An acoustoelectric conversion structure applied to a gas medium piezoelectric ceramic ultrasonic transducer

By constructing a cavity on the backing and integrating it with the piezoelectric ceramic, the acoustic impedance mismatch is optimized, solving the problems of vibration attenuation and performance consistency of gas-mediated piezoelectric ceramic ultrasonic transducers, and achieving efficient and simplified manufacturing and performance improvement.

CN119076353BActive Publication Date: 2026-11-24SUZHOU ZING TECHNOLOGY CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202411211457.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-30
Publication Date
2026-11-24
Estimated Expiration
2044-08-30

AI Technical Summary

Technical Problem

Existing gas-mediated piezoelectric ceramic ultrasonic transducers still produce attenuated vibrations after the circuit excitation stops, affecting the accuracy of signal reception. Furthermore, the complex backing process parameters lead to poor product performance consistency.

Method used

A cavity is constructed on the backing to fit the piezoelectric ceramic, and the matching layer, piezoelectric ceramic and backing are integrated by using plastic materials and molding processes to optimize acoustic impedance mismatch and simplify the manufacturing process.

Benefits of technology

It effectively reduces the constraint of the backing on the piezoelectric ceramic, improves sensitivity and emission intensity, simplifies the production process, improves product consistency and reliability, and reduces production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119076353B_ABST
    Figure CN119076353B_ABST
Patent Text Reader

Abstract

This invention relates to the field of ultrasonic transducer technology, and particularly to an acoustic-electric conversion structure for a gas-medium piezoelectric ceramic ultrasonic transducer. The structure includes a backing, a matching layer, and a piezoelectric ceramic. The backing includes a first accommodating space and a first opening communicating with the first accommodating space. The inner wall of the first accommodating space facing the first opening is a first connecting surface. The matching layer is disposed at the first opening of the backing to close the first opening. The piezoelectric ceramic includes a emitting surface and a back surface, which are respectively disposed on opposite sides of the piezoelectric ceramic. This acoustic-electric conversion structure, by creating a cavity at the first connecting surface on the backing that connects to the back surface of the piezoelectric ceramic, effectively confines the piezoelectric ceramic. This not only ensures the emission intensity of the product but also, through the significant difference between the acoustic impedance of the air in the cavity and the acoustic impedance of the piezoelectric ceramic, creates an acoustic impedance mismatch, reflecting the acoustic energy transmitted to the cavity back to the piezoelectric ceramic, thereby improving the sensitivity of the piezoelectric ceramic.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to an ultrasonic transducer, and more particularly to an acoustic-electric conversion structure for use in a gas-medium piezoelectric ceramic ultrasonic transducer. Background Technology

[0002] With the development of ultrasonic technology, gas-medium ultrasonic applications have been widely used in many fields, such as ultrasonic ranging, object recognition, and traffic detection. Among them, gas-medium ultrasonic transducers have become key components due to their advantages such as non-contact operation, no need for coupling agents, and ease of real-time online detection. Currently, piezoelectric ceramic transducers are the most widely used gas-medium ultrasonic transducers, characterized by their simple structure, reliable performance, and adaptability to harsh environments.

[0003] Gas-mediated piezoelectric ceramic ultrasonic transducers can not only generate ultrasonic waves but also receive them, utilizing the principle of sound wave reflection for detection. In this process, the piezoelectric ceramic transducer undergoes a piezoelectric inverse effect through voltage excitation, generating vibrations and radiating sound waves into the air. When these sound waves propagate through the air and encounter obstacles, they are reflected, and the reflected waves are again captured by the transducer and amplified by the circuitry. However, after the circuit excitation stops, the piezoelectric ceramic transducer still produces damped vibrations, affecting the accuracy of signal reception. Therefore, a backing is typically added to the transducer structure to increase damping, accelerate the vibration attenuation process, reduce damping time, and improve signal reception accuracy. Existing gas-mediated piezoelectric ceramic ultrasonic transducers typically use a dispensing process to create a gel backing on the back of the piezoelectric ceramic.

[0004] However, the dispensing process suffers from numerous and complex process parameters, making it difficult to precisely control the shape and size of the backing, resulting in poor product performance consistency. To overcome this deficiency, some manufacturers have switched to processes that more easily control the shape and size of the backing, forming backings of specific shapes and sizes to improve the designability of product performance. To meet the process requirements for controlled backing molding, the backing materials used in these new processes are typically harder than those used in adhesive backings. However, while this rigid backing can more effectively shorten vibration damping time, it also increases the constraint on the vibration of the piezoelectric ceramic, causing a decrease in the product's emission intensity. Therefore, there is an urgent need to propose an acoustic-electric conversion structure for gas-mediated piezoelectric ceramic ultrasonic transducers to solve the above problems. Summary of the Invention

[0005] The purpose of this invention is to provide an acoustic-electric conversion structure for use in gas-mediated piezoelectric ceramic ultrasonic transducers. By constructing a cavity on the backing that is compatible with the piezoelectric ceramic, the vibration damping time is shortened while also reducing the impact of the backing on the product's emission intensity.

[0006] The technical solution adopted by this invention to solve the above problems is: a sound-to-electricity conversion structure, comprising: The backing includes a first receiving space and a first opening communicating with the first receiving space, the first receiving space including a first connecting surface facing the first opening.

[0007] A matching layer is provided at the first opening to close the first opening.

[0008] The piezoelectric ceramic includes an emitting surface and a back surface, which are respectively disposed on opposite sides of the piezoelectric ceramic. The piezoelectric ceramic is disposed in the first accommodating space. The back surface is connected to the first connecting surface, and the emitting surface is connected to the matching layer.

[0009] A cavity is provided at the first connecting surface on the backing. The orthographic projection of the cavity onto the first connecting surface and the orthographic projection of the back surface onto the first connecting surface have an overlapping area, and the overlapping area is greater than zero.

[0010] Preferably, the piezoelectric ceramic is in the shape of a disc, with the emitting surface and the back surface located at opposite ends of the piezoelectric ceramic.

[0011] Preferably, the piezoelectric ceramic is in the shape of a rectangular sheet, with the emitting surface and the back surface located on opposite sides of the piezoelectric ceramic.

[0012] Preferably, the geometric center of the contour shape of the cavity projected onto the first connecting surface coincides with the geometric center of the contour shape of the back surface projected onto the first connecting surface.

[0013] Preferably, the backing is made of a plastic material by a pressure molding process, so that the backing covers the outside of the matching layer and the piezoelectric ceramic during the pressure molding process, so that the matching layer and the piezoelectric ceramic are integrally formed with the backing, and the matching layer and the piezoelectric ceramic are connected with the backing.

[0014] During the molding process, the pressure applied to the backing material is at least 0.15 MPa.

[0015] Preferably, the backing is formed by injection molding, and the backing is integrally formed with the matching layer and the piezoelectric ceramic during the injection molding process.

[0016] Preferably, the acoustic-to-electric conversion structure further includes: A circuit board is disposed on the backing and is electrically connected to the piezoelectric ceramic.

[0017] The wiring harness is electrically connected to the circuit board.

[0018] The outer shell includes a second accommodating space extending to one side of the outer shell to form a second opening. The backing is disposed within the second accommodating space. The inner wall of the second accommodating space applies a bearing force to the periphery of the backing pointing towards the center of the second opening. The Young's modulus of the outer shell is greater than that of the backing. The orthographic projection line segment of the contact portion between the inner wall of the second accommodating space and the outer side of the backing in the extending direction of the second accommodating space overlaps with the orthographic projection line segment of the contact portion between the outer side of the matching layer and the inner wall of the first accommodating space in the extending direction of the second accommodating space.

[0019] Preferably, the outer shell is formed from a plastic material onto the outside of the backing through a molding process, so that the outer shell and the backing are integrally formed.

[0020] Preferably, the outer shell is formed by injection molding, and the outer shell is integrally formed with the backing during the injection molding process.

[0021] Beneficial effects of the embodiments of the present invention This acoustic-electric conversion structure effectively restrains the piezoelectric ceramic by creating a cavity at the first connection surface on the backing that connects to the back of the piezoelectric ceramic. This not only ensures the emission intensity of the product, but also creates an acoustic impedance mismatch by creating a large difference between the acoustic impedance of the air in the cavity and the acoustic impedance of the piezoelectric ceramic. This reflects the acoustic energy transmitted to the cavity back to the piezoelectric ceramic, thereby improving the sensitivity of the piezoelectric ceramic.

[0022] This acoustic-electric conversion structure, through the use of a malleable material and molding method to form the backing, integrates the matching layer and piezoelectric ceramic with the backing, significantly simplifying the manufacturing process, reducing production steps, and improving production efficiency. Furthermore, the integrated molding process effectively reduces potential manufacturing errors, ensuring a tight fit and structural stability between components, thereby enhancing product consistency and reliability. In addition, through optimized molding processes, this invention allows for performance adjustment solely through injection molding parameters. This not only solves the problems of complex backing design parameters and intricate manufacturing processes in existing gas-mediated piezoelectric ceramic ultrasonic transducers, but also achieves the goal of rapid performance adjustment by simplifying design and reducing processing steps. Attached Figure Description

[0023] Figure 1 This is a schematic cross-sectional view of an acoustic-electric conversion structure proposed in one embodiment of the present invention.

[0024] Figure 2 This is a schematic cross-sectional view of the backing proposed in one embodiment of the present invention. Figure 1 .

[0025] Figure 3 This is a schematic cross-sectional view of a gas-medium piezoelectric ceramic ultrasonic transducer proposed in one embodiment of the present invention.

[0026] Figure 4 This is a diagram of a sound wave propagation model with two media, as proposed in one embodiment of the present invention.

[0027] Figure 5 This is a diagram of a sound wave propagation model with three layers of media proposed in one embodiment of the present invention.

[0028] Figure 6 This is a schematic cross-sectional view of the backing proposed in one embodiment of the present invention. Figure 2 .

[0029] Figure 7 This is a schematic cross-sectional view of a cavity-free backing proposed in one embodiment of the present invention.

[0030] Figure 8 This is a schematic cross-sectional view of a cavity backing as proposed in one embodiment of the present invention.

[0031] Figure 9 This is a vibration displacement curve of a gas-medium piezoelectric ceramic ultrasonic transducer under different operating conditions, as proposed in one embodiment of the present invention.

[0032] Figure 10 This is a maximum amplitude curve of a gas-medium piezoelectric ceramic ultrasonic transducer under the influence of different cavity lengths, as proposed in one embodiment of the present invention.

[0033] Figure 11 This is a vibration displacement curve of a gas-medium piezoelectric ceramic ultrasonic transducer under the influence of different cavity lengths, as proposed in one embodiment of the present invention.

[0034] Figure 12 This is a vibration displacement curve of a gas-medium piezoelectric ceramic ultrasonic transducer under the influence of different cavity heights, as proposed in one embodiment of the present invention.

[0035] Figure 13 This is a maximum amplitude curve of a gas-medium piezoelectric ceramic ultrasonic transducer under the influence of different cavity heights, as proposed in one embodiment of the present invention.

[0036] Figure 14 This is an oscilloscope curve of a material with a hardness of 90A proposed in one embodiment of the present invention, which is TPE.

[0037] Figure 15 This is an oscilloscope curve of a material with a hardness of 75A proposed in one embodiment of the present invention, which is TPE.

[0038] Figure 16 This is an oscilloscope curve of a material of TPE with a hardness of 45A proposed in one embodiment of the present invention.

[0039] Figure 17 This is an oscilloscope curve of PVC material with a hardness of 75A proposed in one embodiment of the present invention.

[0040] Figure 18 This is a schematic cross-sectional view showing that, in one embodiment of the present invention, the area of ​​the overlapping region of the orthographic projection of the cavity on the first connecting surface and the orthographic projection of the back surface on the first connecting surface is larger than the area of ​​the orthographic projection on the back surface.

[0041] Wherein: 100, backing; 110, first accommodating space; 120, first opening; 130, first connecting surface; 131, cavity; 200, matching layer; 300, piezoelectric ceramic; 310, back side; 320, emitting surface; 400, circuit board; 500, wire harness; 600, housing. Detailed Implementation

[0042] The specific embodiments of the present invention will be described in further detail below with reference to the accompanying drawings and examples. The following examples are for illustrative purposes only and are not intended to limit the scope of the invention.

[0043] In the description of this application, it should be understood that the terms "center," "longitudinal," "lateral," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," and "outer," etc., indicating orientation or positional relationships based on the orientation or positional relationships shown in the accompanying drawings, are used only for the convenience of describing this application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation, and therefore should not be construed as limiting the scope of protection of this application. Furthermore, the terms "first," "second," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, features defined with "first," "second," etc., may explicitly or implicitly include one or more of that feature. In the description of this application, unless otherwise stated, "a plurality of" means two or more.

[0044] In the description of this application, it should be noted that, unless otherwise expressly specified and limited, the terms "installation," "connection," and "linking" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal connection between two components. Those skilled in the art will understand the specific meaning of the above terms in this application based on the specific circumstances.

[0045] like Figures 1 to 2As shown. The acoustic-electric conversion structure includes a backing 100, a matching layer 200, and a piezoelectric ceramic 300. The backing 100 includes a first accommodating space 110 and a first opening 120 communicating with the first accommodating space 110. The inner wall of the first accommodating space 110 facing the first opening 120 is a first connecting surface 130. The matching layer 200 is disposed at the first opening 120 of the backing 100 to close the first opening 120. The piezoelectric ceramic 300 includes an emitting surface 320 and a back surface 310, which are respectively disposed on opposite sides of the piezoelectric ceramic 300. The piezoelectric ceramic 300 is disposed in the first accommodating space 110. The back surface 310 is connected to the first connecting surface 130, and the emitting surface 320 is connected to one side of the matching layer 200. A cavity 131 is provided at the first connecting surface 130 on the backing 100, and the orthographic projection of the cavity 131 on the first connecting surface 130 is located within the range of the orthographic projection of the back surface 310 on the first connecting surface 130. This acoustic-electric conversion structure, by creating a cavity 131 at the first connecting surface 130 on the backing 100 that connects to the back surface 310 of the piezoelectric ceramic 300, can effectively reduce the constraint of the backing 100 on the piezoelectric ceramic 300. This not only ensures the emission intensity of the product but also, through the significant difference between the acoustic impedance of the air in the cavity 131 and the acoustic impedance of the piezoelectric ceramic 300, creates an acoustic impedance mismatch, reflecting the acoustic energy transmitted to the cavity 131 back to the piezoelectric ceramic 300, thereby improving the sensitivity of the piezoelectric ceramic 300.

[0046] The matching layer 200 is fixedly connected to the emitting surface 320 of the piezoelectric ceramic 300 in a fitted manner on the side facing the first accommodating space 110. The material of the matching layer 200 can be a polymer or composite material with good acoustic properties to ensure that sound waves can be effectively transmitted to the piezoelectric ceramic 300. Simultaneously, the thickness and material properties of the matching layer 200 can be adjusted according to the design requirements of the acoustic-electric conversion structure to optimize the sound wave transmission efficiency. During manufacturing, the matching layer 200 is fixed at the first opening 120, and the connection between the matching layer 200 and the first opening 120 should be sealed through manufacturing processes or by setting a sealant to ensure the structural stability and airtightness. In this embodiment, the matching layer 200 plays a role in improving the efficiency of sound energy transmission to the air.

[0047] The piezoelectric ceramic 300 is disposed on the side of the matching layer 200 facing the first accommodating space 110. Its back surface 310 is fixedly connected to the first connecting surface 130 in the first accommodating space 110 in a fitted manner. The piezoelectric ceramic 300 utilizes the piezoelectric direct / inverse effect to generate and receive sound energy, converting it into an electrical signal for judgment. The function of the piezoelectric ceramic 300 is to deform and generate sound waves under the influence of electrical signals, or to convert received sound wave signals into electrical signals. In this embodiment, to reduce the vibration and displacement generated by the piezoelectric ceramic 300 during operation, the side of the piezoelectric ceramic 300 facing away from the matching layer 200 is fixedly connected, and the piezoelectric ceramic 300 and the matching layer 200 are bonded together.

[0048] The design of cavity 131 is a key innovation of this invention. Cavity 131 is located on the first connecting surface 130, and is defined as being recessed in a direction away from the first opening 120. The orthographic projection of cavity 131 on the first connecting surface 130 and the orthographic projection of the back surface 310 on the first connecting surface 130 have an overlapping area, and the overlapping area is greater than zero. Regarding the shape of cavity 131, as... Figure 2 and Figure 6 As shown, in specific embodiments, this is manifested as concave curved grooves and cylindrical grooves. This embodiment, by constructing a cavity 131 on the first connecting surface 130, not only optimizes the sound wave reflection performance but also further reduces the impact of the backing 100 on the transducer's emission intensity by reducing direct mechanical constraints on the piezoelectric ceramic 300. Furthermore, the backing 100 can adjust the product's sensitivity and vibration damping time by controlling the size and shape of the cavity 131.

[0049] like Figure 18 As shown, the periphery of the piezoelectric ceramic 300 is fixedly connected to the inner wall of the first accommodating space 110. The periphery of the piezoelectric ceramic 300 can be connected to the inner wall of the periphery of the first accommodating space 110 by adhesive bonding, thereby ensuring that the piezoelectric ceramic 300 is fixed outside the cavity 131 and preventing the piezoelectric ceramic 300 from falling into the cavity 131.

[0050] Furthermore, such as Figure 8As shown, to further optimize the emission intensity and reflectivity of sound waves, this embodiment of the acoustic-electric conversion structure restricts the geometric relationship between the cavity 131 and the piezoelectric ceramic 300. Specifically, the area corresponding to the orthographic projection of the cavity 131 on the first connecting surface 130 is located within the range of the orthographic projection of the back surface 310 on the first connecting surface 130. That is, the area of ​​the orthographic projection of the cavity 131 on the first connecting surface 130 is smaller than the area of ​​the orthographic projection of the back surface 310 on the first connecting surface 130, thereby ensuring that the piezoelectric ceramic 300 can be mounted on the first connecting surface 130. This design ensures that the piezoelectric ceramic 300 receives sufficient support during operation, while limiting the influence range of the cavity 131. In specific embodiments, the piezoelectric ceramic 300 is shaped as a circular piece, a rectangular piece, etc. The relationship between the outline shape of the orthographic projection of the piezoelectric ceramic 300 on the first connecting surface 130 and the outline shape of the orthographic projection of the cavity 131 on the first connecting surface 130 is reflected in specific embodiments as the geometric center of the outline shape of the orthographic projection of the piezoelectric ceramic 300 coincides with or deviates from the geometric center of the outline shape of the orthographic projection of the cavity 131.

[0051] Furthermore, taking the first accommodating space 110 as a circular groove structure with a radius of L1, the cavity 131 as a concave curved groove with a circular orthographic projection on the first connecting surface 130 having a radius of L2, where L1 is greater than L2, and the piezoelectric ceramic 300 as a circular disc, with the geometric shape of the orthographic projection of the piezoelectric ceramic 300 on the first connecting surface 130 coinciding with the geometric shape of the orthographic projection of the cavity 131 on the first connecting surface 130 as an example, this geometric design ensures that the piezoelectric ceramic 300 can partially float above the cavity 131, while the other part directly contacts the first connecting surface 130. This layout not only enhances the stability of the piezoelectric ceramic 300 but also optimizes the propagation path of sound waves, achieving an optimal balance between the emission intensity and reflectivity of the sound waves. Figures 7 to 9 As shown, simulation experiments verified that the geometric relationship between the cavity 131 and the piezoelectric ceramic 300, when meeting the above requirements, can significantly improve the emission intensity and reflectivity of sound waves. Specifically, when the radius of the piezoelectric ceramic 300 is located between the radius of the cavity 131 and the radius of the first accommodating space 110, the sound waves are more evenly distributed on the piezoelectric ceramic 300, avoiding unnecessary energy loss. At the same time, the presence of the cavity 131 provides an enhanced reflective surface effect, further improving the performance of the device.

[0052] In this embodiment, by further restricting the geometric relationship between the cavity 131 and the piezoelectric ceramic 300, the piezoelectric ceramic 300 can be effectively mounted on the first connecting surface 130, thereby optimizing the sound wave emission intensity and reflectivity. This geometric design not only improves the stability of the piezoelectric ceramic 300, but also verifies through simulation experiments that the sound wave propagation effect is optimal under specific geometric conditions, ensuring the high performance and reliability of the product. Through reasonable structural design, this invention achieves optimization of the acoustic-electric conversion structure, further enhancing the product's market competitiveness.

[0053] refer to Figures 7 to 8 To verify the impact of different materials (hard rubber and soft rubber) on the performance of the gas-medium piezoelectric ceramic 300 ultrasonic transducer backing 100 and the presence or absence of a cavity 131, simulation experiments were conducted to verify the following results: Figure 9 As shown, from Figure 9 The simulation results, combined with the sound pressure formula, show that different injection molding materials for the backing 100 can adjust the transducer's emission intensity, while the presence of the cavity 131 can reduce the influence of the backing 100 on the transducer's emission intensity, and even enhance the transducer's emission intensity and sensitivity. The material parameters of different backings 100 in this simulation experiment are shown in Table 1. It should be noted that hard rubber corresponds to the injection molding backing 100 in this experiment, while soft rubber corresponds to the traditional rubber backing 100.

[0054]

[0055] Table 1 Further, refer to Figures 7 to 8 To verify the impact of the cavity 131 size in the gas-medium piezoelectric ceramic 300 ultrasonic transducer on product performance, simulation experiments were conducted to verify the results as follows: Figures 10 to 13 As shown, from Figures 10 to 13 The simulation results, combined with the sound pressure formula, show that the length of the cavity 131 has a significant effect on adjusting the emission intensity of the ultrasonic transducer. Figures 10 to 11 As shown, once cavity 131 appears, the transducer amplitude increases significantly. However, after cavity 131 appears, the change in the height H1 of cavity 131 has no significant effect on the transducer's emission intensity. Figures 12 to 13 As shown in Table 2, the parameters of different cavities 131 of the same material backing 100 in this simulation experiment are shown. It should be noted that: hard rubber corresponds to the injection-molded backing 100 in this experiment, while soft rubber corresponds to the traditional rubber backing 100.

[0056]

[0057] Table 2 It should be noted that when the size L2 of cavity 131 in Table 2 is greater than L1, the corresponding situation is that the orthographic projection of cavity 131 on the first connecting surface 130 and the orthographic projection of the back surface 310 on the first connecting surface 130 overlap. When the size of cavity 131 meets this condition, such as Figure 10 Character Figure 11 As shown, the transducer has the best vibration displacement and maximum vibration amplitude, which means that the piezoelectric ceramic 300 has the highest emission intensity.

[0058] In one embodiment, to further adjust the emission intensity and sensitivity of the product while ensuring product consistency, the backing 100 is manufactured by a molding process. During molding, the backing 100 is integrally formed with the matching layer 200 and the piezoelectric ceramic 300, thereby connecting the matching layer 200 and the piezoelectric ceramic 300 to the backing 100. This molding process for the backing 100 is specifically embodied in injection molding. Taking injection molding as an example, the backing 100 is formed by injection molding, and during the injection molding process, the backing 100 is integrally formed with the matching layer 200 and the piezoelectric ceramic 300.

[0059] Furthermore, in this embodiment, the molding process is a pressure molding process. The backing 100 is made of a plastic material by a pressure molding process, so that the backing 100 covers the outside of the matching layer 200 and the piezoelectric ceramic 300 during the pressure molding process, so that the matching layer 200 and the piezoelectric ceramic 300 are integrally formed with the backing 100, and the matching layer 200 and the piezoelectric ceramic 300 are connected with the backing 100. During the molding process, the pressure (injection pressure) applied to the backing 100 material is at least 0.15 MPa.

[0060] From the perspective of making the connection between the matching layer 200 and the piezoelectric ceramic 300 and the backing 100 more secure, the pressure molding process has advantages such as enhancing interfacial adhesion, reducing interfacial voids and defects, improving material flowability, promoting chemical bonding, and preventing delamination and separation, as detailed below: Enhanced interfacial adhesion: The pressure molding process, by applying pressure, allows the backing material 100 to more tightly encapsulate the matching layer 200 and the piezoelectric ceramic 300 during molding. Pressure facilitates the interpenetration and bonding between material molecules, significantly enhancing the interfacial adhesion between the matching layer 200 and the piezoelectric ceramic 300 and the backing material 100. This strong interfacial adhesion is crucial for ensuring the integrity and reliability of the structure.

[0061] Reducing interfacial voids and defects: During the pressurization process, the applied pressure can effectively eliminate air and micro-voids between materials, thereby reducing voids and micro-defects at the interface. This void-free connection not only increases the physical contact area between the matching layer 200 and the piezoelectric ceramic 300 and the backing 100, but also increases the interfacial strength and reduces mechanical weaknesses caused by interfacial defects.

[0062] Improving material flowability: Pressure allows the material to flow better within the mold, ensuring full filling of all mold cavities and uniform material distribution at the contact interfaces. This uniform material distribution ensures a tight fit between the mating layer 200, the piezoelectric ceramic 300, and the backing 100, preventing weak connections caused by insufficient or uneven material distribution.

[0063] Promoting Chemical Bonding: The pressure molding process typically involves temperature control alongside the application of pressure. This combination of temperature and pressure promotes chemical bonding between the backing material 100 and the mating layer 200 and piezoelectric ceramic 300, such as the formation of covalent or hydrogen bonds, thereby enhancing the interfacial adhesion strength. Enhanced chemical bonding means significantly improved tensile strength and peel resistance at the joints.

[0064] Preventing delamination and separation: The pressure molding process creates a tighter and more uniform bond, effectively preventing delamination or separation during subsequent use. Especially when subjected to mechanical stress or temperature changes in the working environment, the robust bond formed by pressure molding maintains structural integrity and extends product lifespan.

[0065] In summary, the pressure molding process achieves a high-strength, defect-free, and uniform connection between the matching layer 200, the piezoelectric ceramic 300, and the backing 100 by applying pressure, thereby significantly improving the stability and reliability of the entire acoustic-electric conversion structure. This process not only enhances the strength of the connection but also effectively prevents various failure modes that may occur at the interface.

[0066] It is important to note that applying pressure greater than the ambient air pressure during pressurization has advantages such as ensuring material flowability and moldability, improving interfacial bonding strength, eliminating air bubbles and inhomogeneities, preventing external environmental factors from affecting molding quality, and ensuring structural integrity. In short, the pressurization process requires pressure greater than the ambient air pressure to ensure that the material can flow, fill, and bond fully within the mold, thereby achieving a high-quality acoustic-electric conversion structure and ensuring product performance and reliability.

[0067] In this embodiment, the backing 100, matching layer 200, and piezoelectric ceramic 300 are connected through a one-step molding process during injection molding. The advantage of this process is that the backing 100 can be fixed to other components simultaneously during molding, reducing assembly steps and avoiding cumulative errors from multiple processing steps. By rationally controlling injection molding process parameters, such as injection pressure, temperature, and cooling rate, the connection strength between the backing 100, matching layer 200, and piezoelectric ceramic 300 can be further optimized, ensuring the stability and reliability of the entire acoustic-electric conversion structure. Furthermore, the injection molding process ensures precise molding of the cavity 131, avoiding dimensional errors and inconsistencies that may occur in traditional processes. The high efficiency of the injection molding process not only increases production speed but also ensures the consistency of each batch of products, thereby effectively reducing production costs and improving yield. Furthermore, injection molding provides technical support for the flexible adaptability of transducers in different application scenarios. In this way, it effectively overcomes the problems of limited material selection and difficulty in controlling transducer performance in existing technologies, and provides a technical solution that can flexibly adjust the performance of transducers, thereby achieving the effect of optimizing sound-to-electric conversion performance and improving product adaptability.

[0068] Furthermore, in this embodiment, the material of the backing 100 can be selected from thermoplastics, thermosetting plastics, or other polymer materials suitable for injection molding processes, which have good plasticity. By selecting different injection molding materials, the backing 100 can possess different mechanical and electrical properties, thereby imposing different degrees of constraint on the working environment of the piezoelectric ceramic 300. For example, using a material with higher hardness can increase the constraint force on the piezoelectric ceramic 300, reduce its displacement during operation, and thus improve the stability of the transducer. Conversely, selecting a softer or more elastic material can reduce the constraint force, allowing the piezoelectric ceramic 300 to vibrate more freely. Alternatively, selecting a material with lower acoustic impedance can increase the reflectivity of sound waves, thereby making the piezoelectric ceramic 300 more sensitive. In addition, the selection of the injection molding process also provides a wide range of possibilities for adjusting the performance of the transducer. By selecting different materials and controlling the molding process, the characteristics of the backing 100 can be precisely controlled. For example, the vibration characteristics of the piezoelectric ceramic 300 can be affected by adjusting the modulus, damping coefficient, and coefficient of thermal expansion of the material, thereby achieving fine adjustment of the transducer performance without changing other structural designs.

[0069] In this embodiment, the material of the backing 100 is specifically TPE and PVC. The hardness of the TPE material can be selected as 90A, 75A, or 45A, and the hardness of the PVC material is 75A. According to the experimental results shown in the figure, the horizontal axis of the oscilloscope represents time, and the vertical axis represents echo energy. The experiment shows that different materials and hardness have a significant impact on echo energy, as detailed below: TPE (90A): such as Figure 14 As shown, the echo energy is relatively large and the waveform decays quickly, making it suitable for scenarios requiring rapid response and able to reduce residual vibration in a short period of time.

[0070] TPE (75A): such as Figure 15 As shown, the echo energy is relatively balanced and has a moderate decay time, making it suitable for applications that require a balance between response speed and energy transmission.

[0071] TPE (45A): as shown Figure 16 As shown, the echo energy is the strongest, but the attenuation rate is relatively slow, making it suitable for applications requiring high-sensitivity detection and helping to enhance the sensor's sensitivity and signal reception capabilities.

[0072] In summary, TPE (90A) is a relatively hard material. The image shows a large echo energy, but the attenuation rate is the fastest. The backing 100 made of this material provides greater mechanical constraint at the contact surface with the piezoelectric ceramic 300, helping to reduce displacement and distortion of the piezoelectric ceramic 300 during vibration, making it suitable for scenarios requiring rapid response. However, due to the rapid energy attenuation, the sensitivity of the piezoelectric ceramic 300 in detecting weak signals may be reduced.

[0073] TPE (75A) is a medium-hardness material. The image shows a relatively balanced echo energy and a moderate decay rate, achieving a good balance between hardness and sensitivity. It maintains moderate energy decay while ensuring structural stability, making it suitable for applications requiring a balance between response speed and sensitivity. However, in certain applications, the transducer's sensitivity or response speed may not perform as well as a backing material made of extremely hard or soft materials (e.g., 100).

[0074] TPE (45A) is a relatively soft material. The image shows the strongest echo energy but the slowest attenuation rate. The backing 100 made of this material provides less mechanical constraint on the piezoelectric ceramic 300, allowing for greater vibrational freedom and thus improving the transducer's sensitivity, making it suitable for detecting weak signals. However, the slow energy attenuation may result in longer residual vibrations, affecting the clarity of the transducer signal and the detection speed.

[0075] TPE materials with higher hardness (90A) provide stronger mechanical constraint on piezoelectric ceramics, making them suitable for applications requiring rapid response, but may slightly reduce sensitivity. TPE materials with medium hardness (75A) offer a balance between sensitivity and response speed, suitable for applications where both factors need to be considered. TPE materials with lower hardness (45A) provide the least constraint on piezoelectric ceramics, allowing for greater vibrational freedom and improving sensitivity, but resulting in longer residual vibration times, which may affect response speed.

[0076] PVC (75A): such as Figure 17 As shown, similar to TPE (75A), it exhibits moderate echo energy and moderate decay time, but due to different material properties, its application adaptability varies, making it suitable for occasions where an optimal balance between cost and performance is required.

[0077] The PVC (75A) backing, after 100, shows that because PVC (polyvinyl chloride) is a plastic material with good hardness and stability, it typically exhibits high damping and low elasticity. The image shows that the echo energy is slightly lower than that of TPE (75A), and the decay rate is relatively slow. The high damping of PVC helps reduce the vibration energy transmission of the piezoelectric ceramic, thereby reducing the residual vibration time to some extent, which is beneficial to the stability and accuracy of the signal. It is suitable for scenarios with high requirements for signal stability. PVC has high rigidity and low elasticity, which may reduce the vibration degrees of freedom of the piezoelectric ceramic, thus slightly reducing the sensitivity and signal transmission efficiency.

[0078] In summary, the elasticity of the TPE (45A) backing material 100 provides better buffering during the vibration transmission of piezoelectric ceramics, helping to achieve a better balance between sensitivity and stability, making it suitable for applications requiring moderate sensitivity and fast response. PVC (75A), due to its higher damping and lower elasticity, is suitable for applications requiring high signal stability and low residual vibration, but its higher rigidity may slightly limit the vibrational freedom of the piezoelectric ceramics, thus slightly reducing sensitivity. The PVC (75A) backing material 100 is more suitable for applications with higher signal stability requirements, such as ultrasonic equipment requiring long-term continuous monitoring or operating in high-noise environments, ensuring signal reliability and consistency.

[0079] In the above embodiments, the acoustic-electric conversion structure effectively solves the problems of numerous design parameters, cumbersome production processes, and poor product consistency in the prior art by using a plastic material to manufacture the backing 100 and molding the matching layer 200 and piezoelectric ceramic 300 integrally with the backing 100 through molding technology. Specifically, the backing 100 is integrally connected with the matching layer 200 and piezoelectric ceramic 300 through molding technology, which not only simplifies the production process and reduces production steps, but also ensures high consistency of transducer performance in the same batch of products. Furthermore, the transducer performance can be quickly obtained by adjusting only a few design parameters of the backing 100, achieving the effect of reducing production costs and improving product quality. The above embodiments all conform to the principles of virtual work and strain energy, as detailed below: The principle of virtual work: The work done by external forces is equal to the work done by internal stresses.

[0080] For linearly elastic materials, the strain energy can be calculated using Hooke's law, where... , where E is the Young's modulus of the material and ε is the deformation of the structure.

[0081] Under the same deformation, the lower the Young's modulus of the backing material 100, that is, the "softer" the material, the less energy the piezoelectric ceramic 3002 will consume. Assuming that the matching layer 200 and other conditions are the same, the matching layer 200 can be applied with more energy, that is, generate a greater sound pressure.

[0082] Sound pressure calculation formula:

[0083] Displacement: ; speed: ; Acceleration: ; in: This refers to air density. It represents vibration acceleration. The area of ​​vibration. The test radius.

[0084] To improve the transducer's sensitivity, specifically by increasing the acoustic wave reflectivity reflected onto the piezoelectric ceramic 300, this application proposes an embodiment. This acoustic-electric conversion structure includes a backing 100 and the piezoelectric ceramic 300, both playing crucial roles in acoustic wave transmission. To optimize acoustic wave reflection, the acoustic impedance of the backing 100 is specifically designed to be lower than that of the piezoelectric ceramic 300, thereby enhancing the acoustic wave reflectivity. The choice of material for the backing 100 is critical. To ensure that the acoustic impedance of the backing 100 is lower than that of the piezoelectric ceramic 300, this embodiment uses a material with low acoustic impedance, such as a polymer material. This material has high acoustic wave reflection performance, providing better acoustic wave reflection when the piezoelectric ceramic 300 transmits or receives acoustic waves. Specifically, when acoustic waves propagate between the piezoelectric ceramic 300 and the backing 100, a strong acoustic wave reflection occurs at the interface due to the difference in their acoustic impedances. This design significantly enhances the sensitivity of the piezoelectric ceramic 300, making it perform better when detecting weak signals. By optimizing the acoustic impedance of the backing 100, not only can the reflectivity of sound waves be improved, but unnecessary sound wave loss can also be reduced, thereby improving the working efficiency of the piezoelectric ceramic 300. In practical applications, the material and structural design of the backing 100 can be adjusted according to specific needs. For example, materials with different acoustic impedance characteristics can be selected for different application scenarios to achieve the best sound wave reflection effect. In addition, the design of this embodiment can also ensure that the piezoelectric ceramic 300 maintains a high-sensitivity working state without excessive external interference. The acoustic impedance design of the backing 100 allows more sound waves to be reflected back to the piezoelectric ceramic 300, thereby improving its signal detection capability. This is especially important for acoustic-to-electric conversion devices that require high precision and high sensitivity.

[0085] This embodiment selects specific materials to make the acoustic impedance of the backing 100 lower than that of the piezoelectric ceramic 300, thereby significantly enhancing the reflectivity of sound waves. This design effectively improves the sensitivity of the piezoelectric ceramic 300, making it more sensitive and accurate in the sound-to-electric conversion process. This optimized design of materials and structure not only solves the problem of excessive sound wave loss in the prior art, but also improves the overall efficiency and performance of the device, achieving the effect of enhancing signal detection capabilities.

[0086] In one embodiment, such as... Figure 3As shown, the acoustic-to-electric conversion structure includes not only a backing 100, a piezoelectric ceramic 300, a first connecting surface 130, and a back surface 310, but also a circuit board 400, a wiring harness 500, and a housing 600. The integration of these components makes the entire transducer structure more complete and its functions more comprehensive. The circuit board 400 is cleverly positioned on the backing 100 and electrically connected to the piezoelectric ceramic 300. The design and layout of the circuit board 400 fully considers the signal processing requirements of the piezoelectric ceramic 300. Through reasonable circuit design, the circuit board 400 can effectively receive and process the electrical signals converted by the piezoelectric ceramic 300 and transmit the electrical signals to the piezoelectric ceramic 300 to apply voltage excitation. The mounting position of the circuit board 400 close to the piezoelectric ceramic 300 reduces signal loss during transmission while ensuring the transducer's signal quality and response speed. The wiring harness 500 is electrically connected to the circuit board 400, forming a signal transmission channel from the piezoelectric ceramic 300 to external devices. The design of the wiring harness 500 ensures the stability and reliability of signal transmission, maintaining good signal transmission performance in various application scenarios. Furthermore, the wiring harness 500 can be customized in length and wiring method according to specific application requirements to adapt to the connection needs of different devices, improving the transducer's application flexibility. The housing 600 is integrally formed on the outside of the backing 100 through injection molding, providing additional physical protection and structural support. The housing 600 not only protects the internal components from the external environment but also enhances the mechanical strength and durability of the entire transducer through its structural design. The injection molding process ensures a tight fit between the housing 600 and the backing 100, forming an efficient and integrated overall structure. In addition, the housing 600 can be made of suitable materials according to the specific usage environment, thereby enhancing its protective performance, such as waterproofing, dustproofing, or impact resistance.

[0087] In this embodiment, the overall design of the acoustic-to-electric conversion structure is further improved by introducing a circuit board 400, a wiring harness 500, and a housing 600. This results in a transducer that not only possesses excellent signal processing and transmission capabilities but also superior structural protection and application adaptability. The rational arrangement of the circuit board 400 and its tight connection with the piezoelectric ceramic 300 ensure efficient signal transmission and processing. The flexible design of the wiring harness 500 enhances the ease of connection and adaptability of the device. The injection molding of the housing 600 makes the entire transducer structure more robust and durable, significantly improving product reliability and lifespan. Through this series of designs, the present invention achieves comprehensive optimization of the transducer structure, meeting the needs of various application scenarios and enhancing the product's market competitiveness.

[0088] Furthermore, the outer casing 600 includes a second receiving space extending to one side of the outer casing 600 to form a second opening. A backing 100 is disposed within the second receiving space. The inner wall of the second receiving space applies a supporting force towards the center of the second opening to the periphery of the backing 100. The Young's modulus of the outer casing 600 is greater than that of the backing 100, meaning the outer casing 600 has stronger resistance to deformation than the backing 100. The contact portion between the inner wall of the second receiving space and the outer side of the backing 100 is in the extending direction of the second receiving space. The orthographic projection line segment on the upper surface and the contact portion of the outer side of the matching layer 200 with the inner wall of the first accommodating space 110 overlap in the orthographic projection line segment in the extension direction of the second accommodating space, so that the inner wall at the second opening of the outer shell 600 will abut against the corresponding position of the backing 100, thereby causing the inner wall of the first accommodating space 110 at the first opening 120 to abut against the periphery of the matching layer 200, thereby fixing the matching layer 200 at the first opening 120 to prevent the matching layer 200 from detaching from the backing 100.

[0089] The operating principle of an air-medium piezoelectric ceramic 300 ultrasonic transducer using a novel acoustic-electric conversion structure in the above embodiments is as follows: First, the circuit board 400 provides voltage excitation to the piezoelectric ceramic 300, causing it to vibrate due to the inverse piezoelectric effect. Since the matching layer 200, backing 100, and piezoelectric ceramic 300 have a connection area, the piezoelectric ceramic 300 drives the movement of both. The outer shell 600 provides a stabilizing constraint on the system, causing the matching layer 200 and backing 100 to deform. Acoustic energy is transmitted vertically from the piezoelectric ceramic 300 through the matching layer 200 and backing 100. The matching layer 200 improves the efficiency of acoustic energy transmission to the air, thus increasing product sensitivity. The cavity 131 utilizes the acoustic impedance mismatch between the air and the piezoelectric ceramic 300 to reflect acoustic energy back to the piezoelectric ceramic 300, further improving product sensitivity. Simultaneously, the cavity 131 reduces the contact area between the backing 100 and the piezoelectric ceramic 300, thus reducing the energy loss due to deformation of the backing 100. This allows more energy generated by the piezoelectric ceramic 300 to act on the matching layer 200, resulting in greater displacement and thus greater sound pressure. After voltage excitation ends, the piezoelectric ceramic 300 and the matching layer 200 undergo damped vibration, entering the damping phase. The backing 100 provides damping through its own characteristics, accelerating damping and reducing the damping time. When the sound wave is reflected back to the matching layer 200, the piezoelectric ceramic 300 exhibits a positive piezoelectric effect, generating an electrical signal. This signal is amplified and transmitted through the circuit board 400 and wiring harness 500, enabling obstacle differentiation and judgment.

[0090] The above embodiments utilize a novel gas-medium piezoelectric ceramic 300 ultrasonic transducer with a novel acoustic-to-electric conversion structure. The three-layer dielectric model of the transmission and reflection coefficients of the emitted sound waves is as follows: Figure 4 As shown, the two-layer dielectric model with transmission coefficient and reflection coefficient of the piezoelectric ceramic 300 emitting sound waves into the cavity 131 and receiving reflected sound waves is as follows: Figure 5 As shown in the diagram. Here, A represents the medium as piezoelectric ceramic 300, B represents the medium as the matching layer 200, C represents the medium as the air outside the transducer, and D represents the medium as the air inside the cavity 131. i1 represents the emitted wave from the piezoelectric ceramic 300 to the outside of the transducer, t1 represents the transmitted wave after the emitted wave i1 from the piezoelectric ceramic 300 to the outside of the transducer passes through the matching layer 200, r1 represents the reflected wave of the emitted wave i1 from the piezoelectric ceramic 300 to the outside of the transducer reflected back to the piezoelectric ceramic 300 when it reaches the matching layer 200, i2 represents the emitted wave from the piezoelectric ceramic 300 to the cavity 131, t2 represents the transmitted wave after the emitted wave i2 from the piezoelectric ceramic 300 to the cavity passes through the air layer in the cavity 131, and r2 represents the reflected wave of the emitted wave i2 from the piezoelectric ceramic 300 to the cavity 131 reflected back to the piezoelectric ceramic 300 after passing through the air layer inside the cavity 131.

[0091] The formula for calculating the transmission coefficient of the sound waves emitted by the gas-medium piezoelectric ceramic 300 ultrasonic transducer, which utilizes a novel acoustic-electric conversion structure, is as follows:

[0092] in:

[0093] Meaning of other parameters: Let be the density of medium 1, medium 2, and medium 3. Let be the speed of sound in medium 1, medium 2, and medium 3. For wave number, ,in The frequency of the sound wave.

[0094] The thickness of medium 2.

[0095] During the vibration damping period, after the piezoelectric ceramic 300 receives the reflected sound wave, the sound wave propagates in the piezoelectric ceramic 300 and the cavity 131, resulting in the following calculation formulas for the transmission coefficient and reflection coefficient models:

[0096] Transmittance of sound waves :

[0097] in:

[0098] Meaning of other parameters: Let be the density of medium 1 and medium 3.

[0099] Let be the speed of sound in medium 1 and medium 3.

[0100] When the piezoelectric ceramic 300 is PZT-5H, the specific parameters of the piezoelectric ceramic 300, air, and matching layer 200 are shown in Table 3 below. Furthermore, when the matching layer 200 conforms to the quarter-wavelength theory, the transmittance of the two-layer and three-layer media are shown in Table 4 below. According to the table, the transmittance of acoustic energy to the air outside the transducer is much greater than the transmittance of acoustic energy to the air in cavity 131. This is because the intensity of the sound wave emitted by the piezoelectric ceramic 300 in a single emission is constant. The lower the transmittance of acoustic energy to the air in cavity 131, the higher the transmittance of acoustic energy to the air outside the transducer. Therefore, Table 4 shows that when the backing 100 has a cavity 131, the emission intensity of the transducer is effectively enhanced.

[0101]

[0102] Table 3

[0103] Table 4 The above description is merely illustrative of the invention. Those skilled in the art can make various modifications or additions to the described specific embodiments or use similar methods to replace them, as long as they do not depart from the content of this specification or exceed the scope defined by the claims, all of which should fall within the protection scope of this invention.

Claims

1. An acoustic-electric conversion structure for use in a gas-mediated piezoelectric ceramic ultrasonic transducer, characterized in that, include: The backing includes a first receiving space and a first opening communicating with the first receiving space, the first receiving space including a first connecting surface facing the first opening; A matching layer is disposed at the first opening to close the first opening; A piezoelectric ceramic includes an emitting surface and a back surface, the emitting surface and the back surface being respectively disposed on opposite sides of the piezoelectric ceramic, the piezoelectric ceramic being disposed in a first accommodating space, the back surface being connected to a first connecting surface, and the emitting surface being connected to a matching layer; A cavity is provided at the first connecting surface on the backing. The orthographic projection of the cavity onto the first connecting surface and the orthographic projection of the back surface onto the first connecting surface have an overlapping area, and the overlapping area is greater than zero. A circuit board is disposed on the backing, and the circuit board is electrically connected to the piezoelectric ceramic. The wiring harness is electrically connected to the circuit board; The housing includes a second receiving space that extends to one side of the housing to form a second opening, and the backing is disposed within the second receiving space; The backing is made of a plastic material through a pressure molding process, so that the backing covers the outside of the matching layer and the piezoelectric ceramic during the pressure molding process, so that the matching layer and the piezoelectric ceramic are integrally formed with the backing, and the matching layer and the piezoelectric ceramic are connected with the backing.

2. The acoustic-electric conversion structure for a gas-mediated piezoelectric ceramic ultrasonic transducer according to claim 1, characterized in that, The piezoelectric ceramic is in the shape of a circular sheet, with the emitting surface and the back surface located at opposite ends of the piezoelectric ceramic.

3. The acoustic-electric conversion structure for a gas-mediated piezoelectric ceramic ultrasonic transducer according to claim 1, characterized in that, The piezoelectric ceramic is in the shape of a rectangular sheet, with the emitting surface and the back surface located on opposite sides of the piezoelectric ceramic.

4. The acoustic-electric conversion structure for a gas-mediated piezoelectric ceramic ultrasonic transducer according to claim 1, characterized in that, The geometric center of the outline shape of the cavity projected onto the first connecting surface coincides with the geometric center of the outline shape of the back surface projected onto the first connecting surface.

5. A sound-to-electric conversion structure for a gas-medium piezoelectric ceramic ultrasonic transducer according to any one of claims 1 to 4, characterized in that, During the molding process, the pressure applied to the backing material is at least 0.15 MPa.

6. The acoustic-electric conversion structure for a gas-mediated piezoelectric ceramic ultrasonic transducer according to claim 5, characterized in that, The backing is formed by injection molding, and the backing is integrally formed with the matching layer and the piezoelectric ceramic during the injection molding process.

7. The acoustic-electric conversion structure for a gas-mediated piezoelectric ceramic ultrasonic transducer according to claim 6, characterized in that, The inner wall of the second accommodating space is used to apply a supporting force to the periphery of the backing pointing towards the center of the second opening. The Young's modulus of the outer shell is greater than that of the backing. The orthographic projection line segment of the contact portion between the inner wall of the second accommodating space and the outer side of the backing in the extension direction of the second accommodating space overlaps with the orthographic projection line segment of the contact portion between the outer side of the matching layer and the inner wall of the first accommodating space in the extension direction of the second accommodating space.

8. The acoustic-electric conversion structure for a gas-mediated piezoelectric ceramic ultrasonic transducer according to claim 7, characterized in that, The outer shell is formed on the outside of the backing material by a molding process, so that the outer shell and the backing are integrally formed.

9. The acoustic-electric conversion structure for a gas-medium piezoelectric ceramic ultrasonic transducer according to claim 8, characterized in that, The outer shell is formed by injection molding, and the outer shell and the backing are formed as one piece during the injection molding process.

Citation Information

Patent Citations

  • PMUT structure with support layer and manufacturing method thereof

    CN117548318A

  • Anti-attenuation ultrasonic transducer and ultrasonic probe

    CN218279674U