通讯线缆用辐照交联型耐油高抗撕低烟无卤高阻燃护套材料及其制备方法

The communication cable sheath material prepared by using specific raw material components and irradiation crosslinking process solves the problems of insufficient oil resistance and tear resistance, and achieves low smoke, halogen-free, high flame retardancy and improved mechanical properties.

CN122404833APending Publication Date: 2026-07-17SUZHOU PUMA NEW MATERIAL CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
SUZHOU PUMA NEW MATERIAL CO LTD
Filing Date
2026-05-25
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

Existing communication cable sheath materials do not meet the requirements for communication cable use in terms of oil resistance and tear resistance, and there is also the problem of halogen release.

Method used

Sheath materials are prepared by using specific types and amounts of raw material components, including ethylene-vinyl acetate copolymer, ethylene-butyl acrylate copolymer, compatibilizer, composite flame retardant, lubricant, anti-aging and antioxidant agent, and crosslinking agent, through an irradiation crosslinking process.

Benefits of technology

After irradiation crosslinking, the material exhibits high tear resistance, low smoke and halogen-free properties, high flame retardancy, oil resistance that meets the MIL-DTL-24643C standard, and maintains good mechanical properties after short-term aging.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

本发明提供了一种通讯线缆用辐照交联型耐油高抗撕低烟无卤高阻燃护套材料,包括以下重量份数的原料组分:乙烯‑醋酸乙烯共聚物15~17份;高密度聚乙烯11~13份;乙烯‑丙烯酸丁酯共聚物12~14份;相容剂5~7份;复合阻燃剂53~61份;润滑剂1.2~1.7份;防老抗氧剂2.0~2.6份;交联剂1.2~1.5份;所述复合阻燃剂由15~17份超细氢氧化铝、30~32份氢氧化镁、3~5份蒙脱土和5~7份三聚氰胺组成。能够通过ROSH、REACH等环保要求,有低烟高阻燃、燃烧无卤素释放的特点,符合MIL‑DTL‑24643C标准中各种油类在特定条件下的耐油性能。