A self-generating yarn, fabric, method of making a fabric and an article of wear

CN122588749APending Publication Date: 2026-08-18ANTA (CHINA) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610880823.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-06-17
Publication Date
2026-08-18

AI Technical Summary

Technical Problem

[0003]本申请实施例提供一种自发电纱线、织物、织物的制备方法及穿戴物,其旨在于解决相关技术中穿戴式传感器无法在穿戴者静止与运动两种状态下均持续输出可靠的电信号的技术问题

Benefits of technology

[0023]The beneficial effects of this application are as follows: When the wearer is stationary, the triboelectric signal output weakens or is interrupted, but the thermoelectric yarn maintains the signal output by utilizing the continuous temperature difference between the human body and the environment; when the wearer is in motion, the temperature difference tends to disappear and the thermoelectric signal weakens, but the movement of the limbs drives the triboelectric yarn to rub against the object being contacted, thus strengthening the triboelectric signal output. The triboelectric yarn and the thermoelectric yarn complement each other, enabling the self-generating yarn to output reliable electrical signals in both the static and dynamic states of the wearer. In addition, the triboelectric yarn is helical, so that when the self-generating yarn rotates or twists axially, the distribution density of the helical triboelectric yarn in each circumferential direction on the surface of the thermoelectric yarn does not change. Parallel triboelectric yarns only cover one side of the thermoelectric yarn. Once the yarn rotates, the orientation of that side changes. After being woven into the fabric, the triboelectric output capability of the yarn fluctuates depending on its orientation in the fabric. However, the spiral winding structure ensures that the rotation or twisting of the self-heating yarn does not affect the coverage of the yarn surface in all circumferential directions. This makes the triboelectric output capability of each segment of the self-heating yarn consistent after being woven into the fabric, thereby further improving the reliability of the triboelectric yarn's output signal.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122588749A_ABST
    Figure CN122588749A_ABST
Patent Text Reader

Abstract

The application discloses a self-power generation yarn, a fabric, a fabric preparation method and a wearable device. The self-power generation yarn comprises a thermoelectric yarn which extends along the length direction of the self-power generation yarn and is used for generating electric energy under the action of temperature difference; and at least one triboelectric yarn which spirally extends along the length direction of the self-power generation yarn and is combined with the triboelectric yarn and is used for generating electric energy when rubbing with other contact objects. The self-power generation yarn, the fabric, the fabric preparation method and the wearable device can solve the problem that a wearable sensor cannot continuously output reliable electric signals in both static and motion states of a wearer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of yarn, and more particularly to a self-generating yarn, fabric, method for preparing the fabric, and wearable device. Background Technology

[0002] Wearable sensors are made of practical wearable sensing fabrics. Users wear them like clothing, and the sensors can detect human body information whether the user is in motion or at rest. However, in related technologies, wearable sensing fabrics cannot guarantee reliable sensing signals in scenarios where the wearer is alternately stationary and in motion. Summary of the Invention

[0003] This application provides a self-generating yarn, fabric, a method for preparing the fabric, and a wearable device, which aims to solve the technical problem in the related art that wearable sensors cannot continuously output reliable electrical signals in both static and dynamic states of the wearer.

[0004] A first aspect of this application provides a self-generating yarn, comprising: a thermoelectric yarn extending along the length of the self-generating yarn for generating electrical energy under the action of a temperature difference;

[0005] At least one triboelectric yarn, extending in a spiral along the length of the self-generating yarn and combined with the triboelectric yarn, is used to generate electrical energy when rubbed against other contact objects.

[0006] In one possible implementation, the thermoelectric yarn extends in a straight line direction; At least one triboelectric yarn is wound around the outer periphery of the thermoelectric yarn to form a covering layer, which is used to simultaneously act on the temperature difference of the thermoelectric yarn.

[0007] In one possible implementation, the coverage of the thermoelectric yarn by the covering layer is M, where 70% ≤ M ≤ 95%; and / or, The ratio of the diameter of the triboelectric yarn to the pitch of the triboelectric yarn is 0.25-0.5.

[0008] In one possible implementation, at least one triboelectric yarn includes a positive triboelectric yarn and a negative triboelectric yarn, which are used to generate electrical energy through mutual friction. The positive and negative triboelectric yarns have opposite directions of rotation, forming a double helix structure around the triboelectric yarn; or, At least one triboelectric yarn, including a negative triboelectric yarn or a positive triboelectric yarn, is used to generate triboelectricity by friction with other contacting objects.

[0009] In one possible implementation, the triboelectric yarn extends in a spiral shape along the length of the self-generating yarn, and the triboelectric yarns intertwine with each other to form a spiral structure.

[0010] In one possible implementation, at least one triboelectric yarn includes positive and negative triboelectric yarns, which are used to generate electrical energy through mutual friction. The positive, negative, and triboelectric yarns form a triple helix structure, with the positive and negative triboelectric yarns having opposite directions of rotation, or the triboelectric yarns having the same direction of rotation as the positive and negative triboelectric yarns; or... At least one triboelectric yarn includes a positive triboelectric yarn or a negative triboelectric yarn, used to generate triboelectricity by friction with other contacting objects, the triboelectric yarn and the positive triboelectric yarn or the negative triboelectric yarn forming a double helix structure, the triboelectric yarn and the positive triboelectric yarn or the negative triboelectric yarn having the same or opposite helix directions.

[0011] In one possible implementation, the triboelectric yarn includes a conductive layer and a triboelectric skin layer, with the triboelectric skin layer wrapped around the conductive layer. The triboelectric skin layer is used to generate triboelectricity by rubbing against other contacting objects, and the conductive layer is used to transfer the charge corresponding to the electrical energy generated by friction along the length direction of the triboelectric yarn.

[0012] In one possible implementation, the triboelectric yarn includes a buffer layer, a thermoelectric layer, and an encapsulation layer arranged sequentially from the inside out. The thermoelectric layer is wrapped around the outside of the buffer layer, and the encapsulation layer is wrapped around the outside of the thermoelectric layer. The buffer layer is made of a phase change material to maintain the temperature difference between the two sides of the triboelectric yarn, and the thermoelectric layer is used to convert the temperature difference between the two sides of the triboelectric yarn into electrical energy.

[0013] A second aspect of this application provides a fabric in which a plurality of warp yarns include self-generating yarns as described in any of the first aspects, the plurality of warp yarns are arranged along a first direction, a plurality of weft yarns include structural yarns, the plurality of weft yarns are arranged along a second direction, the first direction and the second direction are set at an angle, and the plurality of warp yarns and the plurality of weft yarns are interwoven to form the fabric.

[0014] In one possible implementation, at least one weft yarn is a self-generating yarn.

[0015] In one possible implementation, the self-generating yarn includes a first self-generating yarn and a second self-generating yarn. The triboelectric yarn corresponding to the first self-generating yarn is a positive triboelectric yarn, and the triboelectric yarn corresponding to the second self-generating yarn is a negative triboelectric yarn. The positive and negative triboelectric yarns are used to generate triboelectricity through mutual friction. The first and second self-generating yarns are arranged alternately along a first direction.

[0016] In one possible implementation, the fabric is a 2 / 2 twill weave.

[0017] In one possible implementation, the plurality of warp yarns include structural yarns, and along a first direction, a self-generating yarn is provided every X structural yarns, where 3 ≤ X ≤ 10.

[0018] In one possible implementation, the fabric includes an energy harvesting zone, a motion detection zone, and a reinforcement zone, where the value of X for the energy harvesting zone is X1, the value of X for the motion detection zone is X2, and the value of X for the reinforcement zone is X3, and X1≤X2≤X3.

[0019] A third aspect of this application provides a method for preparing a fabric, in which self-generating yarn is used as warp yarn and structural yarn is used as weft yarn, and the weft yarn and warp yarn are woven together on a loom to form a fabric.

[0020] In one possible implementation, the warp tension is F1, 0.12 cN / dtex ≤ F1 ≤ 0.40 cN / dtex; and / or, The weft tension is F2, 0.21cN / dtex≤F2≤0.38cN / dtex.

[0021] In one possible implementation, the loom speed is N, 300 r / min ≤ N ≤ 600 r / min; and / or, The loom's shedding time is 45ms-115ms; and / or, The loom is either an air-jet loom or a rapier loom.

[0022] A fourth aspect of this application provides a wearable device, including a fabric as described in any of the second aspects, a data acquisition module, a control module, and a communication module, wherein the fabric, data acquisition module, control module, and communication module are electrically connected in sequence, the data acquisition module is used to acquire electrical energy output by the fabric, the control module is used to process the electrical energy acquired by the data acquisition module and generate a detection signal, and the communication module is used to output the detection signal.

[0023] The beneficial effects of this application are as follows: When the wearer is stationary, the triboelectric signal output weakens or is interrupted, but the thermoelectric yarn maintains the signal output by utilizing the continuous temperature difference between the human body and the environment; when the wearer is in motion, the temperature difference tends to disappear and the thermoelectric signal weakens, but the movement of the limbs drives the triboelectric yarn to rub against the object being contacted, thus strengthening the triboelectric signal output. The triboelectric yarn and the thermoelectric yarn complement each other, enabling the self-generating yarn to output reliable electrical signals in both the static and dynamic states of the wearer. In addition, the triboelectric yarn is helical, so that when the self-generating yarn rotates or twists axially, the distribution density of the helical triboelectric yarn in each circumferential direction on the surface of the thermoelectric yarn does not change. Parallel triboelectric yarns only cover one side of the thermoelectric yarn. Once the yarn rotates, the orientation of that side changes. After being woven into the fabric, the triboelectric output capability of the yarn fluctuates depending on its orientation in the fabric. However, the spiral winding structure ensures that the rotation or twisting of the self-heating yarn does not affect the coverage of the yarn surface in all circumferential directions. This makes the triboelectric output capability of each segment of the self-heating yarn consistent after being woven into the fabric, thereby further improving the reliability of the triboelectric yarn's output signal. Attached Figure Description

[0024] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.

[0025] Figure 1 This is one of the structural schematic diagrams of the self-generating yarn provided in the embodiments of the present invention; Figure 2 This is the second schematic diagram of the structure of the self-generating yarn provided in the embodiment of the present invention; Figure 3 This is one of the structural schematic diagrams of the triboelectric yarn provided in the embodiments of the present invention; Figure 4 This is a schematic diagram of the structure of the thermoelectric yarn provided in an embodiment of the present invention; Figure 5 This is the second schematic diagram of the triboelectric yarn structure provided in the embodiment of the present invention; Figure 6 This is a schematic diagram of the structure of the fabric provided in an embodiment of the present invention.

[0026] Explanation of icon numbers: 20. Thermoelectric yarn; 21. Buffer layer; 22. Thermoelectric layer; 23. Encapsulation layer; 30. Triboelectric yarn; 31. Positive triboelectric yarn; 32. Negative triboelectric yarn; 33. Conductive layer; 34. Triboelectric skin layer; 40. Fabric; 41. Warp yarn; 42. Weft yarn; 50. First direction; 60. Second direction. Detailed Implementation

[0027] Before introducing the embodiments of this application, the technical terms and background technology involved in this application will be introduced first.

[0028] In the field of wearable electronic devices, to achieve continuous monitoring of parameters such as human physiological signals and movement posture, the industry often weaves self-generating yarns into clothing fabrics. These yarns generate electrical signals to sense the wearer's movement status or body temperature changes, and can also provide power for miniature sensors. Currently, there are two main technical routes for self-generating yarns: one is triboelectric yarn. The power generation principle of triboelectric yarn is based on the coupling of triboelectric effect and electrostatic induction: when two materials with different electronegativity come into contact, charge transfer occurs at the interface, and the two materials acquire equal amounts of opposite charges; when the two materials separate under external force, the interface charge forms a potential difference on the material surface, driving the flow of electrons in the external circuit to balance the potential, thereby outputting an electrical signal. Structurally, triboelectric yarn is usually composed of an inner conductive yarn (as an electrode) and an outer insulating polymer yarn (as a friction layer). When the wearer walks, swings their arms, or flexes and extends their limbs, causing repeated friction and separation between the triboelectric yarn and other parts of the clothing or the object it contacts, the triboelectric yarn can continuously output high-amplitude AC pulse signals. Secondly, there are thermoelectric yarns. The power generation principle of thermoelectric yarns is based on the Seebeck effect: when a temperature gradient exists in a closed circuit composed of two different conductors or semiconductors, charge carriers (electrons or holes) in the circuit migrate directionally from the hot end to the cold end under the drive of the thermal field, generating a thermoelectric potential between the hot and cold ends and driving the current in the external circuit. Structurally, thermoelectric yarns are typically made of flexible fibers or yarns made of alternating series connection of P-type and N-type thermoelectric materials and covered with an insulating layer. When the wearer is in a static state (such as sitting or sleeping), thermoelectric yarns can continuously generate a direct current signal by relying on the stable temperature difference between the body surface temperature and the external environment temperature.

[0029] However, the signal generation of triboelectric yarns relies on repeated frictional separation at the material interface. When the wearer is stationary (such as sitting or sleeping), the frictional separation frequency drops sharply, causing the electrical signal output to attenuate significantly or even stop, making it impossible to sense the wearer's state or provide electrical energy in such scenarios. The signal generation of thermoelectric yarns relies on a continuous temperature gradient. When the wearer is in motion, convective heat transfer between the body surface and the environment accelerates, the temperature difference tends to shrink or even disappear, and the airflow disturbances generated by movement also disrupt the stability of the temperature gradient, leading to a significant weakening or even complete cessation of thermoelectric signal output. In summary, wearable sensors have the problem of not being able to continuously output electrical signals in both stationary and moving states.

[0030] To address the aforementioned issues, this application provides a self-generating yarn, a fabric, a method for preparing the fabric, and a wearable device. The self-generating yarn includes both thermoelectric and triboelectric yarns. When the wearer is stationary, the triboelectric signal output weakens or is interrupted, but the thermoelectric yarn maintains signal output using the continuous temperature difference between the human body and the environment. When the wearer is in motion, the temperature difference tends to disappear, and the thermoelectric signal weakens, but the movement of the limbs drives the triboelectric yarn to rub against the contacted object, increasing the triboelectric signal output. The triboelectric and thermoelectric yarns complement each other, enabling the self-generating yarn to output reliable electrical signals in both stationary and moving states. Furthermore, the triboelectric yarn is helical, ensuring that the distribution density of the helical triboelectric yarn in each circumferential direction on the surface of the thermoelectric yarn remains unchanged when the self-generating yarn rotates or twists axially. Parallel triboelectric yarns only cover one side of the thermoelectric yarn. Once the yarn rotates, the orientation of that side changes. After being woven into the fabric, the triboelectric output capability of the yarn fluctuates depending on its orientation in the fabric. However, the spiral winding structure ensures that the rotation or twisting of the self-heating yarn does not affect the coverage of the yarn surface in all circumferential directions. This makes the triboelectric output capability of each segment of the self-heating yarn consistent after being woven into the fabric, thereby further improving the reliability of the triboelectric yarn's output signal.

[0031] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those of ordinary skill in the art without creative effort are within the scope of protection of the present invention.

[0032] Please see Figures 1 to 5 As shown, Figure 1 This is one of the structural schematic diagrams of the self-generating yarn provided in the embodiments of the present invention; Figure 2 This is the second schematic diagram of the structure of the self-generating yarn provided in the embodiment of the present invention; Figure 3This is one of the structural schematic diagrams of the triboelectric yarn provided in the embodiments of the present invention; Figure 4 This is a schematic diagram of the structure of the thermoelectric yarn provided in an embodiment of the present invention; Figure 5 This is the second schematic diagram of the triboelectric yarn structure provided in the embodiment of the present invention.

[0033] The present application provides a self-generating yarn, including a thermoelectric yarn 20 extending along the length of the self-generating yarn, for generating electrical energy under the action of temperature difference; At least one triboelectric yarn 30 extends in a spiral shape along the length of the self-generating yarn and is combined with the triboelectric yarn 30 for generating electrical energy when rubbed against other contact objects.

[0034] Thermoelectric yarn 20 refers to yarn that can convert thermal energy into electrical energy when there is a temperature difference in its radial or axial direction, by utilizing the Seebeck effect.

[0035] Triboelectric yarn 30 refers to a yarn that can utilize the triboelectric effect and electrostatic induction coupling to output an electrical signal when it rubs against other contact objects (such as clothing fabric, skin, external objects, or other triboelectric yarns 30).

[0036] When the wearer is in motion, such as walking, running, or swinging their arms, the limb movements cause repeated friction between the outer surface of the triboelectric yarn 30 and adjacent clothing fabric, skin, or other contact objects. During this friction process, the triboelectric yarn 30 and the contact object rub and separate. Upon contact, charge transfer occurs at the interface of the two materials, and they become charged. Upon separation, the interface charges establish a potential difference on the material surface, driving the flow of electrons in the external circuit to balance the potential, forming a current or voltage pulse signal output. The more intense the movement and the higher the frequency, the more times frictional separation occurs, and the greater the pulse density and average power of the triboelectric signal output. When the wearer is in a static state such as sitting or sleeping, the range of limb movement is small, and there is almost no frictional separation between the triboelectric yarn 30 and the external contact object, resulting in a weak or near-zero triboelectric signal output. However, due to the continuous temperature difference between the human body surface temperature and the external environment temperature, when the self-generating yarn is sandwiched between the inner layer of clothing and the skin, the temperature on the side closer to the skin is higher than the temperature on the side closer to the environment, forming a temperature gradient along the radial direction of the yarn. The thermoelectric yarn 20 utilizes the temperature gradient to drive the internal charge carriers to migrate directionally from the hot end to the cold end, generating Seebeck voltage and outputting DC or slowly changing electrical signals, so that the self-generating yarn can output reliable electrical signals in both the static and dynamic states of the wearer.

[0037] The triboelectric yarn 30 is helical, ensuring that the distribution density of the helical triboelectric yarn 30 on the surface of the thermoelectric yarn 20 remains unchanged in all circumferential directions when the self-generating yarn rotates or twists axially. Parallel triboelectric yarns 30 only cover one side of the thermoelectric yarn 20; once the yarn rotates, the orientation of that side changes, and the triboelectric output capability of the yarn fluctuates depending on its orientation within the fabric. However, the helical winding structure ensures that the rotation or twisting of the self-generating yarn does not affect the coverage of the triboelectric yarn 30 on the yarn surface in all circumferential directions, resulting in a consistent triboelectric output capability across all segments of the self-generating yarn after it is woven into the fabric.

[0038] In some embodiments, see Figure 1 The thermoelectric yarn 20 extends in a straight line; at least one triboelectric yarn 30 is wound around the outer periphery of the thermoelectric yarn 20 to form a covering layer, which is used to simultaneously act on the temperature difference of the thermoelectric yarn 20. That is, the triboelectric yarn 30 is spirally wound around the outer surface of the thermoelectric yarn 20 with the center line of the thermoelectric yarn 20 as the axis.

[0039] It should be noted that, Figure 1 This is merely a schematic diagram of the winding method of the triboelectric yarn 30 and does not represent parameters such as the diameter and pitch of the triboelectric yarn 30.

[0040] In practical applications, the covering layer not only serves to generate electrical signals through friction, but also plays a crucial role during the transition from a stationary to a moving state or vice versa. During this transition, environmental convective heat transfer conditions change abruptly (higher airflow velocity and faster heat dissipation during movement; lower airflow velocity and slower heat dissipation during stillness). If the thermoelectric yarn 20 is directly exposed to the environment, this abrupt change in external heat dissipation conditions will immediately manifest as a rapid change in the cold end temperature of the yarn, leading to spikes or drops in the thermoelectric signal. The covering layer acts as a buffer; when external heat dissipation conditions change abruptly, the temperature response of the covering layer exhibits a certain time lag, stabilizing the temperature difference between the hot and cold sides of the thermoelectric yarn 20. This reduces the amplitude of temperature fluctuations in the thermoelectric yarn 20 as the wearer's activity level changes, resulting in a more stable thermoelectric signal output. Furthermore, during movement, the covering layer can isolate most of the external airflow, reducing the impact of airflow heat dissipation on the thermoelectric yarn 20 and further improving the stability of the thermoelectric signal output.

[0041] In some embodiments, the coverage of the covering layer over the thermoelectric yarn 20 is M, where 70% ≤ M ≤ 95%. For example, M can be 71%, 74%, 79%, 84%, 89%, or 94%. And / or, the ratio of the diameter of the triboelectric yarn 30 to the pitch of the triboelectric yarn 30 is 0.25-0.5. For example, it can be 0.26, 0.29, 0.34, 0.39, 0.41, or 0.46.

[0042] Coverage rate refers to the percentage ratio between the projected area of ​​the triboelectric yarn 30 on the outer surface of the thermoelectric yarn 20 and the total area of ​​the outer surface of the thermoelectric yarn 20 when the triboelectric yarn 30 is spirally wound around the outer periphery of the thermoelectric yarn 20.

[0043] When the coverage is between 70% and 95%, the triboelectric yarn 30 has sufficient outer surface area to rub against the object being contacted, and also has enough space to deform to achieve contact and separation during friction. When the coverage is less than 70%, more than 30% of the outer periphery of the thermoelectric yarn 20 is not covered by the covering layer. External low-temperature airflow can directly contact the surface of the thermoelectric yarn 20 through the gap between adjacent spiral coils, resulting in uneven temperature distribution. The areas covered by the covering layer have higher temperatures, while the areas corresponding to the exposed gaps have lower temperatures, leading to unstable thermoelectric output. When the coverage approaches 100%, there are almost no gaps between the spiral coils of the triboelectric yarn 30, with adjacent spiral coils tightly abutting or overlapping radially. When the yarn bends, the tight arrangement without gaps restricts the space for deformation of the triboelectric yarn 30 under stretching or compression, preventing frictional separation during friction and thus affecting the electrical signal output capability of the triboelectric yarn 30.

[0044] Pitch refers to the axial distance between two adjacent turns of the spiral along the axis of the thermoelectric yarn 20 when the triboelectric yarn 30 is wound around the outer surface of the thermoelectric yarn 20 along the spiral path.

[0045] The wire diameter refers to the cross-sectional diameter of the triboelectric yarn 30 itself.

[0046] The triboelectric yarn 30 has an axial gap of more than half the pitch between adjacent spiral coils, which provides sufficient space for the axial movement of each spiral coil when the self-generating yarn bends. This avoids the problem of squeezing and wear between adjacent spiral coils due to bending when the spiral coils are tightly wound side by side, and extends the service life of the triboelectric yarn 30.

[0047] In some embodiments, reference is made to Figure 2 and Figure 3 At least one triboelectric yarn 30 includes a positive triboelectric yarn 31 and a negative triboelectric yarn 32, which are used to generate electrical energy through mutual friction. The positive triboelectric yarn 31 and the negative triboelectric yarn 32 have opposite directions of rotation, forming a double helix structure around the triboelectric yarn 30; or, At least one triboelectric yarn 30 includes a negative triboelectric yarn 32 or a positive triboelectric yarn 31, used to generate triboelectricity by friction with other contacting objects.

[0048] In practical applications, the spiral coils of the positive triboelectric yarn 31 and the negative triboelectric yarn 32 form multiple intersection nodes on the surface of the thermoelectric yarn 20. When the self-generating yarn is bent, stretched, vibrated, or stretched and compressed under the wearer's movement, a small relative displacement occurs between the positive triboelectric yarn 31 and the negative triboelectric yarn 32 in the double-helix structure. This causes friction and separation between the positive and negative triboelectric yarns at the intersection nodes, thereby generating electricity. This eliminates the need for friction between the self-generating yarn and other external contact objects; instead, electricity is generated solely through the mutual friction between the positive and negative triboelectric yarns within the yarn itself. Furthermore, the large number of intersection nodes increases the contact area and frequency between the positive and negative triboelectric yarns, resulting in higher electrical output power and more uniform signal distribution. If the positive triboelectric yarn 31 and the negative triboelectric yarn 32 are arranged side by side, then during the stretching and compression of the self-generating yarn, the positive triboelectric yarn 31 and the negative triboelectric yarn 32 will be stretched or compressed synchronously, and there will be no frictional separation process between the two, so that the charge cannot migrate and thus cannot generate electrical energy.

[0049] If the self-generating yarn contains only one of the positive triboelectric yarn 31 or the negative triboelectric yarn 32, then the self-generating yarn needs to generate electricity through friction with other external contact objects. The outer diameter and cost of the self-generating yarn are both relatively low.

[0050] In some embodiments, reference is made to Figure 2 The thermoelectric yarn 20 extends in a spiral shape along the length of the self-generating yarn, and the thermoelectric yarn 20 and the triboelectric yarn 30 are intertwined to form a spiral structure.

[0051] In practical applications, the thermoelectric yarn 20 and the triboelectric yarn 30 form a double helix structure, which are symmetrically arranged. The tensile and compressive stresses are borne by the thermoelectric yarn 20 and the triboelectric yarn 30 together, resulting in high bending fatigue durability.

[0052] In this embodiment, at least one triboelectric yarn 30 includes a positive triboelectric yarn 31 or a negative triboelectric yarn 32, used to generate triboelectricity by friction with other contacting objects. The triboelectric yarn 30 and the positive triboelectric yarn 31 or the negative triboelectric yarn 32 form a double helix structure, and the directions of rotation of the triboelectric yarn 30 and the positive triboelectric yarn 31 or the negative triboelectric yarn 32 are the same or opposite.

[0053] In some embodiments, at least one triboelectric yarn 30 includes a positive triboelectric yarn 31 and a negative triboelectric yarn 32, which are used to generate electrical energy through mutual friction. The positive triboelectric yarn 31, the negative triboelectric yarn 32, and the triboelectric yarn 30 form a triple helix structure. The positive triboelectric yarn 31 and the negative triboelectric yarn 32 have opposite directions of rotation, and the triboelectric yarn 30 and the positive triboelectric yarn 31 have the same direction of rotation, or the triboelectric yarn 30 and the negative triboelectric yarn 32 have the same direction of rotation.

[0054] In practical applications, the positive triboelectric yarn 31 and the negative triboelectric yarn 32 have opposite directions of rotation. Their spiral paths form a dense network of intersecting nodes in the twisted body. When the yarn is deformed by external force, each intersecting node undergoes micro-friction separation. There are many points of triboelectric charge generation between the positive and negative triboelectric materials, and the distribution density is high. The internal self-friction power generation efficiency of the triple helix structure is high.

[0055] In some embodiments, reference is made to Figure 5 The triboelectric yarn 30 includes a conductive layer 33 and a triboelectric skin layer 34. The triboelectric skin layer 34 is wrapped around the conductive layer 33 and is used to generate triboelectricity by rubbing against other contacting objects. The conductive layer 33 is used to transfer the charge corresponding to the electrical energy generated by friction along the length direction of the triboelectric yarn 30.

[0056] The conductive layer 33 refers to the conductive core inside the triboelectric yarn 30 that extends along the length of the triboelectric yarn 30. Its material has high electrical conductivity and is used to quickly conduct the induced charge generated on the surface of the triboelectric layer 34 along the length of the triboelectric yarn 30 to the end during the triboelectric electrification process.

[0057] The friction layer 34 refers to the surface functional layer wrapped around the conductive layer 33, used for friction with external contact objects. The material of the friction layer 34 is selected from polymer materials that have a large positional difference from the target external contact object in the triboelectric sequence. Its function is to cause interfacial charge transfer during the triboelectric separation process, so that net charge (positive or negative charge) accumulates on the surface of the friction layer 34.

[0058] In related technologies, triboelectric yarns require an air gap between the positive and negative friction materials. This air gap's elastic support allows the two friction materials to separate under pressure, establishing a potential difference. This air gap results in a thick, rigid fabric with poor breathability, and after long-term use, the elastic structure fatigues, and the bonding interfaces between layers are prone to delamination. The triboelectric yarn 30 of this application uses a conductive layer 33 as the core and a friction layer 34 as the skin, which are directly and tightly bonded together, with only two layers in the cross-section. The object of triboelectric generation is an external contact object (or another triboelectric yarn 30 with opposite polarity). Separation is achieved by the yarn's own tiny diameter and slight deformation, eliminating the need for an air gap between the positive and negative friction materials. Eliminating the air gap reduces fabric thickness, and its flexibility and breathability are close to those of ordinary fabrics.

[0059] In this embodiment, 280D / 3-ply silver-plated nylon yarn is selected as the conductive layer 33. The nylon matrix is ​​nylon 6 (PA6) or nylon 66 (PA66) filament, and the bus density after three-ply bonding is approximately 840D. The silver plating layer is deposited on the fiber surface using a chemical silver plating process. After chemical plating, the yarn is annealed at 120°C for 30 minutes to eliminate internal stress in the plating layer. The resistance of the final conductive layer 33 is controlled below 0.5Ω / cm. The triboelectric yarn 30 is prepared as follows: PVDF-TrFE (molar ratio 70:30 or 80:20) powder is dissolved in a mixed solvent of DMF and methyl ethyl ketone (volume ratio 6:4) at a concentration of 15% to 25% (w / v), and stirred at room temperature until homogeneous. Perovskite nanocrystals (average particle size 50 nm to 200 nm) were ultrasonically dispersed and then added to a PVDF-TrFE solution at an amount of 1% to 5% (w / w) of the PVDF-TrFE mass, and stirred until uniformly dispersed. Coating was performed using a coaxial electrospinning process: the conductive layer 33 was passed through the central channel of the coaxial nozzle at a speed of 3 m / min, and the spinning solution was injected into the outer channel at a propulsion rate of 1.0 mL / h. The spinning voltage was 20 kV, and the receiving distance was 18 cm. Under a high-voltage electric field, the spinning solution formed a nanofiber jet that uniformly deposited and coated the surface of the conductive layer 33. The skin thickness was controlled within the range of 50 μm to 500 μm by adjusting the yarn feed speed and propulsion rate. Post-treatment: After coating, the surface was dried in a vacuum oven at 80°C for 2 hours to remove the solvent, followed by oxygen plasma surface treatment (power 100 W, treatment time 60 s) to enhance the density of polar groups on the surface of the friction skin 34 and the interfacial bonding force between the friction skin 34 and the conductive layer 33.

[0060] In some embodiments, reference is made to Figure 4The triboelectric yarn 30 includes a buffer layer 21, a thermoelectric layer 22, and an encapsulation layer 23 arranged sequentially from the inside to the outside. The thermoelectric layer 22 is wrapped around the buffer layer 21, and the encapsulation layer 23 is wrapped around the thermoelectric layer 22. The buffer layer 21 is made of a phase change material to maintain the temperature difference between the two sides of the triboelectric yarn 30. The thermoelectric layer 22 is used to convert the temperature difference between the two sides of the triboelectric yarn 30 into electrical energy.

[0061] In practical applications, the buffer layer 21 uses a phase change material, which utilizes the latent heat absorption / release effect of the phase change process to buffer the impact of external temperature changes on the temperature difference on both sides of the thermoelectric layer 22, reducing the baseline drift amplitude of the thermoelectric signal when the ambient temperature changes abruptly and human activity switches. The phase change material is shaped and encapsulated in the core layer with TPU as the matrix, eliminating the risk of liquid leakage contaminating the thermoelectric layer 22.

[0062] The encapsulation layer 23 physically isolates the thermoelectric layer 22 from the external environment, preventing moisture and chemicals from corroding the thermoelectric material. At the same time, the elastic constraint keeps the layers tightly bonded, eliminates interfacial air gaps, reduces interfacial thermal resistance, improves the effective temperature difference utilization rate from the hot side to the cold side, and improves washability.

[0063] In this embodiment, the phase change layer is made of n-octadecane (phase change temperature approximately 28°C to 30°C, latent heat of phase change ≥180 J / g) or n-eicosane (phase change temperature approximately 36°C to 38°C). The phase change material is blended with TPU granules at a mass ratio of 40:60 to 60:40, and then melt-blended and granulated using a twin-screw extruder to produce a shaped phase change composite material masterbatch in which the phase change material is uniformly dispersed in the TPU matrix. A higher mass proportion of phase change material results in a greater latent heat of phase change and a stronger thermal buffering effect for the buffer layer 21; however, excessive amounts can reduce the mechanical strength and spinnability of the composite material. The latent heat of phase change of the composite material is ≥110 J / g. The thermoelectric layer 22 is made of a composite dispersion of single-walled carbon nanotubes (SWCNTs) and PEDOT:PSS. SWCNTs are prepared at a concentration of 0.5% to 2% (w / v), and PEDOT:PSS at a concentration of 1% to 3% (w / v). The dispersion medium is water or a water / dimethyl sulfoxide (DMSO) mixture. The mixture is ultrasonically dispersed with the addition of a small amount of surfactant (such as Triton X-100) to improve dispersion uniformity. SWCNTs provide an inorganic thermoelectric pathway with high conductivity and intrinsic Seebeck coefficient, while PEDOT:PSS provides flexibility and film-forming properties. The combined Seebeck coefficient is ≥40 μV / K. The encapsulation layer 23 uses a TPU solution (concentration 10% to 20% w / v, solvent is DMF or a DMF / butanone mixture). Polyether-type TPU is selected for better hydrolysis resistance and flexibility. A three-layer coaxial wet spinning process is used: a three-layer coaxial spinning nozzle is employed, with three annular channels corresponding to the buffer layer 21, thermoelectric layer 22, and encapsulation layer 23 from the inside out. The feed rate for the spinning solution (TPU / phase change material blend dissolved in solvent) in buffer layer 21 is 0.5 mL / h, the feed rate for the spinning solution (SWCNT / PEDOT:PSS dispersion) in thermoelectric layer 22 is 1.0 mL / h, and the feed rate for the spinning solution (TPU solution) in encapsulation layer 23 is 1.5 mL / h. The spinning voltage is 25 kV, and the receiving distance is 20 cm. After the nascent yarn is extruded from the nozzle, it enters a coagulation bath (water / ethanol volume ratio 1:1, temperature 15°C) and solidifies for about 30 s, allowing the solvents of each layer to exchange and precipitate in the coagulation bath. The solidified yarn is then stretched (stretch ratio 1.1 to 1.3, so that the SWCNTs in thermoelectric layer 22 are oriented axially to improve axial conductivity), and then dried and shaped with hot air at 50°C to 60°C before being wound and collected.

[0064] The embodiments of this application also provide a fabric 40, see reference. Figure 6Fabric 40 includes a plurality of warp yarns 41 and a plurality of weft yarns 42. The plurality of warp yarns 41 include self-generating yarns and are arranged along a first direction 50. The plurality of weft yarns 42 include structural yarns and are arranged along a second direction 60. The first direction 50 and the second direction 60 are set at an angle. The plurality of warp yarns 41 and the plurality of weft yarns 42 are interwoven to form fabric 40.

[0065] In practical applications, the warp yarns 41 undergo a warping process before weaving. During warping, the self-generating yarns are arranged parallel to each other on the warp beam with constant tension. The spacing and tension between the yarns are uniform, which is beneficial to the consistency of signal output of each self-generating yarn in the fabric 40. Secondly, the warp yarns 41 extend continuously along the length of the fabric 40 during weaving. The working length of the fabric 40 usually corresponds to the direction of the warp yarns 41. A single self-generating yarn can provide a continuous signal acquisition channel throughout the entire fabric 40, resulting in good signal continuity. Furthermore, during weft insertion, the weft yarn 42 needs to pass through the opening of the warp yarn 41 at a high speed. The surface of the self-generating yarn is subjected to greater air pressure and friction, and the sensitive friction layer 34 is easily abraded during high-speed weft insertion. In contrast, the warp yarns 41 only bear the periodic stretching of the opening movement and the friction of the reed beating during weaving, and the stress is relatively controllable. If the surface strength of the self-generating yarn is sufficient to withstand the weft insertion process, the self-generating yarn can also be partially placed in the weft yarn 42.

[0066] In some embodiments, at least one weft yarn 42 is a self-generating yarn. In practical applications, the self-generating yarn is configured in the weft yarn 42 so that the fabric 40 has sensing and power generation capabilities in both the warp and weft directions.

[0067] In some embodiments, the self-generating yarn includes a first self-generating yarn and a second self-generating yarn. The triboelectric yarn 30 corresponding to the first self-generating yarn is a positive triboelectric yarn 31, and the triboelectric yarn 30 corresponding to the second self-generating yarn is a negative triboelectric yarn 32. The positive triboelectric yarn 31 and the negative triboelectric yarn 32 are used to generate electrical energy through mutual friction. The first self-generating yarn and the second self-generating yarn are arranged alternately along a first direction 50.

[0068] In practical applications, positive and negative triboelectric self-generating yarns are alternately arranged in the fabric 40 along the first direction 50. When the fabric 40 is bent or wrinkled, adjacent positive and negative polarity yarns can directly rub against each other to generate triboelectricity. Triboelectric power generation no longer depends on external pairing materials, and the fabric 40 itself constitutes a self-contained triboelectric power generation system.

[0069] In some embodiments, the plurality of warp yarns 41 include structural yarns, and a self-generating yarn is provided every X structural yarns along a first direction 50, where 3 ≤ X ≤ 10.

[0070] Structural yarns refer to conventional textile yarns in fabric 40 that do not perform power generation or sensing functions. Their role is to provide fabric 40 with basic physical properties such as structural strength, dimensional stability, abrasion resistance, soft hand feel, and appearance. Structural yarns can be one or more of the following: cotton yarn, polyester yarn, nylon yarn, acrylic yarn, blended yarn, and various functional conventional yarns (such as elastic core-spun yarn, moisture-wicking yarn, etc.). Their material and yarn count are flexibly selected according to the target use and hand feel requirements of fabric 40.

[0071] In practical applications, the value of X is limited to the range of 3 to 10, and the proportion of self-generating yarn in the warp yarn 41 is controlled between about 9% and 25%. Within this range, the fabric 40 has both effective signal output density and acceptable wearing comfort, avoiding excessive density which would increase the stiffness of the fabric, and also avoiding excessive sparseness which would increase the difficulty of signal acquisition and create local perception blind spots.

[0072] In some embodiments, the fabric 40 includes an energy harvesting area, a motion detection area, and a reinforcement area, where the value of X corresponding to the energy harvesting area is X1, the value of X corresponding to the motion detection area is X2, and the value of X corresponding to the reinforcement area is X3, and X1≤X2≤X3.

[0073] The energy harvesting zone refers to the area in fabric 40 with the highest density of self-generating yarns (X value is the smallest). The main function of this zone is to maximize the harvesting of human body thermal energy and kinetic mechanical energy and convert them into electrical energy to power the subsequent circuit modules. The energy harvesting zone has relatively low requirements for signal time response accuracy, but the highest requirements for continuous and stable power output.

[0074] The motion detection zone refers to the area in fabric 40 configured with a medium density of self-generating yarns. The main function of this zone is to sense human motion signals (such as joint bending, muscle stretching, contact friction, etc.). It requires high temporal resolution of the signals and moderate total power output.

[0075] The reinforced zone refers to the area within the fabric 40 where the density of self-generating yarns is lowest (X value is the highest) or completely absent. The main function of this zone is to provide structural strength, abrasion resistance, and dimensional stability to the fabric, supporting areas of concentrated stress in clothing (such as seams, around buttonholes, and shoulder load-bearing areas). The reinforced zone has a low proportion of self-generating yarns, resulting in a fabric feel closest to conventional textiles, making it suitable for areas in direct contact with the skin.

[0076] In practical applications, the fabric 40 is divided into three functionally differentiated areas: an energy harvesting area, a motion detection area, and a reinforcement area. Each area is configured with a different X value to ensure the density of self-generating yarn as needed. The energy harvesting area has the highest density to ensure sufficient system power supply, the motion detection area has a moderate density to ensure the spatial resolution accuracy of motion signals, and the reinforcement area has the lowest density to ensure structural strength.

[0077] In some embodiments, fabric 40 is a 2 / 2 twill weave.

[0078] In practical applications, the interlacing point spacing of the twill 2 / 2 weave is larger than that of the plain weave, resulting in a gentler bending curvature of the self-generating yarn in the fabric 40. This reduces the tensile strain of the friction skin 34 at the interlacing bends, delaying the generation and peeling of microcracks, and extending the bending fatigue life of the triboelectric yarn 30 and its effective service life in the fabric 40. Furthermore, the longer floats of the warp yarns 41 in the twill 2 / 2 weave provide a longer continuous exposed section of the self-generating yarn on the surface of the fabric 40, increasing the effective area where the friction skin 34 can directly participate in frictional separation, and improving the overall triboelectric signal collection efficiency of the fabric 40.

[0079] The embodiments of this application also provide a method for preparing fabric 40, wherein self-generating yarn is used as warp yarn 41 and structural yarn is used as weft yarn 42, and the weft yarn 42 and warp yarn 41 are woven together by a loom to form fabric 40.

[0080] A loom is a mechanical device used to weave warp yarns 41 and weft yarns 42 together according to a preset weave pattern.

[0081] Woven weaving refers to a weaving method characterized by the perpendicular interlacing of two sets of yarns, warp yarns 41 and weft yarns 42, which is different from knitting, which is characterized by loop interlacing. "Woven fabric 40" includes the cyclical actions of the warp yarns 41 separating vertically on the loom to form a shed according to the weave pattern, the weft yarns 42 passing through the shed through the weft insertion mechanism, and the reed tightening the introduced weft yarns 42 to the weft end.

[0082] In some embodiments, the warp tension 41 is F1, 0.12cN / dtex≤F1≤0.40cN / dtex; and / or, the weft tension 42 is F2, 0.21cN / dtex≤F2≤0.38cN / dtex.

[0083] On-machine tension refers to the axial static tensile force applied to the warp yarn 41 by the loom's warp feed mechanism and tension adjustment device after the warp yarn 41 is unwound from the warp beam and before entering the heald frame and reed. On-machine tension is expressed as force per unit linear density (cN / dtex). This unit eliminates the influence of yarn thickness differences on the tension value, facilitating lateral comparisons between different yarn counts.

[0084] Weft insertion tension refers to the axial tensile force applied to the weft yarn 42 by the weft insertion device as it passes through the shed of the warp yarn 41 after being unwound from the weft yarn 42 bobbin. It is also expressed as a force value per unit linear density (cN / dtex). The weft insertion tension reaches its peak at the moment the weft yarn 42 passes through the shed, and then decreases as the weft yarn 42 is tightened by the reed.

[0085] If F1 is below 0.12 cN / dtex, the warp yarn 41 is not sufficiently tensioned. During shed opening, the upper and lower warp yarns 41 cannot completely separate due to their own weight and electrostatic adsorption between the yarns—resulting in blurred shed boundaries and inconsistent shed heights. The surface of the self-generating yarn is easily scratched by adjacent warp yarns 41 or the reed edge in the blurred shed. Especially when some warp yarns 41 are structural yarns and the tension of adjacent self-generating yarns is low, the self-generating yarn may sag due to its relatively looseness during shed opening and be deviated from its intended path by the high-speed passing weft yarn 42, leading to weft insertion failure or yarn surface damage. Because the triboelectric yarn 30 and thermoelectric yarn 20 have different mechanical properties, when F1 exceeds 0.40 cN / dtex, the tensile strain of the warp yarn 41 may cause microcracks on the yarn surface, leading to increased yarn resistance and directly reducing the collection efficiency of triboelectric charges along the yarn length. Simultaneously, the external functional coating undergoes creep under continuous high tension, resulting in thinning and a corresponding decrease in dielectric properties and Seebeck coefficient. In addition, excessively high warp tension 41 causes significant warp shrinkage of fabric 40 after it comes off the machine, and the designed width and warp and weft density of fabric 40 deviate from the preset values.

[0086] During weft insertion, weft yarn 42 requires sufficient tension to maintain an approximately straight state as it flies over the shed. If the tension is too low, weft yarn 42 will swing excessively in the airflow (air jet weft insertion) or sag under gravity, failing to accurately reach the opposite shed and maintain the predetermined length. Insufficient tension when weft yarn 42 reaches the weft insertion point will also cause it to not adhere tightly to the previous weft yarn 42 during reed bedding, resulting in a low weft density and noticeable sparse-density patterns in the fabric 40. The tension experienced by weft yarn 42 during weft insertion is instantaneous impact-type—rising from zero to a peak value within milliseconds to tens of milliseconds. This impact stress is more likely to generate peeling stress at the material interface within the yarn. Therefore, the safe upper limit of weft yarn 42 tension must be higher than that of warp yarn 41.

[0087] In some embodiments, the loom speed is N, 300 r / min ≤ N ≤ 600 r / min; and / or, The loom's shedding time is 45ms-115ms; and / or, The loom is either an air-jet loom or a rapier loom.

[0088] Loom speed refers to the number of revolutions per minute of the loom spindle, measured in r / min (revolutions per minute).

[0089] Shedding time refers to the complete time interval within a loom's working cycle from the initial up-and-down movement of the heald frame, which separates the warp yarns 41 from their closed state to form the shed, until the shed reaches its maximum opening size, ready for weft insertion. Shedding time is usually measured in milliseconds (ms), and it determines the rate of change of tensile strain of the warp yarns 41 during the shedding process. The shorter the shedding time, the faster the stretching rate of the warp yarns 41 from closed to fully open; the longer the shedding time, the more gradual the stretching of the warp yarns 41.

[0090] When the loom speed is below 300 r / min, the cycle time of each weaving cycle is greater than 200 ms, resulting in low production efficiency and reduced economic viability for large-scale industrial production. Below this speed, the stretching rate of warp yarn 41 during the shedding process is too slow, and the residence time of warp yarn 41 in the fully open shed state is too long—increasing the static creep time experienced by the self-generating yarn in the continuously tensioned fully open shed state, exacerbating the creep accumulation effect of the functional coating. Therefore, 300 r / min is both the minimum speed for economical production and the lower limit for controlling the static creep of the yarn. When the speed exceeds 600 r / min, warp yarn 41 undergoes more than 10 tension-retraction cycles per second. Compared with pure structural yarn, the overall flexibility and fatigue resistance of self-generating yarn are reduced to some extent due to the presence of internal functional materials. Under high-frequency alternating tension, the interface between the functional material and the conductive material in the yarn, and the adhesion interface between the yarn and the coating layer, are subjected to repeated shear stress, which easily leads to the generation and gradual propagation of microcracks. Meanwhile, the frequency of high-speed reciprocating friction of the warp yarn 41 in the heddle eye and reed teeth increases linearly with the machine speed, leading to increased wear on the yarn surface. By controlling the upper limit of the machine speed at 600 r / min, the self-generating yarn can be continuously woven while maintaining its function.

[0091] When the shedding time is too short (below 45 ms), the warp yarn 41 is rapidly stretched from a closed state to a fully open state. The excessively high stretching rate causes the self-generating yarn to experience an almost impact-like tensile load, resulting in dynamic stress on the yarn surface and internal interfaces exceeding normal levels. 45 ms ensures that the shedding stretching process remains within the strain rate range that the yarn material can withstand. An excessively long shedding time prolongs the time the warp yarn 41 remains in a fully stretched state, increasing the cumulative creep under continuous tension. Simultaneously, an excessively long shedding time encroaches on the time windows for weft insertion and beat-up—insufficient weft insertion time results in insufficient weft yarn 42 fly-through, and insufficient beat-up time results in the weft yarn 42 not being sufficiently tightened to the weft end by the reed. 115 ms is the upper limit of the shedding time that can be coordinated with other process times at all machine speeds.

[0092] In the rapier loom, the rapier head feeds the weft yarn 42 via mechanical clamping, ensuring that the weft yarn 42 is not directly eroded by compressed airflow during weft insertion. This characteristic is particularly important for fabrics 40 containing self-generating yarns in the weft yarn 42. High-speed airflow could cause the self-generating yarns to be abraded by the airflow or deviate from their intended flight path due to airflow disturbance when passing over the shed. The warp yarn 41 is also unaffected by the airflow from the auxiliary nozzles during the rapier opening process, resulting in a clear and stable shed.

[0093] Air-jet looms are suitable for fabrics 40 where all weft yarns (42) are structured yarns and do not contain self-generating yarns. Air-jet weft insertion speed is higher than that of rapier looms, resulting in higher production efficiency. However, care must be taken to ensure that the jet direction of the auxiliary nozzles is not deflected to impact the surface of the warp yarn layer (41).

[0094] This application provides a wearable device including a fabric 40, a data acquisition module, a control module, and a communication module. The fabric 40, the data acquisition module, the control module, and the communication module are electrically connected in sequence. The data acquisition module is used to acquire electrical energy output by the fabric 40, the control module is used to process the electrical energy acquired by the data acquisition module and generate a detection signal, and the communication module is used to output the detection signal.

[0095] Wearable items refer to products that can be worn or attached to the body, including but not limited to clothing (such as tops, trousers, underwear, and socks), headwear (such as hats, headscarves, and headbands), neckwear (such as scarves and ties), armwear (such as sleeves, wrist guards, and gloves), legwear (such as knee pads and socks), and torsowear (such as belts, suspenders, and waist supports). Wearable items are primarily composed of fabrics containing self-generating yarns, combining the concealing / protective functions of traditional wearable items with the self-generating sensing function.

[0096] The acquisition module refers to an electronic circuit module electrically connected to the thermoelectric signal output terminal and / or the triboelectric signal output terminal of the fabric 40, used to acquire the temperature difference voltage signal output by the thermoelectric yarn 20 and / or the electrical signal output by the triboelectric yarn 30. The acquisition module may include, but is not limited to, voltage amplifiers, charge amplifiers, analog-to-digital converters (ADCs), rectifier circuits, energy storage capacitors, or miniature batteries. The acquisition module converts the weak electrical signal output by the fabric 40 into a voltage signal or digital signal that can be processed by the subsequent control module.

[0097] The control module refers to a microprocessor or microcontroller unit (MCU) electrically connected to the acquisition module. It analyzes and processes the signals input from the acquisition module and generates detection signals based on the processing results. The control module runs preset signal processing algorithms. For example, it counts pulses of triboelectric pulse signals to estimate the number of steps or the action frequency, calibrates thermoelectric signals to estimate body surface temperature, and encodes the processing results into a detection signal for output.

[0098] A communication module is a wireless or wired communication unit that is electrically connected to the control module. It is used to send the detection signals generated by the control module to external receiving devices (such as smartphones, smartwatches, cloud servers, or local gateways) in the form of wireless radio frequency signals, Bluetooth signals, Wi-Fi signals, near field communication (NFC) signals, or wired serial signals.

[0099] Sequential electrical connection refers to the signal flowing step by step along the transmission path of fabric 40, acquisition module, control module, and communication module. The raw electrical signal output from fabric 40 first enters the acquisition module for amplification and digitization. The digital signal output from the acquisition module enters the control module for analysis and processing. The detection signal generated by the control module enters the communication module for external transmission.

[0100] Wearable devices could be sleep monitoring pajamas, with the collar and cuffs made of fabric 40 woven from self-generating yarn. This fabric utilizes the temperature difference between body and environment during sleep to maintain continuous thermoelectric signal output and monitor body temperature trends. The triboelectric signal segment is activated when the wearer turns over, recording the number of turns. The control module records the body surface temperature change curve and movement data throughout the night, synchronizing to a mobile sleep analysis app via BLE the following morning. Alternatively, a wristband could be made from the self-generating fabric 40, with narrow strips of fabric 40 woven into the wristband using self-generating yarn as warp yarn. The data acquisition module and control communication module are integrated into a silicone-encapsulated button on the outside of the wristband. Wearing the wristband automatically begins monitoring body temperature and wrist movement, with the data read by a mobile phone via NFC. Alternatively, it could be used as clothing or other props in motion capture.

[0101] It should be noted that all directional indications (such as up, down, left, right, front, back, etc.) in the embodiments of the present invention are only used to explain the relative positional relationship and movement of each component in a specific posture. If the specific posture changes, the directional indication will also change accordingly.

[0102] It should also be noted that when a component is referred to as being "fixed to" or "set on" another component, it can be directly on the other component or may be connected to an intermediary component. When a component is referred to as being "connected to" another component, it can be directly connected to the other component or indirectly connected to the other component through an intermediary component.

[0103] Furthermore, the use of terms such as "first" and "second" in this invention is for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined with "first" or "second" may explicitly or implicitly include at least one of that feature. Additionally, the technical solutions of the various embodiments can be combined with each other, but only on the basis of being achievable by those skilled in the art. When the combination of technical solutions is contradictory or impossible to implement, such a combination of technical solutions should be considered non-existent and not within the scope of protection claimed by this invention.

[0104] The above description is merely a preferred embodiment of the present invention and does not limit the patent scope of the present invention. Any equivalent structural transformations made using the contents of the present invention's specification and drawings under the inventive concept of the present invention, or direct / indirect applications in other related technical fields, are included within the patent protection scope of the present invention.

Claims

1. A self-generating yarn, characterized in that, include: Thermoelectric yarn, extending along the length of the self-generating yarn, is used to generate electrical energy under the action of temperature difference; At least one triboelectric yarn, extending in a spiral along the length of the self-generating yarn and combined with the thermoelectric yarn, is used to generate electrical energy when rubbed against other contact objects.

2. The self-generating yarn according to claim 1, characterized in that, The thermoelectric yarn extends in a straight line direction; The at least one triboelectric yarn is wound around the outer periphery of the thermoelectric yarn to form a covering layer, which is used to simultaneously act on the temperature difference of the thermoelectric yarn.

3. The self-generating yarn according to claim 2, characterized in that, The coverage of the thermoelectric yarn by the covering layer is M, where 70% ≤ M ≤ 95%; and / or, The ratio of the diameter of the triboelectric yarn to the pitch of the triboelectric yarn is 0.25-0.

5.

4. The self-generating yarn according to claim 2, characterized in that, The at least one triboelectric yarn includes a positive triboelectric yarn and a negative triboelectric yarn, the positive triboelectric yarn and the negative triboelectric yarn are used to generate electrical energy by mutual friction, and the positive triboelectric yarn and the negative triboelectric yarn have opposite directions of rotation to form a double helix structure around the thermoelectric yarn; or, The at least one triboelectric yarn includes a negative triboelectric yarn or a positive triboelectric yarn, used to generate electrical energy when rubbed against other contacting objects.

5. The self-generating yarn according to claim 1, characterized in that, The thermoelectric yarn extends in a spiral shape; The thermoelectric yarn and the triboelectric yarn are intertwined to form a helical structure.

6. The self-generating yarn according to claim 5, characterized in that, The at least one triboelectric yarn includes a positive triboelectric yarn and a negative triboelectric yarn, which are used to generate electrical energy through mutual friction. The positive triboelectric yarn, the negative triboelectric yarn, and the thermoelectric yarn form a triple helix structure. The positive triboelectric yarn and the negative triboelectric yarn have opposite directions of rotation, and the thermoelectric yarn and the positive triboelectric yarn have the same direction of rotation or the thermoelectric yarn and the negative triboelectric yarn have the same direction of rotation. or, The at least one triboelectric yarn includes a positive triboelectric yarn or a negative triboelectric yarn, used to generate triboelectricity by friction with other contacting objects. The thermoelectric yarn and the positive triboelectric yarn or the negative triboelectric yarn form a double helix structure, and the thermoelectric yarn and the positive triboelectric yarn or the negative triboelectric yarn have the same or opposite helix directions.

7. The self-generating yarn according to claim 1, characterized in that, The triboelectric yarn includes a conductive layer and a triboelectric skin layer. The triboelectric skin layer is wrapped around the conductive layer and is used to generate triboelectricity by rubbing against other contacting objects. The conductive layer is used to transfer the charge corresponding to the electrical energy generated by friction along the length direction of the triboelectric yarn.

8. The self-generating yarn according to claim 1, characterized in that, The thermoelectric yarn includes a buffer layer, a thermoelectric layer, and an encapsulation layer arranged sequentially from the inside out. The thermoelectric layer is wrapped around the buffer layer, and the encapsulation layer is wrapped around the thermoelectric layer. The buffer layer is made of a phase change material to maintain the temperature difference between the two sides of the thermoelectric yarn. The thermoelectric layer is used to convert the temperature difference between the two sides of the thermoelectric yarn into electrical energy.

9. A fabric, characterized in that, The fabric comprises a plurality of warp yarns and a plurality of weft yarns, wherein the plurality of warp yarns include self-generating yarns as described in any one of claims 1-8, the plurality of warp yarns are arranged along a first direction, the plurality of weft yarns include structural yarns, the plurality of weft yarns are arranged along a second direction, the first direction and the second direction are set at an angle, and the plurality of warp yarns and the plurality of weft yarns are interwoven to form the fabric.

10. The fabric according to claim 9, characterized in that, At least one of the weft yarns is a self-generating yarn.

11. The fabric according to claim 9, characterized in that, The self-generating yarn includes a first self-generating yarn and a second self-generating yarn. The triboelectric yarn corresponding to the first self-generating yarn is a positive triboelectric yarn, and the triboelectric yarn corresponding to the second self-generating yarn is a negative triboelectric yarn. The positive triboelectric yarn and the negative triboelectric yarn are used to generate electrical energy through mutual friction. The first self-generating yarn and the second self-generating yarn are arranged alternately along the first direction.

12. The fabric according to claim 9, characterized in that, The fabric is a 2 / 2 twill weave.

13. The fabric according to claim 9, characterized in that, The plurality of warp yarns include structural yarns, and along the first direction, one self-generating yarn is provided every X structural yarns, where 3≤X≤10.

14. The fabric according to claim 13, characterized in that, The fabric includes an energy harvesting zone, a motion detection zone, and a reinforcement zone. The value of X corresponding to the energy harvesting zone is X1, the value of X corresponding to the motion detection zone is X2, and the value of X corresponding to the reinforcement zone is X3, where X1≤X2≤X3.

15. A method for preparing a fabric as described in any one of claims 9-14, characterized in that, The self-generating yarn is used as the warp yarn, and the structural yarn is used as the weft yarn. The weft yarn and the warp yarn are woven together on a loom to form a fabric.

16. The method according to claim 15, characterized in that, The warp tension is F1, 0.12 cN / dtex ≤ F1 ≤ 0.40 cN / dtex; and / or, The weft tension of the weft yarn is F2, 0.21cN / dtex≤F2≤0.38cN / dtex.

17. The method according to claim 15, characterized in that, The loom speed is N, 300 r / min ≤ N ≤ 600 r / min; and / or, The shedding time of the loom is 45ms-115ms; and / or, The loom is either an air-jet loom or a rapier loom.

18. A wearable device, characterized in that, The device includes a fabric, a data acquisition module, a control module, and a communication module as described in any one of claims 9-14. The fabric, data acquisition module, control module, and communication module are electrically connected in sequence. The data acquisition module is used to acquire electrical energy output by the fabric. The control module is used to process the electrical energy acquired by the data acquisition module and generate a detection signal. The communication module is used to output the detection signal.