一种整体壁板口框结构预弯应力精准施加装置及方法

By precisely controlling the pre-bending stress of the integral wall panel frame structure through the pre-bending punch and die device, the structural instability and deformation problems caused by inaccurate pre-bending stress in the existing technology are solved, thereby improving the shot peening forming accuracy and production efficiency of large aluminum alloy integral wall panels.

CN120791657BActive Publication Date: 2026-07-17AVIC XIAN AIRCRAFT IND GRP CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
AVIC XIAN AIRCRAFT IND GRP CO LTD
Filing Date
2025-08-12
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

In the existing technology for shot peening forming of large aluminum alloy integral wall panels, it is difficult to accurately apply the pre-bending stress in the frame structure area, which leads to structural instability and deformation, affecting forming accuracy and production efficiency.

Method used

A pre-bending punch and a pre-bending die device are used, which are fixed to the wall panel frame structure by fasteners to apply pre-bending stress. The pre-bending deformation is precisely controlled by combining three-dimensional modeling and finite element simulation calculation. The fitting surface of the pre-bending punch shim and the die shim with the wall panel is designed.

Benefits of technology

It enables precise application of pre-bending stress to the overall wall panel frame structure, suppresses abrupt changes in structural stiffness and instability, improves the accuracy and production efficiency of shot peening, and reduces the workload of subsequent alignment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120791657B_ABST
    Figure CN120791657B_ABST
Patent Text Reader

Abstract

本发明属于大型飞机整体壁板喷丸成形工装领域,具体是一种整体壁板口框结构预弯应力精准施加装置及方法。包括:预弯凸模垫片,其外形与预弯后壁板口框结构外凸外形一致,直接覆盖在预弯曲变形后的壁板口框上,预弯凹模垫片,其外形与预弯后壁板口框结构内凹外形一致,直接覆盖在与弯曲变形后的壁板口框上,预弯凸模,其外形与预弯凸模垫片外凸外形一致,位于所述预弯凸模垫片外侧,预弯凹模,其外形与预弯凹模垫片内凹外形一致,位于所述预弯凹模垫片外侧,使用紧固件拧紧该装置使整体壁板口框结构预弯变形产生预弯应力,解决整体壁板口框结构预弯应力精准施加问题和高效保护问题。
Need to check novelty before this filing date? Find Prior Art

Citation Information

Patent Citations

  • Prestress shot peening forming tool and method for large-curvature wallboard opening frame structure

    CN118357863A

  • Wallboard pre-stressed shot blasting sizing method and pre-bending fixture

    CN104588441A

  • Assistant mould for pre-forming aerial organic glass

    CN203063105U