Pulp molded packaging articles, and their inside convex forming process and production process
By applying radial inward expansion force to the molded wet pulp product using an inner expansion mold during the hot pressing and shaping stage, the product is compressed, thinned, and shaped into an inner convex structure. This solves the problem of inner diameter expansion during demolding of the inner convex buckle, improves the tightness of the fastening and production efficiency, and avoids the loss of side strength.
Patent Information
- Application Number
- CN202411220900.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-02
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2044-09-02
AI Technical Summary
In existing pulp molded cup lids, the inner diameter of the inner convex buckle tends to expand during hot pressing and demolding when the wet preform is formed, affecting the tightness of the fastening and reducing production efficiency. Furthermore, the existing molding method may damage the strength of the side wing structure and prolong the production cycle.
By using an inner expanding mold in the hot pressing and shaping stage to apply radial inward expansion force to the original side wing wall thickness, it is compressed and thinned to form an inner convex structure. The cooperation between the inner expanding mold and the hot pressing and shaping die ensures that the inner convex structure does not expand during demolding and simplifies the production steps.
It improves the fastening tightness of pulp molded packaging products, simplifies the production process, avoids the risk of inner diameter expansion, improves production efficiency, and maintains the structural strength of the side wing walls.
Smart Images

Figure CN119102145B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the technical field of pulp molded products, and particularly relates to a pulp molded packaging product, its internal convex forming process and production process. Background Technology
[0002] Pulp molded packaging products, such as pulp molded cup lids, often feature an inner convex buckle on the inner wall of the side wing during wet molding. This buckle engages with the opening of the cup body to prevent the lid from detaching. However, this method is not conducive to demolding during subsequent hot pressing. Demolding causes the inner diameter of the buckle to increase, significantly reducing the tightness of the fit with the cup body and lowering production efficiency.
[0003] Of course, some inventors have designed molding methods that involve rolling, spinning, or mechanically pressing the outer wall of the side wing inward after the pulp molded cup lid has been hot-pressed and shaped. For example, CN200910041616.2 describes the manufacturing process of disposable cup lids and the cup lids produced by this process. The specific steps of this process are: raw material pulping - batching - molding - hot pressing - edge trimming and punching - pressing the undercut hook groove. Although the final product has a structure with an inwardly protruding hook on the inner wall of the side wing, the above solutions will damage the structural strength of the side wing, affecting the final tightness of the fit with the cup body. In addition, the added pressing of the undercut hook groove will delay the production cycle and affect production efficiency. Summary of the Invention
[0004] The purpose of this invention is to address the above-mentioned problems by providing a pulp molded packaging product, its internal convex molding process, and its production process.
[0005] To achieve the above objectives, the present invention adopts the following technical solutions:
[0006] Pulp molded packaging products have a set side wing wall thickness.
[0007] The internal convex molding process for this pulp molded packaging product includes the following steps:
[0008] At least it forces the outer diameter of the original sidewall wall thickness of the pulp molded wet preform to remain unchanged;
[0009] The pulp molded wet preform is fitted into a shaping inner bulging mold, and the shaping inner bulging mold applies a radial inward bulging force from the inside to the outside to the original side wing wall thickness. This radial inward bulging force causes the original side wing wall thickness to compress and thin to the set side wing wall thickness; and
[0010] When the radial inward expansion force forces the original side wing wall thickness to compress and thin, at least a portion of the inner wall of the original side wing wall thickness and the shaping inner expansion mold are shaped to form an inward convexity that is set in the opposite direction to the radial inward expansion force.
[0011] In the above-mentioned internal convex forming process of pulp molded packaging products, the shaping internal expansion mold has an internal convex forming groove, and the internal convex forming is performed in the internal convex forming groove.
[0012] In the above-mentioned internal convex molding process of pulp molded packaging products, when the inner bulging mold shrinks radially, it forces the internal convex molding groove to detach from the internal convexity.
[0013] In the above-mentioned internal convex forming process of pulp molded packaging products, the shaping internal expansion mold is a hot-pressing shaping internal expansion punch.
[0014] This application also provides a manufacturing process for molded pulp packaging articles, including the following steps:
[0015] S1. Wet preform forming: Wet preform products with original sidewall thickness are obtained by pulp molding.
[0016] S2, hot pressing shaping, at least forcing the outer diameter of the original side wing wall thickness in S1 to remain unchanged; and
[0017] The pulp molded wet preform is fitted into a shaping inner bulging mold, and the shaping inner bulging mold applies a radial inward bulging force from the inside to the outside to the original side wing wall thickness. This radial inward bulging force causes the original side wing wall thickness to compress and thin to a set side wing wall thickness; and
[0018] When the radial inward expansion force forces the original side wing wall thickness to compress and thin, at least a portion of the inner wall of the original side wing wall thickness and the shaping inner expansion mold are shaped to form an inward protrusion that is set in the opposite direction to the radial inward expansion force;
[0019] S3, demolding, the inner forming mold in S2 shrinks radially, thereby causing the inner forming mold to detach from the inner convex.
[0020] In the above-mentioned production process of pulp molded packaging products, in S2, a hot pressing forming die is provided that is similar to the outer contour of the pulp molded wet preform product. The forming inner expansion die is a hot pressing forming inner expansion punch that is similar to the inner contour of the pulp molded wet preform product. Either the hot pressing forming die or the forming inner expansion die moves relative to the other and forces the forming inner expansion die to apply a radial inward expansion force from the inside to the outside to the original side wing wall thickness.
[0021] In the above-mentioned production process of pulp molded packaging products, during the process of forming the inner convex shape, the shaping inner expansion mold and the hot pressing shaping concave mold respectively heat and dry the pulp molded wet preform product.
[0022] In the above-mentioned production process of pulp molded packaging products, the shaping inner expansion mold has an inner convex forming groove, and the inner convex forming is in the inner convex forming groove.
[0023] In the above-mentioned production process of pulp molded packaging products, in S1 above, the pulp molded wet preform product is a pulp molded wet preform cup lid with equal wall thickness.
[0024] This application also provides a pulp molded packaging article, which is obtained by the production process of pulp molded packaging articles.
[0025] Compared with existing technologies, the advantages of this application are:
[0026] The internal convex structure is shaped during the hot pressing and shaping stage, which can prevent the risk of the internal diameter of the convex structure from further expanding during demolding in subsequent processing, thus giving the pulp molded packaging products better fastening tightness.
[0027] The process of shaping the inner convex structure during the hot pressing stage can simplify the production process. For example, it can omit the separate pressing of the undercut hook after hot pressing and avoid the risk that the inner diameter of the inner convex structure will be further enlarged during demolding due to the hot pressing process when the wet blank is directly formed into an inner convex structure. This can improve production efficiency and ensure stable product quality.
[0028] The internal convex structure is formed during the hot pressing and shaping stage, which can prevent the side wing wall thickness from deteriorating due to processes such as spinning, rolling, or pressing undercut hooks. Attached Figure Description
[0029] Figure 1 This is a schematic diagram showing the changes in pulp molded packaging products obtained after hot pressing and shaping of the pulp molded wet preform provided by the present invention.
[0030] Figure 2 This is a flowchart of the internal convex forming process provided by the present invention;
[0031] Figure 3 This is a schematic diagram of the hot-pressing shaping mold structure provided by the present invention;
[0032] Figure 4 yes Figure 3 Enlarged structural diagram at point A in the diagram;
[0033] Figure 5 This is a production process flow chart of pulp molded packaging products provided by the present invention;
[0034] Figure 6 This is a schematic diagram of the hot-pressing shaping mold opening state provided by the present invention;
[0035] Figure 7 This is a schematic diagram showing the state of the pulp molded wet preform provided by the present invention being fitted onto the shaping inner expansion mold;
[0036] Figure 8This is a schematic diagram of the mold closing state of the hot pressing shaping mold provided by the present invention;
[0037] Figure 9 This is a schematic diagram of the hot-pressing shaping mold in the re-opening state provided by the present invention;
[0038] Figure 10 This is a schematic diagram of the hot-pressing shaping mold in its fully opened state provided by the present invention.
[0039] In the figure, the molded pulp wet preform Z0, the original side wing wall thickness Z01, the top Z02, the transverse part Z03, the molded pulp packaging product Z1, the side wing wall thickness Z10, the inner convex Z11, the shaping inner expansion mold 1, the inner convex forming groove 1a, the guide displacement outer mold 10, the first blind hole 100, the receiving groove 101, the third blind hole 102, the inner expansion mold 11, the transverse spring 12, the fourth blind hole 120, the top mold 13, the demolding air passage 130, the extension part 131, the second through hole 132, the transverse air passage 133, the hot pressing shaping die 2, the mold base 3, the guide groove 30, the second blind hole 300, the elastic component 31, the truncated cone 32, the through hole 320, the first through hole 33, and the cylindrical part 330. Detailed Implementation
[0040] The following are specific embodiments of the invention, which are described in conjunction with the accompanying drawings. The technical solution of the invention will be further described, but the invention is not limited to these embodiments.
[0041] like Figure 1 As shown, the pulp molded packaging product Z1 has a set side wing wall thickness Z10, and an inner protrusion Z11 on the inner wall of the set side wing wall thickness Z10. The inner protrusion Z11 can be a complete ring structure or several arc-shaped structures distributed in a circle.
[0042] The following is a further introduction to pulp molded packaging products Z1, using a pulp molded cup lid as an example:
[0043] Example 1
[0044] like Figure 1 As shown, the internal convex molding process of this pulp molded packaging product is mainly used to manufacture the internal convex Z11, and is in the hot pressing and shaping stage.
[0045] Unlike existing technologies, the inner convex Z11 in this embodiment is obtained by hot pressing, and the finished product is obtained directly after hot pressing, which can completely solve the above-mentioned technical problems of the prior art.
[0046] Specifically, such as Figures 1-3 As shown, the internal convex forming process in this embodiment includes the following steps:
[0047] At least the outer diameter of the original side wing wall thickness Z01 of the pulp molded wet preform Z0 is forced to remain unchanged; in the wet preform state, the thickness of the original side wing wall thickness Z01 is greater than the set side wing wall thickness Z10.
[0048] The outer diameter restriction remains unchanged, and a hot pressing forming die 2 is used. The hot pressing forming die 2 can restrict the outer contour surface of the pulp molded wet preform Z0, so that the original side wing wall thickness Z01 can be subjected to the following forming, compression and thinning process.
[0049] Secondly, the pulp molded wet preform Z0 is fitted into the shaping inner expansion mold 1, which is a hot-pressing shaping inner expansion punch. At this time, the shaping inner expansion mold 1 is in a radially contracted state so that the pulp molded wet preform Z0 can be fitted in. The outer wall of the shaping inner expansion mold 1 has at least a matching contact surface that matches the original side wing wall thickness Z01, and the shaping inner expansion mold 1 applies a radial inward expansion force from the inside to the outside to the original side wing wall thickness Z01. The application of the radial inward expansion force can make the original side wing wall thickness Z01 thinner. At the same time, it can also make the axis of the pulp molded wet preform Z0 passively coincide with the axis of the shaping inner expansion mold 1, so that the original side wing wall thickness Z01 has a uniform thickness. The radial inward expansion force compresses and thins the original side wing wall thickness Z01 to the set side wing wall thickness Z10.
[0050] The radial expansion force is applied in a plane perpendicular to the Z0 axis of the molded pulp preform. When the radial expansion force compresses and thins the original side wing wall thickness Z01, at least a portion of the inner wall of the original side wing wall thickness Z01 and the shaping inner expansion mold 1 are shaped to form an inward protrusion Z11 in the opposite direction to the radial expansion force. This can be explained as follows: an inward protrusion forming chamber is reserved between the inner wall of the original side wing wall thickness Z01 and the shaping inner expansion mold 1. Because the wall thickness is thinned during shaping, part of the material of the original side wing wall thickness Z01 is squeezed into the inward protrusion forming chamber, thus forming the inward protrusion Z11.
[0051] Specifically: such as Figure 4 As shown, the shaping inner bulging mold 1 has an inner convex forming groove 1a, and the inner convex Z11 is formed in the inner convex forming groove 1a. The single-sided cross-section of the inner convex forming groove 1a is C-shaped, U-shaped, or V-shaped, and can also be semi-circular. The inner convex forming groove 1a consists of at least two arc-shaped grooves centered on the axis of the shaping inner bulging mold 1 and distributed in a circular pattern.
[0052] Secondly, when the inner forming mold 1 contracts radially, it forces the inner convex forming groove 1a to disengage from the inner convex Z11. This structure facilitates demolding and prevents the inner diameter of the inner convex Z11 from expanding during demolding.
[0053] like Figure 3As shown, the shaping inner bulging mold 1 and the hot pressing shaping die 2 cooperate with each other to form a hot pressing shaping cavity for accommodating the wet pulp molded preform Z0. During this compression and thinning process, the shaping inner bulging mold 1 expands radially, giving it a radial inward expansion force. The outward expansion of the radial inward expansion force causes the original side wing wall thickness Z01 to be compressed and thinned.
[0054] An inclined internal expansion guide mechanism is provided between the shaping internal expansion mold 1 and the hot pressing shaping die 2, which causes the shaping internal expansion mold 1 to expand radially outward. The shaping internal expansion mold 1 also moves vertically relative to the mold base 3, and the side of the shaping internal expansion mold 1 away from the hot pressing shaping die 2 is connected to the hot pressing shaping die 2 by an elastic component 31.
[0055] The shaping inner bulging mold 1 moves vertically relative to the mold base 3. The side of the shaping inner bulging mold 1 away from the hot-pressing shaping die 2 is connected to the hot-pressing shaping die 2 via an elastic component 31. Specifically, at least a portion of the shaping inner bulging mold 1 is accommodated in the guide groove 30 of the mold base 3, that is, the shaping inner bulging mold 1 and the guide groove 30 are linearly slidingly engaged to realize the displacement of the shaping inner bulging mold 1. The side of the shaping inner bulging mold 1 away from the hot-pressing shaping die 2 is connected to the bottom of the guide groove 30 via the elastic component 31. The elastic extension and contraction direction of the elastic component 31 is the displacement direction of the shaping inner bulging mold 1.
[0056] The function of the hot pressing forming die 2 is as follows:
[0057] The elastic component 31 forces the shaping inner bulging mold 1 away from the bottom of the guide groove 30. That is, at this time, there is a gap between the bottom surface of the shaping inner bulging mold 1 and the bottom of the guide groove 30. Under the drive of the power, the hot pressing shaping die 2 causes the hot pressing shaping die 2 and the shaping inner bulging mold 1 to close. At this time, the pulp molded wet preform Z0 is housed in the hot pressing shaping cavity. As the hot pressing shaping die 2 continues to descend, the elastic component 31 is continuously compressed elastically. In this process, the shaping inner bulging mold 1 and the hot pressing shaping die 2 can heat and dry the pulp molded wet preform Z0 and compress and thin the wall thickness of the pulp molded wet preform Z0, which is hot pressing shaping.
[0058] like Figure 1 and Figure 3As shown, the pulp molded wet preform Z0 includes a top Z02 and an original side wing wall thickness Z01 connected to the top Z02. The original side wing wall thickness Z01 has a transverse portion Z03 that is parallel or approximately parallel to the top Z02. When the hot-pressing forming die 2 closes to the forming inner expansion die 1 and continuously compresses the elastic component 31, an inclined inner expansion guide mechanism is provided between the forming inner expansion die 1 and the die base 3 to cause the forming inner expansion die 1 to expand radially outward. That is, the closing motion of the hot-pressing forming die 2 can drive the forming inner expansion die 1 to compress and thin the original side wing wall thickness Z01 in the radial direction, and also compress and thin the thickness of the top Z02 and the transverse portion Z03. The compressed and thinned pulp molded packaging product Z1 has a uniform wall thickness, except for the localized thickness of the inner convex Z11.
[0059] After hot pressing and shaping, subsequent post-processing such as edge trimming can be carried out. Post-processing does not require the pulp molded packaging product Z1 to be put into the corresponding conforming fixture, thus eliminating the risk of the inner diameter of the convex Z11 being expanded twice or multiple times.
[0060] Specifically, such as Figure 1 and Figure 3 As shown, the structure of the shaping inner expansion mold 1 includes a guide displacement outer mold 10 that is at least partially slidably fitted with the mold base 3, and a plurality of inner expansion molds 11 that are at least partially housed in the guide displacement outer mold 10 and are evenly distributed in a circle.
[0061] Specifically, at least a portion of the guide displacement outer mold 10 slides into the guide groove 30, and the elastic component 31 includes several springs, one end of which acts on the guide displacement outer mold 10 and the other end of which acts on the guide groove 30. To ensure the spring can stably exert its elastic force, a first blind hole 100 is provided at the bottom of the guide displacement outer mold 10, and a second blind hole 300 is provided at the bottom of the guide groove 30. One end of the spring extends into the first blind hole 100 and acts on the bottom of the first blind hole 100, while the other end of the spring extends into the second blind hole 300 and acts on the bottom of the second blind hole 300. At this time, the guide displacement outer mold 10 can move relative to the guide groove 30. When the spring is not compressed, the shaping inner expansion mold 1 is in an unexpanded state. When the spring is compressed to the set length (when the bottom surface of the guide displacement outer mold 10 contacts the bottom of the guide groove 30), the shaping inner expansion mold 1 expands into place, completing the compression and thinning process of the wall thickness of the pulp molded wet preform Z0.
[0062] Several circumferentially evenly distributed inner expansion molds 11 are at least partially housed within the guide displacement outer mold 10. Further, a receiving groove 101 is provided on the upper part of the guide displacement outer mold 10, and at least a portion of the inner expansion molds 11 are located within the receiving groove 101. Preferably, the bottom of the receiving groove 101 and the bottom surface of the inner expansion mold 11 are in sliding contact to achieve radial displacement stability of the inner expansion mold 11. Next, a transverse spring 12 is provided between the outer side of the inner expansion mold 11 and the guide displacement outer mold 10. For example, the outer end of the transverse spring 12 extends into a third blind hole 102 in the vertical groove wall of the receiving groove 101, and the inner end of the transverse spring 12 extends into a fourth blind hole 120 on the outer side of the inner expansion mold 11. The corresponding ends of the transverse spring 12 abut against the bottom of the third blind hole 102 and the bottom of the fourth blind hole 120.
[0063] That is, each inner expansion mold 11 is paired with at least one transverse spring 12. The transverse spring 12 and the elastic component 31 are vertically distributed, that is, the transverse spring 12 provides transverse elastic force, and the elastic component 31 provides vertical elastic force. The elastic force of the transverse spring 12 can cause the inner expansion mold 11 to return to its radial inward position after radial outward expansion. At the same time, the transverse spring 12 can also buffer the inner expansion mold 11 when it expands radially outward, so as to make the inner expansion mold 11 expand smoothly.
[0064] Furthermore, the receiving groove 101 is a stepped groove. The bottom groove wall of the receiving groove 101, parallel to the transverse spring 12, slides in contact with the inner expansion mold 11. The side groove walls of the receiving groove 101, perpendicular to the transverse spring 12, limit the outward displacement of the inner expansion mold 11.
[0065] The top mold 13 is placed on top of the inner expansion mold 11. The top mold 13 is shaped like the top Z02. The inner expansion mold 11 slides to support the bottom surface of the top mold 13. In other words, the top mold 13 will not move radially, but will only move up and down to compress and thin the wall thickness of the top Z02.
[0066] like Figure 1 and Figure 3 As shown, the inclined internal expansion guide mechanism includes the following structure:
[0067] A truncated cone 32 is fixed to the guide groove 30, and is fixed to the center area of the guide groove 30. The outer wall of the truncated cone 32 has a conical surface, and the inner wall of the inner expansion mold 11 has an inclined mating surface that matches the outer wall of the truncated cone 32. When the pulp molded wet preform Z0 is in an uncompressed and thinned state, the upper side of the inclined mating surface extends beyond the top of the truncated cone 32 (due to the elastic force of the elastic component 31). When the hot pressing forming die 2 moves downward, the inner expansion mold 11 moves downward relative to the truncated cone 32. During this displacement, the wall thickness of the pulp molded wet preform Z0 is continuously compressed and thinned. When the bottom of the outer guide mold 10 contacts the bottom of the guide groove 30 and the outer wall of the inner expansion mold 11 abuts against the side wall of the receiving groove 101, the inner expansion mold 11 is in the position of inner expansion and can no longer continue to move outward radially. After the inner expansion mold 11 stays for a certain period of time, the hot pressing forming die 2 is reset upward. At this time, the inner expansion mold 11 is also reset upward. Since the radial inward contraction of the inner expansion mold 11 can avoid the inner diameter of the inner convex Z11 from being enlarged during demolding, and since the inner convex Z11 is formed during hot pressing, the risk of the inner diameter of the inner convex Z11 being enlarged again during post-processing can be eliminated.
[0068] To facilitate the demolding of the top Z02 from the top mold 13, several demolding air channels 130 with open upper ends are provided inside the top mold 13 and / or the inner expansion mold 11. The demolding air channels 130 are connected to the air source. When the inner expansion mold 11 is separated from the inner protrusion Z11, the demolding air channels 130 then perform the action of introducing air pressure so that the top Z02 is demolded from the top mold 13.
[0069] Furthermore, a downwardly extending extension 131 is provided at the center of the lower surface of the top mold 13, and a through hole 320 is provided in the axial direction of the truncated cone 32. The extension 131 is columnar and inserted into the through hole 320, with a clearance fit between the extension 131 and the through hole 320. A through hole 33 is provided on the mold base 3, and a through hole 132 communicating with the through hole 33 is provided in the axial direction of the extension 131. The lower end of the demolding air passage 130 is connected to the transverse air passage 133, which is connected by an air supply pipe passing through the through hole 33 and the through hole 132. The transverse air passage 133 is at least one, and both ends of the transverse air passage 133 are also connected to the outside. The transverse air passage 133 and the demolding air passage 130 can form different orientations for demolding operations.
[0070] As another method of air supply pipeline, a cylindrical part 330 is provided at the upper opening of the through hole 33. The extension part 131 and the cylindrical part 330 are connected to each other and are dynamically sealed. For example, the extension part 131 is inserted into the cylindrical part 330, and the two are dynamically sealed and slidingly fitted, for example by setting a sealing ring. In this case, air blowing demolding can be achieved simply by setting an air source at the lower opening of the through hole 33.
[0071] Example 2
[0072] Based on Embodiment 1, this embodiment further discloses the following:
[0073] like Figure 1 , Figure 2 , Figure 3 and Figure 4 As shown, the manufacturing process of pulp molded packaging products includes the following steps:
[0074] S1. Wet preform forming: A pulp molded wet preform product Z0 with the original side wing wall thickness Z01 is obtained by pulp molding; the pulp molded wet preform product Z0 is a pulp molded wet preform cup lid with equal wall thickness.
[0075] S2, hot pressing shaping, at least forces the outer diameter of the original side wing wall thickness Z01 in S1 to remain unchanged; and
[0076] The pulp molded wet preform Z0 is fitted into the shaping inner bulging mold 1, and the shaping inner bulging mold 1 applies a radial inward bulging force from the inside to the outside to the original side wing wall thickness Z01. The radial inward bulging force compresses and thins the original side wing wall thickness Z01 to a set side wing wall thickness Z10; and
[0077] When the radial inward expansion force forces the original side wing wall thickness Z01 to compress and thin, at least a portion of the inner wall of the original side wing wall thickness Z01 and the shaping inner expansion mold 1 are shaped to form an inward protrusion Z11 that is set in the opposite direction to the radial inward expansion force.
[0078] like Figure 3 and Figures 6-10 As shown, the specific steps of S2 are as follows:
[0079] S21. Place the pulp molded wet preform Z0 between the shaping inner expansion mold 1 and the hot pressing shaping cavity mold 2 in the mold opening state.
[0080] S22. Place the pulp molded wet preform Z0 into the shaping inner expansion mold 1;
[0081] S23, the shaping inner bulging mold 1 and the hot pressing shaping concave mold 2 are closed and the pulp molded wet preform Z0 is hot pressed and shaped, at which time a dried pulp molded packaging product Z1 with at least a set side wing wall thickness Z10 is obtained, and an inner convex Z11 is formed by shaping the inner wall with a set side wing wall thickness Z10; and the top Z02 and the transverse part Z03 are compressed and thinned to a state where the thickness is equal to the set side wing wall thickness Z10.
[0082] S24, the hot pressing forming die 2 opens relative to the forming inner expansion die 1, and the forming inner expansion die 1 contracts radially under the elastic force of the transverse spring 12, causing the inner convex forming groove 1a of the forming inner expansion die 1 to disengage from the inner convex Z11, while the elastic component 31 forces the forming inner expansion die 1 to return to its original position upward.
[0083] Of course, the elastic component 31 can drive the shaping inner expansion mold 1 and the hot pressing shaping die 2 which is closed in the shaping inner expansion mold 1 to reset upward together. After the hot pressing shaping die 2 is reset in place, external force is used to make the hot pressing shaping die 2 open relative to the shaping inner expansion mold 1.
[0084] S25. After the shaping inner bulging mold 1 is detached from the pulp molded packaging product Z1, the pulp molded packaging product Z1 is removed.
[0085] like Figure 1 , Figure 2 , Figure 3 and Figure 4 As shown:
[0086] S3, demolding: the shaping inner bulge mold 1 in S2 shrinks radially, thereby causing the shaping inner bulge mold 1 to detach from the inner convex Z11.
[0087] In the above-mentioned S2, a hot pressing forming die 2 is provided, which is similar to the outer contour of the pulp molded wet preform Z0. The forming inner expansion die 1 is a hot pressing forming inner expansion punch, which is similar to the inner contour of the pulp molded wet preform Z0. Either the hot pressing forming die 2 or the forming inner expansion die 1 moves relative to the other and forces the forming inner expansion die 1 to apply a radial inward expansion force from the inside to the outside to the original side wing wall thickness Z01.
[0088] In this embodiment, the hot pressing forming die 2 moves relative to the forming inner bulging die 1.
[0089] During the molding of the inner convex Z11, the shaping inner bulge mold 1 and the hot pressing shaping cavity mold 2 respectively heat and dry the pulp molded wet preform Z0. The heating and drying are carried out by electric heating or steam heating, etc.
[0090] Example 3
[0091] like Figure 1 As shown, this embodiment provides a pulp molded packaging product, which is manufactured using the pulp molded packaging product manufacturing process of Embodiment 2.
[0092] The specific embodiments described herein are merely illustrative of the spirit of the invention. Those skilled in the art to which this invention pertains may make various modifications or additions to the described specific embodiments or use similar methods to substitute them, without departing from the spirit of the invention or exceeding the scope defined by the appended claims.
Claims
1. An internal convex molding process for pulp molded packaging products, wherein the pulp molded packaging product (Z1) has a set side wing wall thickness (Z10), characterized in that, The internal convex forming process includes the following steps: This at least forces the outer diameter of the original sidewall wall thickness (Z01) of the pulp molded wet preform (Z0) to remain unchanged; The pulp molded wet preform (Z0) is fitted onto the shaping inner bulging mold (1); The hot pressing forming die (2) is provided to conform to the outer contour of the pulp molded wet preform (Z0), and the forming inner expansion die (1) is a hot pressing forming inner expansion punch that conforms to the inner contour of the pulp molded wet preform (Z0); either the hot pressing forming die (2) or the forming inner expansion die (1) moves relative to the other. An inclined internal expansion guide mechanism is provided between the shaping internal expansion mold (1) and the hot pressing shaping die (2); the shaping internal expansion mold (1) is at least partially housed in the guide groove (30) of the mold base (3); the shaping internal expansion mold (1) can move vertically relative to the mold base (3); the side of the shaping internal expansion mold (1) away from the hot pressing shaping die (2) is connected to the mold base (3) through an elastic component (31); The shaping inner expansion mold (1) includes a guide displacement outer mold (10) and several inner expansion molds (11). The guide displacement outer mold (10) is at least partially slidably engaged with the guide groove (30) of the mold base (3). The guide displacement outer mold (10) has a receiving groove (101) on its upper part. The inner expansion mold (11) is at least partially placed in the receiving groove (101). The bottom of the receiving groove (101) is in sliding contact with the bottom surface of the inner expansion mold (11). A transverse spring (12) is assembled between the outer side of the inner expansion mold (11) and the guide displacement outer mold (10). The inclined inner expansion guide mechanism includes a truncated cone (32) fixedly arranged in the central area of the guide groove (30). The outer wall of the truncated cone (32) is provided with a conical surface. The inner wall of the inner expansion mold (11) is provided with an inclined mating surface adapted to the conical surface. During the relative movement between the hot pressing forming die (2) and the forming inner expansion die (1), the forming inner expansion die (1) is driven to expand radially outward by means of the inclined inner expansion guide mechanism, so that the forming inner expansion die (1) applies a radial inward expansion force from the inside to the outside to the original side wing wall thickness (Z01). This radial inward expansion force compresses the original side wing wall thickness (Z01) to thin it to the set side wing wall thickness (Z10). The shaping inner expansion mold (1) has an inner convex forming groove (1a); during the process of compressing the original side wing wall thickness (Z01) with radial inner expansion force to make it thinner, part of the material of the original side wing wall thickness (Z01) is squeezed into the inner convex forming groove (1a), and an inner convex (Z11) is formed between the inner wall of the original side wing wall thickness (Z01) and the shaping inner expansion mold (1), which is oriented in the opposite direction to the radial inner expansion force. The inner convex (Z11) is formed inside the inner convex forming groove (1a).
2. The internal convex forming process for pulp molded packaging products according to claim 1, characterized in that, When the inner forming mold (1) contracts radially, it forces the inner convex forming groove (1a) to disengage from the inner convex (Z11).
3. The production process of pulp molded packaging products, characterized in that, The production process includes the following steps: S1. Wet preform forming: A pulp molded wet preform (Z0) with the original side wing wall thickness (Z01) is obtained by pulp molding. S2. Hot pressing and shaping, using the internal convex forming process of pulp molded packaging products as described in any one of claims 1-2; S3, demolding, the shaping inner bulge mold (1) in S2 shrinks radially so that the shaping inner bulge mold (1) disengages from the inner convex (Z11).
4. The production process of the pulp molded packaging product according to claim 3, characterized in that, During the molding of the inner convex part (Z11), the shaping inner bulge mold (1) and the hot pressing shaping die (2) respectively heat and dry the pulp molded wet preform (Z0).
5. The production process of the pulp molded packaging product according to claim 3, characterized in that, In S1 above, the pulp molded wet preform (Z0) is a pulp molded wet preform cup lid with equal wall thickness.
Citation Information
Patent Citations
Manufacture process of disposable bowl cover and bowl cover made by same
CN101637982A
Hot-pressing shaping mold and production line for molded pulp packaging products
CN223033755U