一种高压低损耗介质材料及其制备方法

By optimizing the composition and manufacturing process of the dielectric material in high-voltage ceramic capacitors, the problems of low dielectric constant, high loss, and poor stability of the dielectric material have been solved, enabling efficient and stable high-voltage applications.

CN120535306BActive Publication Date: 2026-07-17KUNSHAN QINGYUAN ELECTRONIC TECHNOLOGY CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
KUNSHAN QINGYUAN ELECTRONIC TECHNOLOGY CO LTD
Filing Date
2025-05-30
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing high-voltage ceramic capacitors have low dielectric constants, high dielectric losses, poor withstand voltage and high-temperature stability, and contain harmful elements, making it difficult to maintain stable performance under high frequency and high electric field conditions.

Method used

Using barium titanate, strontium titanate, bismuth oxide, etc. as the main raw materials, and by doping with Nb2O5, Y2O3, Sb2O3, etc., the crystal structure and sintering process are optimized, the grains are refined, the dielectric constant is increased and the dielectric loss is reduced, and the mechanical properties and thermal stability are enhanced.

Benefits of technology

This invention achieves dielectric materials with high dielectric constant, low dielectric loss, high withstand voltage, and high temperature stability, suitable for high-voltage ceramic capacitors, thus improving capacitor efficiency and reliability.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

本发明提供一种高压低损耗介质材料及其制备方法,涉及高压陶瓷电容器技术领域,其原料按质量份计包括钛酸钡35‑38份、钛酸锶20‑29.5份、二氧化钛15‑17.5份、氧化铋9‑12份、氧化锆3‑4份、X 0.8‑1.0份、氧化锑1.2‑1.4份、碳酸钙1‑1.2份等。所述介质材料的制备方法,包括以下步骤;将碳酸钙、氧化镁、氧化锌等熔融后水淬、球磨造粒,得到锌硼硅玻璃粉;将锌硼硅玻璃粉与钛酸钡、钛酸锶、二氧化钛等混合均匀,造粒后得到氧化物粉料;将氧化物粉料压片烧结,得到高压低损耗介质材料。本发明的高压低损耗介质材料的介电常数高,介电损耗小,耐压强度高,高温稳定性好,且制备方法简单。