Trench gate MOSFET, preparation method thereof and chip

CN121665625BActive Publication Date: 2026-09-25FOUNDER MICROELECTRONICS INT
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202511697038.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2025-11-19
Publication Date
2026-09-25
Estimated Expiration
2045-11-19

AI Technical Summary

Technical Problem

然而,对于反向阻断模式下的传统SiC沟槽式MOSFET,沟槽底部栅极氧化层中的高电场是主要问题,这使得击穿电压(VBR)在远低于漂移区半导体结击穿固有能力的电压下而受到栅极氧化层崩溃的限制

Benefits of technology

[0015]本申请实施例的有益效果:通过在具有凹形沟槽的栅氧化层的底部形成于P型屏蔽区上,并在P型屏蔽区与栅氧化层的底部之间形成N型注入区,且P型屏蔽区的两端分别与栅氧化层的底部边缘区域接触,栅极材料层形成于栅氧化层的凹槽内,场氧化层与栅氧化层形成包裹栅极材料层的封闭结构,在P型屏蔽区与N型漂移区之间形成PN结,在P型屏蔽区与N型注入区之间形成PN结,从而使得器件在反向偏压的情况下,可以增加耗尽区面积,从而提高击穿电压,实现优化静态品质因数的目的。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121665625B_ABST
    Figure CN121665625B_ABST
Patent Text Reader

Abstract

The application belongs to the technical field of power devices, and provides a trench gate MOSFET, a preparation method thereof and a chip. A P-type shielding region is formed at the bottom of a gate oxide layer with a concave trench, an N-type injection region is formed between the P-type shielding region and the bottom of the gate oxide layer, the two ends of the P-type shielding region are respectively in contact with the edge regions of the bottom of the gate oxide layer, a gate material layer is formed in the concave trench of the gate oxide layer, a field oxide layer and the gate oxide layer form a closed structure wrapping the gate material layer, a PN junction is formed between the P-type shielding region and an N-type drift region, and a PN junction is formed between the P-type shielding region and the N-type injection region, so that the device can increase the area of a depletion region under a reverse bias, thereby improving the breakdown voltage and achieving the purpose of optimizing the static quality factor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application belongs to the field of power device technology, and in particular relates to a trench gate MOSFET and its fabrication method and chip. Background Technology

[0002] Due to their excellent material properties, including wide bandgap, high critical electric field and good thermal conductivity, silicon carbide (SiC) trench-gate metal-oxide-semiconductor field-effect transistors (TG-MOSFETs) have very high gate density without being limited by the parasitic JFET channels in planar SiC MOSFETs, thus reducing the contribution of channel resistance to the total on-resistance.

[0003] Compared to conventional planar MOSFETs, TG-MOSFETs can significantly reduce the specific on-resistance of devices by accommodating more channels on a given chip area and completely eliminating the JFET effect. However, for conventional SiC trench MOSFETs in reverse blocking mode, the high electric field in the gate oxide layer at the bottom of the trench is a major problem, which causes the breakdown voltage (VBR) to be limited by gate oxide collapse at a voltage far below the inherent breakdown capability of the drift region semiconductor junction. Summary of the Invention

[0004] To address the aforementioned technical problems, this application provides a trench gate MOSFET, its fabrication method, and a chip, aiming to improve the breakdown voltage of the device and optimize its static quality factor.

[0005] A first aspect of this application provides a trench gate MOSFET, the trench gate MOSFET comprising: A silicon carbide substrate and a buffer layer, wherein the buffer layer is formed on the front side of the silicon carbide substrate; An N-type drift region with concave grooves is formed on the buffer layer; A current spreading layer is formed on both sides of the N-type drift region; A P-type well region is formed on the current spreading layer; The P-type shielding area is formed at the bottom of the groove in the N-type drift area; A gate oxide layer with concave trenches is formed on the P-type shielding region, and the height of the gate oxide layer is greater than the sum of the heights of the current spreading layer and the P-type well region; An N-type implantation region is formed between the P-type shielding region and the bottom of the gate oxide layer, and the two ends of the P-type shielding region are respectively in contact with the bottom edge region of the gate oxide layer; The N-type heavily doped region is formed on the P-type well region and located on both sides of the gate oxide layer; A p-type heavily doped region is formed on the p-type well region and located next to the n-type heavily doped region; A gate material layer is formed within a groove in the gate oxide layer; A field oxide layer, together with the gate oxide layer, forms a closed structure that encloses the gate material layer; The source layer is in contact with the P-type well region, the N-type heavily doped region, both sides of the gate oxide layer, and the field oxide layer; A drain layer is formed on the back side of the silicon carbide substrate.

[0006] In some embodiments, the P-type shielding region is a concave structure or an arc shape, and the two ends of the P-type shielding region are respectively in contact with the bottom sides of the gate oxide layer.

[0007] In some embodiments, the width of the P-type shielding region is smaller than the width of the bottom of the gate oxide layer.

[0008] In some embodiments, the N-type injection region is opposite to the gate material layer, and the two ends of the P-type shielding region are symmetrically arranged with the N-type injection region as the axis of symmetry.

[0009] In some embodiments, the thickness of the two ends of the P-type shielding region is greater than the sidewall thickness of the gate oxide layer.

[0010] In some embodiments, the width of the N-type injection region gradually decreases from the source layer to the drain layer.

[0011] In some embodiments, the thickness of the N-type injection region is less than one-third of the thickness of the P-type shielding region, and the thickness of the N-type injection region is greater than one-fifth of the thickness of the P-type shielding region.

[0012] In some embodiments, the doping concentration of the P-type shielding region exhibits a gradient distribution.

[0013] A second aspect of this application also provides a method for fabricating a trench gate MOSFET, the method comprising: A buffer layer, an N-type drift region, a current spreading layer, a P-type well doped layer, and an N-type doped layer are sequentially formed on the front side of a silicon carbide substrate. Under the cover of a first mask, a first trench is etched along the central region of the N-type doped layer, extending into the N-type drift region. The P-type well doped layer has a concave structure, and the N-type doped layer is located within the groove of the P-type well doped layer. A current spreading layer, a P-type well region, a heavily doped P-type region, and a heavily doped N-type region are formed on both sides of the first trench, respectively. Remove the first mask and fill the first trench with a first dielectric material; wherein the first dielectric material covers the surface areas of the first trench and the P-type well region and the N-type heavily doped region; A second mask is applied to the first dielectric material, and the first dielectric material is etched according to the pattern of the second mask to form a first dielectric material layer at the bottom and sidewalls of the first trench; wherein the thickness of the first dielectric material layer is less than the thickness of the current spreading layer. P-type doped ions are injected along the trench direction of the first trench, so that the P-type doped ions pass through the first dielectric material layer to form a P-type shielding region in the N-type drift region. The first dielectric material is deposited to cover the first trench, a third mask is deposited on the first dielectric material, and the first dielectric material is etched according to the pattern of the third mask to form a second dielectric material layer at the bottom and sidewalls of the first trench; wherein the thickness of the second dielectric material layer is greater than the thickness of the first dielectric material layer. N-type doped ions are injected along the trench direction of the first trench, so that the N-type doped ions pass through the second dielectric material layer to form an N-type injection region in the P-type shielding region. Remove the second dielectric material layer and activate the P-type shielding region and the N-type injection region; A gate oxide layer is formed at the bottom and sidewalls of the first trench, a gate material layer is formed by filling it with polysilicon material, and a field oxide layer is formed on the gate material layer. Then, a source material is deposited to form a source layer that contacts the P-type well region, the N-type heavily doped region, both sides of the gate oxide layer, and the field oxide layer. The field oxide layer and the gate oxide layer form a closed structure that encloses the gate material layer.

[0014] A third aspect of this application also provides a chip including a trench gate MOSFET as described in any of the above embodiments.

[0015] The beneficial effects of this application embodiment are as follows: By forming a P-type shielding region on the bottom of a gate oxide layer with concave trenches, and forming an N-type injection region between the P-type shielding region and the bottom of the gate oxide layer, with both ends of the P-type shielding region contacting the bottom edge region of the gate oxide layer, a gate material layer is formed in the trench of the gate oxide layer, and the field oxide layer and the gate oxide layer form a closed structure that encloses the gate material layer. A PN junction is formed between the P-type shielding region and the N-type drift region, and between the P-type shielding region and the N-type injection region. This allows the device to increase the depletion region area under reverse bias, thereby improving the breakdown voltage and achieving the purpose of optimizing the static quality factor. Attached Figure Description

[0016] Figure 1 This is a schematic diagram of a trench gate MOSFET provided in an embodiment of this application; Figure 2 This is a schematic diagram of the doping concentration of the trench gate MOSFET provided in the embodiments of this application; Figure 3 This is a schematic diagram of the electric field of the trench gate MOSFET provided in an embodiment of this application; Figure 4 This is a schematic diagram of the electric field distribution curve provided in an embodiment of this application; Figure 5 This is a schematic diagram of the fabrication method of the trench gate MOSFET provided in the embodiments of this application; Figure 6 This is a partial schematic diagram of the method for fabricating a trench gate MOSFET provided in an embodiment of this application; Figure 7 This is a partial schematic diagram of the method for fabricating a trench gate MOSFET provided in an embodiment of this application; Figure 8 This is a partial schematic diagram of the method for fabricating a trench gate MOSFET provided in an embodiment of this application; Figure 9 This is a partial schematic diagram of the method for fabricating a trench gate MOSFET provided in an embodiment of this application; Figure 10 This is a partial schematic diagram of the method for fabricating a trench gate MOSFET provided in an embodiment of this application; Figure 11 This is a partial schematic diagram of the method for fabricating a trench gate MOSFET provided in an embodiment of this application; Figure 12 This is a partial schematic diagram of the fabrication method of the trench gate MOSFET provided in the embodiments of this application. Detailed Implementation

[0017] To make the technical problems, technical solutions, and beneficial effects to be solved by this application clearer, the following detailed description is provided in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and are not intended to limit the scope of this application.

[0018] Compared to conventional planar MOSFETs, TG-MOSFETs can significantly reduce the specific on-resistance of devices by accommodating more channels on a given chip area and completely eliminating the JFET effect. However, for conventional SiC trench MOSFETs in reverse blocking mode, the high electric field in the gate oxide layer at the bottom of the trench is a major problem, which causes the breakdown voltage (VBR) to be limited by gate oxide collapse at a voltage far below the inherent breakdown capability of the drift region semiconductor junction.

[0019] In an N-type epitaxial drift region of a certain thickness grown on a SiC substrate, the area of ​​the N-type drift region is reduced due to the increased shielding P+ area beneath the bottom gate oxide layer. Consequently, the area of ​​the depletion region that can be formed also decreases. During reverse bias operation, although a shielding layer is added to prevent the collapse of the gate oxide layer at the bottom of the trench and instead rely on the cumulative collapse electric field of the PN junction to improve the device's operating voltage withstand capability, the optimal static quality factor (FOM = BV) for device design remains crucial. 2 / Ron) makes the static quality factor as high as possible, and the general focus is on how to increase the breakdown voltage (BV) or reduce the on-resistance (Ron) of the device.

[0020] To address the aforementioned technical problems, this application provides a trench gate MOSFET, see [link to relevant documentation]. Figure 1 As shown, the trench gate MOSFET in this embodiment includes: a drain layer 720, a silicon carbide substrate 100, a buffer layer 200, an N-type drift region 300, a current spreading layer 511, a P-type well region 521, a gate oxide layer 610, a gate material layer 600, a P-type shielding region 400, an N-type implantation region 410, an N-type heavily doped region 531, a P-type heavily doped region 532, a field oxide layer 620, a source layer 710, and a drain layer 720.

[0021] In this embodiment, the drain layer 720, silicon carbide substrate 100, buffer layer 200, and N-type drift region 300 are stacked. The N-type drift region 300 has a concave structure, and a current spreading layer 511 and a P-type well region 521 are sequentially formed on the first and second sides of the N-type drift region 300. A P-type shielding region 400 is formed at the bottom of the groove of the N-type drift region 300, and an N-type injection region 410 is formed between the bottom of the P-type shielding region 400 and the gate oxide layer 610. A PN junction is formed at the junction of the N-type injection region 410 and the P-type shielding region 400. The gate oxide layer 610 has a concave structure, and the gate oxide layer 610 and the field oxide layer 620 form a closed structure that encloses the gate material layer 600. The N-type heavily doped region 531 is formed on the P-type well region 521 and located on both sides of the gate oxide layer 610. The P-type heavily doped region 532 is located on the P-type well region 521 and located next to the N-type heavily doped region 531. The main function of the P-type heavily doped region 532 is to connect the P-type well region 521 and reduce the ohmic contact resistance with the source electrode.

[0022] In some embodiments, the spacing between the two sides of the gate oxide layer 610 gradually increases from the bottom to the opening, the height of the gate oxide layer 610 is greater than the sum of the heights of the current spread layer 511 and the P-type well region 521, and the source layer 710 is in contact with the P-type well region 521, the N-type heavily doped region 531, the two sides of the gate oxide layer 610 and the field oxide layer 620.

[0023] In the trench gate MOSFET of this embodiment, an N-type injection region 410 is formed between the bottom of the gate oxide layer 610 with a concave trench on the P-type shielding region 400 and the bottom of the gate oxide layer 610. The two ends of the P-type shielding region 400 are in contact with the bottom edge region of the gate oxide layer 610. The gate material layer 600 is formed in the trench of the gate oxide layer 610. The field oxide layer 620 and the gate oxide layer 610 form a closed structure that surrounds the gate material layer 600. A PN junction is formed between the P-type shielding region 400 and the N-type drift region 300, and between the P-type shielding region 400 and the N-type injection region 410. This allows the device to increase the depletion region area under reverse bias, thereby improving the breakdown voltage and achieving the purpose of optimizing the static quality factor.

[0024] Combination Figure 2 As shown, with Figure 2 The structural schematic diagram (a) is the baseline structural diagram, in which nitrogen-free ion implantation is performed on the SiC surface adjacent to the gate oxide layer 610 at the bottom of the trench. See [link / reference]. Figure 2 As shown in the structural schematic diagram (b), it is clear that there is an N-type activated nitrogen ion concentration distribution below the center of the gate oxide layer 610 at the bottom of the trench.

[0025] Figure 2Schematic (c) shows the depth concentration distribution curves of activated P-type aluminum ions (Al), N-type nitrogen atoms (N), and net doped activated ions (J) in the region below the center of the gate oxide layer at the bottom of the trench in schematic (a). Schematic (d) shows the depth concentration distribution curves of activated P-type aluminum ions (Al), N-type nitrogen atoms (N), and net doped activated ions (J) in the region below the center of the gate oxide layer 610 at the bottom of the trench in schematic (b). Comparing the curve distributions in schematic (c) and schematic (d), it is clear that a PN junction exists at the junction of the bottom of the P-type shielding region 400 and the N-type drift region 300 in schematic (c). When the device is under reverse bias operation, the depletion region will extend and expand to both sides in the upward and downward directions from this point. The lower epitaxial N-type concentration is lower, so the depletion region area is larger than that of the upper P-type shielding region 400. Compared with schematic diagram (c), schematic diagram (d) clearly shows that another PN junction appears in the gate oxide layer 610 near the bottom of the trench within the P-type shielding region 400. This will enable the device to increase the breakdown voltage (i.e., breakdown voltage) under reverse bias by increasing the area of ​​the depletion region, thereby achieving the purpose of optimizing the static quality factor.

[0026] In some embodiments, Figure 3 The schematic structure (a) in the diagram is Figure 2 The schematic diagram (a) in the figure shows the electric field distribution of the device under reverse bias. Figure 3 The schematic structure (b) in the diagram is Figure 2 The schematic diagram (b) in the figure shows the electric field distribution of the device under reverse bias. The two structures were simulated and tested. Figure 3 The schematic structure (a) in the diagram serves as the reference structure. Its breakdown voltage is 1695V, its on-resistance at 18V is 59.1mR, its Qg is 69.3nC, and its static FOM is 48613. Figure 3 In the schematic structure (b), an injection voltage of 50 keV and an injection dose of 1e14 cm⁻¹ are used. -2 Under N-type doped ion implantation conditions, the breakdown voltage of the trench gate MOSFET with N-type implantation region 410 is 1740V, its on-resistance is 58.44mR at 18V, its Qg is 69nC, and its static FOM is 51807, which is an improvement of 6.6%.

[0027] Combination Figure 4As shown, the horizontal axis represents the vertical depth, and the vertical axis represents the electric field intensity. It is evident that the device (NP) with an additional nitrogen injection into the SiC surface of the N-type injection region 410 formed by the gate oxide layer 610 at the bottom of the trench has a larger area under the electric field curve than the electric field curve of the device (BSL) under reverse bias operation, indicating a significant increase in breakdown voltage (BV). Since the nitrogen injection process does not affect the JFET region and drift region on both sides of the trench when the device is conducting with forward current, the on-resistance (Ron) and Qg do not change significantly.

[0028] In some embodiments, combined with Figure 1 As shown, the gate oxide layer 610 has a concave structure, and the vertical cross-section of the outer side surface of the gate oxide layer 610 can be stepped.

[0029] In this embodiment, the outer surface of the first side of the gate oxide layer 610 contacts the current spreading layer 511, the P-type well region 521, and the heavily doped N-type region 531 on the first side of the N-type drift region 300. The outer surface of the first side of the gate oxide layer 610 can be stepped. The outer surface of the second side of the gate oxide layer 610 contacts the current spreading layer 511, the P-type well region 521, and the heavily doped N-type region 531 on the second side of the N-type drift region 300. The outer surface of the second side of the gate oxide layer 610 is also stepped. This allows for a gradual reduction in the width of the trench gate, minimizing the width of the central oxide layer at the bottom, which helps reduce the gate leakage charge Qgd of the device.

[0030] In some embodiments, the gate oxide layer 610 has a concave structure, and the vertical cross-section of the outer side surface of the gate oxide layer 610 is arc-shaped.

[0031] In this embodiment, the outer surface of the first side of the gate oxide layer 610 contacts the first side of the N-type drift region 300 and the current spreading layer 511, P-type well region 521, and N-type heavily doped region 531 thereon. The outer surface of the first side of the gate oxide layer 610 is arc-shaped. The outer surface of the second side of the gate oxide layer 610 contacts the second side of the N-type drift region 300 and the current spreading layer 511, P-type well region 521, and N-type heavily doped region 531 thereon. The outer surface of the second side of the gate oxide layer 610 is arc-shaped. In this way, the interface between the two sides of the gate oxide layer 610 and the contacting areas can change slowly and continuously, eliminating doping corners, avoiding electric field accumulation, and facilitating the gradual reduction of the trench gate width, so that the width of the central oxide layer at the bottom is minimized, which is beneficial to reducing the gate leakage charge Qgd of the device.

[0032] In some embodiments, the P-type shielding region 400 is a concave structure or an arc shape, and the two ends of the P-type shielding region 400 are in contact with the bottom sides of the gate oxide layer 610, respectively.

[0033] In some embodiments, the width of the P-type shielding region 400 is smaller than the width of the bottom of the gate oxide layer 610.

[0034] In some embodiments, the N-type injection region 410 is opposite to the gate material layer 600, and the two ends of the P-type shielding region are symmetrically arranged with the N-type injection region 410 as the axis of symmetry.

[0035] In some embodiments, the thickness of the two ends of the P-type shielding region is greater than the sidewall thickness of the gate oxide layer 610.

[0036] In some embodiments, the width of the N-type injection region 410 gradually decreases from the source layer 710 toward the drain layer 720.

[0037] In some embodiments, the thickness of the N-type injection region 410 is less than one-third of the thickness of the P-type shielding region 400, and the thickness of the N-type injection region 410 is greater than one-fifth of the thickness of the P-type shielding region 400.

[0038] In some embodiments, the gate oxide layer 610 has a concave structure, the inner wall of the groove of the gate oxide layer 610 is arc-shaped, and the bottom of the gate oxide layer 610 is arc-shaped.

[0039] In this embodiment, the inner wall of the groove of the gate oxide layer 610 is in contact with the gate material layer 600. By setting the inner wall of the groove of the gate oxide layer 610 to be arc-shaped, the angle change of the interface between the gate oxide layer 610 and the gate material layer 600 can be reduced, the electric field accumulation in the N-type drift region 300 can be reduced, and the width of the trench gate can be reduced step by step, so that the width of the central oxide layer at the bottom is minimized, which is beneficial to reducing the gate leakage charge Qgd of the device.

[0040] In some embodiments, isolation protective layers are respectively provided at the two bottom corners of the gate oxide layer 610, and the N-type injection region 410 is located at the central axis of the isolation protective layers at the two corners. The isolation protective layers are respectively attached to the bottom sides of the gate oxide layer 610, and the interface between the isolation protective layer and the N-type drift region 300 is arc-shaped.

[0041] In this embodiment, the width of the gate oxide layer 610 gradually increases from the drain layer 720 to the source layer 710. The bottom of the gate oxide layer 610 is close to the drain layer 720. By setting the interface between the isolation protection layer and the N-type drift region 300 to be arc-shaped, the angle change of the interface between the gate oxide layer 610 and the N-type drift region 300 can be reduced, the electric field accumulation in the N-type drift region 300 can be reduced, and the width of the trench gate can be reduced step by step, so that the width of the central oxide layer at the bottom is minimized, which is beneficial to reducing the gate drain charge Qgd of the device.

[0042] In some embodiments, the gate oxide layer 610 has a concave structure, and the first side and the second side of the gate oxide layer 610 extend outward at their opening positions, respectively. The left extension portion does not exceed the left boundary of the left N-type heavily doped region 531, and the right extension portion does not exceed the right boundary of the right N-type heavily doped region 531.

[0043] In some embodiments, the thickness of the gate oxide layer 610 gradually increases from the drain layer 720 toward the source layer 710, thereby increasing the electric field distribution in the current spread layer 511, P-type well region 521, N-type heavily doped region 531, and N-type heavily doped region 531. This helps to reduce the electric field accumulation in the N-type drift region 300 and also facilitates the gradual reduction of the trench gate width, minimizing the width of the central oxide layer at the bottom, which helps to reduce the gate drain charge Qgd of the device.

[0044] In some embodiments, the width between the two sidewalls of the gate oxide layer 610 gradually increases from the drain layer 720 toward the source layer 710, thereby the electric field distribution in the current spread layer 511, P-type well region 521, N-type heavily doped region 531, and N-type heavily doped region 531 is beneficial to reduce the electric field accumulation in the N-type drift region 300, and can also facilitate the gradual reduction of the trench gate width, so that the width of the bottom central oxide layer is minimized, which is beneficial to reduce the gate drain charge Qgd of the device.

[0045] In some embodiments, the thickness of the isolation protection layer gradually decreases in the longitudinal direction from the drain layer 720 to the source layer 710. This helps to reduce the electric field accumulation in the N-type drift region 300 and also facilitates the gradual reduction of the width of the trench gate, so that the width of the central oxide layer at the bottom is minimized, which helps to reduce the gate drain charge Qgd of the device.

[0046] In some embodiments, the gate oxide layer 610 has a concave structure, the inner wall of the groove of the gate oxide layer 610 is stepped, and the bottom of the gate oxide layer 610 is arc-shaped.

[0047] In some embodiments, the protective layer may be a silicon oxide layer.

[0048] In some embodiments, the gate oxide layer 610 has a symmetrical structure.

[0049] In some embodiments, the interface between the gate oxide layer 610 and the gate material layer 600 is stepped.

[0050] In this embodiment, the inner diameter of the groove in the gate oxide layer 610 gradually decreases from the source layer 710 to the drain layer 720, and the inner wall of the groove in the gate oxide layer 610 has a stepped structure.

[0051] In some embodiments, the two sides of the gate oxide layer 610 have a stepped structure.

[0052] In this embodiment, the inner wall of the groove of the gate oxide layer 610 has a stepped structure, and the outer surfaces of both sides of the gate oxide layer 610 also have a stepped structure.

[0053] In some embodiments, the two sides of the gate oxide layer 610 have a multi-level stepped structure. The boundary of the isolation protective layer on the first side of the gate oxide layer 610 is flush with the boundary of the middle step on the first side of the gate oxide layer 610, so that the shape of the first side of the isolation protective layer matches that of the gate oxide layer 610, and avoids the formation of corners between the isolation protective layer and the bottom of the first side of the gate oxide layer 610, which would cause electric field accumulation.

[0054] In some embodiments, the isolation protective layer located on the second side of the gate oxide layer 610 is flush with the boundary of the intermediate step on the second side of the gate oxide layer 610, so that the isolation protective layer located on the second side of the gate oxide layer 610 matches the shape of the gate oxide layer 610, and avoids the formation of corners between the isolation protective layer and the bottom of the second side of the gate oxide layer 610, which would cause electric field accumulation.

[0055] In some embodiments, combined with Figure 1 As shown, the two ends of the P-type shielding region 400 are attached to the bottom sides of the gate oxide layer 610 at the bottom of the trench. The P-type shielding region 400 is arc-shaped, and the two ends of the P-type shielding region 400 are respectively attached to the isolation protection layer on the bottom sides of the gate oxide layer 610. This can further reduce the electric field concentration effect in the bottom corner area of ​​the gate, avoid high electric field collapse, reduce the gate leakage current phenomenon of the device, and improve the reliability of the device.

[0056] In some embodiments, the top of the first-side step of the gate oxide layer 610 is formed on the upper surface of the N-type heavily doped region 531 on the first side.

[0057] In this embodiment, the first side of the gate oxide layer 610 has a stepped structure. The lower surface of the top of the first step of the gate oxide layer 610 is in contact with the upper surface of the N-type heavily doped region 531, and the top of the first step of the gate oxide layer 610 is not in contact with the P-type well region 521.

[0058] In some embodiments, the top of the second-side step of the gate oxide layer 610 is formed on the upper surface of the N-type heavily doped region 531 on the second side.

[0059] In this embodiment, the second side of the gate oxide layer 610 has a stepped structure. The lower surface of the top of the second step of the gate oxide layer 610 is in contact with the upper surface of the N-type heavily doped region 531 on the second side, and the top of the second step of the gate oxide layer 610 is not in contact with the P-type well region 521 on the second side.

[0060] In some embodiments, the interface between the gate material layer 600 and the field oxide layer 620 is arc-shaped, with the apex of the arc close to the P-type shielding region 400.

[0061] In some embodiments, the P-type well region 521 has an L-shaped structure; the N-type heavily doped region 531 is formed on the horizontal portion of the P-type well region 521.

[0062] In this embodiment, an N-type heavily doped region 531 in contact with the first side of the gate oxide layer 610 is formed by implanting N-type dopant ions into the region of the first P-well region 251 near the gate oxide layer 610, and an N-type heavily doped region 531 in contact with the second side of the gate oxide layer 610 is formed by implanting N-type dopant ions into the region of the second P-well region 252 near the gate oxide layer 610, thereby forming an L-shaped P-well region 521.

[0063] In some embodiments, the doping concentration of the P-type shielding region 400 exhibits a gradient distribution.

[0064] This application also provides a method for fabricating a trench gate MOSFET, see [link to relevant documentation]. Figure 5 As shown, the preparation method in this embodiment includes steps S100 to S800.

[0065] In step S100, combined Figure 6 As shown, a buffer layer 200, an N-type drift region 300, a current spreading layer 510, a P-type well doped layer 520, an N-type doped layer 530, and a P-type heavily doped region 532 are sequentially formed on the front side of the silicon carbide substrate 100. Under the cover of the first mask 101, a first trench extending into the N-type drift region 300 is formed by etching along the central region of the N-type doped layer 530.

[0066] In this embodiment, combined with Figure 6 As shown in the schematic structure (a), the P-type well doped layer 520 has a concave structure, and the N-type doped layer 530 is located in the groove of the P-type well doped layer 520. Under the cover of the first mask 101, a first trench is etched along the central region of the N-type doped layer 530, extending into the N-type drift region 300. The first trench divides the current spreading layer 510 into left and right opposite current spreading layers 511, divides the P-type well doped layer 520 into left and right opposite P-type well regions 521, and divides the N-type doped layer 530 into left and right heavily doped N-type regions 531. The heavily doped P-type region 532 is located on the P-type well region 521 and is located beside the heavily doped N-type region 531. Figure 6 The schematic structure (b) is shown in the figure.

[0067] In some embodiments, N-type dopant ions can be sequentially implanted onto the front side of the silicon carbide substrate 100 via epitaxial growth or ion implantation to form a buffer layer 200, an N-type drift region 300, and a current spreading layer 510. Then, P-type dopant ions are implanted to form a P-type well doped layer 520, and N-type dopant ions are implanted into a predetermined region of the P-type well doped layer 520 to form an N-type doped layer 530. Figure 2 The schematic structure (a) is shown in the figure.

[0068] In step S200, combined Figure 6 As shown, the first mask 101 is removed, and the first dielectric material 621 is filled into the first trench.

[0069] In this embodiment, the first dielectric material 621 covers the surface areas of the first trench, the P-type well region 521, and the N-type heavily doped region 531.

[0070] In step S300, combined Figure 7 As shown, a second mask 102 is applied to the first dielectric material 621, and the first dielectric material 621 is etched according to the pattern of the second mask 102 to form a first dielectric material layer 622 at the bottom and sidewalls of the first trench, as shown. Figure 7 The schematic structure (b) is shown in the figure. Then the second mask 102 is removed, as shown in the figure. Figure 7 The schematic structure (c) is shown in the figure.

[0071] In this embodiment, the thickness of the first dielectric material layer 622 is less than the thickness of the current spreading layer 511.

[0072] In some embodiments, the thickness of the first dielectric material layer 622 is less than 1 μm.

[0073] In step S400, combined Figure 8 As shown, P-type doped ions are injected along the trench direction of the first trench, so that the P-type doped ions pass through the first dielectric material layer 622 to form a P-type shielding region 400 within the N-type drift region 300, as shown. Figure 8 The schematic structure is shown in (a).

[0074] In step S500, the first dielectric material 623 is deposited to cover the first trench, as follows: Figure 8 As shown in schematic structure (b), a third mask 103 is covered on the first dielectric material 623, as follows. Figure 8 As shown in schematic structure (c), the first dielectric material 623 is etched according to the pattern of the third mask 103 to form a second dielectric material layer 624 at the bottom and sidewalls of the first trench, as follows. Figure 9 The schematic structure is shown in (a).

[0075] In this embodiment, the thickness of the second dielectric material layer 624 is greater than the thickness of the first dielectric material layer 622.

[0076] In step S600, the third mask 103 is removed, as follows: Figure 9 As shown in schematic structure (b), N-type doped ions are then injected along the trench direction of the first trench, so that the N-type doped ions pass through the second dielectric material layer 624 to form an N-type injection region 410 within the P-type shielding region 400, as shown. Figure 9 The schematic structure (c) is shown in the middle.

[0077] In this embodiment, since the thickness of the second dielectric material layer 624 is greater than the thickness of the first dielectric material layer 622, after the inner wall of the first trench is covered by the second dielectric material layer 624, its ion implantation width becomes smaller, thereby the area for implanting N-type doped ions is smaller, making the width of the N-type implantation region 410 smaller than the width of the P-type shielding region 400.

[0078] In some embodiments, the doping concentration of the P-type shielding region 400 exhibits a gradient distribution.

[0079] In some embodiments, the closer a region is to the N-type implantation region 410 within the P-type shielding region 400, the higher its doping concentration.

[0080] In step S700, the second dielectric material layer is removed, such as... Figure 10 As shown in schematic structure (a), the P-type shielding region 400 and the N-type injection region 410 are activated.

[0081] In this embodiment, annealing can be used to activate the doped ions in the P-type shielding region 400 and the N-type implantation region 410, so that a PN junction is formed at the junction of the P-type shielding region 400 and the N-type implantation region 410.

[0082] In some embodiments, the second dielectric material layer 624 may be silicon oxide.

[0083] In step S800, a gate oxide layer 610 is formed at the bottom and sidewalls of the first trench, such as... Figure 10 The schematic structure (b) is shown in the diagram. Combined with... Figure 11 As shown, a gate material layer 600 is formed by filling polysilicon material, and a field oxide layer 620 is formed on the gate material layer 600. Then, a source material is deposited to form a source layer 710 that contacts the P-type well region 521, the N-type heavily doped region 531, the two sides of the gate oxide layer 610, and the field oxide layer 620.

[0084] In this embodiment, the field oxide layer 620 and the gate oxide layer 610 form a closed structure that encloses the gate material layer 600.

[0085] In some embodiments, combined with Figure 10 As shown in schematic structures (b) and (c), after etching away the second dielectric material layer 624, a gate oxide layer 610 can be formed on the device surface, the bottom of the trench, and the inner wall by a thermal oxidation process, and an N-type polysilicon material can be deposited to form a gate material layer 600 as shown in schematic structure (c). The N-type polysilicon material outside the trench is removed by an etching process, as shown in schematic structure (c). Figure 11 As shown in the schematic structure (a), a field oxide layer 620 is formed by depositing field oxide material, as shown in the figure. Figure 11 As shown in the schematic structure (b), the field oxide layer 620 and the gate oxide layer 610 are etched under the cover of the fourth mask 104, as follows. Figure 11 The schematic structure (c) in the diagram and as shown in the diagram Figure 12 The schematic structure is shown in (a). After etching, the fourth mask 104 is removed, as shown in the diagram. Figure 12 The schematic structure (b) is shown in the figure.

[0086] This application also provides a chip including a trench gate MOSFET as described in any of the above embodiments.

[0087] In this embodiment, the chip includes a chip substrate, and the trench gate MOSFET can be disposed on the chip substrate as described in any of the above embodiments.

[0088] In one specific application embodiment, other related semiconductor devices can also be integrated on the chip substrate to form an integrated circuit with the trench gate MOSFET.

[0089] In one specific application embodiment, the chip can be a switch chip or a driver chip.

[0090] The beneficial effects of this application embodiment are as follows: By forming a P-type shielding region on the bottom of a gate oxide layer with concave trenches, and forming an N-type injection region between the P-type shielding region and the bottom of the gate oxide layer, with both ends of the P-type shielding region contacting the bottom edge region of the gate oxide layer, a gate material layer is formed in the trench of the gate oxide layer, and the field oxide layer and the gate oxide layer form a closed structure that encloses the gate material layer. A PN junction is formed between the P-type shielding region and the N-type drift region, and between the P-type shielding region and the N-type injection region. This allows the device to increase the depletion region area under reverse bias, thereby improving the breakdown voltage and achieving the purpose of optimizing the static quality factor.

[0091] Those skilled in the art will clearly understand that, for the sake of convenience and brevity, the above-described division of doped regions and devices is used as an example. In practical applications, the above functions can be assigned to different doped regions and devices as needed, that is, the internal structure of the device can be divided into different doped regions to complete all or part of the functions described above. In the embodiments, the doped regions and devices can be integrated into one unit, or each unit can exist physically separately, or two or more units can be integrated into one unit.

[0092] Furthermore, the specific names of each doped region and device are only for the purpose of distinguishing them from each other and are not intended to limit the scope of protection of this application.

[0093] In the above embodiments, the descriptions of each embodiment have different focuses. For parts that are not described in detail or recorded in a certain embodiment, please refer to the relevant descriptions of other embodiments.

[0094] In addition, in the various embodiments of this application, each doped region can be integrated into one unit, or each unit can exist physically separately, or two or more units can be integrated into one unit.

[0095] The above-described embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of this application, and should all be included within the protection scope of this application.

Claims

1. A trench gate MOSFET, characterized in that, The trench gate MOSFET includes: A silicon carbide substrate and a buffer layer, wherein the buffer layer is formed on the front side of the silicon carbide substrate; An N-type drift region with concave grooves is formed on the buffer layer; A current spreading layer is formed on both sides of the N-type drift region; A P-type well region is formed on the current spreading layer; The P-type shielding area is formed at the bottom of the groove in the N-type drift area; A gate oxide layer with concave trenches is formed on the P-type shielding region, and the height of the gate oxide layer is greater than the sum of the heights of the current spreading layer and the P-type well region; An N-type implantation region is formed between the P-type shielding region and the bottom of the gate oxide layer, and the two ends of the P-type shielding region are respectively in contact with the bottom edge region of the gate oxide layer; The N-type heavily doped region is formed on the P-type well region and located on both sides of the gate oxide layer; A p-type heavily doped region is formed on the p-type well region and located next to the n-type heavily doped region; A gate material layer is formed within a groove in the gate oxide layer; A field oxide layer, together with the gate oxide layer, forms a closed structure that encloses the gate material layer; The source layer is in contact with the P-type well region, the N-type heavily doped region, both sides of the gate oxide layer, and the field oxide layer; A drain layer is formed on the back side of the silicon carbide substrate.

2. The trench gate MOSFET as described in claim 1, characterized in that, The P-type shielding area has a concave or arc-shaped structure, and its two ends are in contact with the bottom sides of the gate oxide layer, respectively.

3. The trench gate MOSFET as described in claim 2, characterized in that, The width of the P-type shielding region is smaller than the width of the bottom of the gate oxide layer.

4. The trench gate MOSFET as described in claim 2, characterized in that, The N-type injection region is opposite to the gate material layer, and the two ends of the P-type shielding region are symmetrically arranged with the N-type injection region as the axis of symmetry.

5. The trench gate MOSFET as claimed in claim 1, characterized in that, The thickness of the two ends of the P-type shielding region is greater than the sidewall thickness of the gate oxide layer.

6. The trench gate MOSFET as claimed in claim 1, characterized in that, The width of the N-type injection region gradually decreases from the source layer to the drain layer.

7. The trench gate MOSFET according to any one of claims 1-6, characterized in that, The thickness of the N-type injection region is less than one-third of the thickness of the P-type shielding region, and the thickness of the N-type injection region is greater than one-fifth of the thickness of the P-type shielding region.

8. The trench gate MOSFET according to any one of claims 1-6, characterized in that, The doping concentration of the P-type shielding region exhibits a gradient distribution.

9. A method for fabricating a trench gate MOSFET, characterized in that, The preparation method includes: A buffer layer, an N-type drift region, a current spreading layer, a P-type well doped layer, an N-type doped layer, and a heavily P-type doped region are sequentially formed on the front side of a silicon carbide substrate. Under the cover of a first mask, a first trench is etched along the central region of the N-type doped layer to penetrate into the N-type drift region. The first trench divides the current spreading layer into oppositely arranged current spreading layers, the P-type well doped layer into oppositely arranged P-type well regions, and the N-type doped layer into oppositely arranged heavily N-type doped regions. The heavily P-type doped region is located on the P-type well region and is located next to the heavily N-type doped region. Remove the first mask and fill the first trench with a first dielectric material; wherein the first dielectric material covers the surface areas of the first trench and the P-type well region and the N-type heavily doped region; A second mask is applied to the first dielectric material, and the first dielectric material is etched according to the pattern of the second mask to form a first dielectric material layer at the bottom and sidewalls of the first trench; wherein the thickness of the first dielectric material layer is less than the thickness of the current spreading layer. P-type doped ions are injected along the trench direction of the first trench, so that the P-type doped ions pass through the first dielectric material layer to form a P-type shielding region in the N-type drift region. The first dielectric material is deposited to cover the first trench, a third mask is deposited on the first dielectric material, and the first dielectric material is etched according to the pattern of the third mask to form a second dielectric material layer at the bottom and sidewalls of the first trench; wherein the thickness of the second dielectric material layer is greater than the thickness of the first dielectric material layer. N-type doped ions are injected along the trench direction of the first trench, so that the N-type doped ions pass through the second dielectric material layer to form an N-type injection region in the P-type shielding region. Remove the second dielectric material layer and activate the P-type shielding region and the N-type injection region; A gate oxide layer is formed at the bottom and sidewalls of the first trench, a gate material layer is formed by filling it with polysilicon material, and a field oxide layer is formed on the gate material layer. Then, a source material is deposited to form a source layer that contacts the P-type well region, the N-type heavily doped region, both sides of the gate oxide layer, and the field oxide layer. The field oxide layer and the gate oxide layer form a closed structure that encloses the gate material layer.

10. A chip, characterized in that, Including the trench gate MOSFET as described in any one of claims 1-8.

Citation Information

Patent Citations

  • Groove gate-type silicon carbide MOSFET device and fabrication method thereof

    CN109904220A

  • Shielded trench devices

    US20190348510A1