Laser welding quality detection method and system
By acquiring equipment operating parameters and real-time image data during laser welding, and combining adaptive topology learning and a welding defect recognition layer, the welding quality is dynamically evaluated. This solves the problem of low detection accuracy caused by offline analysis in existing technologies and improves the detection capability of hidden defects.
Patent Information
- Application Number
- CN202510912305.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-07-03
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2045-07-03
AI Technical Summary
Current laser welding quality inspection methods are mostly offline, which cannot monitor the molten pool state and heat-affected zone in real time. This results in low accuracy in identifying defects such as incomplete fusion and porosity, and lacks adaptability to complex components, affecting production yield and efficiency.
By connecting to a laser welding machine to obtain equipment operating parameters, and combining this with adaptive topology learning to establish a welding quality evaluation model, real-time image data is acquired using image acquisition equipment, and a welding defect identification layer is embedded to dynamically evaluate welding quality.
It enables dynamic monitoring of the entire welding process, improves the detection accuracy of latent defects, and provides strong support for the optimization of laser welding processes.
Smart Images

Figure CN120755556B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of quality inspection technology, and in particular to laser welding quality inspection methods and systems. Background Technology
[0002] Laser welding offers advantages such as small weld seams, minimal deformation, high quality, and high welding speed, and is used in fields such as aerospace, electronics, and automotive. Weld quality is a key factor in evaluating the performance and reliability of welded joints, and it directly affects the safety and lifespan of products.
[0003] Currently, conventional laser welding monitoring systems are usually offline and cannot access dynamic image data such as the state of the molten pool and the heat-affected zone in real time. The accuracy of identifying typical defects such as incomplete fusion and porosity is insufficient and lags behind the welding process. In addition, since the welding parameters are set based on experience or fixed process specifications, they lack adaptability to the differences in the structure of combined welded products and the changes in the shape of small welding points. In the welding of complex components, misjudgments and omissions often occur, which seriously affect the production yield and efficiency.
[0004] In summary, existing laser welding quality inspection technologies mostly rely on offline analysis, making it difficult to effectively detect latent defects such as cooling shrinkage cracks and residual stress accumulation. Summary of the Invention
[0005] The purpose of this application is to provide a laser welding quality inspection method and system to solve the technical problem that existing laser welding quality inspection methods are mostly offline analyses, making it difficult to effectively detect latent defects such as cooling shrinkage cracks and residual stress accumulation.
[0006] In view of the above problems, this application provides a laser welding quality inspection method and system.
[0007] In a first aspect, this application provides a laser welding quality inspection method, which is implemented through a laser welding quality inspection system. The method includes: connecting a laser welding machine and acquiring equipment operating parameters, including laser power, welding time points, and shielding gas flow rate; establishing a welding quality evaluation model based on historical operating parameter sets corresponding to the preheating stage, the welding stage, and the cooling stage, combined with adaptive topology learning; the welding quality evaluation model is used to dynamically evaluate the welding quality of each welding point; determining a welding defect identification layer based on welding defect records in a laser welding database, where welding defect types include incomplete fusion, porosity, slag inclusions, and cracks; acquiring real-time image data during the welding process using an image acquisition device; uploading the real-time image data to the welding defect identification layer, where the real-time image data includes the molten pool state and the heat-affected zone; embedding the welding defect identification layer into the welding quality evaluation model, and determining the welding quality inspection result based on the equipment operating parameters.
[0008] Secondly, this application also provides a laser welding quality inspection system for performing the laser welding quality inspection method as described in the first aspect, wherein the system includes: an operating parameter acquisition module, which is connected to a laser welding machine to acquire equipment operating parameters, including laser power, welding time points, and shielding gas flow rate; and an evaluation model establishment module, which is used to establish a welding quality evaluation model based on historical operating parameter sets corresponding to the preheating stage, the welding stage, and the cooling stage, combined with adaptive topology learning, wherein the welding quality evaluation model is used for dynamic... The system evaluates the welding quality at each welding point; an image acquisition module, which, based on welding defect records in a laser welding database, determines a welding defect identification layer defined by welding defect types, including incomplete fusion, porosity, slag inclusions, and cracks. Using an image acquisition device, it acquires real-time image data during the welding process and uploads this data to the welding defect identification layer. The real-time image data includes the molten pool state and the heat-affected zone. A quality inspection result acquisition module embeds the welding defect identification layer into the welding quality evaluation model and, in conjunction with the equipment operating parameters, determines the welding quality inspection result.
[0009] One or more technical solutions provided in this application have at least the following technical effects or advantages: By establishing welding operation nodes corresponding to each welding point based on the weld seam in a laser welding process, and connecting a laser welding machine to acquire equipment operating parameters including laser power, welding time nodes, and shielding gas flow rate, a welding quality evaluation model is established based on historical operating parameter sets corresponding to the preheating, welding, and cooling stages, combined with adaptive topology learning. This model dynamically evaluates the welding quality of each welding point. Based on welding defect records in the laser welding database, a welding defect identification layer is determined, defined by welding defect types including incomplete fusion, porosity, slag inclusions, and cracks. Real-time image data during the welding process is acquired using image acquisition equipment and uploaded to the welding defect identification layer, which includes the molten pool state and heat-affected zone. The welding defect identification layer is embedded into the welding quality evaluation model, and combined with the equipment operating parameters, the welding quality detection result is determined. This achieves the technical effect of dynamically monitoring the entire welding process by collecting equipment operating parameters from the preheating, welding, and cooling stages, improving the detection accuracy of latent defects, and providing strong support for the optimization of laser welding processes.
[0010] The above description is merely an overview of the technical solution of this application. To better understand the technical means of this application and to facilitate its implementation according to the description, and to make the above and other objects, features, and advantages of this application more apparent, specific embodiments of this application are described below. It should be understood that the content described in this section is not intended to identify key or important features of the embodiments of this application, nor is it intended to limit the scope of this application. Other features of this application will become readily apparent through the following description. Attached Figure Description
[0011] To more clearly illustrate the technical solutions in this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are merely exemplary. For those skilled in the art, other drawings can be obtained based on the provided drawings without creative effort.
[0012] Figure 1 This is a flowchart illustrating the laser welding quality inspection method of this application.
[0013] Figure 2 This is a schematic diagram of the laser welding quality inspection system of this application.
[0014] Figure labeling: Module 11 for obtaining running parameters, Module 12 for establishing evaluation models, Module 13 for image acquisition, and Module 14 for obtaining quality detection results. Detailed Implementation
[0015] This application provides a laser welding quality inspection method and system, which solves the technical problem that laser welding quality inspection is mostly based on offline analysis, making it difficult to effectively detect latent defects such as cooling shrinkage cracks and residual stress accumulation. It achieves the technical effect of improving the detection accuracy of latent defects by collecting equipment operating parameters during the preheating, welding, and cooling stages and dynamically monitoring the entire welding process, thus providing strong support for the optimization of laser welding processes.
[0016] The technical solutions of this application will now be clearly and completely described with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of this application, and not all of them. It should be understood that this application is not limited to the exemplary embodiments described herein. All other embodiments obtained by those skilled in the art based on the embodiments of this application without creative effort are within the scope of protection of this application. It should also be noted that, for ease of description, only the parts related to this application are shown in the accompanying drawings, not all of them.
[0017] Example 1 Please see the appendix Figure 1 This application provides a laser welding quality inspection method, wherein the method is applied to a laser welding quality inspection system, and the method specifically includes the following steps: S1: Connect to the laser welding machine and obtain the equipment operating parameters, including laser power, welding time point, and shielding gas flow rate.
[0018] Specifically, connect the laser welding machine to a host computer, such as a PC, using a suitable data cable or communication interface. Data transmission can be performed using interfaces such as USB, RS232, or Ethernet. Open the control software and establish a connection with the laser welding machine. Locate the device parameter options to access the device parameter settings interface. Device operating parameters include laser power, welding time points, and shielding gas flow rate. The laser power displays the current output power of the laser. This parameter determines the energy density and welding speed during welding. The welding time points display data at various key time points during the welding process, such as welding start time and end time.
[0019] The protective gas flow rate display shows the flow rate of the protective gas. The protective gas plays a role in preventing oxidation and protecting the quality of the weld during the welding process.
[0020] S2: Based on the historical operating parameter set corresponding to the preheating stage, the historical operating parameter set corresponding to the welding stage, and the historical operating parameter set corresponding to the cooling stage, a welding quality evaluation model is established by combining adaptive topology learning. The welding quality evaluation model is used to dynamically evaluate the welding quality of each welding point.
[0021] Specifically, outliers, duplicates, and missing values are removed to ensure data accuracy and completeness. Features highly correlated with welding quality, such as laser power, welding speed, and shielding gas flow rate, are selected. The relationship between parameter variations and welding quality in historical data is analyzed to learn the topological structure of the data. As new data is continuously added, the model can automatically adjust its topological structure to adapt to new data distributions and feature relationships. Features representative of welding quality are extracted using statistical methods, signal processing techniques, or machine learning algorithms. For example, features can be extracted by calculating the fluctuation range of laser power and the distribution of welding time. Machine learning algorithms, such as Support Vector Machines (SVM), Random Forests, or Neural Networks, are selected to train the model. The preprocessed historical data is used as the training set to train a model capable of predicting welding quality. The preprocessed dataset is divided into training and validation sets. The model is trained using the training set, and its performance is optimized by adjusting the model's parameters and structure. The model is evaluated using an independent test set to test its performance in practical applications. Precision, recall, and other metrics are calculated to assess the model's predictive ability. During the actual welding process, the operating parameters of each welding point are collected in real time. Real-time data is input into the trained model to obtain predicted welding quality values for each welding point. Based on the prediction results, welding parameters are adjusted or other measures are taken in a timely manner to improve welding quality.
[0022] S3: Based on the welding defect records in the laser welding database, determine the welding defect identification layer under the limitation of welding defect types. The welding defect types include incomplete fusion, porosity, slag inclusion, and cracks. Use an image acquisition device to acquire real-time image data during the welding process and upload the real-time image data to the welding defect identification layer. The real-time image data includes the state of the molten pool and the heat-affected zone.
[0023] Specifically, the types of welding defects to be detected are clearly defined, typically including lack of fusion, porosity, slag inclusions, and cracks. These defects have a significant impact on the quality and performance of the welded joint, thus requiring timely and accurate identification and treatment. Historical image data containing various welding defects is extracted from a laser welding database. This data will be used to train and validate the welding defect recognition model. Based on the characteristics of the welding defects, appropriate image recognition and machine learning algorithms are selected to build the recognition model. For example, convolutional neural networks in deep learning can be used to train the model, enabling it to automatically identify welding defects from image data. The trained model is validated using an independent validation set to evaluate its accuracy and reliability in identifying welding defects. The model is then adjusted and optimized as necessary based on the validation results. High-resolution, high-speed image acquisition equipment is used to capture image data of key areas such as the molten pool state and heat-affected zone in real time during the welding process. The real-time image data is uploaded to the welding defect recognition layer for processing. This is achieved through wired or wireless network connections to ensure the real-time nature and accuracy of the data.
[0024] S4: Embed the welding defect identification layer into the welding quality evaluation model, and determine the welding quality inspection result by combining the equipment operating parameters.
[0025] Specifically, a welding defect identification layer is embedded into the welding quality evaluation model. When evaluating welding quality, the identification results of welding defects are considered simultaneously. It is ensured that the welding defect identification layer can receive real-time image data from the image acquisition device and output the identification results to other parts of the welding quality evaluation model. It is ensured that the data from welding operation nodes and the acquisition of real-time image data are synchronized in time to accurately correspond to the operation and potential defects at each welding stage. Data from welding operation nodes, such as welding speed, welding current, and voltage, are combined with the welding defect identification results to analyze the potential correlation between operation and defects. Operating parameters of the welding equipment during the welding process, such as laser power, shielding gas flow rate, and welding head movement trajectory, are collected. These equipment operating parameters are compared and analyzed with the welding defect identification results to identify equipment operation modes or parameter settings that may lead to defects. A comprehensive evaluation of welding quality is performed by considering the welding defect identification results, welding operation node data, and equipment operating parameters. For example, if a serious welding defect is identified and the equipment operating parameters show unstable laser power, then the welding quality can be judged as poor.
[0026] Furthermore, this application also includes: The welding stages are determined by classifying the operating status of the equipment operating parameters. The welding stages include a preheating stage, a welding stage, and a cooling stage. The laser welding database is connected, and data is extracted based on the welding stages to obtain the historical operating parameter sets corresponding to the preheating stage, the welding stage, and the cooling stage.
[0027] Specifically, the welding stages are determined by classifying the operating status of the equipment's operating parameters, including the preheating stage, welding stage, and cooling stage. A laser welding database is then connected, and data extraction is performed based on these welding stages to obtain the corresponding historical operating parameter sets. Specifically, classifying the operating status of the equipment's operating parameters refers to determining the welding stage based on real-time changes in parameters such as laser power, welding time points, and shielding gas flow rate, according to preset classification rules. Connecting to the laser welding database involves establishing a communication link with a database storing a large amount of historical welding data to extract the required data. Data extraction involves filtering the corresponding historical operating parameter set from the database based on the determined welding stage for subsequent model building and other operations.
[0028] By monitoring the operating status of equipment parameters, the welding stages are divided. This process accurately divides the entire welding process into three stages: preheating, welding, and cooling. This provides a clear timeline for subsequent targeted quality inspection and model building. Precisely dividing the welding stages improves the controllability of the welding process. Connecting to the laser welding database and extracting the historical operating parameter sets corresponding to each stage provides a wealth of past welding experience data. Combining this with the current welding process provides massive data support for building a welding quality evaluation model with learning and predictive capabilities.
[0029] Furthermore, the method described in this application also includes obtaining the set of historical operating parameters corresponding to the welding stage: Based on the laser welding process, welding operation nodes are set for each welding point based on the weld seam. A parameter time series matrix is constructed based on the welding operation nodes corresponding to each welding point and the equipment operating parameter sequence corresponding to each welding point. Based on the parameter time series matrix and combined with welding process standards, welding quality influencing factors are configured. These welding quality influencing factors are strongly correlated with the input layer weights and node activation functions of the welding quality evaluation model.
[0030] Specifically, along the weld seam and according to welding process requirements, a series of specific welding operation points are determined on the weld seam, and each point is assigned a corresponding welding operation instruction, such as setting points for parameters like welding speed and laser power. Furthermore, the equipment operation parameter sequence refers to a sequence of parameter values arranged chronologically at each welding operation node, such as the sequence of laser power changes over time at a certain welding point. Constructing a parameter time-series matrix integrates the equipment operation parameter sequences of each welding point into a matrix form, where rows represent different welding points and columns represent parameter values at various time points, thus forming a multi-dimensional data structure. This helps to present parameter changes during the welding process in the form of a mathematical model, facilitating subsequent analysis and processing. Welding quality influencing factors refer to the characteristic quantities of parameters or combinations of parameters that significantly affect welding quality. The strong correlation between these factors and the input layer weights and node activation functions of the welding quality evaluation model means that these influencing factors will directly affect the model's evaluation results for welding quality; that is, the model will judge the quality of welding based on the weights and activation functions of these factors.
[0031] First, welding operation nodes are set based on the laser welding process to ensure refined management of the welding process. Precise welding operations can be performed at each critical position of the weld. Then, a parameter time series matrix is constructed based on the welding operation nodes and equipment operating parameter sequences. This effectively integrates parameter change information during the welding process and transforms the welding process into a quantifiable and analyzable data structure. Preferably, by constructing the parameter time series matrix, the equipment operating parameter sequences of multiple welding points are integrated. Each equipment operating parameter sequence contains parameter values corresponding to timestamps, providing a detailed data foundation for subsequent quality analysis.
[0032] Finally, based on the parameter time series matrix and combined with the welding process standard configuration of welding quality influencing factors, the data in the parameter time series matrix is used to mine features that have a significant impact on welding quality, and these features are associated with the input layer weights and node activation functions of the evaluation model. This enables the model to more accurately evaluate welding quality. Preferably, by configuring the welding quality influencing factors, the accuracy of welding quality assessment is improved. Through the above steps, key data support and model optimization basis are provided for establishing an accurate welding quality evaluation model, ensuring the accuracy and reliability of welding quality detection.
[0033] Furthermore, this application also includes: Based on the requirements of laser welding, a collaborative operation strategy is set for each welding point and the welding robot arm; the laser welding machine and the robot arm control system are connected, and welding parameter-robot arm trajectory information is obtained in combination with the collaborative operation strategy; the welding quality detection results obtained are dynamically evaluated through the welding quality evaluation model, and welding collaborative operation is performed based on the welding parameter-robot arm trajectory information.
[0034] Specifically, the location of each welding point is determined based on the workpiece structure and welding requirements. For each welding point, the robotic arm's movement trajectory is planned to ensure the laser welding head can accurately and efficiently reach and complete the welding task. Appropriate parameters such as laser power, welding speed, and welding distance are set according to the workpiece's material and thickness. The welding parameters are ensured to match the robotic arm trajectory for high-quality welding. The laser welding machine and robotic arm control system are connected through appropriate interfaces and protocols. Stable and real-time data transmission between the two is ensured. Welding parameters and robotic arm trajectory information are synchronized to the control system. The laser welding machine and robotic arm can operate collaboratively according to the set parameters and trajectory. Specific welding parameters, such as laser power and welding speed, are set in the control system. The robotic arm's trajectory information, including the coordinates and movement path of each welding point, is input. The accuracy of the welding parameters and robotic arm trajectory is verified through simulation or test runs. Parameters and trajectories are adjusted until the expected results are achieved. During the welding process, the welding quality is dynamically evaluated using a welding quality evaluation model. Various parameters during the welding process, such as weld morphology and molten pool condition, are monitored in real time. Based on feedback from the quality evaluation model, welding parameters or robotic arm trajectories are adjusted in real time to ensure that welding quality remains within the preset standard range.
[0035] Furthermore, this application also includes: The temperature and stress field distribution of the current welding area are monitored in real time using real-time monitoring equipment. Based on the temperature and stress field distribution of the current welding area, the microstructure and mechanical properties of the welded joint are predicted. According to the prediction results, welding adjustment parameters are obtained, and the welding adjustment parameters meet the laser welding process parameters corresponding to the laser welding requirements.
[0036] Specifically, high-precision temperature and stress sensors are installed in the welding area to monitor temperature and stress changes in real time during the welding process. The sensors transmit the collected temperature and stress data to a data processing system. Using the real-time temperature and stress field data, combined with the physical properties of the welding material and a thermodynamic model of the welding process, the microstructure changes of the weld joint are simulated and analyzed. Based on the processed data, a predictive model of the weld joint's microstructure and mechanical properties is established using numerical simulation techniques or machine learning algorithms. This model can predict the microstructure and potential mechanical properties of the weld joint based on the current temperature and stress field distribution. Based on the predicted microstructure and mechanical properties output by the model, the quality of the joint under the current welding parameters is analyzed to determine whether it meets expectations. If not, adjustments are needed. Based on the prediction results and analysis, the algorithms determine the welding parameters that need adjustment. These parameters include laser power, welding speed, and welding sequence. The goal of the adjustment is to ensure that the microstructure and mechanical properties of the weld joint meet the requirements of laser welding.
[0037] Furthermore, this application also includes: The target welding product is identified, including combined welding products and micro welding products; based on the target welding product, the layout of each welding point corresponding to the laser welding process is optimized, and the welding operation node is updated.
[0038] Specifically, after identifying the target product to be welded, the layout of the laser welding process and the welding operation nodes can be optimized and updated based on the product's characteristics. The connection methods and welding requirements between various components must be identified. The components requiring welding, as well as the strength and sealing requirements, must be determined. Based on the product structure, the layout of welding points should be rationally planned to reduce welding deformation and stress concentration. The welding sequence should be optimized to ensure uniform heat distribution during the welding process, avoiding hot cracking and residual stress. Based on the layout optimization results, the position and sequence of welding operation nodes should be adjusted. Clear operating instructions and quality control standards should be ensured for each welding operation node. For micro-welded products, higher welding precision is required, therefore precise positioning of welding points is essential. High-precision positioning and fixture equipment should be used to ensure the stability and accuracy of the welding process. The layout of welding points should be optimized for the characteristics of micro-products to reduce the heat-affected zone and welding deformation. Micro-welding technology or laser micro-welding can be used to improve welding quality and precision. Based on the characteristics of the micro-products and the layout optimization results, the parameter settings of the welding operation nodes, such as laser power and welding speed, should be adjusted. Strengthen quality control and inspection of welding operation nodes to ensure that the welding quality of each node meets the requirements of micro products.
[0039] Furthermore, this application also includes: The welding component structure of the combined welding product is obtained, the welding component structure including multiple welding components; based on the welding component structure, structurally differentiated laser welding process parameters are set; the structurally differentiated laser welding process parameters are used as constraint information and added to the welding defect identification layer for real-time classification and identification of welding defects, and a first-class identification result is obtained.
[0040] Specifically, the detailed structure of the welded components of the assembled welded product is obtained, including the material, thickness, shape, and connection method of each welded component. The welded components are classified according to their structural characteristics, such as thickness and material type. For different categories of welded components, appropriate laser welding process parameters are determined based on their structural characteristics. These parameters include laser power, welding speed, spot diameter, and welding angle. The initially determined process parameters are optimized through simulation to ensure welding quality and efficiency. Structurally differentiated laser welding process parameters are added as constraint information to the welding defect identification layer. Differences in process parameters between different welded components are considered when identifying welding defects. During the welding process, the updated welding defect identification layer is used to classify and identify welding defects in real time. After real-time classification and identification, a single identification result is output, representing the specific type of welding defect identified based on the welded component structure and differentiated process parameters.
[0041] Furthermore, this application also includes: Based on the micro-welding product, the changes in the shape of the welding point are output synchronously; based on the changes in the shape of the welding point, distributed welding point process parameters are set; the distributed welding point process parameters are used as constraint information and added to the welding defect identification layer to perform real-time classification and identification of welding defects, and obtain two types of identification results.
[0042] Specifically, a high-resolution camera system or sensor is used to monitor the morphological changes of weld points in micro-welded products in real time. This includes the formation of weld points, the dynamics of the molten pool, and the fusion of the weld joint. The monitored weld point morphological change data is recorded in real time. Based on the real-time monitoring and recording of weld point morphological change data, the formation process and characteristics of the weld points are analyzed. Corresponding distributed weld point process parameters are set for different weld point morphologies and change characteristics. These parameters include fine-tuning of laser power, adjustment of welding speed, and the spacing and arrangement of weld points. These distributed weld point process parameters are added as new constraint information to the welding defect identification layer. Thus, when identifying welding defects, both the morphological changes of the weld points and the corresponding process parameters are considered simultaneously. The welding defect identification layer is ensured to receive and process these new process parameters for more accurate real-time classification and identification of welding defects. During the welding process, the updated welding defect identification layer, combined with the distributed weld point process parameters, is used to classify and identify welding defects in real time. Two types of identification results are output: the specific welding defect type identified based on the morphological changes of the weld points in the micro-welded product and the distributed process parameters.
[0043] Furthermore, this application also includes: A critical recognition margin is set according to the structurally differentiated laser welding process parameters; an initial population is obtained based on each welding point, and a search space is set according to the critical recognition margin; based on the initial population, the layout of each welding point is optimized within the search space, and the welding operation node is updated after the layout optimization is completed.
[0044] Specifically, based on the structurally differentiated laser welding process parameters, a critical recognition margin is set. This margin is a threshold used to determine the acceptable adjustment range of the welding point layout during the optimization process. It should be reasonably set according to specific welding requirements and product quality standards to ensure a balance between welding quality and recognition accuracy. Based on the current welding points, an initial welding point layout scheme is obtained, which constitutes the initial population. Each welding point is considered an individual in this initial population. Next, a search space is set according to the critical recognition margin. This search space defines the range and method that the welding points can be adjusted during the optimization process. For example, the maximum movement distance of each welding point in a specific direction can be set, or the minimum and maximum spacing between welding points can be set. After setting the initial population and search space, optimization algorithms, such as genetic algorithms and particle swarm optimization, are used to find the optimal welding point layout within the search space. During this process, the algorithm continuously adjusts the position of the welding points to seek the optimal solution that satisfies all welding requirements and process parameter constraints. After the layout optimization is completed, an optimized welding point layout scheme is obtained. Based on this plan, the welding operation details are updated, including the specific location of each welding point, the welding sequence, and the laser welding process parameters used. These updates should be accurately reflected in the welding operation plan to ensure that the actual welding process proceeds according to the optimized plan.
[0045] In summary, the laser welding quality inspection method provided in this application has the following technical advantages: A laser welding machine is connected to acquire its operating parameters, including laser power, welding time points, and shielding gas flow rate. Based on historical operating parameter sets corresponding to the preheating, welding, and cooling stages, and combined with adaptive topology learning, a welding quality evaluation model is established. This model dynamically assesses the welding quality at each welding point. Based on welding defect records in the laser welding database, a welding defect identification layer is determined, defined by welding defect types, including incomplete fusion, porosity, slag inclusions, and cracks. Real-time image data during the welding process is acquired using an image acquisition device and uploaded to the welding defect identification layer. This real-time image data includes the molten pool state and the heat-affected zone. The welding defect identification layer is embedded into the welding quality evaluation model, and combined with the equipment operating parameters, the welding quality detection result is determined. This achieves the technical effect of dynamically monitoring the entire welding process by collecting equipment operating parameters during the preheating, welding, and cooling stages, improving the detection accuracy of hidden defects, and providing strong support for the optimization of laser welding processes.
[0046] Example 2 Based on the laser welding quality inspection method described in the foregoing embodiments, and using the same inventive concept, this application also provides a laser welding quality inspection system. Please refer to the appendix. Figure 2 The system includes: The operating parameter acquisition module 11 is used to connect to the laser welding machine and acquire the equipment operating parameters, including laser power, welding time node, and shielding gas flow rate.
[0047] The evaluation model establishment module 12 is used to establish a welding quality evaluation model based on the historical operating parameter set corresponding to the preheating stage, the historical operating parameter set corresponding to the welding stage, and the historical operating parameter set corresponding to the cooling stage, combined with adaptive topology learning. The welding quality evaluation model is used to dynamically evaluate the welding quality of each welding point.
[0048] Image acquisition module 13 is used to determine a welding defect identification layer under the limitation of welding defect type based on welding defect records in the laser welding database. The welding defect type includes incomplete fusion, porosity, slag inclusion, and crack. The image acquisition module 13 uses an image acquisition device to acquire real-time image data during the welding process and uploads the real-time image data to the welding defect identification layer. The real-time image data includes the state of the molten pool and the heat-affected zone.
[0049] The quality inspection result acquisition module 14 is used to embed the welding defect identification layer into the welding quality evaluation model and determine the welding quality inspection result in combination with the equipment operating parameters.
[0050] Furthermore, the system includes: The welding stages are determined by classifying the operating status of the equipment operating parameters. The welding stages include a preheating stage, a welding stage, and a cooling stage. The laser welding database is connected, and data is extracted based on the welding stages to obtain the historical operating parameter sets corresponding to the preheating stage, the welding stage, and the cooling stage.
[0051] Furthermore, the system also includes: Based on the laser welding process, welding operation nodes are set for each welding point based on the weld seam. A parameter time series matrix is constructed based on the welding operation nodes corresponding to each welding point and the equipment operating parameter sequence corresponding to each welding point. Based on the parameter time series matrix and combined with welding process standards, welding quality influencing factors are configured. These welding quality influencing factors are strongly correlated with the input layer weights and node activation functions of the welding quality evaluation model.
[0052] Furthermore, the system also includes: Based on the requirements of laser welding, a collaborative operation strategy is set for each welding point and the welding robot arm; the laser welding machine and the robot arm control system are connected, and welding parameter-robot arm trajectory information is obtained in combination with the collaborative operation strategy; the welding quality detection results obtained are dynamically evaluated through the welding quality evaluation model, and welding collaborative operation is performed based on the welding parameter-robot arm trajectory information.
[0053] Furthermore, the system also includes: The temperature and stress field distribution of the current welding area are monitored in real time using real-time monitoring equipment. Based on the temperature and stress field distribution of the current welding area, the microstructure and mechanical properties of the welded joint are predicted. According to the prediction results, welding adjustment parameters are obtained, and the welding adjustment parameters meet the laser welding process parameters corresponding to the laser welding requirements.
[0054] Furthermore, the system also includes: The target welding product is identified, including combined welding products and micro welding products; based on the target welding product, the layout of each welding point corresponding to the laser welding process is optimized, and the welding operation node is updated.
[0055] Furthermore, the system also includes: The welding component structure of the combined welding product is obtained, the welding component structure including multiple welding components; based on the welding component structure, structurally differentiated laser welding process parameters are set; the structurally differentiated laser welding process parameters are used as constraint information and added to the welding defect identification layer for real-time classification and identification of welding defects, and a first-class identification result is obtained.
[0056] Furthermore, the system also includes: Based on the micro-welding product, the changes in the shape of the welding point are output synchronously; based on the changes in the shape of the welding point, distributed welding point process parameters are set; the distributed welding point process parameters are used as constraint information and added to the welding defect identification layer to perform real-time classification and identification of welding defects, and obtain two types of identification results.
[0057] Furthermore, the system also includes: A critical recognition margin is set according to the structurally differentiated laser welding process parameters; an initial population is obtained based on each welding point, and a search space is set according to the critical recognition margin; based on the initial population, the layout of each welding point is optimized within the search space, and the welding operation node is updated after the layout optimization is completed.
[0058] The various embodiments in this specification are described in a progressive manner, with each embodiment focusing on its differences from other embodiments. Figure 1 The laser welding quality inspection method and specific examples in Embodiment 1 are also applicable to the laser welding quality inspection system of this embodiment. Through the foregoing detailed description of the laser welding quality inspection method, those skilled in the art can clearly understand the laser welding quality inspection system of this embodiment; therefore, for the sake of brevity, it will not be described in detail here. As for the system disclosed in the embodiments, since it corresponds to the method disclosed in the embodiments, the description is relatively simple; relevant details can be found in the method section.
[0059] The above description of the disclosed embodiments enables those skilled in the art to make or use this application. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of this application. Therefore, this application is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features disclosed herein.
[0060] Obviously, those skilled in the art can make various modifications and variations to this application without departing from the spirit and scope of this application. Therefore, if such modifications and variations fall within the scope of this application and its equivalents, this application also intends to include such modifications and variations.
Claims
1. A laser welding quality inspection method, characterized in that, The method includes: Connect to the laser welding machine and obtain the equipment operating parameters, including laser power, welding time point, and shielding gas flow rate; Based on the historical operating parameter sets corresponding to the preheating stage, the welding stage, and the cooling stage, a welding quality evaluation model is established by combining adaptive topology learning. The welding quality evaluation model is used to dynamically evaluate the welding quality of each welding point. Based on welding defect records in the laser welding database, a welding defect identification layer is determined under the limitation of welding defect types, including incomplete fusion, porosity, slag inclusion, and cracks. Using an image acquisition device, real-time image data of the welding process is acquired and uploaded to the welding defect identification layer. The real-time image data includes the state of the molten pool and the heat-affected zone. The welding defect identification layer is embedded into the welding quality evaluation model, and the welding quality inspection results are determined in combination with the equipment operating parameters.
2. The laser welding quality inspection method as described in claim 1, characterized in that, The method includes: The welding stage is determined by classifying the operating status of the equipment based on the operating parameters. The welding stage includes the preheating stage, the welding stage, and the cooling stage. Connect to the laser welding database and extract data based on the welding stage to obtain the historical operating parameter set corresponding to the preheating stage, the historical operating parameter set corresponding to the welding stage, and the historical operating parameter set corresponding to the cooling stage.
3. The laser welding quality inspection method as described in claim 2, characterized in that, The method further includes obtaining a set of historical operating parameters corresponding to the welding stage. Based on the laser welding process, welding operation nodes are set for each welding point based on the weld seam. Based on the welding operation nodes corresponding to each welding point as the weld seam, and the equipment operation parameter sequence corresponding to each welding point, a parameter time series matrix is constructed. Based on the parameter time series matrix and combined with welding process standards, welding quality influencing factors are configured. These welding quality influencing factors are strongly correlated with the input layer weights and node activation functions of the welding quality evaluation model.
4. The laser welding quality inspection method as described in claim 2, characterized in that, To determine the welding quality inspection results, the method further includes: Based on the requirements of laser welding, a collaborative operation strategy between each welding point and the welding robot arm is set. Connect the laser welding machine and the robotic arm control system, and combine the aforementioned collaborative operation strategy to obtain welding parameters-robotic arm trajectory information; The welding quality inspection results obtained by the dynamic evaluation of the welding quality evaluation model are used to perform welding collaborative operation based on the welding parameters and robotic arm trajectory information.
5. The laser welding quality inspection method as described in claim 4, characterized in that, The method further includes acquiring real-time image data of the welding process using an image acquisition device. The temperature and stress field distribution in the current welding area is monitored in real time using real-time monitoring equipment. Based on the temperature and stress field distribution in the current welding area, the microstructure and mechanical properties of the welded joint are predicted. Based on the prediction results, welding adjustment parameters are obtained, which satisfy the laser welding process parameters corresponding to the laser welding requirements.
6. The laser welding quality inspection method as described in claim 3, characterized in that, Based on the laser welding process, the method further includes: Identify the target welding product, which includes combined welding products and micro-welding products; Based on the target welding product, the layout of each welding point corresponding to the laser welding process is optimized, and the welding operation node is updated.
7. The laser welding quality inspection method as described in claim 6, characterized in that, The target welded product includes a combined welded product, and the method includes: Obtain the welding assembly structure of a combined welded product, the welding assembly structure comprising multiple welded components; Based on the structure of the welding assembly, structurally differentiated laser welding process parameters are set. The structurally differentiated laser welding process parameters are used as constraint information and added to the welding defect identification layer to perform real-time classification and identification of welding defects, thereby obtaining a type of identification result.
8. The laser welding quality inspection method as described in claim 6, characterized in that, The target welded product includes micro-welded products, and the method further includes: Based on micro-welding products, the changes in the shape of the welding point are output synchronously; Based on the changes in the welding point morphology, process parameters for distributed welding points are set. The process parameters of the distributed welding points are used as constraint information and added to the welding defect identification layer to perform real-time classification and identification of welding defects, and obtain two types of identification results.
9. The laser welding quality inspection method as described in claim 7, characterized in that, The method includes optimizing the layout of each welding point corresponding to the laser welding process and updating the welding operation nodes. In accordance with the aforementioned structurally differentiated laser welding process parameters, a critical recognition margin is set, wherein the critical recognition margin is a threshold used to determine the acceptable adjustment range of the welding point layout during the optimization process; Based on each welding point, an initial population is obtained, and a search space is set according to the critical recognition margin. Based on the initial population, the layout of each welding point is optimized within the search space, and the welding operation node is updated after the layout optimization is completed.
10. A laser welding quality inspection system, characterized in that, The system comprises: steps for implementing the method according to any one of claims 1 to 9 The operating parameter acquisition module is used to connect to the laser welding machine and acquire the equipment operating parameters, including laser power, welding time point, and shielding gas flow rate. The evaluation model establishment module is used to establish a welding quality evaluation model based on the historical operating parameter set corresponding to the preheating stage, the historical operating parameter set corresponding to the welding stage, and the historical operating parameter set corresponding to the cooling stage, combined with adaptive topology learning. The welding quality evaluation model is used to dynamically evaluate the welding quality of each welding point. An image acquisition module is used to determine a welding defect identification layer under the limitation of welding defect types based on welding defect records in the laser welding database. The welding defect types include incomplete fusion, porosity, slag inclusion, and cracks. The image acquisition module uses an image acquisition device to acquire real-time image data during the welding process and uploads the real-time image data to the welding defect identification layer. The real-time image data includes the state of the molten pool and the heat-affected zone. The quality inspection result acquisition module is used to embed the welding defect identification layer into the welding quality evaluation model and determine the welding quality inspection result in combination with the equipment operating parameters.
Citation Information
Patent Citations
Pre-welding process parameter determination method, welding quality online prediction method and device and storage medium
CN116618878A
Whole welding process quality regulation and control method of welding robot
CN119501241A