A friction-reducing coating with a lateral gradient and a method for producing the same

CN119465143BActive Publication Date: 2026-03-03SHANDONG UNIV
2 Cites 0 Cited by

Patent Information

Application Number
CN202411522326.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-10-29
Publication Date
2026-03-03
Estimated Expiration
2044-10-29

Smart Images

  • Figure CN119465143B_ABST
    Figure CN119465143B_ABST
Patent Text Reader

Abstract

This invention discloses a friction-reducing coating with a transverse gradient and its preparation method, belonging to the field of friction-reducing coating technology. The coating comprises a self-lubricating material powder and a metal powder bonded together; the ratio of the self-lubricating material powder to the metal powder varies gradient along a direction parallel to the friction surface; the self-lubricating material powder is selected from one or more of MoS2 and WS2; the metal powder is selected from one of Ti, Co, or Ni; the mass ratio of the self-lubricating material powder to the metal powder is (5-10):(0-5). Because the material properties gradually change along the direction of friction, the stress is more evenly distributed on the coating surface, no longer limited to the interface in the vertical direction, effectively reducing local stress concentration.
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Two-dimension gradient structure transition layer

    CN109825796A

  • Preparation process of chessboard alternate type soft and hard composite coating

    CN116856024A