ASA composite material and method for producing the same
By increasing the amount of brightener in ASA composite materials and introducing modified boron nitride and modified organomontmorillonite, the problem of increased gloss but decreased impact strength was solved, achieving a synergistic improvement in both gloss and impact strength.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- BINZHOU YONGHONG NEW MATERIAL TECH CO LTD
- Filing Date
- 2026-04-29
- Publication Date
- 2026-07-17
AI Technical Summary
While increasing the amount of brightener in existing ASA composite materials improves gloss, it reduces impact strength, making it difficult to maintain or improve impact strength while increasing gloss.
By increasing the amount of brightener and introducing modified boron nitride and modified organomontmorillonite, the interfacial bonding force is improved by the intercalation and exfoliation of modified organomontmorillonite and the silver ion doping, and the surface lubrication and smoothing effect of modified boron nitride, thus synergistically enhancing the impact strength of the composite material.
While improving gloss, it significantly enhances the impact strength of ASA composite materials, maintains the gloss of the material, and restores stress transfer efficiency.