AI Technical Summary
[0008]有鉴于此,本发明提供了一种制备锗晶体的复合坩埚及其使用方法,以解决现有坩埚难以兼顾高纯熔体隔离与低成本制造、内胆不可独立更换、涂层易开裂剥落、内胆易发生开裂、卡死、上浮或装配偏心,以及籽晶区热接触不稳定导致晶体取向继承差的问题
1、本发明所述复合坩埚包括外支撑坩埚、内胆、籽晶定位座、限位防浮结构、导热耦合结构和防泄漏结构,其中,外支撑坩埚仅负责机械承载与热传导,可重复使用;熔融锗仅与可更换的内胆接触,从根本上阻断了外支撑坩埚引入硅、碳、硼、氧等杂质的路径。而且当复合坩埚的内胆发生局部损伤时,只需要单独更换内胆,无需整体报废外支撑坩埚,因此明显降低了大尺寸坩埚的使用成本和维护周期。
Smart Images

Figure CN122833714A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of semiconductor crystal preparation technology, and in particular to a composite crucible for preparing germanium crystals and its method of use. Background Technology
[0002] Germanium crystals possess a wide infrared transmission band, high carrier mobility, and excellent radiation response characteristics, making them a core fundamental material in fields such as infrared optical windows, semiconductor devices, space multi-junction solar cell substrates, and high-purity germanium detectors. Using directional solidification techniques such as casting, vertical gradient solidification (VGF), and the Bridgman process, germanium crystals with large cross-sectional dimensions can be prepared by controlling the temperature gradient of the melt within the crucible and the propagation process of the solid-liquid interface. In these methods, the crucible directly determines the cleanliness of the melt interface, heat flux distribution, seed crystal stability, the difficulty of crystal extraction, and equipment operating costs, making it a critical component of the entire growth system.
[0003] Existing technologies commonly use quartz, graphite, high-purity silicon, boron nitride (BN), or pyrolytic boron nitride (PBN) crucibles. However, quartz crucibles are prone to wetting and adhesion to the molten germanium at high temperatures, and pose an oxygen contamination problem. When graphite crucibles are in direct contact with molten germanium, they face the risk of impurities such as carbon, boron, and ash migrating into the melt. Although high-purity silicon crucibles provide good thermal conductivity and mechanical support, they can still introduce silicon impurities into the molten germanium under prolonged high-temperature contact. Integral PBN crucibles have excellent chemical inertness and are almost not wetted by the molten germanium; however, large-size manufacturing costs are extremely high, the thin-walled structure has limited mechanical strength, and once local damage occurs, the entire crucible usually needs to be scrapped, resulting in poor maintainability.
[0004] To balance purity and cost, another approach involves preparing barrier coatings such as PBN, BN, AlN, or SiC on the inner wall of high-purity silicon, graphite, or ceramic crucibles. These coatings are firmly bonded to the substrate, making them highly susceptible to defects such as pinholes, cracks, localized peeling, or interfacial debonding during repeated heating, cooling, loading, and crystal removal. Once the germanium melt penetrates through these defects and contacts the external crucible material, the introduction of impurities and harmful interfacial reactions remain difficult to avoid. Furthermore, increasing the coating thickness to enhance coverage often introduces significant residual stress due to the mismatch in thermal expansion coefficients between the coating and the substrate, further exacerbating the risk of coating failure.
[0005] In addition, existing technologies employ a combination structure of a thin-walled inner liner and an outer supporting crucible to achieve a balance between cost and purity. However, this structure still faces several engineering challenges in practical applications: the thin-walled inner liner may float, shift, or even become suspended at the bottom during heating and melting due to density differences or melt buoyancy; the outer crucible and inner liner have different coefficients of thermal expansion, and if the assembly gap is too small, the inner liner is prone to cracking due to compression or jamming after cooling; if the gap is too large, the bottom thermal contact state is unstable, seriously affecting the temperature gradient and solid-liquid interface morphology of the seed crystal area. Existing structures often only focus on isolating melt contamination, but fail to simultaneously address the integrated requirements of replaceability, thermal expansion compensation, precise seed crystal positioning, anti-floating restraint, and bottom thermal coupling.
[0006] In summary, existing crucible solutions for preparing germanium crystals still have significant shortcomings in the following aspects: When the outer crucible is in direct or indirect contact with the germanium melt, it is difficult to completely avoid the introduction of impurities such as oxygen, silicon, carbon, and boron, making it impossible to achieve a good balance between high purity and low cost; integral PBN or BN crucibles are not only expensive and have limited resistance to mechanical impact, but also cannot individually replace the parts in contact with the melt after local damage; the fixed barrier coating is prone to pinholes, cracks, and peeling under thermal cycling and mechanical operation, and is difficult to repair or replace on-site after failure; the inner liner is prone to cracking, jamming, floating, or assembly misalignment; the instability of the bottom thermal resistance and contact state of the seed crystal area will directly cause local temperature gradient fluctuations, thereby interfering with the limited melting control of the seed crystal, the maintenance of interface morphology, and the inheritance of crystal orientation.
[0007] Therefore, there is an urgent need to provide a composite crucible and its usage method that takes into account both high-purity melt isolation and low-cost manufacturing, has a replaceable inner liner and thermal expansion compensation capability, and can stably maintain the temperature gradient of the seed crystal region and the inheritance of crystal orientation. Summary of the Invention
[0008] In view of this, the present invention provides a composite crucible for preparing germanium crystals and a method for using it, in order to solve the problems of existing crucibles, such as difficulty in achieving both high-purity melt isolation and low-cost manufacturing, inability to independently replace the inner liner, easy cracking and peeling of the coating, easy cracking, jamming, floating or assembly misalignment of the inner liner, and poor crystal orientation inheritance due to unstable thermal contact in the seed crystal area.
[0009] To achieve the above objectives, the present invention adopts the following technical solution: This invention provides a composite crucible for preparing germanium crystals, comprising an outer support crucible, an inner liner, a seed crystal positioning seat, a limiting and anti-floating structure, a thermally conductive coupling structure, and a leakage-proof structure; The inner liner is disposed inside the outer supporting crucible; The seed crystal positioning seat is located at the bottom of the inner liner and is used to fix the germanium single crystal seed crystal. The limiting and anti-floating structure is located at the top of the inner liner; The thermally conductive coupling structure is disposed between the bottom of the outer supporting crucible and the bottom of the inner liner; The leak-proof structure is located on the bottom outer side of the inner liner; A number of positioning protrusions, flexible pads or limiting ribs are provided between the outer surface of the inner liner and the inner wall of the outer support crucible to form a thermal expansion compensation gap. The thermal expansion compensation gap is used to allow the inner liner and the outer support crucible to undergo relative thermal expansion when the temperature changes. The gap width of the thermal expansion compensation gap is 0.1~1.0 mm.
[0010] Preferably, the material of the external support crucible includes high-purity silicon, high-purity graphite, silicon carbide, silicon carbide coated graphite, aluminum nitride, or boron nitride.
[0011] Preferably, the inner liner is detachably installed inside the outer support crucible; the material of the inner liner includes PBN, BN, PBN-BN composite material, or a layered material with PBN as the melt contact layer and BN as the structural support layer; the thickness of the inner liner is 0.5~3.0 mm.
[0012] Preferably, the seed crystal positioning seat includes a flat base, a conical base, a spherical crown-shaped base, an arc transition base, or a stepped base; the material of the seed crystal positioning seat includes PBN, BN, PBN-BN composite material, SiC, AlN, or SiC or AlN material with a PBN-BN layer on the surface; the depth of the seed crystal positioning seat is 2~15 mm.
[0013] Preferably, the limiting and anti-floating structure includes one or more of the following: an upper pressure cap, an annular pressure plate, a split retaining ring, an outward-flared limiting step, a positioning pin, a positioning pin hole, a wedge-shaped pressure block, a threaded pressure sleeve, and a ceramic locking nut; the limiting and anti-floating structure is connected to the upper end of the outer support crucible by pressing, snapping, embedding, pinning, or threaded locking, and cooperates with the outward-flared edge or upper edge step of the inner liner to limit the axial upward floating, circumferential rotation, and radial displacement of the inner liner; the material of the limiting and anti-floating structure includes PBN, BN, silicon carbide, or high-purity graphite; and the contact part between the limiting and anti-floating structure and the inner liner is provided with rounded corners, bevels, PBN isolation plates, BN isolation plates, or flexible graphite isolation plates.
[0014] Preferably, the thermally conductive coupling structure is detachably installed between the bottom outer side of the inner liner and the bottom inner side of the outer support crucible; the thermally conductive coupling structure includes one or more of flexible graphite sheets, graphite paper, PBN sheets, BN sheets and silicon carbide gaskets.
[0015] Preferably, the leak-proof structure includes an isolation tray, an annular collection tank, or a bottom receiving plate; the material of the leak-proof structure includes one of PBN, BN, SiC, and high-purity graphite with a PBN or BN layer on the surface.
[0016] The present invention also provides a method for using the above-mentioned composite crucible for preparing germanium crystals, comprising the following steps: Assemble the composite crucible and place the germanium single crystal seed in the seed positioning seat. Fill the top of the germanium single crystal seed with high-purity germanium. Then place the composite crucible in the furnace for heating. When the high-purity germanium melts and the remaining height of the germanium single crystal seed after melting is 3~12 mm, control the solid-liquid interface to advance from the top of the germanium single crystal seed to the top for directional solidification growth by adjusting the power of the upper and lower heating zones in the furnace, the heat dissipation intensity at the bottom, the crucible pulling speed, and the temperature zone moving speed. After the directional solidification growth is completed, perform medium-temperature annealing and cooling in sequence to obtain the germanium crystal.
[0017] Preferably, the height of the germanium single crystal seed is 10~30 mm; the filling height of the high-purity germanium is 60~75% of the effective height of the inner liner; and the purity of the high-purity germanium is ≥6N.
[0018] Preferably, the heating temperature is 960~980℃, and the atmosphere is an inert atmosphere.
[0019] Preferably, the solidification interface propagation rate of the directional solidification growth is 0.01~0.08 mm / min; during the directional solidification growth process, the axial temperature gradient inside the inner liner is 1~10 K / cm.
[0020] Preferably, the temperature of the medium-temperature annealing is 350~550℃, and the time is 1~6 h.
[0021] As can be seen from the above technical solution, compared with the prior art, the beneficial effects of the present invention are as follows: 1. The composite crucible of this invention includes an outer support crucible, an inner liner, a seed crystal positioning seat, a limiting and anti-floating structure, a thermally conductive coupling structure, and a leakage-proof structure. The outer support crucible is only responsible for mechanical load-bearing and heat conduction and is reusable. The molten germanium only contacts the replaceable inner liner, fundamentally blocking the pathway for impurities such as silicon, carbon, boron, and oxygen to be introduced from the outer support crucible. Furthermore, when the inner liner of the composite crucible suffers localized damage, only the inner liner needs to be replaced, eliminating the need to scrap the entire outer support crucible. This significantly reduces the usage cost and maintenance cycle of large-size crucibles.
[0022] 2. The radial thermal expansion compensation gap between the inner liner and the outer support crucible in the composite crucible of the present invention can effectively absorb the dimensional differences caused by the mismatch of material thermal expansion during the heating and cooling process, reduce the compressive stress on the thin-walled inner liner, thereby avoiding cracking or jamming after cooling, and improving the service reliability of the inner liner.
[0023] 3. The limiting and anti-floating structure in the composite crucible of the present invention can limit the axial upward floating and assembly offset of the inner liner. Together with the seed crystal positioning seat, it can ensure the accurate and stable position of the germanium single crystal seed, the inner liner and the high-purity germanium loading system throughout the process, effectively suppress the drift of the germanium single crystal seed, and provide mechanical guarantee for the accurate inheritance of crystal orientation.
[0024] 4. The bottom thermally conductive coupling structure in the composite crucible of the present invention can compensate for assembly errors and adjust the contact thermal resistance of germanium single crystal seed crystal, making the thermal boundary conditions more controllable. This is beneficial to achieve limited melting and controlled directional solidification of germanium single crystal seed crystal, allowing the solid-liquid interface to steadily advance upward from the germanium single crystal seed crystal, thereby significantly improving the crystal orientation inheritance and crystal integrity.
[0025] 5. Compared with the fixed barrier coating solution, the composite crucible of the present invention completely avoids the hidden pollution risks caused by coating pinholes, cracks or peeling; the detachable inner liner, as an independent melt contact component, facilitates visual inspection and individual replacement after crystal removal, making the process more reliable and maintenance decisions clearer.
[0026] 6. The composite crucible described in this invention can work well with VGF, Bridgman or casting directional solidification processes, and is not limited to specific furnace types or sizes, and can meet the needs of germanium single crystal preparation with different sizes and crystal orientations. Attached Figure Description
[0027] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are only embodiments of the present invention. For those skilled in the art, other drawings can be obtained based on the provided drawings without creative effort.
[0028] Figure 1 This is a schematic diagram of the composite crucible of the present invention; wherein, 1, outer support crucible; 2, inner liner; 3, seed crystal positioning seat; 4, limiting and anti-floating structure; 5, thermally conductive coupling structure; 6, anti-leakage structure; 7, thermal expansion compensation gap; 8, germanium single crystal seed crystal; 9, high-purity germanium. Detailed Implementation
[0029] like Figure 1 As shown, the present invention provides a composite crucible for preparing germanium crystals, including an outer support crucible, an inner liner, a seed crystal positioning seat, a limiting and anti-floating structure, a thermally conductive coupling structure, and a leakage-proof structure; The inner liner is disposed inside the outer supporting crucible; The seed crystal positioning seat is located at the bottom of the inner liner and is used to fix the germanium single crystal seed crystal. The limiting and anti-floating structure is located at the top of the inner liner; The thermally conductive coupling structure is disposed between the bottom of the outer supporting crucible and the bottom of the inner liner; The leak-proof structure is located on the bottom outer side of the inner liner; Several positioning protrusions, flexible pads, or limiting ribs are provided between the outer surface of the inner liner and the inner wall of the outer support crucible to form a thermal expansion compensation gap. The thermal expansion compensation gap is used to allow the inner liner and the outer support crucible to undergo relative thermal expansion when the temperature changes (heating, heat preservation, and cooling), while avoiding excessive eccentricity or shaking of the inner liner. The gap width of the thermal expansion compensation gap is 0.1~1.0 mm, preferably 0.2~0.8 mm, more preferably 0.3~0.6 mm, and even more preferably 0.5 mm.
[0030] In this invention, the material of the external support crucible preferably includes high-purity silicon, high-purity graphite, silicon carbide, silicon carbide coated graphite, aluminum nitride, or boron nitride.
[0031] In this invention, the cross-sectional shape of the outer support crucible preferably includes a cylindrical, square, polygonal, or irregularly shaped structure adapted to the cross-section of the target ingot. Its main functions are to provide mechanical support, transfer heat, define the shape of the inner liner, and bear the weight of the loading material and the crystal. In addition, the inner surface of the outer support crucible does not directly contact the germanium raw material, molten germanium, or grown crystal.
[0032] In this invention, when the material of the outer support crucible is high-purity silicon, the purity of the high-purity silicon is preferably ≥6N; when the material of the outer support crucible is graphite, the graphite is preferably purified at high temperature and the ash and boron content is controlled; when the material of the outer support crucible is SiC-coated graphite, the outer surface coating of the SiC-coated graphite is used to improve corrosion resistance and particle control capabilities, but does not replace the melt isolation function of the replaceable inner liner.
[0033] In this invention, the inner wall of the outer support crucible is preferably provided with positioning marks, temperature sensing holes or observation slots for monitoring the inner liner offset and / or temperature.
[0034] In this invention, the inner liner is detachably installed inside the outer support crucible; the material of the inner liner preferably includes PBN, BN, PBN-BN composite material, or a layered material with PBN as the melt contact layer and BN as the structural support layer; the thickness of the inner liner is 0.5~3.0 mm, preferably 0.8~2.8 mm, more preferably 1.0~2.5 mm, and even more preferably 1.5~2.0 mm.
[0035] In this invention, the inner surface of the inner liner can directly contact the germanium raw material, molten germanium, and the growing germanium crystal. The inner liner is preferably able to be pulled out as a whole, disassembled in sections, or extracted by flipping the top edge. For large-size or high-load crucibles, local reinforcing ribs, flanging, or thickness gradient zones can be added without affecting the thermal response.
[0036] In this invention, the seed crystal positioning seat preferably includes a flat base, a conical base, a spherical crown-shaped base, an arc transition base, or a stepped base; the seed crystal positioning seat is an independent positioning component disposed on the inner side of the bottom of the inner liner, and it is fixed to the bottom of the inner liner by mechanical limiting; the material of the seed crystal positioning seat includes PBN, BN, PBN-BN composite material, SiC, AlN, or SiC or AlN material with a PBN-BN layer on the surface, preferably PBN or dense BN; the depth of the seed crystal positioning seat is 2~15 mm, preferably 3~13 mm, more preferably 4~11 mm, and more preferably 5~10 mm.
[0037] In this invention, the seed crystal positioning seat does not contain metal binder, has an opening porosity of ≤1%, and a purity of ≥99.9%, more preferably ≥99.99%.
[0038] In this invention, the size of the seed crystal positioning seat is adapted to the germanium single crystal seed crystal, so that the germanium single crystal seed crystal maintains its central position and predetermined crystal orientation during the processes of loading, vacuuming, gas filling, heating and melting.
[0039] In this invention, the cross-sectional dimension of the positioning recess in the seed crystal positioning seat is preferably larger than the cross-sectional dimension of the germanium single crystal seed crystal, forming a lateral assembly gap of 0.05~1.00 mm, preferably 0.10~0.50 mm; the lateral assembly gap is used to compensate for the difference in thermal expansion between the germanium single crystal seed crystal and the seed crystal positioning seat during the heating process, and allows molten germanium to fill, thereby improving the continuity of wetting contact between the seed crystal and the melt.
[0040] In this invention, the limiting and anti-floating structure includes one or more of the following: an upper pressure cap, an annular pressure plate, a split retaining ring, an outward-flared limiting step, a positioning pin, a positioning pin hole, a wedge-shaped pressure block, a threaded pressure sleeve, and a ceramic locking nut. The limiting and anti-floating structure is connected to the upper end of the outer support crucible by pressing, snapping, embedding, pinning, or threaded locking, and cooperates with the outward-flared edge or upper edge step of the inner liner to limit the axial upward floating, circumferential rotation, and radial displacement of the inner liner. The material of the limiting and anti-floating structure preferably includes PBN, BN, silicon carbide, or high-purity graphite. The contact area between the limiting and anti-floating structure and the inner liner is preferably provided with rounded corners, bevels, PBN isolation plates, BN isolation plates, or flexible graphite isolation plates to avoid cracking of the thin-walled inner liner due to local point loads.
[0041] In this invention, the limiting and anti-floating structure is preferably disposed at the upper end of the outer support crucible and cooperates with the top of the inner liner, rather than being directly fixed to the inner liner by adhesive, welding or metal fasteners; the top of the inner liner is preferably provided with an outward flange, an upper edge boss or an annular step, and the limiting and anti-floating structure is fixed to the upper end of the outer support crucible by pressing, snapping, embedding, pinning or thread locking, and limits the top of the inner liner from the axial and / or radial direction.
[0042] In this invention, the upper pressure cap or annular pressure plate is used to press down the outward flange of the top of the inner liner; the segmented retaining ring is embedded in the annular retaining groove at the top of the outer support crucible to prevent the inner liner from floating axially upward; the positioning pin and positioning pin hole are used to prevent the upper pressure cap, annular pressure plate or segmented retaining ring from rotating circumferentially; the wedge-shaped pressure block is used to compensate for assembly gaps and limit the radial offset of the inner liner; the threaded pressure sleeve or ceramic locking nut is threadedly connected to the upper end of the outer support crucible to provide adjustable clamping force.
[0043] In this invention, an axial clearance of 0.05 to 0.50 mm is preferably maintained between the limiting anti-floating structure and the top of the inner liner, so that the inner liner can undergo a small amount of thermal expansion displacement during the heating and cooling process.
[0044] In this invention, the limiting and anti-floating structure is also preferably used to retain the space required for the thermal expansion of the inner liner.
[0045] In this invention, the thermally conductive coupling structure is detachably installed between the bottom outer side of the inner liner and the bottom inner side of the outer support crucible; the thermally conductive coupling structure includes one or more of flexible graphite sheets, graphite paper, PBN sheets, BN sheets and silicon carbide gaskets; the thermally conductive coupling structure does not need to be permanently fixed, thereby ensuring effective heat transfer and allowing the inner liner to undergo slight thermal expansion displacement during heating and cooling, avoiding cracking of the inner liner due to thermal stress caused by rigid connection.
[0046] In this invention, the thermally conductive coupling structure preferably functions to compensate for bottom assembly errors, improve the repeatability of thermal contact in the seed crystal area, adjust the axial temperature gradient, and suppress local overmelting or incomplete melting of the seed crystal. The thermally conductive coupling structure is preferably a partitioned form with high thermal conductivity at the center and low thermal conductivity at the edges, or low thermal conductivity at the center and high thermal conductivity at the edges, in order to coordinate with the furnace thermal field to adjust the solid-liquid interface shape. For processes that require a flat interface, thermal resistance matching can be achieved by changing the material, thickness, and contact area of the thermally conductive coupling structure.
[0047] In this invention, the leak-proof structure preferably includes an isolation tray, an annular liquid collection tank, or a bottom receiving plate to reduce the risk of the molten material contacting the outer support crucible when the inner liner is damaged; the leak-proof structure is preferably made of a material that is resistant to high temperature, low in pollution, and does not easily react with molten germanium, and the material preferably includes one of PBN, BN, SiC, or high-purity graphite with a PBN or BN layer on the surface.
[0048] In this invention, the bottom of the outer support crucible is preferably provided with an installation step, a positioning groove, or a support platform. The leak-proof structure is placed at the installation position at the bottom of the outer support crucible and is installed at the bottom of the outer support crucible by means of step limiting, positioning groove embedding, snap-fit, or pressing. Under normal working conditions, a certain gap is maintained between the leak-proof structure and the bottom of the inner liner, and it does not participate in normal load-bearing. When the inner liner partially cracks or melt leakage occurs, the molten germanium first falls into the receiving area formed by the leak-proof structure, thereby preventing the molten germanium from directly contacting the outer support crucible.
[0049] The present invention also provides a method for using the above-mentioned composite crucible for preparing germanium crystals, comprising the following steps: Assemble the composite crucible and place the germanium single crystal seed in the seed positioning seat. Fill the top of the germanium single crystal seed with high-purity germanium. Then place the composite crucible in the furnace for heating. When the high-purity germanium melts and the remaining height of the germanium single crystal seed after melting is 3~12 mm, control the solid-liquid interface to advance from the top of the germanium single crystal seed to the top for directional solidification growth by adjusting the power of the upper and lower heating zones in the furnace, the heat dissipation intensity at the bottom, the crucible pulling speed, and the temperature zone moving speed. After the directional solidification growth is completed, perform medium-temperature annealing and cooling in sequence to obtain the germanium crystal.
[0050] In this invention, the height of the germanium single crystal seed is 10-30 mm, preferably 12-28 mm, more preferably 15-25 mm, and even more preferably 18-20 mm; the height of the germanium single crystal seed is preferably sufficient to withstand limited erosion; the growth surface of the germanium single crystal seed is preferably a {100} or {111} crystal plane or other crystal planes selected according to the intended use of the target crystal; the filling height of the high-purity germanium is 60-75% of the effective height of the inner liner, preferably 65-70%; after filling, at least 20% of the effective height of the inner liner should be left in the upper part of the inner liner to prevent overflow when the germanium raw material melts, thermally expands, or the melt fluctuates; the purity of the high-purity germanium is preferably ≥6N, more preferably one of 6N, 7N, 8N, and 9N.
[0051] In this invention, the effective height of the inner liner refers to the height from the upper surface of the seed crystal positioning seat or the upper surface of the germanium single crystal seed crystal to the safe liquid level at the upper edge of the inner liner.
[0052] In this invention, the furnace preferably includes a VGF furnace, a Bridgman furnace, or a directional solidification furnace.
[0053] In this invention, the remaining height of the germanium single crystal seed is preferably 5-10 mm, more preferably 6-9 mm, and even more preferably 7-8 mm, to avoid the seed crystal from completely melting through or the solid-liquid interface from separating from the positioning seat.
[0054] In this invention, the heating temperature is 960~980℃, preferably 965~975℃, and more preferably 970℃; the heating atmosphere is an inert atmosphere, and the gas in the inert atmosphere is preferably one or more of nitrogen, argon and helium.
[0055] In this invention, the solidification interface propagation rate of the directional solidification growth is 0.01~0.08 mm / min, preferably 0.02~0.07 mm / min, more preferably 0.03~0.06 mm / min, and even more preferably 0.04~0.05 mm / min; the interface propagation rate is reduced at the end of the directional solidification growth and the impurity enrichment zone is controlled; during the directional solidification growth process, the axial temperature gradient inside the inner liner is 1~10 K / cm, preferably 2~8 K / cm, more preferably 3~6 K / cm, and even more preferably 4~5 K / cm; the transverse temperature difference of the same horizontal cross section inside the inner liner is preferably ≤3 K, more preferably 1~2.5 K, and even more preferably 1.5~2 K.
[0056] In this invention, the temperature of the intermediate-temperature annealing is 350~550℃, preferably 380~520℃, more preferably 400~500℃, and even more preferably 450℃; the time of the intermediate-temperature annealing is 1~6 h, preferably 1.5~5 h, more preferably 2~4 h, and even more preferably 3 h; the intermediate-temperature annealing is used to release the thermal stress inside the germanium crystal after directional solidification, and reduce the risk of cracks and dislocation proliferation during the cooling stage.
[0057] The technical solutions provided by the present invention will be described in detail below with reference to the embodiments, but they should not be construed as limiting the scope of protection of the present invention.
[0058] Example 1
[0059] This embodiment provides a composite crucible for preparing germanium crystals by casting and its usage method: The composite crucible includes an outer support crucible, an inner liner, a seed crystal positioning seat, a limiting and anti-floating structure, a thermally conductive coupling structure, and a leakage-proof structure. The outer support crucible is made of high-purity silicon material with a purity of 6N. The outer support crucible has a cylindrical structure with an inner diameter of 100 mm, a height of 120 mm, and a bottom thickness of 10 mm. The inner liner, which is detachably installed inside the outer support crucible, is made of PBN material with a thickness of 1.0 mm. A radial thermal expansion compensation gap of 0.4 mm is formed between the outer wall of the inner liner and the inner wall of the outer support crucible. A PBN seed crystal positioning seat is set on the inner side of the bottom of the inner liner. The seed crystal positioning seat is set at the bottom of the inner liner by a stepped embedding method. The upper surface of the seed crystal positioning seat has a flat-bottomed positioning recess with a depth of 8 mm. The outer support crucible has a diameter of 0.3 mm and is used to place germanium single crystal seed crystals. The limiting and anti-floating structure includes an annular pressure plate and a segmented retaining ring. The annular pressure plate is made of PBN material, and the segmented retaining ring is made of high-purity graphite material and is embedded in the annular groove at the upper end of the outer support crucible. The annular pressure plate is pressed against the outer flange of the top of the inner liner to limit the axial upward floating and radial displacement of the inner liner. The contact part between the limiting and anti-floating structure and the inner liner is rounded to avoid cracking of the thin-walled inner liner due to local point load. The thermally conductive coupling structure is a flexible graphite sheet with a thickness of 0.3 mm, which is detachably set between the bottom of the outer support crucible and the bottom of the inner liner and is embedded in the positioning groove at the bottom of the outer support crucible. The anti-leakage structure is a PBN isolation tray, which is set on the outside of the bottom of the inner liner and maintains a 2 mm gap with the bottom of the inner liner.
[0060] In use, a germanium single crystal seed with a height of 20 mm and a {111} crystal plane is placed in the positioning recess of the seed crystal positioning seat. High-purity germanium particles with a purity of 6N are filled above the germanium single crystal seed, with a particle size of 3~20 mm, and the filling height is 65% of the effective height of the inner liner. Then, the composite crucible is placed in a VGF furnace, evacuated, and filled with high-purity argon as an inert atmosphere. The temperature is raised to 970℃ at a heating rate of 3℃ / min to melt the high-purity germanium raw material, and limited melting is controlled at the top of the germanium single crystal seed, with the remaining height of the seed crystal controlled to 7 mm. Subsequently, by adjusting the power of the upper and lower heating zones, the solid-liquid interface is advanced from the top of the germanium single crystal seed upwards. The solidification interface advancement rate is 0.04 mm / min, the axial temperature gradient is 4 K / cm, and the transverse temperature difference at the same horizontal section is 2 K. After directional solidification, the temperature was lowered to 600℃ at a rate of 0.3℃ / min, then lowered to 450℃ at a rate of 0.8℃ / min, and held at 450℃ for 3 h for medium-temperature annealing. Subsequently, the temperature was cooled to room temperature in the furnace to obtain germanium crystals.
[0061] Example 2
[0062] This embodiment provides another composite crucible for preparing germanium crystals by casting and its usage method: Unlike Example 1, in this example, the outer support crucible is made of high-purity graphite material and has undergone high-temperature purification treatment, with an ash content of less than 10 ppm. The inner diameter of the outer support crucible is 150 mm and the height is 160 mm. The inner liner is made of PBN-BN composite material, wherein the inner surface of the inner liner is a PBN melt contact layer, the outer layer is a dense BN support layer, the total thickness of the inner liner is 1.5 mm, and the radial thermal expansion compensation gap between the outer wall of the inner liner and the inner wall of the outer support crucible is 0.5 mm. The seed crystal positioning seat is made of dense BN material and is installed on the inner side of the bottom of the inner liner by means of a boss limiting method. The upper surface of the seed crystal positioning seat is provided with a conical positioning recess with a depth of 10 mm. The thickness of the cap is 0.6 mm, used to improve the centering stability of the seed crystal; the limiting and anti-floating structure includes an upper pressure cap, an annular pressure plate and a positioning pin. The upper pressure cap is made of high-purity graphite material, the annular pressure plate is made of PBN material, and the positioning pin is made of SiC material. The upper pressure cap is fixed to the upper end of the outer support crucible, the annular pressure plate is pressed against the outer flange of the inner liner, and the positioning pin cooperates with the positioning hole at the upper end of the outer support crucible to prevent the pressure cap and the annular pressure plate from rotating circumferentially; the thermal coupling structure adopts a PBN sheet and flexible graphite sheet stacked structure, wherein the PBN sheet is close to the bottom of the inner liner and the flexible graphite sheet is close to the bottom of the outer support crucible, and the total thickness of the stack is 0.6 mm; the anti-leakage structure is an annular liquid collection tank made of SiC material, which is embedded in the receiving cavity at the bottom of the outer support crucible.
[0063] In operation, a germanium single crystal seed with a height of 25 mm and a growth plane of {100} is placed in the positioning recess of the seed crystal positioning seat. High-purity germanium raw material with a purity of 7N is then filled above it, with a filling height of 70% of the effective height of the inner liner. The composite crucible is then placed in a Bridgman furnace and heated to 975°C under a high-purity argon atmosphere, causing the high-purity germanium raw material to melt from top to bottom, while controlling the remaining height of the germanium single crystal seed to be 8 mm. Subsequently, directional solidification is performed using a crucible pull-down method at a speed of 0.03 mm / min, an axial temperature gradient of 5 K / cm, and a lateral temperature difference of 3 K at the same horizontal cross-section. After directional solidification, the temperature is lowered to 600°C at a rate of 0.2°C / min, then lowered to 400°C and held for 4 hours for medium-temperature annealing. After annealing, the temperature is cooled to room temperature with the furnace to obtain the germanium crystal.
[0064] Example 3
[0065] This embodiment provides another composite crucible for preparing germanium crystals by casting and its method of use: Unlike Example 1, in this example, the outer support crucible is made of silicon carbide, with an inner diameter of 200 mm and a height of 200 mm. The inner liner is made of dense BN material with a thickness of 2.0 mm. A radial thermal expansion compensation gap of 0.6 mm is provided between the outer wall of the inner liner and the inner wall of the outer support crucible. An outward flange is provided at the top of the inner liner, and a PBN insulating sheet is provided between the lower surface of the outward flange and the top support of the outer support crucible. The seed crystal positioning seat is made of SiC material with a PBN layer on its surface, where SiC serves as the structural support and the PBN layer serves as the melt contact layer. The PBN layer has a thickness of 50 μm. The seed crystal positioning seat is installed on the inner side of the bottom of the inner liner by means of a tenon and groove fit. An arc transition positioning recess is provided on the upper surface of the seed crystal positioning seat, with a depth of 6 mm. mm; the limiting and anti-floating structure includes a threaded sleeve, an annular pressure plate, and a flexible graphite isolation sheet. The threaded sleeve is threadedly connected to the upper end of the outer support crucible. The annular pressure plate is pressed against the outer flange of the inner liner. The flexible graphite isolation sheet is placed between the annular pressure plate and the outer flange of the inner liner to avoid local stress concentration. The thermal coupling structure is a partitioned thermal pad, with a SiC pad in the central area and a BN pad in the edge area, used to adjust the thermal resistance between the center and the edge of the bottom of the inner liner. The leak-proof structure is a bottom receiving plate made of AlN material and is embedded in the bottom of the outer support crucible through a limiting block.
[0066] In use, a germanium single crystal seed with a height of 18 mm and a {111} crystal plane is placed in the positioning recess of the seed crystal positioning seat. High-purity germanium raw material with a purity of 6N is filled above the germanium single crystal seed, with a filling height of 60% of the effective height of the inner liner. Then, the composite crucible is placed in a directional solidification furnace and heated to 965℃ under a high-purity argon atmosphere to melt the germanium raw material, while controlling the remaining height of the germanium single crystal seed after melting to be 6 mm. Subsequently, directional solidification is carried out by moving the temperature zone upward, with a solid-liquid interface advancement rate of 0.02 mm / min, an axial temperature gradient of 3 K / cm, and a transverse temperature difference of 2 K in the same horizontal section. After directional solidification, the temperature is lowered to 600℃ at a rate of 0.1℃ / min, then lowered to 500℃ at a rate of 0.5℃ / min, and held at 500℃ for 2 h for medium-temperature annealing. Finally, the furnace is cooled to room temperature to obtain the germanium crystal.
[0067] Comparative Example 1
[0068] Germanium crystals were prepared using an integral PBN crucible with a non-external support composite structure, under the same conditions as in Example 1, and finally, germanium crystals were obtained.
[0069] Comparative Example 2
[0070] Germanium crystals were prepared by depositing a 300 μm PBN coating on the inner wall of a high-purity silicon crucible under the same conditions as in Example 1.
[0071] Comparative Example 3
[0072] Germanium crystals were prepared by directly loading a high-purity graphite crucible with the same preparation conditions as in Example 1, and finally obtained germanium crystals.
[0073] Comparative Example 4
[0074] The only difference between this comparative example and Example 1 is that the PBN inner liner and the graphite outer support crucible are tightly fitted together, and no radial thermal expansion compensation gap is set to prepare germanium crystals. The preparation conditions are the same as in Example 1, and germanium crystals are finally obtained.
[0075] Comparative Example 5
[0076] The only difference between this comparative example and Example 1 is that the inner liner is placed inside the outer support crucible, and no limiting or anti-floating structure is set to prepare germanium crystals. The preparation conditions are the same as in Example 1, and germanium crystals are finally obtained.
[0077] The germanium crystals obtained in Examples 1-3 and Comparative Examples 1-5 were subjected to the following tests: (1) Impurity content detection: Samples were taken from the top, middle and bottom of the germanium crystal and the contents of impurities such as Si, C, B and O were tested by GDMS; if necessary, ICP-MS or SIMS were used for verification.
[0078] (2) Crystal integrity detection: Infrared transmission imaging is used to perform overall detection of germanium crystals to observe whether there are macroscopic cracks, holes, inclusions or continuous defect bands inside the crystal.
[0079] (3) Inclusion ratio detection: Perform image analysis on infrared images or metallographic images of slices and count the inclusion area ratio; the inclusion ratio is calculated as the percentage of the inclusion area to the area of the detection section.
[0080] (4) Dislocation density detection: Selective etching of defects is performed on single crystal or quasi-single crystal regions, and the dislocation density is statistically analyzed using the EPD method.
[0081] (5) Crystal orientation inheritance test: X-ray diffraction, Laue back reflection or EBSD is used to test the crystal orientation consistency of the crystal above the seed crystal region to evaluate the seed crystal orientation inheritance effect.
[0082] Testing revealed that the Si content in the germanium crystals prepared in Examples 1-3 was all below 10 ppbw, no macroscopic cracks were observed in infrared transmission imaging, the inclusion ratio was less than 1%, and the crystals exhibited good seed crystal orientation inheritance.
[0083] In contrast, while Comparative Example 1 yielded germanium crystals with lower contamination levels, the overall PBN crucible was expensive and required complete replacement after damage. In Comparative Example 2, cracks or pinholes appeared in the fixed PBN coating after thermal cycling, leading to an increase in local Si impurities and crystal defects. In Comparative Example 3, the graphite crucible directly contacted the molten germanium, resulting in an increase in C, B, and other impurities and inclusion ratios. In Comparative Example 4, due to the lack of a thermal expansion compensation gap between the inner liner and the outer support crucible, the inner liner was subjected to radial compression during heating and cooling cycles, resulting in localized pressure cracks or cooling jamming. This altered the thermal contact state in the bottom and sidewall regions, and the resulting germanium crystal showed dark spots or localized cracks in the infrared transmission image, with an inclusion ratio higher than in Example 1. EPD detection results showed a significant increase in dislocation density in the crystal edge region. Laue back reflection or X-ray diffraction results showed that the local crystal... The stability of the seed crystal's orientation inheritance decreased. This indicates that the thermal expansion compensation gap can reduce the thermal stress of the inner liner and maintain stable thermal boundary conditions, which is beneficial to improving the integrity of the germanium crystal. In Comparative Example 5, due to the lack of a limiting and anti-floating structure, the inner liner experienced slight floating or eccentricity during the melting stage of the germanium raw material. This caused changes in the contact state between the bottom of the inner liner and the thermally conductive coupling structure, resulting in a decrease in the positioning stability of the seed crystal. In the infrared transmission image of the obtained germanium crystal, local defect areas or dark spot areas were visible at the bottom, and the inclusion ratio was higher than that in Example 1. EPD detection results showed that the dislocation density in the area above the seed crystal increased. X-ray diffraction or Laue back reflection results showed that the consistency of crystal orientation inheritance decreased. This indicates that the limiting and anti-floating structure can restrict the axial floating, radial displacement, and circumferential rotation of the inner liner during the melting and directional solidification process, thereby maintaining the stability of the seed crystal position and bottom thermal contact, and improving the orientation inheritance and integrity of the germanium crystal.
[0084] Therefore, the composite crucible structure of the present invention not only reduces the cost of using the crucible and the difficulty of maintenance, but also improves the purity, integrity and crystal orientation inheritance quality of the final germanium crystal through the synergistic effect of the inner liner isolation, thermal expansion compensation, limiting and anti-floating and bottom thermal conduction coupling.
[0085] The above description is only a preferred embodiment of the present invention. It should be noted that for those skilled in the art, several improvements and modifications can be made without departing from the principle of the present invention, and these improvements and modifications should also be considered within the scope of protection of the present invention.
Claims
1. A composite crucible for preparing germanium crystals, characterized in that, This includes an external support crucible, an inner liner, a seed crystal positioning seat, a limiting and anti-floating structure, a thermally conductive coupling structure, and a leakage prevention structure; The inner liner is disposed inside the outer supporting crucible; The seed crystal positioning seat is located at the bottom of the inner liner and is used to fix the germanium single crystal seed crystal. The limiting and anti-floating structure is located at the top of the inner liner; The thermally conductive coupling structure is disposed between the bottom of the outer supporting crucible and the bottom of the inner liner; The leak-proof structure is located on the bottom outer side of the inner liner; A number of positioning protrusions, flexible pads or limiting ribs are provided between the outer surface of the inner liner and the inner wall of the outer support crucible to form a thermal expansion compensation gap. The thermal expansion compensation gap is used to allow the inner liner and the outer support crucible to undergo relative thermal expansion when the temperature changes. The gap width of the thermal expansion compensation gap is 0.1~1.0 mm.
2. The composite crucible for preparing germanium crystals according to claim 1, characterized in that, The material of the external support crucible includes high-purity silicon, high-purity graphite, silicon carbide, silicon carbide coated graphite, aluminum nitride, or boron nitride.
3. The composite crucible for preparing germanium crystals according to claim 2, characterized in that, The inner liner is detachably installed inside the outer support crucible; The inner liner is made of PBN, BN, PBN-BN composite material or a layered material with PBN as the melt contact layer and BN as the structural support layer. The thickness of the inner liner is 0.5~3.0 mm.
4. A composite crucible for preparing germanium crystals according to any one of claims 1 to 3, characterized in that, The seed crystal positioning seat includes a flat base, a conical base, a spherical crown-shaped base, an arc transition base, or a stepped base; The seed crystal positioning seat is made of materials including PBN, BN, PBN-BN composite material, SiC, AlN, or SiC or AlN material with a PBN-BN layer on the surface. The depth of the seed crystal positioning seat is 2~15 mm.
5. The composite crucible for preparing germanium crystals according to claim 4, characterized in that, The limiting and anti-floating structure includes one or more of the following: upper pressure cover, annular pressure plate, split retaining ring, outward flange limiting step, positioning pin, positioning pin hole, wedge-shaped pressure block, threaded pressure sleeve and ceramic lock nut. The limiting and anti-floating structure is connected to the upper end of the outer support crucible by pressing, snapping, embedding, pinning or thread locking, and cooperates with the outer flange or upper edge step of the inner liner to limit the axial upward floating, circumferential rotation and radial displacement of the inner liner. The material of the limiting and anti-floating structure includes PBN, BN, silicon carbide or high-purity graphite; and the contact part between the limiting and anti-floating structure and the inner liner is provided with rounded corners, bevels, PBN isolation sheets, BN isolation sheets or flexible graphite isolation sheets.
6. The composite crucible for preparing germanium crystals according to claim 5, characterized in that, The thermally conductive coupling structure is detachably installed between the bottom outer side of the inner liner and the bottom inner side of the outer support crucible; The thermally conductive coupling structure includes one or more of the following: flexible graphite sheet, graphite paper, PBN sheet, BN sheet, and silicon carbide pad.
7. The composite crucible for preparing germanium crystals according to claim 6, characterized in that, The leak-proof structure includes an isolation tray, an annular liquid collection tank, or a bottom receiving plate; The material of the leak-proof structure includes one of PBN, BN, SiC, and high-purity graphite with a PBN or BN coating.
8. A method of using the composite crucible for preparing germanium crystals according to any one of claims 1 to 7, characterized in that, Includes the following steps: Assemble the composite crucible and place the germanium single crystal seed in the seed positioning seat. Fill the top of the germanium single crystal seed with high-purity germanium. Then place the composite crucible in the furnace for heating. When the high-purity germanium melts and the remaining height of the germanium single crystal seed after melting is 3~12 mm, control the solid-liquid interface to advance from the top of the germanium single crystal seed to the top for directional solidification growth by adjusting the power of the upper and lower heating zones in the furnace, the heat dissipation intensity at the bottom, the crucible pulling speed, and the temperature zone moving speed. After the directional solidification growth is completed, perform medium-temperature annealing and cooling in sequence to obtain the germanium crystal.
9. The method of using the composite crucible for preparing germanium crystals according to claim 8, characterized in that, The height of the germanium single crystal seed crystal is 10~30 mm; The high-purity germanium is filled to a height of 60-75% of the effective height of the inner liner; The purity of the high-purity germanium is ≥6N.
10. A method of using the composite crucible for preparing germanium crystals according to claim 9, characterized in that, The heating temperature is 960~980℃, and the atmosphere is an inert atmosphere; The solidification interface propagation rate of the directional solidification growth is 0.01~0.08 mm / min; During the directional solidification growth process, the axial temperature gradient inside the inner liner is 1~10 K / cm; The intermediate-temperature annealing temperature is 350~550℃, and the time is 1~6 h.