A weak magnetic flaw detection evaluation method for surface scratches of an undercarriage inner tube
Patent Information
- Application Number
- CN202610947865.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-06-29
- Publication Date
- 2026-09-04
AI Technical Summary
[0005]本发明的目的在于提供一种起落架内筒表面划痕的弱磁探伤评估方法,以解决上述背景技术中提出的现有弱磁检测技术主要针对顺磁性金属材料(如奥氏体不锈钢)的裂纹缺陷进行定性或定量评价,对于航空起落架内筒常用的超高强度钢(铁磁性材料)表面划痕的弱磁检测与评估方法尚缺乏系统研究,特别是,起落架内筒为回转体结构,表面曲率大,且材料具有高磁导率特性,其弱磁信号特征与平板类试件存在显著差异,直接套用现有方法难以获得准确的评估结果,现有方法仅能判断缺陷有无,无法对划痕的危险程度给出定量评估,限制了检测结果在维修决策中的直接应用问题
本发明采用柔性载体搭载多个传感器,通过自适应的布设方式实现传感器与内筒曲面的良好贴合,有效克服了起落架内筒圆柱面曲率对检测信号一致性的影响,提高了检测的重复性和可靠性,采用基于小波阈值的自适应噪声抑制方法,能够在保留微弱划痕漏磁信号特征的同时有效滤除地磁背景噪声和电路噪声,相比传统的滤波方法具有更好的信号保真度,通过构建包含漏磁信号峰值、峰谷差和有效信号宽度的多维特征参数体系,并结合量化评估模型对划痕危险程度进行分级,克服了现有方法仅能判断缺陷有无的局限,为起落架维修决策提供了直接的量化依据。
Smart Images

Figure CN122689938A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of nondestructive testing technology, specifically to a weak magnetic flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder. Background Technology
[0002] The landing gear is one of the most important load-bearing components of an aircraft. During takeoff, landing, and taxiing, it bears enormous impact loads and alternating stresses. As an important part of the cushioning system, the surface integrity of the landing gear inner cylinder directly affects the service life of the landing gear and flight safety. In actual use, the surface of the landing gear inner cylinder is prone to various types of surface scratches due to sand and gravel impacts, foreign object wear, improper maintenance, and other reasons. If these surface scratches are not detected and accurately assessed in time, they may expand into fatigue cracks under alternating loads, seriously threatening flight safety.
[0003] Currently, the main methods for detecting scratches on the inner surface of landing gear cylinders include magnetic particle testing, penetrant testing, and eddy current testing. Magnetic particle testing has high sensitivity, but it requires an external magnetization device and demagnetization after testing. It also requires a high level of experience from the testing personnel and is difficult to achieve quantitative assessment. Penetrant testing is simple to operate, but it can only detect defects that open on the surface, and the testing process involves chemical reagents, which is not environmentally friendly. Eddy current testing can achieve non-contact testing, but it is sensitive to the lift-off effect and has limited sensitivity for detecting shallow defects such as scratches, making it difficult to accurately assess the depth parameters of the scratches.
[0004] Weak magnetic field testing is an emerging non-destructive testing method that utilizes the Earth's magnetic field as a natural excitation source. High-sensitivity magnetic sensors capture weak magnetic anomalies in ferromagnetic materials caused by defects or stress concentration. Compared to traditional magnetic particle testing and eddy current testing, weak magnetic field testing offers advantages such as no need for an external excitation source, non-contact operation, no pollution, and the ability to penetrate coatings. However, existing weak magnetic field testing technologies primarily focus on qualitative or quantitative evaluation of crack defects in paramagnetic metallic materials (such as austenitic stainless steel). Systematic research is lacking on weak magnetic field testing and evaluation methods for surface scratches on ultra-high-strength steel (ferromagnetic material) commonly used in aircraft landing gear inner cylinders. In particular, the landing gear inner cylinder is a rotating structure with a large surface curvature and high magnetic permeability, resulting in significantly different weak magnetic signal characteristics compared to flat plate specimens. Directly applying existing methods makes it difficult to obtain accurate evaluation results. Existing methods can only determine the presence or absence of defects but cannot provide a quantitative assessment of the severity of scratches, limiting the direct application of test results in maintenance decisions. Summary of the Invention
[0005] The purpose of this invention is to provide a weak magnetic flaw detection assessment method for surface scratches on landing gear inner cylinders. This addresses the problem that existing weak magnetic detection technologies, as mentioned in the background, primarily focus on qualitative or quantitative evaluation of crack defects in paramagnetic metallic materials (such as austenitic stainless steel). Systematic research is lacking on weak magnetic detection and assessment methods for surface scratches on ultra-high strength steel (ferromagnetic material) commonly used in aircraft landing gear inner cylinders. In particular, the landing gear inner cylinder is a rotating structure with a large surface curvature and high magnetic permeability, resulting in significantly different weak magnetic signal characteristics compared to flat plate specimens. Directly applying existing methods makes it difficult to obtain accurate assessment results. Existing methods can only determine the presence or absence of defects but cannot provide a quantitative assessment of the severity of the scratches, thus limiting the direct application of detection results in maintenance decisions.
[0006] To achieve the above objectives, the present invention provides the following technical solution: a weak magnetic flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder, the evaluation method comprising the following steps: S1. First, the surface of the landing gear inner cylinder to be tested needs to be pre-treated by cleaning. Under the condition of no external excitation magnetic field, the geomagnetic field environment of the landing gear inner cylinder surface is calibrated by using the geomagnetic field as a natural excitation source to establish a background magnetic field baseline. According to the outer diameter and surface curvature radius R of the landing gear inner cylinder, N triaxial weak magnetic sensors are arranged at equal angles along the circumference of the inner cylinder on a flexible carrier. The flexible carrier covers the outer surface of the section of the inner cylinder to be tested, and the sensitive axis of the sensor points to the radial direction of the inner cylinder. By adjusting the tension of the flexible carrier, the sensitive surface of each sensor is kept at a lifting distance of 0.5~1.5mm from the surface of the inner cylinder.
[0007] S2. Then, a three-axis magnetic field weakening sensor is used to perform multiple scans along the axial direction of the landing gear inner tube to collect raw data of the magnetic field weakening signal on the inner tube surface. The raw data of the magnetic field weakening signal includes a magnetic induction intensity component perpendicular to the inner tube surface. The collected raw data of the magnetic field weakening signal is preprocessed, including adaptive noise suppression and trend term removal. The magnetic anomaly feature signal of the scratch area is extracted from the preprocessed signal.
[0008] S3. Finally, multi-dimensional scratch feature parameters need to be extracted from the magnetic anomaly feature signal. The multi-dimensional scratch feature parameters include time domain feature parameters, frequency domain feature parameters and morphological feature parameters. The extracted feature parameters are input into the pre-constructed scratch hazard assessment model. At the same time, the maximum values of leakage magnetic signal peak value, peak-to-valley difference and effective signal width need to be extracted for all sensor locations. These are the corresponding preset thresholds. According to the assessment index H, the scratch hazard level is divided into three levels: safety level, concern level and danger level.
[0009] Preferably, the number of the triaxial magnetic field weakening sensors is N=16, the circumferential angular interval of the triaxial sensors is Δθ=22.5°, the lift-off distance of the triaxial magnetic field weakening sensors is 1.0mm, the scanning speed of the triaxial magnetic field weakening sensors is set to 1.0mm / s, and the sampling frequency is set to 500Hz.
[0010] Preferably, the threshold processing employs a soft thresholding method, where the absolute value is less than a threshold T. j The wavelet coefficients are set to zero, and for those whose absolute values are greater than or equal to the threshold T... j The wavelet coefficients shrink to zero, and the safety level threshold is H. safe =0.8, the hazard level threshold is H danger =1.3; when H≤H safe Scratches are considered safe at this level; when H... safe <H≤H danger The level of attention is determined by the number of scratches, when H>H. danger Scratches are classified as dangerous.
[0011] Preferably, the flexible carrier is a polyimide flexible circuit board. The scratch hazard level assessment results are correlated with the circumferential and axial position information of the scratch on the landing gear inner cylinder surface to generate a scratch distribution assessment report on the landing gear inner cylinder surface. The assessment report uses a circumferential-axial two-dimensional coordinate system to mark the location and hazard level of each scratch level.
[0012] Preferably, the geomagnetic field environment calibration specifically includes: selecting multiple calibration points in the scratch-free area of the landing gear inner cylinder, collecting the magnetic induction intensity values at each calibration point, calculating their mean and standard deviation, and establishing a background magnetic field baseline. The background magnetic field baseline is used for trend term removal and background field compensation in subsequent signal processing.
[0013] Preferably, the adaptive noise suppression adopts a threshold denoising method based on wavelet transform. By adaptively selecting the wavelet basis function and the number of decomposition layers, Gaussian white noise and sensor background noise in the weak magnetic signal are suppressed. The trend term removal adopts a background field subtraction method based on polynomial fitting. The trend term obtained by fitting the background magnetic field baseline is subtracted from the measured signal to obtain a feature signal containing only scratch magnetic anomaly information.
[0014] Preferably, the time-domain feature parameters include the peak value, peak-to-peak value, root mean square value, and waveform factor of the magnetic anomaly signal; the frequency-domain feature parameters include the spectral energy concentration, main frequency amplitude, and frequency band energy distribution extracted after fast Fourier transform; and the morphological feature parameters include the full width at half maximum (FWHM), signal area, and magnetic anomaly gradient of the magnetic anomaly signal.
[0015] Preferably, the construction of the scratch weak magnetic evaluation model includes: preparing a standard specimen of the landing gear inner cylinder with artificial scratches of different geometric parameters, the geometric parameters including the length, width and depth of the scratches; performing weak magnetic detection and feature parameter extraction on the standard specimen; establishing a sample library of mapping relationships between scratch geometric parameters and multi-dimensional feature parameters; and training a quantitative evaluation model of scratch geometric parameters based on a support vector regression algorithm or a random forest regression algorithm, using the multi-dimensional feature parameters as input and the scratch geometric parameters as output.
[0016] Compared with the prior art, the beneficial effects of the present invention are as follows: This invention employs a flexible carrier to mount multiple sensors, achieving excellent fit between the sensors and the inner cylinder surface through an adaptive deployment method. This effectively overcomes the influence of the cylindrical curvature of the landing gear inner cylinder on the consistency of the detection signal, improving the repeatability and reliability of the detection. An adaptive noise suppression method based on wavelet thresholding is used, which can effectively filter out geomagnetic background noise and circuit noise while preserving the characteristics of weak scratch leakage magnetic signals. Compared with traditional filtering methods, it has better signal fidelity. By constructing a multi-dimensional feature parameter system including the peak value, peak-valley difference, and effective signal width of the leakage magnetic signal, and combining it with a quantitative evaluation model to classify the degree of scratch danger, this invention overcomes the limitation of existing methods that can only determine the presence or absence of defects, providing a direct quantitative basis for landing gear maintenance decisions.
[0017] This invention utilizes the Earth's magnetic field as a natural excitation source, eliminating the need for external magnetization devices. The detection process is radiation-free, pollution-free, and requires no demagnetization, resulting in high detection efficiency. It is suitable for rapid on-site detection of landing gear without disassembly. A specialized geomagnetic environment calibration method and background magnetic field baseline have been established to address the rotating structure and ferromagnetic material characteristics of the landing gear inner cylinder. This effectively eliminates the influence of differences in inner cylinder curvature and material permeability on the detection signal, improving detection accuracy. By extracting multi-dimensional feature parameters in the time domain, frequency domain, and morphology, and employing machine learning regression algorithms to construct a scratch weak magnetic field assessment model, quantitative assessment of scratch length, width, and depth is achieved, overcoming the limitation of traditional detection methods that can only make qualitative judgments. Attached Figure Description
[0018] Figure 1 This is an overall flowchart of the present invention; Figure 2 This is a flowchart of the magnetic field weakening signal preprocessing of the present invention; Figure 3 This is a flowchart illustrating the construction of the scratch weak magnetic field evaluation model of the present invention; Figure 4 This is a flowchart of the signal acquisition and processing of the present invention. Detailed Implementation
[0019] The technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0020] Example 1: This invention provides a weak magnetic flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder, comprising the following steps: S1. First, the surface of the landing gear inner cylinder to be tested needs to be pre-treated by cleaning. Without an external excitation magnetic field, the geomagnetic field is used as a natural excitation source to calibrate the geomagnetic environment of the landing gear inner cylinder surface, establishing a background magnetic field baseline. Based on the outer diameter and surface curvature radius R of the landing gear inner cylinder, N triaxial magnetic weakening sensors are arranged at equal angles along the circumference of the inner cylinder on a flexible carrier. The flexible carrier covers the outer surface of the section of the inner cylinder to be tested, with the sensor sensitive axes pointing radially towards the inner cylinder. By adjusting the tension of the flexible carrier, a lift-off distance of 0.5~1.5mm is maintained between the sensor sensitive surface and the inner cylinder surface. The number of triaxial magnetic weakening sensors N=16, and the circumferential angular interval Δθ=22.5° is between the triaxial sensors. The lift-off distance of the triaxial magnetic weakening sensors is 1.0mm, the scanning speed is set to 1.0mm / s, the sampling frequency is set to 500Hz, and a soft thresholding method is used for threshold processing. For values less than the threshold T... j The wavelet coefficients are set to zero, and for those whose absolute values are greater than or equal to the threshold T... j The wavelet coefficients shrink to zero, and the safety level threshold is H. safe =0.8, the hazard level threshold is H danger =1.3; when H≤H safe Scratches are considered safe at this level; when H... safe <H≤H danger The level of attention is determined by the number of scratches, when H>H. danger Scratches are classified as dangerous.
[0021] S2. Next, a triaxial weak magnetic field sensor is used to perform multiple scans along the axial direction of the landing gear inner cylinder to collect raw data of weak magnetic field signals on the inner cylinder surface. The raw data of weak magnetic field signals includes magnetic induction intensity components perpendicular to the inner cylinder surface. The collected raw data of weak magnetic field signals is preprocessed, including adaptive noise suppression and trend term removal. Magnetic anomaly feature signals of the scratch area are extracted from the preprocessed signal. The flexible carrier is a polyimide flexible circuit board. The scratch hazard level assessment results are correlated with the circumferential and axial position information of the scratch on the landing gear inner cylinder surface to generate a scratch distribution assessment report on the landing gear inner cylinder surface. The assessment report marks the location and hazard level of each scratch level in a circumferential-axial two-dimensional coordinate system. The geomagnetic field environment calibration specifically includes: selecting multiple calibration points in the scratch-free area of the landing gear inner cylinder, collecting the magnetic induction intensity values at each calibration point, calculating their mean and standard deviation, and establishing a background magnetic field baseline. The background magnetic field baseline is used for trend term removal and background field compensation in subsequent signal processing.
[0022] S3. Finally, multi-dimensional scratch feature parameters need to be extracted from the magnetic anomaly characteristic signal. These parameters include time-domain, frequency-domain, and morphological features. The extracted parameters are input into a pre-constructed scratch hazard assessment model. Simultaneously, the maximum values of the leakage magnetic field signal peak, peak-to-valley difference, and effective signal width need to be extracted for all sensor locations, corresponding to pre-set thresholds. Based on the assessment index H, the scratch hazard level is divided into three levels: safe, concerning, and dangerous. Adaptive noise suppression uses a threshold denoising method based on wavelet transform. By adaptively selecting the wavelet basis function and decomposition level, Gaussian white noise and sensor background noise in the weak magnetic signal are suppressed. Trend term removal uses a background field subtraction method based on polynomial fitting. The measured signal is subtracted from the trend term obtained by fitting the background magnetic field baseline. The model for assessing magnetic field weakening based on scratches includes the following features: time-domain features include peak value, peak-to-peak value, root mean square value, and waveform factor; frequency-domain features include spectral energy concentration, dominant frequency amplitude, and frequency band energy distribution extracted after fast Fourier transform; and morphological features include full width at half maximum (FWHM), signal area, and magnetic anomaly gradient. The model involves preparing standard landing gear inner cylinder specimens with artificial scratches of different geometric parameters (length, width, and depth), performing magnetic field weakening detection and feature parameter extraction on the standard specimens, establishing a mapping relationship sample library between scratch geometric parameters and multi-dimensional feature parameters, and training a quantitative assessment model for scratch geometric parameters based on support vector regression or random forest regression algorithms, using multi-dimensional feature parameters as input and scratch geometric parameters as output.
[0023] Example 2: This embodiment is basically the same as Embodiment 1, except that: An anisotropic magnetoresistive sensor with a resolution of 0.5 nT was employed. The lift-off distance between the probe and the inner cylinder surface was set to 3 mm, and the scanning speed was increased to 30 mm / s to meet the needs of rapid on-site inspection. The scratch weak magnetic field assessment model adopted a random forest regression algorithm, with 100 decision trees and a maximum depth of 10 layers per tree. Compared to support vector regression, the random forest regression algorithm has better anti-overfitting ability and robustness to noisy data. The confidence level of the scratch weak magnetic field assessment model was evaluated by calculating the relative error between the scratch depth value output by the model and the scratch depth value measured by a high-precision profilometer. The relative error threshold is set to 15%. When the relative error exceeds 15%, the system issues a re-detection prompt and automatically increases the scanning density of the area, increasing the width of the overlapping area of the scanning channels to 50% of the sensor width for retesting.
[0024] Example 3: This embodiment is basically the same as Embodiment 1, except that: N=8 sensors are used, the angle interval Δθ=45°, the scanning speed v=2.0mm / s, and the sampling frequency f=200Hz. A shallow scratch with a depth of approximately 0.3mm on the inner cylinder surface is detected, and the feature parameter P is extracted. max =3.8μT, ΔP max =7.2μT, W max =1.3s, calculate the evaluation index H=0.4×(3.8 / 5.0)+0.4×(7.2 / 10.0)+0.2×(1.3 / 1.5)=0.304+0.288+0.173=0.765. Since H=0.765 <H safe =0.8, the scratch is judged to be of a safe level and no treatment is required.
[0025] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.
Claims
1. A weak magnetic field flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder, characterized in that, Its evaluation method includes the following steps: S1. First, the surface of the landing gear inner cylinder to be tested needs to be pre-treated by cleaning. Under the condition of no external excitation magnetic field, the geomagnetic field environment of the landing gear inner cylinder surface is calibrated using the geomagnetic field as a natural excitation source to establish a background magnetic field baseline. According to the outer diameter and surface curvature radius R of the landing gear inner cylinder, N triaxial weak magnetic sensors are arranged at equal angles along the circumference of the inner cylinder on a flexible carrier. The flexible carrier covers the outer surface of the section of the inner cylinder to be tested, and the sensitive axis of the sensor points to the radial direction of the inner cylinder. By adjusting the tension of the flexible carrier, the sensitive surface of each sensor is kept at a lifting distance of 0.5~1.5mm from the surface of the inner cylinder. S2. Then, a three-axis magnetic field weakening sensor is used to perform multiple scans along the axial direction of the landing gear inner tube to collect raw data of the magnetic field weakening signal on the inner tube surface. The raw data of the magnetic field weakening signal includes a magnetic induction intensity component perpendicular to the inner tube surface. The collected raw data of the magnetic field weakening signal is preprocessed, including adaptive noise suppression and trend term removal. The magnetic anomaly feature signal of the scratch area is extracted from the preprocessed signal. S3. Finally, multi-dimensional scratch feature parameters need to be extracted from the magnetic anomaly feature signal. The multi-dimensional scratch feature parameters include time domain feature parameters, frequency domain feature parameters and morphological feature parameters. The extracted feature parameters are input into the pre-constructed scratch hazard assessment model. At the same time, the maximum values of leakage magnetic signal peak value, peak-to-valley difference and effective signal width need to be extracted for all sensor locations. These are the corresponding preset thresholds. According to the assessment index H, the scratch hazard level is divided into three levels: safety level, concern level and danger level.
2. The weak magnetic field flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder according to claim 1, characterized in that: The number of triaxial magnetic field weakening sensors is N=16, and the circumferential angular interval of the triaxial sensors is Δθ=22.5°. The lift-off distance of the triaxial magnetic field weakening sensors is 1.0mm. The scanning speed of the triaxial magnetic field weakening sensors is set to 1.0mm / s, and the sampling frequency is set to 500Hz.
3. The weak magnetic field flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder according to claim 1, characterized in that: The threshold processing employs a soft thresholding method, where the absolute value is less than the threshold T. j The wavelet coefficients are set to zero, and for those whose absolute values are greater than or equal to the threshold T... j The wavelet coefficients shrink to zero, and the safety level threshold is H. safe =0.8, the hazard level threshold is H danger =1.3; when H≤H safe Scratches are considered safe at this level; when H... safe <H≤H danger The level of attention is determined by the number of scratches, when H>H. danger Scratches are classified as dangerous.
4. The weak magnetic field flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder according to claim 1, characterized in that: The flexible carrier is a polyimide flexible circuit board. The scratch hazard level assessment results are correlated with the circumferential and axial position information of the scratch on the landing gear inner cylinder surface to generate a scratch distribution assessment report on the landing gear inner cylinder surface. The assessment report marks the location and hazard level of each scratch level in a circumferential-axial two-dimensional coordinate system.
5. The weak magnetic field flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder according to claim 1, characterized in that: The geomagnetic field environment calibration specifically includes: selecting multiple calibration points in the scratch-free area of the landing gear inner cylinder, collecting the magnetic induction intensity values at each calibration point, calculating their mean and standard deviation, and establishing a background magnetic field baseline; the background magnetic field baseline is used for trend term removal and background field compensation in subsequent signal processing.
6. The weak magnetic field flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder according to claim 1, characterized in that: The adaptive noise suppression adopts a threshold denoising method based on wavelet transform. By adaptively selecting the wavelet basis function and the number of decomposition layers, Gaussian white noise and sensor background noise in the weak magnetic signal are suppressed. The trend term removal adopts a background field subtraction method based on polynomial fitting. The trend term obtained by fitting the background magnetic field baseline is subtracted from the measured signal to obtain a feature signal containing only scratch magnetic anomaly information.
7. The weak magnetic field flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder according to claim 1, characterized in that: The time-domain characteristic parameters include the peak value, peak-to-peak value, root mean square value, and waveform factor of the magnetic anomaly signal; the frequency-domain characteristic parameters include the spectral energy concentration, main frequency amplitude, and frequency band energy distribution extracted after fast Fourier transform; and the morphological characteristic parameters include the full width at half maximum (FWHM), signal area, and magnetic anomaly gradient of the magnetic anomaly signal.
8. The weak magnetic field flaw detection evaluation method for scratches on the surface of the landing gear inner cylinder according to claim 1, characterized in that: The construction of the scratch-induced magnetic field assessment model includes: preparing standard specimens of landing gear inner cylinders with artificial scratches of different geometric parameters, including the length, width, and depth of the scratches; performing weak magnetic field detection and feature parameter extraction on the standard specimens; establishing a sample library of mapping relationships between scratch geometric parameters and multi-dimensional feature parameters; and training a quantitative assessment model of scratch geometric parameters based on support vector regression or random forest regression algorithms, using the multi-dimensional feature parameters as input and the scratch geometric parameters as output.