A mud film, a preparation method and application thereof
By adding porous silica to the aqueous phase of the mud film, the problem of high-temperature water discharge from the mud film was solved, and the high-temperature stability and production efficiency were improved at a low cost.
Patent Information
- Application Number
- CN202510354240.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-03-25
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2045-03-25
AI Technical Summary
Existing mud films are prone to water seepage during high-temperature stability tests, and current solutions are limited, affecting product quality.
Adding porous silica to the aqueous phase of the mud film converts free water into bound water, reducing high-temperature effluent.
It significantly reduces or avoids the problem of high-temperature water discharge from mud films, ensuring product stability, maintaining production efficiency and quality, and at a low cost.
Smart Images

Figure CN120154537B_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of cosmetics, and more specifically, to a mud mask, its preparation method, and its application. Background Technology
[0002] Mud masks, as a daily skin care product, are loved by consumers for their excellent oil absorption and skin cleansing abilities, and have gradually become a part of consumers' daily skin care routine.
[0003] During the research and development of mud films, high-temperature stability is a crucial evaluation target (typically set at 45℃ for 3 months). During stability observation, most mud films on the market exhibit water seepage, severely impacting product quality. This issue is common to this formulation, and there's no significant way to improve it. Current conventional solutions involve adding ingredients to prevent powder aggregation, such as magnesium aluminum silicate, or increasing the mud film's consistency. However, these methods only alleviate the water seepage problem to a certain extent; if the product itself contains excessive powder, these solutions are very limited.
[0004] In view of this, the present invention is proposed. Summary of the Invention
[0005] The purpose of this invention is to provide a mud film, its preparation method, and its application.
[0006] This invention is implemented as follows: In a first aspect, embodiments of the present invention provide a mud film composition comprising an oil phase component and an aqueous phase component; the aqueous phase component comprises a first silica; the first silica comprises porous silica.
[0007] Secondly, embodiments of the present invention provide a method for preparing a mud film, which includes mixing the mud film composition described in the foregoing embodiments.
[0008] Thirdly, embodiments of the present invention provide a mud film prepared by the preparation method described in the foregoing embodiments.
[0009] Fourthly, embodiments of the present invention provide the application of porous silica in the preparation of mud films, wherein the porous silica is the first silica described in the foregoing embodiments.
[0010] The present invention has the following beneficial effects: This invention, by adding porous silica to the aqueous phase component of mud film raw materials, can convert free water in the mud film formulation into bound water, thereby avoiding or significantly reducing the problem of high-temperature water discharge from mud film. Moreover, this solution is simple and easy to implement, does not affect the production and efficacy of mud film, and can solve the problem of high-temperature water discharge from mud film at low cost, providing a way for high-quality production of mud film. Attached Figure Description
[0011] To more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings used in the embodiments will be briefly introduced below. It should be understood that the following drawings only show some embodiments of the present invention and should not be regarded as a limitation on the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.
[0012] Figure 1 The water effluent from the mud film (Comparative Example 1) after one month of high-temperature stability without the addition of porous, highly adsorbent materials (now restored to room temperature) is shown in the red box, which represents the water precipitated during high-temperature stability. Figure 2 The effluent condition of the mud film (Example 1) after one month of high-temperature stability (after returning to room temperature) with the addition of 0.5% porous silica. Figure 3 The image shows the effluent from the mud film in Comparative Example 4. Figure 4 The image shows the effluent from the mud film in Comparative Example 5. Detailed Implementation
[0013] To make the objectives, technical solutions, and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below. Where specific conditions are not specified in the embodiments, conventional conditions or conditions recommended by the manufacturer shall apply. Reagents or instruments whose manufacturers are not specified are all conventional products that can be purchased commercially.
[0014] This invention discovers that by adding porous silica to the aqueous phase component of the mud film raw material, free water in the mud film formulation can be converted into bound water, which can avoid or significantly reduce the problem of high-temperature water discharge from the mud film. When using samples for verification, without the addition of porous silica, water discharge problems appeared after one month of high-temperature stability testing; after adding porous silica, the water discharge problem was solved after one month of high-temperature stability testing, and the high-temperature stability test was passed after three months.
[0015] The solution provided by this invention is simple to implement and has significant effects. There is almost no free water precipitation after high temperature, and the entire paste is fine and uniform. It does not affect the production process and efficacy of mud film, and can solve the problem of high-temperature water discharge of mud film at low cost, providing a way for high-quality production of mud film.
[0016] Specific technical solutions On one hand, embodiments of the present invention provide a mud film composition comprising an oil phase component and an aqueous phase component; the aqueous phase component comprises a first silica, wherein the first silica comprises porous silica.
[0017] In some embodiments, the first silica includes silica obtained by a vapor phase process.
[0018] In some embodiments, the first silica includes AEROSIL® 200.
[0019] In some embodiments, the aqueous phase component includes: water, polyol, illite mica, potassium sodium aluminum silicate, second silica, anionic emulsifier, EDTA-2Na, and the first silica.
[0020] In some embodiments, the polyol includes any one or more of 1,3-propylene glycol, glycerol, propylene glycol, butylene glycol, dipropylene glycol, and methylpropylene glycol.
[0021] In some embodiments, the anionic emulsifier includes any one or more of sodium stearoyl glutamate, potassium cetyl phosphate, and potassium lauryl phosphate.
[0022] In some embodiments, the aqueous phase component comprises, by weight, 20-50 parts water, 5-10 parts polyol, 15-20 parts illite mica, 7-10 parts potassium sodium aluminum silicate, 7-10 parts second silica, 0.1-1 parts anionic emulsifier, 0.01-1 parts EDTA-2Na and 0.1-1 parts the first silica.
[0023] Specifically, the weight percentage of water can be any one or any two of the following: 20, 22, 24, 26, 28, 30, 32, 34, 36, 38, 40, 42, 44, 46, 48, and 50 parts. The weight percentage of polyol can be any one or any two of the following: 5, 6, 8, and 10 parts. The weight percentage of illite mica can be any one or any two of the following: 15, 16, 18, and 20 parts. The weight percentage of potassium sodium aluminum silicate can be any one or any two of the following: 7, 8, 9, and 10 parts. The weight percentage of secondary silica can be any one or any two of the following: 7, 8, 9, and 10 parts. The weight percentage of anionic emulsifier can be any one or any two of the following: 0.1, 0.2, 0.4, 0.6, 0.8, and 1 part. The weight percentages of EDTA-2Na can be any one or any two of the following: 0.01, 0.05, 0.1, 0.2, 0.4, 0.6, 0.8, and 1 part. The weight percentages of the first silica can be any one or any two of the following: 0.1, 0.2, 0.4, 0.6, 0.8, and 1 part.
[0024] In some embodiments, the second silica comprises silica prepared by a precipitation process.
[0025] In some embodiments, the oil phase component includes: emulsifier, co-emulsifier, oil, and titanium dioxide.
[0026] In some embodiments, the oil phase component comprises, by weight, 2 to 8 parts emulsifier, 1 to 5 parts co-emulsifier, 5 to 15 parts oil and grease, and 1 to 5 parts titanium dioxide.
[0027] Specifically, the emulsifier can be any one or any two of the following weight parts: 2, 4, 6, or 8 parts. The co-emulsifier can be any one or any two of the following weight parts: 1, 2, 3, 4, or 5 parts. The oil can be any one or any two of the following weight parts: 5, 6, 8, 10, 12, 14, or 15 parts. The titanium dioxide can be any one or any two of the following weight parts: 1, 2, 3, 4, or 5 parts.
[0028] In some embodiments, the emulsifier comprises any one or more of the following: glyceryl stearate, PEG-100 stearate, sorbitan stearate, cetearyl oleate, sorbitan oleate, sorbitan sesquioleate, sorbitan caprylate, PEG-40 stearate, cetearyl glucoside, and C12-20 PEG-8 ester.
[0029] In some embodiments, the co-emulsifier includes any one or more of cetearyl alcohol, cetyl alcohol, stearyl alcohol, and behenyl alcohol.
[0030] In some embodiments, the oil comprises any one or more of the following: C9-12 alkylene, coconut oil alcohol-caprylate / capric acid ester, caprylic / capric acid triglyceride, ethylhexyl palmitate, hydrogenated polyisobutylene, squalane, dioctyl carbonate, neopentyl glycol diheptanoate, isohexadecane, triglyceride (ethylhexanoate), polydimethylsiloxane, phenyl polytrimethylsiloxane, trimethylsiloxane-oxyphenyl polydimethylsiloxane, and diphenyl polydimethylsiloxane.
[0031] In some embodiments, the titanium dioxide comprises CI 77891.
[0032] In some embodiments, the mud film composition further includes excipients.
[0033] In some embodiments, the excipients include any one or more of preservatives and other active ingredients; the other active ingredients include any one or more of purslane extract, dipotassium glycyrrhizate, and Sophora flavescens root extract.
[0034] In some embodiments, the preservative includes any one or more of phenoxyethanol, methylparaben, methylisothiazolinone, p-hydroxyacetophenone, and 1,2-hexanediol.
[0035] In some embodiments, the other active ingredients in the mud film composition are present in a weight percentage of 1% to 5%, and the preservatives are present in a weight percentage of 0.1% to 5%.
[0036] On the other hand, embodiments of the present invention also provide a method for preparing a mud film, which includes mixing the mud film composition described in any of the foregoing embodiments.
[0037] In some embodiments, the step of mixing the mud film composition includes: first mixing the aqueous phase component in the mud film composition to obtain an aqueous phase, and mixing the oil phase component to obtain an oil phase; and then emulsifying the oil phase and the aqueous phase.
[0038] In some embodiments, the step of mixing the aqueous phase components includes: heating the mixture to 80-90°C to obtain the aqueous phase. Specifically, this temperature can be any one or a range between any two of 80, 82, 84, 86, 88, and 90°C.
[0039] In some embodiments, the first silica and water in the aqueous phase are first mixed, and then other aqueous phase components are added. After mixing, the mixture is heated to 80-90°C to obtain the aqueous phase. The mixing time of the first silica and water can be 1-30 min, specifically any one or any two of 1, 5, 10, 15, 20, 25, and 30 min.
[0040] In some embodiments, the step of mixing the oil phase components includes: heating the mixture to 80-90°C to obtain the oil phase. Specifically, this temperature can be any one or a range between any two of 80, 82, 84, 86, 88, and 90°C.
[0041] In some embodiments, prior to the mixing and emulsification, the preparation method further includes holding the aqueous phase at 80–90°C for 10–20 min. The holding time can be any one or a range between any two of 10, 12, 14, 16, 18, and 20 min. The holding temperature can be any one or a range between any two of 80, 82, 84, 86, 88, and 90°C.
[0042] In some embodiments, when the mud film composition further includes the excipients described in any of the foregoing embodiments, the preparation method further includes: after performing the mixing and emulsification, cooling the emulsion product to 40~60°C and adding the excipients.
[0043] In some embodiments, the step of adding the excipients includes: First, cool the emulsified product to 50~60℃, add preservatives, stir evenly, and obtain the first product; the specific temperature can be any one or any two of 50, 52, 54, 56, 58, and 60℃. The temperature of the first product is lowered to 40-50℃, other active ingredients are added, and the mixture is stirred evenly to obtain the second product; the temperature can be any one or any two of 40, 42, 44, 46, 48, and 50℃. The second product is cooled to 35-45°C, stirring is stopped, and the final product is obtained. This temperature can be any one or any two of 35, 36, 38, 40, 42, 44, and 45°C.
[0044] On the other hand, embodiments of the present invention also provide a mud film, which is prepared by the preparation method described in any of the foregoing embodiments.
[0045] Furthermore, embodiments of the present invention also provide the application of porous silica in the preparation of mud films, wherein the porous silica is the first silica described in any of the foregoing embodiments.
[0046] The features and performance of the present invention will be further described in detail below with reference to embodiments.
[0047] The first silica used in this example is trade name: AEROSIL® 200; standard Chinese name: silica. Manufacturer: Evonik Specialty Chemicals (Shanghai) Co., Ltd. The production process of this raw material can be simply described as follows: silicon tetrachloride is burned at high temperature with hydrogen and air to produce colloidal silica and hydrogen chloride gas, which are then separated to obtain the product.
[0048] The example uses a mixed raw material (Illite hydromica, potassium sodium aluminum silicate, and secondary silica). Trade name: GM-800; Standard Chinese name: Illite hydromica, potassium sodium aluminum silicate, silica. Manufacturer: Anhui Gree New Material Technology Co., Ltd. The production process of this raw material can be simply described as follows: raw ore --- wet grinding --- classification and purification --- heavy metal removal --- pressure filtration and dehydration --- drying and packaging --- finished product.
[0049] The examples used a mixed raw material (glycerol stearate and PEG-100 stearate). Trade name: SP ARLACEL170 MBAL-PA-(SG); Standard Chinese names: glycerol stearate, PEG-100 stearate. Manufacturer: Croda Chemicals (Shanghai) Co., Ltd. The production process of this raw material can be simply described as follows: glycerol stearate and PEG-100 stearate are mixed and filtered.
[0050] The examples used a mixed feedstock (C9-12 alkylene, coconut oil alcohol-octanoate / decanoate). Trade name: Vegelight 1214 LC; Standard Chinese name: C9-12 alkylene, coconut oil alcohol-octanoate / decanoate. Manufacturer: BIOSYNTHIS. The production process of this feedstock can be simply described as follows: coconut oil alcohol-octanoate / decanoate is blended with C9-12 alkylene to obtain the final product.
[0051] Example 1 This embodiment provides a mud film, the composition of which and its preparation method are as follows.
[0052] Table 1. Mud film formulation
[0053] The mud film was prepared using the formula shown in Table 1, and the preparation method is as follows: (1) Preparation of aqueous phase Add water from component A to a beaker, add the first silica to the water, and stir and disperse with a stirrer (IKA® RW20digital) for about 20 minutes to allow the fumed silica to come into full contact with the water, converting a small amount of free water into bound water. Then add the other raw materials of the aqueous phase and heat to 85°C to obtain the aqueous phase. (2) Preparation of oil phase Component B was added to a fuel tank and stirred to disperse it. The temperature was then raised to 85°C to obtain the oil phase. (3) Emulsification The aqueous phase is pumped into the emulsification tank, kept at 85°C for 20 minutes, and the emulsification stirring is started. The oil phase is drawn into the emulsification tube, and homogenization emulsification is started; (4) Adding excipients After emulsification is complete, turn on the cooling water and when the temperature drops to 55°C, add component C (preservative) and stir well. Continue cooling to 45℃, then add phase D (other active ingredients) and stir until homogeneous; Continue cooling to 37℃, stop stirring, take samples for testing, and discharge the material after it passes the test.
[0054] Example 2 This embodiment provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those in Example 1. The difference is that the raw material 1,3-propylene glycol in Example 1 is replaced with butanediol, as shown in Table 2.
[0055] Table 2. Mud film formulation .
[0056] Example 3 This embodiment provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those in Example 1. The difference is that in this embodiment, raw material No. 13, caprylic / capric triglyceride, is replaced with ethylhexyl palmitate.
[0057] Table 3. Mud film formulation .
[0058] Example 4 This embodiment provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those in Example 1. The difference is that in this embodiment, raw material No. 12, polydimethylsiloxane, is replaced with phenyl polytrimethylsiloxane.
[0059] Table 4. Mud film formulation .
[0060] Example 5 This embodiment provides a mud film and its preparation method. The formula and preparation method of the mud film are roughly the same as those in Embodiment 1. The difference is that in this embodiment, the amount of first silica added is 0.1%; the amount of water is adjusted accordingly, and the total mass of the mud film is the same as that in Embodiment 1.
[0061] Table 5. Mud film formulation .
[0062] Example 6 This embodiment provides a mud film and its preparation method. The formula and preparation method of the mud film are roughly the same as those in Example 1. The difference is that in this embodiment, the amount of first silica added is 0.8%; the amount of water is adjusted accordingly, and the total mass of the mud film is the same as that in Example 1.
[0063] Table 6. Mud Film Formulation .
[0064] Comparative Example 1 This comparative example provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those in Example 1. The difference is that no first silica was added in Comparative Example 1; the amount of water was adjusted accordingly; and the total mass of the mud film was the same as that in Example 1.
[0065] Table 7. Mud Film Formulation .
[0066] Comparative Example 2 This comparative example provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those of Example 2. The difference is that no first silica was added in Comparative Example 2; the amount of water was adjusted accordingly; and the total mass of the mud film was the same as that of Example 2.
[0067] Table 8. Mud Film Formulation .
[0068] Comparative Example 3 This comparative example provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those in Example 1. The difference is that in Comparative Example 3, the first silica is replaced with the second silica.
[0069] Table 9. Mud Film Formulation .
[0070] Comparative Example 4 This comparative example provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those in Example 1. The difference is that in Comparative Example 4, the first silica is replaced with magnesium aluminum silicate.
[0071] Table 10 Mud Film Formulation .
[0072] Comparative Example 5 This comparative example provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those in Example 1. The difference is that in Comparative Example 5, the first silica is replaced with modified corn starch.
[0073] Table 11 Mud Film Formulation .
[0074] Comparative Example 6 This comparative example provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those of Example 1. The difference is that the amount of first silica added in Comparative Example 6 is 5%; the amount of water is adjusted accordingly; and the total mass of the mud film is the same as that of Example 1.
[0075] The addition of silica in Comparative Example 6 made the material very thick and hard, making it difficult to stir and impossible to prepare a mud film.
[0076] Comparative Example 7 This comparative example provides a mud film and its preparation method. The formulation and preparation method of the mud film are roughly the same as those in Example 1. The difference is that in Comparative Example 7, the first silica is used as the oil phase component for preparation.
[0077] Verification Example The mud films from Examples 1-6 and Comparative Examples 1-5 and 7 were subjected to high-temperature stability tests. The test method included placing the mud films in 250g plastic bottles and setting up control and experimental groups respectively. The control group was placed in a room-temperature, light-protected environment, while the laboratory group was placed in a 45°C oven for one month and three months respectively.
[0078] The test results are as follows.
[0079] Examples 1, 2, 3, 4, and 6 passed the high-temperature stability test after 1 and 3 months, while Examples 5 and Comparative Examples 1, 2, 3, 4, 5, and 7 failed the high-temperature stability test after 1 and 3 months.
[0080] Figure 1 The water effluent from the mud membrane (Comparative Example 1) after one month of high-temperature stability (after returning to room temperature) without the addition of porous, highly adsorbent materials is shown in the red box. Figure 2 With the addition of 0.5% silica, the effluent from this mud film (Example 1) after one month of high-temperature stability (after returning to room temperature) shows that the material is fine and no water has been released. The effluent from Comparative Examples 4-5 is shown below. Figures 3-4 .
[0081] The above description is merely a preferred embodiment of the present invention and is not intended to limit the invention. Various modifications and variations can be made to the present invention by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of the present invention should be included within the scope of protection of the present invention.
Claims
1. A pack composition, characterized by, It consists of an oil phase component, an aqueous phase component, and auxiliary materials; By weight, the aqueous phase component comprises the following: 20-50 parts water, 5-10 parts polyol, 15-20 parts illite mica, 7-10 parts potassium sodium aluminum silicate, 7-10 parts second silica, 0.1-1 parts anionic emulsifier, 0.01-1 parts EDTA-2Na, and 0.4-1 parts first silica, wherein the first silica is AEROSIL® 200, and the second silica is silica prepared by a precipitation process; The oil phase component, by weight, consists of: 2 to 8 parts emulsifier, 1 to 5 parts co-emulsifier, 5 to 15 parts oil and fat, and 1 to 5 parts titanium dioxide.
2. The mud film composition according to claim 1, wherein The polyols include any one or more of 1,3-propylene glycol, glycerol, propylene glycol, butylene glycol, dipropylene glycol, and methylpropylene glycol.
3. The mud film composition according to claim 1, characterized in that, The anionic emulsifier includes any one or more of sodium stearoyl glutamate, potassium cetyl phosphate, and potassium lauryl phosphate.
4. The mud film composition according to claim 1, characterized in that, The emulsifier includes any one or more of the following: glyceryl stearate, PEG-100 stearate, sorbitan stearate, cetearyl oleate, sorbitan oleate, sorbitan sesquioleate, sorbitan caprylate, PEG-40 stearate, cetearyl glucoside, and C12-20 PEG-8 ester.
5. The mud film composition according to claim 1, characterized in that, The co-emulsifier includes any one or more of cetearyl alcohol, cetyl alcohol, stearyl alcohol, and behenyl alcohol.
6. The mud film composition according to claim 1, characterized in that, The oils include any one or more of the following: C9-12 alkylene, coconut oil alcohol-caprylate / capric acid ester, caprylic / capric acid triglyceride, ethylhexyl palmitate, hydrogenated polyisobutylene, squalane, dioctyl carbonate, neopentyl glycol diheptanoate, isohexadecane, triglyceride (ethylhexanoate), polydimethylsiloxane, phenyl polytrimethylsiloxane, trimethylsiloxane-oxyphenyl polydimethylsiloxane, and diphenyl polydimethylsiloxane.
7. The mud film composition according to claim 1, characterized in that, The titanium dioxide includes CI 77891.
8. The mud film composition according to claim 1, characterized in that, The excipients include any one or more of preservatives and other active ingredients; the other active ingredients include any one or more of purslane extract, dipotassium glycyrrhizate, and Sophora flavescens root extract.
9. The mud film composition according to claim 8, characterized in that, The preservatives include any one or more of phenoxyethanol, methylparaben, methylisothiazolinone, p-hydroxyacetophenone, and 1,2-hexanediol.
10. The mud film composition according to claim 8, characterized in that, In the mud film composition, the weight percentage of the other active ingredients is 1% to 5%.
11. A method for preparing a mud film, characterized in that, It includes mixing the mud film composition according to any one of claims 1 to 10.
12. The preparation method according to claim 11, characterized in that, The steps of mixing the mud film composition include: first mixing the aqueous phase components in the mud film composition to obtain an aqueous phase, and mixing the oil phase components to obtain an oil phase; and then emulsifying the oil phase and the aqueous phase.
13. The preparation method according to claim 12, characterized in that, The step of mixing the aqueous components includes: heating the mixture to 80~90℃ to obtain the aqueous phase.
14. The preparation method according to claim 13, characterized in that, The steps for mixing the aqueous phase components include: first mixing the first silica and water in the aqueous phase, then adding other aqueous phase components, and then heating the mixture to 80~90℃ to obtain the aqueous phase.
15. The preparation method according to claim 12, characterized in that, The step of mixing the oil phase components includes: heating the mixture to 80~90℃ to obtain the oil phase.
16. The preparation method according to claim 12, characterized in that... Before performing the mixing and emulsification, the preparation method further includes keeping the aqueous phase at 80-90°C for 10-20 minutes.
17. The preparation method according to claim 12, characterized in that, When the mud film composition further includes the excipients as described in any one of claims 9 to 10, the preparation method further includes: after performing the mixing and emulsification, cooling the emulsion product to 40 to 60°C and adding the excipients.
18. The preparation method according to claim 17, characterized in that, When the excipients include preservatives and other active ingredients, the steps of adding the excipients include: first, cooling the emulsified product to 50-60°C, adding preservatives, stirring evenly to obtain a first product; then, lowering the temperature of the first product to 40-50°C, adding other active ingredients, stirring evenly to obtain a second product; and finally, cooling the second product to 35-45°C to obtain a mud film.
19. A mud film, characterized in that, It is prepared by the preparation method described in any one of claims 11 to 18.
Citation Information
Patent Citations
Cosmetic and use thereof
JP2004149463A