A multi-field coupling test device and method for simulating deterioration of a seabed shield tunnel structure
By using a multi-field coupled test device and method to simulate the structural degradation of submarine shield tunnels, the problem of structural degradation under extreme erosion environments, which was not considered in traditional tunnel design, has been solved. This has enabled efficient simulation and evaluation of the structural degradation behavior of shield tunnels, and improved the scientific rigor and accuracy of the test.
Patent Information
- Application Number
- CN202511827455.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2025-12-05
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2045-12-05
AI Technical Summary
Traditional tunnel design theories have failed to effectively consider the structural deterioration of shield tunnels in extreme corrosive environments. In particular, undersea shield tunnels face the combined effects of high water and soil loads, high seepage water pressure, and high concentrations of corrosive ions, leading to phenomena such as steel corrosion and concrete cracking, which affect the long-term service life and safety of the structure.
A multi-field coupling test device and method for simulating the structural deterioration of submarine shield tunnels is provided. By applying circumferential constraint force, injecting corrosive liquid and applying an electric field, the multi-field coupling effect of micro electric field-high pressure seepage-continuous loading is simulated, and the structural deterioration behavior is monitored in real time.
It realistically simulates the complex working conditions in the actual service environment of submarine tunnels, significantly shortens the test cycle, improves simulation efficiency, and can monitor the deterioration behavior of the tunnel lining components in real time, providing an efficient assessment of the long-term durability performance of shield tunnels.
Smart Images

Figure CN121577518B_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of tunnel engineering testing technology, and in particular to a multi-field coupling test device and method for simulating the structural deterioration of submarine shield tunnels. Background Technology
[0002] Shield tunnels are the core structural form for modern urban underground engineering projects such as subways, highways, railways, water conservancy, and municipal pipelines. The long-term safety and durability of their permanent structure—the prefabricated segment lining—directly affects the operational safety of the entire underground network. Traditional tunnel design theory primarily focuses on the mechanical response of the segments under external soil and water loads, without considering the structural performance degradation during tunnel service and the resulting long-term structural safety issues. However, as underground space development expands towards greater burial depths, more complex geological conditions, and more extreme service environments, shield tunnel structures face severe challenges, mainly in the following aspects.
[0003] Extreme corrosive environments lead to the deterioration of tunnel lining structures: Tunnels operating in corrosive environments, such as undersea shield tunnels, face the combined effects of high soil and water loads, high permeability water pressure, and high concentrations of corrosive ions during their service life. Prefabricated segment linings inevitably experience steel corrosion, concrete cracking, and spalling. In particular, the superimposed effect of the physical-chemical field of the corrosive environment and the mechanical field of structural deterioration causes the tunnel's main structure (segment lining) to undergo a spiral-accelerated deterioration process, significantly shortening its service life.
[0004] The cascading hazards of joint leakage: The joints of tunnel segments are the first line of defense for waterproofing in shield tunnels, but also the weakest link. Under bending loads, structural deformation, and long-term loads, the joint sealant may fail, leading to leakage. Leaking water carries corrosive ions (such as chloride and sulfate ions) that penetrate into the concrete, inducing corrosion of bolts and joint reinforcement, deterioration of the concrete near the joint, and reduced joint stiffness and strength. This will increase structural deformation, weaken the cross-sectional safety redundancy, and seriously affect the long-term safety and serviceability of the tunnel structure. Summary of the Invention
[0005] This application provides a multi-field coupled test apparatus for simulating the structural deterioration of subsea shield tunnels, which enables the simulation and evaluation of the structural deterioration behavior of subsea shield tunnels under the coupled action of micro-electric field-high-pressure seepage-continuous loading. Furthermore, this application also provides a test method applicable to the aforementioned multi-field coupled test apparatus for simulating the structural deterioration of subsea shield tunnels.
[0006] To achieve the above objectives, this application provides the following technical solution: A multi-field coupled test device for simulating the structural deterioration of an underwater shield tunnel includes: The segment lining components are arranged in a ring, and the segment lining components are cast from concrete and steel bars set in the concrete. The hoop force application module includes a force application component disposed on the outer periphery of the segment lining member; The injection module includes a first sealing cap that seals a first end of the segment lining member, a second sealing cap that seals a second end of the segment lining member, a connecting rod assembly that connects the first sealing cap and the second sealing cap, and a water injection pump. The first sealing cap is located on top of the second sealing cap and has an injection hole. Water-stopping elements are provided between the first sealing cap and the segment lining member, and between the second sealing cap and the segment lining member. The first sealing cap, the second sealing cap, and the segment lining member enclose a sealed cavity. The data acquisition module includes an electrode array embedded in concrete, a resistivity acquisition instrument electrically connected to the electrode array, a water pressure sensor, a component internal force sensor, and a data acquisition instrument used in conjunction with the component internal force sensor. During the experiment, corrosive liquid was injected into the sealed cavity through the injection hole, and the injection pump was pressurized based on a preset permeation water pressure. The pressurized corrosive liquid drove the corrosive ions inside to migrate into the concrete, thereby inducing steel corrosion and concrete deterioration. The water permeation state, stress state and water pressure value inside the sealed cavity were monitored in real time by the data acquisition module.
[0007] Optionally, the multi-field coupling test device for simulating the structural deterioration of the submarine shield tunnel mentioned above also includes an electrochemical corrosion module. The electrochemical corrosion module includes a cathode component coaxially arranged with the segment lining component and a power supply for conducting the anode component and the cathode component. The anode component is composed of reinforcing steel bars. A DC electric field is applied between the anode component and the cathode component to drive the corrosion ions in the corrosive liquid to migrate directionally in the concrete, thereby accelerating the corrosion of the reinforcing steel bars and the deterioration of the concrete.
[0008] Optionally, in the above-mentioned multi-field coupling test device for simulating the structural deterioration of a submarine shield tunnel, the connecting rod assembly consists of multiple tension rods with telescopic functions.
[0009] Optionally, in the above-mentioned multi-field coupling test device for simulating the structural deterioration of a submarine shield tunnel, the force application component includes a metal strand wound around the outer peripheral wall of the segment lining member and a tensioning device for tensioning the metal strand.
[0010] Optionally, in the above-mentioned multi-field coupling test device for simulating the structural deterioration of a submarine shield tunnel, the segment lining component is composed of multiple annular segments combined along the axial direction of the segment lining component; or, the segment lining component is composed of multiple arc-shaped segments; or, the segment lining component is composed of a single annular segment.
[0011] Optionally, in the above-mentioned multi-field coupling test device for simulating the structural deterioration of submarine shield tunnels, the electrode array is embedded inside the concrete and distributed in an array along the circumference of the segment lining component.
[0012] Optionally, in the above-mentioned multi-field coupling test device for simulating the structural deterioration of submarine shield tunnels, the data acquisition module further includes distributed fiber optic sensors, which are arranged along the circumference of the segment lining component on the outer and inner circumferential walls of the segment lining component.
[0013] Optionally, in the above-mentioned multi-field coupling test device for simulating the structural deterioration of a submarine shield tunnel, the first sealing cover has a through hole, the second sealing cover has a groove on the side facing the sealing cavity, the cathode component passes through the through hole and is embedded in the groove, wherein the axis of the through hole and the groove coincides with the axis of the segment lining component.
[0014] Optionally, in the above-mentioned multi-field coupling test device for simulating the structural deterioration of a submarine shield tunnel, both the first sealing cover and the second sealing cover are made of metal, and both the first sealing cover and the second sealing cover are provided with an insulating layer on the side facing the sealing cavity, and an insulating seal is provided between the through hole and the cathode component.
[0015] A multi-field coupled test method for simulating the structural deterioration of an undersea shield tunnel, applicable to the multi-field coupled test apparatus for simulating the structural deterioration of an undersea shield tunnel as described in any of the above claims, and comprising: Step 1: Start the tensioning device and use the tensioning device to apply circumferential constraints to the segment lining member through the metal strands, and gradually increase the tension force according to the preset level until the uniform pressure on the outer peripheral wall of the segment lining member reaches the first preset value. Step 2: Start the water injection pump to inject corrosive liquid into the sealed cavity, and gradually pressurize the corrosive liquid inside the sealed cavity until the uniform water pressure on the inner peripheral wall of the segment lining component reaches the second preset value. Step 3: Connect the positive terminal of the power supply to the anode component and connect the negative terminal of the power supply to the cathode component. Step 4: Start the data acquisition module.
[0016] This application provides a multi-field coupled test device for simulating the structural deterioration of a submarine shield tunnel. It applies circumferential constraint force to the lining components using a hoop force application module, and injects corrosive liquid containing corrosive ions into a sealed cavity via an injection module. The injection pump is pressurized based on a preset seepage water pressure, causing the corrosive ions within the pressurized liquid to migrate into the concrete, thereby inducing steel corrosion and concrete deterioration. A data acquisition module monitors in real time the water seepage state, stress state, and water pressure within the sealed cavity of the lining components. This allows for the simulation and evaluation of the structural deterioration behavior of a submarine shield tunnel under the multi-field coupled action of micro-electric field – high-pressure seepage – continuous loading.
[0017] In this way, this application overcomes the problem of traditional tests that only consider the influence of a single factor, and realistically simulates the complex working conditions of high water pressure, low oxygen seawater infiltration, chloride ion corrosion, electrochemical corrosion of steel bars and continuous loading in the actual service environment of submarine tunnels; the electroosmotic pressure module accelerates the corrosion process of steel bars, significantly shortens the test cycle and improves simulation efficiency; through the setting of the data module, various state parameters of the tunnel lining components can be monitored in real time, thus reflecting the deterioration behavior of the tunnel lining components under multi-field coupling. Attached Figure Description
[0018] To more clearly illustrate the technical solutions in the embodiments of this application or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of this application. For those skilled in the art, other drawings can be obtained based on the provided drawings without creative effort.
[0019] Figure 1 This is a structural schematic diagram of the segment lining component provided in this application; Figure 2 A structural schematic diagram of a segment lining component consisting of a single annular segment provided in this application; Figure 3 A structural schematic diagram of a segment lining component composed of multiple annular segments provided in this application; Figure 4 A structural schematic diagram of a segment lining component composed of multiple arc-shaped segments provided in this application; Figure 5 A schematic diagram of the internal structure of the segment lining component provided in this application; Figure 6 Assembly process diagram of the segment lining components provided in this application; Figure 7 A schematic diagram of the arrangement of the water pressure sensors provided in this application; Figure 8 A schematic diagram of the electrode arrangement provided in this application; Figure 9 A schematic diagram of the fiber optic sensor arrangement provided in this application; Figure 10 A schematic diagram showing the radial pressure acting on the outer peripheral wall of the segment lining member provided in this application; Figure 11 A schematic diagram of the radial pressure acting on the inner circumferential wall of the segment lining member provided in this application; Figure 12 This is a schematic diagram of the segment lining member subjected to radial pressure provided in this application.
[0020] 1. Segment lining components; 2. Reinforcing bars; 3. First sealing cap; 4. Second sealing cap; 5. Connecting rod assembly; 6. Water injection hole; 7. Cathode component; 8. Electrode array; 9. Water pressure sensor; 10. Distributed fiber optic sensor; 11. Metal stranded wire; 12. Tensioning device; 13. Anchor bolts. Detailed Implementation
[0021] This application provides a multi-field coupled test apparatus for simulating the structural deterioration of subsea shield tunnels, which enables the simulation and evaluation of the structural deterioration behavior of subsea shield tunnels under the coupled action of micro-electric field-high-pressure seepage-continuous loading. Furthermore, this application also provides a test method applicable to the aforementioned multi-field coupled test apparatus for simulating the structural deterioration of subsea shield tunnels.
[0022] like Figures 1-12As shown, this application provides a multi-field coupling test device for simulating the structural deterioration of a submarine shield tunnel, comprising: a segment lining component 1 arranged in a ring, the segment lining component 1 being cast from concrete and steel reinforcement 2; a ring force application module, including a force application component disposed on the outer periphery of the segment lining component 1; and an injection module, including a first sealing cap 3 sealing the first end of the segment lining component 1, a second sealing cap 4 sealing the second end of the segment lining component 1, a connecting rod assembly 5 connecting the first sealing cap 3 and the second sealing cap 4, and a water injection pump. The first sealing cap 3 is located on top of the second sealing cap 4, and the first sealing cap 3 has an injection hole. An injection port is provided between the first sealing cap 3 and the segment lining component 1, and between the second sealing cap 4 and the segment lining component 1. A sealing cavity is formed by a water-stopping device, a first sealing cover 3, a second sealing cover 4, and a segment lining component 1. The data acquisition module includes an electrode array 8 embedded in the concrete, a resistivity acquisition instrument electrically connected to the electrode array 8, a water pressure sensor 9, a component internal force sensor, and a data acquisition instrument used in conjunction with the component internal force sensor. During the test, corrosive liquid is injected into the sealing cavity through the injection hole, and the injection pump is pressurized based on the preset permeation water pressure. The pressurized corrosive liquid drives the corrosive ions inside it to migrate into the concrete, thereby inducing the corrosion of the steel reinforcement 2 and the deterioration of the concrete. The data acquisition module monitors the water permeation state, stress state, and water pressure value inside the sealing cavity of the segment lining component 1 in real time.
[0023] It should be noted that the water-stopping component is a water-stopping rubber strip; the water injection pump is preferably a high-pressure water injection pump; the corrosive liquid isolates air to reduce the oxygen concentration on the lining surface, and the environment in which the segment lining component 1 is located is seawater or seawater prepared using chemical experiments. The corrosive liquid is a liquid containing specific corrosive ions, including Cl-. - SO4 2- Mg 2+ Water pressure sensor 9 is used to monitor the water pressure value of the corrosive liquid in the sealed cavity; electrode array 8 and resistivity acquisition instrument electrically connected to electrode array 8 are used to detect the water permeation state inside the segment lining component 1.
[0024] It should also be noted that the component internal force sensor is a distributed optical fiber sensor 10. The distributed optical fiber sensor 10 is arranged along the axial direction of the reinforcing bar 2 and along the circumferential direction on the inner and outer peripheral walls of the segment lining component 1. Preferably, the distributed optical fiber sensor 10 is arranged at equal intervals along the circumferential direction on the inner and outer peripheral walls of the segment lining component 1. The data acquisition instrument is an optical fiber demodulator. The component internal force sensor is used to sense the strain or internal force state of the segment lining component 1 under complex loads and environmental action. The matching data acquisition instrument is responsible for acquiring, converting and transmitting the signal. The two work together to realize real-time monitoring and quantitative evaluation of the structural mechanical performance.
[0025] Specifically, the segment lining component 1 is cast from concrete and reinforced steel 2, and serves as the test object of this application. The dimensions of the segment lining component 1 are proportionally scaled to the dimensions of the actual object to be simulated. Furthermore, the segments that enclose the segment lining component 1, as well as the joint structures between the segments, are designed according to the scale of actual engineering segments to simulate the prefabricated segment lining ring in a shield tunnel in actual engineering. Based on the thin-walled cylinder theory, this application applies external radial pressure and internal radial water pressure, transforming them, according to the principles of elasticity, into circumferential compressive stress (specific formulas will be explained later) and tensile stress (specific formulas will be explained later) on the cross-section of the segment lining component 1. Through their superposition, precise control of the complex stress state of the model cross-section is achieved, ensuring it reaches the pre-set stress state for the experiment.
[0026] It should be noted that the sealed cavity is filled with water and pressurized, which is not only used to generate circumferential tension in the segment lining component 1, but also serves as a seepage pressure to realistically simulate the leakage development process of key parts such as segment lining and joints under high water pressure. The stress state and seepage pressure environment are kept uniform in each scaled segment lining unit.
[0027] More specifically, the force-applying component is located on the outer peripheral wall of the segment lining member 1 and is used to apply radial constraint force to the outer peripheral wall of the segment lining member 1. Corrosive liquid is injected into the sealed cavity by a water pump to pressurize and apply radial hydrostatic pressure to the segment lining member 1, thereby applying circumferential tensile force and the required permeation water pressure within the segment lining specimen. By adjusting the difference between the circumferential pressure and the tensile force, water permeation within the segment lining is simultaneously achieved under a specified stress state and permeation water pressure.
[0028] It should be noted that when the force-applying component applies radial constraint force to the segment lining member 1, it can be applied in stages, and the pressure of the corrosive liquid injected into the sealed cavity by the water injection pump can also be gradually increased.
[0029] In this way, this application overcomes the problem of traditional tests that only consider the influence of a single factor, and realistically simulates the complex working conditions of high water pressure, low oxygen seawater infiltration, chloride ion corrosion, electrochemical corrosion of steel bar 2 and continuous load in the actual service environment of the submarine tunnel; the corrosion progress of steel bar 2 is accelerated by the electro-osmotic pressure module, which significantly shortens the test cycle and improves the simulation efficiency; through the setting of the data module, the various state parameters of the segment lining component 1 can be monitored in real time, so as to comprehensively reflect the deterioration behavior of segment lining component 1 under multi-field coupling.
[0030] Furthermore, the device also includes an electrochemical corrosion module, including a cathode 7 coaxially arranged with the segment lining component 1 and a power supply for conducting the anode and cathode 7. The reinforcing steel 2 constitutes the anode. A DC electric field is applied between the anode and cathode 7 to drive the corrosion ions in the corrosive liquid to migrate directionally in the concrete, thereby accelerating the corrosion of the reinforcing steel and the deterioration of the concrete.
[0031] A stable electric potential field is established between the positive terminal of a DC regulated power supply connected to steel bar 2 and the negative terminal connected to a copper rod, thereby creating a stable electric potential field between the sealed cavity and the corrosive liquid. Specifically, the negatively charged chloride ions (Cl-) in the corrosive liquid... - Under the influence of the electric field, the iron migrates directionally towards the anode (reinforcing bar 2). An electrochemical reaction of iron occurs on the surface of the anode (reinforcing bar 2): Fe → Fe 2+ + 2e - Meanwhile, chloride ions migrating to the surface of steel bar 2 disrupt the stability of the passivation film, forming a corrosion cell; on the surface of cathode 7 (copper rod), a hydrogen evolution and oxygen reduction reaction occurs. The entire system constitutes a complete electrolytic circuit. By adjusting the output voltage or current of the DC regulated power supply, the electric field strength is controlled, driving anions (such as chloride ions) in the corrosive liquid to migrate directionally towards the anode, achieving the following two functions: first, accelerating the penetration rate of the corrosive medium inside the concrete; and second, promoting the electrochemical corrosion reaction on the surface of steel bar 2. The electrochemical corrosion module works synchronously with the ring force application module and the injection module, forming a multi-field coupled test environment of micro-electric field-high pressure seepage-continuous loading, providing an efficient test method for studying the long-term durability evolution of shield tunnel segments under high water pressure. Furthermore, the data acquisition module is used to monitor the water penetration state and stress state inside the lining component 1 of the tunnel segment and the water pressure value in the sealed cavity in real time, realizing the simulation and evaluation of the structural deterioration behavior of the submarine shield tunnel under the multi-field coupled action of micro-electric field-high pressure seepage-continuous loading.
[0032] It should be noted that the cathode component 7 is a copper rod; the power supply is a DC regulated power supply.
[0033] The connecting rod assembly 5 consists of multiple telescopic tie rods. During the simulation experiment, the height of the segment lining component 1 is based on the simulated object, and there are instances where specific segments are disassembled during the simulation. It should be noted that when the segment lining component 1 is composed of multiple segments, it can be disassembled according to experimental requirements, which will result in different heights for the segment lining component 1. The tie rods have telescopic functionality, allowing their length to be dynamically adjusted according to changes in the number of assembled layers of the segment lining component 1 during the experiment, thus improving the practicality of the tie rods.
[0034] It should be noted that the outer peripheral wall of the tie rod is threaded, and the first sealing cover 3 and the second sealing cover 4 are firmly pressed against both ends of the segment lining component 1 by screwing them together with the anchor bolt 13.
[0035] In an optional embodiment, the force-applying component includes a metal strand 11 wound around the outer periphery of the tunnel lining member 1 and a tensioning device 12 for tensioning the metal strand 11. The metal strand 11 can be, but is not limited to, steel strand, and multiple metal strands 11 are provided. The tensioning device 12 can be, but is not limited to, a hydraulic jack or a servo-electric tensioner, and both ends of the metal strand 11 are connected to the tensioning device 12. By simultaneously tensioning all the metal strands 11 through the tensioning device 12, a uniform radial constraint force is applied to the tunnel lining member 1. This uniform radial constraint pressure, according to the thick-walled cylinder theory in elasticity, can be directly equivalent to a uniform circumferential compressive stress on the cross-section of the tunnel segment, facilitating the precise setting of the initial stress level and improving the repeatability and scientific validity of the test. At the same time, using the tensioning of steel strands to simulate external pressure replaces the complex multi-jack loading system, greatly reducing the cost and complexity of the device.
[0036] In this way, multiple metal strands 11 are tensioned simultaneously, ensuring that the radial pressure is continuously and symmetrically distributed along the circumference of the segment, avoiding local stress concentration, and truly replicating the mechanical characteristics of the confining pressure of the formation. The combination of metal strands 11 and tensioning device 12 is flexible and suitable for segment models of different sizes and reinforcement forms. Furthermore, the tensioning device 12 can be adjusted in real time to support graded loading and long-term load-bearing tests.
[0037] In optional embodiments, the segment lining component 1 is composed of multiple annular segments arranged along the axial direction of the segment lining component 1; or, the segment lining component 1 is composed of multiple arc-shaped segments; or, the segment lining component 1 is composed of a single annular segment. This can be understood as follows: when multiple annular segments are longitudinally connected in series, the influence of the longitudinal segment inter-ring splice joints on the seepage path can be examined; when further using arc-shaped segments and implementing staggered assembly, the more complex three-dimensional seepage behavior under staggered assembly conditions in actual engineering can be simulated. This design greatly expands the research dimensions and simulation capabilities of the experimental device.
[0038] In other alternative embodiments, the segment lining component 1 may also employ a single annular module, which is suitable for one-dimensional radial seepage analysis of the segment ring under simplified conditions.
[0039] The electrode array 8 is embedded inside the concrete and is distributed at equal intervals along the circumference of the segment lining component 1.
[0040] When the electrode array 8 is distributed circumferentially, it can identify the state of steel corrosion caused by leakage and local cracks at the joint.
[0041] The electrode array 8 can also be distributed in a grid pattern along the circumference, and the guide of the electrode array 8 is led out to the data acquisition instrument for inverting the water penetration depth and distribution through resistivity changes.
[0042] In other alternative embodiments, the electrode array 8 is embedded inside the concrete and is distributed in an array along the circumference of the segment lining member 1.
[0043] In an optional embodiment, the data acquisition module further includes distributed fiber optic sensors 10, arranged along the circumference of the segment lining member 1 on the outer and inner peripheral walls of the segment lining member 1. This is used to monitor the structural stress state and local strain changes.
[0044] In an optional embodiment, the first sealing cover 3 has a through hole, and the second sealing cover 4 has a groove on the side facing the sealing cavity. The cathode component 7 passes through the through hole and is embedded in the groove, wherein the axes of the through hole and the groove coincide with the axis of the segment lining component 1. Specifically, a smooth copper rod is vertically inserted into the groove from top to bottom, and during the insertion process, a special positioning clamp ensures that the axis of the copper rod always coincides with the central axis of the segment lining component 1. In this way, firstly, the symmetry and uniform distribution of the electric field are improved; secondly, the stability of the cathode component 7 in the sealing cavity is improved.
[0045] Both the first sealing cover 3 and the second sealing cover 4 are made of metal. An insulating layer is provided on the side of both the first sealing cover 3 and the second sealing cover 4 facing the sealing cavity, and an insulating seal is provided between the through hole and the cathode component 7. The insulating seal is preferably a high-pressure waterproof insulating seal. Specifically, the upper end of the copper rod (referring to the part facing away from the sealing cavity and protruding from the first sealing cover 3) is machined with external threads. After passing through the first sealing cover 3, it mates with the internal threaded hole of the high-pressure waterproof insulating seal. This insulating seal adopts a multi-layer structure design, consisting of a fluororubber sealing ring, a polytetrafluoroethylene insulating bushing, and a stainless steel compression flange from bottom to top. By symmetrically tightening the bolts on the compression flange, the sealing ring undergoes uniform radial deformation, achieving reliable sealing under high-pressure water conditions.
[0046] The insulating layer is an insulating layer sprayed on the inner surface (towards the sealing cavity) of the first sealing cover 3 and the second sealing cover 4.
[0047] In this way, electrical insulation and pressure sealing are achieved in high-pressure water environments.
[0048] It should be noted that both the first sealing cover 3 and the second sealing cover 4 are made of high-strength steel plates.
[0049] A multi-field coupled test method for simulating the structural deterioration of an undersea shield tunnel, applicable to the aforementioned multi-field coupled test apparatus for simulating the structural deterioration of an undersea shield tunnel, and comprising: Step 1: Start the tensioning device 12. Use the tensioning device 12 to apply circumferential constraints to the segment lining member 1 through the metal strand 11, and gradually increase the tension force according to the preset level until the uniform pressure (i.e., circumferential force) on the outer peripheral wall of the segment lining member 1 reaches the first preset value.
[0050] The surface of the predetermined monitoring points of the reinforcing bar 2 was treated by surface grinding and acetone cleaning. High-temperature epoxy adhesive was used to tightly bond the fiber optic grating sensor to the surface along the axial direction of the reinforcing bar 2. All fiber optic leads were fixed along the direction of the reinforcing bar 2 and centrally passed through the concrete protective layer, connecting to the fiber optic demodulator. Thus, the local strain of the reinforcing bar 2 was converted into changes in optical wavelength using the fiber optic grating sensor, and the fiber optic demodulator read and analyzed the FBG wavelength changes to output accurate strain data. After fabricating the concrete annular / arc module of the reinforcing bar 2, thanks to the modular assembly design of the device, various test conditions can be flexibly configured according to specific research objectives, such as a single annular segment, or multiple annular segments and multiple arc segments spliced together. When assembling the segment lining component 1, a joint waterproof gasket was installed at the joint according to the test requirements, thus obtaining the annular segment lining component 1. To monitor internal permeability, an electrode array 8 was pre-embedded in the segment lining component 1 in key sections (such as the joint influence zone). The electrodes were distributed in a grid pattern, and the wires were led out to the data acquisition instrument. The outer surface of the tunnel lining component 1 is ground to ensure its flatness in contact with the steel strands. Several distributed fiber optic sensors 10 are evenly arranged axially on the inner and outer walls of the tunnel lining component 1 to collect stress and deformation data. At the same time, a water pressure sensor 9 is installed at the bottom of the sealed cavity to accurately monitor the internal water pressure.
[0051] The segment lining component 1 is placed on top of the second sealing cover 4, with a water-stop strip between their mating surfaces. During installation, the center of the second sealing cover 4 and the segment lining component 1 must be strictly aligned to ensure accurate sealing surface alignment. Then, the first sealing cover 3 is placed on the segment lining component 1, again with a water-stop strip between their mating surfaces. Strict alignment is maintained during installation to ensure accurate sealing surface alignment. Finally, six high-strength, telescopic tie rods are used to symmetrically screw the first sealing cover 3 and the second sealing cover 4 onto them, ensuring the sealing reliability of the entire sealing cavity. A through hole, i.e., a copper rod insertion port, is precisely machined at the center of the first sealing cover 3. The smooth copper rod is inserted vertically from top to bottom, and a special positioning clamp is used during insertion to ensure that the axis of the copper rod always coincides with the central axis of the segment lining component 1. The upper end of the copper rod is machined with external threads, which, after passing through the sealing chamber cover, mate with the internal threaded hole of the insulating seal.
[0052] At the start of the test, the tensioning device 12 was activated to perform symmetrical, graded tensioning on the circumferentially uniformly arranged steel strands. The tensioning process adopted a force-controlled mode, with the load increasing gradually. Each load level lasted for 3-5 minutes, and the next level of loading was carried out after the data stabilized, until the preset external radial pressure value (i.e., the first preset value) was reached. During this stage, the segment lining member 1 was formed into a tight band in the radial direction, and a stable initial circumferential compressive stress field was established in its cross-section.
[0053] Step 2: Start the water injection pump to inject corrosive liquid into the sealed cavity, and gradually pressurize the corrosive liquid inside the sealed cavity until the uniform pressure (i.e., expansion force) on the inner peripheral wall of the segment lining component 1 reaches the second preset value. The reading of the water pressure sensor is the second preset value.
[0054] After the tunnel lining component 1 is pre-secured radially, the water injection pump is started, and corrosive liquid is injected into the sealed cavity through the two water injection holes 6 opened in the first sealing cover 3, gradually increasing the pressure until the predetermined stress state is reached. Distributed fiber optic sensors 10, arranged on the inner and outer surfaces of the tunnel lining component 1, collect strain and deformation data of the tunnel lining component 1 under load in real time, and analyze and invert the monitoring data based on elasticity theory to dynamically obtain the actual stress distribution state of the tunnel lining component 1. Figure 10 As shown, specifically, the circumferential stress (vertical principal stress of the normal section) inside the segment lining member 1 under the action of external pressure: ; ; ; Where: a is the inner radius; b is the outer radius; t is the wall thickness; P represents the circumferential stress (vertical principal stress of the normal section) inside segment lining member 1 under external pressure; o denoted as external radial pressure; F is the total tension of the steel strand; L is the axial length of the circular specimen; and D is the average circumference of the circular specimen.
[0055] like Figure 11 As shown, specifically, the circumferential stress (vertical principal stress of the normal section) inside the segment lining member 1 under the action of internal pressure: ; Where: a is the inner radius; b is the outer radius; t is the wall thickness; p i Internal radial pressure; The circumferential stress (vertical principal stress of the normal section) inside the segment lining member 1 under the action of internal pressure.
[0056] like Figure 12 As shown, specifically, the circumferential stress (vertical principal stress of the normal section) of segment lining member 1 under the combined action of external and internal pressures is as follows: ; Where: a is the inner radius; b is the outer radius; p i For internal radial pressure; p o External radial pressure; t is wall thickness; The circumferential stress (vertical principal stress of the normal section) of the segment lining member 1 under the combined action of external and internal pressure.
[0057] Based on the above formula, it can be seen that the annular stress of the lining segment component can be adjusted by adjusting the total tension of the steel strand and the injection pressure.
[0058] The circumferential strain of the inner and outer walls of the segment lining component 1 is measured by a distributed fiber optic sensor 10, and the average circumferential strain is calculated. The stress state of the ring is deduced based on the principles of elasticity. Specifically: ; ; : Circumferential stress; E: Elastic modulus of reinforced concrete segment; : Cross-sectional area; Circumferential strain on the outer wall of the tube segment; Circumferential strain of the inner wall of the tube segment; : Average circumferential strain of the tube segment.
[0059] During the experiment, it is necessary to first determine the internal stress σ of the segment lining structure required for the experiment. 目标值 and osmotic pressure p 目标值 Then, the test load is input based on the following process: (1) Based on the seepage water pressure and inner radial pressure p of the segment lining component to be studied. i Based on the principle of equality, the circumferential stress inside segment lining member 1 under internal pressure is obtained. (1) Vertical principal stress of the cross section); (2) Circumferential stress of the segment lining member 1 under the combined action of external and internal pressures that need to be studied. (Vertical principal stress of the cross section,) It should be equal to σ 目标值 ), and deduce the total tension F of the steel strand, and use the above p i The value of F is the initial value for loading, used to input p. i The values of F and F cause the circumferential stress within the structure to reach σ. 目标值 (3) The structural stress σ derived from the strain obtained by the distributed optical fiber sensor and the target circumferential stress σ are compared. 目标值 Compare, such as with σ 目标值 If discrepancies exist, the value of F is further adjusted until the reading of the distributed fiber optic sensor matches the strain corresponding to the preset stress value (i.e., σ = σ). 目标值 ).
[0060] Step 3: Connect the positive terminal of the power supply to the anode component and connect the negative terminal of the power supply to the cathode component 7.
[0061] The steel bar 2, embedded in the concrete, serves as the anode and is connected to a DC regulated power supply via an insulated wire. The positive terminal of the DC regulated power supply is connected to the steel bar 2, and the negative terminal is connected to the copper rod, thus establishing a stable DC electric field inside the tunnel lining component 1, between the corrosive liquid and the copper rod. Under the action of the DC electric field, anions dissolved in the corrosive liquid (such as Cl-)... - The chloride ions migrate directionally towards the anode (reinforcing bar 2). This process significantly accelerates the penetration rate of corrosive media such as chloride ions in concrete and their enrichment on the surface of reinforcing bar 2, thereby accelerating penetration: greatly shortening the time required for chloride ions to penetrate to the surface of reinforcing bar 2 and reach the critical concentration. It also accelerates corrosion: directly accelerating the anodic electrochemical reaction of reinforcing bar 2 through electrochemical action, inducing and accelerating the corrosion of reinforcing bar 2.
[0062] Step 4: Start the data acquisition module.
[0063] When the experiment reaches a certain stage, the electrode array 8 embedded in the concrete and the resistivity acquisition instrument electrically connected to the electrode array 8 are used to capture and analyze the seepage path, penetration depth, and leakage changes of the corrosive liquid inside the concrete segment in real time. Fiber optic sensors tightly bonded to the surface of key parts of the reinforcing steel 2 are used to monitor the sudden changes in local strain caused by the volume expansion of corrosion products in the lining component 1 of the segment in real time. Once a characteristic continuous strain increase is detected and the influence of mechanical load is eliminated, the precise location and quantitative assessment of the corrosion initiation point, development range, and degree of corrosion of the reinforcing steel 2 can be achieved. At a specific time point in the experiment, the internal water pressure and external radial pressure can be gradually unloaded to a safe state according to a preset program, and the internal water is pumped out. Then, the constraints of the first sealing cover 3 and the second sealing cover 4 and the tie rod are released, the device is disassembled, and the segment ring (or arc-shaped segment) of the designated layer is taken out as the research sample for that time point. This sample can be used for microstructure observation, penetration depth measurement, and material performance analysis. After sampling, the remaining segment rings and components can be reassembled according to the predetermined assembly process by adjusting the extension length of the tie rods to match the total height of the remaining assembled segments, restoring the original sealing and load conditions, and continuing the subsequent stages of testing. This allows for the simulation of seawater infiltration, structural deterioration, and failure processes under different stress states and combined seawater pressures in the shield tunnel segment lining.
[0064] The basic principles of this application have been described above with reference to specific embodiments. However, it should be noted that the advantages, benefits, and effects mentioned in this application are merely examples and not limitations, and should not be considered as essential features of each embodiment of this application. Furthermore, the specific details disclosed above are for illustrative and facilitative purposes only, and are not limitations. These details do not limit the application to the necessity of employing the aforementioned specific details for implementation.
[0065] The block diagrams of devices, apparatuses, devices, and systems involved in this application are merely illustrative examples and are not intended to require or imply that they must be connected, arranged, or configured in the manner shown in the block diagrams. As those skilled in the art will recognize, these devices, apparatuses, devices, and systems can be connected, arranged, and configured in any manner. Words such as “comprising,” “including,” “having,” etc., are open-ended terms meaning “including but not limited to,” and are used interchangeably with them. The terms “or” and “and” as used herein refer to the terms “and / or,” and are used interchangeably with them unless the context clearly indicates otherwise. The term “such as” as used herein refers to the phrase “such as but not limited to,” and is used interchangeably with it.
[0066] It should also be noted that in the apparatus, equipment, and housing of this application, the components or steps can be disassembled and / or reassembled. These disassemblies and / or reassemblies should be considered as equivalent solutions of this application.
[0067] The above description of the disclosed aspects is provided to enable any person skilled in the art to make or use this application. Various modifications to these aspects will be readily apparent to those skilled in the art, and the general principles defined herein can be applied to other aspects without departing from the scope of this application. Therefore, this application is not intended to be limited to the aspects shown herein, but rather to be accorded the widest scope consistent with the principles and novel features disclosed herein.
[0068] It should be understood that the qualifiers “first,” “second,” “third,” “fourth,” “fifth,” and “sixth” used in the description of the embodiments of this application are only used to more clearly illustrate the technical solutions and are not intended to limit the scope of protection of this application.
[0069] The above description has been given for purposes of illustration and description. Furthermore, this description is not intended to limit the embodiments of this application to the forms disclosed herein. Although numerous exemplary aspects and embodiments have been discussed above, those skilled in the art will recognize certain variations, modifications, alterations, additions, and sub-combinations thereof.
Claims
1. A multi-field coupled test device for simulating the structural deterioration of an underwater shield tunnel, characterized in that, include: The segment lining components are arranged in a ring, and the segment lining components are cast from concrete and steel bars set in the concrete. The hoop force application module includes a force application component disposed on the outer periphery of the segment lining member; The injection module includes a first sealing cap that seals a first end of the segment lining member, a second sealing cap that seals a second end of the segment lining member, a connecting rod assembly that connects the first sealing cap and the second sealing cap, and a water injection pump. The first sealing cap is located on top of the second sealing cap and has an injection hole. Water-stopping elements are provided between the first sealing cap and the segment lining member, and between the second sealing cap and the segment lining member. The first sealing cap, the second sealing cap, and the segment lining member enclose a sealed cavity. The data acquisition module includes an electrode array embedded in concrete, a resistivity acquisition instrument electrically connected to the electrode array, a water pressure sensor, a component internal force sensor, and a data acquisition instrument used in conjunction with the component internal force sensor. An electrochemical corrosion module includes a cathode coaxially arranged with the segment lining component and a power supply for conducting the anode and the cathode. The anode is formed by reinforcing steel bars. A DC electric field is applied between the anode and the cathode to drive the corrosion ions in the corrosive liquid to migrate directionally in the concrete, thereby accelerating the corrosion of the reinforcing steel bars and the deterioration of the concrete. The first sealing cover has a through hole, and the second sealing cover has a groove on the side facing the sealing cavity. The cathode component passes through the through hole and is embedded in the groove, wherein the axis of the through hole and the groove coincides with the axis of the segment lining component. Both the first sealing cap and the second sealing cap are made of metal. Both the first sealing cap and the second sealing cap have an insulating layer on the side facing the sealing cavity, and an insulating seal is provided between the through hole and the cathode. During the experiment, corrosive liquid was injected into the sealed cavity through the injection hole, and the corrosive liquid was pressurized to a preset water pressure by the water pump. The pressurized corrosive liquid drove the corrosive ions inside to migrate into the concrete, thereby inducing steel corrosion and concrete deterioration. The water penetration state, stress state and water pressure value inside the sealed cavity were monitored in real time by the data acquisition module.
2. The multi-field coupled test device for simulating the structural deterioration of a submarine shield tunnel as described in claim 1, characterized in that, The linkage assembly consists of multiple telescopic rods.
3. The multi-field coupled test device for simulating the structural deterioration of a submarine shield tunnel as described in claim 1, characterized in that, The force-applying component includes a metal strand wound around the outer periphery of the segment lining member and a tensioning device for tensioning the metal strand.
4. The multi-field coupled test device for simulating the structural deterioration of a submarine shield tunnel as described in claim 1, characterized in that, The segment lining component is composed of multiple annular segments arranged along the axial direction of the segment lining component; or, the segment lining component is composed of multiple arc-shaped segments; or, the segment lining component is composed of a single annular segment.
5. The multi-field coupled test device for simulating the structural deterioration of a submarine shield tunnel according to claim 4, characterized in that, The electrode array is embedded inside the concrete and is distributed in an array along the circumference of the segment lining component.
6. The multi-field coupled test device for simulating the structural deterioration of a submarine shield tunnel according to claim 1, characterized in that, The internal force sensor of the component is a distributed optical fiber sensor, which is arranged along the circumference of the segment lining component on the outer and inner peripheral walls of the segment lining component.
7. A multi-field coupled test method for simulating the structural deterioration of an undersea shield tunnel, employing the multi-field coupled test apparatus for simulating the structural deterioration of an undersea shield tunnel as described in any one of claims 1-6, and comprising: Step 1: Start the tensioning device and use the tensioning device to apply circumferential constraints to the segment lining member through the metal strands, and gradually increase the tension force according to the preset level until the uniform pressure on the outer peripheral wall of the segment lining member reaches the first preset value. Step 2: Start the water injection pump to inject corrosive liquid into the sealed cavity, and gradually pressurize the corrosive liquid inside the sealed cavity until the uniform water pressure on the inner peripheral wall of the segment lining component reaches the second preset value. Step 3: Connect the positive terminal of the power supply to the anode component and connect the negative terminal of the power supply to the cathode component. Step 4: Start the data acquisition module.
Citation Information
Patent Citations
Experimental device and method for shield tunnel segment performance degradation mechanism research
CN114279947A
A sensor apparatus and method
WO2011048378A2