A repair device for OVD deposition and a control method thereof

By using a deposition torch and a repair torch in conjunction with a particle monitor and control unit during the OVD deposition process of optical fiber preforms, the problem of easy breakage of porous optical fiber preforms is solved, and the production quality of optical fiber preforms is improved.

CN119191698BActive Publication Date: 2026-11-24TENGCANG FENGHUO PHOTOELECTRIC MATERIAL TECH CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202411464713.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-10-21
Publication Date
2026-11-24
Estimated Expiration
2044-10-21

AI Technical Summary

Technical Problem

During the OVD deposition process, the irregular movement of silica particles and uneven temperature cause the porous structure of the optical fiber preform to easily break, affecting the production quality.

Method used

By using deposition torches and repair torches in conjunction with particle monitors and control units, the emission of combustion gases can be monitored and controlled in real time, thereby increasing the deposition temperature in areas at risk of rupture and reducing the risk of rupture.

Benefits of technology

This effectively reduces the risk of edge breakage in optical fiber preforms, improving the quality and production efficiency of optical fiber preforms.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119191698B_ABST
    Figure CN119191698B_ABST
Patent Text Reader

Abstract

This application relates to a repair apparatus and control method for OVD deposition. The apparatus includes: a deposition torch, which moves along the axial direction of an optical fiber preform and sprays reactive gas toward the optical fiber preform; a repair torch, which is located on different sides of the deposition torch and sprays combustible gas toward a fracture risk area; a particle monitor, whose camera is positioned toward the fracture risk area of ​​the optical fiber preform, and which monitors particle state parameters in the space where the fracture risk area is located when the deposition torch moves around the fracture risk area; and a control unit, which controls the repair torch to spray combustible gas according to the particle state parameters in the space where the fracture risk area is located. This application can repair the loose material deposited on the optical fiber preform online during the OVD deposition process, reducing the fracture risk.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application relates to the field of optical fiber preform manufacturing technology, specifically to a repair device and its control method for OVD deposition. Background Technology

[0002] The production of optical fiber preforms involves an OVD deposition process. During the OVD deposition process, a deposition torch moves back and forth in the deposition chamber, spraying gaseous raw materials onto the core rod through an oxyhydrogen flame, and finally reacting and depositing to form a porous silica body.

[0003] The silica particles generated after the raw material reaction are submicron in size and have an individual temperature of around 1000℃. They move at high speed with the oxyhydrogen flame and then adhere to the surface of the mandrel. The silica particles exhibit irregular movement due to the influence of airflow, temperature, and morphology, and the aggregate volume of each silica particle is also inconsistent. This causes the porous silica mass to be prone to breakage at any time due to stress. Summary of the Invention

[0004] Based on the above description, this application provides a repair device and control method for OVD deposition to solve the problem of the risk of breakage of the porous material deposited on the optical fiber preform.

[0005] According to a first aspect, this application provides a repair apparatus for OVD deposition, comprising:

[0006] A deposition torch is positioned on the outside of the optical fiber preform and moves along the axial direction of the optical fiber preform. The deposition torch is used to spray reactive gas toward the optical fiber preform.

[0007] A repair torch and a deposition torch are located on different sides of the optical fiber preform, and the repair torch is used to spray combustion gas toward the crack risk area of ​​the optical fiber preform.

[0008] A particle monitor, wherein the camera of the particle monitor is positioned facing the fracture risk area of ​​the optical fiber preform, the particle monitor being used to monitor particle state parameters in the space where the fracture risk area is located as the deposition torch moves to the vicinity of the fracture risk area; and

[0009] The control unit is connected to the repair torch and the particle monitor signal respectively. The control unit controls the repair torch to spray combustion gas according to the particle state parameters of the space where the rupture risk area is located. The rupture risk area includes the edge area of ​​at least one side of the optical fiber preform along the axial direction.

[0010] In one or more embodiments, the repair torch is configured to be movable to one side of the area at risk of breakage of the optical fiber preform; or

[0011] The repair torch is positioned towards the side of the fiber optic preform at risk of breakage.

[0012] In one or more embodiments, the repair torch is configured to be movable to one side of the standby position of the deposition torch; the particle monitor's camera is positioned close to the standby position of the deposition torch and is rotatable.

[0013] When the deposition torch returns to the standby position, the control unit controls the particle monitor to rotate the camera and monitor the particle state parameters in the space where the nozzle of the deposition torch is located, so as to control the repair torch to spray cleaning gas.

[0014] In one or more embodiments, the standby position of the deposition torch is located on one side of the axial direction of the optical fiber preform, and the breakage risk area is the edge region of the optical fiber preform near the standby position of the deposition torch.

[0015] In one or more embodiments, the particle monitor includes a camera and an information processing unit that are communicatively connected;

[0016] The camera includes an infrared camera unit and a high-definition camera unit. The infrared camera unit is used to acquire heat distribution images, and the high-definition camera unit is used to acquire particle space images.

[0017] The information processing unit is used to determine the particle state parameters of the monitored particles based on the heat distribution image and the particle space image. The particle state parameters include particle temperature, particle size and particle motion speed.

[0018] According to a second aspect, this application provides a control method for a repair apparatus for OVD deposition, comprising:

[0019] Turn on the deposition torch. The deposition torch moves along the axis of the optical fiber preform and sprays the reactive gas onto the optical fiber preform. The repair torch is in standby mode.

[0020] When the deposition torch moves to the vicinity of the fracture risk area of ​​the optical fiber preform, the control unit controls the particle monitor to monitor the particle state parameters in the space where the fracture risk area is located.

[0021] When the particle state parameter meets the first preset condition, the control unit controls the repair torch to spray a first flow rate of combustion gas toward the rupture risk area;

[0022] The particle state parameters include particle temperature, particle size, and particle velocity.

[0023] The first preset condition is: the proportion of the number of particles with a temperature greater than a first temperature threshold and a size greater than a first size threshold to the total number of monitored particles is greater than a first proportion threshold, while the proportion of the number of particles with a temperature greater than a first temperature threshold and a velocity greater than a first velocity threshold to the total number of monitored particles is less than a second proportion threshold.

[0024] In one or more embodiments, it further includes:

[0025] After the repair torch sprays out a first flow rate of combustion gas and continues for a first preset time, if the particle state parameters still meet the first preset condition, the control unit controls the repair torch to spray out a second flow rate of combustion gas and continues for a second preset time before returning to standby mode.

[0026] Wherein, the second flow rate is greater than the first flow rate; and the second preset time is greater than the first preset time.

[0027] In one or more embodiments, the repair torch is configured to be movable to one side of the standby position of the deposition torch; the camera of the particle monitor is positioned close to the standby position of the deposition torch and is rotatable; the control method further includes:

[0028] When the deposition torch returns to the standby position after spraying for a preset time, the control unit controls the rotation of the camera of the particle monitor to monitor the particle state parameters in the space where the nozzle of the deposition torch is located.

[0029] When the particle state parameter meets the second preset condition, the control unit controls the repair torch to move to one side of the standby position of the deposition torch and sprays a third flow of cleaning gas toward the nozzle of the deposition torch.

[0030] The second preset condition is that the proportion of particles with a temperature greater than the second temperature threshold and a size greater than the second size threshold to the total number of monitored particles is greater than the third proportion threshold, while the proportion of particles with a temperature greater than the second temperature threshold and a motion rate greater than the second velocity threshold to the total number of monitored particles is less than the fourth proportion threshold.

[0031] In one or more embodiments, the second temperature threshold is less than the first temperature threshold, the second size threshold is greater than the first size threshold, the second rate threshold is less than the first rate threshold, the third ratio threshold is greater than the first ratio threshold, and the fourth ratio threshold is less than the second ratio threshold.

[0032] In one or more embodiments, it further includes:

[0033] After the repair blowtorch sprays out a third flow rate of cleaning gas for a third preset time, if the particle state parameters still meet the second preset condition, the control unit controls the repair blowtorch to spray out a fourth flow rate of cleaning gas for a fourth preset time and then returns to the standby state.

[0034] Wherein, the fourth flow rate is greater than the third flow rate; the fourth preset time is greater than the third preset time. Compared with the prior art, the technical solution of this application has the following beneficial technical effects:

[0035] By setting up a deposition torch, a repair torch, a particle monitor, and a control unit, and designating at least one edge region along the axial direction of the optical fiber preform as a breakage risk area, the deposition torch reciprocates along the axial direction of the optical fiber preform and sprays reactive gas. When the deposition torch moves to the breakage risk area of ​​the optical fiber preform, the particle monitor uses a camera to monitor the particle state parameters in the space where the breakage risk area is located. Based on the particle state parameters in the space where the breakage risk area is located, the control unit can control the repair torch to spray combustion gas towards the breakage risk area, thereby helping to increase the silica particle deposition temperature in the breakage risk area, reduce the breakage risk in the edge region of the optical fiber preform, and improve the quality of the optical fiber preform. Attached Figure Description

[0036] Figure 1 A schematic diagram of a repair apparatus for OVD deposition in a usage state, provided as an embodiment of this application;

[0037] Figure 2 A schematic diagram of the structure of a repair device for OVD deposition provided in another embodiment of this application in another usage state;

[0038] Figure 3 A schematic flowchart of a control method for a repair apparatus for OVD deposition provided in an embodiment of this application;

[0039] Figure 4 A schematic flowchart of a control method for a repair apparatus for OVD deposition, provided in another embodiment of this application.

[0040] Explanation of reference numerals in the attached figures:

[0041] Deposition torch 10;

[0042] Repairing a blowtorch: 20;

[0043] Particle monitor 30, camera 31, information processing unit 32;

[0044] Control unit 40;

[0045] Optical fiber preform L;

[0046] Rupture risk zone r;

[0047] First direction F1, second direction F2. Detailed Implementation

[0048] To facilitate understanding of this application, a more complete description will be provided below with reference to the accompanying drawings, which illustrate embodiments of the present application. However, the present application can be implemented in many different forms and is not limited to the embodiments described herein. Rather, these embodiments are provided so that the disclosure of this application will be thorough and complete.

[0049] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this application belongs. The terminology used herein is for the purpose of describing particular embodiments only and is not intended to be limiting of the application.

[0050] It is understood that when one element is considered to be "connected" to another element, it can be directly connected to the other element or connected to the other element through an intermediary element. In the following embodiments, "connection" should be understood as "electrical connection," "communication connection," etc., if the connected circuits, modules, units, etc., have the transmission of electrical signals or data between them.

[0051] See Figure 1 , Figure 1 A schematic diagram of a repair apparatus for OVD deposition provided in an embodiment of this application is shown. The repair apparatus for OVD deposition provided in an embodiment of this application includes a deposition torch 10, a repair torch 20, a particle monitor 30, and a control unit 40. A deposition torch 10 is located on the outside of the optical fiber preform L and is movable along the axial direction of the optical fiber preform L. The deposition torch 10 is used to spray reactive gas toward the optical fiber preform L. A repair torch 20 and the deposition torch 10 are located on different sides of the optical fiber preform L, and the repair torch 20 is used to spray combustion gas toward the fracture risk region r of the optical fiber preform L. The camera 31 of the particle monitor 30 is positioned toward the fracture risk region r of the optical fiber preform L. The particle monitor 30 is used to monitor the particle state parameters in the space where the fracture risk region r is located when the deposition torch 10 moves to the fracture risk region r. A control unit 40 is signal-connected to the repair torch 20 and the particle monitor 30 respectively. The control unit 40 controls the repair torch 20 to spray combustion gas according to the particle state parameters in the space where the fracture risk region r is located. The fracture risk region r includes at least one edge region along the axial direction of the optical fiber preform L. The first direction F1 is parallel to the axial direction of the optical fiber preform L.

[0052] It should be noted that the repair device in this embodiment is installed in the deposition chamber, where the deposition and repair process of the optical fiber preform L is completed. The optical fiber preform L is initially a core rod, which is installed in the deposition chamber. In this embodiment, the optical fiber preform L is rotatable along its axial direction to ensure sufficient deposition of porous material on its circumferential surface. During the deposition of porous material on the optical fiber preform L, since one edge region along the axial direction of the optical fiber preform L is the starting deposition region and the other edge region is the ending deposition region, the deposition temperature in the two edge regions is relatively unstable, leading to a higher risk of breakage of the porous material deposited in the two edge regions. Therefore, in this embodiment, the breakage risk area r of the optical fiber preform L includes at least one edge region along the axial direction of the optical fiber preform L, and at least one edge region of the optical fiber preform L is monitored and repaired.

[0053] Specifically, the deposition torch 10 is generally made of quartz glass, and the core temperature during deposition is relatively high, around 1200℃. During the deposition process, the deposition torch 10 reciprocates along the first direction F1, while simultaneously spraying reactive gases, including hydrogen, oxygen, and reactants (such as silicon tetrachloride), onto the optical fiber preform L to generate silicon dioxide particles that are deposited on the optical fiber preform L, while also generating a high-temperature flame. It should be noted that the reciprocating motion of the deposition torch 10 along the first direction F1 can be achieved by setting a guide rail and a motor. The setting of the guide rail and motor is a conventional mechanical technique and will not be elaborated upon in this embodiment. In this embodiment, the number of deposition torches 10 can be one or more, with multiple deposition torches 10 spaced apart. For example, it can be set to one, two, three, or four deposition torches 10, depending on the length of the optical fiber preform L and the deposition time, etc., and this embodiment does not impose any limitations.

[0054] Repair torch 20 and deposition torch 10 are located on different sides of the optical fiber preform L. Repair torch 20 is used to spray combustion gas toward the fracture risk area r of the optical fiber preform L. The combustion gas is used to increase heat to compensate for the deposition temperature in the fracture risk area r, thereby reducing the occurrence of fracture. In this embodiment, the combustion gas includes hydrogen and oxygen. Furthermore, nitrogen may be added to the combustion gas to prevent hydrogen dispersion, thereby allowing the combustion flame to concentrate and further increasing the temperature.

[0055] The particle monitor 30 is used to monitor the state parameters of silica particles floating in the space of the fracture risk region r when the deposition torch 10 moves to the vicinity of the fracture risk region r. The camera 31 of the particle monitor 30 is positioned facing the fracture risk region r of the optical fiber preform L. The camera 31 and the repair torch 20 are located at different peripheral positions on the optical fiber preform L. The camera 31 monitors the product particle images in the space of the fracture risk region r, and determines the particle state parameters through image analysis. These particle state parameters may include particle temperature, particle size, and particle velocity. It should be noted that the position of the deposition torch 10 can be detected by a position sensor. When the deposition torch 10 moves to the vicinity of the fracture risk region r of the optical fiber preform L or to a designated position, the position sensor feeds a position signal back to the control unit 40. The control unit 40 then controls the particle monitor 30 to monitor the particle state parameters in the space of the fracture risk region r of the optical fiber preform L.

[0056] It is understood that the number of repair torches 20 and particle monitors 30 can be set to one or two. For example, a repair torch 20 and a particle monitor 30 can be set near the edge area on one side of the optical fiber preform L, or a repair torch 20 and a particle monitor 30 can be set near the edge areas on both sides of the optical fiber preform L. The specific setting can be reasonably set according to the actual process and cost considerations. This embodiment does not impose any restrictions here.

[0057] The control unit 40 can be a microcontroller or an embedded controller. The control unit 40 is connected to the repair torch 20 and the particle monitor 30 respectively. The control unit 40 controls the operation of the repair torch 20 according to the particle state parameters of the space where the fracture risk area r is located. For example, if the temperature, size or movement rate of most of the currently monitored silica particles does not meet the conditions for sufficient deposition or meets the conditions for deposition fracture, the control unit 40 controls the repair torch 20 to spray combustion gas and controls parameters such as spray flow rate and time.

[0058] In this embodiment, during the pre-deposition or deposition process, the deposition torch 10 reciprocates along the axial direction of the optical fiber preform L and sprays reactive gas. When the deposition torch 10 moves to the fracture risk area r of the optical fiber preform L, the control unit 40 controls the camera 31 of the particle monitor 30 to monitor the particle state parameters in the space where the fracture risk area r is located. Based on the particle state parameters in the space where the fracture risk area r is located, the control unit 40 can control the repair torch 20 to spray combustion gas toward the fracture risk area r, thereby helping to increase the deposition temperature of the fracture risk area r, reduce the fracture risk of the optical fiber preform L, and improve the quality of the optical fiber preform L.

[0059] In some embodiments, the repair torch 20 is configured to move to one side of the fracture risk area r of the optical fiber preform L. Specifically, the control unit 40 can control the repair torch 20 to move from a standby position along a first direction F1 to the fracture risk area r of the optical fiber preform L, thereby enabling the repair torch 20 to spray combustion gas toward the fracture risk area r, or to reciprocate along the first direction F1 during the spraying of combustion gas, so as to expand the spray range and fully cover the area near the fracture risk area r. It should be noted that the movable function of the repair torch 20 along the first direction F1 can be achieved by setting a guide rail and a motor. The setting of the guide rail and motor is a conventional mechanical technology, and will not be described in detail in this embodiment.

[0060] Alternatively, the repair torch 20 can be positioned towards the fracture risk area r of the optical fiber preform L. Specifically, both the repair torch 20 and the camera 31 of the particle monitor 30 are positioned towards the fracture risk area r of the optical fiber preform L, and the repair torch 20 and the camera 31 of the particle monitor 30 are positioned opposite each other, thereby enabling the monitoring and repair of product particles in the space where the fracture risk area r is located.

[0061] During the OVD deposition process of related technologies, the deposition torch 10 may accumulate unwanted silica particles in the nozzle due to high temperature. If there are too many, it will interfere with the flame and normal silica particle deposition, and may even cause the porous body to crack and stop during the OVD deposition process.

[0062] Based on this, see Figure 1 and Figure 2 In some embodiments, the repair torch 20 is configured to be movable to one side of the standby position of the deposition torch 10; the camera 31 of the particle monitor 30 is positioned close to the standby position of the deposition torch 10 and is rotatable; when the deposition torch 10 returns to the standby position, the control unit 40 controls the particle monitor 30 to rotate the camera 31 and monitor the particle state parameters in the space where the nozzle of the deposition torch 10 is located, so as to control the repair torch 20 to spray cleaning gas.

[0063] It should be noted that, in this embodiment, the standby positions of the repair torch 20 and the deposition torch 10 are both located near one side of the optical fiber preform L-axis direction and are arranged opposite each other along the second direction F2. The repair torch 20 can be moved along the second direction F2 to the vicinity of the standby position of the deposition torch 10. The camera 31 of the particle monitor 30 can be rotated about 90° so that the camera 31 can face the nozzle of the deposition torch 10 located in the standby position.

[0064] Specifically, in the later stages of deposition, the deposition torch 10 may accumulate unwanted silica particles in the nozzle due to high temperature. When the deposition torch 10 returns to the standby position, the control unit 40 controls the particle monitor 30 to rotate the camera 31 to monitor the state parameters of the silica particles floating in the space where the nozzle of the deposition torch 10 is located. Based on the particle state parameters in the space where the nozzle of the deposition torch 10 is located, the control unit 40 controls the action of the repair torch 20. For example, based on the particle state parameters in the space where the nozzle of the deposition torch 10 is located, if the temperature, size, or movement rate of most of the silica particles meets the cleaning conditions, the control unit 40 controls the repair torch 20 to move from the standby position along the second direction F2 to the vicinity of the standby position of the deposition torch 10, spray cleaning gas towards the nozzle of the deposition torch 10, and control parameters such as spray flow rate and time. It should be noted that nitrogen can be used as the cleaning gas. Nitrogen is used to purge and purify the silica particles deposited on the nozzle of the deposition torch 10 to reduce interference with the reaction flame, so that the silica particles can be deposited normally on the optical fiber preform L, thereby reducing the risk of the loose body breaking and shutting down during the OVD deposition process.

[0065] In some embodiments, the standby position of the deposition torch 10 is located on one side of the optical fiber preform L along the axial direction, and the breakage risk area r is the edge region on the optical fiber preform L near the standby position of the deposition torch 10.

[0066] Specifically, as the deposition torch 10 moves from the standby position along the first direction F1 and sprays reactive gas onto the optical fiber preform L, the temperature in the edge region of the optical fiber preform L near the standby position of the deposition torch 10 rises from an initial low temperature to a high temperature, resulting in a large temperature change. The risk of cracking of the porous deposited body in the edge region of the optical fiber preform L on this side is higher than that on the other side. Furthermore, based on OVD deposition process experience, cracking is more common in the edge region of the optical fiber preform L near the standby position of the deposition torch 10. Considering cost control, in this embodiment, the edge region of the optical fiber preform L near the standby position of the deposition torch 10 is monitored and repaired.

[0067] In some embodiments, the particle monitor 30 includes a camera 31 and an information processing unit 32 connected in communication; the camera 31 includes an infrared camera unit and a high-definition camera unit, the infrared camera unit is used to acquire heat distribution images, and the high-definition camera unit is used to acquire particle space images; the information processing unit 32 is used to determine the particle state parameters of the monitored particles based on the heat distribution images and the particle space images, the particle state parameters including particle temperature, particle size and particle motion rate.

[0068] Specifically, camera 31 includes an infrared camera unit and a high-definition camera unit, and collects information to the information processing unit 32. The infrared camera unit can acquire heat distribution images of the monitored object (silica particles) within a specified monitoring range of 100*100mm, providing temperature data with a temperature range of 50–2000℃, an accuracy of ±0.2℃, and a sampling frequency of 1μs–100s. The high-definition camera unit can capture particle spatial images of the monitored object (silica particles) within a specified monitoring range of 100*100mm, providing particle diameter data with a diameter range of 0.1–100mm and a sampling frequency of 1μs–100s. It should be noted that each camera unit has 50 channels, enabling simultaneous monitoring of 0–50 silica particles. The information processing unit 32 determines the diameter of each monitored particle by calculating pixel coordinates based on the real-time acquired particle space image, and calculates the motion speed of each monitored particle based on the different coordinates of the monitored particles at different time points. The particle motion speed is in the range of 2m / s to 50m / s. The infrared camera unit and the high-definition camera unit share the same position coordinates. The information processing unit 32 determines the temperature of each monitored particle based on the real-time acquired heat distribution image. In this way, the particle state parameters of the monitored particles are accurately determined based on the heat distribution image and the particle space image.

[0069] See Figure 1 and Figure 3 Based on the same inventive concept, embodiments of this application also provide a control method for a repair apparatus for OVD deposition, comprising:

[0070] S301. Turn on the deposition torch 10. The deposition torch 10 moves along the axis of the optical fiber preform L and sprays reaction gas onto the optical fiber preform L. The repair torch 20 is in standby mode.

[0071] S302. When the deposition torch 10 moves to the vicinity of the fracture risk area r of the optical fiber preform L, the control unit 40 controls the particle monitor 30 to monitor the particle state parameters in the space where the fracture risk area r is located.

[0072] S303. When the particle state parameter meets the first preset condition, the control unit 40 controls the repair torch 20 to spray a first flow rate of combustion gas toward the rupture risk area r.

[0073] The particle state parameters include particle temperature, particle size, and particle velocity. The first preset condition is that the proportion of particles with a temperature greater than a first temperature threshold and a size greater than a first size threshold to the total number of monitored particles is greater than a first proportional threshold, while the proportion of particles with a temperature greater than the first temperature threshold and a velocity greater than a first velocity threshold to the total number of monitored particles is less than a second proportional threshold. In this embodiment, the first temperature threshold is 450°C to 550°C, specifically 450°C, 480°C, 500°C, 520°C, or 550°C. The first size threshold is 0.8mm to 1.2mm, specifically 0.8mm, 0.9mm, 1mm, 1.1mm, or 1.2mm. The first velocity threshold is 18m / s to 22m / s, specifically 18m / s, 19m / s, 20m / s, 21m / s, or 22m / s. The first percentage threshold is 25% to 35%, specifically 25%, 30%, or 35%; the second percentage threshold is 75% to 85%, specifically 75%, 80%, or 85%.

[0074] Specifically, the deposition torch 10 moves from its standby position along the first direction F1, simultaneously spraying hydrogen, oxygen, and reaction materials toward the optical fiber preform L. The repair torch 20 is in standby mode, spraying combustion gas at a standby flow rate, which is relatively low. The combustion gas includes hydrogen and oxygen. Furthermore, nitrogen can be added to this combustion gas to prevent hydrogen dispersion, thereby allowing the combustion flame to concentrate and further increasing the temperature. In this embodiment, the first flow rate of the combustion gas is 2.5 to 3.5 times the standby flow rate, specifically 2.5 times, 3 times, or 3.5 times, which can be set according to actual conditions.

[0075] In a specific embodiment, when the deposition torch 10 moves to the vicinity of the fracture risk area r or a designated position of the optical fiber preform L, it can be detected by a position sensor and fed back to the control unit 40. The control unit 40 controls the particle monitor 30 to monitor the particle state parameters in the space where the fracture risk area r is located. The particle monitor 30 or the control unit 40 can calculate the proportion a1 of the number of particles with a temperature greater than 500° and a particle size greater than 1 mm to the total number of monitored particles, and the proportion b1 of the number of particles with a temperature greater than 500° and a particle speed greater than 20 m / s to the total number of monitored particles. When a1 is greater than 1 mm, the particle size distribution is considered to be larger than 1 mm. When the concentration of a1 is 30% and b1 is less than 80%, it is determined that the loose material deposited in the fracture risk area r may fracture at any time. The control unit 40 then controls the repair torch 20 to move along the first direction F1 to the fracture risk area r of the optical fiber preform L and spray hydrogen and oxygen at 3 times the standby flow rate, while the nitrogen flow rate remains unchanged until a1 is less than or equal to 30%, and / or b1 is greater than or equal to 80%. At this time, the repair torch 20 returns to the standby state. In this way, the deposition status of the fracture risk area r of the optical fiber preform L is monitored in real time and repaired online to reduce the risk of loose material fracture and improve the quality of the optical fiber preform L.

[0076] In some embodiments, after the repair torch 20 sprays a first flow rate of combustion gas and continues for a first preset time, if the particle state parameters still meet the first preset condition, the control unit 40 controls the repair torch 20 to spray a second flow rate of combustion gas and continue for a second preset time before returning to the standby state; the second flow rate is greater than the first flow rate; the second preset time is greater than the first preset time.

[0077] Specifically, in this embodiment, the second flow rate of the combustion gas is 4.5 to 5.5 times the standby flow rate, specifically 4.5 times, 5 times, or 5.5 times. The first preset time is 2.5 min to 3.5 min, specifically 2.5 min, 3 min, or 3.5 min. The second preset time is 4.5 min to 5.5 min, specifically 4.5 min, 5 min, or 5.5 min.

[0078] In one specific embodiment, the control unit 40 controls the repair torch 20 to spray hydrogen and oxygen at three times the standby flow rate for 3 minutes. If the particle state parameters still meet the first preset condition, the control unit 40 controls the repair torch 20 to spray hydrogen and oxygen at five times the standby flow rate for 5 minutes before returning to standby mode. Thus, during the repair process, the spray flow rate and spray time of the repair torch 20 are adjusted according to the real-time monitored particle state parameters to precisely control the repair effect, reducing the silica porosity cracking rate by 40% during the OVD deposition stage and effectively improving the quality of the optical fiber preform L.

[0079] See Figure 1, Figure 2 and 4 In some embodiments, the repair torch 20 is configured to be movable to one side of the standby position of the deposition torch 10; the camera 31 of the particle monitor 30 is positioned close to the standby position of the deposition torch 10 and is rotatable; the control method of this application further includes:

[0080] S401 When the deposition torch 10 returns to the standby position after spraying for a preset spray time, the control unit 40 controls the camera 31 of the particle monitor 30 to rotate in order to monitor the particle state parameters in the space where the nozzle of the deposition torch 10 is located.

[0081] S402. When the particle state parameter meets the second preset condition, the control unit 40 controls the repair torch 20 to move to one side of the standby position of the deposition torch 10, and sprays a third flow rate of cleaning gas toward the nozzle of the deposition torch 10. In this embodiment, the cleaning gas can be nitrogen.

[0082] The second preset condition is as follows: the proportion of particles with a temperature greater than a second temperature threshold and a size greater than a second size threshold to the total number of monitored particles is greater than a third proportion threshold, while the proportion of particles with a temperature greater than the second temperature threshold and a velocity greater than a second velocity threshold to the total number of monitored particles is less than a fourth proportion threshold. Further, the second temperature threshold is less than the first temperature threshold, the second size threshold is greater than the first size threshold, the second velocity threshold is less than the first velocity threshold, the third proportion threshold is greater than the first proportion threshold, and the fourth proportion threshold is less than the second proportion threshold. In this embodiment, the second temperature threshold is 350° to 450°, specifically 350°, 380°, 400°, 420°, or 450°. The first size threshold is 2.5mm to 3.5mm, specifically 2.5mm, 2.8mm, 3mm, 3.2mm, or 3.5mm. The first velocity threshold is 8m / s to 12m / s, specifically 8m / s, 9m / s, 10m / s, 11m / s, or 12m / s. The first proportional threshold is 45% to 55%, specifically taking the values ​​of 45%, 50%, or 55%. The second proportional threshold is 45% to 55%, specifically taking the values ​​of 45%, 50%, or 55%. Furthermore, in this embodiment, the third flow rate of the cleaning gas is 3.5 to 4.5 times the standby flow rate, specifically 3.5 times, 4 times, or 4.5 times, which can be set according to the actual situation.

[0083] In a specific embodiment, during the later stage of deposition, the deposition torch 10 returns to the standby position along the first direction F1. That is, when the deposition torch 10 returns to the standby position after spraying for a preset spray time, the control unit 40 controls the camera 31 of the particle monitor 30 to rotate to monitor the particle state parameters in the space where the nozzle of the deposition torch 10 is located. The particle monitor 30 or the control unit 40 can calculate the proportion a2 of the number of particles with a temperature greater than 400° and a particle size greater than 3mm to the total number of monitored particles, and the proportion b2 of the number of particles with a temperature greater than 400° and a particle speed greater than 10m / s to the total number of monitored particles. When a2 is greater than 50% and b2 is less than 50%, it is determined that the deposition torch 10 has deposited... If there are too many silica particles deposited, the control unit 40 controls the repair torch 20 to move from the standby position along the second direction F2 to the vicinity of the standby position of the deposition torch 10, and sprays nitrogen gas at 4 times the standby flow rate. At the same time, hydrogen and oxygen maintain the standby flow rate until a2 is less than or equal to 50%, and / or b2 is greater than or equal to 50%. Then the repair torch 20 returns to the standby state. In this way, the excessive silica particles deposited on the deposition torch 10 are monitored and repaired online. The silica particles deposited on the nozzle of the deposition torch 10 are purged with nitrogen gas to reduce interference with the reaction flame, so that the subsequent silica particles can be deposited normally on the optical fiber preform L, reducing the risk of the loose body breaking and shutdown during the OVD deposition process.

[0084] In some embodiments, the control method of this application further includes:

[0085] After the repair blowtorch 20 sprays a third flow rate of cleaning gas for a third preset time, if the particle state parameters still meet the second preset condition, the control unit 40 controls the repair blowtorch 20 to spray a fourth flow rate of cleaning gas for a fourth preset time before returning to standby mode; wherein, the fourth flow rate is greater than the third flow rate; and the fourth preset time is greater than the third preset time.

[0086] Specifically, in this embodiment, the fourth flow rate of the cleaning gas is 5.5 to 6.5 times the standby flow rate, specifically 5.5 times, 6 times, or 6.5 times. The first preset time is 0.8 min to 1.2 min, specifically 0.8 min, 1 min, or 1.2 min. The second preset time is 1.8 min to 2.2 min, specifically 1.8 min, 2 min, or 2.2 min.

[0087] In one specific embodiment, after the repair blowtorch 20 sprays nitrogen at four times the standby flow rate for 1 mm, if the particle state parameters still meet the second preset condition, the control unit 40 controls the repair blowtorch 20 to spray nitrogen at six times the standby flow rate for 2 mm before returning to standby mode. Thus, during the cleaning of the nozzle of the deposition blowtorch 10, the spray flow rate and spray time of the repair blowtorch 20 are adjusted according to the real-time monitored particle state parameters to precisely control the cleaning effect, effectively blowing away the silica particles deposited on the nozzle of the deposition blowtorch 10, thereby extending the service life of the deposition blowtorch 10 by 150%.

[0088] The above description is only a preferred embodiment of this application and is not intended to limit this application. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this application should be included within the protection scope of this application.

Claims

1. A repair apparatus for OVD deposition, characterized in that, include: A deposition torch is located on the outside of the optical fiber preform and is movable along the axial direction of the optical fiber preform. The deposition torch is used to spray reactive gas toward the optical fiber preform. A repair torch and a deposition torch are located on different sides of the optical fiber preform, and the repair torch is used to spray combustion gas toward the crack risk area of ​​the optical fiber preform. A particle monitor, wherein the camera of the particle monitor is positioned toward the fracture risk area of ​​the optical fiber preform, and the particle monitor is used to monitor the particle state parameters in the space where the fracture risk area is located when the deposition torch moves to the vicinity of the fracture risk area. and The control unit is connected to the repair torch and the particle monitor signal respectively. The control unit controls the repair torch to spray combustion gas according to the particle state parameters of the space where the rupture risk area is located. The rupture risk area includes the edge area of ​​at least one side of the optical fiber preform along the axial direction.

2. The repair apparatus for OVD deposition according to claim 1, characterized in that, The repair torch is configured to be movable to one side of the area at risk of breakage of the optical fiber preform; or The repair torch is positioned towards the side of the fiber optic preform at risk of breakage.

3. The repair apparatus for OVD deposition according to claim 1, characterized in that, The repair torch is configured to be movable to one side of the standby position of the deposition torch; the camera of the particle monitor is positioned close to the standby position of the deposition torch and is rotatable. When the deposition torch returns to the standby position, the control unit controls the particle monitor to rotate the camera and monitor the particle state parameters in the space where the nozzle of the deposition torch is located, so as to control the repair torch to spray cleaning gas.

4. The repair apparatus for OVD deposition according to claim 1, characterized in that, The standby position of the deposition torch is located on one side of the optical fiber preform along the axial direction, and the breakage risk area is the edge area of ​​the optical fiber preform near the standby position of the deposition torch.

5. The repair apparatus for OVD deposition according to claim 1, characterized in that, The particle monitor includes a camera and an information processing unit that are connected in communication. The camera includes an infrared camera unit and a high-definition camera unit. The infrared camera unit is used to acquire heat distribution images, and the high-definition camera unit is used to acquire particle space images. The information processing unit is used to determine the particle state parameters of the monitored particles based on the heat distribution image and the particle space image. The particle state parameters include particle temperature, particle size and particle motion speed.

6. A control method for a repair apparatus for OVD deposition as described in any one of claims 1-5, characterized in that, include: Turn on the deposition torch. The deposition torch moves along the axis of the optical fiber preform and sprays reactive gas onto the optical fiber preform. The repair torch is in standby mode. When the deposition torch moves to the vicinity of the fracture risk area of ​​the optical fiber preform, the control unit controls the particle monitor to monitor the particle state parameters in the space where the fracture risk area is located. When the particle state parameter meets the first preset condition, the control unit controls the repair torch to spray a first flow rate of combustion gas toward the rupture risk area; The particle state parameters include particle temperature, particle size, and particle velocity. The first preset condition is: the proportion of the number of particles with a temperature greater than a first temperature threshold and a size greater than a first size threshold to the total number of monitored particles is greater than a first proportion threshold, while the proportion of the number of particles with a temperature greater than a first temperature threshold and a velocity greater than a first velocity threshold to the total number of monitored particles is less than a second proportion threshold.

7. The control method for the repair apparatus for OVD deposition according to claim 6, characterized in that, Also includes: After the repair torch sprays out a first flow rate of combustion gas and continues for a first preset time, if the particle state parameters still meet the first preset condition, the control unit controls the repair torch to spray out a second flow rate of combustion gas and continues for a second preset time before returning to standby mode. Wherein, the second flow rate is greater than the first flow rate; and the second preset time is greater than the first preset time.

8. The control method for the repair apparatus for OVD deposition according to claim 6, characterized in that, The repair torch is configured to be movable to one side of the standby position of the deposition torch; the camera of the particle monitor is positioned close to the standby position of the deposition torch and is rotatable. The control method further includes: When the deposition torch returns to the standby position after spraying for a preset time, the control unit controls the rotation of the camera of the particle monitor to monitor the particle state parameters in the space where the nozzle of the deposition torch is located. When the particle state parameter meets the second preset condition, the control unit controls the repair torch to move to one side of the standby position of the deposition torch and sprays a third flow of cleaning gas toward the nozzle of the deposition torch. The second preset condition is that the proportion of particles with a temperature greater than the second temperature threshold and a size greater than the second size threshold to the total number of monitored particles is greater than the third proportion threshold, while the proportion of particles with a temperature greater than the second temperature threshold and a motion rate greater than the second velocity threshold to the total number of monitored particles is less than the fourth proportion threshold.

9. The control method for the repair apparatus for OVD deposition according to claim 8, characterized in that, The second temperature threshold is less than the first temperature threshold, the second size threshold is greater than the first size threshold, the second rate threshold is less than the first rate threshold, the third ratio threshold is greater than the first ratio threshold, and the fourth ratio threshold is less than the second ratio threshold.

10. The control method for the repair apparatus for OVD deposition according to claim 9, characterized in that, Also includes: After the repair blowtorch sprays out a third flow rate of cleaning gas for a third preset time, if the particle state parameters still meet the second preset condition, the control unit controls the repair blowtorch to spray out a fourth flow rate of cleaning gas for a fourth preset time and then returns to the standby state. Wherein, the fourth flow rate is greater than the third flow rate; and the fourth preset time is greater than the third preset time.

Citation Information

Patent Citations

  • Repair device for OVD deposition

    CN223386046U