Welding method for a gas seal body
By employing circular component welding and positioning support technology, the problem of accumulated welding deformation in the gas seal body was solved, achieving a high-precision and efficient welding method and simplifying the processing.
Patent Information
- Application Number
- CN202411528282.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-30
- Publication Date
- 2026-11-20
- Estimated Expiration
- 2044-10-30
AI Technical Summary
Existing welding methods for gas seals result in cumulative welding deformation, leading to low overall precision after assembly. Furthermore, a large machining allowance must be reserved during welding, which affects processing efficiency.
The process involves welding circular parts, using positioning shafts and positioning sleeves to support and position the inner hole and outer sleeve, and controlling welding deformation through tooling equipment. The parts are first cut along the split surface and supplementary materials are welded on. During welding, the split surfaces are kept aligned, and the weld is kept warm and ground after welding to reduce deformation errors.
It improves the overall precision after welding, reduces machining, reduces welding deformation, simplifies the structure, and improves assembly precision and processing efficiency.
Smart Images

Figure CN119501478B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of welding technology, and in particular to a welding method for a gas seal. Background Technology
[0002] A steam seal is a device installed between the turbine shaft and the casing to prevent the leakage of high-pressure steam inside the turbine. Generally, both ends of the shaft need to be sealed by a steam seal. For example, a certain steam seal... Figure 1 As shown, the assembly includes a flange 1, an outer sleeve 2, a first ring plate 3, a second ring plate 4, a third ring plate 5, a first ring sleeve 6, a second ring sleeve 7, a third ring sleeve 8, a connecting ring plate 9, an inner sleeve 10, and a cover 11. The flange 1 is located on the outer wall of the outer sleeve 2. The first ring plate 3, the second ring plate 4, and the third ring plate 5 are located on the inner wall of the outer sleeve 2. The first ring sleeve 6, the second ring sleeve 7, and the third ring sleeve 8 are fixedly connected to the inner sides of the first ring plate 3, the second ring plate 4, and the third ring plate 5, respectively. The connecting ring plate 9 fixes the first ring sleeve 6 and the inner sleeve 10 together. The cover 11 is a 1 / 2 frustum-shaped cover, with its small end fixedly connected to the third ring sleeve 8 and its large end connected to a fourth ring sleeve 12. During manufacturing, all connections between components are welded. To facilitate assembly, the entire steam seal body is divided into two equal parts along the split surface, with the cover 11 positioned on one part of the third ring sleeve 8. Currently, the two parts are machined and welded separately. The deformation generated during welding accumulates, resulting in low overall precision after assembly. A large machining allowance needs to be reserved during welding, which is not conducive to improving processing efficiency. Summary of the Invention
[0003] The technical problem to be solved by the present invention is to provide a welding method for gas seals to improve the overall accuracy after welding.
[0004] To solve the above problems, the technical solution adopted by the present invention is: a gas seal welding method, comprising the following steps:
[0005] S1. Prepare the first ring plate, the second ring plate, the third ring plate, the first ring sleeve, the second ring sleeve, and the third ring sleeve of the annulus;
[0006] Prepare a semi-circular flange, outer sleeve, connecting ring plate, inner sleeve, fourth ring sleeve, and enclosure;
[0007] S2. Weld the first ring plate to the outer wall of the first ring sleeve to obtain the first component; weld the second ring plate to the outer wall of the second ring sleeve to obtain the second component; weld the third ring plate to the outer wall of the third ring sleeve to obtain the third component;
[0008] S3. Cut the first component, the second component, and the third component along the midline.
[0009] S4. First, weld the first component into the outer sleeve, then weld the second and third components into the outer sleeve. During welding, use tooling for positioning, and ensure that the mid-section of the first, second, and third components coincides with the mid-section of the outer sleeve.
[0010] S5. Weld the connecting ring plate into the first ring sleeve, and weld the inner sleeve into the connecting ring plate. The mid-sections of the connecting ring plate, the outer sleeve, and the inner sleeve coincide.
[0011] S6. Weld the flange to the outer wall of the outer sleeve, with the center surfaces of the flange and the outer sleeve coinciding;
[0012] S7. Weld the fourth ring to the large end of the enclosure, and weld the small end of the enclosure to the third ring.
[0013] S8, Tempering.
[0014] Further, step S4 includes:
[0015] S41. Preparation fixture: The fixture includes a horizontal base and a frame set above the base. A vertical positioning shaft is set on the base. The positioning shaft is a hollow shaft and a first heating mechanism is set inside the positioning shaft. A detachable positioning boss is set on the outer wall of the positioning shaft. A positioning sleeve is set on the second frame. The positioning sleeve is coaxial with the positioning shaft. A second heating mechanism is set on the outer wall of the positioning sleeve. The positioning sleeve is connected to a first driving mechanism that drives the positioning sleeve to move axially.
[0016] S42. A first pad is placed on the base, and the second component is placed on the base. The second ring plate of the second component is attached to the first pad, and the second ring is sleeved on the positioning shaft and attached to the positioning boss. Then, the outer sleeve is placed on the base and sleeved over the second ring plate. The positioning shaft is heated to an outer wall temperature of 100°C to 150°C using the first heating mechanism, and the positioning sleeve is heated to 100°C to 150°C using the second heating mechanism. Then, the positioning sleeve is pushed downward by the first driving mechanism and sleeved over the outer sleeve. The second heating mechanism stops heating, and the first heating mechanism continues heating to weld the second ring plate to the outer sleeve.
[0017] S43. A second pad is provided on the upper surface of the second ring plate, and a third pad is provided on the upper surface of the second ring sleeve. The first component is pressed between the positioning shaft and the outer sleeve. The first ring plate of the first component is in contact with the second pad, and the first ring sleeve is in contact with the third pad. Then the first ring plate is welded to the outer sleeve to obtain the fourth component.
[0018] S44. Remove the fourth component, remove the first, second and third pads, flip the fourth component over and place it on the base, then set the fourth pad on the upper surface of the second ring plate and the fifth pad on the upper surface of the second ring sleeve, press the third component between the positioning shaft and the outer sleeve, the third ring plate of the third component is in contact with the fourth pad, the third ring sleeve is in contact with the fifth pad, and then weld the third ring plate to the outer sleeve.
[0019] Furthermore, in step S3, wire cutting is used to cut the first component, the second component, and the third component along the mid-section.
[0020] Further, after step S3, the dimensions of the cut first component, second component and third component are detected. When the dimensions of the split surfaces of the first component, second component and third component are less than the set dimensions, welding is performed on the split surfaces of the first component, second component and third component.
[0021] Furthermore, the weld between the first ring plate and the first ring sleeve is a double-sided butt weld, and the weld between the first ring plate and the outer sleeve is an outer side butt weld; the weld between the second ring plate and the first ring sleeve is a double-sided butt weld, and the weld between the second ring plate and the outer sleeve is a double-sided butt weld; the weld between the third ring plate and the third ring sleeve is a double-sided butt weld, and the weld between the third ring plate and the outer sleeve is an outer side butt weld; the weld between the connecting ring plate and the first ring sleeve is a double-sided butt weld, and the weld between the connecting ring plate and the inner sleeve is a double-sided butt weld; the weld between the flange and the outer sleeve is a double-sided butt weld; the weld between the fourth ring sleeve and the enclosure is an inner side butt weld, and the weld between the enclosure and the third ring sleeve is an inner side butt weld.
[0022] Furthermore, in steps S4 to S7, after welding, there is an anti-sticking section between the weld and the split surface. After step S7, the steam seal body is divided into two parts along the split surface, and then the anti-sticking section is welded again.
[0023] Further, in step S7, half of the steam seal body is placed on a horizontal support base. The support base is equipped with a slide and a vertical center-side limiting plate. The slide is slidably engaged with the support base and is connected to a second driving mechanism that drives the slide to move toward the center-side limiting plate. An inverted L-shaped pressure plate is provided on the slide, and a support cover is provided on the upper surface of the pressure plate. The center-side of the steam seal body is attached to the center-side limiting plate, and the pressure plate is attached to the outer wall and top wall of the steam seal body. Then, the enclosure and the fourth ring are placed on the support cover. Both the enclosure and the fourth ring are attached to the support cover, and the center-side of the enclosure and the fourth ring are attached to the center-side limiting plate. Then, welding is performed.
[0024] Furthermore, in step S7, after welding, the weld is kept at a temperature of 200 to 250°C for 3 to 4 hours and then ground.
[0025] Furthermore, the support base is installed on a pair of horizontal rails, and the support base is connected to a third drive mechanism that drives the support base to move along the rails. After welding, the third drive mechanism drives the support base to move to the grinding and heat preservation station.
[0026] The grinding and insulation station is equipped with a lifting frame, on which a vertical rotating shaft is mounted. The rotating shaft is connected to a fourth driving mechanism that drives the rotating shaft to rotate. At least three positioning rods perpendicular to the rotating shaft are fixedly mounted on the rotating shaft. Each positioning rod has a cantilever that slides with the positioning rod. Locking nuts with threaded engagement with the positioning rods are provided on both sides of the cantilever. A detachable grinding ring is provided at the end of the cantilever. The grinding ring has a grinding surface and a third heating mechanism is provided inside the grinding ring.
[0027] The beneficial effects of the present invention are as follows: The first ring plate, the second ring plate, the third ring plate, the first ring sleeve, the second ring sleeve and the third ring sleeve of the present invention are made of complete circular ring parts, which have higher integrity and smaller deformation during welding, which helps to reduce the amount of machining. In addition, the first component, the second component and the third component obtained by welding are relatively thin, the structure is relatively simple, and the cutting and processing after welding is more convenient.
[0028] When the first, second, and third components are welded to the outer sleeve, a positioning shaft is used to support the inner hole, a positioning sleeve is used to tighten the outer sleeve, and a pad is used for axial positioning. This ensures tight assembly between the components, reduces welding deformation, and the semi-circular parts are spliced into complete circular rings. The two semi-circular parts are welded simultaneously, resulting in high overall consistency. This further reduces dimensional errors caused by welding deformation and improves subsequent assembly accuracy. Attached Figure Description
[0029] Figure 1 This is a cross-sectional view of the steam seal body of the present invention when the cross-section is perpendicular to the split plane;
[0030] Figure 2 This is a schematic diagram of the welding process for the second component;
[0031] Figure 3 This is a schematic diagram of the welding process for the first component;
[0032] Figure 4 This is a schematic diagram of the welding process for the third component;
[0033] Figure 5 This is a schematic diagram of each weld seam;
[0034] Figure 6 This is a schematic diagram of step S7;
[0035] Figure 7 This is a schematic diagram of weld grinding in step S7;
[0036] Figure 8 yes Figure 7 An enlarged schematic diagram of part A in the middle;
[0037] Reference numerals: 1—Flange; 2—Outer sleeve; 3—First ring plate; 4—Second ring plate; 5—Third ring plate; 6—First ring sleeve; 7—Second ring sleeve; 8—Third ring sleeve; 9—Connecting ring plate; 10—Inner sleeve; 11—Enclosure; 12—Fourth ring sleeve; 20—Positioning shaft; 21—First heating mechanism; 22—Positioning boss; 23—Base; 24—Base; 25—Positioning sleeve; 26—Second heating mechanism; 27—First drive mechanism; 28—First pad; 210 —Second pad; 211—Third pad; 214—Fourth pad; 215—Fifth pad; 30—Support seat; 31—Slide seat; 32—Center split-face limiting plate; 33—Second drive mechanism; 34—Pressure plate; 35—Support cover; 36—Rail; 37—Third drive mechanism; 38—Lifting frame; 39—Rotating shaft; 310—Fourth drive mechanism; 311—Positioning rod; 312—Cantilever; 313—Locking nut; 314—Grinding ring; 315—Third heating mechanism. Detailed Implementation
[0038] The present invention will be further described below with reference to the accompanying drawings and embodiments.
[0039] The vapor seal welding method of the present invention includes the following steps:
[0040] S1. Prepare the first ring plate 3, the second ring plate 4, the third ring plate 5, the first ring sleeve 6, the second ring sleeve 7, and the third ring sleeve 8 of the annulus.
[0041] Prepare a semi-circular flange 1, an outer sleeve 2, a connecting ring plate 9, an inner sleeve 10, a fourth ring sleeve 12, and a cover 11.
[0042] The first ring plate 3, the second ring plate 4, the third ring plate 5, the first ring sleeve 6, the second ring sleeve 7, and the third ring sleeve 8 can be cut from sheet metal. After cutting, the inner and outer circles are machined to remove burrs, and welding bevels are also processed.
[0043] Flange 1, outer sleeve 2, connecting ring plate 9, and fourth ring sleeve 12 can be cut from sheet metal, then rough-machined and have their welding bevels machined. Inner sleeve 10 and enclosure 11 are first cut from sheet metal, then rolled into the required shape, and then rough-machined and have their welding bevels machined.
[0044] S2. Weld the first ring plate 3 to the outer wall of the first ring sleeve 6 to obtain the first component; weld the second ring plate 4 to the outer wall of the second ring sleeve 7 to obtain the second component; weld the third ring plate 5 to the outer wall of the third ring sleeve 8 to obtain the third component.
[0045] The first ring plate 3, the second ring plate 4, the third ring plate 5, the first ring sleeve 6, the second ring sleeve 7, and the third ring sleeve 8 form a complete ring. During welding, the overall integrity is higher and the deformation of the parts is smaller. Moreover, the thickness of the first, second, and third components obtained after welding is small, which can be easily divided into two parts.
[0046] S3. Cut the first component, the second component, and the third component along the midline.
[0047] After welding, the first, second, and third components can be tempered separately to remove welding stress. Then, they can be cut along the split plane, which is the plane that passes through the center of the first, second, and third components and extends radially, dividing the first, second, and third components into two equal parts, each part being a semi-circular ring.
[0048] The cutting can be done by flame cutting, water jet cutting, etc. To improve the accuracy of the cut surface, wire EDM is preferred to cut the first, second, and third components along the mid-section. Wire EDM has high precision and produces a smooth cut surface.
[0049] After cutting, a kerf is inevitably created. During subsequent welding, the mid-sections of the first, second, and third components will be difficult to fit tightly together. Therefore, it is necessary to check the dimensions of the first, second, and third components after cutting. If the dimensions of the mid-sections of the first, second, and third components are smaller than the set dimensions, then weld overlay is performed on the mid-sections of the first, second, and third components, and the surface of the weld overlay is ground smooth. The material used for weld overlay is the same as that used for the first, second, and third components. By overlaying a certain thickness of metal material, the material removed during cutting can be supplemented, ensuring that the dimensions of the first, second, and third components meet the requirements, and that the mid-sections of the first, second, and third components can fit tightly together during subsequent welding.
[0050] S4. First, weld the first component into the outer sleeve 2, then weld the second and third components into the outer sleeve 2. During welding, use tooling for positioning, and ensure that the mid-section of the first, second, and third components coincides with the mid-section of the outer sleeve 2.
[0051] from Figure 1 As can be seen, the gap between the first ring sleeve 6, the second ring sleeve 7 and the third ring sleeve 8 is small, making it difficult to reach into the gap between the first ring plate 3, the second ring plate 4 and the third ring plate 5 before welding. Therefore, the second ring plate 4 located in the middle is welded first, and then the first ring plate 3 and the third ring plate 5 located at both ends are welded to ensure that the welding gun has sufficient operating space.
[0052] To reduce welding deformation and improve dimensional accuracy, the specific welding process includes:
[0053] S41. Preparation fixture: The fixture includes a horizontal base 23 and a frame 24 disposed above the base 23. A vertical positioning shaft 20 is disposed on the base 23. The positioning shaft 20 is a hollow shaft and a first heating mechanism 21 is disposed inside the positioning shaft 20. A detachable positioning boss 22 is disposed on the outer wall of the positioning shaft 20. A positioning sleeve 25 is disposed on the second frame 24. The positioning sleeve 25 is coaxial with the positioning shaft 20. A second heating mechanism 26 is disposed on the outer wall of the positioning sleeve 25. The positioning sleeve 25 is connected to a first driving mechanism 27 that drives the positioning sleeve 25 to move axially.
[0054] The base 23 can be fixed to the ground. After the base 23 is installed, the levelness of the upper surface of the base 23 is checked to ensure that the upper surface of the base 23 is in a horizontal state. The outer diameter of the positioning shaft 20 is adapted to the inner diameter of the first ring sleeve 6, the second ring sleeve 7, and the third ring sleeve 8, ensuring that the inner walls of the first ring sleeve 6, the second ring sleeve 7, and the third ring sleeve 8 can fit tightly against the outer wall of the positioning shaft 20. The first heating mechanism 21 is used to heat the positioning shaft 20. According to the principle of thermal expansion and contraction, the outer diameter of the positioning shaft 20 increases after heating, which can more tightly support the first ring sleeve 6, the second ring sleeve 7, and the third ring sleeve 8. The positioning boss 22 is annular and can be sleeved on the positioning shaft 20 and slide in cooperation with the positioning shaft 20, which can facilitate the installation and removal of the positioning boss 22. The inner diameter of the positioning sleeve 25 is adapted to the outer diameter of the outer sleeve 2, ensuring that the inner wall of the positioning sleeve 25 can fit tightly against the outer wall of the outer sleeve 2. The second heating mechanism 26 is used to heat the positioning sleeve 25. The positioning sleeve 25 expands when heated, increasing its inner diameter to facilitate its placement on the outer sleeve 2. After placement, the second heating mechanism 26 stops heating, and the positioning sleeve 25 gradually cools and contracts, decreasing its inner diameter, thereby clamping the outer sleeve 2 tightly and stably positioning it. This ensures that the two semi-circular outer sleeves 2 form a complete annular outer sleeve 2, while also reducing deformation during welding. The first heating mechanism 21 and the second heating mechanism 26 can be heating wires. To reduce heat loss, a heat-insulating layer covering the second heating mechanism 26 can be provided on the outer wall of the positioning sleeve 25. The first drive mechanism 27 can be a hydraulic cylinder or similar device.
[0055] S42. A first pad 28 is provided on the base 23 to support the second ring plate 4. The second component is placed on the base 23, with the second ring plate 4 of the second component fitting against the first pad 28. The second ring sleeve 7 is fitted onto the positioning shaft 20 and fits against the positioning boss 22. Then, the outer sleeve 2 is placed on the base 23, fitting over the second ring plate 4. Both the second component and the outer sleeve 2 are semi-circular rings, and there are two of them. After assembly, their mid-faces fit together to form a circular second component and outer sleeve 2, with the mid-face of the second component and the mid-face of the outer sleeve 2 on the same plane. The positioning boss 22 and the first pad 28 ensure that the second ring sleeve 7 and the second ring plate 4 are in a set axial position.
[0056] The positioning sleeve 25 is heated to 100°C to 150°C using the second heating mechanism 26. Then, the positioning sleeve 25 is pushed downwards and fitted onto the outer sleeve 2 using the first driving mechanism 27. The positioning sleeve 25 expands upon heating, increasing its inner diameter, allowing it to be easily fitted onto the outer sleeve 2. Next, the positioning shaft 20 is heated to an outer wall temperature of 100°C to 150°C using the first heating mechanism 21. The positioning shaft 20 expands upon heating, increasing its outer diameter, thereby tightening the second ring sleeve 7. When the first heating mechanism 21 is running, the second heating mechanism 26 stops heating, and the positioning sleeve 25 gradually cools, tightly holding the outer sleeve 2. To improve the stability of the second ring sleeve 7 and the second ring plate 4, a pressing mechanism can be provided on the upper surface of the second ring plate 4 or the second ring sleeve 7 to press the second ring plate 4 or the second ring sleeve 7 downwards.
[0057] After the second component and the outer sleeve 2 are stably assembled, the second ring plate 4 can be welded to the outer sleeve 2. During welding, the first heating mechanism 21 continuously heats the surface.
[0058] This invention utilizes the positioning shaft 20 to tighten the inner hole of the second ring sleeve 7 and the positioning sleeve 25 to hold the outer sleeve 2, ensuring stable assembly and tight fit of the semi-circular parts, while limiting the deformation of the parts during welding. Furthermore, assembling the semi-circular parts into a complete ring part before welding eliminates the need for separate welding, avoiding the accumulation of welding deformation errors and improving the dimensional accuracy after welding.
[0059] S43. A second pad 210 is provided on the upper surface of the second ring plate 4, and a third pad 211 is provided on the upper surface of the second ring sleeve 7. The first component is pressed between the positioning shaft 20 and the outer sleeve 2. The first ring plate 3 of the first component is attached to the second pad 210, and the first ring sleeve 6 is attached to the third pad 211. Then the first ring plate 3 is welded to the outer sleeve 2 to obtain the fourth component.
[0060] The second pad 210 and the third pad 211 are used to determine the axial position of the first component and ensure that the spacing between the first component and the second component meets the requirements. A pressing mechanism can also be provided on the upper surface of the first ring plate 3 or the first ring sleeve 6 to press the first ring plate 3 or the first ring sleeve 6 downward, thereby improving the stability of the first ring plate 3 and the first ring sleeve 6 and preventing deformation.
[0061] To facilitate the removal of the second pad 210, the second pad 210 can be multiple sector-shaped metal blocks.
[0062] S44. After the first component is welded, the fourth component is removed. Specifically, the positioning sleeve 25 is heated to 100°C to 150°C using the second heating mechanism 26, and then the positioning sleeve 25 is moved upward above the fourth component using the first drive mechanism 27. Then the fourth component is removed from the positioning shaft 20.
[0063] Remove the first pad 28, the second pad 210, the third pad 211, and the positioning boss 22. Flip the fourth component over and place it on the base 23, ensuring the inner wall of the fourth component fits against the outer wall of the positioning shaft 20. Then, use the first drive mechanism 27 to move the positioning sleeve 25 downwards, so that the positioning sleeve 25 is once again fitted onto the outer sleeve 2. Next, place the fourth pad 214 on the upper surface of the second ring plate 4 and the fifth pad 215 on the upper surface of the second ring sleeve 7. Press the third component between the positioning shaft 20 and the outer sleeve 2. The third ring plate 5 of the third component fits against the fourth pad 214, and the third ring sleeve 8 fits against the fifth pad 215. Then, weld the third ring plate 5 to the outer sleeve 2. After welding, use the first drive mechanism 27 to move the positioning sleeve 25 upwards to remove the steam seal.
[0064] S5. Weld the connecting ring plate 9 into the first ring sleeve 6, and weld the inner sleeve 10 onto the connecting ring plate 9. The mid-sections of the connecting ring plate 9, the outer sleeve 2, and the inner sleeve 10 coincide.
[0065] During welding, the components of the steam seal can be assembled on a horizontal platform first, and then welded.
[0066] S6. Weld flange 1 to the outer wall of outer sleeve 2, so that the mid-sections of flange 1 and outer sleeve 2 coincide.
[0067] S7. Weld the fourth ring 12 to the large end of the cover 11, and weld the small end of the cover 11 to the third ring 8.
[0068] Specifically, half of the steam seal body is placed on a horizontal support 30. The support 30 is equipped with a slide 31 and a vertical center-side limiting plate 32. The slide 31 slides in conjunction with the support 30, and the slide 31 is connected to a second drive mechanism 33 that drives the slide 31 to move toward the center-side limiting plate 32. The second drive mechanism 33 can be a hydraulic cylinder or other equipment. An inverted L-shaped pressure plate 34 is provided on the slide 31, and a support cover 35 is provided on the upper surface of the pressure plate 34. The center-side of the steam seal body is attached to the center-side limiting plate 32, and the pressure plate 34 is attached to the outer wall and top wall of the steam seal body. Then, the enclosure 11 and the fourth ring 12 are placed on the support cover 35. The enclosure 11 and the fourth ring 12 are both attached to the support cover 35, and the center-side of the enclosure 11 and the fourth ring 12 is attached to the center-side limiting plate 32. Then, welding is performed.
[0069] A semi-circular steam seal body is placed between the pressure plate 34 and the center-parting limiting plate 32, with the center-parting surface of the steam seal body adhering to the center-parting limiting plate 32. Then, the second drive mechanism 33 pushes the pressure plate 34 towards the center-parting limiting plate 32, causing the pressure plate 34 to press the steam seal body tightly. The pressure plate 34 includes an arc-shaped vertical plate and a horizontal top plate. The vertical plate can press against the outer wall of the steam seal body, while the top plate can adhere to the top wall of the steam seal body, thus ensuring the stability of the steam seal body. The shape and size of the support cover 35 are adapted to the shape and size of the enclosure 11 and the fourth ring 12. It includes a frustum-shaped first support body, a horizontal support body, and a circular clamp. The support cover 35 can stably support the enclosure 11 and the fourth ring 12. To improve the stability of the enclosure 11 and the fourth ring 12, a clamping mechanism can be used to press the enclosure 11 and the fourth ring 12 tightly.
[0070] Because the enclosure 11 is an arc-shaped structure, it is more prone to deformation during welding, resulting in higher welding stress. Therefore, after welding, the weld is kept at a temperature of 200 to 250°C for 3 to 4 hours and then ground. By keeping the weld warm, welding stress can be reduced, preventing defects such as cracks from appearing inside the weld.
[0071] The support base 30 is mounted on a pair of horizontal rails 36, and the support base 30 is connected to a third drive mechanism 37 that drives the support base 30 to move along the rails 36. After welding, the third drive mechanism 37 drives the support base 30 to move to the grinding and heat preservation station.
[0072] Since the enclosure 11 is only connected to the third ring 8 via a weld, the weight of the enclosure 11 and the fourth ring 12 needs to be supported by the weld. Furthermore, because there is a horizontal distance between the center of the enclosure 11 and the weld, the weight of the enclosure 11 will generate torque on the weld. If the pressure plate 34 and the support cover 35 are removed immediately after welding, the weld is not yet stable, and the weight of the enclosure 11 and the fourth ring 12 can easily cause significant stress in the weld between the enclosure 11 and the third ring 8, leading to defects such as cracks inside the weld. To solve this problem, during welding, the third drive mechanism 37 moves the support seat 30 to the welding station. After welding, the third drive mechanism 37 moves the support seat 30 and the steam seal body to the grinding and insulation station. During the grinding and insulation process, the pressure plate 34 and the support cover 35 maintain support and positioning for the steam seal body. The weight of the enclosure 11 and the fourth ring 12 is borne by the support cover 35 and is not transmitted to the weld between the enclosure 11 and the third ring 8, which helps to ensure weld quality. The third drive mechanism 37 can be a conventional drive mechanism such as a screw and nut mechanism driven by a motor.
[0073] Currently, grinding is typically performed after the weld is insulated, which is time-consuming and affects production efficiency. To improve efficiency, this invention directly transports the support base 30 along with the steam seal body to the grinding and insulation station after welding, facilitating the transfer of the steam seal body and eliminating the need for secondary positioning.
[0074] The grinding and heat preservation station is equipped with a lifting frame 38, which is connected to a hydraulic cylinder and other lifting mechanisms. A vertical rotating shaft 39 is mounted on the lifting frame 38, and a fourth drive mechanism 310, which drives the rotating shaft 39, is connected to it. The fourth drive mechanism 310 can be a servo motor. At least three positioning rods 311, perpendicular to the rotating shaft 39, are fixedly mounted on the rotating shaft 39. Cantilever arms 312, which slide and engage with the positioning rods 311, are mounted on the positioning rods 311. Locking nuts 313, threaded into the positioning rods 311, are mounted on both sides of the cantilever arms 312. A detachable grinding ring 314 is mounted at the end of the cantilever arm 312. The grinding ring 314 has a grinding surface with a wear-resistant layer, which can be made of existing wear-resistant materials. A third heating mechanism 315, which can be an electric heating wire, is installed inside the grinding ring 314.
[0075] During grinding, the lifting frame 38 moves downward, causing the grinding ring 314 to move downward, so that the grinding surface of the grinding ring 314 contacts the weld. Then, the fourth drive mechanism 310 drives the rotating shaft 39 to rotate at high speed. The rotating shaft 39 drives the grinding ring 314 to rotate at high speed through the positioning rod 311 and the cantilever 312, thus grinding the weld. During grinding, the third heating mechanism 315 heats the grinding ring 314 to 200 to 250°C, so that the weld is always kept at a temperature of 200 to 250°C. After grinding, the third heating mechanism 315 continues to heat and keep the weld warm. When the weld has been kept warm for the required time, the lifting frame 38 moves upward, and the grinding ring 314 disengages from the weld. After the weld cools to room temperature, the third drive mechanism 37 drives the pressure plate 34 and the support cover 35 to move away from the steam seal body, releasing the support for the enclosure 11 and the fourth ring 12.
[0076] In this invention, the weld is ground simultaneously with heat preservation, which saves grinding time and improves efficiency compared to the traditional method of performing heat preservation and grinding separately. Furthermore, the weld temperature during grinding is between 200 and 250°C, which is relatively high, and the material is softer, making it easier to grind smooth.
[0077] In the grinding and heat preservation device of the present invention, the cantilever 312 is vertically arranged, and the grinding ring 314 can be connected to the cantilever 312 by screws. The grinding ring 314 with a corresponding grinding surface can be replaced according to the shape and size of the weld. The grinding ring 314 with different inner and outer diameters can also be replaced according to the inner and outer diameters of the annular weld. When replacing, rotate the locking nut 313, slide the cantilever 312, adjust the distance between the cantilever 312 and the rotating shaft 39, and then lock the cantilever 312 with the locking nut 313.
[0078] S8. Tempering: Remove welding stress. A conventional tempering process can be used.
[0079] In this invention, such as Figure 5 As shown, the weld between the first ring plate 3 and the first ring sleeve 6 is a double-sided butt weld, and the weld between the first ring plate 3 and the outer sleeve 2 is an outer side butt weld; the weld between the second ring plate 4 and the first ring sleeve 6 is a double-sided butt weld, and the weld between the second ring plate 4 and the outer sleeve 2 is a double-sided butt weld; the weld between the third ring plate 5 and the third ring sleeve 8 is a double-sided butt weld, and the weld between the third ring plate 5 and the outer sleeve 2 is an outer side butt weld; the weld between the connecting ring plate 9 and the first ring sleeve 6 is a double-sided butt weld, and the weld between the connecting ring plate 9 and the inner sleeve 10 is a double-sided butt weld; the weld between the flange 1 and the outer sleeve 2 is a double-sided butt weld; the weld between the fourth ring sleeve 12 and the enclosure 11 is an inner side butt weld, and the weld between the enclosure 11 and the third ring sleeve 8 is an inner side butt weld.
[0080] Double-sided butt welding involves machining bevels on both sides of the part, and then performing butt welding on both sides of the part during welding. In step S42, welding can be performed first on one side of the second ring plate 4 to obtain a butt weld on one side. In step S44, the fourth component is flipped over and welded on the other side of the second ring plate 4 to obtain a butt weld on the other side. Then, the fourth pad 214 and the fifth pad 215 are set.
[0081] When the first ring plate 3 and the third ring plate 5 are welded to the outer sleeve 2, the welding can only be performed on the outside of the first ring plate 3 and the third ring plate 5. Therefore, only the outer side butt welds can be used. The outer side butt welds penetrate the first ring plate 3 and the third ring plate 5, and the width of the outer side butt welds decreases from the outside to the inside. Similarly, when the fourth ring sleeve 12 is welded to the cover 11 and the cover 11 is welded to the third ring sleeve 8, the welding torch can only be used on the inside of the cover 11. Therefore, it is an inner side butt weld.
[0082] In steps S4 to S7, each component is assembled from semi-circular parts into a complete ring. During welding, if the weld extends to the split surface, the molten metal will flow to the split surface, connecting the parts on both sides of the split surface together. After welding, the material on the split surface must be removed to separate the components along the split surface, thus damaging the split surface. Therefore, in steps S4 to S7, after welding, there is an anti-sticking section between the weld and the split surface. That is, the weld does not extend to the split surface, leaving a distance unwelded. The length of the anti-sticking section is 30 to 50 mm. This prevents the molten metal at the weld from flowing to the split surface during welding, thus preventing the parts on both sides of the split surface from becoming one. After step S7, the steam seal body is divided into two parts along the split surface, and then the anti-sticking section is welded on.
[0083] The above description is merely a preferred embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. A method for welding a gas seal body, characterized in that, Includes the following steps: S1. Prepare the first ring plate (3), the second ring plate (4), the third ring plate (5), the first ring sleeve (6), the second ring sleeve (7), and the third ring sleeve (8) of the annular ring. Prepare a semi-circular flange (1), an outer sleeve (2), a connecting ring plate (9), an inner sleeve (10), a fourth ring sleeve (12), and a cover (11). S2. Weld the first ring plate (3) to the outer wall of the first ring sleeve (6) to obtain the first component; weld the second ring plate (4) to the outer wall of the second ring sleeve (7) to obtain the second component; weld the third ring plate (5) to the outer wall of the third ring sleeve (8) to obtain the third component; S3. Cut the first component, the second component, and the third component along the midline. S4. First, weld the first component into the outer sleeve (2), then weld the second and third components into the outer sleeve (2). During welding, use tooling for positioning, and the mid-section of the first component, the second component, the third component and the outer sleeve (2) coincide. include: S41. Preparation fixture: The fixture includes a horizontal base (23) and a frame (24) set above the base (23). A vertical positioning shaft (20) is provided on the base (23). The positioning shaft (20) is a hollow shaft and a first heating mechanism (21) is provided inside the positioning shaft (20). A detachable positioning boss (22) is provided on the outer wall of the positioning shaft (20). A positioning sleeve (25) is provided on the second frame (24). The positioning sleeve (25) is coaxial with the positioning shaft (20). A second heating mechanism (26) is provided on the outer wall of the positioning sleeve (25). The positioning sleeve (25) is connected to a first driving mechanism (27) that drives the positioning sleeve (25) to move axially. S42. Set a first pad (28) on the base (23), place the second component on the base (23), the second ring plate (4) of the second component is attached to the first pad (28), the second ring sleeve (7) is fitted on the positioning shaft (20) and is attached to the positioning boss (22), and then place the outer sleeve (2) on the base (23), the outer sleeve (2) is fitted outside the second ring plate (4); use the first heating mechanism (21) to heat the positioning shaft (20) to the outer wall temperature of 100°C to 150°C, use the second heating mechanism (26) to heat the positioning sleeve (25) to 100°C to 150°C, and then use the first driving mechanism (27) to push the positioning sleeve (25) downward and fit it outside the outer sleeve (2), the second heating mechanism (26) stops heating, the first heating mechanism (21) continues heating, and the second ring plate (4) is welded to the outer sleeve (2); S43. A second pad (210) is set on the upper surface of the second ring plate (4), and a third pad (211) is set on the upper surface of the second ring sleeve (7). The first component is pressed between the positioning shaft (20) and the outer sleeve (2). The first ring plate (3) of the first component is attached to the second pad (210), and the first ring sleeve (6) is attached to the third pad (211). Then the first ring plate (3) is welded to the outer sleeve (2) to obtain the fourth component. S44. Remove the fourth component, remove the first pad (28), the second pad (210) and the third pad (211), flip the fourth component over and place it on the base (23), then set the fourth pad (214) on the upper surface of the second ring plate (4) and the fifth pad (215) on the upper surface of the second ring sleeve (7), press the third component between the positioning shaft (20) and the outer sleeve (2), the third ring plate (5) of the third component is attached to the fourth pad (214), the third ring sleeve (8) is attached to the fifth pad (215), and then weld the third ring plate (5) to the outer sleeve (2); S5. Weld the connecting ring plate (9) into the first ring sleeve (6), and weld the inner sleeve (10) onto the connecting ring plate (9). The mid-sections of the connecting ring plate (9), the outer sleeve (2), and the inner sleeve (10) coincide. S6. Weld the flange (1) to the outer wall of the outer sleeve (2), with the mid-section of the flange (1) and the outer sleeve (2) coinciding; S7. Weld the fourth ring (12) to the large end of the cover (11) and weld the small end of the cover (11) to the third ring (8); S8, Tempering.
2. The welding method for a gas seal body as described in claim 1, characterized in that, In step S3, wire cutting is used to cut the first component, the second component, and the third component along the mid-section.
3. The welding method for a gas seal body as described in claim 1, characterized in that, After step S3, the dimensions of the first, second, and third components after cutting are detected. When the dimensions of the split surfaces of the first, second, and third components are smaller than the set dimensions, welding is performed on the split surfaces of the first, second, and third components.
4. The welding method for a gas seal body as described in claim 1, characterized in that, The weld between the first ring plate (3) and the first ring sleeve (6) is a double-sided weld, and the weld between the first ring plate (3) and the outer sleeve (2) is an outer side weld; the weld between the second ring plate (4) and the first ring sleeve (6) is a double-sided weld, and the weld between the second ring plate (4) and the outer sleeve (2) is a double-sided weld; the weld between the third ring plate (5) and the third ring sleeve (8) is a double-sided weld, and the weld between the third ring plate (5) and the outer sleeve (2) is a double-sided weld. The weld between the connecting ring plate (9) and the first ring sleeve (6) is a double-sided weld, and the weld between the connecting ring plate (9) and the inner sleeve (10) is a double-sided weld; the weld between the flange (1) and the outer sleeve (2) is a double-sided weld; the weld between the fourth ring sleeve (12) and the enclosure (11) is an inner side butt weld, and the weld between the enclosure (11) and the third ring sleeve (8) is an inner side butt weld.
5. The welding method for a gas seal body as described in claim 1, characterized in that, In steps S4 to S7, after welding, there is an anti-sticking section between the weld and the split surface. After step S7, the steam seal body is divided into two parts along the split surface, and then the anti-sticking section is welded again.
6. The welding method for a gas seal body as described in claim 1, characterized in that, In step S7, half of the steam seal body is placed on a horizontal support (30). The support (30) is provided with a slide (31) and a vertical center-side limiting plate (32). The slide (31) is slidably engaged with the support (30), and the slide (31) is connected to a second drive mechanism (33) that drives the slide (31) to move toward the center-side limiting plate (32). The slide (31) is provided with an inverted L-shaped pressure plate (34). The upper surface of 34) is provided with a support cover (35); the middle part of the steam seal body is attached to the middle part limiting plate (32), and the pressure plate (34) is attached to the outer side wall and the top wall of the steam seal body; then the enclosure (11) and the fourth ring (12) are placed on the support cover (35), the enclosure (11) and the fourth ring (12) are attached to the support cover (35), and the middle part of the enclosure (11) and the fourth ring (12) are attached to the middle part limiting plate (32), and then welding is performed.
7. The welding method for a gas seal body as described in claim 6, characterized in that, In step S7, after welding, the weld is kept at a temperature of 200 to 250°C for 3 to 4 hours and then ground.
8. The welding method for a gas seal body as described in claim 7, characterized in that, The support base (30) is installed on a pair of horizontal rails (36), and the support base (30) is connected to a third drive mechanism (37) that drives the support base (30) to move along the rails (36). After welding, the third drive mechanism (37) drives the support base (30) to move to the grinding and heat preservation station. The grinding and heat preservation station is equipped with a lifting frame (38), on which a vertical rotating shaft (39) is installed. The rotating shaft (39) is connected to a fourth driving mechanism (310) that drives the rotating shaft (39) to rotate. At least three positioning rods (311) perpendicular to the rotating shaft (39) are fixedly installed on the rotating shaft (39). A cantilever (312) that slides with the positioning rod (311) is installed on the positioning rod (311). Locking nuts (313) that are threaded with the positioning rod (311) are installed on both sides of the cantilever (312). A detachable grinding ring (314) is installed at the end of the cantilever (312). The grinding ring (314) has a grinding surface and a third heating mechanism (315) is installed inside the grinding ring (314).
Citation Information
Patent Citations
Steam turbine steam seal structure capable of realizing axial yielding and working method of structure
CN110130997A
Flange connection device and forming method thereof, welding ring sealing piece and welding ring half part