A combined homogenization method of donkey-hide gelatin glue liquid, a production method of donkey-hide gelatin finished product and the donkey-hide gelatin finished product
Patent Information
- Application Number
- CN202610795077.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-06-04
- Publication Date
- 2026-09-22
AI Technical Summary
[0004]本发明的目的在于克服现有阿胶生产工艺中人工打沫效率低下、批次稳定性差、胶液损耗严重等技术缺陷,提供一种阿胶胶液的联合均质方法、阿胶成品的生产方法及阿胶成品
1.产品质量显著改善。将胶体磨与微射流高压均质两种破碎技术进行有机串联,形成梯度破碎工艺。胶体磨作为初级破碎设备,利用其高速旋转的磨盘产生强大的剪切力,对胶液中的较大颗粒进行初步破碎和均质化处理,有效降低胶液粒度分布范围,为后续深度破碎创造有利条件,避免后续微射流高压均质腔体管道堵塞。微射流高压均质则作为深度破碎,加压至1500-1800bar,使胶液在极短时间内经历剧烈剪切、高速撞击及空穴效应三重作用,实现纳米级颗粒的破碎效果。两种破碎方式的协同作用,使胶液中的脂肪类物质及水不溶物被充分破碎、分散,通过微射流高压均质破碎阿胶胶液后,胶液的平均粒径均为纳米级别,质地更加细腻,流动性提升明显且胶液挂壁现象减弱;
Smart Images

Figure CN122787101A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of deep processing technology of donkey-hide gelatin, specifically to a combined homogenization method for donkey-hide gelatin liquid, a production method for finished donkey-hide gelatin products, and the finished donkey-hide gelatin products. Background Technology
[0002] Asini Corii Colla is a traditional and precious tonic in my country, known for its blood-nourishing, yin-tonifying, dryness-moistening, and hemostatic effects. In traditional Asini Corii Colla production, the gelatin solution often contains a large amount of foam and impurities, rich in fatty substances and water-insoluble components, significantly affecting the internal quality and appearance of the finished product. Traditional impurity removal relies heavily on repeated manual skimming of the surface foam, which is not only cumbersome and inefficient but also prone to batch-to-batch quality inconsistencies due to significant human error. Furthermore, this method easily leads to gelatin solution loss and nutrient depletion, restricting product yield and quality improvement.
[0003] Based on the above-mentioned technical background, this invention addresses the prominent problems in traditional donkey-hide gelatin production processes, such as low efficiency of manual foaming, poor batch stability, and large loss of gelatin solution. It innovatively proposes a gelatin solution processing technology that combines colloid milling and micro-jet high-pressure homogenization. Summary of the Invention
[0004] The purpose of this invention is to overcome the technical defects of existing donkey-hide gelatin production processes, such as low efficiency of manual foaming, poor batch stability, and serious loss of gelatin solution. This invention provides a combined homogenization method for donkey-hide gelatin solution, a production method for the finished donkey-hide gelatin product, and the finished product itself. This method combines colloid milling and micro-jet high-pressure homogenization in series to form a gradient crushing process, achieving highly efficient refining of the donkey-hide gelatin solution and significantly improving the quality and batch-to-batch stability of the finished gelatin blocks.
[0005] To solve the above-mentioned technical problems, this application is implemented as follows: According to one aspect of this application, an embodiment of this application provides a method for the combined homogenization of donkey-hide gelatin liquid, the method comprising: pre-treating the donkey-hide gelatin liquid to be processed to obtain a first liquid; The first adhesive solution is subjected to colloid milling to obtain the second adhesive solution; The second adhesive solution is subjected to micro-jet high-pressure homogenization and crushing treatment to obtain the third adhesive solution; In a preferred embodiment, the third adhesive has an average particle size of 160-200 nm and a viscosity of 378-423 cp.
[0006] In some optional embodiments, the pretreatment includes: heating and dissolving the gelatin liquid to be treated, adjusting the temperature of the liquid, controlling the temperature of the liquid to 40℃~60℃, and the water content of the liquid to 65%~80%, to obtain a first liquid; wherein the heating and dissolving temperature is 60℃~70℃, and the dissolving time is 2h~6h.
[0007] To compare and test the effects, the adhesive solution can be preheated to 40-60℃ and stirred evenly. The initial particle size (D10, D50, D90) can be measured as a control group. The viscosity can be recorded using a rotational viscometer.
[0008] In some optional embodiments, the operating conditions for the colloid milling process include: The grinding disc gap in a colloid mill is 0.5-2.5 mm. A serrated grinding disc can be used as the dispersion device. The grinding disc gap should be precisely calibrated beforehand.
[0009] Preferably, the stator and rotor structure of the colloid mill is of the toothed type, helical tooth type, perforated type or disc type.
[0010] Preferably, the grinding disc of the colloid mill is made of one or more of the following materials: tungsten carbide (WC), zirconium oxide (ZrO2), 304 stainless steel, 316L stainless steel, or cemented carbide.
[0011] Preferably, the rotational speed of the colloid mill is 1800-2200 rpm.
[0012] Preferably, the temperature is stabilized at 40-60℃. The temperature of the colloid mill system can be stabilized at 40~60℃ by turning on the circulating water cooling system.
[0013] As a preferred option, the crushing cycle should be 3-5 times.
[0014] As a further preferred embodiment, the grinding disc gap is set to 0.5 mm, and / or the number of crushing cycles is 3.
[0015] In some optional embodiments, the operating conditions for the microjet high-pressure homogenization process include: The pressure for micro-jet high-pressure homogenization is 1500-1800 bar.
[0016] Preferably, the temperature is 25-60℃. During homogenization, the equipment uses a water circulation temperature control system to maintain the equipment temperature within the above range and prevent it from becoming too high.
[0017] As a preferred method, the homogenization cycle is 2-5 times.
[0018] After homogenization, the adhesive solution can be collected and sampled to determine the particle size distribution (D10, D50, D90) of the broken adhesive solution, and compared with the control group.
[0019] As a further preferred embodiment, the microjet high-pressure homogenization crushing pressure is 1500 bar.
[0020] As a preferred method, the homogenization cycle is repeated 3 times.
[0021] According to another aspect of this application, embodiments of this application provide a method for producing a finished donkey-hide gelatin product, the method comprising: Provide donkey-hide gelatin liquid; The donkey-hide gelatin solution was processed using the aforementioned combined homogenization method to obtain a third gelatin solution; The third gelatin solution is concentrated and dried to obtain the finished donkey-hide gelatin product.
[0022] In some alternative embodiments, the concentration pressure is -0.1 MPa to 0.0 MPa; As a further preferred embodiment, the concentration pressure is -0.06 MPa.
[0023] In some alternative implementations, the drying method includes air drying.
[0024] As a further preferred embodiment, the moisture content of the dried donkey-hide gelatin product is ≤15%.
[0025] According to another aspect of this application, an embodiment of this application provides a finished donkey-hide gelatin product, which is prepared using the aforementioned production method for finished donkey-hide gelatin products.
[0026] In some optional embodiments, the moisture content of the finished donkey-hide gelatin product is ≤15%.
[0027] In some optional embodiments, the water-insoluble matter content of the finished donkey-hide gelatin product is ≤1.2%.
[0028] In some alternative implementations, the radius of the light-transmitting spot of the finished donkey-hide gelatin product is 600-800px.
[0029] Implementing the technical solution of the present invention has at least the following beneficial effects: 1. Significantly Improved Product Quality. The colloid mill and micro-jet high-pressure homogenization technologies are organically linked to form a gradient crushing process. The colloid mill, as the primary crushing device, utilizes its high-speed rotating grinding disc to generate strong shearing force, initially crushing and homogenizing larger particles in the colloid solution. This effectively reduces the particle size distribution range of the colloid solution, creating favorable conditions for subsequent deep crushing and preventing blockage of the micro-jet high-pressure homogenization chamber. Micro-jet high-pressure homogenization, as the deep crushing process, applies pressure to 1500-1800 bar, subjecting the colloid solution to intense shearing, high-speed impact, and cavitation effects in a very short time, achieving nanoscale particle crushing. The synergistic effect of the two crushing methods ensures that fatty substances and water-insoluble matter in the colloid solution are fully crushed and dispersed. After micro-jet high-pressure homogenization, the average particle size of the colloid solution is at the nanoscale, resulting in a finer texture, significantly improved fluidity, and reduced adhesion to the walls. The water-insoluble matter content of the finished product obtained by the concentration and drying of the adhesive is reduced by 50% compared with the traditional process, the radius of the light-transmitting spot is increased by 3 times, the appearance is more transparent and amber-colored, the texture is more uniform and delicate, the nutrients are more evenly dispersed, which is conducive to the absorption and utilization of the human body.
[0030] 2. Significantly improved process efficiency. Traditional manual foam removal processes require operators to continuously monitor and repeatedly scrape off the foam, with a single batch processing time reaching tens of hours or even longer, and the labor intensity is high. This invention adopts a mechanized continuous crushing process, where the colloid mill and micro-jet high-pressure homogenizer can achieve automated continuous operation, improving overall production efficiency by more than 50% and significantly reducing labor costs and labor intensity.
[0031] 3. Highly controllable batch stability. Mechanized crushing technology eliminates subjective differences caused by manual operation. Process parameters such as temperature, pressure, and number of cycles can be precisely set and monitored in real time, ensuring a high degree of consistency in quality indicators between different batches of products, thus laying a technical foundation for the standardized production of donkey-hide gelatin products.
[0032] 4. Significantly improved raw material utilization. In traditional manual foaming processes, some of the adhesive is scraped off along with the foam, resulting in raw material loss. This invention uses a physical crushing method, with the adhesive circulating in a closed system, eliminating material loss and achieving a near 100% raw material utilization rate, resulting in significant economic benefits.
[0033] 5. Safe and environmentally friendly process. Both the colloid mill and micro-jet high-pressure homogenization are carried out in closed equipment, avoiding the pollution risks that may be caused by traditional open operations when manually defoaming; at the same time, the physical crushing method does not introduce any chemical additives, ensuring the natural properties and food safety of the product.
[0034] The method described in this invention is applicable to the industrial production of donkey-hide gelatin products and has broad prospects for promotion and application, as well as significant practical value.
[0035] Additional aspects and advantages of this application will be set forth in part in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention. Attached Figure Description
[0036] Figure 1 The finished adhesive block is produced using the method described in Embodiment 1 of this application; Figure 2 A comparison image of the finished adhesive block produced for this application and the finished product made using traditional methods, taken under light. Figure 3 Image showing the measurement results of the light transmittance radius of the adhesive block produced by traditional process; Figure 4 The image shows the results of measuring the transmitted light spot radius of the finished adhesive block produced by the method described in Example 1 of this application; Figure 5 The image shows the measurement results of the light transmittance radius of the finished adhesive block produced by the method described in Example 2 of this application; The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.
[0037] The endpoints and any values of the ranges disclosed herein are not limited to the precise ranges or values, and these ranges or values should be understood to include values close to these ranges or values. For numerical ranges, the endpoint values of the ranges, the endpoint values of the ranges, or individual point values, and individual point values can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed herein. Furthermore, in the specification and claims, "and / or" indicates at least one of the connected objects, and the character " / " generally indicates that the preceding and following related objects are in an "or" relationship.
[0038] Unless otherwise specified, the terms "comprising" and "including" as used in this application can be open-ended or closed-ended. For example, "comprising" and "including" can mean that other components not listed may also be included, or that only the listed components may be included.
[0039] The embodiments of this application will be described in detail below with reference to the accompanying drawings and specific examples and application scenarios.
[0040] In existing technologies, homogenization of donkey-hide gelatin liquid mainly employs single methods such as high-pressure homogenization, high-shear colloid milling, ultrasonic homogenization, and traditional mechanical stirring. While these methods have some effect on refining particles and improving dispersibility, they still have significant drawbacks, making it difficult to balance homogenization efficiency, product quality, and the needs of industrial production. Traditional mechanical stirring homogenization lacks particle refinement capabilities and cannot solve problems such as particle agglomeration, stratification, and sedimentation in the gelatin liquid. It suffers from low mixing efficiency, poor uniformity, and the tendency to introduce air and form foam, making it unable to independently meet homogenization requirements. High-pressure homogenization technology, as the mainstream industrial method, achieves particle refinement through shearing, cavitation, and impact generated by high-pressure slits. However, impurities such as skin residue and fiber impurities easily become entangled and accumulate at the homogenization valve slits, causing channel blockage and wear of the homogenization valve. Furthermore, the particle size distribution is uneven, making it difficult to achieve uniform refinement throughout the entire system. The gap between the valve core and valve seat, the contact surface of the impact ring, mechanical friction, and high-speed shearing in the slits generate significant heat, reaching over 70°C locally, which can easily cause denaturation of heat-sensitive components. High-shear colloid mills rely on high-speed shearing of the rotor and stator to grind particles. However, the shearing force is limited, resulting in insufficient refining effect on high-viscosity, large-particle colloids. The particle size distribution is wide, making it difficult to meet the fineness requirements of high-end products. High-speed friction also generates significant temperature rise, exacerbating the loss of heat-sensitive components. Furthermore, the small gap between the stator and rotor makes them prone to wear over long-term operation. Ultrasonic homogenization utilizes the cavitation effect of high-frequency sound waves to break particles. It is suitable for laboratory and small-batch production. However, the local temperature in the homogenization zone can reach thousands of degrees instantaneously, which can easily cause localized protein denaturation and off-odors. Moreover, in high-viscosity colloids, sound waves decay rapidly, and the homogenization effect decreases sharply with depth, making it difficult to guarantee the uniformity of the system.
[0041] With the continuous development of bioseparation technology, microjet high-pressure homogenization has been increasingly applied to bioseparation processes. This method accelerates fluids to hundreds of meters per second through micron-level channels, achieving efficient homogenization and crushing of materials through high-pressure shearing, impact, and cavitation effects. It can break down material particles and agglomerates to the nanoscale. Microjet technology exhibits significant advantages in nanoscale particle preparation due to its low temperature rise and narrower, more uniform particle size distribution. However, its application in the refining of donkey-hide gelatin (Ejiao) liquid has not been systematically reported. Furthermore, when directly applying microjet high-pressure homogenization to reduce fatty substances and water-insoluble matter in Ejiao liquid, large particles may cause blockage of the microjet cavity, affecting the stability of the homogenization process. This invention, based on in-depth research on the application of microjet high-pressure homogenization technology in the refining of Ejiao liquid, proposes a combined homogenization method for Ejiao liquid, a production method for Ejiao products incorporating this combined homogenization method, and the Ejiao products produced using this method. The aim is to address the shortcomings of traditional processes and improve the quality and production efficiency of Ejiao products. The following is a detailed description of this application.
[0042] This embodiment provides a combined homogenization method for donkey-hide gelatin liquid, the method comprising: pre-treating the donkey-hide gelatin liquid to be processed to obtain a first liquid; The first adhesive solution is subjected to colloid milling to obtain the second adhesive solution; The second adhesive solution is subjected to micro-jet high-pressure homogenization and crushing treatment to obtain the third adhesive solution; This method employs a two-stage gradient crushing process. First, a colloid mill is used to perform preliminary homogenization of the gelatin solution, reducing particle size and improving particle uniformity. Then, micro-jet high-pressure homogenization technology is used to further crush the pre-crushed solution, minimizing particle size and significantly improving particle solubility, thereby effectively reducing the content of water-insoluble matter. Simultaneously, this method prevents large particles from entering the micro-jet homogenization chamber, which could potentially cause blockage and affect the stability of the micro-jet homogenization crushing process.
[0043] In this embodiment, the average particle size of the third adhesive liquid is 160-200 nm, and the viscosity is 378-423 cp. To achieve the above effects, the inventors of this application, through research and comparison of colloid mill and microjet high-pressure homogenization parameters and product quality, have developed an optimal combined crushing method for the adhesive liquid. This method achieves thorough crushing of water-insoluble substances in the donkey-hide gelatin liquid, resulting in a finer texture and significantly improved fluidity.
[0044] In some preferred embodiments, the operating conditions for the colloid milling process include: The colloid mill disc clearance is 0.5-2.5mm, the colloid mill speed is 1800-2200rpm, the colloid mill system temperature is stable at 40-60℃, and the crushing cycle is 3-5 times.
[0045] As an example, the gap between the grinding discs in a colloid mill should not be too small. The smaller the gap, the stronger the shearing force, which will break the collagen molecules in the donkey-hide gelatin and cause the temperature to rise rapidly. Donkey-hide gelatin has high viscosity and is easy to gel. If the gap is too small, the gelatin liquid will thicken instantly between the grinding discs, stick to the shaft, and become blocked, making continuous processing impossible. The grinding disc gap can be 0.5mm, 0.7mm, 1mm, 1.2mm, 1.5mm, 1.7mm, 2.0mm, 2.2mm, 2.5mm, etc., with 0.5mm being the preferred size. Excessively high-speed colloid milling of donkey-hide gelatin can easily lead to excessively high material temperature, collagen denaturation and degradation, decreased gel strength, darkening of color, and off-odors, seriously affecting the quality and molding effect of the finished product. Therefore, the rotation speed of the colloid mill is limited to 1800 rpm, 1900 rpm, 2000 rpm, 2100 rpm, 2200 rpm, etc., with 2000 rpm being the preferred speed; the temperature of the colloid mill system is preferably kept stable at 40-50℃. Insufficient cycles in a colloid mill will not achieve the desired pre-crushing effect, failing to ensure the particle size meets the requirements for entry into the ultra-high pressure microjet. However, more cycles are not necessarily better. Excessive cycles can lead to excessive shearing, a sustained increase in material temperature, resulting in collagen degradation, reduced gel strength, protein denaturation, darkening of color, and off-odors, ultimately lowering the quality of the donkey-hide gelatin. Therefore, 3, 4, or 5 cycles are recommended, with 3 cycles being the preferred option.
[0046] In some embodiments, the stator and rotor structure of the colloid mill is of the toothed type, helical type, perforated type or disc type, with the toothed type being preferred.
[0047] In some embodiments, the grinding disc of the colloid mill can be made of one or more of tungsten carbide (WC), zirconium oxide (ZrO2), 304 stainless steel, 316L stainless steel or cemented carbide, with tungsten carbide being preferred.
[0048] In some preferred embodiments, the operating conditions for the microjet high-pressure homogenization process include: The micro-jet high-pressure homogenization crushing pressure is 1500-1800 bar, the temperature is 25-60℃, and the homogenization cycle is 2-5 times.
[0049] Excessive homogenization pressure in ultra-high pressure microfluidic homogenization, such as exceeding 2000 bar, can lead to excessive collagen degradation, significantly reduced gel strength, protein denaturation, blackening of color, and off-odors due to excessive shear force and instantaneous high temperature. For example, the breaking pressure of microfluidic high pressure homogenization is 1500 bar, 1600 bar, 1700 bar, 1800 bar, etc., with 1500 bar being preferred. The preferred temperature is 25-60℃. During homogenization, the equipment is equipped with a water circulation temperature control system to maintain the equipment temperature within the above range and avoid excessive temperature. As the number of homogenization cycles of ultra-high pressure micro-jet increases, the material will be subjected to repeated strong shearing and cavitation, leading to excessive degradation of collagen in donkey-hide gelatin and a decrease in gel strength. At the same time, the material temperature will continue to rise, causing protein denaturation, darkening of color, and the generation of off-odors, which will seriously degrade the quality of donkey-hide gelatin. Therefore, the number of homogenization cycles is 2, 3, 4, 5, etc., with 3 cycles being the preferred option.
[0050] After homogenization, the adhesive solution can be collected and sampled to determine the particle size distribution (D10, D50, D90) of the broken adhesive solution, and compared with the control group.
[0051] In some preferred embodiments, pretreatment of the donkey-hide gelatin solution to be treated includes: heating and dissolving the donkey-hide gelatin solution to be treated, adjusting the temperature of the solution, controlling the temperature of the solution to 40℃~60℃, and the water content of the solution to 65%~80%, to obtain a first solution; wherein the heating and dissolving temperature is 60℃~70℃, and the dissolving time is 2h~6h.
[0052] As an example, the temperature of the adhesive solution can be 40℃, 45℃, 50℃, 55℃, 60℃, etc., preferably 50~55℃; the water content of the adhesive solution can be 65%, 70%, 75%, 80%, etc., preferably 70~75%; the heating and dissolving temperature can be 60℃, 62℃, 64℃, 66℃, 70℃, etc., preferably 62~66℃; the dissolving time can be 2h, 3h, 4h, 5h, 6h, etc., preferably 3~5h.
[0053] To compare and test the effects, the adhesive solution can be preheated to 40-60℃ and stirred evenly. The initial particle size (D10, D50, D90) can be measured as a control group, and its viscosity can be recorded using a rotational viscometer.
[0054] Thus, through the combined treatment of the above pretreatment, colloid mill and micro-jet high-pressure homogenization crushing method, and by optimizing the operating conditions of each step, the fatty substances and water-insoluble substances in the gelatin solution are fully crushed, the particle size reaches the nanoscale, the distribution is more uniform, the texture is more delicate, the fluidity is significantly improved, and the phenomenon of gelatin solution sticking to the wall is reduced, which is conducive to improving the quality of the subsequent donkey-hide gelatin product.
[0055] Therefore, another embodiment also provides a method for producing a finished donkey-hide gelatin product, the method comprising: Provide donkey-hide gelatin liquid; The donkey-hide gelatin solution was processed using the aforementioned combined homogenization method to obtain a third gelatin solution; The third gelatin solution is concentrated and dried to obtain the finished donkey-hide gelatin product.
[0056] In this embodiment of the application, the finished product of donkey-hide gelatin includes donkey-hide gelatin blocks.
[0057] In some preferred embodiments, the steps of concentrating and drying the third gelatin solution to obtain the finished donkey-hide gelatin product include: concentrating the third gelatin solution under a concentration pressure of -0.1MPa to 0.0MPa, cooling and setting it, and then air-drying it in a drying place to obtain the finished donkey-hide gelatin product with a moisture content of ≤15%.
[0058] As an example, the concentration pressure is -0.01 MPa, -0.02 MPa, -0.03 MPa, -0.04 MPa, -0.05 MPa, -0.06 MPa, -0.07 MPa, -0.08 MPa, -0.09 MPa, etc., with -0.06 MPa being preferred.
[0059] Therefore, another embodiment provides a finished product of donkey-hide gelatin, which is prepared by the aforementioned production method of the finished product of donkey-hide gelatin, wherein the water content of the finished product of donkey-hide gelatin is ≤15%, the water insoluble content of the finished product of donkey-hide gelatin is ≤1.2%, and the light transmittance radius of the finished product of donkey-hide gelatin is 600-800px.
[0060] As an example, the water content of the finished donkey-hide gelatin product is 7.0%, 10.0%, 13.0%, 15.0%, etc., preferably 13.0% to 15.0%; the water-insoluble matter content of the finished donkey-hide gelatin product is 0.1%, 0.2%, 0.3%, 0.4%, 0.5%, 0.6%, 0.7%, 0.8%, 0.9%, 1.0%, 1.1%, 1.2%, etc., preferably 0.1% to 0.4%; the light transmittance radius of the finished donkey-hide gelatin product is 600px, 700px, 800px, etc.
[0061] Therefore, based on the above settings, the combined homogenization method for donkey-hide gelatin solution, the production method for donkey-hide gelatin products, and the donkey-hide gelatin products provided in the embodiments of the present invention have many beneficial effects: This invention utilizes a combination of colloid milling and micro-jet high-pressure homogenization to break down donkey-hide gelatin solution. The average particle size of the solution decreases from approximately 800 nm to 160–200 nm, and the D90 decreases from approximately 850 nm to approximately 250 nm, representing a significant reduction in particle size compared to before breaking down. Furthermore, the solution becomes more uniform after breaking down. The processed solution has a finer texture, free of agglomerates and large particles, exhibits a stable dispersion system, and a viscosity of 378–423 cp. This significantly improves fluidity and reduces the tendency for the solution to adhere to the walls of containers, resulting in smoother and more stable processes during conveying, filtering, concentration, filling, and molding. Simultaneously, it improves the transparency and fineness of the final product.
[0062] The method described in this invention can more thoroughly remove water-insoluble matter from donkey-hide gelatin solution. The water-insoluble matter content of the finished donkey-hide gelatin product is less than 1.2%, and can even reach 0.1-0.4%.
[0063] The embodiments of the present invention have low water-insoluble matter content, smaller and more uniform particle size, and a light transmittance spot radius of 600-800px. The light transmittance spot radius is tested to be 3 times that of the original process product, and the quality improvement effect is obvious.
[0064] In this embodiment of the invention, after the gelatin liquid is crushed by a colloid mill, the D90 and average particle size decrease from approximately 850 nm to about 650 nm. This shows that the initial crushing by the colloid mill effectively reduces the particle size, resulting in a uniform distribution and the absence of particles of significantly different sizes. This minimizes agglomerates, fibers, large particles, and other insoluble substances in the gelatin liquid, ensuring that the gelatin liquid entering the microjet cavity does not clog or scratch the microjet homogenization cavity pipes, thus improving the effect and stability of further microjet homogenization crushing. Moreover, after the initial crushing by the colloid mill, the particle size of the gelatin liquid is significantly reduced and uniformly distributed, resulting in less heat generation during microjet high-pressure homogenization crushing and better preservation of the nutritional components in the gelatin liquid.
[0065] The mechanized continuous crushing process of this invention enables automated continuous operation of the colloid mill and micro-jet high-pressure homogenizer, improving overall production efficiency by more than 50%, significantly reducing labor costs and labor intensity. The mechanized crushing process eliminates subjective differences caused by manual operation, and process parameters such as temperature, pressure, and number of cycles can be precisely set and monitored in real time, ensuring a high degree of consistency in quality indicators between different batches of products.
[0066] The embodiments of this invention employ a physical crushing method, in which the colloid is circulated in a closed system, resulting in no material loss and a raw material utilization rate of nearly 100%. Both the colloid mill and the micro-jet high-pressure homogenization are carried out in closed equipment, avoiding the contamination risks that may arise from traditional open operations during manual defoaming. At the same time, the physical crushing method does not introduce any chemical additives, ensuring the natural properties and food safety of the product.
[0067] The following describes the implementation methods of this application. The implementation methods described below are exemplary and are only used to explain this application, and should not be construed as limiting this application. Where specific techniques or conditions are not specified in the implementation methods, they shall be performed in accordance with the techniques or conditions described in the literature in this field or according to the product instructions. Reagents, materials, or instruments used, unless otherwise specified, are all conventional products that can be obtained commercially.
[0068] It should be noted that the donkey-hide gelatin liquid in this invention is provided by Dong-E-E-Jiao Co., Ltd.
[0069] In this invention, the finished gelatin blocks used as the control group were produced and provided by Dong-E-E-Jiao Co., Ltd. using traditional production processes, which involve manual skimming without any homogenization.
[0070] In this invention, any instrument capable of detecting light transmittance can be used to detect the light transmittance radius of the finished gelatin blocks. For example, the NEV-TRD-10NS visual inspection and analysis instrument for gelatin blocks produced by Nawell (Changsha) Intelligent Technology Co., Ltd. can be used to detect the light transmittance radius of the finished gelatin blocks. A fixed light source is used to illuminate the gelatin blocks, which are all of the same size. The gelatin block samples are placed in the dark chamber of the testing instrument, and the placement is consistent each time to ensure that the fixed light source can pass through the center of the gelatin block. After passing through the gelatin block, the radius of the light spot is measured at a fixed position. The size of the "light spot radius" displayed directly on the screen indicates the intensity of the sample's light transmittance.
[0071] The conventional finished glue block used as a reference in this invention has a water content of 7.6%, a water-insoluble content of 0.84%, and a light transmittance radius of 239px.
[0072] Method for calculating the moisture content of donkey-hide gelatin solution: After the skin has softened, the moisture content of the solution is determined by differential weighing. Accurately weigh 2.000 g of the solution, place it in a forced-air drying oven at 105 ℃ for 4 hours, weigh it, and then place it in the forced-air drying oven to dry until constant weight. The difference between the weighing and drying times should not exceed 0.002 g. Subtract the bottle weight and record the dried weight.
[0073] Formula for calculating moisture content: Moisture content of donkey-hide gelatin solution (%) = The particle size distribution of the adhesive was detected using a laser particle size analyzer.
[0074] The water-insoluble matter content of the finished product was determined by the differential weighing method. After accurately weighing the finished product powder, 10 mL of hot water was added to dissolve it. The mixture was centrifuged at 3000 rpm for 10 min, the supernatant was removed, and then 10 mL of pure water was added and mixed well. The mixture was centrifuged again with the same parameters, the supernatant was removed, and the product was dried in an oven at 105℃ until constant weight was achieved.
[0075] Formula for calculating water-insoluble matter content: Example 1
[0076] A method for producing a finished donkey-hide gelatin product includes: (1) Take 2.0L of the gelatin solution after heating at 62℃ for 2 hours to dissolve, control the temperature of the solution at 40℃, stir evenly and measure the water content of the solution. The water content is 72.6%, and the first solution is obtained.
[0077] The initial particle size distribution of the first adhesive solution was measured, using D10, D50, D90, and average particle size as evaluation indicators. The measured particle size distribution of the first adhesive solution was 407.9 nm for D10, 597.6 nm for D50, 848.7 nm for D90, and 797.2 nm for the average particle size. The initial viscosity of the first adhesive solution was measured to be 378 cp.
[0078] (2) The colloid mill rotor is of the toothed type, and the grinding disc gap is set to 0.5 mm. Clean water is added to circulate and clean the pipeline until the water is clear and transparent. Then, the first colloid solution is added, and the circulating crushing begins. The number of cycles is set to 3. After the crushing is completed, the colloid solution is collected to obtain the second colloid solution. Using the colloid solution's D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the second colloid solution was measured to be D10 409.6 nm, D50 568.3 nm, D90 644.8 nm, and average particle size 764.9 nm. The second colloid solution was observed to be uniformly distributed with no obviously unevenly sized particles.
[0079] (3) After the micro-jet high-pressure homogenizer is turned on, water is circulated for cooling at 60℃. Clean water is added to circulate and clean the pipes. The homogenization pressure is set to 1500 bar before adding the second adhesive. The homogenization cycle is repeated 3 times. The homogenized adhesive is collected to obtain the third adhesive. The particle size distribution of the third adhesive is measured. The particle size distribution of the third adhesive is D10 117.4 nm, D50 182.1 nm, D90 266.3 nm, and the average particle size is 185.7 nm. The viscosity of the third adhesive is measured to be 400 cp using a rotational viscometer. The adhesive is observed to be uniformly distributed, with improved fluidity and reduced wall adhesion.
[0080] (4) The third gelatin solution is concentrated under vacuum at a pressure of -0.06 MPa. After cooling and setting, it is air-dried in a cool, dry place to obtain a finished donkey-hide gelatin product with a moisture content of ≤15%. Figure 1 As shown, through Figure 1 It can be seen that the particle size of the rubber block is uniformly dispersed, without large particles or agglomerates. This is in contrast to rubber blocks produced using traditional manufacturing processes. Figure 2 As shown, Figure 2 In the middle section, (1) is a glue block produced by traditional manufacturing process, and (2) is the finished glue block obtained in Example 1 of this invention. Visually, the light transmittance of the finished glue block obtained in Example 1 is significantly better than that of the glue block produced by traditional process. Figure 4 The measured radius of the transmitted light spot on the finished donkey-hide gelatin block is 650px. Figure 3 The measurement of the light-transmitting spot radius of the glue block produced by the traditional process is 239px, proving that the light-transmitting spot radius of the glue block in Example 1 is significantly higher than that of the glue block produced by the traditional process, about 3 times that of the finished product of the traditional process.
[0081] (5) After the gelatin block is dried, it is crushed into powder. 2.0013g of gelatin powder is accurately weighed and placed in a constant weight weighing bottle. It is then placed in a forced-air drying oven at 105 ℃ for 4 h. The moisture content of the gelatin block is calculated to be 8.7% using the differential weighing method. The water-insoluble matter content is determined to be 0.31%.
[0082] Comparative Example 1 The production method of this comparative example is used to demonstrate a comparative experiment involving only one colloid milling process without microfluidic high-pressure homogenization. The method includes the following steps: (1) Take 2.0L of the gelatin solution after heating at 62℃ for 2 hours to dissolve, control the temperature of the solution at 40℃, stir evenly and measure the water content of the solution. The water content is 74.4%, and the first solution is obtained.
[0083] The initial particle size distribution of the first adhesive solution was measured, using D10, D50, D90, and average particle size as evaluation indicators. The measured particle size distribution of the first adhesive solution was: D10 436.7 nm, D50 667.3 nm, D90 851.4 nm, and average particle size 792.7 nm. The initial viscosity of the adhesive solution was measured to be 389 cp.
[0084] (2) The colloid mill's stator and rotor are of the toothed type, and the grinding disc gap is set to 0.5 mm. Clean water is added to circulate and clean the pipes until the water is clear and transparent. The first colloid solution is then added, and the circulating crushing process begins. The number of cycles is set to 1. After the crushing process, the colloid solution is collected to obtain the second colloid solution. Using the colloid solution's D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the second colloid solution was measured: D10 = 420.2 nm, D50 = 643.8 nm, D90 = 799.6 nm, and the average particle size = 788.8 nm. The condition of the second colloid solution was observed to show no significant change compared to the first colloid solution. The results indicate that the effect of three colloid mill crushing cycles was not achieved, and the colloid solution cannot be used to produce finished products.
[0085] Comparative Example 2 This comparative production method is used to demonstrate a comparative experiment of micro-jet high-pressure homogenization treatment without colloid milling and only involving three cycles at 1500 bar pressure, and includes the following steps: (1) Take 2L of gelatin solution that has been dissolved by heating at 62℃ for two hours, control the temperature of the solution at 40℃, stir evenly and measure the water content of the solution. The water content is 68.4%, and the first solution is obtained.
[0086] The initial particle size distribution of the first adhesive sample was determined. Using D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the first adhesive sample was determined to be: D10 448.6 nm, D50 701.4 nm, D90 889.3 nm, and average particle size 825.6 nm. The initial viscosity of the adhesive was determined to be 374 cp.
[0087] (2) After the micro-jet high-pressure homogenizer is turned on, water is circulated for cooling, and the temperature is 60℃. Clean water is added to circulate and clean the pipeline, and the first adhesive solution is added after the homogenization pressure is set to 1500 bar. The homogenization cycle is 3 times. During the homogenization process, the pipeline was blocked 4 times, and the homogenization process had to be stopped and the micro-jet homogenizer pipeline had to be backflushed to clean it before homogenization could continue, which greatly reduced the efficiency. Compared with Example 1, the efficiency of the adhesive treatment process was greatly reduced, the service life of the instrument was shortened, and the cost of manual cleaning of the instrument was increased.
[0088] Comparative Example 3 This comparative production method is used to demonstrate a comparative experiment involving only 5 cycles of colloid milling without microfluidic high-pressure homogenization, and includes the following steps: (1) Take 2.0L of the gelatin solution after heating at 62℃ for 2 hours to dissolve, control the temperature of the solution at 40℃, stir evenly and measure the water content of the solution. The water content is 73.7%, and the first solution is obtained.
[0089] The initial particle size distribution of the first adhesive solution was measured. Using D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the first adhesive solution was measured to be: D10 438.1 nm, D50 671.4 nm, D90 855.2 nm, and average particle size 801.0 nm. The initial viscosity of the adhesive solution was measured to be 377 cp.
[0090] (2) The colloid mill's stator and rotor are of the toothed type, and the grinding disc gap is set to 0.5 mm. After starting the machine, clean water is added to circulate and clean the pipes until the water is clear and transparent. Then, the first colloid solution is added, and the circulatory crushing begins. The number of cycles is set to 5. After the crushing is completed, the colloid solution is collected to obtain the second colloid solution. Using the colloid solution's D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the second colloid solution was measured: D10 = 401.7 nm, D50 = 564.4 nm, D90 = 637.5 nm, and the average particle size is 762.3 nm. Observing the condition of the second colloid solution, it shows a uniform distribution with no obviously unevenly sized particles. The results show no significant difference compared to the colloid mill's crushing cycle of 3 times; therefore, setting the colloid mill's crushing cycle to 3 times is optimal.
[0091] Comparative Example 4 The production method of this comparative example is used to demonstrate a single comparative experiment of microjets performing high-pressure homogenization, and includes the following steps: (1) Take 2.0L of the gelatin solution after heating at 62℃ for 2 hours to dissolve, control the temperature of the solution at 40℃, stir evenly and measure the water content of the solution. The water content is 75.8%, and the first solution is obtained.
[0092] The initial particle size distribution of the first adhesive solution was measured. Using D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the first adhesive solution was measured to be: D10 441.2 nm, D50 673.5 nm, D90 857.1 nm, and average particle size 811.4 nm. The initial viscosity of the adhesive solution was measured to be 380 cp.
[0093] (2) The colloid mill rotor is of the toothed type, and the grinding disc gap is set to 0.5 mm. Clean water is added to circulate and clean the pipes until the water is clear and transparent. The first colloid solution is then added, and the circulating crushing begins. The number of cycles is set to 3. After the crushing is complete, the colloid solution is collected to obtain the second colloid solution. Using the colloid solution's D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the second colloid solution was measured: D10 = 420.0 nm, D50 = 548.2 nm, D90 = 651.0 nm, and the average particle size is 677.5 nm. The second colloid solution was observed to be uniformly distributed with no obviously unevenly sized particles.
[0094] (3) After the micro-jet high-pressure homogenizer is turned on, water circulation is introduced for cooling, and the temperature is 60℃. Clean water is added to circulate and clean the pipeline. After setting the homogenization pressure to 1500 bar, the second adhesive solution is added. The homogenization cycle is 1 time. The homogenized adhesive solution is collected to obtain the third adhesive solution. The particle size distribution of the third adhesive solution is measured. The particle size distribution of the third adhesive solution is D10 320.6 nm, D50 493.9 nm, D90 551.2 nm, and the average particle size is 593.4 nm. The viscosity of the third adhesive solution is measured to be 392 cp using a rotational viscometer. The state of the third adhesive solution is observed. The third adhesive solution has poor fluidity and still has a strong wall adhesion phenomenon.
[0095] (4) The third gelatin solution was vacuum concentrated at a pressure of -0.06 MPa. After cooling and shaping, it was air-dried in a cool and dry place to obtain a finished product with a water content of ≤15%. The radius of the light-transmitting spot of the finished gelatin block was measured to be 308px, which is an improvement over the finished product of the traditional process but not significant.
[0096] (5) After the gelatin block was dried, it was crushed into powder. 2.0528g of gelatin powder was accurately weighed and placed in a constant weight weighing bottle. It was then placed in a forced-air drying oven at 105 ℃ for 4 h. The moisture content of the gelatin block was calculated to be 8.6% using the differential weighing method. The water-insoluble content was determined to be 1.12%, which is 3 to 4 times higher than that in the example.
[0097] Comparative Example 5 This comparative production method is used to demonstrate a five-cycle comparative experiment of microjets undergoing high-pressure homogenization, and includes the following steps: (1) Take 2.0L of the gelatin solution after heating at 62℃ for 2 hours to dissolve, control the temperature of the solution at 40℃, stir evenly and measure the water content of the solution. The water content is 69.8%, and the first solution is obtained.
[0098] The initial particle size distribution of the first adhesive solution was measured. Using D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the first adhesive solution was measured to be: D10 438.1 nm, D50 671.4 nm, D90 855.2 nm, and average particle size 801.0 nm. The initial viscosity of the adhesive solution was measured to be 377 cp.
[0099] (2) The colloid mill rotor is of the toothed type, and the grinding disc gap is set to 0.5 mm. Clean water is added to circulate and clean the pipes until the water is clear and transparent. The first colloid solution is then added, and the circulating crushing begins. The number of cycles is set to 3. After the colloid solution is finished, it is collected to obtain the second colloid solution. Using the colloid solution's D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the second colloid solution was measured: D10 = 418.2 nm, D50 = 559.3 nm, D90 = 643.0 nm, and the average particle size is 684.3 nm. The condition of the second colloid solution was observed; it showed a uniform distribution with no obviously unevenly sized particles.
[0100] (3) After the micro-jet high-pressure homogenizer is turned on, water is circulated for cooling at 60℃. Clean water is added to circulate and clean the pipes. The homogenization pressure is set to 1500 bar before adding the second adhesive. The homogenization cycle is 5 times. The homogenized adhesive is collected to obtain the third adhesive. The particle size distribution of the third adhesive is measured. The particle size distribution of the third adhesive is D10 114.6 nm, D50 174.6 nm, D90 249.6 nm, and the average particle size is 180.1 nm. The viscosity of the third adhesive is measured to be 402 cp using a rotational viscometer. The third adhesive is observed to be uniformly distributed, with improved fluidity and reduced wall adhesion. The homogenization cycle is 5 times. The particle size and dispersion effect are slightly improved compared to 3 cycles, but not significantly. Therefore, 3 cycles of micro-jet high-pressure homogenization are optimal.
[0101] (4) The third gelatin solution was vacuum concentrated at a pressure of -0.06 MPa. After cooling and shaping, it was air-dried in a cool and dry place to obtain a finished product with a water content of ≤15%. The radius of the light-transmitting spot of the finished gelatin block was measured to be 665px, which is 3 times that of the finished product made by traditional process.
[0102] (5) After the gelatin block is dried, it is crushed into powder. 2.1107g of gelatin powder is accurately weighed and placed in a constant weight weighing bottle. It is then placed in a forced-air drying oven at 105 ℃ for 4 h. The moisture content of the gelatin block is calculated to be 8.3% using the differential weighing method. The water-insoluble content is determined to be 0.28%.
[0103] Example 2
[0104] A method for producing a finished donkey-hide gelatin product includes: (1) Take 2.0L of the gelatin solution after heating at 65℃ for 3 hours to dissolve, control the temperature of the solution at 45℃, stir evenly and measure the water content of the solution. The water content is 74.7%, and the first solution is obtained.
[0105] The initial particle size distribution of the first adhesive solution was measured. Using D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the first adhesive solution was measured to be: D10 433.4 nm, D50 665.3 nm, D90 861.7 nm, and average particle size 806.4 nm. The initial viscosity of the first adhesive solution was measured to be 702 cp.
[0106] (2) The colloid mill rotor is of the toothed type, and the grinding disc gap is set to 0.5 mm. Clean water is added to circulate and clean the pipes until the water is clear and transparent. The first colloid solution is then added, and the circulating crushing begins. The number of cycles is set to 3. After the crushing is complete, the colloid solution is collected to obtain the second colloid solution. Using the colloid solution's D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the second colloid solution was measured: D10 = 409.7 nm, D50 = 557.0 nm, D90 = 651.2 nm, and the average particle size is 667.6 nm. The second colloid solution was observed to be uniformly distributed with no obviously unevenly sized particles.
[0107] (3) After the micro-jet high-pressure homogenizer is turned on, water is circulated for cooling at 60℃. Clean water is added to circulate and clean the pipes. The homogenization pressure is set to 1600 bar before adding the second adhesive. The homogenization cycle is repeated 3 times. The homogenized adhesive is collected to obtain the third adhesive. The particle size distribution of the third adhesive is measured. The particle size distribution of the third adhesive is D10 117.2 nm, D50 165.3 nm, D90 255.6 nm, and the average particle size is 183.0 nm. The viscosity of the third adhesive is measured to be 400 cp using a rotational viscometer. The third adhesive is observed to be uniformly distributed, with improved fluidity and reduced wall adhesion.
[0108] (4) The third gelatin solution is vacuum concentrated at a pressure of -0.06 MPa, cooled and shaped, and then air-dried in a cool, dry place to obtain a finished product of donkey-hide gelatin with a moisture content of ≤15%. A comparison is made with gelatin blocks produced using traditional methods, such as... Figure 2 As shown, Figure 2 Block (1) is a rubber block produced by traditional manufacturing process, and block (3) is the finished rubber block obtained in Example 2 of this invention. Visually, the light transmittance of the finished rubber block obtained in Example 2 is significantly better than that of the rubber block produced by traditional process. Figure 5 The measured radius of the transmitted light spot on the finished donkey-hide gelatin block is 647px. Figure 3 The measurement of the light-transmitting spot radius of the glue block produced by the traditional process is 239px, proving that the light-transmitting spot radius of the glue block in Example 2 is significantly higher than that of the glue block produced by the traditional process, about 3 times that of the finished product of the traditional process.
[0109] (5) After the gelatin block was dried, it was crushed into powder. 2.0528g of gelatin powder was accurately weighed and placed in a constant weight weighing bottle. It was then placed in a forced-air drying oven at 105 ℃ for 4 h. The moisture content of the gelatin block was calculated to be 7.9% using the differential weighing method. The water-insoluble content was determined to be 0.37%.
[0110] Example 3
[0111] A method for producing a finished donkey-hide gelatin product includes: (1) Take 2.0L of the gelatin solution after heating at 67℃ for 4 hours to dissolve, control the temperature of the solution at 50℃, stir evenly and measure the water content of the solution. The water content is 75.2%, and the first solution is obtained.
[0112] The initial particle size distribution of the adhesive solution was measured, using D10, D50, D90, and average particle size as evaluation indicators. The particle size distribution of the first adhesive solution was measured to be D10 427.8 nm, D50 665.2 nm, D90 838.4 nm, and average particle size 805.2 nm. The initial viscosity of the adhesive solution was measured to be 378 cp.
[0113] (2) The colloid mill rotor is of the toothed type, and the grinding disc gap is set to 0.5 mm. Clean water is added to circulate and clean the pipeline until the water is clear and transparent. The first colloid solution is then added, and the circulating crushing begins. The number of cycles is set to 3. After the crushing is complete, the colloid solution is collected to obtain the second colloid solution. Using the colloid solution's D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the second colloid solution was measured: D10 = 420.8 nm, D50 = 551.3 nm, D90 = 642.4 nm, and the average particle size = 661.5 nm. The condition of the second colloid solution was observed, showing uniform distribution.
[0114] (3) After the micro-jet high-pressure homogenizer is turned on, water is circulated for cooling at 60℃. Clean water is added to circulate and clean the pipes. The homogenization pressure is set to 1800 bar before adding the second adhesive. The homogenization cycle is repeated 3 times. The homogenized adhesive is collected to obtain the third adhesive. The particle size distribution of the third adhesive is measured. The particle size distribution of the third adhesive is D10 119.0 nm, D50 155.6 nm, D90 251.2 nm, and the average particle size is 179.6 nm. The viscosity of the third adhesive is measured to be 403 cp using a rotational viscometer. The third adhesive is observed to be uniformly distributed, with improved fluidity and reduced wall adhesion.
[0115] (4) The third gelatin solution is vacuum concentrated at a pressure of -0.06 MPa. After cooling and shaping, it is air-dried in a cool and dry place to obtain a finished product of donkey-hide gelatin with a water content of ≤15%. The radius of the light-transmitting spot of the finished product of donkey-hide gelatin is measured to be 715px, which is about 3 times that of the finished product of traditional process.
[0116] (5) After the gelatin block is dried, it is crushed into powder. 2.0013g of gelatin powder is accurately weighed and placed in a constant weight weighing bottle. It is then placed in a forced-air drying oven at 105 ℃ for 4 h. The moisture content of the gelatin block is calculated to be 7.4% using the differential weighing method. The water-insoluble content is determined to be 0.41%.
[0117] Example 4
[0118] A method for producing a finished donkey-hide gelatin product includes: (1) Take 2.0L of the gelatin solution after heating at 70℃ for 5 hours to dissolve, control the temperature of the solution at 55℃, stir evenly and measure the water content of the solution. The water content is 72.8%, and the first solution is obtained.
[0119] The initial particle size distribution of the first adhesive solution was measured. Using D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the first adhesive solution was measured to be: D10 422.9 nm, D50 670.3 nm, D90 851.2 nm, and average particle size 810.3 nm. The initial viscosity of the adhesive solution was measured to be 378 cp.
[0120] (2) The colloid mill rotor is of the toothed type, and the grinding disc gap is set to 0.5 mm. Clean water is added to circulate and clean the pipeline until the water is clear and transparent. Then, the first colloid solution is added, and the circulating crushing begins. The number of cycles is set to 5. After the cycle, the colloid solution is collected to obtain the second colloid solution. Using the colloid solution's D10, D50, D90, and average particle size as evaluation indicators, the particle size distribution of the second colloid solution was measured: D10 = 408.5 nm, D50 = 560.3 nm, D90 = 653.2 nm, and the average particle size is 659.3 nm. Observation of the second colloid solution shows a uniform distribution with no obviously unevenly sized particles.
[0121] (3) After the micro-jet high-pressure homogenizer is turned on, water circulation is introduced for cooling, and the temperature is 60℃. Clean water is added to circulate and clean the pipeline. After setting the homogenization pressure to 1800 bar, the second adhesive solution is added. The homogenization cycle is 3 times. The homogenized adhesive solution is collected to obtain the third adhesive solution. The particle size distribution of the third adhesive solution is measured. The particle size distribution of the third adhesive solution is D10 108.2 nm, D50 137.9 nm, D90 246.3 nm, and the average particle size is 176.5 nm. The viscosity of the third adhesive solution is measured to be 403 cp using a rotational viscometer. The third adhesive solution is observed to be uniformly distributed, with improved fluidity and reduced wall adhesion. The particle size does not change significantly with the increase of homogenization pressure.
[0122] (4) The third gelatin solution is vacuum concentrated at a pressure of -0.06 MPa. After cooling and shaping, it is air-dried in a cool and dry place to obtain a finished product of donkey-hide gelatin with a water content of ≤15%. The radius of the light-transmitting spot of the finished product of donkey-hide gelatin is measured to be 768px, which is more than 3 times that of the finished product of traditional process.
[0123] (5) After the gelatin block is dried, it is crushed into powder. 2.117g of gelatin powder is accurately weighed and placed in a constant weight weighing bottle. It is then placed in a forced-air drying oven at 105 ℃ for 4 h. The moisture content of the gelatin block is calculated to be 8.3% using the differential weighing method. The water-insoluble content is determined to be 0.37%.
[0124] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them; although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features; and these modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A combined homogenization method for donkey-hide gelatin liquid, characterized in that, The method includes: The gelatinous liquid to be processed is pretreated to obtain the first gelatinous liquid; The first adhesive solution is subjected to colloid milling to obtain the second adhesive solution; The second adhesive solution is subjected to micro-jet high-pressure homogenization and crushing treatment to obtain the third adhesive solution; The third adhesive has an average particle size of 160-200 nm and a viscosity of 378-423 cp. The colloid mill disc clearance is 0.5-2.5 mm, and / or the colloid mill speed is 1800~2200 rpm, and / or the temperature is stable at 40~60℃, and / or the number of crushing cycles is 3-5. The microjet high-pressure homogenizing crushing pressure is 1500-1800 bar, and / or the temperature is 25-60℃, and / or the number of homogenization cycles is 2-5.
2. The method according to claim 1, characterized in that, The pretreatment includes: heating and dissolving the gelatin liquid to be treated, adjusting the temperature of the liquid, controlling the temperature of the liquid to 40℃~60℃, and the water content of the liquid to 65%~80%, to obtain the first liquid. The heating and dissolving temperature is 60℃~70℃, and the dissolving time is 2h~6h.
3. The method according to claim 1, characterized in that, The grinding disc gap is set to 0.5 mm, and / or the number of crushing cycles is 3.
4. The method according to claim 1, characterized in that, The microjet high-pressure homogenization crushing pressure is 1500 bar, and / or the homogenization cycle is 3 times.
5. A method for producing a finished donkey-hide gelatin product, characterized in that, include: Provide donkey-hide gelatin liquid; The donkey-hide gelatin solution is processed using the combined homogenization method described in any one of claims 1 to 4 to obtain a third gelatin solution; The third gelatin solution is concentrated and dried to obtain the finished donkey-hide gelatin product.
6. The method for producing the finished donkey-hide gelatin product according to claim 5, characterized in that, The concentration pressure is -0.1 MPa to 0.0 MPa; And / or, the moisture content of the dried product is ≤15%; And / or, the drying method includes air drying.
7. The method for producing the finished donkey-hide gelatin product according to claim 6, characterized in that, The concentration pressure is -0.06 MPa, and / or the moisture content of the dried donkey-hide gelatin product is ≤15%.
8. A finished donkey-hide gelatin product, characterized in that, The product is prepared by the production method of the donkey-hide gelatin product according to any one of claims 5 to 7, wherein the water content of the donkey-hide gelatin product is ≤15% and the water-insoluble matter content is ≤1.2%.