Method for reducing residual alkali of layered oxide positive electrode material

CN119400815APending Publication Date: 2025-02-07ANHUI XINNA MATERIAL SCIENCE & TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411399239.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-08
Publication Date
2025-02-07

Smart Images

  • Figure CN119400815A_ABST
    Figure CN119400815A_ABST
Patent Text Reader

Abstract

The invention discloses a method for reducing residual alkali of a layered oxide positive electrode material, and belongs to the field of energy materials and energy storage. In the sintering process, conventional constant-temperature solid-phase sintering is broken, sintering tail end variable-temperature sintering is adopted, a rapid heating section is introduced, residual alkali on the surface of the layered oxide material is volatilized, the crystallinity of the material is further improved, and therefore the electrochemical performance and structural stability of the positive electrode material are improved. The 0.1 C first-circle discharge capacity is increased from 134 mAh / g to 137 mAh / g, the 1C discharge capacity is increased from 119 mAh / g to 125 mAh / g, and the 50-cycle cycle retention rate is increased from 75% to 90%).