A short-process, high-efficiency method for recycling and remelting thick-walled zirconium tube heads.

CN122303600APending Publication Date: 2026-06-30WESTERN TITANIUM TECH

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
WESTERN TITANIUM TECH
Filing Date
2026-05-18
Publication Date
2026-06-30

Smart Images

  • Figure CN122303600A_ABST
    Figure CN122303600A_ABST
Patent Text Reader

Abstract

This invention discloses a short-process, high-efficiency method for recycling and remelting thick-walled zirconium tube heads. The method includes the following steps: Step 1, recycling thick-walled zirconium tube heads, wherein the tube head has a wall thickness greater than 5 mm and a length less than 20 mm; Step 2, encapsulating the recycled thick-walled zirconium tube head in Step 1 with molten zirconium to obtain an ingot; Step 3, subjecting the ingot obtained in Step 2 to VAR melting to obtain a finished zirconium ingot. This invention, by using molten zirconium to encapsulate thick-walled zirconium tube heads, can obtain an ingot that meets the requirements for VAR melting in a single process. Furthermore, VAR melting can be used to prepare a finished zirconium ingot with a chemical composition that meets national standards, achieving a short-process recycling of thick-walled zirconium tube heads. This method is applicable to fields such as nuclear reactors, aerospace, semiconductors and new energy, and petrochemicals.
Need to check novelty before this filing date? Find Prior Art