一种抗裂的多彩装饰涂料

By combining a specific ratio of continuous phase, base paint, and granulation solution with raw materials such as polyurethane-acrylic hybrid emulsion and toughening fibers, a toughened composite structure is formed, which solves the problem of insufficient crack resistance of multicolor decorative coatings under uneven deformation or impact, and achieves higher crack resistance.

CN120758149BActive Publication Date: 2026-07-17JIANGSU STAVANGER NEW MATERIALS CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
JIANGSU STAVANGER NEW MATERIALS CO LTD
Filing Date
2025-08-22
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing multicolor decorative coatings have insufficient crack resistance when faced with large, uneven deformation or impact, especially when encountering uneven substrate deformation or impact, they are difficult to resist effectively.

Method used

By using a specific ratio of continuous phase, base paint and granulation solution, combined with raw materials such as polyurethane-acrylic hybrid emulsion, toughening fiber, sericite powder and rubber powder, a toughened composite structure is formed. The crack resistance of the coating is improved by the "rigid-flexible" network of polyurethane-acrylic hybrid emulsion and the energy dissipation of plastic deformation of toughening fiber.

Benefits of technology

It significantly improves the crack resistance of multicolor decorative coatings to large, uneven deformation or impact, enhances the toughness and crack resistance of the coatings, and can better resist uneven deformation and impact.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005560294220000111
    Figure BDA0005560294220000111
Patent Text Reader

Abstract

本申请涉及建筑装饰材料的技术领域,具体公开了一种抗裂的多彩装饰涂料。该涂料包括:连续相60‑70%、基础漆25‑35%和造粒溶液5‑10%;连续相包括聚氨酯‑丙烯酸杂化乳液等原料;基础漆包括硅丙乳液、绢云母粉、增韧纤维、橡胶粉等原料;造粒溶液是粘度为2680‑3550mPa·s的硅酸镁锂水溶液。本申请采用具有特定原料配比的连续相、基础漆和造粒溶液,提高了多彩装饰涂料对较大的、不均匀的变形或冲击的抗裂性能。