一种轻质高强建筑玻璃及其制备方法

CN121651698BActive Publication Date: 2026-07-17BEIJING WUZHOU GLOBAL CONSTR TECH CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
BEIJING WUZHOU GLOBAL CONSTR TECH CO LTD
Filing Date
2025-12-30
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

There are technical bottlenecks in achieving both lightweight and high strength in existing architectural glass. Physically tempered glass has a high risk of spontaneous breakage, laminated or hollow structures increase self-weight, lightweight paths lack sufficient strength, and functional coatings are prone to aging, making it difficult to meet the requirements of high-performance green buildings.

Method used

Lightweight and high-strength architectural glass is prepared by using a mixture of modified nano-reinforcing phase, silica, boron oxide, aluminum oxide, lithium oxide, sodium oxide, calcium oxide and composite foaming regulator through two-stage heating, heat preservation, pressing, annealing and impregnation treatment. The modified nano-reinforcing phase improves the interfacial bonding force through mesoporous silica coating and fluorosilane modification.

Benefits of technology

It improves the mechanical properties, thermal stability, thermal insulation performance, and antistatic properties of architectural glass, solves the problem of balancing lightweight and high strength, and enhances safety and overall performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

本发明涉及一种轻质高强建筑玻璃及其制备方法,属于建筑玻璃技术领域,所述制备方法包括以下步骤:将改性纳米增强相、二氧化硅、氧化硼、氧化铝、氧化锂、氧化钠、氧化钙和复合发泡调控剂混合,制得玻璃混合料;将玻璃混合料经第一阶段升温、保温,再经第二阶段升温、保温,搅拌均匀,制得均化玻璃熔体;将均化玻璃熔体浇注,压制成型,制得玻璃原板;将玻璃原板退火,保温,冷却,制得退火玻璃板;将退火玻璃板经预热,进行离子交换处理,取出水洗,冷却,制得轻质高强建筑玻璃;本发明通过介孔二氧化硅包覆纳米粒子,然后进行氟硅烷表面修饰,再负载到低熔点硼硅酸盐微球上,制得改性纳米增强相;总体提升了建筑玻璃的综合性能。
Need to check novelty before this filing date? Find Prior Art