Protective film structure with composite hardening layer

By incorporating a tiled layer with gaps and a composite hardening layer structure on the flexible screen, the problem of the flexible screen breaking during folding is solved, achieving micro-fracture protection when foreign objects come into contact with it, and maintaining rigidity and display effect.

CN119261311BActive Publication Date: 2026-11-20SUPERC TOUCH CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202410729307.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2023-07-04
Filing Date
2024-06-06
Publication Date
2026-11-20
Estimated Expiration
2044-06-06

AI Technical Summary

Technical Problem

In existing technologies, the protective layer of flexible screens is prone to breakage during folding, which can damage the touch layer and the display screen. Furthermore, traditional plastic materials are prone to collapse or scratches when exposed to foreign objects, affecting the display effect.

Method used

The structure employs a gapped ply layer and a composite hardening layer. By placing a composite hardening layer between adjacent ply layers, sufficient rigidity is provided and it is allowed to stretch under external forces, thus preventing breakage.

Benefits of technology

It effectively protects the flexible screen from shattering during folding and causes only micro-cracks when exposed to foreign objects, maintaining its rigidity and display effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119261311B_ABST
    Figure CN119261311B_ABST
Patent Text Reader

Abstract

A protective film structure with composite hardening layers includes a transparent substrate and at least two tiling layers. The at least two tiling layers include a first tiling layer disposed on a surface of the transparent substrate and including a plurality of first tiling islands with a gap between adjacent first tiling islands, and a second tiling layer disposed on a side of the first tiling layer opposite the transparent substrate and including a plurality of second tiling islands with a gap between adjacent second tiling islands. At least one composite hardening layer is interposed between adjacent tiling layers, each of the composite hardening layers including a first hard film layer and a second hard film layer. The first hard film layer and the second hard film layer are different materials and the first hard film layer has a greater material hardness than the second hard film layer. The composite hardening layers are provided to provide sufficient hardness to the protective film structure and the gaps between the tiling layers provide space for the composite hardening layers to expand when pressed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to a protective membrane structure, and more particularly to a protective membrane structure having a composite hardening layer. Background Technology

[0002] Flexible and foldable screens, due to their lightweight nature and ability to adhere to curved surfaces, are widely used in mobile phones, e-readers, electronic posters, and electronic tags. Traditional screens use protective glass to protect them from external damage, but traditional protective glass is rigid and cannot be bent, making it unsuitable for flexible screen applications. Protecting flexible screens has become a crucial issue. Current technologies can be categorized into two types. One type uses transparent plastic materials (such as transparent PI or PET) coated with a hard coating to replace traditional protective glass. This hard coating is often made of glass-like materials such as silicon dioxide. However, because plastic is soft, it is prone to collapse when exposed to foreign objects. This collapse causes the hard coating to crack, losing its protective effect, resulting in poor performance in practical applications. The second method utilizes the bendable properties of ultra-thin glass to protect the flexible screen, which is currently widely used in foldable phones. However, the production, processing, post-processing, and yield of ultra-thin glass are poor, resulting in significantly increased product costs. Furthermore, ultra-thin glass is easily shattered by impacts, so a layer of plastic material must be attached to its surface for shock absorption, serving as a protective layer. This overlapping process results in insufficient surface hardness, making it susceptible to scratches from foreign objects, affecting the screen's display performance. To address the shortcomings of the aforementioned technologies, this patent applies a hard coating to the surface of the flexible material, which resists crack propagation. This prevents complete shattering when scratched by foreign objects, instead causing only micro-fractures that are kept within an acceptable range. This maintains surface hardness and effectively protects the screen.

[0003] Figure 1 The diagram shows a folding schematic of a prior art electronic product 100' with a foldable display screen, such as a smartphone with a foldable display screen or an e-book with electronic paper. Figure 2 This figure shows a partial structural cross-sectional view of the electronic product 100' with a foldable display screen. As shown, the electronic product 100' has, for example, at least a protective layer 10', a touch layer 20', and a bendable or foldable display screen 30', from top to bottom. The protective layer 10' needs to have a certain degree of hardness to provide scratch resistance, and its transparency is preferably greater than 70%. If the material of the protective layer 10' is too hard or too thick, the protective layer 10' may crack when the display screen 30' is bent or folded. See also... Figure 3A and 3BTo illustrate the problems that occur when this electronic product 100' with a foldable display screen is folded, as shown in these figures, because the protective layer 10' of the existing foldable display screen must have a certain hardness and thickness to resist scratches, the protective layer 10' may crack when folded due to insufficient flexibility. The internal structure of the touch layer 20' under the protective layer 10' will also be affected and crack, and in more serious cases, it may even damage the display screen, causing the electronic product 100' with the foldable display screen to deteriorate or even malfunction. If only the hardness and thickness of the protective layer 10' of the existing foldable display screen are reduced, although flexibility can be improved, the hardness will be insufficient when foreign objects come into contact with it, resulting in cracking and scratches. Summary of the Invention

[0004] The purpose of this invention is to overcome the above-mentioned defects. By providing a plywood layer with gaps and a composite hardening layer between two adjacent plywood layers, the composite hardening layer can provide sufficient rigidity for the protective film structure, and the gaps between the plywood layers can provide space for the composite hardening layer to stretch when pressed.

[0005] To achieve the above objectives, the present invention aims to provide a protective film structure with a composite hardening layer, comprising: a transparent substrate including a first surface and a second surface; at least two planar layers, including: a first planar layer disposed on one side of the first surface of the transparent substrate, comprising a plurality of first planar islands, with a gap between adjacent first planar islands; a second planar layer disposed on the side of the first planar layer opposite to the transparent substrate, comprising a plurality of second planar islands, with a gap between adjacent second planar islands; at least one composite hardening layer disposed between adjacent planar layers; each composite hardening layer comprising a first hard film layer and a second hard film layer, the first hard film layer and the second hard film layer being made of different materials and the material hardness of the first hard film layer being greater than that of the second hard film layer.

[0006] According to one embodiment of the present invention, a second tiling island of the second tiling layer partially overlaps with a first tiling island of the first tiling layer in the projection direction. Furthermore, a second tiling island of the second tiling layer partially overlaps with at least two or three different first tiling islands of the first tiling layer in the projection direction.

[0007] According to one embodiment of the present invention, a third tiling layer is located on the side of the second tiling layer facing away from the first tiling layer. The third tiling layer has a plurality of third tiling islands and there is a gap between each adjacent third tiling island. The area of ​​one of the third tiling islands overlaps with that of one of the second tiling islands of the second tiling layer in the projection direction.

[0008] According to one embodiment of the present invention, the area of ​​each of the first tiling islands and each of the second tiling islands is not less than 250 square micrometers and not more than 50 square millimeters.

[0009] According to one embodiment of the present invention, the composite hardening layer comprises three hard film layers.

[0010] According to one embodiment of the present invention, the protective film structure having a composite hardening layer further includes at least one hard film layer sandwiched between the transparent substrate and the first planar layer.

[0011] According to one embodiment of the present invention, the invention further includes an outer hard film layer, the outer hard film layer having a pencil hardness greater than 6 and being disposed on the side of the ply layer furthest from the transparent substrate, facing away from the substrate. The outer hard film layer is, for example, a silicon nitride hard film with a thickness of less than 1 µm.

[0012] According to one embodiment of the present invention, each of the ply layers is composed of an organic material and has a thickness of not less than 0.5 µm. The organic material is either acrylic or photosensitive polyimide.

[0013] According to one embodiment of the present invention, the transparent substrate is a polymer material substrate or an ultrathin glass substrate with a thickness of no more than 200µm. Attached Figure Description

[0014] Figure 1 This diagram illustrates the folding of a prior art electronic product with a foldable display screen.

[0015] Figure 2 This shows a partial structural cross-sectional view of the electronic product with a foldable display screen.

[0016] Figure 3A and 3B These are schematic diagrams illustrating the problems that occur when this electronic product with a foldable display screen is folded.

[0017] Figure 4 A cross-sectional view illustrating a protective film structure according to an embodiment of the present invention.

[0018] Figure 5 For the corresponding Figure 4 Top view of the illustrated embodiment.

[0019] Figure 6 This is a cross-sectional view of a protective film structure according to another embodiment of the present invention.

[0020] Figure 7 This is a cross-sectional view of a protective film structure according to another embodiment of the present invention.

[0021] In the picture: 100': Electronic products 10: Protective membrane structure 10': Protective layer 20': Touch layer 12, 12': First composite hardening layer 14: Second composite hardening layer 16: Third composite hardening layer 22: First paving layer 22A: First flat island block 24: Second tiling layer 24A: Second flat island block 121, 141, 161: First dura mater layer 122, 142, 162: Second hard film layer 30, 30': Display screen 40: Transparent substrate 41: First Surface 42: Second Surface 50: Outer dura mater. Detailed Implementation

[0022] The present invention will be further described below with reference to the accompanying drawings and specific embodiments, so that those skilled in the art can better understand and implement the present invention. However, the embodiments described are not intended to limit the present invention.

[0023] See Figure 4 This is a cross-sectional view illustrating a protective film structure 10 according to an embodiment of the present invention. This protective film structure 10 includes, for example, from top to bottom, an outer hard film layer 50, a second ply layer 24, a first composite hardening layer 12, a first ply layer 22, a second composite hardening layer 14, and a transparent substrate 40, and is disposed on a display screen 30. The term "from top to bottom" can refer to the conventional direction of operation for electronic products (e.g., smartphones) having this composite hardening layer, i.e., the user's finger is at the top, and the smartphone's display screen 30 is at the bottom. However, the above definition is merely an exemplary directional description used to illustrate the technical features of the present invention and is not intended to limit the scope of the invention.

[0024] like Figure 4As shown, the first tile layer 22 comprises a plurality of first tile islands 22A. According to one embodiment of the present invention, each first tile island 22A may be, for example, a trapezoidal island protrusion with an upper base width smaller than a lower base width. Furthermore, each first tile island 22A has a gap between it to define a first gap between two adjacent first tile islands 22A. Similarly, the second tile layer 24 comprises a plurality of second tile islands 24A. According to one embodiment of the present invention, each tile island 24A may be, for example, a trapezoidal island protrusion with an upper base width smaller than a lower base width. Furthermore, each second tile island 24A has a gap between it to define a second gap between two adjacent second tile islands 24A. The aforementioned first tile islands 22A and second tile islands 24A are made of an organic material with a thickness of not less than 0.5 micrometers (µm), such as an acrylic material or a photosensitive polyimide. Furthermore, the shapes of the first tiling island 22A and the second tiling island 24A of the present invention are not limited to the above-described exemplary shapes. Any shape that can form a gap between adjacent first tiling island 22A and adjacent second tiling island 24A is within the scope of the present invention.

[0025] The first composite hardening layer 12 includes, for example, a first hard film layer 121, a second hard film layer 122, and a first hard film layer 121 from top to bottom; in addition, the second composite hardening layer 14 includes a first hard film layer 141 and a second hard film layer 142 from top to bottom.

[0026] exist Figure 4 In the illustrated embodiment, the first hard film layers 121, 141 may be, for example, silicon nitride (SiNx) with a hardness greater than 6H (i.e., pencil hardness 6H); while the second hard film layers 122, 142 may be, for example, silicon oxide (SiOx) with a hardness greater than 3H (i.e., pencil hardness 3H) or acrylic with a hardness greater than 1H (i.e., pencil hardness 1H). Furthermore, in Figure 4 In the first composite hardening layer 12 and the second composite hardening layer 14 shown, the hardness difference between two adjacent hard film layer materials (i.e., the first hard film layer 121 and the second hard film layer 122, or the first hard film layer 141 and the second hard film layer 142) is preferably not less than the pencil hardness 3H, and the hardness of the first hard film layer 121 (141) is greater than the hardness of the second hard film layer 122 (142).

[0027] In addition, Figure 4In the illustrated embodiment, the transparent substrate 40 has a first surface 41 and a second surface 42, and the transparent substrate 40 is, for example, a polymer material substrate, which can be a PI substrate or a PET substrate. Furthermore, the transparent substrate 40 can also be, for example, an ultrathin glass substrate with a thickness not exceeding 200µm. The outer hard film layer 50 is disposed on the side of the planar layer furthest from the transparent substrate 40, facing away from the transparent substrate 40, i.e., as shown... Figure 4 The second planar layer 24 shown is on the side facing away from the transparent substrate 40. According to one embodiment of the invention, the outer hard film layer 50 is a hard film layer with a hardness greater than 6H, and for example, a silicon nitride hard film layer with a thickness of less than 1µm. See also... Figure 4 At least one composite hardening layer is sandwiched between adjacent ply layers, that is, at least one first composite hardening layer 12 is sandwiched between the first ply layer 22 and the second ply layer 24. Furthermore, according to one embodiment of the present invention, the thickness of the first ply layer 22 may be greater than the thickness of the first composite hardening layer 12, thereby forming a first notch with sufficient depth so that the first composite hardening layer 12 can extend sufficiently within the first notch.

[0028] See Figure 5 , for the corresponding Figure 4 The top view of the illustrated embodiment shows that a second tiling island 24A of the second tiling layer 24 partially overlaps with at least one first tiling island 22A of the first tiling layer 22 in the projection direction; for example, as shown in the figure, a second tiling island 24A of the second tiling layer 24 partially overlaps with four different first tiling islands 22A of the first tiling layer 22 in the projection direction. However, the scope of the invention is not limited to this. Figure 5 In the illustrated embodiment, according to one embodiment of the present invention, one second tiling island 24A of the second tiling layer 24 overlaps with a portion of the area of ​​at least two different first tiling islands 22A of the first tiling layer 22 in the projection direction. According to another embodiment of the present invention, one second tiling island 24A of the second tiling layer 24 overlaps with a portion of the area of ​​at least three different first tiling islands 22A of the first tiling layer 22 in the projection direction. In other words, the effect of this solution can be achieved as long as one second tiling island 24A of the second tiling layer 24 overlaps with a portion of the area of ​​at least one or two different first tiling islands 22A of the first tiling layer 22 in the projection direction. Furthermore, in Figure 5 In this invention, the first tiled island 22A and the second tiled island 24A are rectangular in shape in the projection direction only for illustrative purposes; their shapes are not limited to this. Their shapes in the projection direction can be triangular, circular, or various polygons, etc.

[0029] See compound combination Figure 4 and Figure 5Each of the tiled islands 22A has a gap between each other to define a first gap between two adjacent tiled islands 22A, and each of the tiled islands 24A has a gap between each other to define a second gap between two adjacent tiled islands 24A. Therefore, as Figure 4 As shown, a portion of the structure of the first composite hardened layer 12 extends downward due to the first notch. Furthermore, a second tiling island 24A of the second tiling layer 24 overlaps in the projection direction with a portion of the area of ​​at least one first tiling island 22A of the first tiling layer 22. In addition, the materials of the first tiling island 22A and the second tiling island 24A are softer than those of the first hardened film layer 121 (141) and the second hardened film layer 122 (142). Therefore, when this protective film structure 10 is deformed by external force, such as downward pressure, the first composite hardened layer 12 can extend downward through the first notch, thus avoiding cracking. When the external force presses upward, the first composite hardened layer 12, having a downwardly extending portion, is advantageous for upward extension, thus avoiding cracking.

[0030] See Figure 6 This is a cross-sectional view of a protective film structure 10 according to another embodiment of the present invention. This protective film structure 10 also includes, for example, an outer hard film layer 50, a second ply layer 24, a first composite hardening layer 12', a first ply layer 22, a second composite hardening layer 14, and a transparent substrate 40, from top to bottom. Figure 6 Examples and Figure 4 The embodiment differs in that the first composite hardened layer 12' comprises five hard film layers, namely, from top to bottom: first hard film layer 121, second hard film layer 122, first hard film layer 121, second hard film layer 122, and first hard film layer 121. Providing more hard film layers enhances the structural strength of the protective film structure 10. Similarly, the first tiled islands 22A have a gap between each other to define a first notch between two adjacent first tiled islands 22A; the second tiled islands 24A have a gap between each other to define a second notch between two adjacent second tiled islands 24A. The first tiled islands 22A and the second tiled islands 24A are made of organic materials with a thickness of not less than 0.5 micrometers (µm), such as acrylic materials or photosensitive polyimide. Furthermore, Figure 6 The top view of the embodiment can also be as follows Figure 5 As shown, a second tiling island 24A of the second tiling layer 24 overlaps partially with the area of ​​at least one first tiling island 22A of the first tiling layer 22 in the projection direction; for example, as shown in the figure, a second tiling island 24A of the second tiling layer 24 overlaps partially with the area of ​​four different first tiling islands 22A of the first tiling layer 22 in the projection direction. However, the scope of the present invention is not limited to this. Figure 5In the illustrated embodiment, according to one embodiment of the present invention, one second tiling island 24A of the second tiling layer 24 overlaps with a portion of the area of ​​at least two different first tiling islands 22A of the first tiling layer 22 in the projection direction. According to another embodiment of the present invention, one second tiling island 24A of the second tiling layer 24 overlaps with a portion of the area of ​​at least three different first tiling islands 22A of the first tiling layer 22 in the projection direction. In other words, the effect of this solution can be achieved as long as one second tiling island 24A of the second tiling layer 24 overlaps with a portion of the area of ​​at least one or two different first tiling islands 22A of the first tiling layer 22 in the projection direction. Furthermore, in Figure 5 In this invention, the first tiled island 22A and the second tiled island 24A are rectangular in shape in the projection direction only for illustrative purposes; their shapes are not limited to this. Their shapes in the projection direction can be triangular, circular, or various polygons, etc.

[0031] See compound combination Figure 6 and Figure 5 Each of the tiled islands 22A has a gap between each other to define a first gap between two adjacent tiled islands 22A, and each of the tiled islands 24A has a gap between each other to define a second gap between two adjacent tiled islands 24A. Therefore, as Figure 6 As shown, a portion of the structure of the first composite hardened layer 12' extends downward due to the first notch. Furthermore, a second tiling island 24A of the second tiling layer 24 overlaps in the projection direction with a portion of the area of ​​at least one first tiling island 22A of the first tiling layer 22. In addition, the materials of the first tiling island 22A and the second tiling island 24A are softer than those of the first hardened film layer 121 (141) and the second hardened film layer 122 (142). Therefore, when this protective film structure 10 is deformed by external force, such as downward pressure, the first composite hardened layer 12' can extend downward through the first notch, thus avoiding cracking. When the external force presses upward, the first composite hardened layer 12', having a downwardly extending portion, is advantageous for upward extension, thus avoiding cracking.

[0032] See Figure 7 This is a cross-sectional view of a protective film structure 10 according to another embodiment of the present invention. The protective film structure 10 includes, for example, from top to bottom, an outer hard film layer 50, a third ply layer 26, a third composite hardening layer 16, a second ply layer 24, a first composite hardening layer 12, a first ply layer 22, a second composite hardening layer 14, and a transparent substrate 40.

[0033] The third tile layer 26 comprises a plurality of third tile islands 26A. According to one embodiment of the present invention, each of the third tile islands 26A may be, for example, an island-shaped protrusion with a trapezoidal cross-section, and the width of the upper base is smaller than the width of the lower base. Furthermore, each of the third tile islands 26A has a gap with each other to define a third notch between two adjacent third tile islands 26A. Similarly, the aforementioned third tile islands 26A are made of an organic material with a thickness of not less than 0.5 micrometers (µm), such as an acrylic material or photosensitive polyimide. Furthermore, the shape of the third tile islands 26A of the present invention is not limited to the above-described exemplary shape; any shape that can form a notch between adjacent third tile islands 26A is within the scope of the present invention.

[0034] This third composite hardened layer 16 includes, for example, a first hard film layer 161, a second hard film layer 162, and the first hard film layer 161 from top to bottom. Figure 7 In the illustrated embodiment, the first hard film layer 161 may be, for example, a silicon nitride material (SiNx) with a hardness greater than 6H (i.e., pencil hardness 6H); while the second hard film layer 162 may be, for example, a silicon oxide material (SiOx) with a hardness greater than 3H (i.e., pencil hardness 3H) or an acrylic material with a hardness greater than 1H (i.e., pencil hardness 1H). Furthermore, in Figure 7 In the third composite hardening layer 16 shown, the hardness difference between two adjacent hard film layer materials (i.e., the first hard film layer 161 and the second hard film layer 162) is preferably not less than the pencil hardness 3H, and the hardness of the first hard film layer 161 is greater than the hardness of the second hard film layer 162.

[0035] See compound combination Figure 7 and Figure 5 Each of the first tiling islands 22A has a gap between each other to define a first gap between two adjacent first tiling islands 22A, and each of the second tiling islands 24A is separated from each other to define a second gap between two adjacent second tiling islands 24A. Therefore, as Figure 7 As shown, a portion of the structure of the first composite hardening layer 12 extends downward due to the first notch; a portion of the structure of the third composite hardening layer 16 also extends downward due to the second notch. Furthermore, a second tiling island 24A of the second tiling layer 24 overlaps with a portion of the area of ​​at least one first tiling island 22A of the first tiling layer 22 in the projection direction, and a third tiling island of the third tiling layer 26 overlaps with a portion of the area of ​​at least one second tiling island of the second tiling layer 24 in the projection direction.

[0036] Furthermore, the materials of the first tiled island 22A, the second tiled island 24A, and the third tiled island 26A are softer than those of the first hard film layer 121 (141, 161) and the second hard film layer 122 (142, 162). Therefore, when this protective film structure 10 is deformed by external force, such as downward pressure, the first composite hardening layer 12 and the third composite hardening layer 16 can extend downward through the first notch and the second notch, respectively, thus avoiding cracking. When the external force is applied upward, the first composite hardening layer 12 and the third composite hardening layer 16, having downward extending portions, are conducive to upward extension, thus avoiding cracking. In the above embodiments, the area of ​​each first tiled island 22A and each second tiled island 24A is not less than 250 square micrometers and not greater than 50 square millimeters.

[0037] The above-described embodiments are merely preferred embodiments provided to fully illustrate the present invention, and the scope of protection of the present invention is not limited thereto. Equivalent substitutions or modifications made by those skilled in the art based on the present invention are all within the scope of protection of the present invention. The scope of protection of the present invention is defined by the claims.

Claims

1. A protective film structure with a composite hardening layer, characterized in that, Include: A transparent substrate comprising a first surface and a second surface; At least two tiling layers, including: A first tile layer is disposed on one side of the first surface of the transparent substrate, and includes a plurality of first tile islands, with a gap between each adjacent first tile island; A second tile layer is disposed on the side of the first tile layer opposite to the transparent substrate, and includes a plurality of second tile islands, with a gap between each adjacent second tile island; At least one composite hardening layer is disposed between each of the adjacent ply layers; Each of the composite hardening layers includes a first hard film layer and a second hard film layer, wherein the first hard film layer and the second hard film layer are made of different materials and the material hardness of the first hard film layer is greater than that of the second hard film layer. The second tiling layer's second tiling island partially overlaps with the area of ​​the first tiling island in the first tiling layer in the projection direction.

2. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, One of the second tiling islands of the second tiling layer overlaps with a portion of the area of ​​at least two different first tiling islands of the first tiling layer in the projection direction.

3. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, One of the second tiling islands of the second tiling layer overlaps with a portion of the area of ​​at least three different first tiling islands of the first tiling layer in the projection direction.

4. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, It further includes a third tiling layer located on the side of the second tiling layer facing away from the first tiling layer. The third tiling layer has a plurality of third tiling islands and there is a gap between each adjacent third tiling island. The area of ​​one of the third tiling islands overlaps with that of a portion of the second tiling island in the projection direction.

5. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, The area of ​​each of the first and second tiling islands is not less than 250 square micrometers.

6. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, The area of ​​each of the first and second tiling islands is no greater than 50 square millimeters.

7. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, The composite hardening layer consists of three hard film layers.

8. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, It further includes at least one hard film layer sandwiched between the transparent substrate and the first planar layer.

9. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, It further includes an outer hard film layer, the outer hard film layer having a pencil hardness greater than 6 and being disposed on the side of the ply layer furthest from the transparent substrate, facing away from the substrate.

10. The protective film structure with a composite hardening layer as described in claim 9, characterized in that, The outer hard film layer is a silicon nitride hard film with a thickness of less than 1µm.

11. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, Each of the aforementioned ply layers is composed of organic materials and has a thickness of not less than 0.5µm.

12. The protective film structure with a composite hardening layer as described in claim 11, characterized in that, The organic material is either acrylic or photosensitive polyimide.

13. The protective film structure with a composite hardening layer as described in claim 1, characterized in that, The transparent substrate is a polymer material substrate or an ultra-thin glass substrate with a thickness of no more than 200µm.

Citation Information

Patent Citations

  • Protective film

    CN107263946A