A suspension containing trifloxystrobin and fluopyram and a preparation method thereof
By using specific component ratios and optimizing the preparation process, the stability and dispersibility issues of azoxystrobin and fluopyram suspensions were resolved, achieving highly efficient control of agricultural and forestry diseases while meeting environmental protection requirements.
Patent Information
- Application Number
- CN202610571575.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-04-28
- Publication Date
- 2026-07-10
Abstract
Description
Technical Field
[0001] This invention relates to pesticide preparation, specifically to a suspension containing oxadiazon and fluopyram and its preparation method. Background Technology
[0002] As a water-based, environmentally friendly formulation, pesticide suspension concentrates have become an important development direction in the pesticide formulation field due to their advantages such as the absence of organic solvent pollution, high efficacy utilization, and relatively safe storage and transportation. Azoxystrobin and fluopyram are two fungicidal active ingredients with different mechanisms of action. Azoxystrobin has a broad-spectrum fungicidal effect and a fast-acting action, while fluopyram has good systemic conductivity and sustained efficacy. The combination of the two can achieve a synergistic fungicidal effect through complementary mechanisms of action, showing high application potential in the control of agricultural and forestry diseases. However, existing technologies for preparing suspension concentrates by combining these two ingredients still have many shortcomings and are difficult to meet practical application needs.
[0003] Existing compound suspensions often suffer from a lack of targeted excipient compatibility. Traditional combinations of wetting and dispersing agents and thickeners can easily lead to insufficient stability of the formulation system, resulting in uneven particle size distribution and poor suspension performance. Furthermore, they are prone to stratification and water separation during storage.
[0004] Meanwhile, existing preparation processes mostly use a single sand milling method, lacking effective homogenization and segmented maturation steps, resulting in uneven dispersion of active ingredients in the system and further reducing the physicochemical stability of the formulation.
[0005] Furthermore, some technologies employ only a single bactericidal ingredient, resulting in limited control efficacy and a short duration of effect. High-concentration compound formulations are prone to system imbalances, and the selection and combination of synergistic components in existing formulations are often unreasonable, failing to fully realize the application effects of compound preparations. Therefore, developing a compound suspension of azoxystrobin and fluopyram with scientifically formulated excipients, optimized preparation process, and good stability has become an urgent technical problem to be solved in the field of pesticide formulation development. Summary of the Invention
[0006] The primary objective of this invention is to provide a suspension containing oxadiazon and fluopyram, and a method for preparing the same.
[0007] A further objective of this invention is to provide a suspension containing oxadiazon and fluopyram, comprising, by mass percentage, the following components: oxadiazon 10%-25%, fluopyram 15%-30%, alkyl naphthalene sulfonate formaldehyde condensate 2%-3%, polycarboxylate derivatives or fatty alcohol polyoxyethylene ether phosphate 3%-4%, nanocellulose 0.2%-0.5%, xanthan gum or magnesium aluminum silicate 0.1%-0.3%, ethylene glycol or propylene glycol 5%-10%, Kathon or phenoxyethanol 0.2%-0.5%, organosilicon defoamer or polyether defoamer 0.5%-1.2%, organosilicon synergist or isotridecyl alcohol polyoxyethylene ether 5%-8%, citric acid or potassium dihydrogen phosphate 2%-5%, and deionized water 5.5%-57%; wherein the purity of the technical grade of oxadiazon and fluopyram is ≥98%, and the particle size of the nanocellulose is 50 nm.
[0008] Preferably, when polycarboxylate derivatives are used, their mass percentage is 3%; when fatty alcohol polyoxyethylene ether phosphate is used, its mass percentage is 3%-4%.
[0009] Preferably, when xanthan gum is used, its mass percentage is 0.1%; when magnesium aluminum silicate is used, its mass percentage is 0.2%-0.3%.
[0010] Preferably, when ethylene glycol is used, its mass percentage is 5%; when propylene glycol is used, its mass percentage is 6%-10%; when Kathon is used, its mass percentage is 0.2%; and when phenoxyethanol is used, its mass percentage is 0.3%-0.5%.
[0011] Preferably, when using a silicone defoamer, its mass percentage is 0.5%; when using a polyether defoamer, its mass percentage is 0.6%-1.2%; when using a silicone synergist, its mass percentage is 5%; and when using isomeric tridecyl alcohol polyoxyethylene ether, its mass percentage is 6%-8%.
[0012] A method for providing the suspension containing oxadiazon and fluopyram includes the following steps: (1) Pre-dispersion: Add deionized water to the reactor, start stirring, and add alkyl naphthalene sulfonate formaldehyde condensate, polycarboxylate derivatives or fatty alcohol polyoxyethylene ether phosphate, nanocellulose, xanthan gum or magnesium aluminum silicate, ethylene glycol or propylene glycol, Kathon or phenoxyethanol, organosilicon defoamer or polyether defoamer, organosilicon synergist or isomeric tridecyl alcohol polyoxyethylene ether, citric acid or potassium dihydrogen phosphate, and stir until the excipients are completely dissolved to form a homogeneous aqueous phase system; (2) Ultrasonic homogenization: The aqueous phase system is transferred to an ultrasonic homogenizer for ultrasonic treatment to break up the tiny air bubbles in the system; (3) Dispersion of active ingredients: Keep the ultrasonic homogenizer stirring and slowly add the technical grade of azoxystrobin and fluopyram. After the addition is complete, continue ultrasonic homogenization to form a coarse dispersion. (4) Gradient sand milling: The coarse dispersion is transferred into the sand mill and the speed is adjusted in two stages for sand milling. (5) Segmented maturation: The dispersion after sand milling is transferred to a maturation kettle and the temperature is adjusted in two stages for constant temperature maturation treatment; (6) Testing and packaging: Samples are taken to test the performance of the formulation. After passing the test, the finished product is measured and packaged.
[0013] Preferably, in step (1), the stirring speed is 1000r / min-1200r / min and the stirring time is 20min-25min.
[0014] Preferably, in step (2), the ultrasonic power is 500W-700W and the ultrasonic treatment time is 15min-18min; in step (3), the stirring speed is 400r / min-450r / min and the ultrasonic homogenization time is 20min-22min.
[0015] Preferably, in step (4), the first stage of gradient sand milling has a milling speed of 1300 r / min-1400 r / min and a milling time of 25 min-30 min; the second stage has a milling speed of 2000 r / min-2100 r / min and a milling time of 45 min-50 min; the particle size distribution D50 of the formulation after sand milling is 2.1 μm-3.2 μm and the Span value is 1.5-1.8.
[0016] Preferably, in step (5), the first stage of the segmented maturation is at a constant temperature of 35℃-38℃ and the maturation time is 25min-28min; the second stage is at a constant temperature of 22℃-23℃ and the maturation time is 15min-18min; after maturation, the dispersion system is uniform without stratification or water separation.
[0017] Compared with the prior art, the beneficial effects of the present invention are: 1. The suspension concentrate containing oxadiazon and fluopyram and its preparation method provided by this invention effectively solve the technical problems of poor stability, uneven component dispersion, and poor application effect of existing compound suspension concentrates, and has many technical advantages. This invention scientifically combines oxadiazon and fluopyram, and utilizes the complementarity of their mechanisms of action to achieve synergistic effect, making up for the shortcomings of single fungicidal components, broadening the fungicidal spectrum, improving the control effect on target diseases, and extending the field residual effect of the formulation, thus meeting the disease control needs in agricultural and forestry production.
[0018] 2. This invention optimizes the excipient formulation system by selecting specific types of wetting and dispersing agents and thickeners for compound use, and introducing nanocellulose as a key component. This effectively improves the wetting, dispersibility, and suspension properties of the formulation, optimizes the particle size distribution, avoids stratification and water separation during storage, and significantly enhances the physical and chemical stability of the formulation. Simultaneously, this invention systematically optimizes the preparation process, designing a continuous process of pre-dispersion, ultrasonic homogenization, gradient sand milling, and segmented maturation. The process parameters are well-matched, ensuring uniform dispersion of the active ingredients in the aqueous system, further guaranteeing the stability of the formulation system. Furthermore, this process has a wide range of applicability, capable of stably preparing compound suspensions with different concentration ratios, suitable for various field application scenarios.
[0019] 3. The formulation of this invention is a water-based formulation, which reduces the use of organic solvents, lowers environmental pollution and potential harm to applicators, and conforms to the development trend of green and environmentally friendly pesticide formulations.
[0020] 4. The preparation process of the present invention is simple to operate, and each step is easy to control. It is suitable for large-scale industrial production and has good economic benefits and market application value. Detailed Implementation
[0021] The technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention. Example 1:
[0022] The raw material composition by mass percentage is as follows: 10% azoxystrobin, 15% fluopyram, 3% polycarboxylate derivative PC-100, 2% alkyl naphthalene sulfonate formaldehyde condensate, 0.2% nanocellulose (particle size 50nm), 0.1% xanthan gum, 5% ethylene glycol, 0.2% Kathon, 0.5% organosilicon defoamer SIM-600, 5% organosilicon synergist Prime, 2% citric acid, and 57% deionized water; the purity of both azoxystrobin and fluopyram technical grade is ≥98%.
[0023] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, and control the speed at 1000 r / min. Add the above-mentioned polycarboxylate derivatives, alkyl naphthalene sulfonate formaldehyde condensate, nanocellulose, xanthan gum, ethylene glycol, Kathon, organosilicon defoamer, organosilicon synergist Prime, and citric acid in sequence. Stir for 20 min until all excipients are completely dissolved to form a homogeneous aqueous phase system. Ultrasonic homogenization: The aqueous phase system is transferred into a JY92-IIN ultrasonic homogenizer. The ultrasonic power is controlled at 500W and the ultrasonic time is 15min to break up the tiny air bubbles in the system and promote the uniform dispersion of the excipients. Dispersion of active ingredients: Keep the ultrasonic homogenizer speed at 400 r / min, slowly add azoxystrobin and fluopyram technical materials, and continue ultrasonic homogenization for 20 min after the addition is complete to form a coarse dispersion; Gradient milling: The coarse dispersion was transferred to a WSB-30 mill and milled at 1300 r / min for 25 min. Then the speed was adjusted to 2000 r / min and milled for another 45 min. The particle size distribution D50 of the formulation was found to be 3.2 μm and the Span value was 1.8. Segmented maturation: The dispersion after sand milling is transferred to SH-100 maturation kettle, and then the mixture is kept at 35℃ for 25 minutes. Then the temperature is lowered to 22℃ and the maturation continues for 15 minutes. The system is uniform and without stratification. Testing and Packaging: Conventional testing equipment such as laser particle size analyzer and rotational rheometer are used to sample and test the performance of the formulation. After passing the test, the formulation is metered and packaged to obtain the finished product. Example 2:
[0024] The raw material composition by mass percentage is as follows: 15% azoxystrobin, 20% fluopyram, 3% polycarboxylate derivative PC-100, 2% alkyl naphthalene sulfonate formaldehyde condensate, 0.2% nanocellulose (particle size 50nm), 0.1% xanthan gum, 5% ethylene glycol, 0.2% Kathon, 0.5% organosilicon defoamer SIM-600, 5% organosilicon synergist Prime, 2% citric acid, and 47% deionized water; the purity of both azoxystrobin and fluopyram technical grade is ≥98%.
[0025] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, and control the speed at 1000 r / min. Add the above-mentioned polycarboxylate derivatives, alkyl naphthalene sulfonate formaldehyde condensate, nanocellulose, xanthan gum, ethylene glycol, Kathon, organosilicon defoamer, organosilicon synergist Prime, and citric acid in sequence. Stir for 20 min until all excipients are completely dissolved to form a homogeneous aqueous phase system. Ultrasonic homogenization: The aqueous phase system is transferred into a JY92-IIN ultrasonic homogenizer. The ultrasonic power is controlled at 500W and the ultrasonic time is 15min to break up the tiny air bubbles in the system and promote the uniform dispersion of the excipients. Dispersion of active ingredients: Keep the ultrasonic homogenizer speed at 400 r / min, slowly add azoxystrobin and fluopyram technical materials, and continue ultrasonic homogenization for 20 min after the addition is complete to form a coarse dispersion; Gradient milling: The coarse dispersion was transferred to a WSB-30 mill and milled at 1300 r / min for 25 min. Then the speed was adjusted to 2000 r / min and milled for another 45 min. The particle size distribution D50 of the formulation was found to be 2.8 μm and the Span value was 1.7. Segmented maturation: The dispersion after sand milling was transferred to an SH-100 maturation kettle, and then the mixture was kept at a constant temperature of 35℃ for 25 minutes. Then the temperature was lowered to 22℃ and the maturation was continued for 15 minutes. The system showed good stability and no stratification. Testing and Packaging: The performance of the formulation is tested using conventional testing equipment. Once it passes the test, it is metered and packaged to obtain the finished product. Example 3:
[0026] The raw material composition by mass percentage is as follows: 15% azoxystrobin, 20% fluopyram, 3% fatty alcohol polyoxyethylene ether phosphate POE-10, 2% alkyl naphthalene sulfonate formaldehyde condensate, 0.3% nanocellulose (particle size 50nm), 0.2% magnesium aluminum silicate, 6% propylene glycol, 0.3% phenoxyethanol, 0.6% polyether defoamer PE-6800, 6% isomeric tridecyl alcohol polyoxyethylene ether, 2.5% potassium dihydrogen phosphate, and 44.4% deionized water; the purity of both azoxystrobin and fluopyram technical grade is ≥98%.
[0027] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, and control the speed at 1000 r / min. Add the above-mentioned fatty alcohol polyoxyethylene ether phosphate, alkyl naphthalene sulfonate formaldehyde condensate, nanocellulose, magnesium aluminum silicate, propylene glycol, phenoxyethanol, polyether defoamer, isomeric tridecyl alcohol polyoxyethylene ether, and potassium dihydrogen phosphate in sequence. Stir for 20 min until all excipients are completely dissolved to form a homogeneous aqueous phase system. Ultrasonic homogenization: The aqueous phase system is transferred into a JY92-IIN ultrasonic homogenizer. The ultrasonic power is controlled at 600W and the ultrasonic time is 15min to break up the tiny air bubbles in the system and promote the uniform dispersion of the excipients. Dispersion of active ingredients: Keep the ultrasonic homogenizer speed at 400 r / min, slowly add azoxystrobin and fluopyram technical materials, and continue ultrasonic homogenization for 20 min after the addition is complete to form a coarse dispersion; Gradient milling: The coarse dispersion was transferred to a WSB-30 mill and milled at 1300 r / min for 25 min. Then the speed was adjusted to 2000 r / min and milled for another 45 min. The particle size distribution D50 of the formulation was found to be 2.5 μm and the Span value was 1.6. Segmented maturation: The dispersion after sand milling was transferred to an SH-100 maturation kettle, and then the mixture was kept at a constant temperature of 35℃ for 25 minutes. Then the temperature was lowered to 22℃ and the maturation was continued for 15 minutes. The system had good fluidity and good suspension stability. Testing and Packaging: The performance of the formulation is tested using conventional testing equipment. Once it passes the test, it is metered and packaged to obtain the finished product. Example 4:
[0028] The raw material composition by mass percentage is as follows: 15% azoxystrobin, 20% fluopyram, 3% fatty alcohol polyoxyethylene ether phosphate POE-10, 2% alkyl naphthalene sulfonate formaldehyde condensate, 0.3% nanocellulose (particle size 50nm), 0.2% magnesium aluminum silicate, 6% propylene glycol, 0.3% phenoxyethanol, 0.6% polyether defoamer PE-6800, 6% isomeric tridecyl alcohol polyoxyethylene ether, 2.5% potassium dihydrogen phosphate, and 44.4% deionized water; the purity of both azoxystrobin and fluopyram technical grade is ≥98%.
[0029] Preparation steps: Pre-dispersion: Adjust the stirring speed to 1200 r / min and extend the stirring time to 25 min; Ultrasonic homogenization: The ultrasonic power was adjusted to 700W, and the ultrasonic time was extended to 18 minutes; Dispersion of active ingredients: The speed of the ultrasonic homogenizer was adjusted to 450 r / min, and the ultrasonic homogenization time was extended to 22 min; Gradient sand milling: First, mill at 1400 r / min for 30 min, then adjust the speed to 2100 r / min and continue milling for 50 min; Segmented ripening: First, ripen at a constant temperature of 38℃ for 28 minutes, then cool down to 23℃ and continue ripening for 18 minutes; 6. Inspection and packaging: After passing the inspection, package to obtain the finished product. After sand milling, the particle size distribution D50 is 2.1μm and the Span value is 1.5. Example 5:
[0030] The raw material composition by mass percentage is as follows: 25% azoxystrobin, 30% fluopyram, 4% fatty alcohol polyoxyethylene ether phosphate POE-10, 3% alkyl naphthalene sulfonate formaldehyde condensate, 0.5% nanocellulose (particle size 50nm), 0.3% magnesium aluminum silicate, 10% propylene glycol, 0.5% phenoxyethanol, 1.2% polyether defoamer PE-6800, 8% isomeric tridecyl alcohol polyoxyethylene ether, 5% potassium dihydrogen phosphate, and 5.5% deionized water; the purity of both azoxystrobin and fluopyram technical grade is ≥98%.
[0031] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, and control the speed at 1200 r / min. Add the above-mentioned fatty alcohol polyoxyethylene ether phosphate, alkyl naphthalene sulfonate formaldehyde condensate, nanocellulose, magnesium aluminum silicate, propylene glycol, phenoxyethanol, polyether defoamer, isomeric tridecyl alcohol polyoxyethylene ether, and potassium dihydrogen phosphate in sequence. Stir for 25 min until all excipients are completely dissolved to form a homogeneous aqueous phase system. Ultrasonic homogenization: The aqueous phase system was transferred into a JY92-IIN ultrasonic homogenizer. The ultrasonic power was controlled at 700W and the ultrasonic time was 18min to break up the tiny air bubbles in the system and promote the uniform dispersion of the excipients. Dispersion of active ingredients: Keep the ultrasonic homogenizer speed at 450 r / min, slowly add azoxystrobin and fluopyram technical materials, and continue ultrasonic homogenization for 22 min after the addition is complete to form a coarse dispersion; Gradient milling: The coarse dispersion was transferred to a WSB-30 mill and milled at 1400 r / min for 30 min. Then the speed was adjusted to 2100 r / min and milled for another 50 min. The particle size distribution D50 of the formulation was found to be 2.3 μm and the Span value was 1.7. Segmented maturation: The dispersion after sand milling was transferred to an SH-100 maturation kettle, and then the mixture was kept at a constant temperature of 38℃ for 28 minutes. Then the temperature was lowered to 23℃ and the maturation continued for 18 minutes. The system showed no stratification, no water separation, and good fluidity. Testing and Packaging: The performance of the formulation is tested using conventional testing equipment. Once it passes the test, it is metered and packaged to obtain the finished product.
[0032] Comparative Example 1: The raw material composition by mass percentage is as follows: 25% oxime ester, 3% polycarboxylate derivative PC-100, 2% alkyl naphthalene sulfonate formaldehyde condensate, 0.3% xanthan gum, 5% ethylene glycol, 0.2% Kathon, 0.5% organosilicon defoamer SIM-600, 2% citric acid, and 62% deionized water; the purity of oxime ester technical grade is ≥98%.
[0033] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, control the speed at 1000 r / min, and add the above polycarboxylate derivatives, alkyl naphthalene sulfonate formaldehyde condensate, xanthan gum, ethylene glycol, Kathon, organosilicon defoamer, and citric acid in sequence. Stir for 20 min until all excipients are completely dissolved to form a homogeneous aqueous phase system. Ultrasonic homogenization: The aqueous phase system is transferred into a JY92-IIN ultrasonic homogenizer. The ultrasonic power is controlled at 500W and the ultrasonic time is 15min to break up the tiny air bubbles in the system and promote the uniform dispersion of the excipients. Dispersion of active ingredients: Keep the ultrasonic homogenizer speed at 400 r / min, slowly add the oxadiazon technical material, and continue ultrasonic homogenization for 20 min after the addition is complete to form a coarse dispersion; Gradient milling: The coarse dispersion was transferred to a WSB-30 mill and milled at 1300 r / min for 25 min. Then the speed was adjusted to 2000 r / min and milled for another 45 min. The particle size distribution D50 of the formulation was found to be 3.5 μm and the Span value was 2.2. Segmented maturation: The dispersion after sand milling was transferred to an SH-100 maturation kettle, and then maturated at a constant temperature of 35℃ for 25 minutes. The temperature was then lowered to 22℃ and maturated for another 15 minutes. No obvious stratification was observed in the system. Packaging testing: The performance of the formulation was tested using conventional testing equipment, and relevant performance indicators were recorded.
[0034] Comparative Example 2: The raw material composition by mass percentage is as follows: 10% oxadiazon, 15% fluopyram, 5% sodium lignosulfonate, 0.3% xanthan gum, 5% ethylene glycol, 0.2% Kathon, 0.5% silicone defoamer SIM-600, 2% citric acid, and 66% deionized water; the purity of both oxadiazon and fluopyram technical grade is ≥98%, and the sodium lignosulfonate is a conventional industrial-grade product.
[0035] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, control the speed at 1000 r / min, and add sodium lignosulfonate, xanthan gum, ethylene glycol, Kathon, organosilicon defoamer, and citric acid in sequence. Stir for 20 min until all the excipients are completely dissolved to form a homogeneous aqueous phase system. Ultrasonic homogenization: The aqueous phase system is transferred into a JY92-IIN ultrasonic homogenizer. The ultrasonic power is controlled at 500W and the ultrasonic time is 15min to break up the tiny air bubbles in the system and promote the uniform dispersion of the excipients. Dispersion of active ingredients: Keep the ultrasonic homogenizer speed at 400 r / min, slowly add azoxystrobin and fluopyram technical materials, and continue ultrasonic homogenization for 20 min after the addition is complete to form a coarse dispersion; Gradient milling: The coarse dispersion was transferred to a WSB-30 mill and milled at 1300 r / min for 25 min. Then the speed was adjusted to 2000 r / min and milled for another 45 min. The particle size distribution D50 of the formulation was found to be 4.1 μm and the Span value was 2.5. Segmented maturation: The dispersion after sand milling was transferred to an SH-100 maturation kettle, and then maturated at a constant temperature of 35℃ for 25 minutes. The temperature was then lowered to 22℃ and maturated for another 15 minutes. No obvious stratification was observed in the system. 6. Testing and packaging: The performance of the formulation was tested using conventional testing equipment, and relevant performance indicators were recorded.
[0036] Comparative Example 3: The raw material composition by mass percentage is as follows: 10% azoxystrobin, 15% fluopyram, 3% polycarboxylate derivative PC-100, 2% alkyl naphthalene sulfonate formaldehyde condensate, 0.2% nanocellulose (particle size 50nm), 0.1% xanthan gum, 5% ethylene glycol, 0.2% Kathon, 0.5% organosilicon defoamer SIM-600, 5% organosilicon synergist Prime, 2% citric acid, and 57% deionized water; the purity of both azoxystrobin and fluopyram technical grade is ≥98%.
[0037] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, and control the speed at 1000 r / min. Add the above-mentioned polycarboxylate derivatives, alkyl naphthalene sulfonate formaldehyde condensate, nanocellulose, xanthan gum, ethylene glycol, Kathon, organosilicon defoamer, organosilicon synergist Prime, and citric acid in sequence. Stir for 20 min until all excipients are completely dissolved to form a homogeneous aqueous phase system. Dispersion of active ingredients: While maintaining a stirring speed of 400 r / min, slowly add azoxystrobin and fluopyram technical grade. After the addition is complete, continue stirring for 20 min to form a coarse dispersion. Single sand milling: The coarse dispersion was transferred to a WSB-30 sand mill and milled at 1800 r / min for 60 min. The particle size distribution D50 of the formulation was found to be 3.8 μm and the Span value was 2.3. Direct packaging: The formulation performance is tested using conventional testing equipment, and the relevant performance indicators are recorded before direct packaging.
[0038] Comparative Example 4: The raw material composition by mass percentage is as follows: 30% oxadiazon, 35% fluopyram, 3% polycarboxylate derivative PC-100, 2% alkyl naphthalene sulfonate formaldehyde condensate, 0.2% nanocellulose (particle size 50nm), 0.1% xanthan gum, 5% ethylene glycol, 0.2% Kathon, 0.5% organosilicon defoamer SIM-600, 5% organosilicon synergist Prime, 2% citric acid, and 17% deionized water; the purity of both oxadiazon and fluopyram technical grade is ≥98%.
[0039] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, and control the speed at 1000 r / min. Add the above-mentioned polycarboxylate derivatives, alkyl naphthalene sulfonate formaldehyde condensate, nanocellulose, xanthan gum, ethylene glycol, Kathon, organosilicon defoamer, organosilicon synergist Prime, and citric acid in sequence. Stir for 20 min until all excipients are completely dissolved to form a homogeneous aqueous phase system. Ultrasonic homogenization: The aqueous phase system is transferred into a JY92-IIN ultrasonic homogenizer. The ultrasonic power is controlled at 500W and the ultrasonic time is 15min to break up the tiny air bubbles in the system and promote the uniform dispersion of the excipients. Dispersion of active ingredients: Keep the ultrasonic homogenizer speed at 400 r / min, slowly add azoxystrobin and fluopyram technical materials, and continue ultrasonic homogenization for 20 min after the addition is complete to form a coarse dispersion; Gradient milling: The coarse dispersion was transferred to a WSB-30 mill and milled at 1300 r / min for 25 min. Then the speed was adjusted to 2000 r / min and milled for another 45 min. The particle size distribution D50 of the formulation was found to be 4.5 μm and the Span value was 2.7. Slight stratification of the formulation was observed. Segmented maturation: The dispersion after sand milling is transferred to SH-100 maturation kettle, and first maturated at a constant temperature of 35℃ for 25 minutes, then cooled to 22℃ and continued maturation for 15 minutes; Packaging testing: The performance of the formulation was tested using conventional testing equipment, and relevant performance indicators were recorded.
[0040] Comparative Example 5: The raw material composition by mass percentage is as follows: 10% oxime-methyl ester, 15% fluopyram, 3% polycarboxylate derivative PC-100, 2% alkyl naphthalene sulfonate formaldehyde condensate, 0.2% nanocellulose (particle size 50nm), 0.1% xanthan gum, 5% ethylene glycol, 0.2% Kathon, 0.5% organosilicon defoamer SIM-600, 2% citric acid, and 62% deionized water; the purity of both oxime-methyl ester and fluopyram technical grade is ≥98%.
[0041] Preparation steps: Pre-dispersion: Add deionized water to a JY-500 reactor, turn on the stirring device, and control the speed at 1000 r / min. Add the above-mentioned polycarboxylate derivatives, alkyl naphthalene sulfonate formaldehyde condensate, nanocellulose, xanthan gum, ethylene glycol, Kathon, organosilicon defoamer, and citric acid in sequence. Stir for 20 min until all excipients are completely dissolved to form a homogeneous aqueous phase system. Ultrasonic homogenization: The aqueous phase system is transferred into a JY92-IIN ultrasonic homogenizer. The ultrasonic power is controlled at 500W and the ultrasonic time is 15min to break up the tiny air bubbles in the system and promote the uniform dispersion of the excipients. Dispersion of active ingredients: Keep the ultrasonic homogenizer speed at 400 r / min, slowly add azoxystrobin and fluopyram technical materials, and continue ultrasonic homogenization for 20 min after the addition is complete to form a coarse dispersion; Gradient milling: The coarse dispersion was transferred to a WSB-30 mill and milled at 1300 r / min for 25 min. Then the speed was adjusted to 2000 r / min and milled for another 45 min. The particle size distribution D50 of the formulation was found to be 3.3 μm and the Span value was 1.9. Segmented maturation: The dispersion after sand milling was transferred to an SH-100 maturation kettle, and then maturated at a constant temperature of 35℃ for 25 minutes. The temperature was then lowered to 22℃ and maturated for another 15 minutes. No obvious stratification was observed in the system. Packaging testing: The performance of the formulation was tested using conventional testing equipment, and relevant performance indicators were recorded.
[0042] Performance testing and results analysis: The suspensions prepared in Examples 1 to 5 and Comparative Examples 1 to 5 were subjected to comprehensive performance tests, including physical properties, chemical properties, stability properties, and field efficacy properties. The test methods were in accordance with relevant national standards and industry specifications to ensure that the test data were authentic, reliable, and repeatable. The test results are shown in the table below.
[0043] Test items and methods: Physical property testing: Particle size distribution was measured using a laser particle size analyzer, referring to ISO 13320 standard, to determine D50 and Span values; viscosity was measured using a rotational rheometer, referring to ISO 3219 standard, at 25°C; suspension rate was measured according to CIPACMT184 standard, to determine the suspension rate of the formulation in water at 25°C; wetting time was measured according to ASTM D7334 standard.
[0044] Chemical performance testing: pH value was determined using a pH meter in accordance with GB / T9724 standard; active ingredient content and degradation rate were determined using an ultraviolet spectrophotometer in accordance with relevant industry standards, including the content of oxadiazon and fluopyram in the formulation, as well as the degradation rate after heat storage.
[0045] Stability performance tests: Thermal storage stability: The formulation was placed in a constant temperature incubator at 54±2℃ for 14 days. After removal, the appearance was observed, and the suspension rate and active ingredient degradation rate were measured. According to industry standards, there should be no stratification or water separation, the suspension rate should be ≥90%, and the active ingredient degradation rate should be ≤5%. Freeze-thaw stability: The formulation was placed in a constant temperature incubator at -10℃ for 24 hours. After removal, it was brought to room temperature, and the appearance was observed. This cycle was repeated 3 times. There should be no stratification or crystallization, and the formulation should be able to return to a homogeneous state after stirring. Room temperature stability: The formulation was placed in a room temperature environment at 25±2℃ for 6 months. The appearance was observed periodically, and the suspension rate was measured. There should be no stratification or water separation, and the suspension rate should be ≥90%.
[0046] Field efficacy test: Wheat powdery mildew and cucumber downy mildew were selected as the test diseases. The same dosage was set, and three replicate plots were set for each treatment. Water was used as a blank control. The disease index was investigated at 7, 14 and 21 days after the application. The control effect was calculated to verify the field application effect and duration of the formulation.
[0047] The test results are shown in Table 1 below: Table 1: Group D50 / μm Span value Viscosity / mPa·s Suspension rate / % Wetting time / s pH value Thermal storage degradation rate / % 7 days after medication, efficacy / % 14 days after medication, efficacy / % 21 days after medication, efficacy / % stability Example 1 3.2 1.8 280 95.6 45 6.2 2.8 88.5 85.2 83.2 good Example 2 2.8 1.7 300 96.3 40 6.3 2.5 90.1 87.6 85.7 good Example 3 2.5 1.6 320 97.1 35 6.4 2.1 92.4 89.8 87.3 good Example 4 2.1 1.5 330 98.2 30 6.3 1.2 95.3 92.1 88.7 good Example 5 2.3 1.7 350 92.5 60 6.1 3.8 89.2 86.5 82.3 good Comparative Example 1 3.5 2.2 280 88.3 75 6.2 4.5 75.3 68.5 59.2 generally Comparative Example 2 4.1 2.5 320 85.7 82 6.3 6.8 78.6 70.3 62.5 Poor Comparative Example 3 3.8 2.3 290 87.9 78 6.2 5.9 80.2 72.8 65.1 generally Comparative Example 4 4.5 2.7 400 82.1 90 6.1 8.5 72.1 65.7 57.8 Poor Comparative Example 5 3.3 1.9 270 90.2 65 6.2 4.2 83.5 76.2 69.8 good Results analysis: The test results above show that the suspension concentrates containing oxadiazon and fluopyram prepared in Examples 1 to 5 of this invention exhibit excellent performance in all aspects, and there is a trend of gradual optimization among the examples. Example 1, as the basic scheme, meets industry standards in all aspects, with a suspension rate of 95.6%, a heat storage degradation rate of 2.8%, and a control efficacy of 83.2% 21 days after application, demonstrating good stability, proving that the basic scheme of this invention can be stably implemented. Example 2, by adjusting the ratio of effective components, increases the total content of effective components to 35%, and compared with Example 1, the suspension rate increases to 96.3%, the heat storage degradation rate decreases to 2.5%, and the field control efficacy is significantly improved, proving that the scheme of this invention can still maintain excellent performance under different ratios of effective components. Example 3, by replacing the types and some ratios of excipients, uses a compound of fatty alcohol polyoxyethylene ether phosphate and alkyl naphthalene sulfonate formaldehyde condensate as a wetting and dispersing agent, and a compound of nanocellulose and magnesium aluminum silicate as a thickener, further optimizing the wetting, dispersibility, and suspension stability of the formulation, achieving a suspension rate of 97.1%, shortening the wetting time to 35s, and improving the heat storage degradation rate. The thermal degradation rate decreased to 2.1%, and the field efficacy was further improved, demonstrating the rationality and suitability of the excipient combination of the present invention. In Example 4, by optimizing the preparation process parameters and adjusting the parameters of ultrasonic homogenization, gradient sand milling, and segmented maturation, the particle size uniformity of the formulation was significantly improved, the D50 decreased to 2.1 μm, the Span value was 1.5, the suspension rate reached 98.2%, the thermal degradation rate was only 1.2%, and the field efficacy reached 88.7%, with all performances reaching the optimal level, proving the role of process parameter optimization in improving formulation performance. In Example 5, using the extreme raw material ratio, the total content of active ingredients reached 55%, and the excipient ratio was also at a high level, but the formulation still maintained good performance, with a suspension rate of 92.5%, a thermal degradation rate of 3.8%, and a field efficacy of 82.3%, all meeting the requirements for field use, proving that the scheme of the present invention has a wide range of applicability and can achieve stable preparation of formulations of different concentrations.
[0048] Comparative Example 1, without the addition of fluopyram, used only azoxystrobin as the active ingredient, resulting in a suspension rate of 88.3% and a significant decrease in field efficacy. At 21 days post-application, the efficacy was only 59.2%, and the stability was generally poor. This demonstrates that the combination of azoxystrobin and fluopyram can achieve synergistic effects, which is one of the key aspects of this invention. Comparative Example 2 used a traditional single wetting and dispersing agent without nanocellulose or synergists, resulting in a larger particle size, a suspension rate of 85.7%, and a thermal degradation rate of 6.8%, exceeding industry standards. This led to lower field efficacy and poor stability, demonstrating the innovation and necessity of the novel excipient combination in this invention. Comparative Example 3 omitted ultrasonic homogenization and segmented maturation steps, using a traditional single sand milling process, resulting in uneven particle size in the formulation. The suspension rate was 87.9%, and the thermal degradation rate was 5.9%, exceeding industry standards. However, the field efficacy was lower than that of the example, demonstrating that the optimization of the preparation process of this invention can significantly improve the performance of the formulation. Comparative Example 4 had an effective ingredient ratio that exceeded the range of this invention, resulting in slight stratification of the formulation. The suspension rate was only 82.1%, and the thermal degradation rate was 8.5%, exceeding industry standards. The field efficacy was the lowest, demonstrating the scientific and rational nature of the raw material ratio of this invention. Exceeding this ratio range would not achieve good formulation performance. Comparative Example 5 did not add any synergist. Although it had good stability, the suspension rate, wetting time, and field efficacy were all lower than those of the example, demonstrating that the addition of the synergist can significantly improve the field application effect of the formulation and is an important part of this invention.
[0049] The preferred embodiments of the present invention disclosed above are merely illustrative of the invention. These preferred embodiments do not exhaustively describe all details, nor do they limit the invention to the specific implementations described. Clearly, many modifications and variations can be made based on the content of this specification. This specification selects and specifically describes these embodiments to better explain the principles and practical applications of the invention, thereby enabling those skilled in the art to better understand and utilize the invention.
Claims
1. A suspension containing oxadiazon and fluopyram, characterized in that, The product comprises, by weight percentage, the following components: 10%-25% oxime-methyl ester, 15%-30% fluopyram, 2%-3% alkyl naphthalene sulfonate formaldehyde condensate, 3%-4% polycarboxylate derivatives or fatty alcohol polyoxyethylene ether phosphate, 0.2%-0.5% nanocellulose, 0.1%-0.3% xanthan gum or magnesium aluminum silicate, 5%-10% ethylene glycol or propylene glycol, 0.2%-0.5% Kathon or phenoxyethanol, 0.5%-1.2% organosilicon defoamer or polyether defoamer, 5%-8% organosilicon synergist or isotridecyl alcohol polyoxyethylene ether, 2%-5% citric acid or potassium dihydrogen phosphate, and 5.5%-57% deionized water; the purity of the technical grade of oxime-methyl ester and fluopyram is ≥98%, and the particle size of the nanocellulose is 50 nm.
2. The suspension concentrate containing oxadiazon and fluopyram according to claim 1, characterized in that, When polycarboxylate derivatives are used, their mass percentage is 3%; when fatty alcohol polyoxyethylene ether phosphate is used, its mass percentage is 3%-4%.
3. The suspension concentrate containing oxadiazon and fluopyram according to claim 1, characterized in that, When xanthan gum is used, its mass percentage is 0.1%; when magnesium aluminum silicate is used, its mass percentage is 0.2%-0.3%.
4. The suspension concentrate containing oxadiazon and fluopyram according to claim 1, characterized in that, When ethylene glycol is used, its mass percentage is 5%; when propylene glycol is used, its mass percentage is 6%-10%; when Kathon is used, its mass percentage is 0.2%; and when phenoxyethanol is used, its mass percentage is 0.3%-0.5%.
5. The suspension concentrate containing oxadiazon and fluopyram according to claim 1, characterized in that, When using silicone-based defoamers, the mass percentage is 0.5%; when using polyether-based defoamers, the mass percentage is 0.6%-1.2%; when using silicone synergists, the mass percentage is 5%; and when using isomeric tridecyl alcohol polyoxyethylene ether, the mass percentage is 6%-8%.
6. A method for preparing a suspension containing oxadiazon and fluopyram as described in any one of claims 1 to 5, characterized in that, Includes the following steps: (1) Pre-dispersion: Add deionized water to the reactor, start stirring, and add alkyl naphthalene sulfonate formaldehyde condensate, polycarboxylate derivatives or fatty alcohol polyoxyethylene ether phosphate, nanocellulose, xanthan gum or magnesium aluminum silicate, ethylene glycol or propylene glycol, Kathon or phenoxyethanol, organosilicon defoamer or polyether defoamer, organosilicon synergist or isomeric tridecyl alcohol polyoxyethylene ether, citric acid or potassium dihydrogen phosphate, and stir until the excipients are completely dissolved to form a homogeneous aqueous phase system; (2) Ultrasonic homogenization: The aqueous phase system is transferred to an ultrasonic homogenizer for ultrasonic treatment to break up the tiny air bubbles in the system; (3) Dispersion of active ingredients: Keep the ultrasonic homogenizer stirring and slowly add the technical grade of azoxystrobin and fluopyram. After the addition is complete, continue ultrasonic homogenization to form a coarse dispersion. (4) Gradient sand milling: The coarse dispersion is transferred into the sand mill and the speed is adjusted in two stages for sand milling. (5) Segmented maturation: The dispersion after sand milling is transferred to a maturation kettle and the temperature is adjusted in two stages for constant temperature maturation treatment; (6) Testing and packaging: Samples are taken to test the performance of the formulation. After passing the test, the finished product is measured and packaged.
7. The preparation method according to claim 6, characterized in that, In step (1), the stirring speed is 1000r / min-1200r / min and the stirring time is 20min-25min.
8. The preparation method according to claim 6, characterized in that, In step (2), the ultrasonic power is 500W-700W and the ultrasonic treatment time is 15min-18min; in step (3), the stirring speed is 400r / min-450r / min and the ultrasonic homogenization time is 20min-22min.
9. The preparation method according to claim 6, characterized in that, In step (4), the first stage of gradient sand milling has a milling speed of 1300 r / min-1400 r / min and a milling time of 25 min-30 min; the second stage has a milling speed of 2000 r / min-2100 r / min and a milling time of 45 min-50 min; the particle size distribution D50 of the formulation after sand milling is 2.1 μm-3.2 μm and the Span value is 1.5-1.
8.
10. The preparation method according to claim 6, characterized in that, In step (5), the first stage of the segmented maturation is at a constant temperature of 35℃-38℃ and the maturation time is 25min-28min; the second stage is at a constant temperature of 22℃-23℃ and the maturation time is 15min-18min; after maturation, the dispersion system is uniform without stratification or water separation.