A large-energy high-performance combined welding method suitable for thick-walled high-strength steel
By using machine learning algorithms and online monitoring technology, a temperature prediction and linear regression model was constructed. Combined with a PID control model, the problem of inaccurate penetration control in the welding of thick-walled high-strength steel was solved, achieving stability and consistency in the welding process, and improving welding efficiency and quality.
Patent Information
- Application Number
- CN202411867595.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-12-18
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2044-12-18
AI Technical Summary
In the welding of thick-walled high-strength steel, the welding quality, especially the precision of the penetration depth, is difficult to control. Traditional methods cannot provide real-time feedback and adjustment, resulting in instability and quality fluctuations in the welding process.
A temperature prediction model and a linear regression model are constructed using machine learning algorithms. Combined with acoustic and visual inspection technologies, a comprehensive evaluation index is generated. Welding parameters are adjusted in real time through a PID control model to achieve stability and consistency in the welding process.
It improves welding efficiency and weld quality, reduces material waste and rework rate, and is suitable for aerospace, marine engineering and high-pressure vessel fields with high-quality welding requirements.
Smart Images

Figure CN119681425B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of high-strength steel welding technology, specifically to a high-input-energy, high-performance combined welding method suitable for thick-walled high-strength steel. Background Technology
[0002] In traditional thick-walled high-strength steel welding processes, controlling weld quality, especially the precision of weld penetration, is often challenging. The complexity of the welding environment and the variability of material properties significantly increase the difficulty of welding. For example, adjusting parameters such as preheating temperature, equipment power, and welding speed is difficult, making traditional empirical formulas and simple control methods insufficient for high-quality welding requirements. Particularly in high-heat welding processes, controlling the heat input is crucial for weld formation and is easily affected by changes in preheating temperature, ambient temperature, and the thermophysical properties of the material. Furthermore, post-weld quality evaluation largely relies on post-weld inspection, lacking real-time feedback for adjusting welding parameters. This leads to instability during the welding process and fluctuations in weld quality.
[0003] The information disclosed in the background section is only intended to enhance the understanding of the background of this disclosure, and therefore may include information that does not constitute prior art known to those skilled in the art. Summary of the Invention
[0004] The purpose of this invention is to provide a high-energy, high-performance combined welding method suitable for thick-walled, high-strength steel, in order to solve the problems mentioned in the background art.
[0005] To achieve the above objectives, the present invention provides the following technical solution:
[0006] A high-energy, high-performance combined welding method for thick-walled, high-strength steel, comprising the following steps:
[0007] S1: Collect historical welding information, including steel material data, size data, preheating temperature and ambient temperature during successful welding, actual weld penetration after welding, and welding parameters of welding equipment. Construct a temperature prediction model based on machine learning algorithms, and divide the material data, size data, and preheating temperature into a first training set and a first validation set to train the temperature prediction model.
[0008] S2: After the temperature prediction model is trained, the input heat during welding is calculated based on the preheating temperature and simplified heat balance equation generated by the temperature prediction model. Then, the input heat is corrected based on the ambient temperature. Based on the corrected input heat and welding parameters, a linear regression model about the actual penetration depth is constructed. The collected preheating temperature, welding parameters, and actual penetration depth are divided into a second training set and a second validation set to optimize the linear regression model.
[0009] S3: Collect material and dimensional data of the steel to be welded, input them into the temperature prediction model to generate the preheating temperature and calculate the input heat, then input the input heat and the user-preset theoretical melting depth into the linear regression model to solve, generate the corresponding welding parameters, and weld a section of the steel to be welded.
[0010] S4: After welding is completed, the weld is inspected by acoustic wave and visual inspection. A comprehensive evaluation index is generated based on the inspection results. The theoretical penetration depth preset by the user is then adjusted based on the comprehensive evaluation index. The next section of steel to be welded is then welded, and this step is repeated until all steel to be welded is completed.
[0011] Preferably, the material data is the content ratio of C, Mn, and Si in the steel, the size data includes the thickness, length, and width of the steel, and the welding parameters include laser power and welding speed.
[0012] Preferably, the temperature prediction model is constructed using a support vector machine algorithm, and a feature set is built based on material data and size data, which is used as the input to the temperature prediction model. The preheating temperature at successful welding is used as the output. The expression of the temperature prediction model is:
[0013]
[0014] In the formula , , These represent the percentages of C, Mn, and Si content in the steel, respectively. , These represent the thickness and width of the steel, respectively. This indicates the output preheating temperature.
[0015] The preferred calculation method for correcting the input heat based on ambient temperature is as follows:
[0016]
[0017] In the formula This indicates the heat input during welding. , , , These represent the density, initial temperature, heat transfer coefficient, and surface area of the steel, respectively. Indicates ambient temperature.
[0018] Preferably, the linear regression model of the actual melting depth is expressed as:
[0019]
[0020] In the formula , , These represent the coefficients of the first model, the coefficients of the second model, and the coefficients of the third model, respectively. Represents the residual constant. , These represent the laser power and welding speed, respectively.
[0021] Preferably, the generation logic of the comprehensive evaluation index is as follows:
[0022] Based on AUT technology, acoustic wave detection is performed on the weld to obtain the length of defects inside the weld. An internal evaluation index is then generated based on the defect type and defect length. The calculation method is as follows:
[0023]
[0024] In the formula This represents the internal evaluation index. , These represent the defect length and the corresponding weighting coefficient, respectively. Indicates the total length of the weld, subscript The number indicating the defect. ;
[0025] Acquire surface images of the weld exterior, perform grayscale processing on the surface images, detect abnormal areas in the surface images, determine whether the abnormal areas are cracks or voids, and calculate the appearance evaluation index based on the area size of the abnormal areas. The calculation method is as follows:
[0026]
[0027] In the formula This represents the appearance evaluation index. , These represent the area of the cracks in the abnormal region and the corresponding weighting coefficient, respectively. , These represent the area of the cavity in the abnormal region and the corresponding weighting coefficient, respectively. Indicates the total area of the weld, subscript This indicates the number of the crack in the abnormal area. , Indicates the number of the cavity in the abnormal area. , This indicates the preset adjustment coefficient;
[0028] A comprehensive evaluation index is generated based on the internal evaluation index and the appearance evaluation index. The calculation method is as follows:
[0029]
[0030] In the formula , These represent the first and second proportionality coefficients, respectively. ,and .
[0031] The preferred method for determining whether an abnormal area is a crack or a cavity is as follows:
[0032] Get the grayscale value of each pixel subscript Represents the coordinates of a pixel. , And use the Prewitt operator to calculate the gradient value of each pixel. and gradient direction ;
[0033] Gradient value of each pixel Compared with the preset segmentation threshold A comparison will be performed to ensure that the following conditions are met. The pixels are labeled as the image background, satisfying the following conditions: The pixels are marked as the target edge, and then a closed shape is formed according to the corresponding gradient direction. This closed shape is considered to be an abnormal region.
[0034] The aspect ratio is calculated based on the length of the abnormal area in both the horizontal and vertical directions. The calculation method is as follows:
[0035]
[0036] In the formula , These represent the lengths of the abnormal region in the horizontal and vertical directions, respectively.
[0037] Compare the aspect ratio with the preset ratio threshold. When a comparison is performed, At that time, the abnormal area was considered to be a crack. At that time, the abnormal area was considered to be a cavity.
[0038] Preferably, the segmentation threshold The method for determining it is as follows:
[0039] Calculate the average gradient values of the image background and the detected target respectively. , The calculation method is as follows:
[0040]
[0041]
[0042] In the formula This indicates the number of pixels in the image background. This indicates the number of pixels in the detected target. This represents the gradient value of the pixel that is calibrated as the image background. This represents the gradient value of the pixel that is identified as an abnormal region;
[0043] Then calculate the inter-class variance of the image background and the detected target. The calculation method is as follows:
[0044]
[0045] Change the segmentation threshold Size, traversal Given the grayscale range, calculate the average grayscale value of the corresponding image background and the detected target. , and inter-class variance It will have the largest inter-class variance The grayscale value is used as the segmentation threshold. .
[0046] Preferably, the method for adjusting the user-preset theoretical melting depth based on the comprehensive evaluation index is as follows:
[0047] The theoretical melting depth is calibrated as A control model is constructed based on the PID algorithm, and the model expression is:
[0048]
[0049] In the formula This indicates the new theoretical melting depth that needs to be adjusted. This indicates the preset evaluation threshold. , , These represent the preset proportional gain, integral gain, and derivative gain, respectively.
[0050] The comprehensive evaluation index of the weld is substituted into the control model to calculate the new theoretical penetration depth and make adjustments.
[0051] Compared with the prior art, the beneficial effects of the present invention are:
[0052] This invention addresses technical challenges such as insufficient automation and difficulty in setting welding parameters during the welding of thick-walled high-strength steel by integrating machine learning algorithms and online monitoring technology. First, a temperature prediction model built using the SVM algorithm accurately predicts the preheating temperature based on material and dimensional data, enabling more effective control of heat input during welding. Second, a linear regression model further optimizes the relationship between welding parameters and actual weld penetration, improving the accuracy of parameter settings. Finally, a comprehensive evaluation index generated by combining acoustic and visual inspection technologies is used, and a PID control model adjusts welding parameters in real time, ensuring the stability of the welding process and the consistency of weld quality. This improves welding efficiency and weld quality, reduces material waste and rework rates, and offers significant economic and social benefits for fields requiring high-quality welding, such as aerospace, marine engineering, and high-pressure vessels. Attached Figure Description
[0053] Figure 1 This is a schematic diagram of the overall method flow of the present invention. Detailed Implementation
[0054] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to specific embodiments.
[0055] It should be noted that, unless otherwise defined, the technical or scientific terms used in this invention should have the ordinary meaning understood by one of ordinary skill in the art to which this invention pertains. The terms "first," "second," and similar terms used in this invention do not indicate any order, quantity, or importance, but are merely used to distinguish different components. Terms such as "comprising" or "including" mean that the element or object preceding the word encompasses the elements or objects listed following the word and their equivalents, without excluding other elements or objects. Terms such as "connected" or "linked" are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. Terms such as "upper," "lower," "left," and "right" are used only to indicate relative positional relationships; when the absolute position of the described object changes, the relative positional relationship may also change accordingly.
[0056] Example:
[0057] Please see Figure 1 The present invention provides a technical solution:
[0058] A high-energy, high-performance combined welding method for thick-walled, high-strength steel, comprising the following steps:
[0059] S1: Collect historical welding information, including steel material data, dimensional data, preheating temperature and ambient temperature during successful welding, actual weld penetration after welding, and welding equipment parameters. Historical welding information refers to the welding parameters and data collected in past welding operations. The material data refers to the percentage of C, Mn, and Si in the steel. The dimensional data includes the thickness, length, and width of the steel. Welding parameters include laser power and welding speed. A temperature prediction model is constructed based on a machine learning algorithm, and the material data, dimensional data, and preheating temperature are divided into a first training set and a first validation set to train the temperature prediction model.
[0060] The temperature prediction model is constructed using the Support Vector Machine (SVM) algorithm. This is because the SVM algorithm is more suitable for processing data with a small number of samples. Furthermore, it constructs a feature set based on material and dimensional data, which is then used as the input to the temperature prediction model. The preheating temperature at successful welding is used as the output. The expression for the temperature prediction model is:
[0061]
[0062] In the formula , , These represent the percentages of C, Mn, and Si content in the steel, respectively. , These represent the thickness and width of the steel, respectively. This indicates the output preheating temperature.
[0063] In this step, the chemical composition of the steel is used. and size , The preheating temperature is used as an input feature variable. To make predictions, an appropriate kernel function (such as radial basis function) is selected, and the optimal hyperparameters (such as penalty parameter C) are adjusted and selected through cross-validation. The model is then trained using the training set to find the optimal decision boundary to minimize prediction error. Error analysis can be performed using statistical metrics such as mean squared error (MSE) and R². Finally, the model's predictive performance is evaluated using the validation set, focusing primarily on its accuracy, stability, and generalization ability.
[0064] By using machine learning models to predict preheating temperature, personalized temperature settings can be implemented based on the actual material composition (C, Mn, Si content) and steel dimensions (thickness, length, width). Compared to traditional empirical formulas or fixed parameter settings, this method more accurately reflects the needs of the actual welding process, improving the adaptability and accuracy of the welding process. Furthermore, through analysis and learning from historical welding information, the machine learning model can comprehensively consider the influence of multiple factors on the preheating temperature, thereby optimizing the heat input during the welding process. This strategy effectively reduces weld quality problems caused by improper heat control during welding, such as weld deformation and crack formation, ensuring the consistency and stability of weld quality.
[0065] S2: After the temperature prediction model is trained, the input heat during welding is calculated based on the preheating temperature and simplified heat balance equation generated by the temperature prediction model. Then, the input heat is corrected based on the ambient temperature. Based on the corrected input heat and welding parameters, a linear regression model about the actual penetration depth is constructed. The collected preheating temperature, welding parameters, and actual penetration depth are divided into a second training set and a second validation set to optimize the linear regression model.
[0066] The calculation method for correcting the input heat based on ambient temperature is as follows:
[0067]
[0068] In the formula This indicates the heat input during welding. , , , These represent the density, initial temperature, heat transfer coefficient, and surface area of the steel, respectively. Indicates ambient temperature.
[0069] The first part of the formula represents the theoretically required input heat for the steel to reach its preheating temperature, while the second part represents the input heat wasted due to heat dissipation from the steel. Overall, it reflects the input energy required during the preheating stage. By considering the influence of ambient temperature changes, the control of welding heat becomes more precise and scientific, allowing for better control of the welding process, reducing overheating or underheating, adapting to a wider range of working environments, ensuring the stability and reliability of the welding process, thereby improving welding quality, reducing energy consumption and material waste, and lowering production costs.
[0070] The linear regression model for the actual melting depth is expressed as follows:
[0071]
[0072] In the formula , , These represent the coefficients of the first model, the coefficients of the second model, and the coefficients of the third model, respectively. Represents the residual constant. , These represent the laser power and welding speed, respectively. This formula is used to reflect the actual penetration depth of the steel after the preheating and welding stages.
[0073] In this step, the introduction of data-driven decision support enhances the innovation and sophistication of the welding process, enabling it to automatically adjust to actual conditions (such as different ambient temperatures and material properties), thereby improving the adaptability and flexibility of the welding process.
[0074] S3: Collect material and dimensional data of the steel to be welded, input them into the temperature prediction model to generate the preheating temperature and calculate the input heat, then input the input heat and the user-preset theoretical melting depth into the linear regression model to solve, generate the corresponding welding parameters, and weld a section of the steel to be welded.
[0075] In this step, after obtaining the specific data of the material, the theoretical melting depth is substituted into the linear regression model. Welding parameters can be obtained directly through the model, which speeds up production preparation and process optimization, ensuring that each weld reaches the expected penetration depth, ensuring product consistency, reducing errors that may occur when manually setting parameters, reducing rework and scrap, and improving overall production efficiency.
[0076] S4: After welding is completed, the weld is inspected by acoustic wave and visual inspection. A comprehensive evaluation index is generated based on the inspection results. The theoretical penetration depth preset by the user is then adjusted based on the comprehensive evaluation index. The next section of steel to be welded is then welded, and this step is repeated until all steel to be welded is completed.
[0077] The logic for generating the comprehensive evaluation index is as follows:
[0078] Based on AUT technology, acoustic wave detection is performed on the weld to obtain the length of internal defects. An internal evaluation index is then generated based on the defect type and length. The calculation method is as follows:
[0079]
[0080] In the formula This represents the internal evaluation index. , These represent the defect length and the corresponding weighting coefficient, respectively. Indicates the total length of the weld, subscript The number indicating the defect. .
[0081] For defect length, different intervals result in different severity judgments and have different impacts on the overall weld. Therefore, different weighting coefficients need to be set to reflect this impact. The judgment intervals for defect length have different standards depending on the actual situation. They can be set according to the actual situation to divide defects of different lengths and match them with the corresponding weighting coefficients.
[0082] Acquire surface images of the weld exterior, perform grayscale processing on the surface images, detect abnormal areas in the surface images, determine whether the abnormal areas are cracks or voids, and calculate the appearance evaluation index based on the area size of the abnormal areas. The calculation method is as follows:
[0083]
[0084] In the formula This represents the appearance evaluation index. , These represent the area of the cracks in the abnormal region and the corresponding weighting coefficient, respectively. , These represent the area of the cavity in the abnormal region and the corresponding weighting coefficient, respectively. Indicates the total area of the weld, subscript This indicates the number of the crack in the abnormal area. , Indicates the number of the cavity in the abnormal area. , This represents the preset adjustment coefficient, here , These values reflect the magnitude of the impact of cracks and voids on the overall quality of the weld, and the specific values can be set by the user.
[0085] The method for determining whether an abnormal area is a crack or a cavity is as follows:
[0086] Get the grayscale value of each pixel subscript Represents the coordinates of a pixel. , And use the Prewitt operator to calculate the gradient value of each pixel. and gradient direction ;
[0087] Gradient value of each pixel Compared with the preset segmentation threshold A comparison will be performed to ensure that the following conditions are met. The pixels are labeled as the image background, satisfying the following conditions: The pixels are marked as the target edge, and then a closed shape is formed according to the corresponding gradient direction. This closed shape is considered to be an abnormal region.
[0088] The aspect ratio is calculated based on the length of the abnormal area in both the horizontal and vertical directions. The calculation method is as follows:
[0089]
[0090] These represent the lengths of the abnormal region in the horizontal and vertical directions, respectively. This formula takes... The longer segment is designated as the length, and the shorter segment as the width, ensuring that the aspect ratio is always ≥1 for easy judgment. The aspect ratio is then compared with a preset ratio threshold. When a comparison is performed, At that time, the abnormal area was considered to be a crack. At that time, the abnormal area was considered to be a cavity.
[0091] This is because cracks are typically elongated, resulting in a large length-to-width ratio, while holes are generally round or elliptical, resulting in a small length-to-width ratio. Therefore, the proportional threshold... It should be greater than or equal to 1 and be close to 1. The specific size is set by the user.
[0092] The segmentation threshold The method for determining it is as follows:
[0093] Calculate the average gradient values of the image background and the detected target respectively. , The calculation method is as follows:
[0094]
[0095]
[0096] In the formula This indicates the number of pixels in the image background. This indicates the number of pixels in the detected target. This represents the gradient value of the pixel that is calibrated as the image background. This represents the gradient value of the pixel that is identified as an abnormal region;
[0097] Then calculate the inter-class variance of the image background and the detected target. The calculation method is as follows:
[0098]
[0099] Change the segmentation threshold Size, traversal Given the grayscale range, calculate the average grayscale value of the corresponding image background and the detected target. , and inter-class variance It will have the largest inter-class variance The grayscale value is used as the segmentation threshold. .
[0100] This method can automatically determine a suitable threshold to segment the image into two categories: image background and abnormal regions, thereby maximizing the inter-class variance, that is, maximizing the difference between image background and abnormal regions.
[0101] A comprehensive evaluation index is generated based on the internal evaluation index and the appearance evaluation index. The calculation method is as follows:
[0102]
[0103] In the formula , These represent the first and second proportionality coefficients, respectively. ,and .
[0104] The comprehensive evaluation index is used to make a comprehensive judgment based on the quality of the weld's internal and external surfaces. The longer the internal defects and the larger the abnormal areas on the surface, the higher the comprehensive evaluation index value, and the worse the weld quality.
[0105] The method for adjusting the user-preset theoretical melting depth based on the comprehensive evaluation index is as follows:
[0106] The theoretical melting depth is calibrated as A control model is constructed based on the PID algorithm, and the model expression is:
[0107]
[0108] In the formula This indicates the new theoretical melting depth that needs to be adjusted. This indicates the preset evaluation threshold. , , These represent the preset proportional gain, integral gain, and derivative gain, respectively. The comprehensive evaluation index of the weld is substituted into the control model to calculate the new theoretical weld penetration depth and make adjustments. , , The value can be obtained by the user in advance through simulation software, or by performing trial welding on a batch of steel.
[0109] Since the comprehensive evaluation index is positively correlated with the defect length and the area of the abnormal region, it needs to be adjusted when it exceeds the preset evaluation threshold. The biggest reason for internal defects, cracks, and voids is insufficient theoretical penetration depth of the steel, leading to undersized welding parameters and excessively low welding temperatures that prevent complete melting of the weld metal. When the comprehensive evaluation index decreases (indicating weld quality exceeds expectations), the theoretical penetration depth needs to be appropriately reduced to adjust welding parameters and avoid over-welding caused by occasional power fluctuations in the equipment. Conversely, if the comprehensive evaluation index increases (indicating weld quality does not meet expectations), the theoretical penetration depth needs to be increased to improve weld quality, thereby achieving dynamic optimization and automatic adjustment of weld quality.
[0110] In summary, this invention innovatively solves several technical challenges in the welding process of thick-walled high-strength steel by integrating machine learning algorithms and online monitoring technology. First, the temperature prediction model built using the SVM algorithm can accurately predict the preheating temperature based on material and dimensional data, thus enabling more effective control of heat input during welding. Second, the linear regression model further optimizes the relationship between welding parameters and actual weld penetration, improving the accuracy of welding parameter settings. Finally, by combining a comprehensive evaluation index generated from acoustic and visual inspection technologies, and using a PID control model to adjust welding parameters in real time, the stability of the welding process and the consistency of weld quality are ensured. The implementation of this solution can improve welding efficiency and weld quality, reduce material waste and rework rates, and has significant economic and social benefits for fields such as aerospace, marine engineering, and high-pressure vessels where high-quality welding is required.
[0111] The above formulas are all dimensionless calculations. The formulas are derived from software simulations based on a large amount of collected data to obtain the most recent real-world results. The preset parameters in the formulas are set by those skilled in the art according to the actual situation.
[0112] The above embodiments can be implemented, in whole or in part, by software, hardware, firmware, or any other combination thereof. When implemented in software, the above embodiments can be implemented, in whole or in part, as a computer program product. Those skilled in the art will recognize that the units and algorithm steps of the various examples described in conjunction with the embodiments disclosed herein can be implemented by electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are implemented in hardware or software depends on the specific application and design constraints of the technical solution.
[0113] The units described as separate components may or may not be physically separate. The components shown as units may or may not be physical units; they may be located in one place or distributed across multiple network units. Some or all of the units can be selected to achieve the purpose of this embodiment according to actual needs.
[0114] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any changes or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application.
Claims
1. A high-input-energy, high-performance combined welding method suitable for thick-walled, high-strength steel, characterized in that, The specific steps include: S1: Collect historical welding information, including steel material data, size data, preheating temperature and ambient temperature during successful welding, actual weld penetration after welding, and welding parameters of welding equipment. Construct a temperature prediction model based on machine learning algorithms, and divide the material data, size data, and preheating temperature into a first training set and a first validation set to train the temperature prediction model. The temperature prediction model is constructed using a support vector machine algorithm. It builds a feature set based on material and dimensional data, which is then used as input to the model. The preheating temperature at successful welding is output. The expression for the temperature prediction model is: ; In the formula , , These represent the percentages of C, Mn, and Si content in the steel, respectively. , These represent the thickness and width of the steel, respectively. Indicates the output preheating temperature; S2: After the temperature prediction model is trained, the input heat during welding is calculated based on the preheating temperature and simplified heat balance equation generated by the temperature prediction model. Then, the input heat is corrected based on the ambient temperature. Based on the corrected input heat and welding parameters, a linear regression model about the actual penetration depth is constructed. The collected preheating temperature, welding parameters, and actual penetration depth are divided into a second training set and a second validation set to optimize the linear regression model. S3: Collect material and dimensional data of the steel to be welded, input them into the temperature prediction model to generate the preheating temperature and calculate the input heat, then input the input heat and the user-preset theoretical melting depth into the linear regression model to solve, generate the corresponding welding parameters, and weld a section of the steel to be welded. S4: After welding is completed, the weld is inspected by sound waves and appearance. A comprehensive evaluation index is generated based on the inspection results of the weld. The theoretical penetration depth preset by the user is then adjusted based on the comprehensive evaluation index. The next section of steel to be welded is then welded, and this step is repeated until all steel to be welded is completed. The logic for generating the comprehensive evaluation index is as follows: Based on AUT technology, acoustic wave detection is performed on the weld to obtain the length of internal defects. An internal evaluation index is then generated based on the defect type and length. The calculation method is as follows: ; In the formula This represents the internal evaluation index. , These represent the defect length and the corresponding weighting coefficient, respectively. Indicates the total length of the weld, subscript The number indicating the defect. ; Acquire surface images of the weld exterior, perform grayscale processing on the surface images, detect abnormal areas in the surface images, determine whether the abnormal areas are cracks or voids, and calculate the appearance evaluation index based on the area size of the abnormal areas. The calculation method is as follows: ; In the formula This represents the appearance evaluation index. , These represent the area of the cracks in the abnormal region and the corresponding weighting coefficient, respectively. , These represent the area of the cavity in the abnormal region and the corresponding weighting coefficient, respectively. Indicates the total area of the weld, subscript This indicates the number of the crack in the abnormal area. , Indicates the number of the cavity in the abnormal area. , This indicates the preset adjustment coefficient; A comprehensive evaluation index is generated based on the internal evaluation index and the appearance evaluation index. The calculation method is as follows: ; In the formula , These represent the first and second proportionality coefficients, respectively. ,and .
2. The high heat input high performance combined welding method for thick-walled high-strength steel according to claim 1, characterized in that: The material data refers to the percentage of C, Mn, and Si content in the steel, the size data includes the thickness, length, and width of the steel, and the welding parameters include laser power and welding speed.
3. The high heat input and high performance combined welding method for thick-walled high-strength steel according to claim 1, characterized in that: The method for determining whether an abnormal area is a crack or a cavity is as follows: Get the grayscale value of each pixel subscript Represents the coordinates of a pixel. , And use the Prewitt operator to calculate the gradient value of each pixel. and gradient direction ; Gradient value of each pixel Compared with the preset segmentation threshold A comparison will be performed to ensure that the following conditions are met. The pixels are labeled as the image background, satisfying the following conditions: The pixels are marked as the target edge, and then a closed shape is formed according to the corresponding gradient direction. This closed shape is considered to be an abnormal region. The aspect ratio is calculated based on the length of the abnormal area in both the horizontal and vertical directions. The calculation method is as follows: ; In the formula , These represent the lengths of the abnormal region in the horizontal and vertical directions, respectively. This formula is used to determine... The longer segment is designated as the length, and the shorter segment as the width, to ensure that the aspect ratio is always ≥1; Compare the aspect ratio with the preset ratio threshold. When a comparison is performed, At that time, the abnormal area was considered to be a crack. At that time, the abnormal area was considered to be a cavity.
4. The high heat input high performance combined welding method for thick-walled high-strength steel according to claim 3, characterized in that: The segmentation threshold The method for determining it is as follows: Calculate the average gradient values of the image background and the detected target respectively. , The calculation method is as follows: ; ; In the formula This indicates the number of pixels in the image background. This indicates the number of pixels in the detected target. This represents the gradient value of the pixel that is calibrated as the image background. This represents the gradient value of the pixel that is identified as an abnormal region; Then calculate the inter-class variance of the image background and the detected target. The calculation method is as follows: ; Change the segmentation threshold Size, traversal Given the grayscale range, calculate the average grayscale value of the corresponding image background and the detected target. , and inter-class variance It will have the largest inter-class variance The grayscale value is used as the segmentation threshold. .
Citation Information
Patent Citations
Method and device for calculating welding quality determination set value and welding method
JP2020146704A