双色塑料容器生产方法、挤出吹塑设备及双色塑料容器

By adjusting the temperature, pressure, and extrusion rate of the secondary flow channel in real time during the production of two-color plastic containers, the problem of unstable color area size under the influence of external factors was solved, achieving high-precision and stable production results.

CN119078154BActive Publication Date: 2026-07-17FOSHAN LIANGLAI PLASTIC PACKAGING CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
FOSHAN LIANGLAI PLASTIC PACKAGING CO LTD
Filing Date
2024-09-25
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

In existing technologies, the color area size of two-color plastic containers is easily affected by changes in equipment operating time, plastic melt quality, and ambient temperature, making it difficult for molding equipment to maintain high precision. Increasing the frequency of inspection can only reduce the number of defective products, but cannot completely solve the problem.

Method used

By setting a secondary flow channel in the extrusion blow molding equipment, the temperature, pressure and extrusion volume can be adjusted in real time. The secondary flow channel's second temperature, second pressure and second extrusion volume can be automatically adjusted according to the actual size deviating from the preset range, ensuring that the actual size gradually returns to the preset range and avoiding the generation of defective products.

Benefits of technology

It enables automatic adjustment of production parameters under the influence of external factors, ensuring that the actual size of the two-color plastic containers remains within the preset range, reducing the generation of defective products, and improving production stability and accuracy.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119078154B_ABST
    Figure CN119078154B_ABST
Patent Text Reader

Abstract

本发明公开了一种双色塑料容器生产方法、挤出吹塑设备及双色塑料容器,属于塑料容器生产技术领域,获取双色塑料容器的拼色体的实际尺寸,在实际尺寸处于预设范围时,预设范围小于拼色体尺寸的合格公差范围,获取副流道的第一温度、第一压力和第一挤出量,由多个第一温度得出温度范围、由多个第一压力得出压力范围、由多个第一挤出量得出挤出量范围;在实际尺寸受设备运行时间、塑料熔体的来料质量、环境温度变化等外界因素影响而偏离预设范围后,自动调整副流道的第二温度、第二压力和第二挤出量,进而让后续产品的实际尺寸能够逐渐调整到预设范围内,以避免产生不良品。