A mine filling body tensile strength monitoring system based on guided wave feature recognition

CN122836201BActive Publication Date: 2026-11-20BACKFILL ENGINEERING LABORATORY SHANDONG GOLD MINING TECHNOLOGY CO LTD +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202611316363.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-08-28
Publication Date
2026-11-20
Estimated Expiration
2046-08-28

Smart Images

  • Figure CN122836201B_ABST
    Figure CN122836201B_ABST
Patent Text Reader

Abstract

The present application relates to the technical fields of mine filling quality monitoring and ultrasonic guided wave detection, in particular to a mine filling tensile strength monitoring system based on guided wave characteristic identification, the present application excites wideband guided wave signals covering coexisting frequency bands of longitudinal guided wave mode and bending guided wave mode through waveguide rods embedded in the filling body, performs synchronous extrusion wavelet transform and time-frequency ridge extraction on the guided wave receiving signals to separate the longitudinal guided wave mode and the bending guided wave mode, respectively calculates the longitudinal mode group velocity value and the bending mode group velocity value, takes the ratio of the bending mode group velocity value to the longitudinal mode group velocity value as the group velocity ratio characteristic parameter, constructs a dynamic reduction coefficient changing with the shear bonding state of the cementation interface according to the group velocity ratio characteristic parameter, and multiplies the dynamic reduction coefficient by the uniaxial compressive strength of the filling body to obtain the tensile strength of the filling body, thereby reducing the monitoring error and improving the accuracy of the filling body stability evaluation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of mine backfill quality monitoring and ultrasonic guided wave detection technology, specifically to a mine backfill tensile strength monitoring system based on guided wave feature recognition. Background Technology

[0002] The tensile strength of mine backfill is one of the parameters for evaluating its stability. In engineering, guided wave or acoustic wave methods are used to monitor the uniaxial compressive strength of the backfill. The tensile strength of the backfill is then indirectly obtained by multiplying the uniaxial compressive strength by a reduction factor. The tensile strength of the backfill originates from the cementing effect between the hydration products of the cementitious material and the tailings particles. The uniaxial compressive strength of the backfill is controlled by both the cementing effect and the interlocking effect of the particle skeleton. The formation mechanisms of the two strengths are different. The ratio of tensile strength to uniaxial compressive strength changes with the curing age and the bonding state of the cementation interface. In the early stage of backfill pouring... The low amount of hydration products and weak bonding at the cementation interface result in a small ratio of tensile strength to uniaxial compressive strength. As the curing age increases, the amount of hydration products increases, the bonding at the cementation interface strengthens, and the ratio of tensile strength to uniaxial compressive strength increases. When calculating the tensile strength of backfill at different curing ages using a fixed reduction factor, the calculated results deviate from the measured values ​​of the Brazilian splitting test, making it difficult to reflect the change law of tensile strength of backfill with curing age. To solve this technical problem, we provide a monitoring system for the tensile strength of mine backfill based on guided wave feature recognition. Summary of the Invention

[0003] The purpose of this invention is to provide a monitoring system for the tensile strength of mine backfill based on guided wave feature recognition, so as to solve the problems mentioned in the background art.

[0004] To achieve the above objectives, a monitoring system for the tensile strength of mine backfill bodies based on guided wave feature recognition is provided, comprising:

[0005] The broadband guided wave excitation and acquisition unit is used to excite a broadband guided wave signal covering the frequency band where longitudinal guided wave modes and flexural guided wave modes coexist through a waveguide rod pre-embedded in the filling body, so that the longitudinal guided wave mode and flexural guided wave mode are excited at the same time, and to acquire the guided wave received signal modulated by the filling body.

[0006] The mode separation unit is used to perform synchronous squeezed wavelet transform on the guided wave received signal and extract the time-frequency ridge, separate the aliased longitudinal guided wave modes from the curved guided wave modes, and obtain the arrival time series of the longitudinal mode and the arrival time series of the curved mode.

[0007] The group velocity calculation unit is used to calculate the longitudinal mode group velocity value and the bending mode group velocity value respectively at the preset characteristic frequency within the waveguide sensitive frequency band of the filling body, based on the arrival time sequence of the longitudinal mode and the arrival time sequence of the bending mode, combined with the propagation distance of the waveguide rod.

[0008] The group velocity ratio construction unit is used to calculate the ratio of the bending mode group velocity value to the longitudinal mode group velocity value based on the longitudinal mode group velocity value and the bending mode group velocity value. This ratio is used as a group velocity ratio characteristic parameter to characterize the shear bonding state of the cementation interface between the waveguide rod and the filling body.

[0009] The tensile strength inversion unit is used to construct a dynamic reduction coefficient that varies with the shear bonding state of the cement interface based on the group velocity ratio characteristic parameter, and to invert the uniaxial compressive strength of the filling body based on the longitudinal modal group velocity value. The uniaxial compressive strength of the filling body is then corrected with the dynamic reduction coefficient to obtain the tensile strength of the filling body.

[0010] Compared with the prior art, the beneficial effects of the present invention are as follows:

[0011] This invention simultaneously excites longitudinal guided wave modes and bending guided wave modes in a waveguide rod. Utilizing the physical properties of the longitudinal guided wave modes being sensitive to the bulk elasticity of the filling material and the bending guided wave modes being sensitive to the shear-bond state of the cemented interface, the ratio of the bending mode group velocity value to the longitudinal mode group velocity value is used as a group velocity ratio characteristic parameter. This group velocity ratio eliminates the influence of excitation source fluctuations and acquisition system gain changes on the absolute value of the group velocity, allowing the group velocity ratio characteristic parameter to reflect changes in the shear-bond state of the cemented interface. Based on the group velocity ratio characteristic parameter, a dynamic reduction coefficient that changes with the shear-bond state of the cemented interface is constructed, replacing the fixed reduction coefficient used in engineering. The dynamic reduction coefficient changes with the curing age and the bonding state of the cemented interface; the reduction coefficient is smaller in the early curing stage and increases in the later curing stage, consistent with the actual change law of the ratio of the tensile strength to the uniaxial compressive strength of the filling material. This reduces the calculation error of tensile strength and improves the accuracy of the filling material stability evaluation. Attached Figure Description

[0012] Figure 1 This is an overall block diagram of the present invention. Detailed Implementation

[0013] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0014] This invention provides a monitoring system for the tensile strength of mine backfill based on guided wave feature recognition. Please refer to [link / reference]. Figure 1 As shown, it includes:

[0015] The broadband guided wave excitation and acquisition unit is used to excite a broadband guided wave signal covering the frequency band where longitudinal guided wave modes and flexural guided wave modes coexist through a waveguide rod pre-embedded in the filling body, so that the longitudinal guided wave mode and flexural guided wave mode are excited at the same time, and to acquire the guided wave received signal modulated by the filling body.

[0016] The mode separation unit is used to perform synchronous squeezed wavelet transform on the guided wave received signal and extract the time-frequency ridge, separate the aliased longitudinal guided wave modes from the curved guided wave modes, and obtain the arrival time series of the longitudinal mode and the arrival time series of the curved mode.

[0017] The group velocity calculation unit is used to calculate the longitudinal mode group velocity value and the bending mode group velocity value respectively at the preset characteristic frequency within the waveguide sensitive frequency band of the filling body, based on the arrival time sequence of the longitudinal mode and the arrival time sequence of the bending mode, combined with the propagation distance of the waveguide rod.

[0018] The group velocity ratio construction unit is used to calculate the ratio of the bending mode group velocity value to the longitudinal mode group velocity value based on the longitudinal mode group velocity value and the bending mode group velocity value. This ratio is used as a group velocity ratio characteristic parameter to characterize the shear bonding state of the cementation interface between the waveguide rod and the filling body.

[0019] The tensile strength inversion unit is used to construct a dynamic reduction coefficient that varies with the shear bonding state of the cement interface based on the group velocity ratio characteristic parameter, and to invert the uniaxial compressive strength of the filling body based on the longitudinal modal group velocity value. The uniaxial compressive strength of the filling body is then corrected with the dynamic reduction coefficient to obtain the tensile strength of the filling body.

[0020] Before determining the excitation frequency range of the broadband guided wave signal, it is necessary to first establish the waveguide dispersion equation and solve the dispersion curve under the constraint of the filling body. The purpose of this step is to theoretically determine the frequency range in which the longitudinal guided wave mode and the bending guided wave mode can be excited simultaneously and can be distinguished in the guided wave received signal, so as to avoid mode loss or mode aliasing caused by improper selection of excitation frequency.

[0021] First, obtain the material and geometric parameters of the waveguide rod. The material parameters of the waveguide rod include the waveguide rod density. Waveguide rod elastic modulus Poisson's ratio of waveguide rod The geometric parameters of the waveguide rod include the waveguide rod radius. Taking a 20mm diameter 304 stainless steel waveguide as an example, the waveguide density... Take 7930 kg / m 3 waveguide rod elastic modulus Pick Pa, waveguide rod Poisson's ratio Take 0.29, waveguide rod radius Take a depth of 0.01m and simultaneously obtain the elastic parameters of the filling material, including the density of the filling material. Elastic modulus of filling material Poisson's ratio of the filling material and the viscoelastic damping coefficient of the filling body Taking a fully cemented tailings backfill with a sand-to-cement ratio of 1:4 and a mass concentration of 72% as an example, after 28 days of curing, the density of the backfill is... Take 1800 kg / m 3 Elastic modulus of filling material Pick Pa, Poisson's ratio of the filling material Take 0.25 as the viscoelastic damping coefficient of the filling material. Pick s, determined by the elastic modulus of the waveguide rod Poisson's ratio of waveguide rod Calculate the Lamé constant of the waveguide rod and waveguide rod shear modulus The calculation formula is:

[0022] ;

[0023] Substituting the values ​​yields Pa, Pa, and The units for all values ​​are Pa, and the Lamé constant of the filling material is calculated using the same formula. and the shear modulus of the filling body Substituting the values, we get Pa, Pa, considering the viscoelastic properties of the filling material during curing, the Lamé constant and shear modulus of the filling material are modified to complex values. The complex Lamé constant of the filling material... and the complex shear modulus of the filling body The calculation formula is:

[0024] ;

[0025] in Angular frequency, in rad / s. Where f is the frequency in Hz and i is the imaginary unit, the benefit of introducing viscoelastic correction is that the solution to the guided wave dispersion equation is a complex wavenumber. The real part of the complex wavenumber corresponds to the phase velocity, and the imaginary part corresponds to the attenuation coefficient. This allows the obtained dispersion curve to simultaneously contain velocity and attenuation information, which better reflects the mechanical behavior of the infill material in the early stages of curing. The displacement field of the longitudinal guided wave mode within the waveguide rod is represented by a potential function in cylindrical coordinates, and the compression wave potential function is... and shear wave potential function Take them as follows:

[0026] ;

[0027] Where A and B are the amplitude coefficients of the waveguide rod's internal potential function. and Let be the zeroth-order and first-order Bessel functions of the first kind, respectively; k be the wavenumber in rad / m; z be the axial coordinate of the waveguide rod in meters; t be time in seconds; and p and q be the radial wavenumber components of the compression wave and shear wave within the waveguide rod, respectively. The calculation formula is as follows:

[0028] ;

[0029] Both p and q are in rad / m, and the external compression potential function corresponds to the longitudinal guided wave mode in the filling material. and lay shear potential function Take them as follows:

[0030] ;

[0031] Where C and D are the potential function amplitude coefficients in the filling body. and These are the zeroth-order and first-order Hankel functions of the first kind, respectively. The first-order Hankel function represents an outwardly propagating wave radially outward. and These are the radial wavenumber components of the compression wave and the radial wavenumber components of the shear wave in the filling material, respectively. The calculation formula is as follows:

[0032] :

[0033] This invention introduces a spring layer interface model between the waveguide rod and the filler to describe the shear bonding state of the adhesive interface. The spring layer interface model includes the normal spring stiffness. and tangential spring stiffness Normal spring stiffness and tangential spring stiffness The units are all N / m 3 Normal spring stiffness Characterizing the normal stress transfer capability between the waveguide rod and the filling material, tangential spring stiffness Characterizes the ability of tangential stress transmission between the waveguide rod and the filling material.

[0034] When the stiffness of the tangential spring When the spring layer interface model is zero, it degenerates into a free rod boundary condition. When the tangential spring stiffness... As the boundary value approaches infinity, the spring layer interface model degenerates into a fully bonded boundary condition, while the shear bond state of the filler cement interface lies between the two. The tangential spring stiffness... The value is determined through indoor pull-out tests. The longer the curing age of the filling material, the better the shear bond state of the cement interface, and the better the tangential spring stiffness. The larger the value, the better.

[0035] On the surface of the waveguide rod At this point, the boundary conditions for the spring layer interface model are written as follows:

[0036] ;

[0037] ;

[0038] in It is radial normal stress. It is the radial and axial shear stress. For radial displacement, For axial displacement, superscript Indicates the physical quantity within the waveguide rod, superscript Let A, B, C, and D represent the physical quantities in the filling body, with stress in Pa and displacement in m. Substituting the potential functions inside the waveguide rod and in the filling body into the geometric and physical equations of displacement and stress, and then into the boundary conditions of the spring layer, we obtain a homogeneous linear system of equations for the four unknowns A, B, C, and D, which can be written in matrix form as follows:

[0039] ;

[0040] in Given a 4x4 matrix of longitudinal mode coefficients, the condition for the homogeneous linear system of equations to have non-zero solutions is that the determinant of the longitudinal mode coefficient matrix is ​​zero, i.e.:

[0041] ;

[0042] This is the waveguide dispersion equation for the longitudinal guided wave mode. The circumferential order corresponds to the bending guided wave mode. The wave solution shows that the potential function of the bent guided wave mode exhibits a first-order trigonometric function variation in the circumferential direction, and the compression potential function of the bent guided wave mode within the waveguide rod is taken as... The shear wave potential function includes in-plane and out-of-plane shear components to describe the polarization characteristics of bending vibration. There are three potential function amplitude coefficients inside the waveguide rod and in the filling body. Using the same derivation method as for the longitudinal guided wave mode, the potential function is substituted into the elastic dynamic equation in cylindrical coordinates and the spring layer boundary conditions are applied to obtain a 6-row, 6-column bending mode coefficient matrix. The waveguide dispersion equation for the bent waveguide mode is:

[0043] ;

[0044] Numerical solutions were performed for the waveguide dispersion equations of the longitudinal waveguide mode and the flexural waveguide mode, respectively. The numerical solution employed the wavenumber scanning method, with frequency steps ranging from 1 kHz to 200 kHz. Point-by-point scanning, at each frequency point Angular frequency Substituting into the guided wave dispersion equation, with wavenumber For the unknown quantity, a parabolic iteration method combined with the bisection method is used in the interval 0.1 to 1000. The search engine searches for the real roots of the determinant, recording the range of sign changes during the search and iterating to wavenumber precision within that range. rad / m.

[0045] For viscoelastic media, the determinant is a complex number. The minimum point of the determinant's modulus is taken as the root of the guided wave dispersion equation, and the longitudinal mode wavenumbers at each frequency are obtained by solving the equation. and bending mode wavenumber Then, defined by phase velocity. Calculate the longitudinal modal phase velocity and bending mode phase velocity The unit of phase velocity is Group velocity is defined by group velocity. The calculations, using the central difference approximation at discrete frequency points, yield the following formulas for calculating the longitudinal mode group velocity and the bending mode group velocity:

[0046] ;

[0047] Group velocity unit is ,molecular The unit of is rad / s, and the unit of the wavenumber difference in the denominator is rad / m. Dividing the two gives m / s, which is dimensionally consistent. The longitudinal mode group velocity at each frequency point is... The longitudinal guided wave mode dispersion curves are obtained by connecting them sequentially, and the bending mode group velocities at each frequency point are then calculated. By sequentially connecting these, the bending guided wave mode dispersion curves are obtained. After obtaining the longitudinal guided wave mode dispersion curve and the bending guided wave mode dispersion curve, it is necessary to determine the frequency range in which both dispersion curves coexist. The longitudinal guided wave mode dispersion curve is located at a frequency... to There exists an effective solution within the range, and the mode dispersion curve of the bent guided wave exists at the frequency. to There exists a valid solution within the range, and the endpoint frequencies of the frequency interval where both dispersion curves coexist are taken as:

[0048] ;

[0049] Taking a 304 stainless steel waveguide rod with a radius of 0.01m embedded in a filling body with a ash-to-sand ratio of 1:4 as an example, the longitudinal guided wave modes... An effective solution exists above 5kHz, for the bent guided wave mode. There are valid solutions above 8kHz, and both dispersion curves have valid solutions within 200kHz. Therefore, the frequency range in which they coexist is from 8kHz to 200kHz.

[0050] Within a coexisting frequency range, two dispersion curves may be very close in certain frequency bands, making it impossible to distinguish between longitudinal guided wave modes and flexural guided wave modes in the guided wave received signal. Therefore, the group velocity difference between the longitudinal mode group velocity and the flexural mode group velocity at each frequency point is calculated:

[0051] ;

[0052] Group velocity difference is measured in m / s. Preset modal resolution threshold. The arrival time difference between the two modes is determined based on the minimum resolvable time difference of the receiving transducer and the propagation distance of the waveguide rod. Where L is the propagation distance of the waveguide rod. The group velocity reference value is determined by the following conditions: Therefore, the formula for calculating the preset modal resolution threshold is:

[0053] ;

[0054] in The smallest resolvable time difference of arrival for the receiving transducer, measured in seconds. The average of the longitudinal mode group velocity and the bending mode group velocity is taken, in m / s, and L is the waveguide rod propagation distance, in meters. The unit is m / s, and the dimension is The minimum arrival time difference of the receiving transducer. Waveguide rod propagation distance Group velocity reference value For example, substituting into the formula yields... .

[0055] Determine the group velocity difference point by point within the simultaneously existing frequency range. Is it greater than the preset modal resolution threshold? Frequency points meeting the conditions are grouped into the same continuous frequency segment and denoted as a sub-interval. If the frequency points meeting the conditions are divided into multiple discontinuous frequency segments, the continuous frequency segment containing the preset characteristic frequency is selected as the sub-interval. The preset characteristic frequency is determined based on the waveguide sensitive frequency band of the filling material. The waveguide sensitive frequency band of the filling material is the frequency range in which the guided wave responds significantly to changes in the elastic parameters of the filling material, ranging from 20kHz to 60kHz. The lower limit frequency of the sub-interval is denoted as... The upper frequency of the sub-interval is denoted as Lower limit frequency and upper limit frequency The defined frequency range is the frequency band where longitudinal guided wave modes and bending guided wave modes coexist.

[0056] Taking a 304 stainless steel waveguide rod with a radius of 0.01m embedded in a filling material with a ash-to-sand ratio of 1:4 as an example, the longitudinal mode group velocity in the range of 20kHz to 60kHz is obtained by numerical solution. Approximately 4500 Up to 5200 Bending mode group velocity Approximately 2800 Up to 3200 Group velocity difference Approximately 1300 Up to 2400 Greater than the preset modal resolution threshold Considering that the bending mode group velocity varies greatly with frequency and the mode energy is relatively weak in the range of 8kHz to 20kHz, the coexistence frequency band is finally set to 10kHz to 80kHz to leave a frequency margin.

[0057] After determining the coexistence frequency band of the longitudinal guided wave mode and the flexural guided wave mode, the broadband guided wave excitation acquisition unit excites the broadband guided wave signal within the coexistence frequency band, so that the longitudinal guided wave mode and the flexural guided wave mode are excited simultaneously and the group velocity difference between the two modes is greater than the preset mode resolution threshold. This ensures that the subsequent mode separation unit can separate the aliased longitudinal guided wave mode and the flexural guided wave mode. The lower limit frequency and upper limit frequency of the coexistence frequency band are also used to set the cutoff frequency for bandpass filtering. When performing bandpass filtering on the guided wave received signal, the high-pass cutoff frequency is set to one octave below the lower limit frequency, and the low-pass cutoff frequency is set to one octave above the upper limit frequency. This preserves the effective signal within the coexistence frequency band and suppresses out-of-band noise, thereby improving the signal-to-noise ratio of the guided wave received signal.

[0058] Broadband guided wave signals propagate axially as elastic waves within the waveguide rod. During propagation, particles on the waveguide rod surface undergo radial and axial displacement. When the waveguide rod is encased in filler, a coupling interface is formed between the waveguide rod and the filler. This coupling interface is the physical channel through which broadband guided wave signal energy is transferred from the waveguide rod to the filler, and it is also the physical channel through which the mechanical parameters of the filler react on the waveguide propagation characteristics. Understanding the energy distribution and mechanical action at the coupling interface is a prerequisite for comprehending the different modulation information carried by longitudinal and bending guided wave modes. The propagation distance of the broadband guided wave signal along the waveguide rod is... The guided wave energy after It follows the law of exponential decay:

[0059] ;

[0060] in The initial energy of the guided wave input at the excitation end is expressed in J, and f is the frequency of the broadband guided wave signal in Hz. For frequency The total attenuation coefficient at the point is expressed in Np / m. The total attenuation coefficient is determined by the damping attenuation coefficient of the waveguide rod material. and coupling interface leakage attenuation coefficient The two parts are added together to form:

[0061] ;

[0062] Waveguide rod material damping attenuation coefficient The material of the waveguide rod determines the performance; for 304 stainless steel waveguide rods... Take 0.005 Np / m as the leakage attenuation coefficient at the coupling interface. The attenuation rate of a portion of the broadband guided wave signal's energy leaking through the coupling interface to the filling material is characterized by the attenuation rate. The coupling interface leakage attenuation coefficient is related to the impedance ratio of the filling material and the waveguide rod, as well as the normal coupling coefficient and the tangential coupling coefficient. The calculation formula is as follows:

[0063] ;

[0064] in This refers to the density of the filling material, expressed in kg / m³. The longitudinal wave velocity in the filling material is expressed in m / s. Waveguide rod density, in kg / m³. Let be the longitudinal wave velocity in the waveguide rod, in m / s, and 'a' be the radius of the waveguide rod, in meters. The normal coupling coefficient is... The tangential coupling coefficient, normal coupling coefficient, and tangential coupling coefficient are both dimensionless parameters. The normal coupling coefficient... The ratio of radial displacement on the waveguide rod surface to normal stress transmitted through the coupling interface to the filling material is characterized by the normal coupling coefficient and the normal spring stiffness. The relationship is:

[0065] :

[0066] Tangential coupling coefficient The tangential coupling coefficient and tangential spring stiffness characterize the proportion of axial displacement on the waveguide rod surface that transmits tangential stress to the filling material through the coupling interface. The relationship is:

[0067] ;

[0068] Normal spring stiffness and tangential spring stiffness The units for all values ​​are N / m³, representing the normal spring stiffness. The bulk elastic parameters of the filling material determine the bulk elasticity of the filling material, which includes the elastic modulus of the filling material. Poisson's ratio of filling material Tangential spring stiffness The shear bond state of the cement interface between the waveguide rod and the filling material is determined by the formula. The unit is (N / m³)·m = N / m² = Pa. The unit is (kg / m³)(m / s)²=kg / (m·s²)=Pa. The ratio of the two is dimensionless and dimensionally consistent.

[0069] When the curing period of the filling material is short, the shear bond at the cement interface is weak, and the tangential spring stiffness is low. Smaller, tangential coupling coefficient The energy leakage of the bending guided wave mode through the coupling interface is close to zero. As the curing age of the filling material increases, the shear bond state of the cemented interface strengthens, and the tangential spring stiffness increases. Increase the tangential coupling coefficient As the bending waveguide mode increases, the energy leakage through the coupling interface increases. The bulk elastic parameters of the filling material act on the longitudinal waveguide mode through the coupling interface in a normal coupling manner. The particle displacement of the longitudinal waveguide mode within the waveguide rod cross-section mainly changes alternately between radial contraction and axial elongation. The radial displacement generates normal contact stress at the coupling interface. The magnitude of the normal contact stress is proportional to the bulk elastic parameters of the filling material. The constraint reaction force of the filling material on the radial displacement of the waveguide rod surface changes the normal boundary conditions of the longitudinal waveguide mode, causing the longitudinal mode group velocity to change relative to the free state. The quantitative relationship between the change in the longitudinal mode group velocity and the normal spring stiffness is:

[0070] ;

[0071] in The longitudinal modal group velocity is given by the infill constraint, in m / s. The longitudinal mode group velocity of the waveguide rod in its free state is expressed in m / s. The normal coupling sensitivity coefficient, in m² / N, is determined by indoor calibration tests based on the waveguide rod's material and geometric parameters. A negative sign indicates that the longitudinal mode group velocity decreases as the normal spring stiffness increases. The shear bond state at the bonding interface between the waveguide rod and the filler acts on the bending waveguide mode via tangential coupling. The particle displacement of the bending waveguide mode within the waveguide rod's cross-section is primarily transverse bending vibration. Axial displacement generates tangential contact stress at the coupling interface, the magnitude of which is proportional to the shear bond state at the bonding interface. The shear constraint reaction force of the filler on the axial displacement of the waveguide rod surface alters the tangential boundary conditions of the bending waveguide mode, causing a change in the bending mode group velocity relative to the free state. The quantitative relationship between the change in bending mode group velocity and the tangential spring stiffness is:

[0072] ;

[0073] in The bending mode group velocity under infill constraint is expressed in m / s. The bending mode group velocity of the waveguide rod in its free state is expressed in m / s. The tangential coupling sensitivity coefficient, expressed in m² / N, is determined by indoor calibration tests. In the formula... The unit is (m² / N)(N / m³), where m=1, and it is a dimensionless quantity. Similarly, dimensional consistency, normal coupling sensitivity coefficient and tangential coupling sensitivity coefficient The difference in values ​​is due to the different displacement distribution patterns of the longitudinal waveguide mode and the bending waveguide mode on the waveguide rod surface. The radial displacement of the longitudinal waveguide mode is uniformly distributed along the circumference on the waveguide rod surface, while the lateral displacement of the bending waveguide mode is distributed in a sinusoidal pattern along the circumference on the waveguide rod surface. The two displacement distributions have different responses to normal and tangential constraints.

[0074] The two formulas above establish a quantitative mapping relationship between the mechanical parameters of the filling material and the changes in the guided wave group velocity, specifically the longitudinal modal group velocity. The change is mainly due to the normal spring stiffness Control, and normal spring stiffness The longitudinal mode group velocity is determined by the bulk elastic parameters of the filling material. It primarily reflects the bulk elastic properties of the filling material and is used in subsequent tensile strength inversion units to invert the uniaxial compressive strength and bending mode group velocity of the filling material. The change is mainly due to the tangential spring stiffness Control, and tangential spring stiffness The bending mode group velocity is determined by the shear bond state of the cemented interface. It primarily reflects the shear bond quality of the cemented interface, and is related to the longitudinal modal group velocity in subsequent group velocity ratio building units. Together they constitute the group velocity ratio characteristic parameter.

[0075] The longitudinal and flexural guided wave modes, carrying the modulation information of the filling material, continue to propagate along the waveguide rod. Receiver transducers, using piezoelectric ceramic sheets, are spaced axially on the waveguide rod. These transducers are fixed to the waveguide rod surface by adhesive bonding or mechanical clamping. Under the influence of particle vibration on the waveguide rod surface, the piezoelectric ceramic sheets generate a charge proportional to the particle vibration velocity. This charge is converted into a voltage signal by the built-in charge amplifier in the receiver transducer, thus converting mechanical vibration into an electrical signal. The voltage signal output by the receiver transducer... for:

[0076] ;

[0077] in The velocity sensitivity of the receiving transducer, expressed in V / (m / s). The velocity of the particles on the waveguide rod surface is expressed in m / s, t is time expressed in seconds, and the spacing of the receiving transducers along the waveguide rod axis is also given. Determined based on spatial sampling conditions:

[0078] ;

[0079] in Longitudinal mode group velocity With bending mode group velocity The smaller value in the range, in m / s. The upper limit frequency of the coexistence band, in Hz, is expressed as the bending mode group velocity. Taking an upper frequency limit of 80kHz as an example, the spacing between receiving transducers The actual distance is taken as 0.01m to 0.02m. The electrical signal output from the receiving transducer first enters the preamplifier for signal amplification. The preamplifier adopts a frequency-variable gain compensation circuit. Frequency-variable gain compensation is a technical feature that distinguishes this invention from conventional fixed-gain amplification. Due to the leakage attenuation coefficient at the coupling interface... The gain increases with frequency, and high-frequency components attenuate more during propagation. If a fixed-gain amplification is used, the spectrum of the guided wave receiver signal will tilt towards lower frequencies. The energy of the bending guided wave modes in the high-frequency band may be lower than the noise level. The frequency-varying gain compensation circuit applies a gain to different frequency components that matches the leakage attenuation. Amplifier gain at the location for:

[0080] ;

[0081] in As the reference gain, The waveguide rod propagation distance is expressed in meters (m), with the exponent term being... Converting the leakage attenuation coefficient (in Np / m) to the gain compensation (in dB), the amplified electrical signal is represented in the frequency domain as follows:

[0082] ;

[0083] in To receive the transducer output voltage signal The Fourier transform and frequency-varying gain compensation make the amplitude of each frequency component of the amplified electrical signal tend to be consistent in the coexisting frequency band, avoiding the high-frequency curved waveguide mode being submerged by noise, and providing the signal-to-noise ratio conditions for subsequent synchronous squeezing wavelet transform to extract the time-frequency ridge.

[0084] The amplified electrical signal enters a bandpass filter for bandpass filtering. A fourth-order Butterworth bandpass filter is used, and the high-pass cutoff frequency for bandpass filtering is... and low-pass cutoff frequency Based on the lower limit frequency of the coexistence band and upper limit frequency Sure:

[0085] ;

[0086] Taking a coexisting frequency band of 10kHz to 80kHz as an example, the Qualcomm cutoff frequency Low-pass cutoff frequency The cutoff frequency is set to twice the bandwidth of the coexisting frequency band boundary to avoid attenuation of the edge mode signals of the coexisting frequency band by the filter transition band. This affects the amplitude-frequency response of the bandpass filter. for:

[0087] ;

[0088] The exponent 8 corresponds to the attenuation slope of the fourth-order Butterworth filter, which has two orders of attenuation at each cutoff frequency, for a total of four orders. The bandpass filtering process suppresses low-frequency drift noise below the high-pass cutoff frequency and high-frequency electromagnetic interference above the low-pass cutoff frequency, while retaining the signal components of longitudinal guided wave modes and curved guided wave modes in the coexisting frequency band and its neighborhood.

[0089] The electrical signal, after signal amplification and bandpass filtering, is converted from analog to digital by the data acquisition card. The sampling rate of the data acquisition card is... According to the Nyquist sampling condition, the following conditions are met. Taking a low-pass cutoff frequency of 160kHz as an example, the sampling rate is... To ensure the amplitude and phase accuracy of the analog-to-digital conversion, a discrete digital signal is obtained after the analog-to-digital conversion. :

[0090] ;

[0091] in The discrete digital signal is the time-domain electrical signal after signal amplification and bandpass filtering, where N is the number of sampling points and n is the discrete-time index. This refers to the acquired guided wave receiver signal. In the process, the modulation information carried by the longitudinal guided wave mode is manifested as the change of the longitudinal mode group velocity with the volumetric elastic parameters of the filling body, while the modulation information carried by the flexural guided wave mode is manifested as the change of the flexural mode group velocity with the shear bonding state of the cemented interface. The two types of modulation information are superimposed in the guided wave received signal in the form of different arrival times and different frequency components. In the subsequent mode separation unit, they are separated by synchronous extrusion wavelet transform and time-frequency ridge extraction to form the longitudinal mode arrival time series and the flexural mode arrival time series, respectively.

[0092] Taking a 304 stainless steel waveguide rod with a diameter of 20mm, a propagation distance of 3m, a filling material with a sand-to-cement ratio of 1:4, and a curing period of 28 days as an example, the waveguide rod density... Longitudinal wave velocity of waveguide rod , filling body density longitudinal wave velocity of the filling material Normal spring stiffness Tangential spring stiffness Normal coupling coefficient Tangential coupling coefficient At a frequency of 30kHz, the leakage attenuation coefficient at the coupling interface The leakage attenuation factor after propagation for 3m is Approximately 67% of the guided wave energy is retained within the waveguide rod. This energy level ensures that the receiving transducer can acquire guided wave reception signals with a signal-to-noise ratio that meets the mode separation requirements. The separation description of normal coupling and tangential coupling modes allows the longitudinal guided wave mode and the bending guided wave mode to carry modulation information of different mechanical properties of the filling body, respectively. This provides a physical basis for subsequently distinguishing the shear bonding state and bulk elastic properties of the cemented interface through group velocity ratio characteristic parameters. Frequency-varying gain compensation and bandpass filtering ensure the separability of the two types of mode information in the guided wave reception signal from the signal acquisition level.

[0093] The purpose of time-frequency analysis of guided wave received signals is to separate the aliased longitudinal guided wave modes and flexural guided wave modes in the time domain on the time-frequency plane. Synchronous squeezing wavelet transform redistributes the coefficients of continuous wavelet transform along the instantaneous frequency direction, making the concentration of time-frequency energy distribution higher than that of continuous wavelet transform, thus providing resolution conditions for subsequent time-frequency ridge extraction.

[0094] First, a preset wavelet mother function is selected. The preset wavelet mother function adopts the improved Morlet wavelet. The improved Morlet wavelet introduces a bandwidth adjustment factor on the basis of the Morlet wavelet to match the frequency band characteristics of the guided wave signal in the coexisting frequency band. The time domain expression of the improved Morlet wavelet is as follows:

[0095] ;

[0096] in Time, in seconds. The wavelet center angular frequency is expressed in rad / s. This is the bandwidth adjustment factor, measured in seconds. , Based on the lower and upper frequency limits of the coexisting frequency band, the frequency support interval of the improved Morlet wavelet is determined to cover the coexisting frequency band. The calculation formula is:

[0097] ;

[0098] in This is the lower limit frequency of the coexistence band. This represents the upper limit frequency of the coexisting frequency band, with units of Hz. The conversion factor between the Morlet wavelet half-power bandwidth and standard deviation is used, taking the coexisting frequency band of 10kHz to 80kHz as an example. The advantage of introducing a bandwidth adjustment factor is that it allows the time-frequency resolution of the preset wavelet mother function to match the bandwidth of the guided wave signal within the coexisting frequency band, avoiding mode aliasing due to an excessively wide wavelet time window or an increase in frequency estimation variance due to an excessively narrow time window. After selecting the preset wavelet mother function, a continuous wavelet transform is performed on the received guided wave signal. The calculation formula for the continuous wavelet transform is as follows:

[0099] ;

[0100] in For guided wave reception signals, the unit is V, a is the scale factor (dimensionless), and b is the translation factor (unit is s). To predetermine the complex conjugate of the wavelet mother function, These are continuous wavelet transform coefficients, in units of V·s. Scale factor a and analysis frequency The correspondence is The range of scale factor values ​​is determined based on the coexisting frequency bands, and the minimum scale factor... Maximum scale factor ,exist to Take logarithmically uniformly within the range Discrete scale points, translation factor By sampling interval Values ​​are taken within the time length of the guided wave received signal. After obtaining the continuous wavelet transform coefficients, the instantaneous frequency at each scale is calculated. The formula for calculating the instantaneous angular frequency is:

[0101] ;

[0102] in Let be the instantaneous angular frequency at scale a and translation b, in rad / s, where i is the imaginary unit. The partial derivatives of the continuous wavelet transform coefficients with respect to the translation factor are used in the discrete implementation, which employs the central difference approximation.

[0103] This invention introduces scale-adaptive thresholding before synchronous squeezing and redistribution to suppress the spread of noise coefficients during the redistribution process. Scale-adaptive thresholding sets coefficients in the continuous wavelet transform with energy below the scale-adaptive threshold to zero. The calculation formula is:

[0104] ;

[0105] in V represents the variance of the noise in the guided wave received signal, expressed in V², and N is the number of sampling points in the guided wave received signal. For scale-related factors, The scale correlation factor decreases as the scale factor increases, making the threshold at the low-frequency end of the large scale lower than the threshold at the high-frequency end of the small scale. This adapts to the characteristics of guided wave signals, which have high low-frequency energy and low high-frequency energy. (Noise variance...) The variance of the received waveguide signal before the arrival of the waveguide is estimated.

[0106] The continuous wavelet transform coefficients after thresholding are denoted as: :

[0107] ;

[0108] The threshold-processed continuous wavelet transform coefficients are synchronously squeezed and redistributed along the instantaneous frequency direction. This synchronous squeezing and redistribution accumulates the continuous wavelet transform coefficients with the same instantaneous frequency near the same moment onto the same frequency grid point, thus synchronously squeezing the time-frequency energy distribution. The continuous form is:

[0109] ;

[0110] in For Dirac functions, For a moment The set of scales retained after thresholding. The energy conservation correction factor, in discrete form, is:

[0111] ;

[0112] in This represents the k-th discrete angular frequency grid point, in rad / s. The nth discrete time point is represented by a time interval in seconds (s). The interval between adjacent angular frequency grid points, in rad / s. For the j-th scale interval, the synchronous extrusion time-frequency energy distribution The unit is V·s The squared modulus of the time-frequency energy distribution during synchronous extrusion The unit is V²·s, which represents the signal energy within a unit angular frequency interval on the time-frequency plane.

[0113] The advantage of synchronous squeezing redistribution lies in compressing the energy diffused along the scale direction in the continuous wavelet transform to the frequency grid points corresponding to the instantaneous frequency, making the energy trajectories of the longitudinal and curved guided wave modes on the time-frequency plane finer and improving the mode separation capability. After obtaining the synchronous squeezing time-frequency energy distribution, the energy peak point is searched along the time axis time-by-time. At each discrete time... Search Local maxima along the frequency axis, which satisfy the following:

[0114] ;

[0115] In the discrete implementation, local maxima are determined by comparing the energy of each frequency grid point with its left and right adjacent grid points. Frequency grid points with energy greater than their left and right adjacent grid points are denoted as energy peak points. At each time step, one or more energy peak points may be found; the set of energy peak points is denoted as [the set of energy peak points]. .

[0116] After finding the energy peak point, the energy peak points of adjacent times are connected to form a time-frequency ridge. This invention uses a cost function minimization method to connect energy peak points instead of directly connecting the peak points with the largest energy at adjacent times. The cost function comprehensively considers both energy continuity and frequency continuity. The definition of is:

[0117] ;

[0118] in As a candidate time-frequency ridge, For the ridge line at time angular frequency at that point Weights for continuous frequency terms, in rad. ·s , The weight of the energy term is dimensionless, and it is the first term. The second term constrains the ridge frequency to not jump between adjacent time points. To extend the ridgeline along a path with high energy, the Viterbi dynamic programming algorithm is used to search for a path in the set of energy peak points that minimizes the cost function. The path that minimizes the cost function is identified as the time-frequency ridge.

[0119] If there are multiple time-frequency ridges on the time-frequency plane, the initial arrival time of each time-frequency ridge is calculated separately. The initial arrival time is the moment when the energy on the time-frequency ridge first exceeds the ridge energy threshold. The time-frequency ridge with the earliest arrival time is determined as the longitudinal mode time-frequency ridge, and the time-frequency ridge with the latest arrival time is determined as the bending mode time-frequency ridge. The physical reason for the earliest arrival time is that the group velocity of the longitudinal guided wave mode is greater than that of the bending guided wave mode. The time required for the longitudinal guided wave mode to propagate from the excitation end to the receiving transducer is shorter than that of the bending guided wave mode.

[0120] To improve the reliability of modal determination, an energy centroid frequency criterion is added as an auxiliary criterion based on the arrival time criterion. The calculation formula is:

[0121] ;

[0122] in The frequency of the nth point on the ridge line is expressed in Hz. The energy centroid frequency reflects the frequency position where the energy of the time-frequency ridge line is concentrated. The energy centroid frequency of the longitudinal mode time-frequency ridge line and the energy centroid frequency of the bending mode time-frequency ridge line correspond to different positions on the dispersion curve. When the arrival time criterion and the energy centroid frequency criterion are consistent, the mode determination result is confirmed. When the two criteria are inconsistent, the arrival time criterion shall prevail and the mode determination result at that moment shall be marked for subsequent manual review.

[0123] After determining the longitudinal mode time-frequency ridge and the bending mode time-frequency ridge, the arrival time series of the longitudinal mode is read according to the time of each point on the longitudinal mode time-frequency ridge, and the arrival time series of the bending mode is read according to the time of each point on the bending mode time-frequency ridge. The arrival time series of the longitudinal mode and the arrival time series of the bending mode are sequences formed by arranging the arrival times of the longitudinal mode time-frequency ridge and the bending mode time-frequency ridge at each frequency point, respectively.

[0124] Taking a guided wave receiver signal with a sampling rate of 1MHz and a length of 0.01s as an example, the number of sampling points for the guided wave receiver signal is... The scaling factor is taken from 256 log-uniform scaling points in the range of 10kHz to 80kHz, which improves the center angular frequency of the Morlet wavelet. The continuous wavelet transform yields a 256 x 10000 continuous wavelet transform coefficient matrix. After scale-adaptive thresholding and synchronous squeezing redistribution, the synchronous squeezing time-frequency energy distribution is obtained. The arrival time of the longitudinal mode time-frequency ridge is approximately 0.0007 s near 30 kHz, and the arrival time of the bending mode time-frequency ridge is approximately 0.0011 s. The time interval between the two time-frequency ridges on the time-frequency plane is approximately 0.0004 s. This time interval is greater than the minimum arrival time difference of 2 μs that the receiving transducer can resolve. The longitudinal mode time-frequency ridge and the bending mode time-frequency ridge are resolvable.

[0125] Compared to continuous wavelet transform, synchronous squeezing wavelet transform improves the clustering of time-frequency energy distribution, making the trajectories of longitudinal mode time-frequency ridges and bending mode time-frequency ridges clearer on the time-frequency plane. The ridge connection method with cost function minimization avoids ridge breakage and jumps caused by noise peak points. Scale-adaptive threshold processing suppresses the spread of noise in synchronous squeezing redistribution. These three techniques work together to ensure the accuracy of reading the arrival time series of longitudinal mode and bending mode, providing arrival time data for the subsequent group velocity calculation unit to calculate the group velocity values ​​of longitudinal mode and bending mode.

[0126] After performing synchronous squeezing wavelet transform on the received guided wave signal to obtain the time-frequency energy distribution, the time-frequency energy distribution contains not only the energy trajectories corresponding to the longitudinal guided wave mode and the curved guided wave mode, but also the energy peaks generated by noise and the discontinuous energy trajectories generated by electromagnetic interference. It is necessary to separate the energy trajectories corresponding to the longitudinal guided wave mode and the curved guided wave mode from the time-frequency energy distribution through candidate time-frequency ridge extraction and multi-level screening. This step directly affects the reading accuracy of the arrival time series of the longitudinal mode and the arrival time series of the curved mode.

[0127] The time-frequency energy distribution is obtained by performing synchronous squeezing wavelet transform on the guided wave received signal. ,in For discrete angular frequency grid points, For discrete time intervals, the calculation process for time-frequency energy distribution is consistent with the calculation process for time-frequency energy distribution during synchronous extrusion.

[0128] Candidate time-frequency ridges are extracted from the time-frequency energy distribution. The extraction of candidate time-frequency ridges adopts a method combining time-by-time peak search and connected component labeling. At each discrete time... Search along the frequency axis to satisfy and For local peak points, all local peak points at any given time are labeled as connected components based on temporal and frequency adjacency. Temporal adjacency is defined as the time difference between two peak points being equal to one sampling interval, and frequency adjacency is defined as the frequency difference between peak points at adjacent times being less than a preset frequency jump threshold. The preset frequency jump threshold is set to three times the interval between adjacent frequency grid points. Peak points within the same connected domain are connected in chronological order to form a candidate time-frequency ridge. Multiple candidate time-frequency ridges may be extracted from the time-frequency energy distribution. Each candidate time-frequency ridge is denoted as... , M represents the total number of candidate time-frequency ridges.

[0129] For each candidate time-frequency ridge, ridge continuity is calculated. Ridge continuity is the proportion of sampling points with energy values ​​greater than a preset ridge energy threshold on the time axis to the total number of sampling points of the candidate time-frequency ridge. This invention introduces energy weighting in the ridge continuity calculation, ensuring that sampling points with higher energy contribute more to the continuity calculation than those with lower energy. The calculation formula is:

[0130] ;

[0131] in This is an indicator function; the indicator function takes the value 1 if the condition within the square brackets is true, and takes the value 0 if the condition is false. To preset the ridge energy threshold, The energy weight of the nth sampling point on the candidate time-frequency ridge. , The maximum energy value in the time-frequency energy distribution, and the energy weight. For dimensionless quantities, weighted ridge continuity It is a dimensionless quantity.

[0132] Preset spine energy threshold Based on the noise floor in the time-frequency energy distribution, the value is determined to be three times the average energy of the time-frequency energy distribution in the guided wave reception signal before the arrival of the guided wave.

[0133] ;

[0134] in The mean energy of the time-frequency energy distribution before the arrival of the guided wave is expressed in V²·s. The basis for taking 3 times is that when the noise energy follows an exponential distribution, the false alarm probability corresponding to 3 times the mean is about 5%.

[0135] Weighted ridge continuity of each candidate time-frequency ridge line With preset continuity threshold Comparison with preset continuity threshold Take 0.6, when Candidate time-frequency ridges are determined to be generated by noise or interference and are removed. The advantage of retaining candidate time-frequency ridges and introducing energy weighting is to prevent individual high-energy noise points on the candidate time-frequency ridges from misjudging discontinuous noise trajectories as continuous ridges, and to prevent individual low-energy points on the candidate time-frequency ridges from mistakenly removing true modal ridges.

[0136] The modal energy percentage is calculated for the retained candidate time-frequency ridges. The modal energy percentage is the proportion of the energy of the candidate time-frequency ridge within a preset frequency window to the total energy of the time-frequency energy distribution. This invention introduces dispersion weights in the modal energy percentage calculation. These dispersion weights are determined based on the numerically solved longitudinal guided wave mode dispersion curves and curved guided wave mode dispersion curves, thus giving greater weight to the energy on the candidate time-frequency ridges that is close to the frequency position of the theoretical dispersion curve. The proportion of dispersion-weighted mode energy of the retained candidate time-frequency ridges within the preset frequency window for:

[0137] ;

[0138] in The frequency of the nth sampling point on the candidate time-frequency ridge is expressed in Hz. and These represent the lower and upper frequency limits of the preset frequency window, respectively, in Hz. K is the total number of frequency grid points, N is the total number of time sampling points, and the denominator is the total energy of the time-frequency energy distribution, in V²·s. This is the dispersion weight, and the formula for calculating the dispersion weight is:

[0139] ;

[0140] in For the theoretical dispersion curve at time... The corresponding frequency, in Hz. Here, represents the standard deviation of the dispersion weight, expressed in Hz. The dispersion weight is a dimensionless quantity. Take 5 times the spacing between adjacent frequency grid points.

[0141] The preset frequency window is determined based on the frequency distribution range of the longitudinal guided wave mode and the curved guided wave mode on the dispersion curve. The preset frequency window for the longitudinal guided wave mode is 20kHz to 80kHz, and the preset frequency window for the curved guided wave mode is 10kHz to 50kHz. For each retained candidate time-frequency ridge, the modal energy ratio within the two preset frequency windows is calculated and denoted as . and .

[0142] Based on the arrival times of the longitudinal guided wave mode and the flexural guided wave mode, the retained candidate time-frequency ridges are classified into longitudinal guided wave modes and flexural guided wave modes, respectively. First, the start and arrival times of each retained candidate time-frequency ridge are calculated. The initial arrival time is when the energy on the candidate time-frequency ridge first exceeds the preset ridge energy threshold. At the specified time, the remaining candidate time-frequency ridges are arranged in ascending order of their initial arrival time. When there are two remaining candidate time-frequency ridges, the candidate time-frequency ridge with the earliest initial arrival time is classified as the longitudinal guided wave mode, and the candidate time-frequency ridge with the latest initial arrival time is classified as the curved guided wave mode. When there are three or more remaining candidate time-frequency ridges, each candidate time-frequency ridge is compared... and The size, when When candidate time-frequency ridges are classified as longitudinal guided wave modes, Candidate time-frequency ridges are classified as curved guided wave modes. The classification results of arrival time order and mode energy ratio are cross-checked. When the two classification results are inconsistent, the classification result of mode energy ratio shall prevail and the candidate time-frequency ridge shall be marked for subsequent verification.

[0143] For candidate time-frequency ridges classified as longitudinal guided wave modes, the arrival time of the longitudinal mode is picked up at each frequency point using the AIC first-arrival picking algorithm. Specifically, for each frequency point on the candidate time-frequency ridge... ,by Gaussian narrowband filtering is applied to the guided wave received signal at the center frequency. The Gaussian narrowband filtering is implemented in the frequency domain as follows:

[0144] ;

[0145] in For receiving signals by guided waves Fourier transform, Center frequency Gaussian window function, , The standard deviation of the Gaussian window is set to 2kHz. Center frequency The narrowband filtered signal at a given location is used to calculate the AIC function.

[0146] ;

[0147] Where k is the sequence number of the dividing point. Set the AIC window length to 512 sampling points. Let V be the variance of the first to the kth sampling points in the narrowband filtered signal. The first in the narrowband filtered signal The first to the second The variance of each sampling point, where the AIC function is a dimensionless quantity, is denoted as the sampling point corresponding to the minimum value of the AIC function. .

[0148] This invention introduces an energy ratio constraint on the AIC first-arrival picking algorithm to improve picking accuracy at low signal-to-noise ratio frequency points. Calculate the energy ratio function within the range of each of the M sampling points before and after:

[0149] ;

[0150] in The energy ratio half-window length is set to 20 sampling points. The energy ratio function is dimensionless. The sampling point corresponding to the maximum value of the energy ratio function is denoted as . The weighted average of the location of the minimum value of the AIC function and the location of the maximum value of the energy ratio function is taken as the arrival time of the longitudinal mode:

[0151] ;

[0152] in The weighting coefficient is set to 0.6. Sampling rate, Let be the arrival time of the longitudinal mode at the j-th frequency point, in seconds. The advantage of introducing the energy ratio constraint is that the minimum position of the AIC function may shift to the noise segment when the signal-to-noise ratio is low. The energy ratio function is more sensitive to the energy change at the arrival time of the signal. The weighting of the two can suppress the picking bias.

[0153] Arrange the arrival times of the longitudinal modes at each frequency point in ascending order of frequency to form a longitudinal mode arrival time series. , Given the total number of frequency points, the arrival time of the bending mode is picked up in the same way for the candidate time-frequency ridges classified as bending guided wave modes. That is, the guided wave received signal is subjected to Gaussian narrowband filtering with each frequency point on the candidate time-frequency ridge as the center frequency. The AIC function and energy ratio function are calculated on the narrowband filtered signal, and the weighted average is taken to obtain the arrival time of the bending mode. Arrival times of bending modes at each frequency point are arranged according to frequency to form a bending mode arrival time series. .

[0154] Taking a guided wave receiver signal with a sampling rate of 1MHz and a length of 0.01s as an example, the time-frequency energy distribution is a matrix of 10,000 time sampling points multiplied by 256 frequency grid points. Five candidate time-frequency ridges are extracted. Among them, the weighted ridge continuity of three candidate time-frequency ridges are 0.32, 0.41, and 0.55, respectively, which are below the preset continuity threshold of 0.6 and are therefore rejected. The remaining two candidate time-frequency ridges have weighted ridge continuity of 0.87 and 0.82, respectively, and start arrival times of 0.0007s and 0.0011s, respectively. The candidate time-frequency ridge with a start arrival time of 0.0007s has a 20kHz range. The modal energy proportion within the 20kHz to 80kHz window is 0.34, which is greater than the modal energy proportion within the 10kHz to 50kHz window (0.12). This is classified as a longitudinal guided wave mode. The candidate time-frequency ridge with an initial arrival time of 0.0011s has a modal energy proportion of 0.28 within the 10kHz to 50kHz window, which is greater than the modal energy proportion within the 20kHz to 80kHz window (0.09). This is classified as a bent guided wave mode. At the 30kHz frequency point, the minimum AIC function corresponds to sampling point 700, and the maximum energy ratio function corresponds to sampling point 703. The weighted longitudinal mode arrival time is... After the arrival time series of the longitudinal mode and the arrival time series of the bending mode are formed, they are sent to the group velocity calculation unit. The group velocity calculation unit calculates the group velocity values ​​of the longitudinal mode and the bending mode based on the arrival time of each frequency point and the propagation distance of the waveguide rod. The weighted ridge continuity screening and the dispersion weighted mode energy ratio classification ensure that the candidate time-frequency ridges entering the AIC first arrival pickup are the true energy trajectories of the longitudinal waveguide mode and the bending waveguide mode. The joint pickup of AIC and energy ratio improves the pickup accuracy of the arrival time of each frequency point and provides reliable time data for group velocity calculation.

[0155] The arrival time series of the longitudinal and flexural modes provide the arrival times of the longitudinal and flexural guided wave modes at each discrete frequency sampling point. However, group velocity calculation requires comparing the propagation times of the two modes at a uniform frequency. Therefore, it is necessary to determine a preset characteristic frequency and read the arrival times of the two modes at the preset characteristic frequency. The selection of the preset characteristic frequency directly affects the sensitivity of the longitudinal and flexural mode group velocity values ​​to changes in the mechanical parameters of the filling material. The preset characteristic frequency is not arbitrarily specified, but is determined based on the difference in group velocities on the dispersion curves of the longitudinal and flexural guided wave modes, as well as the energy of the two modes in the time-frequency energy distribution. A characteristic frequency quality factor is defined. for:

[0156] ;

[0157] in and Frequency distribution on longitudinal guided wave mode dispersion curves and bending guided wave mode dispersion curves The longitudinal mode group velocity and bending mode group velocity at the location, in m / s. The reference group velocity is taken as 5000 m / s. and The longitudinal mode time-frequency ridge and the bending mode time-frequency ridge in the time-frequency energy distribution at frequency The energy at a given point is expressed in V²·s. The first term is the normalized group velocity difference, the second term is the harmonic average of the two-mode energies, and the characteristic frequency quality factor is also given. It is a dimensionless quantity.

[0158] The waveguide sensitive frequency band of the filling material is the frequency range in which the guided wave responds significantly to changes in the elastic parameters of the filling material. Within the waveguide sensitive frequency band of the filling material, the characteristic frequency quality factor is maximized. The frequency at which the maximum value is taken is determined as the preset characteristic frequency:

[0159] ;

[0160] in and These are the lower and upper limits of the waveguide sensitive frequency band for the infill body, respectively, in Hz. The advantage of determining the preset characteristic frequency in this way is that the velocity difference between the two mode groups is large and the energy of the two modes is sufficient at the preset characteristic frequency, which ensures that the longitudinal waveguide mode and the bending waveguide mode can be distinguished in terms of arrival time and also ensures the accuracy of arrival time pickup.

[0161] After determining the preset characteristic frequency, the arrival time of the longitudinal mode corresponding to the preset characteristic frequency is read from the longitudinal mode arrival time series. The longitudinal mode arrival time series consists of discrete frequency sampling points. and corresponding arrival time Composition, when the preset characteristic frequency With a certain discrete frequency sampling point Read directly when they are equal As the longitudinal mode arrival time at the preset characteristic frequency, when the preset characteristic frequency does not fall on the discrete frequency sampling points of the longitudinal mode arrival time series, the adjacent discrete frequency sampling points on both sides of the preset characteristic frequency are found. and satisfy ,exist and Linear interpolation is performed between the longitudinal mode arrival times:

[0162] ;

[0163] in The arrival time of the longitudinal mode at the preset characteristic frequency is expressed in seconds. The physical basis of linear interpolation is that the arrival time changes approximately linearly with the frequency when the interval between adjacent discrete frequency sampling points is small enough.

[0164] Before interpolation and The arrival time at a given point is used to determine the pickup quality. Pickup quality is measured by the second difference of the AIC function at its minimum. Arrival times with a second difference less than a preset curvature threshold are considered unreliable. Take when it is an unreliable point and Perform interpolation when Take when it is an unreliable point and Perform interpolation when and When all points are unreliable, extend the sampling point by one point on each side. and Perform linear interpolation.

[0165] The arrival times of the bending modes at the preset characteristic frequencies are obtained from the bending mode arrival time series using the same method. First, it is determined whether the preset characteristic frequency falls on the discrete frequency sampling point of the arrival time series of the bending mode. If it falls on the discrete frequency sampling point, it is read directly. If it does not fall on the discrete frequency sampling point, linear interpolation is performed between the two adjacent discrete frequency sampling points. Before interpolation, the picking quality is also judged.

[0166] After obtaining the arrival times of the longitudinal mode and the bending mode at the preset characteristic frequency, the system delay time needs to be subtracted. The system delay time includes the electromechanical conversion delay of the excitation transducer, the electromechanical conversion delay of the receiving transducer, and the electrical delay of the data acquisition circuit. The system delay time does not change with the propagation distance of the waveguide rod but is related to the frequency of the guided wave mode and needs to be calibrated in advance.

[0167] This invention employs a dual-distance calibration method to calibrate the system delay time. Before the waveguide rod is embedded in the filling material, it is placed in a free state. One excitation transducer and two receiving transducers are arranged axially on the waveguide rod. The distance from the excitation transducer to the first receiving transducer is... The distance from the excitation transducer to the second receiving transducer is , and The units are all in meters (m). A calibration guided wave signal with the same frequency band as the broadband guided wave signal is excited, and the arrival time of the preset characteristic frequency at the two receiving transducers is recorded respectively. and The arrival time meets the following requirements:

[0168] ;

[0169] in The group velocity at a preset characteristic frequency for the waveguide rod in its free state, in m / s. Let be the system delay time, in seconds. Subtracting the two equations to eliminate the system delay time yields the free state group velocity:

[0170] ;

[0171] Substituting the free state group velocity into the first equation yields the system delay time:

[0172] ;

[0173] in the formula The unit is m. The unit is s. The unit is m / s, and the dimensions are consistent. The unit is m·s, divided by The unit m is used to obtain s. The unit is s, and the dimensions are self-consistent.

[0174] The dual-distance calibration method does not require the theoretical value of the free-state group velocity of the waveguide rod. It directly eliminates the system delay time using measurements of two propagation distances, thus avoiding the influence of waveguide rod material parameter deviations on calibration accuracy. The system delay time is calibrated separately for the longitudinal guided wave mode and the bending guided wave mode. The system delay time for the longitudinal guided wave mode is denoted as... The system delay time of the curved guided wave mode is denoted as Subtract the pre-calibrated system delay time from the arrival time of the longitudinal mode at the preset characteristic frequency. The net propagation time of the longitudinal mode is obtained as follows:

[0175] ;

[0176] The longitudinal mode group velocity is obtained by dividing the waveguide rod propagation distance by the net propagation time of the longitudinal mode:

[0177] ;

[0178] Where L is the waveguide rod propagation distance, in meters (m). The net propagation time for the longitudinal mode is expressed in seconds. The longitudinal modal group velocity value, in m / s, is calculated by subtracting the system delay time from the arrival time of the bending mode at the preset characteristic frequency. The net propagation time of the bending mode is obtained as follows:

[0179] ;

[0180] The bending mode group velocity is obtained by dividing the waveguide rod propagation distance by the net propagation time of the bending mode:

[0181] ;

[0182] in The net propagation time of the bending mode is expressed in seconds. This represents the bending mode group velocity value, in m / s.

[0183] Since the group velocity drifts with temperature due to the change in the elastic modulus of the waveguide rod, this invention introduces a temperature correction in the group velocity calculation, by installing a temperature sensor on the waveguide rod to measure its temperature. , to calibrate temperature Based on this, the temperature-corrected longitudinal mode group velocity value is:

[0184] ;

[0185] in This is the group velocity temperature coefficient of the waveguide rod material, expressed in 1 / ℃. For 304 stainless steel... Pick The negative sign indicates that the waveguide rod's elastic modulus decreases with increasing temperature, leading to a decrease in group velocity. The bending mode group velocity value is obtained by applying the same formula with temperature correction. The group velocity ratio characteristic parameters are then calculated using temperature-corrected longitudinal modal group velocity values ​​and bending modal group velocity values ​​in subsequent group velocity ratio building units.

[0186] Taking a waveguide with a 20mm diameter, 3m propagation distance, and a waveguide filling material in the sensitive frequency band of 20kHz to 60kHz as an example, the characteristic frequency quality factor is calculated from the dispersion curve and time-frequency energy distribution. , The maximum value is taken at 35kHz, the preset characteristic frequency is determined to be 35kHz, and the discrete frequency sampling point interval of the longitudinal mode arrival time series is 0.5kHz. 35kHz falls exactly on the discrete frequency sampling point. The arrival time of the bending mode at 35 kHz falls between 34.5 kHz and 35.5 kHz in the time series. , Linear interpolation yields Dual-distance calibration , , , Free state group velocity System delay time Longitudinal mode net propagation time Longitudinal mode group velocity value Net propagation time of bending mode Bending mode group velocity values .

[0187] After the longitudinal modal group velocity values ​​and the bending modal group velocity values ​​are calculated, they are sent to the group velocity ratio construction unit. The group velocity ratio construction unit calculates the ratio of the bending modal group velocity value to the longitudinal modal group velocity value as the group velocity ratio characteristic parameter. The characteristic frequency quality factor is maximized to ensure the sensitivity of the difference between the two modal group velocities at the preset characteristic frequency to changes in the mechanical parameters of the filling body. The dual-distance calibration method eliminates the influence of the system delay time on the absolute value of the group velocity. Temperature correction suppresses the group velocity drift caused by changes in ambient temperature. The three techniques work together to improve the calculation accuracy of the longitudinal modal group velocity values ​​and the bending modal group velocity values.

[0188] The absolute values ​​of the longitudinal mode group velocity and the bending mode group velocity are affected by the deviation of the waveguide rod material parameters, the deviation of the geometric parameters, and the ambient temperature. Directly using the ratio of the bending mode group velocity to the longitudinal mode group velocity as the group velocity ratio characteristic parameter will introduce systematic errors. Performing free state calibration and calculating the normalized group velocity ratio before the waveguide rod is embedded in the filling body can eliminate the influence of the waveguide rod's own parameter deviation on the group velocity ratio characteristic parameter, so that the group velocity ratio characteristic parameter only reflects the change of the shear bonding state of the cemented interface.

[0189] Before the waveguide rod is embedded in the filling material, the waveguide rod is placed in a free state. The free state refers to the state in which the waveguide rod is not constrained by the filling material and the surface of the waveguide rod is not in contact with other solids. The waveguide rod is suspended by elastic ropes or fixed by foam support to reduce the influence of the support structure on the propagation of guided waves. In the free state, a calibration guided wave signal with the same frequency band as the broadband guided wave signal is excited. The excitation waveform and frequency range of the calibration guided wave signal are consistent with the broadband guided wave signal and are generated by the same excitation transducer. The guided wave received signal in the free state is collected.

[0190] The free-state guided wave received signal is processed in the same way as the guided wave received signal, including mode separation and group velocity calculation. Specifically, synchronous squeeze wavelet transform, time-frequency ridge extraction, candidate time-frequency ridge screening, AIC first arrival picking, and group velocity calculation are performed sequentially to obtain the longitudinal mode free group velocity value and the bending mode free group velocity value.

[0191] To reduce random errors in a single measurement, this invention repeatedly excites the calibration guided wave signal in a free state. Each time, after excitation, a set of free-state guided wave received signals is acquired, and a set of longitudinal mode free group velocity values ​​and bending mode free group velocity values ​​are obtained. Take 10, with The arithmetic mean of the measurements is used as the longitudinal modal free group velocity value and the bending modal free group velocity value:

[0192] ;

[0193] in and The first The longitudinal modal free group velocity and bending modal free group velocity values ​​obtained from this measurement are in m / s.

[0194] This invention also calculates the group velocity ratio at multiple frequency points near a preset characteristic frequency and performs a weighted average to reduce the impact of single-point frequency measurement errors on the group velocity ratio. Take from both sides There are a total of discrete frequency sampling points. At each frequency point, Calculate the longitudinal modal free group velocity values ​​at each location. and bending mode free group velocity values Characteristic frequency quality factor Weighted average of the weights, benchmark group velocity ratio The calculation formula is:

[0195] ;

[0196] in The interval between discrete frequency sampling points. Take 5 as the reference group velocity ratio It is a dimensionless quantity.

[0197] Since the ambient temperature during free-state calibration and on-site monitoring may differ, the waveguide rod's elastic modulus changes with temperature, causing variations in the longitudinal and bending mode free group velocities. Therefore, a temperature correction is needed for the reference group velocity ratio. The temperature-corrected reference group velocity ratio is:

[0198] ;

[0199] in To calibrate the waveguide rod temperature during guided wave signal acquisition, the unit is ℃. The waveguide rod temperature during on-site monitoring is expressed in °C. The group velocity ratio temperature coefficient, expressed in units of 1 / ℃, is obtained through repeated free-state calibration at different temperatures. For a 304 stainless steel waveguide... Pick The temperature correction factor is a dimensionless quantity.

[0200] The ratio of the bending modal group velocity to the longitudinal modal group velocity is calculated based on the longitudinal modal group velocity and the bending modal group velocity, and is used as the measured group velocity ratio. The measured group velocity ratio is also calculated using a multi-frequency weighted average.

[0201] ;

[0202] in and Frequency The longitudinal modal group velocity and bending modal group velocity values ​​at the location are in m / s, and the measured group velocity ratio is... It is a dimensionless quantity.

[0203] The normalized group velocity ratio is obtained by dividing the measured group velocity ratio by the reference group velocity ratio:

[0204] ;

[0205] Normalized group velocity ratio As a dimensionless quantity, the normalized group velocity ratio is used as a characteristic parameter of the group velocity ratio. The physical meaning of the normalized group velocity ratio is as follows: when the waveguide rod is in a free state, the measured group velocity ratio is equal to the reference group velocity ratio, and the normalized group velocity ratio is equal to 1; when the waveguide rod is embedded in the filler, the shear bonding state of the cemented interface causes the reduction in the bending mode group velocity value to be greater than the reduction in the longitudinal mode group velocity value, the measured group velocity ratio is less than the reference group velocity ratio, and the normalized group velocity ratio is less than 1; the stronger the shear bonding state of the cemented interface, the greater the reduction in the bending mode group velocity value, and the smaller the normalized group velocity ratio.

[0206] Normalized group velocity ratio and tangential spring stiffness The approximate relationship between them is:

[0207] ;

[0208] in The group velocity ratio sensitivity coefficient, with units of m² / N. Determined by indoor calibration tests, This refers to the tangential spring stiffness, expressed in N / m³. The radius of the waveguide rod is in meters. Since it is a dimensionless quantity, this formula shows that the normalized group velocity ratio decreases linearly with the increase of tangential spring stiffness. In the subsequent tensile strength inversion unit, a dynamic reduction coefficient is constructed based on the normalized group velocity ratio.

[0209] To assess the reliability of the group velocity ratio characteristic parameter, this invention also calculates the synthesis uncertainty of the normalized group velocity ratio:

[0210] ;

[0211] in The uncertainty of the measured group velocity ratio is given by the standard deviation of the group velocity ratio from multiple field monitoring data. The uncertainty of the reference group velocity ratio is given by The standard deviation of the sub-free state measurement is given. Let be the uncertainty of the normalized group velocity ratio, and be a dimensionless quantity. When the uncertainty exceeds the preset uncertainty threshold of 0.05, the group velocity ratio characteristic parameter of this monitoring is marked as low reliability data, and the weight of low reliability data is reduced in the subsequent construction of dynamic reduction coefficient.

[0212] Taking a 304 stainless steel waveguide rod with a diameter of 20mm and a propagation distance of 3m as an example, the longitudinal mode free group velocity values ​​were obtained from 10 measurements in the free state. Flexural mode free group velocity values Reference group velocity ratio Calibration temperature On-site temperature Temperature-corrected reference group velocity ratio Longitudinal mode group velocity values ​​were obtained from on-site monitoring. Bending mode group velocity values The measured group velocity ratio Normalized group velocity ratio The reason why the normalized group velocity ratio is greater than 1 is that the constraint of the filling body causes the longitudinal modal group velocity value to decrease by a greater margin than the bending modal group velocity value. As the curing age of the filling body increases and the shear bonding state of the cement interface strengthens, the bending modal group velocity value decreases by a greater margin, and the normalized group velocity ratio gradually decreases to less than 1.

[0213] The normalized group velocity ratio eliminates the influence of waveguide rod material parameter deviation, geometric parameter deviation, and temperature change on the absolute value of the group velocity ratio, making the group velocity ratio characteristic parameters of different waveguide rods and different monitoring times comparable. Multi-frequency point weighted averaging reduces the error of single-point frequency measurement, and the combined uncertainty assessment provides a quantitative basis for the reliability of the subsequent dynamic reduction coefficient. The normalized group velocity ratio is fed into the tensile strength inversion unit as a group velocity ratio characteristic parameter to construct the dynamic reduction coefficient.

[0214] The dynamic reduction factor needs to establish a quantitative relationship between the group velocity ratio characteristic parameter and the reduction factor through indoor calibration tests. The specimen design and fitting model selection of the calibration test directly affect the accuracy of the dynamic reduction factor. Using a fitting model with physical constraints can avoid the risk of extrapolation outside the calibration data range due to pure empirical fitting.

[0215] Multiple sets of calibration specimens for infill bodies with different mix proportions and curing ages were prepared. The mix proportions included two factors: the cement-sand ratio and the mass concentration. The cement-sand ratios were taken at three levels: 1:4, 1:6, and 1:8. The mass concentrations were taken at three levels: 68%, 72%, and 76%. The curing ages were taken at five levels: 3d, 7d, 14d, 28d, and 60d. A total of nine sets of calibration specimens for infill bodies with different mix proportions were prepared using an orthogonal experimental design. Three parallel specimens were prepared for each mix proportion at each curing age. The specimens used for the uniaxial compression test were cubes with a side length of 70.7 mm, and the specimens used for the Brazilian splitting test were discs with a diameter of 50 mm and a thickness of 25 mm. The cube specimens and disc specimens were cast and cured under the same conditions.

[0216] During the casting of each set of filling body calibration specimens, a waveguide rod segment of the same material and diameter as the one on site was embedded in the center of the cubic specimen. The waveguide rod segment was 200mm long, and one end of the waveguide rod segment extended 50mm out of the specimen surface for installing the excitation transducer and the receiving transducer. The distance between the excitation transducer and the receiving transducer was reduced to 0.3m proportionally to the propagation distance of the waveguide rod on site.

[0217] After the infill calibration specimens reach the predetermined curing age, guided wave testing is performed first, followed by mechanical testing. Guided wave testing is completed within 2 hours before the mechanical testing to ensure the mechanical state of the infill calibration specimens remains unchanged. Broadband guided wave signals are excited for each group of infill calibration specimens, and calibration guided wave received signals are acquired. The frequency range and excitation waveform of the broadband guided wave signals are consistent with the broadband guided wave signals used for on-site monitoring. Mode separation, group velocity calculation, and group velocity ratio calculation are performed sequentially on the calibration guided wave received signals. Mode separation employs synchronous extrusion wavelet transform and time-frequency ridge extraction. Group velocity calculation is performed at a preset characteristic frequency. Group velocity ratio calculation includes free state calibration and normalization processing. The calibration group velocity ratio characteristic parameters for each group of infill calibration specimens are obtained, and these characteristic parameters are denoted as [reference needed]. , The specimen groups are numbered, and the average value of the calibration group velocity ratio characteristic parameter of the three parallel specimens in each group is taken as the representative value of the group.

[0218] After the guided wave test, uniaxial compression and Brazilian splitting tests were performed on each group of infill calibration specimens. In the uniaxial compression test, axial pressure was applied to the cubic specimen at a loading rate of 0.5 mm / min on a pressure testing machine until the specimen failed, and the failure load was recorded. calibrating uniaxial compressive strength The calculation formula is:

[0219] ;

[0220] in The bearing area of ​​the cubic specimen is in m². The unit is N. The unit is Pa.

[0221] The Brazilian splitting test involves applying a radial-to-linear load to a disc specimen on a compression testing machine at a loading rate of 0.2 mm / min until the disc splits and fails. The splitting failure load is then recorded. calibrated tensile strength The calculation formula is:

[0222] ;

[0223] in The diameter of the disc specimen is... The thickness of the disc specimen is given in meters (m). The unit is N. The unit is Pa, in the formula The dimension is N / m² = Pa.

[0224] The actual reduction factor for each group of infill calibration specimens is obtained by dividing the calibrated tensile strength by the calibrated uniaxial compressive strength:

[0225] ;

[0226] Actual reduction factor As a dimensionless quantity, the actual reduction factor reflects the true ratio of the tensile strength to the uniaxial compressive strength of the filling material under different mix proportions and curing ages. The actual reduction factor of the filling material is not a fixed constant but changes with the shear bonding state of the cement interface. This is the basis for using a dynamic reduction factor instead of a fixed reduction factor.

[0227] The calibration group velocity ratio characteristic parameters of each group of filling body calibration specimens are fitted with the actual reduction coefficients. This invention uses a power function model with physical constraints as the calibration mapping relationship. The form of the power function model is as follows:

[0228] ;

[0229] in This is the reduction factor. For the normalized group velocity ratio, and These are the lower and upper bounds of the reduction factor, respectively. The fitting index is... and The determination is based on the characteristics of the backfill material, for cemented tailings backfill. Take 0.05, Taking 0.20, the lower and upper bounds of the reduction factor are dimensionless. These are dimensionless fitting parameters. The physical constraint of the power function model is: when When the waveguide is in a free state, the reduction factor is taken as the upper bound. The limiting case where the shear bond state at the cemented interface is zero; when As the shear bond at the cemented interface decreases, the reduction coefficient decreases according to a power function and gradually approaches the lower bound. .

[0230] Using the least squares method to evaluate the parameters We perform a fitting operation, and the objective function for fitting is:

[0231] ;

[0232] in To calibrate the number of test specimen groups, For the first The weights of the groups are calculated by taking the reciprocal of the ratio of the group velocity to the standard deviation of the characteristic parameter for each of the three parallel specimens in the group. Groups with smaller standard deviations have larger weights to improve fitting accuracy.

[0233] This invention introduces the longitudinal modal group velocity increment as a correction variable based on the power function model to improve the accuracy of the calibration mapping relationship. The longitudinal modal group velocity increment reflects the change in the volumetric elastic parameters of the filling body. Under the same group velocity ratio characteristic parameter, the elastic state of the filling body is different when the longitudinal modal group velocity increment is different, and the reduction coefficient is different. The corrected calibration mapping relationship is as follows:

[0234] ;

[0235] in The longitudinal mode group velocity increment obtained from on-site monitoring. To calibrate the average longitudinal modal group velocity increment of the specimen at 28 days of age, The correction factor is set to 0.15. and All units are in m / s, and the correction term is dimensionless. The coefficient of determination is calculated after fitting. Assess the goodness of fit:

[0236] ;

[0237] in To calibrate the mapping relationship in The predicted reduction factor at the location, The coefficient of determination is the average of the actual reduction factors for each group. For a dimensionless quantity, when When the calibration mapping relationship meets the accuracy requirements, Increase the number of calibration test specimens and refit.

[0238] The dynamic reduction coefficient is obtained by looking up the calibration mapping relationship based on the group velocity ratio characteristic parameters, and the normalized group velocity ratio obtained from field monitoring is then used. and longitudinal mode group velocity increment Substituting the corrected calibration mapping relationship, the calculated result is... This is the dynamic reduction factor.

[0239] Taking 45 sets of calibration data from 9 mix proportions at 5 ages as an example, the characteristic parameters of the group velocity ratio of the calibration specimens of the filling body with a 3-day age, a sand-cement ratio of 1:8, and a mass concentration of 68%, were calibrated. calibrating uniaxial compressive strength calibrated tensile strength Actual reduction factor Calibration of group velocity ratio characteristic parameters for 28-day-old infill specimens with a sand-to-cement ratio of 1:4 and a mass concentration of 76%. calibrating uniaxial compressive strength calibrated tensile strength Actual reduction factor ; Fitting results Coefficient of determination ; the normalized group velocity ratio at a certain moment as monitored on-site Longitudinal mode group velocity increment , Dynamic reduction factor .

[0240] After obtaining the dynamic reduction coefficient, it is fed into the tensile strength inversion unit. The tensile strength inversion unit multiplies the dynamic reduction coefficient by the uniaxial compressive strength of the filling body to obtain the tensile strength of the filling body. The power function model with physical constraints ensures that the dynamic reduction coefficient has reasonable values ​​both within and outside the calibration data range. The longitudinal mode group velocity increment correction term considers the influence of the bulk elastic state of the filling body on the reduction coefficient. Weighted least squares fitting and determination coefficient evaluation ensure the fitting accuracy of the calibration mapping relationship.

[0241] The uniaxial compressive strength of the filling increases with the curing age, and the longitudinal modal group velocity value changes with the increase of the elastic modulus of the filling. Calculating the longitudinal modal group velocity increment based on the longitudinal modal group velocity value at the initial setting time can eliminate the influence of waveguide rod installation state and system parameters on the absolute value of the group velocity, and establish a stable correspondence between the longitudinal modal group velocity increment and the uniaxial compressive strength of the filling.

[0242] The guided wave receiver signal was first acquired after the initial setting of the backfill material, and the initial longitudinal mode group velocity value was calculated. The initial setting time was automatically determined by the guided wave energy change rate. After the backfill material was completed, the guided wave receiver signal was continuously acquired at 1-minute intervals, and the signal energy of the guided wave receiver signal in the coexisting frequency band at each time point was calculated. :

[0243] ;

[0244] in The signal received by the guided wave at time k is N, where N is the number of sampling points. The unit is V², and the rate of change of guided wave energy is defined as follows:

[0245] ;

[0246] in The sampling interval is expressed in seconds (s). Units are When the rate of change of guided wave energy The filling material is considered to have reached the initial setting state when the initial setting energy change rate exceeds a preset threshold for three consecutive time periods. The preset initial setting energy change rate threshold is set to 0.01. The initial freezing point is recorded as ,exist The guided wave receiver signal is acquired for the first time, and the initial longitudinal mode group velocity value is calculated according to the mode separation and group velocity calculation process. The initial longitudinal mode group velocity value is calculated at a preset characteristic frequency.

[0247] In subsequent monitoring, guided wave receiver signals were acquired at preset time intervals, and the longitudinal modal group velocity values ​​at each monitoring moment were calculated. The preset time intervals were set according to the curing stage: 2 hours within 24 hours after initial setting, 12 hours from 24 hours to 7 days, and 24 hours after 7 days. Each monitoring moment was recorded as follows: , At each monitoring time Acquire guided wave received signals and calculate longitudinal mode group velocity values The longitudinal modal group velocity increment is obtained by subtracting the initial longitudinal modal group velocity value from the longitudinal modal group velocity value at each monitoring time.

[0248] ;

[0249] Longitudinal mode group velocity increment The unit is m / s. A positive value for the longitudinal mode group velocity increment indicates that the longitudinal mode group velocity value increases with the increase of the elastic modulus of the filling body. If a negative value appears, it is marked as abnormal data and the waveguide coupling status is checked.

[0250] Calibrated specimens of the filling material were prepared with the same mix proportions as the in-situ filling material. The ash-sand ratio, mass concentration, and raw materials of the calibration specimens were consistent with those of the in-situ filling material. During the casting of the calibration specimens, waveguide rod sections of the same material and diameter as those in the in-situ filling material were embedded. The longitudinal modal group velocity value measured for the first time after the initial setting of the calibration specimens was used as a benchmark. The longitudinal modal group velocity increment of the calibration specimens was tested at different curing ages. Seven curing ages were selected: 1 day, 3 days, 7 days, 14 days, 28 days, 60 days, and 90 days. Three parallel specimens were prepared for each age. At each curing age, guided wave testing was performed first to calculate the longitudinal modal group velocity increment. Then, uniaxial compression tests were performed on the calibration specimens to obtain the calibrated uniaxial compressive strength. The uniaxial compression test applied axial pressure at a loading rate of 0.5 mm / min until the specimen failed. The calibrated uniaxial compressive strength was calculated by dividing the failure load by the bearing area of ​​the specimen.

[0251] This invention uses a hyperbolic model to establish the strength calibration relationship between the longitudinal modal group velocity increment and the uniaxial compressive strength. The form of the hyperbolic model is as follows:

[0252] ;

[0253] in This refers to uniaxial compressive strength, expressed in MPa. This represents the ultimate uniaxial compressive strength as the longitudinal mode group velocity increment approaches infinity, expressed in MPa. The longitudinal modal group velocity increment, in m / s, is given when the uniaxial compressive strength reaches half of the ultimate uniaxial compressive strength. The hyperbolic model satisfies... and Two physical boundary conditions, when hour .

[0254] Using the Levenberg-Marquardt nonlinear least squares method and We perform a fitting operation, and the objective function is:

[0255] ;

[0256] in To determine the number of data points, and The first The calibration uniaxial compressive strength and longitudinal mode group velocity increment of each calibration data point.

[0257] Since the difference between the on-site temperature and the calibration temperature can affect the hydration process of the infill, this invention introduces the Arrhenius equivalent age to correct the longitudinal modal group velocity increment for temperature. The equivalent age... The calculation formula is:

[0258] ;

[0259] in The activation energy for the hydration reaction of the filling material is taken as 33500 J / mol, and R, the gas constant, is taken as 8.314 J / (mol·K). For reference temperature, we take 293K, which is 20℃. For the first The average temperature over a time interval, expressed in Kelvin (K). For time intervals, equivalent age The unit is h. The temperature-corrected longitudinal mode group velocity increment is obtained by interpolation on the calibration curve according to the equivalent age.

[0260] Calculate the coefficient of determination after fitting. Evaluate the fitting accuracy of the intensity calibration relationship:

[0261] ;

[0262] in For strength calibration relationship in Predicted uniaxial compressive strength at the location, The average value of the calibrated uniaxial compressive strength for each group, when The strength calibration relationship is determined to meet the accuracy requirements.

[0263] The uniaxial compressive strength of the filling material was obtained by referring to the strength calibration relationship based on the longitudinal modal group velocity increment obtained from on-site monitoring. The temperature-corrected longitudinal modal group velocity increment was then used. Substituting into the hyperbola model, the calculated That is Uniaxial compressive strength of the filling material at a given time.

[0264] Taking a cemented tailings backfill with a 1:4 lime-sand ratio and a mass concentration of 72% as an example, the initial longitudinal mode group velocity value at the initial setting time... Longitudinal mode group velocity value after 28 days of curing Longitudinal mode group velocity increment The calibration test yielded , Coefficient of determination Substituting into the hyperbolic model, the uniaxial compressive strength of the filling material is obtained. The error is 3% compared with the uniaxial compression test result of 5.5 MPa for the same specimen.

[0265] After obtaining the uniaxial compressive strength of the filling material, it is fed into the tensile strength inversion unit. The tensile strength inversion unit multiplies the uniaxial compressive strength of the filling material by the dynamic reduction factor to obtain the tensile strength of the filling material. The longitudinal mode group velocity increment based on the initial setting time eliminates the influence of waveguide rod installation state and system parameters. The hyperbolic model satisfies the physical boundary conditions and has few fitting parameters. The Arrhenius equivalent age correction eliminates the influence of the difference between the field temperature and the calibration temperature on the hydration process. The three technical means work together to ensure the inversion accuracy of the uniaxial compressive strength of the filling material.

[0266] The dynamic reduction coefficient obtained from a single monitoring is subject to fluctuations due to random noise and mode separation error in the guided wave receiver signal. Directly using the single dynamic reduction coefficient to correct the uniaxial compressive strength of the filling body can lead to unreasonable jumps in the tensile strength of the filling body. Applying a sliding window weighted average to the time series of the dynamic reduction coefficient can suppress random fluctuations while preserving the trend of the reduction coefficient, thereby improving the temporal stability of the tensile strength monitoring results of the filling body.

[0267] The group velocity ratio characteristic parameters were continuously acquired multiple times according to a preset monitoring cycle, and dynamic reduction coefficients were constructed for each monitoring time. The preset monitoring cycle was set according to the curing stage: 2 hours within 24 hours after initial setting, 12 hours from 24 hours to 7 days, and 24 hours after 7 days. At each monitoring time, guided wave receiver signals were collected, and mode separation, group velocity calculation, group velocity ratio calculation, and calibration mapping relationship lookup were performed sequentially to obtain the dynamic reduction coefficients for each monitoring time. , K represents the total number of monitoring times. This is the k-th monitoring time. The dynamic reduction coefficients for each monitoring time are arranged chronologically to form a dynamic reduction coefficient time series. .

[0268] Before performing a sliding window weighted average, outlier identification and removal are performed on the dynamic reduction coefficient time series. This invention uses the median absolute deviation method to identify outliers and calculates the median of the dynamic reduction coefficient time series within the current window. Absolute deviation from the median:

[0269] ;

[0270] When the dynamic reduction factor at a certain monitoring time satisfies:

[0271] ;

[0272] When Outliers are marked as outliers, where 1.4826 is the coefficient for converting the absolute deviation of the median to the standard deviation. Outliers are not included in the sliding window weighted average but are retained in the dynamic reduction coefficient time series for subsequent analysis.

[0273] The smoothed reduction coefficient is obtained by performing a sliding window weighted average on the time series of dynamic reduction coefficients. The sliding window weighted average takes the dynamic reduction coefficient at the current monitoring time as the center, takes the dynamic reduction coefficient within a preset window length before and after the current monitoring time, assigns weights according to the time distance between the monitoring time corresponding to each dynamic reduction coefficient and the current monitoring time, and then sums them up.

[0274] This invention introduces two improvements to the sliding window weighted average: adaptive window length and Gaussian weight. The adaptive window length is adjusted according to the local rate of change of the dynamic reduction coefficient. When the local rate of change is large, the window length is shortened to track the changing trend of the reduction coefficient; when the local rate of change is small, the window length is increased to suppress noise. (The current monitoring time...) Half length of window for:

[0275] ;

[0276] in One monitoring interval is taken as the minimum window half-length. Five monitoring intervals are taken for the maximum half-length of the window. The sensitivity coefficient is set to 0.5. For the dynamic reduction factor in Local rate of change at that location The unit is , The unit is the number of monitoring intervals.

[0277] The weights for each monitoring time point within the window are calculated using a Gaussian function:

[0278] ;

[0279] in For the first in the window Each monitoring time is relative to the current monitoring time. The weight, Take the standard deviation of the Gaussian weights The closer the time interval, the greater the weight; the farther the time interval, the smaller the weight. Gaussian weights are dimensionless. The formula for calculating the sliding window weighted average is:

[0280] ;

[0281] in For Centered on and half-length is The set of monitoring times within the window that were not marked as outliers. This is the smoothing reduction factor.

[0282] When the current monitoring time is at the beginning or end of the dynamic reduction coefficient time series, there is insufficient data on one side of the window. In this case, an asymmetric window is used, and the available monitoring times on one side of the current monitoring time are used to participate in the weighted average. When there are fewer than 3 available data points, the dynamic reduction coefficient of the current monitoring time is directly taken as the smoothing reduction coefficient.

[0283] Since the tensile strength of the filling material does not decrease monotonically with the curing age, the product of the smooth reduction coefficient and the uniaxial compressive stiffness of the filling material should also satisfy the condition of monotonicity. Therefore, this invention applies a monotonic constraint correction to the smooth reduction coefficient:

[0284] ;

[0285] in The smooth reduction coefficient is the result of monotonic constraint correction. When the smooth reduction coefficient at the current monitoring time is less than the correction value at the previous monitoring time, the correction value at the previous monitoring time is taken to avoid a decline in the tensile strength of the filling material.

[0286] The tensile strength of the filling material is obtained by multiplying the smoothing reduction factor by the uniaxial compressive strength of the filling material:

[0287] ;

[0288] in for The uniaxial compressive strength of the filling material at a given time is obtained by referring to the strength calibration relationship from the longitudinal modal group velocity increment. for The tensile strength of the filling material at a given time, expressed in MPa.

[0289] To evaluate the reliability of the tensile strength of the filling material, this invention also calculates the combined uncertainty of the tensile strength of the filling material:

[0290] ;

[0291] in To smooth out the uncertainty of the reduction factor, the standard deviation of the dynamic reduction factor within the window is given. The uncertainty of the uniaxial compressive strength of the filling material is given by the fitting residual of the strength calibration relationship. The combined uncertainty of the tensile strength of the filling material is expressed in MPa. A result greater than 0.1 indicates that the tensile strength of the filling material at that moment is a low reliability result.

[0292] Taking the monitoring of backfill in a mine as an example, the preset monitoring period was 12 hours from 7 to 28 days. At 14 days, the dynamic reduction coefficients for each monitoring time point were 0.082, 0.079, 0.085, 0.081, 0.083, 0.078, 0.080, and 0.084, respectively. The median was 0.0815, the absolute deviation of the median was 0.0015, and the threshold of 3 times the standard deviation was... All data are within the threshold and have no outliers. The local change rate at the current monitoring time is 0.002 / d, and the half-length of the window is... Each monitoring interval, Gaussian weighted standard deviation The smoothing reduction coefficient is obtained by weighted averaging the monitoring intervals. Uniaxial compressive strength of the filling material at 14 days Tensile strength of filling material Combined uncertainty The relative uncertainty is 5.4%.

[0293] Once the tensile strength of the filling material is obtained, it can be compared with the design value. An early warning is issued when the tensile strength of the filling material is lower than the design value. The sliding window weighted average suppresses the random fluctuation of the dynamic reduction coefficient. The adaptive window length automatically shortens the window in the early curing stage when the reduction coefficient changes rapidly to avoid smoothing over. Gaussian weighting makes the contribution of data with a closer time distance greater than that of data with a longer time distance. Monotonic constraint correction ensures that the tensile strength of the filling material does not decrease monotonically with the curing age. The median absolute deviation outlier identification eliminates outlier data caused by signal interference. These four technical means work together to ensure the stability and rationality of the monitoring results of the tensile strength of the filling material.

[0294] The foregoing has shown and described the basic principles, main features, and advantages of the present invention. Those skilled in the art should understand that the present invention is not limited to the above embodiments. The embodiments and descriptions in the specification are merely preferred examples and are not intended to limit the invention. Various changes and modifications can be made to the invention without departing from its spirit and scope, and all such changes and modifications fall within the scope of the present invention as claimed. The scope of protection of the present invention is defined by the appended claims and their equivalents.

Claims

1. A monitoring system for the tensile strength of mine backfill based on guided wave feature recognition, characterized in that, include: The broadband guided wave excitation and acquisition unit is used to excite a broadband guided wave signal covering the frequency band where longitudinal guided wave modes and flexural guided wave modes coexist through a waveguide rod pre-embedded in the filling body, so that the longitudinal guided wave mode and flexural guided wave mode are excited at the same time, and to acquire the guided wave received signal modulated by the filling body. The mode separation unit is used to perform synchronous squeezed wavelet transform on the received waveguide signal and extract the time-frequency ridge, separate the aliased longitudinal waveguide modes from the flexural waveguide modes, and obtain the longitudinal mode arrival time series and the flexural mode arrival time series. The group velocity calculation unit is used to calculate the longitudinal mode group velocity value and the bending mode group velocity value respectively at a preset characteristic frequency within the waveguide sensitive frequency band of the filling body, based on the arrival time sequence of the longitudinal mode and the arrival time sequence of the bending mode, combined with the propagation distance of the waveguide rod. A group velocity ratio construction unit is used to calculate the ratio of the bending mode group velocity value to the longitudinal mode group velocity value based on the longitudinal mode group velocity value and the bending mode group velocity value, and to use this ratio as a group velocity ratio characteristic parameter characterizing the shear bonding state of the cementing interface between the waveguide rod and the filling body; The tensile strength inversion unit is used to construct a dynamic reduction coefficient that varies with the shear bonding state of the cement interface based on the group velocity ratio characteristic parameter, and to invert the uniaxial compressive strength of the filling body based on the longitudinal modal group velocity value. The uniaxial compressive strength of the filling body is then corrected with the dynamic reduction coefficient to obtain the tensile strength of the filling body.

2. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: The broadband guided wave signal covering the frequency band where longitudinal guided wave modes and curved guided wave modes coexist specifically includes: Based on the material and geometric parameters of the waveguide rod and the elastic parameters of the filling material, a waveguide dispersion equation is established for the waveguide rod under the constraint of the filling material. The waveguide dispersion equation is numerically solved to obtain the longitudinal waveguide mode dispersion curve and the bending waveguide mode dispersion curve. The frequency range in which the longitudinal waveguide mode dispersion curve and the bending waveguide mode dispersion curve coexist is determined. Within the frequency range, a sub-interval in which the group velocity difference between the longitudinal waveguide mode dispersion curve and the bending waveguide mode dispersion curve is greater than a preset mode resolution threshold is selected. The frequency range defined by the lower limit frequency and the upper limit frequency of the sub-interval is determined as the frequency band in which the longitudinal waveguide mode and the bending waveguide mode coexist.

3. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: The guided wave receiver signal modulated by the filling material is obtained through the following process: When a broadband guided wave signal propagates along the waveguide rod, the waveguide rod and the filling material form a coupling interface. Part of the energy of the broadband guided wave signal leaks into the filling material through the coupling interface. The bulk elastic parameters of the filling material act on the longitudinal guided wave mode through the coupling interface in a normal coupling manner. The shear bonding state of the cemented interface between the waveguide rod and the filling material acts on the bending guided wave mode through the coupling interface in a tangential coupling manner. The longitudinal and bending guided wave modes, carrying the modulation information of the filling material, continue to propagate along the waveguide rod. Receiver transducers are arranged axially at intervals on the waveguide rod. The receiver transducers convert the mechanical vibrations of the longitudinal and bending guided wave modes carrying the modulation information of the filling material into electrical signals. The electrical signals are then sequentially amplified and bandpass filtered to obtain the guided wave received signal.

4. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: The step of performing synchronous squeezing wavelet transform on the guided wave received signal and extracting the time-frequency ridge line specifically includes: A preset wavelet mother function is selected, and a continuous wavelet transform is performed on the guided wave received signal to obtain continuous wavelet transform coefficients. The instantaneous frequency at each scale is calculated based on the continuous wavelet transform coefficients. The continuous wavelet transform coefficients are synchronously squeezed and redistributed along the instantaneous frequency direction to obtain a synchronously squeezed time-frequency energy distribution. Energy peak points are searched along the time axis moment by moment on the synchronously squeezed time-frequency energy distribution. The energy peak points at adjacent moments are connected to form time-frequency ridges. The time-frequency ridge with the earliest arrival time is determined as the longitudinal mode time-frequency ridge, and the time-frequency ridge with the latest arrival time is determined as the bending mode time-frequency ridge.

5. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: The separation of aliased longitudinal waveguide modes from curved waveguide modes to obtain longitudinal mode arrival time series and curved mode arrival time series specifically includes: The guided wavelet received signal is subjected to synchronous squeezing wavelet transform to obtain a time-frequency energy distribution. Candidate time-frequency ridges are extracted from the time-frequency energy distribution. The ridge continuity is calculated for each candidate time-frequency ridge, which is the proportion of the number of sampling points of the candidate time-frequency ridge with energy values ​​greater than a preset ridge energy threshold on the time axis to the total number of sampling points of the candidate time-frequency ridge. Candidate time-frequency ridges with ridge continuity values ​​lower than the preset continuity threshold are removed. The modal energy proportion is calculated for the retained candidate time-frequency ridges, which is the sum of the energy values ​​of the candidate time-frequency ridge within a preset frequency window and the proportion of the total energy values ​​of the candidate time-frequency ridge within the preset frequency window. The proportion of total energy in the time-frequency energy distribution, combined with the arrival time sequence of the longitudinal guided wave mode and the curved guided wave mode, classifies the retained candidate time-frequency ridges into longitudinal guided wave modes and curved guided wave modes respectively. For the candidate time-frequency ridges classified as longitudinal guided wave modes, the arrival time of the longitudinal mode is picked up at each frequency point using the AIC first arrival picking algorithm. The arrival times of the longitudinal mode at each frequency point are arranged according to frequency to form a longitudinal mode arrival time sequence. For the candidate time-frequency ridges classified as curved guided wave modes, the arrival time of the curved mode is picked up in the same way to form a curved mode arrival time sequence.

6. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: The arrival time of the longitudinal mode corresponding to the preset characteristic frequency is read from the longitudinal mode arrival time series. When the preset characteristic frequency does not fall on the discrete frequency sampling point of the longitudinal mode arrival time series, the longitudinal mode arrival time is linearly interpolated between the discrete frequency sampling points adjacent to the preset characteristic frequency to obtain the longitudinal mode arrival time at the preset characteristic frequency. The arrival time of the flexural mode at the preset characteristic frequency is obtained from the flexural mode arrival time series in the same way. The pre-calibrated system delay time is subtracted from the longitudinal mode arrival time at the preset characteristic frequency to obtain the longitudinal mode net propagation time. The longitudinal mode group velocity value is obtained by dividing the waveguide rod propagation distance by the longitudinal mode net propagation time. The flexural mode net propagation time is obtained by subtracting the system delay time from the flexural mode arrival time at the preset characteristic frequency. The flexural mode group velocity value is obtained by dividing the waveguide rod propagation distance by the flexural mode net propagation time.

7. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: The ratio of the bending mode group velocity value to the longitudinal mode group velocity value is calculated based on the longitudinal mode group velocity value and the bending mode group velocity value, specifically including: Before the waveguide rod is embedded in the filling material, the waveguide rod is placed in a free state and a calibration guided wave signal in the same frequency band as the broadband guided wave signal is excited. The free state guided wave received signal is acquired, and the free state guided wave received signal is processed in the same way as the guided wave received signal to perform mode separation and group velocity calculation, to obtain the longitudinal mode free group velocity value and the bending mode free group velocity value. The ratio of the bending mode free group velocity value to the longitudinal mode free group velocity value is calculated as the reference group velocity ratio. Based on the longitudinal mode group velocity value and the bending mode group velocity value, the ratio of the bending mode group velocity value to the longitudinal mode group velocity value is calculated as the measured group velocity ratio. The measured group velocity ratio is divided by the reference group velocity ratio to obtain the normalized group velocity ratio, and the normalized group velocity ratio is used as the characteristic parameter of the group velocity ratio.

8. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: Based on the group velocity ratio characteristic parameter, a dynamic reduction coefficient is constructed that varies with the shear bond state of the cemented interface, specifically including: Multiple sets of infill calibration specimens with different mix proportions and curing ages were prepared. Broadband guided wave signals were excited for each set of infill calibration specimens, and calibration guided wave received signals were acquired. Mode separation, group velocity calculation, and group velocity ratio calculation were performed sequentially on the calibration guided wave received signals to obtain the calibration group velocity ratio characteristic parameters of each set of infill calibration specimens. Uniaxial compression tests and Brazilian splitting tests were conducted on each set of infill calibration specimens to obtain the calibration uniaxial compressive strength and calibration tensile strength. The actual reduction coefficient of each set of infill calibration specimens was obtained by dividing the calibration tensile strength by the calibration uniaxial compressive strength. The calibration group velocity ratio characteristic parameters of each set of infill calibration specimens were fitted with the actual reduction coefficients to establish a calibration mapping relationship between the group velocity ratio characteristic parameters and the reduction coefficients. The dynamic reduction coefficient was obtained by looking up the calibration mapping relationship based on the group velocity ratio characteristic parameters.

9. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: The uniaxial compressive strength of the filling material is inverted based on the longitudinal mode group velocity values, specifically including: After the initial setting of the backfill material, guided wave reception signals were collected for the first time, and the initial longitudinal modal group velocity value was calculated. In subsequent monitoring, guided wave reception signals were collected at preset time intervals, and the longitudinal modal group velocity value at each monitoring time was calculated. The longitudinal modal group velocity increment was obtained by subtracting the initial longitudinal modal group velocity value from the longitudinal modal group velocity value at each monitoring time. A calibration specimen of the backfill material with the same mix ratio as the on-site backfill material was prepared. Based on the longitudinal modal group velocity value first measured after the initial setting of the calibration specimen, the longitudinal modal group velocity increment of the calibration specimen was tested at different curing ages. A uniaxial compression test was performed on the calibration specimen to obtain the calibrated uniaxial compressive strength. A strength calibration relationship between the longitudinal modal group velocity increment and the uniaxial compressive strength was established. The uniaxial compressive strength of the backfill material was obtained by referring to the strength calibration relationship based on the longitudinal modal group velocity increment obtained from the on-site monitoring.

10. The mine backfill tensile strength monitoring system based on guided wave feature recognition according to claim 1, characterized in that: The uniaxial compressive strength of the filling material is corrected using the dynamic reduction factor to obtain the tensile strength of the filling material, specifically including: The group velocity ratio characteristic parameters are continuously acquired multiple times according to a preset monitoring cycle, and the dynamic reduction coefficients at each monitoring time are constructed. The dynamic reduction coefficients at each monitoring time are arranged by time to form a dynamic reduction coefficient time series. The dynamic reduction coefficient time series is then subjected to a sliding window weighted average to obtain a smooth reduction coefficient. The sliding window weighted average is calculated by taking the dynamic reduction coefficient at the current monitoring time as the center, taking the dynamic reduction coefficients within a preset window length before and after the current monitoring time, assigning weights according to the time distance between the monitoring time corresponding to each dynamic reduction coefficient and the current monitoring time, and then summing them up. The smooth reduction coefficient is multiplied by the uniaxial compressive strength of the filling body to obtain the tensile strength of the filling body.

Citation Information

Patent Citations

  • Waveguide acoustic monitoring method and device for strength evolution and development of tailing cemented filling body

    CN111337578A

  • Method for optimizing strength of high-temperature metal mine filling mining cemented filling body

    CN119538535A