微纳磁性介质密封装置和泄漏率检测方法

By welding the sealing pole shoe to the outer shell gap and using a helium mass spectrometer leak detector, the error problem of detecting the leakage rate of magnetic liquid seals under low temperature conditions was solved, and accurate detection of micro-nano magnetic media seals was achieved.

CN120608957BActive Publication Date: 2026-07-17TSINGHUA UNIVERSITY

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
TSINGHUA UNIVERSITY
Filing Date
2025-05-19
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing technologies, under extreme conditions such as low temperatures, cause errors in the detection results of magnetic liquid seal leakage rate due to leakage of static sealing components, making it impossible to accurately detect the leakage rate of micro-nano magnetic media seals.

Method used

The gap between the pole shoe and the outer shell is sealed by welding. A helium mass spectrometer leak detector is used to detect gas leaks on the low-pressure side. A multi-step detection method is used to ensure the accuracy of the detection and to seal the leakage channel at the rubber ring seal.

Benefits of technology

It improves the detection accuracy of micro-nano magnetic media seals under extreme working conditions, provides a stable and reliable basis for operation, and ensures the accuracy of detection results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120608957B_ABST
    Figure CN120608957B_ABST
Patent Text Reader

Abstract

本发明公开了一种微纳磁性介质密封装置和泄漏率检测方法。所述装置包括外壳、端盖、转轴、第一极靴、磁性件和第二极靴。所述方法包括:将未加工的第一极靴装入外壳,通过焊接的方式密封后检测是否泄漏,若无泄漏,将磁性件和未加工的第二极靴依次装入外壳,通过焊接的方式密封后检测是否泄漏,若无泄漏,对未加工的第一极靴和第二极靴的开孔并加工极齿,向极齿上加注微纳磁性介质,将外壳、第一极靴、磁铁、第二极靴安装在转轴上,将端盖安装在外壳上,在低压侧检测磁性密封处的泄漏率。本发明利用焊接的方法封堵相关技术中极靴与外壳之间的橡胶圈密封处的泄漏通道,使得检测的泄漏率即为微纳磁性介质密封的泄漏率。