattern obtained by the preparation method of the present application;
[0034] Fig.12 is a schematic diagram of a second embodiment of a pattern obtained by an existing preparation method;
[0035] Fig.13 is a schematic diagram of a ninth embodiment of a pattern obtained by the preparation method of the present application;
[0036] Fig.14 is a schematic diagram of a third embodiment of a pattern obtained by an existing preparation method;
[0037] Fig.15 is a schematic diagram of a tenth embodiment of a pattern obtained by the preparation method of the present application;
[0038] Fig.16 It is a schematic diagram of a fourth embodiment of a pattern obtained by an existing preparation method. DETAILED DESCRIPTION
[0039] The scheme of the embodiment of the present application is described in detail below in conjunction with the drawings of the specification.
[0040] In the following description, for the purpose of explanation rather than limitation, specific details such as specific system structures, interfaces, and technologies are provided to facilitate a thorough understanding of the present application.
[0041] Reference to "embodiments" in this application means that a particular feature, structure, or characteristic described in conjunction with the embodiments may be included in at least one embodiment of the present application. The appearance of the phrase in various locations in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0042] The term "and / or" in this application is only a description of the association relationship of associated objects, indicating that there may be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the objects associated before and after are in an "or" relationship. In addition, "many" in this article means two or more than two. In addition, the term "at least one" in this article means any combination of at least two of any one or more of a plurality of, for example, including at least one of A, B, and C, and can mean including any one or more elements selected from the set consisting of A, B, and C. In addition, the terms "first", "second", and "third" in this application are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features.
[0043] In order to avoid the dark areas produced by magnetic optically variable ink after printing, the prior art generally adopts multiple printing operations and multiple magnetization operations to increase the number of coating layers so that the pattern can present a complete visual effect under different viewing angles. However, the existing technical production process is complicated, which is not conducive to the control of production costs and increases the complexity of production. Therefore, the present application provides a preparation method for a pattern with multiple effects that can be achieved with one printing, as follows:
[0044] See also Figure 1 , Figure 1 : is a flow chart of an embodiment of the preparation method provided in the present application. The preparation method for realizing a multi-effect pattern provided in the present application specifically comprises the following steps:
[0045] S1: preparing varnish, magnetic pigment and transparent optically variable pigment, and mixing the varnish, magnetic pigment and transparent optically variable pigment to obtain ink.
[0046] First, prepare varnish, magnetic pigment and transparent optically variable pigment. Varnish is a kind of oil used to adjust the viscosity or thinness of ink, and its main purpose is to improve the printing performance of ink. Magnetic pigment is a special pigment with magnetism, which can change its arrangement or show a specific visual effect under the action of an external magnetic field. Varnish and magnetic pigment on the market can be used as varnish and magnetic pigment used in this application.
[0047] Transparent photovariable pigments need to be prepared in advance. Transparent photovariable pigments are special pigments with light transmittance that can reflect colorful and changing colors according to the observation angle and the incident angle of light. Specifically, transparent photovariable pigments can be obtained through film structure design and vacuum coating with dielectric materials. In the structural design, all-dielectric nano-thin film materials with different refractive indices can be superimposed. The generated transparent photovariable pigments are free of heavy metals, safe and environmentally friendly, have strong angular color characteristics, and can show unique color changes.
[0048] In one embodiment, the light transmittance of the transparent optically variable pigment in the light band is greater than or equal to 60%.
[0049] In another embodiment, the optical transmittance of the magnetic pigment is less than or equal to 10%.
[0050] After the varnish, the magnetic pigment and the transparent optically variable pigment are prepared, the varnish, the magnetic pigment and the transparent optically variable pigment may be further mixed to obtain ink.
[0051] In one embodiment, the varnish, the magnetic pigment and the transparent optically variable pigment may be placed in a special mixing device for mixing, thereby improving the efficiency of mixing the varnish, the magnetic pigment and the transparent optically variable pigment.
[0052] S2: The ink is uniformly coated on the substrate, and the substrate coated with the ink is subjected to a magnetization operation to form a pattern on the substrate.
[0053] After obtaining the ink in step S1, the ink can be evenly coated on the substrate using a printing device, and the substrate coated with the ink is placed under a magnetic orientation device for magnetic orientation operation to form a pattern on the substrate. The magnetic orientation device can be a device in the prior art, which will not be described in detail here.
[0054] In one embodiment, the substrate may include one of paper, metal, PET film, glass, wood, etc. The material of the substrate may be selected according to the user's printing requirements, and this application does not impose any restrictions on this.
[0055] In another embodiment, the method of uniformly applying the ink to the substrate may include offset printing, gravure printing, flexographic printing, screen printing, letterpress printing, spraying, and roller coating. The present application does not limit the specific method of uniformly applying the ink to the substrate in the preparation method.
[0056] After placing the substrate coated with ink under the magnetic orientation device, the magnetic pigment in the ink moves under the action of the magnetic field generated by the magnetic orientation device to form a specific pattern, with bright and dark areas. Since the transparent optically variable pigment has light transmittance, it can be ensured that the transparent optically variable pigment does not block the magnetic pigment and affect the magnetic effect of the magnetic pigment, and the transparent optically variable pigment does not have the function of moving under the guidance of the magnetic field. Therefore, the transparent optically variable pigment is evenly distributed in the ink coating, and the transparent optically variable pigment can produce color in the dark area of the pattern formed by the magnetic pigment, increase the brightness of the dark area, and make the pattern fully presented at different viewing angles.
[0057] S3: performing a drying and curing operation on the patterned substrate to form a multi-effect pattern on the substrate.
[0058] In step S2, the ink coating applied on the substrate is magnetized to form a specific pattern, and then the substrate with the pattern can be further dried and cured to form a multiple effect pattern on the substrate, thereby ensuring the quality of the multiple effect pattern, obtaining good paint film performance, and realizing continuous pattern production.
[0059] In one embodiment, the method of drying and curing the substrate with the pattern may include at least one of UV curing, LED curing, electron beam curing, oxidative polymerization drying, physical drying, etc. For example, the present application may use UV curing to dry and cure the substrate with the pattern, or may use UV curing + oxidative polymerization drying to dry and cure the substrate with the pattern, etc. That is, the present application does not limit the specific selection of the method of drying and curing the substrate with the pattern, and the number of specific selected methods.
[0060] In summary, in the preparation method for realizing a multiple-effect pattern provided in the present application, an ink containing a transparent optically variable pigment can be prepared first. Due to the presence of the transparent optically variable pigment, the brightness of the dark area formed by the magnetic pigment can be increased, thereby ensuring the overall brightness of the specific pattern formed by the ink, ensuring the complete presentation of the pattern at each viewing angle, and improving the user experience of the multiple-effect pattern.
[0061] Furthermore, in the preparation method provided in the present application, a multiple-effect pattern can be obtained by printing the ink once and magnetizing it once. While ensuring dynamic optics, it simplifies the user's pattern manufacturing process, reduces the pattern manufacturing cost, improves the practicality of the preparation method provided in the present application, and enhances the user's experience of the preparation method.
[0062] In another embodiment, in order to reduce the number of printing times, pigments that are not affected by the magnetic field, such as color paste, can be mixed with magnetic pigments and varnish to obtain ink containing color paste. The color paste can also increase the brightness of the dark area, but because the color paste is not light-transmitting, it will affect the magnetic effect of the magnetic pigment during the magnetic operation and reduce the efficiency of the generated pattern. Therefore, in the preparation method provided in the present application, transparent optically variable pigments are the best choice.
[0063] In one embodiment, please continue to refer to Figure 2 , Figure 2 1 is a flow chart of an embodiment of step S1. In step S1, the specific steps of mixing the varnish oil, the magnetic pigment and the transparent optically variable pigment to obtain the ink include:
[0064] S21: Mixing the varnish, the magnetic pigment and the transparent optically variable pigment to obtain a mixture.
[0065] Among them, varnish, magnetic pigment and transparent optically variable pigment can be prepared first, and then the varnish, magnetic pigment and transparent optically variable pigment are mixed to obtain a mixture.
[0066] S22: Dispersing the mixture at a low speed to obtain ink.
[0067] Furthermore, a mechanical high-speed disperser can be used to disperse the mixture at a low speed to obtain ink. The time for dispersing the mixture at a low speed is 10 to 40 minutes, such as 10 minutes, 20 minutes, 25 minutes, 30 minutes, 40 minutes, etc., preferably 30 minutes. The time for dispersing the mixture at a low speed can be set based on the content of the magnetic pigment and the transparent optically variable pigment in the mixture to improve the mixing efficiency of the mixture, and this application does not limit this.
[0068] Furthermore, during the low-speed dispersion of the mixture, it can be carried out at room temperature and in a light-proof environment to prevent the ambient light from affecting the magnetic pigment and the transparent optically variable pigment in the mixture.
[0069] Wherein, the mass of the pigment mixture formed by the magnetic pigment and the transparent optically variable pigment in step S1 of the preparation method is 3% to 40% of the mass of the obtained ink.
[0070] Specifically, the mass of the magnetic pigment accounts for more than 1% of the mass of the ink, and the mass of the transparent optically variable pigment accounts for more than 2% of the mass of the ink.
[0071] like Figure 3 As stated, Figure 3Schematic diagram of the first embodiment of the pattern obtained by the preparation method of the present application. In the first embodiment, the average particle size of the magnetic pigment in the ink is 15 μm, and the mass of the magnetic pigment accounts for 1% of the mass of the ink, and the average particle size of the transparent optically variable pigment is 15 μm, and the mass of the transparent optically variable pigment accounts for 10% of the mass of the ink. Figure 3 (a) is the pattern observed from the front view. Figure 3 (b) is the pattern observed from a side perspective. It can be seen that in this embodiment, the pattern is observed from a front perspective very well, and when the pattern is observed from a side perspective, the edge of the pattern can still be clearly presented, which reflects that the use of the preparation method provided in the present application to prepare the pattern can achieve good results.
[0072] Please continue reading Figure 4 , Figure 4 Schematic diagram of the second embodiment of the pattern obtained by the preparation method of the present application. In the second embodiment, the average particle size of the magnetic pigment in the ink is 15 μm, and the mass of the magnetic pigment accounts for 3% of the mass of the ink, and the average particle size of the transparent optically variable pigment is 15 μm, and the mass of the transparent optically variable pigment accounts for 10% of the mass of the ink. Figure 4 (a) is the pattern observed from the front view. Figure 4 (b) is the pattern observed from a side perspective. It can be seen that in this embodiment, the effect of observing the pattern from a front perspective is very good. When the pattern is observed from a side perspective, the edge of the pattern can still be clearly presented, which reflects that the use of the preparation method provided in the present application to prepare the pattern can achieve good results.
[0073] Compared with the pattern presented in the first embodiment, Figure 4 The width of the bright light band in the pattern shown is wider and the brightness of the bright light band is stronger. That is, in the preparation method provided in the present application, the width and brightness of the bright light band of the prepared pattern can be increased by increasing the mass proportion of the magnetic pigment in the ink.
[0074] Please continue reading Figure 5 , Figure 5 Schematic diagram of the third embodiment of the pattern obtained by the preparation method of the present application. In the third embodiment, the average particle size of the magnetic pigment in the ink is 15 μm, and the mass of the magnetic pigment accounts for 10% of the mass of the ink, and the average particle size of the transparent optically variable pigment is 15 μm, and the mass of the transparent optically variable pigment accounts for 3% of the mass of the ink. Figure 5 (a) is the pattern observed from the front view. Figure 5 (b) is the pattern observed from a side perspective. It can be seen that in this embodiment, the effect of observing the pattern from a front perspective is very good. When the pattern is observed from a side perspective, the edge of the pattern can still be clearly presented, which reflects that the use of the preparation method provided in the present application to prepare the pattern can achieve good results.
[0075] Compared with the patterns presented in the first embodiment or the second embodiment, Figure 5 The width of the bright light band in the pattern shown is wider and the brightness of the bright light band is stronger, but when the pattern is observed from a side perspective, the clarity of the pattern edge is poorer than the patterns presented in the first and second embodiments. That is, in the preparation method provided in the present application, the width and brightness of the bright light band in the prepared pattern can be increased by increasing the mass proportion of the magnetic pigment in the ink; the brightness of the edge area in the prepared pattern can be increased by increasing the mass proportion of the transparent optically variable pigment in the ink. Users can adjust the mass proportion of the magnetic pigment and the mass proportion of the transparent optically variable pigment in the ink according to their own needs, and the present application does not impose any restrictions on this.
[0076] For further information, see Figure 6 , Figure 6 Schematic diagram of the fourth embodiment of the pattern obtained by the preparation method of the present application. In the fourth embodiment, the average particle size of the magnetic pigment in the ink is 15 μm, the mass of the magnetic pigment accounts for 10% of the mass of the ink, and the average particle size of the transparent optically variable pigment is 15 μm, and the mass of the transparent optically variable pigment accounts for 0.5% of the mass of the ink. Figure 6 (a) is the pattern observed from the front view. Figure 6 (b) is the pattern observed from the side view. It can be seen that in this embodiment, the effect of observing the pattern from the front view is better. Compared with the pattern presented in the third embodiment, when the pattern in the fourth embodiment is observed from the side view, the edge of the pattern cannot be clearly presented. By comparing the third embodiment with the fourth embodiment, it can be seen that the mass ratio of the magnetic pigment in the ink in the third embodiment is the same as the mass ratio of the magnetic pigment in the ink in the fourth embodiment, while the mass ratio of the transparent optically variable pigment in the ink in the fourth embodiment is less than the mass ratio of the transparent optically variable pigment in the ink in the third embodiment, and the integrity of the pattern observed from the side view cannot be fully reflected.
[0077] Based on the fourth embodiment, the content ratio of the transparent optically variable pigment in the ink is further increased. Please refer to Figure 7 , Figure 7 Schematic diagram of the fifth embodiment of the pattern obtained by the preparation method of the present application. In the fifth embodiment, the average particle size of the magnetic pigment in the ink is 15 μm, and the mass of the magnetic pigment accounts for 10% of the mass of the ink, and the average particle size of the transparent optically variable pigment is 15 μm, and the mass of the transparent optically variable pigment accounts for 1.5% of the mass of the ink. Figure 7 (a) is the pattern observed from the front view. Figure 7(b) is the pattern observed from the side view. It can be seen that in this embodiment, the effect of observing the pattern from the front view is better. Compared with the pattern presented in the fourth embodiment, when the pattern is observed from the side view in the fifth embodiment, the edge of the pattern is clearer, but some parts are still not clear enough. By comparing the fourth embodiment with the fifth embodiment, it can be seen that the mass ratio of the magnetic pigment in the ink in the fourth embodiment is the same as the mass ratio of the magnetic pigment in the ink in the fifth embodiment, while the mass ratio of the transparent optically variable pigment in the ink in the fourth embodiment is less than the mass ratio of the transparent optically variable pigment in the ink in the fifth embodiment. The pattern presented in the fifth embodiment is slightly clearer at the edge than the pattern presented in the fourth embodiment, but it still cannot fully reflect the integrity of the pattern observed from the side view angle.
[0078] In summary, by comparing the pattern presented in the first embodiment with the pattern presented in the second embodiment, it can be concluded that when the mass ratio of the transparent optically variable pigment in the ink is the same, increasing the mass ratio of the magnetic pigment in the ink can increase the width and brightness of the bright light area in the pattern. Figure 3 In the pattern shown, the width and brightness of the bright area in the pattern are slightly weak. Therefore, in order to ensure the quality of the bright area in the pattern, the present application proposes that the mass of the magnetic pigment accounts for more than 1% of the mass of the ink.
[0079] Furthermore, by comparing the pattern presented in the third embodiment, the pattern presented in the fourth embodiment, and the pattern presented in the fifth embodiment, it can be found that when the mass ratio of the magnetic pigment in the ink is the same, increasing the mass ratio of the transparent optically variable pigment in the ink can improve the clarity of the edge of the pattern. Figure 6 and Figure 7 The clarity of the edge of the pattern shown is still slightly weak. Therefore, in order to ensure the clarity of the edge of the pattern, the present application proposes that the mass of the transparent optically variable pigment accounts for more than 2% of the mass of the ink.
[0080] In ink, varnish is an oil used to adjust the viscosity or thickness of ink, and is used to improve the printing performance of ink. Therefore, if the mass proportion of varnish in ink is too small, it may affect the quality of ink printed on the substrate. Therefore, the present application proposes that the mass of the pigment mixture formed by the magnetic pigment and the transparent optically variable pigment is 3% to 40% of the mass of the ink, that is, the mass of the varnish is 60% to 97% of the mass of the ink. Users can adjust the mass proportion of the magnetic pigment, the mass proportion of the transparent optically variable pigment and the mass proportion of the varnish in the ink based on their needs. The present application does not limit the specific mass proportion of the magnetic pigment, the specific mass proportion of the transparent optically variable pigment and the specific mass proportion of the varnish in the ink.
[0081] In one embodiment, the average particle size of the magnetic pigment is 5 to 100 μm. For example, the average particle size of the magnetic pigment can be 5 μm, 10 μm, 15 μm, 30 μm, 45 μm, 55 μm, 60 μm, 90 μm, 100 μm, etc., among which the average particle size of the magnetic pigment is preferably 5 to 45 μm.
[0082] The average particle size of the transparent optically variable pigment is 5 to 100 μm. For example, the average particle size of the magnetic pigment can be 5 μm, 10 μm, 20 μm, 35 μm, 45 μm, 50 μm, 65 μm, 85 μm, 100 μm, etc. Among them, the average particle size of the transparent optically variable pigment is preferably 5 to 45 μm.
[0083] Please continue reading Figure 8 , Figure 8 Schematic diagram of the sixth embodiment of the pattern obtained by the preparation method of the present application. In the sixth embodiment, the average particle size of the magnetic pigment in the ink is 15 μm, and the mass of the magnetic pigment accounts for 10% of the mass of the ink, and the average particle size of the transparent optically variable pigment is 45 μm, and the mass of the transparent optically variable pigment accounts for 3% of the mass of the ink. Figure 8 (a) is the pattern observed from the front view. Figure 8 (b) is the pattern observed from a side perspective. It can be seen that in this embodiment, the effect of observing the pattern from a front perspective is very good. When the pattern is observed from a side perspective, the edge of the pattern can still be clearly presented, which reflects that the use of the preparation method provided in the present application to prepare the pattern can achieve good results.
[0084] Compared to Figure 5 The pattern presented in the third embodiment, the effect of the bright light area in the pattern presented in the sixth embodiment is basically the same as the effect of the bright light area in the pattern described in the third embodiment, and the edge of the pattern in the sixth embodiment is relatively clear as the edge of the pattern in the third embodiment. Among them, the mass ratio of the magnetic pigment in the ink and the mass ratio of the transparent optically variable pigment in the ink in the sixth embodiment are the same as the mass ratio of the magnetic pigment in the ink and the mass ratio of the transparent optically variable pigment in the ink in the third embodiment, and the average particle size of the magnetic pigment is the same, and the average particle size of the transparent optically variable pigment in the sixth embodiment is larger than the average particle size of the optically variable pigment in the third embodiment.
[0085] In summary, by comparing the pattern presented in the third embodiment with the pattern presented in the sixth embodiment, it can be concluded that within the allowable range, the change in the average particle size of the magnetic pigment and the average particle size of the transparent optically variable pigment will not affect the quality of the prepared pattern. In the range of the average particle size of the magnetic pigment being 5 to 100 μm and the average particle size of the transparent optically variable pigment being 5 to 100 μm, the present application does not limit the specific selection of the average particle size of the magnetic pigment and the average particle size of the transparent optically variable pigment.
[0086] As mentioned above, the method of uniformly applying the ink on the substrate in step S2 may include offset printing, gravure printing, flexographic printing, screen printing, letterpress printing, spraying and roller coating, etc., and different coating methods may correspond to the mass proportion of the pigment mixture formed by the magnetic pigment and the transparent optically variable pigment in the ink. For example, in the offset printing method and the flexographic printing method, the mass proportion of the pigment mixture formed by the magnetic pigment and the transparent optically variable pigment in the ink is 15% to 35%, while in the gravure printing method, screen printing method, letterpress printing method, spraying and roller coating method, the mass proportion of the pigment mixture formed by the magnetic pigment and the transparent optically variable pigment in the ink is 5% to 20%. By using different printing methods to correspond to different mass proportions of the pigment mixture formed by the magnetic pigment and the transparent optically variable pigment in the ink, the efficiency of applying the ink to the substrate is improved.
[0087] In the preparation method provided in the present application, based on the different mass proportions of varnish oil, magnetic pigment, and transparent fluorescent pigment in the ink, different colors of magnetic pigments, different colors of transparent fluorescent pigments, different ways of applying the ink to the substrate, etc., the presented pattern will have different effects. The preparation method provided in the present application is described below in conjunction with the accompanying drawings.
[0088] In one embodiment, if Fig. 9 As shown, Fig. 9 It is a schematic diagram of the seventh embodiment of the pattern obtained by the preparation method of the present application. In the seventh embodiment, 85 parts of UV screen printing ink oil, 13 parts of magnetic silver pigment and 2 parts of transparent green-to-blue light-changing pigment are used. The above raw materials are mixed in the corresponding proportions and dispersed at a low speed for 30 minutes in a mechanical high-speed disperser. The components are fully mixed to form a "multiple effect" ink. Further, the above-obtained ink is hung on black cardboard using a 250-mesh screen, and the black cardboard coated with ink is placed on a magnetic orientation device for magnetization, and the coating is UV cured to obtain a coating with multiple effects. Fig. 9 (a) is the pattern observed from the front view. Fig. 9 (b) The pattern is observed from the side.
[0089] Please continue reading Fig.10 , Fig.10 Schematic diagram of the first embodiment of the pattern obtained by the existing preparation method. Fig.10 In the pattern shown, the same proportion of UV screen printing varnish and magnetic color pigment as in the above embodiment is used to mix into ink, and the coating is prepared by the same steps as above. Fig.10 (a) is the pattern observed from the front view. Fig.10 (b) The pattern is observed from the side.
[0090] It can be seen that in the pattern prepared by the existing preparation method without adding the transparent green-to-blue photovariable pigment, the edge of the pattern is very unclear when the pattern is observed from the side. However, since the ink of the present application includes the transparent green-to-blue photovariable pigment, the edge of the generated pattern presents a blue-green effect, which further improves the clarity of the edge of the pattern, reflects the multiple effects of the pattern, reflects the necessity of adding the transparent photovariable pigment to the ink, improves the practicality of the preparation method provided by the present application, and has obvious advantages over the existing preparation methods.
[0091] Among them, when the ink is applied to the substrate by screen printing, screens with different mesh densities can also be used, specifically 200-420 mesh screens, such as 200 mesh screen, 250 mesh screen, 350 mesh screen, 400 mesh screen, etc. This application does not impose any restrictions on this.
[0092] Among them, other methods such as offset printing, gravure printing, flexographic printing, letterpress printing, spraying and roller coating can also be used to apply the processing ink on the substrate.
[0093] In another embodiment, if Fig.11 As shown, Fig.11 It is a schematic diagram of the eighth embodiment of the pattern obtained by the preparation method of the present application. In the eighth embodiment, 85 parts of UV silk screen ink oil, 13 parts of magnetic silver pigment and 2 parts of transparent blue-to-red light-changing pigment are used. The above raw materials are mixed in the corresponding proportions and dispersed at a low speed for 30 minutes in a mechanical high-speed disperser to fully mix the components to form a "multiple effect" ink. Further, the ink obtained above is hung on black cardboard using a 250 mesh screen, and the black cardboard coated with ink is placed on a magnetic orientation device for magnetization, and the UV-cured coating is obtained to obtain a coating with multiple effects. Fig.11 (a) is the pattern observed from the front view. Fig.11 (b) The pattern is observed from the side.
[0094] Please continue reading Fig.12 , Fig.12 Schematic diagram of the second embodiment of the pattern obtained by the existing preparation method. Fig.12 In the pattern shown, the same proportion of UV screen printing varnish and magnetic silver pigment as in the above embodiment is used to mix into ink, and the coating is prepared by the same steps as above. Fig.12 (a) is the pattern observed from the front view. Fig.12(b) is a side view of the pattern. It can be seen that in the pattern prepared by the existing preparation method without adding a transparent blue-to-red photovariable pigment, the edge of the pattern is very unclear when the pattern is observed from a side view, further demonstrating the practicality of the preparation method provided in the present application.
[0095] In another embodiment, if Fig.13 As shown, Fig.13 It is a schematic diagram of the ninth embodiment of the pattern obtained by the preparation method of the present application. In the ninth embodiment, 85 parts of UV silk screen ink oil, 12 parts of magnetic silver pigment and 3 parts of transparent green-to-blue light-changing pigment are used. The above raw materials are mixed in the corresponding proportions and dispersed at a low speed for 30 minutes in a mechanical high-speed disperser to fully mix the components to form a "multiple-effect" ink. Further, the ink obtained above is hung on black cardboard using a 250-mesh screen, and the black cardboard coated with ink is placed on a magnetic orientation device for magnetization, and the coating is UV cured to obtain a coating with multiple effects. Fig.13 (a) is the pattern observed from the front view. Fig.13 (b) The pattern is observed from the side.
[0096] Please continue reading Fig.14 , Fig.14 FIG. 1 is a schematic diagram of a third embodiment of a pattern obtained by an existing preparation method. Fig.14 In the pattern shown, the same proportion of UV screen printing varnish and magnetic silver pigment as in the above embodiment is used to mix into ink, and the coating is prepared by the same steps as above. Fig.14 (a) is the pattern observed from the front view. Fig.14 (b) is the pattern observed from a side perspective. It can be seen that in the pattern prepared by the existing preparation method without adding a transparent green-to-blue photovariable pigment, the edge of the pattern is very unclear when the pattern is observed from a side perspective, further demonstrating the practicality of the preparation method provided in the present application.
[0097] In other embodiments, Fig.15 As shown, Fig.15 It is a schematic diagram of the tenth embodiment of the pattern obtained by the preparation method of the present application. In the tenth embodiment, 85 parts of UV screen printing ink oil, 11 parts of magnetic red-to-green pigment and 4 parts of transparent green-to-blue light-changing pigment are used. The above raw materials are mixed in the corresponding proportions and dispersed at a low speed for 30 minutes in a mechanical high-speed disperser. The components are fully mixed to form a "multiple effect" ink. Further, the ink obtained above is hung on black cardboard using a 250-mesh screen, and the black cardboard coated with ink is placed on a magnetic orientation device for magnetization, and the UV-cured coating is obtained to obtain a coating with multiple effects. Fig.15 (a) is the pattern observed from the front view. Fig.15(b) The pattern is observed from the side.
[0098] Please continue reading Fig.16 , Fig.16 Schematic diagram of the fourth embodiment of the pattern obtained by the existing preparation method. Fig.16 In the pattern shown, the same proportion of UV screen printing varnish and magnetic red-to-green pigment as in the above embodiment is used to mix into ink, and the coating is prepared by the same steps as above. Fig.16 (a) is the pattern observed from the front view. Fig.16 (b) is the pattern observed from a side perspective. It can be seen that in the pattern prepared by the existing preparation method without adding a transparent green-to-blue photovariable pigment, the edge of the pattern is very unclear when the pattern is observed from a side perspective, further demonstrating the practicality of the preparation method provided in the present application.
[0099] In summary, by comparing the pattern obtained by the preparation method of the present application with the pattern formed in the prior art without adding transparent optically variable pigments, it can be clearly seen that the pattern obtained by the preparation method of the present application has good clarity at the edge and has a good presentation effect when observed from different viewing angles, which can meet the user's demand for pattern effects; and the pattern can be obtained by only one printing and one magnetization, which simplifies the process, reduces costs, and improves the user's experience of the preparation method provided by the present application.
[0100] Furthermore, as described above, in the preparation method provided by the present application, the width and brightness of the bright light area in the formed pattern and the clarity of the pattern edge can be changed by changing the content of the magnetic pigment and the transparent light-variable pigment. At the same time, the user can make the pattern more colorful by selecting different colors of the magnetic pigment and different colors of the transparent light-variable pigment, further meeting the needs of the user.
[0101] The above description is only an implementation method of the present application, and does not limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly used in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. A method for preparing a multi-effect pattern, It is characterized in that The preparation method comprises: Providing varnish, magnetic pigment and transparent optically variable pigment, and mixing the varnish, magnetic pigment and transparent optically variable pigment to obtain ink; Uniformly coating the ink on a substrate, and subjecting the substrate coated with the ink to a magnetization operation to form a pattern on the substrate; The substrate with the pattern formed thereon is dried and cured to form a multiple effect pattern on the substrate.
2. The preparation method according to claim 1, It is characterized in that The mass of the pigment mixture formed by the magnetic pigment and the transparent optically variable pigment is 3% to 40% of the mass of the ink.
3. The preparation method according to claim 2, It is characterized in that The average particle size of the magnetic pigment is 5 to 100 μm, and the average particle size of the transparent optically variable pigment is 5 to 100 μm.
4. The preparation method according to claim 2, It is characterized in that The mass of the magnetic pigment accounts for more than 1% of the mass of the ink, and the mass of the transparent optically variable pigment accounts for more than 2% of the mass of the ink.
5. The preparation method according to claim 2, It is characterized in that The light band transmittance of the transparent optically variable pigment is greater than or equal to 60%.
6. The preparation method according to claim 2, It is characterized in that The mass of the varnish is 60% to 97% of the mass of the ink.
7. The preparation method according to claim 1, It is characterized in that The step of mixing the varnish, the magnetic pigment and the transparent optically variable pigment to obtain ink comprises: Mixing the varnish, the magnetic pigment and the transparent optically variable pigment to obtain a mixture; The mixture is dispersed at a low speed to obtain the ink, wherein the time for dispersing the mixture at a low speed is 10 to 40 minutes.
8. The preparation method according to claim 1, It is characterized in that The material of the substrate includes one of paper, metal, PET film, glass and wood.
9. The preparation method according to claim 1, It is characterized in that The method of uniformly coating the ink on the substrate includes one of offset printing, gravure printing, flexographic printing, screen printing, letterpress printing, spraying and roller coating.
10. The preparation method according to claim 1, It is characterized in that The method of performing drying and curing operation on the substrate forming the pattern includes at least one of UV curing method, LED curing method, electron beam curing method, oxidative polymerization drying method, and physical drying method.