Trimming-free rubber ring vulcanizing mold

By designing a fleece-free rubber ring vulcanization mold, using the H-type rubber inlet channel and sealing ring design, the problem of uneven flying and rubber injection during the rubber ring molding process is solved, and an efficient and automated rubber molding process is achieved, saving costs and improving work efficiency.

CN120023979AActive Publication Date: 2025-05-23SUZHOU MENGDE MOLD MFG CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202510441616.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-04-09
Publication Date
2025-05-23
Estimated Expiration
2045-04-09

AI Technical Summary

Technical Problem

During the injection molding process of rubber rings, existing molds are prone to flashing, and the glue injection is uneven, resulting in large local pressure and many flashing.

Method used

设计了一种无飞边橡胶圈硫化模具,包含上模板和下模板,设置有导向孔、导向柱、进胶口、成型槽、进胶槽和密封槽,通过H型进胶通道和密封圈的设计,确保胶料均匀注入并形成密封性好的成型腔。

Benefits of technology

The rubber ring molding has been achieved without flares, saving the cost of rubber raw materials and manual cleaning of flares, solving the problem of automated production of rubber products, faster rubber injection and better molding effect, and two rubber rings can be formed at one time, improving work efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120023979A_ABST
    Figure CN120023979A_ABST
Patent Text Reader

Abstract

The invention discloses a non-flash rubber ring vulcanization mold. The non-flash rubber ring vulcanization mold comprises a runner plate, an upper mold plate, a lower mold plate, a first sealing ring and a second sealing ring, wherein the runner plate is provided with a glue inlet runner; a plurality of guide holes, a pair of glue inlets, a pair of upper forming grooves and a pair of upper glue inlets are formed in the upper mold plate; the upper ends of the pair of glue inlets are communicated with the glue inlet runner, and the lower ends are respectively communicated with the pair of upper glue inlet grooves in a one-to-one correspondence manner; a plurality of guide columns, a pair of first sealing grooves, a pair of lower forming grooves and a pair of lower glue feeding grooves are formed in the lower mold plate; a pair of second sealing grooves are symmetrically formed in the two sides of each lower glue feeding groove; the first sealing ring is arranged in the first sealing groove; the second sealing ring is arranged in the second sealing groove; the first sealing ring and the second sealing ring are made of PEEK materials. The sealing problem is solved, no flash exists in product forming, and rubber raw materials and the cost for manually cleaning the flash are saved; the problem of automatic production of rubber products is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of rubber component molding dies, in particular to a vulcanization die for a rubber ring without flash. Background Art

[0002] During the injection molding process of the rubber ring, a certain gap is easily generated between the upper mold plate and the lower mold plate, resulting in a circle of flash around the rubber ring. In the prior art, most of the lower mold plates are provided with tearing grooves, but the effect is sometimes not ideal, and the rubber will overflow outside the tearing groove, resulting in a large amount of flash. In addition, the rubber ring mold usually has only one glue inlet, which easily leads to a large local pressure, resulting in uneven glue injection or more local flash. Summary of the invention

[0003] According to an embodiment of the present invention, a flash-free rubber ring vulcanization mold is provided, comprising: A flow channel plate, wherein a glue inlet flow channel is arranged on the flow channel plate; The upper template is provided with a plurality of guide holes, a pair of glue inlets, a pair of upper molding grooves and a pair of upper glue inlet grooves; the upper ends of the pair of glue inlets are connected with the glue inlet flow channel, and the lower ends are respectively corresponding to and connected with the pair of upper glue inlet grooves; The lower template is provided with a plurality of guide posts, a pair of first sealing grooves, a pair of lower molding grooves and a pair of lower glue inlet grooves, the plurality of guide posts correspond to the plurality of guide holes one by one and can be inserted into the corresponding guide holes; the pair of first sealing grooves, the pair of lower molding grooves and the pair of lower glue inlet grooves correspond to each other one by one; The first sealing groove surrounds the corresponding lower molding groove for one circle, and the lower molding groove surrounds the corresponding lower glue inlet groove for one circle; A pair of second sealing grooves are symmetrically arranged on both sides of each lower glue inlet groove, and the second sealing grooves are arranged on the inner circle of the lower molding groove; The upper molding groove matches with the lower molding groove to form a complete molding cavity; the upper glue feeding groove matches with the lower glue feeding groove to form a complete glue feeding channel; The glue feeding channel is H-shaped, and a plurality of glue feeding holes are arranged at both ends of the glue feeding channel, and the glue feeding holes are connected with the molding cavity; A first sealing ring, which is disposed in the first sealing groove and protrudes out of the first sealing groove; A second sealing ring, which is arranged in the second sealing groove and protrudes out of the second sealing groove; The first sealing ring and the second sealing ring are made of PEEK material.

[0004] Furthermore, a pair of residual material grooves are symmetrically arranged at both ends of the first sealing groove, and the residual material grooves are connected to the lower forming groove.

[0005] Furthermore, a pair of first slots are symmetrically arranged between the lower molding groove and the first sealing groove; a pair of second slots are symmetrically arranged at both ends of the first sealing ring; a pair of third slots are symmetrically arranged between the first sealing groove and the pair of residual material slots; the first slot, the second slot, the third slot and the residual material slot correspond one by one, and the lower molding groove is connected with the residual material slot through the first slot, the second slot and the third slot.

[0006] Furthermore, an air extraction hole and a detection hole are provided on the upper template, the air extraction hole is connected to one of the residual material troughs, and the detection hole is connected to the other residual material trough.

[0007] Furthermore, a triangular material blocking block is provided at each of the forks at both ends of the glue feeding channel, so that the liquid glue is divided into two paths and flows through the plurality of glue feeding holes respectively.

[0008] Furthermore, chamfers are provided on both sides of the bottom of the first sealing ring, so that a gap is left between the bottom of the first sealing ring and the first sealing groove.

[0009] Furthermore, chamfers are provided on both sides of the bottom of the second sealing ring, so that a gap is left between the bottom of the second sealing ring and the second sealing groove.

[0010] Furthermore, a third sealing groove is arranged on the lower template, the third sealing groove surrounds the pair of first sealing grooves, and a third sealing ring is arranged in the third sealing groove.

[0011] Furthermore, a fourth sealing groove is provided on the upper template, the fourth sealing groove surrounds a pair of glue inlets, and a fourth sealing ring is provided in the fourth sealing groove.

[0012] The flash-free rubber ring vulcanization mold according to the embodiment of the present invention solves the sealing problem, and the product is molded without flash, saving the cost of rubber raw materials and manual flash cleaning; it solves the problem of automated production of rubber products; the glue feeding is faster through the vacuum extraction and the setting of the glue feeding channel, so that the molding effect of the product is better; two rubber rings can be molded at one time, which improves work efficiency.

[0013] It is to be understood that both the foregoing general description and the following detailed description are exemplary, and are intended to provide further explanation of the technology as claimed. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 An exploded view of a vulcanization mold for a rubber ring without flash according to an embodiment of the present invention; Figure 2 for Figure 1 A magnified image of point A; Figure 3 It is a schematic diagram of a front view of a vulcanization mold for a rubber ring without flash according to an embodiment of the present invention; Figure 4A schematic top view of a vulcanization mold for a rubber ring without flash according to an embodiment of the present invention; Figure 5 for Figure 4 AA section view; Figure 6 for Figure 5 The enlarged view of point B; Figure 7 for Figure 4 BB section view; Figure 8 for Figure 7 Enlarged view of point C; Fig. 9 is a schematic structural diagram of a lower template according to an embodiment of the present invention; Fig.10 for Fig. 9 The enlarged view of point D; Fig.11 A partial enlarged view of a glue feeding channel according to an embodiment of the present invention; Fig.12 Schematic diagram of the structure of the first sealing ring and the second sealing ring according to an embodiment of the present invention. DETAILED DESCRIPTION

[0015] The preferred embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings to further illustrate the present invention.

[0016] First, combine Figures 1 to 12 A flash-free rubber ring vulcanization mold according to an embodiment of the present invention is described, which is used for the production of rubber parts and has a wide range of application scenarios.

[0017] like Figures 1 to 12 As shown, the flash-free rubber ring vulcanization mold of the embodiment of the present invention comprises: A flow channel plate 1, on which a glue inlet flow channel 11 is provided; The upper template 2 is provided with a plurality of guide holes 21, a pair of glue inlets 22, a pair of upper molding grooves 23 and a pair of upper glue inlet grooves 24; the upper ends of the pair of glue inlets 22 are connected to the glue inlet flow channel 11, and the lower ends are respectively corresponding to and connected to the pair of upper glue inlet grooves 24; The lower template 3 is provided with a plurality of guide posts 31, a pair of first sealing grooves 32, a pair of lower molding grooves 33 and a pair of lower glue inlet grooves 34. The plurality of guide posts 31 correspond to the plurality of guide holes 21 one by one and can be inserted into the corresponding guide holes 21. The guide posts 31 play a guiding role when the mold is closed; the pair of first sealing grooves 32, the pair of lower molding grooves 33 and the pair of lower glue inlet grooves 34 correspond to each other one by one. The first sealing groove 32 surrounds the corresponding lower molding groove 33, and the lower molding groove 33 surrounds the corresponding lower glue feeding groove 34. A pair of second sealing grooves 35 are symmetrically arranged on both sides of each lower glue inlet groove 34, and the second sealing grooves 35 are arranged on the inner circle of the lower molding groove 33; The upper molding groove 23 and the lower molding groove 33 match to form a complete molding cavity a; the upper glue feeding groove 24 and the lower glue feeding groove 34 match to form a complete glue feeding channel b; The glue inlet channel b is H-shaped, and a plurality of glue inlet holes b1 are arranged at both ends of the glue inlet channel b. The glue inlet holes b1 are connected to the molding cavity a, so that the glue material enters the molding cavity a evenly from the glue inlet holes b1 at both ends of the glue inlet channel b during the glue injection process; The first sealing ring 4 is arranged in the first sealing groove 32 and protrudes out of the first sealing groove 32. When the upper mold plate 2 is closed, it contacts and squeezes the first sealing ring 4 to achieve a better sealing effect; The second sealing ring 5 is arranged in the second sealing groove 35 and protrudes out of the second sealing groove 35. When the mold is closed, the upper mold plate 2 contacts and squeezes the second sealing ring 5 to achieve a better sealing effect; The first sealing ring 4 and the second sealing ring 5 are made of PEEK material. PEEK material is corrosion-resistant and aging-resistant, has strong flexibility and rigidity, and has strong wear resistance. Therefore, the first sealing ring 4 and the second sealing ring 5 are made of PEEK material, which greatly improves the sealing between the lower template 3 and the upper template 2, and prevents the generation of flash during the rubber ring molding process due to the gap between the upper template 2 and the lower template 3.

[0018] Further, if Figure 2 , 12 As shown, in this embodiment, a pair of residual material grooves 36 are symmetrically arranged at both ends of the first sealing groove 32, and the residual material grooves 36 are connected to the lower molding groove 33. The residual material grooves 36 are used to hold excess liquid material during injection molding and gas generated during the molding process.

[0019] Further, if Figure 2 , 12 As shown, in this embodiment, a pair of first notches 37 are symmetrically arranged between the lower molding groove 33 and the first sealing groove 32; a pair of second notches 38 are symmetrically arranged at both ends of the first sealing ring 4; a pair of third notches 39 are symmetrically arranged between the first sealing groove 32 and the pair of residual material grooves 36; the first notch 37, the second notch 38, the third notch 39 and the residual material groove 36 correspond one to one, and the lower molding groove 33 is connected with the residual material groove 36 through the first notch 37, the second notch 38, and the third notch 39, so that the residual material can better enter the residual material groove 36.

[0020] Further, if Figure 7As shown, in this embodiment, the upper mold plate 2 is provided with an air extraction hole 25 and a detection hole 26, and the air extraction hole 25 is connected to one of the residual material grooves 36. After the mold is closed, the vacuum generator evacuates the molding cavity a through the air extraction hole 25 to facilitate the material to enter the molding cavity a better. The air extraction hole 25 is directly connected to the residual material groove 36, which not only simplifies the structure, but also better maintains the sealing of the molding cavity a, and further prevents the generation of flash. The detection hole 26 is connected to the other residual material groove 36, and a negative pressure gauge is installed in the detection hole 26 for detecting the pressure in the mold.

[0021] Further, if Figures 10-11 As shown, in this embodiment, a triangular blocking block b2 is provided at each fork at both ends of the glue feeding channel b, so that the liquid glue flows through several glue feeding holes b1 in two ways respectively, so that the glue can flow through each glue feeding hole b1 more evenly, thereby achieving a better molding effect.

[0022] Further, if Figure 6 As shown, in this embodiment, chamfers 41 are provided on both sides of the bottom of the first sealing ring 4, so that a gap is left between the bottom of the first sealing ring 4 and the first sealing groove 32, so that the first sealing ring 4 has a deformation margin when the mold is closed.

[0023] Further, if Figure 6 As shown, in this embodiment, chamfers 51 are provided on both sides of the bottom of the second sealing ring 5, so that a gap is left between the bottom of the second sealing ring 5 and the second sealing groove 35, so that the second sealing ring 5 has a deformation margin when the mold is closed.

[0024] Further, if Figure 1 As shown, in this embodiment, a third sealing groove 310 is provided on the lower template 3, and the third sealing groove 310 surrounds a pair of first sealing grooves 32. A third sealing ring 6 is provided in the third sealing groove 310 to improve the sealing between the upper template 2 and the lower template 3 to achieve a better vacuuming effect.

[0025] Further, if Figure 1 As shown, in this embodiment, a fourth sealing groove 27 is provided on the upper template 2, and the fourth sealing groove 27 surrounds a pair of glue inlets 22. A fourth sealing ring 7 is provided in the fourth sealing groove 27 to improve the sealing between the flow channel plate 1 and the upper template 2, so as to achieve a better vacuuming effect.

[0026] Furthermore, in this embodiment, the third sealing ring 6 and the fourth sealing ring 7 are made of rubber material.

[0027] Working principle: First, put the first sealing ring 4 into the corresponding first sealing groove 32, put the second sealing ring 5 into the corresponding second sealing groove 35, put the third sealing ring 6 into the corresponding third sealing groove 310, and put the fourth sealing ring 7 into the corresponding fourth sealing groove 27; then, close the mold, and the upper template 2 contacts and squeezes the first sealing ring 4 and the second sealing ring 5 to make the upper template 2 and the lower template 3 sealed; then, vacuumize the molding cavity a through the exhaust hole 25; then, inject the material, and the liquid glue enters the molding cavity a through the glue inlet 22, the glue inlet channel b, and the glue inlet hole b1 for molding. Finally, open the mold after cooling and take out the two rubber rings.

[0028] Above, refer to Figures 1 to 12 The invention describes a vulcanization mold for a rubber ring without flash according to an embodiment of the invention, which solves the sealing problem, and the product is molded without flash, thereby saving the cost of rubber raw materials and manual cleaning of flash; it solves the problem of automated production of rubber products; through vacuuming and setting of a glue feeding channel b, the glue feeding is made more uniform and faster, and the molding effect of the product is better; two rubber rings can be molded at one time, thereby improving work efficiency.

[0029] It should be noted that, in this specification, the terms "include", "comprises" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprises..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.

[0030] Although the content of the present invention has been described in detail through the above preferred embodiments, it should be appreciated that the above description should not be considered as a limitation of the present invention. After reading the above content, it will be apparent to those skilled in the art that various modifications and substitutions of the present invention will occur. Therefore, the protection scope of the present invention should be limited by the appended claims.

Claims

1. A vulcanization mold for a rubber ring without flash, characterized in that: Include: A flow channel plate, wherein a glue inlet flow channel is arranged on the flow channel plate; An upper template, wherein the upper template is provided with a plurality of guide holes, a pair of glue inlets, a pair of upper molding grooves and a pair of upper glue inlet grooves; the upper ends of the pair of glue inlets are connected to the glue inlet flow channel, and the lower ends correspond to and are connected to the pair of upper glue inlet grooves one by one; A lower template, wherein the lower template is provided with a plurality of guide posts, a pair of first sealing grooves, a pair of lower molding grooves and a pair of lower glue feeding grooves, wherein the plurality of guide posts correspond to the plurality of guide holes one by one and can be inserted into the corresponding guide holes; the pair of first sealing grooves, the pair of lower molding grooves and the pair of lower glue feeding grooves correspond to each other one by one; The first sealing groove surrounds the corresponding lower molding groove for one circle, and the lower molding groove surrounds the corresponding lower glue inlet groove for one circle; A pair of second sealing grooves are symmetrically arranged on both sides of each lower glue inlet groove, and the second sealing grooves are arranged on the inner circle of the lower molding groove; The upper molding groove matches with the lower molding groove to form a complete molding cavity; the upper glue feeding groove matches with the lower glue feeding groove to form a complete glue feeding channel; The glue inlet channel is H-shaped, and a plurality of glue inlet holes are arranged at both ends of the glue inlet channel, and the glue inlet holes are connected to the molding cavity; A first sealing ring, which is disposed in the first sealing groove and protrudes out of the first sealing groove; a second sealing ring, the second sealing ring being disposed in the second sealing groove and protruding out of the second sealing groove; The first sealing ring and the second sealing ring are made of PEEK material.

2. The flashless rubber ring vulcanization mold according to claim 1, characterized in that: A pair of residual material grooves are symmetrically arranged at both ends of the first sealing groove, and the residual material grooves are communicated with the lower forming groove.

3. The flashless rubber ring vulcanization mold according to claim 2, characterized in that: A pair of first notches are symmetrically arranged between the lower molding groove and the first sealing groove; a pair of second notches are symmetrically arranged at both ends of the first sealing ring; a pair of third notches are symmetrically arranged between the first sealing groove and the pair of residual material grooves; the first notch, the second notch, the third notch and the residual material groove correspond one to one, and the lower molding groove is connected with the residual material groove through the first notch, the second notch and the third notch.

4. The flashless rubber ring vulcanization mold according to claim 2, characterized in that: The upper template is provided with an air extraction hole and a detection hole, the air extraction hole is connected with one of the residual material troughs, and the detection hole is connected with the other residual material trough.

5. The flashless rubber ring vulcanization mold according to claim 1, characterized in that: A triangular material blocking block is respectively arranged at the forks at both ends of the glue feeding channel, so that the liquid glue is divided into two paths and flows through the plurality of glue feeding holes respectively.

6. The flashless rubber ring vulcanization mold according to claim 1, characterized in that: Chamfers are arranged on both sides of the bottom of the first sealing ring, so that a gap is left between the bottom of the first sealing ring and the first sealing groove.

7. The flashless rubber ring vulcanization mold according to claim 1, characterized in that: Chamfers are arranged on both sides of the bottom of the second sealing ring, so that a gap is left between the bottom of the second sealing ring and the second sealing groove.

8. The flashless rubber ring vulcanization mold according to claim 1, characterized in that: The lower template is provided with the third sealing groove, which surrounds the pair of first sealing grooves, and a third sealing ring is provided in the third sealing groove.

9. The flashless rubber ring vulcanization mold according to claim 1, characterized in that: The upper template is provided with the fourth sealing groove, the fourth sealing groove surrounds the pair of glue inlets, and a fourth sealing ring is provided in the fourth sealing groove.

Citation Information

Patent Citations

  • Composite laminated plate manufacturing mold

    CN108215249A

  • Improved cold runner injection sealing ring mold

    CN115464839A