Methods, systems, and readable media for safety evaluation of delayed hydrogen-induced cracking crack initiation
By obtaining test samples of zirconium alloy components, determining the baseline function and probability density function, and calculating the crack initiation probability by combining stress data, the safety assessment problem of delayed hydrogen-induced cracking in zirconium alloy components was solved, improving the accuracy of the assessment and the safety of nuclear reactors.
Patent Information
- Application Number
- CN202611374772.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-07
- Publication Date
- 2026-11-24
- Estimated Expiration
- 2046-09-07
AI Technical Summary
Existing technologies are insufficient to effectively assess the safety risks of delayed hydrogen-induced cracking in zirconium alloy components in nuclear reactors, which affects the operational safety of nuclear power plants.
By acquiring test samples of defective components, determining the benchmark function and probability density function, and combining the initiation stress threshold, characteristic peak stress, and stress data, the total number of overload cycles and crack initiation probability of the defective components are calculated, providing a safety assessment method and system.
This improves the accuracy of assessing delayed hydrogen-induced crack initiation in zirconium alloy components, enabling the quantification of the crack initiation probability during the service life and ensuring the safety of nuclear reactors.
Smart Images

Figure CN122863240B_ABST
Abstract
Description
Technical Field
[0001] This application relates primarily to the field of nuclear power technology, and in particular to a safety assessment method, system, and readable medium for delayed hydrogen-induced crack initiation. Background Technology
[0002] Zirconium alloys are widely used as fuel cladding and core structural components in nuclear reactors due to their low thermal neutron absorption cross-section, good resistance to high-temperature and high-pressure water corrosion, high mechanical strength, and excellent thermal conductivity. In particular, the pressure tubes of heavy water reactors are made of zirconium alloys. As containers for fuel rod bundles and coolant in heavy water reactors, the pressure tubes are a crucial component of the primary coolant circuit.
[0003] During reactor operation, zirconium alloy components continuously absorb hydrogen. Under stress, hydrogen atoms diffuse into high-stress areas and precipitate brittle hydride phases. These brittle phases fracture under stress, leading to crack initiation and propagation. This repeated process is known as DHC (Delayed Hydride Cracking). DHC is considered one of the most significant potential risks associated with zirconium alloys during service, directly impacting the operational safety of nuclear power plants.
[0004] Therefore, there is an urgent need for a safety assessment method for delayed hydrogen-induced crack initiation that can effectively evaluate the corresponding risks of components affected by DHC. Summary of the Invention
[0005] The technical problem to be solved by this application is to provide a method, system and readable medium for safety assessment of delayed hydrogen-induced crack initiation, which can improve the accuracy of assessment of DHC crack initiation in components.
[0006] To address the aforementioned technical problems, this application provides a safety assessment method for delayed hydrogen-induced crack initiation, applied to defective components of a nuclear reactor. The defective component has a real notch. The safety assessment method includes: acquiring multiple test samples corresponding to the defective component, wherein the test samples include simulated notches corresponding to the real notches; determining a baseline function and a probability density function corresponding to the defective component based on the multiple test samples, wherein the baseline function reflects the mapping relationship between different peak stresses and corresponding temperature cycle numbers, and the probability density function reflects the probability density between the same peak stress and multiple different temperature cycle numbers; acquiring the initiation stress threshold, characteristic peak stress, and stress data within the target service life of the defective component; determining the total number of overload cycles of the defective component based on the stress data and the initiation stress threshold; and determining the crack initiation probability of the defective component based on the characteristic peak stress, total number of overload cycles, the baseline function, and the probability density function.
[0007] Optionally, the stress data includes multiple peak stresses corresponding to multiple temperature cycles. The step of determining the total number of overloads of the defective component based on the stress data and the effective stress threshold further includes: for each temperature cycle corresponding to the stress data, if the peak stress corresponding to the temperature cycle is greater than the effective stress threshold, then the temperature cycle is taken as an effective temperature cycle; the total number of effective temperature cycles is taken as the total number of overloads.
[0008] Optionally, the effective stress threshold is the critical stress at which the material of the defective component undergoes hydride redirection.
[0009] Optionally, the step of determining the crack initiation probability of a defective component based on the characteristic peak stress, total number of overload cycles, reference function, and probability density function further includes: determining the average number of temperature cycles based on the characteristic peak stress and reference function; and determining the crack initiation probability based on the average number of temperature cycles, total number of overload cycles, and probability density function.
[0010] Optionally, the probability density function is expressed as: In the formula Based on the benchmark function and peak stress A set number of temperature cycles, Standard deviation, To achieve peak stress Number of temperature cycles The probability density.
[0011] Optionally, the expression for calculating the crack initiation probability is: In the formula This represents the probability of crack initiation. Let be the cumulative distribution function corresponding to the probability density function. Total number of overload cycles This represents the average number of temperature cycles. The standard deviation is denoted as .
[0012] Optionally, the probability density function is expressed as: In the formula For Weibull modulus, Based on the benchmark function and peak stress A set number of temperature cycles, To achieve peak stress Number of temperature cycles The probability density.
[0013] Optionally, the expression for calculating the crack initiation probability is: In the formula This represents the probability of crack initiation. Total number of overload cycles This represents the average number of temperature cycles.
[0014] Optionally, the step of obtaining multiple test samples corresponding to the defective component further includes: obtaining an initial sample corresponding to the defective component; hydrogenating the initial sample to obtain a hydrogenated sample; and setting a simulated notch on the hydrogenated sample according to the actual notch to obtain a test sample.
[0015] Optionally, the step of determining the baseline function and probability density function corresponding to the defective component based on multiple test samples further includes: applying different constant loads to each test sample; determining the peak stress corresponding to the constant load for each test sample; determining the number of temperature cycles corresponding to the delayed hydrogen-induced crack initiation for each test sample based on multiple temperature cycles; and determining the baseline function based on the peak stresses corresponding to multiple test samples and the number of temperature cycles corresponding to each peak stress.
[0016] Optionally, the step of determining the baseline function and probability density function corresponding to the defective component based on multiple test samples further includes: applying the same constant load to each test sample; determining the peak stress corresponding to the constant load; determining the number of temperature cycles corresponding to the delayed hydrogen-induced crack initiation of each test sample based on multiple temperature cycles; and determining the probability density function based on the peak stress and the number of temperature cycles corresponding to multiple test samples.
[0017] Optionally, the safety assessment method further includes: if the crack initiation probability is less than or equal to the risk probability threshold, the safety assessment result is determined to be safe; if the crack initiation probability is greater than the risk probability threshold, the safety assessment result is determined to be risky.
[0018] To address the aforementioned technical problems, this application provides a safety assessment system for delayed hydrogen-induced crack initiation, comprising: a memory for storing instructions executable by a processor; and a processor for executing the instructions to implement the aforementioned safety assessment method for delayed hydrogen-induced crack initiation.
[0019] To address the aforementioned technical problems, this application provides a computer-readable medium storing computer program code, which, when executed by a processor, implements the aforementioned safety assessment method for delayed hydrogen-induced crack initiation.
[0020] Compared with existing technologies, this application has the following advantages: It effectively obtains the relationship between the peak stress and the number of temperature cycles during DHC crack initiation in defective components by using test samples containing simulated notches, thus obtaining the baseline function and probability density function. Based on this, the total number of DHC temperature cycles, i.e., the total number of overloads, is effectively determined by using the effective stress threshold. Therefore, by using the total number of overloads, characteristic peak stress, baseline function, and probability density function, the probability of DHC crack initiation under characteristic peak stress within the range not exceeding the total number of overloads is effectively determined, i.e., the crack initiation probability. This allows for an effective assessment of the probability that a defective component will experience DHC crack initiation during its entire service life, thus affecting nuclear reactor safety. Attached Figure Description
[0021] The accompanying drawings are included to provide a further understanding of this application; they are incorporated into and constitute a part of this application. The drawings illustrate embodiments of this application and, together with this specification, serve to explain the principles of this application. In the drawings: Figure 1 This is a flowchart illustrating a safety assessment method for delayed hydrogen-induced crack initiation according to an embodiment of this application. Figure 2 yes Figure 1 A flowchart illustrating the sub-steps of step S1 in the illustrated embodiment; Figure 3 yes Figure 1 A flowchart illustrating the sub-steps of step S2 in the illustrated embodiment; Figure 4 yes Figure 1 A schematic diagram of the temperature curves corresponding to the three consecutive temperature cycles experienced by the defective component in the illustrated embodiment. Figure 5 yes Figure 1 A flowchart illustrating the sub-steps of step S2 in the illustrated embodiment; Figure 6 yes Figure 1 A flowchart illustrating the sub-steps of step S4 in the illustrated embodiment; Figure 7 yes Figure 1 A flowchart illustrating the sub-steps of step S5 in the illustrated embodiment. Figure 8 This is a flowchart illustrating a safety assessment method for delayed hydrogen-induced crack initiation according to an embodiment of this application. Figure 9 This is a schematic diagram of a safety assessment system for delayed hydrogen-induced crack initiation according to an embodiment of this application. Detailed Implementation
[0022] To more clearly illustrate the technical solutions of the embodiments of this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are merely some examples or embodiments of this application. For those skilled in the art, these drawings can be applied to other similar scenarios without creative effort. Unless obvious from the context or otherwise specified, the same reference numerals in the drawings represent the same structures or operations.
[0023] As indicated in this application and claims, unless the context clearly indicates otherwise, the words "a," "an," "an," and / or "the" are not specifically singular and may include plural forms. Generally speaking, the terms "comprising" and "including" only indicate the inclusion of explicitly identified steps and elements, which do not constitute an exclusive list, and the method or apparatus may also include other steps or elements.
[0024] Unless otherwise specifically stated, the relative arrangement, numerical expressions, and values of the components and steps described in these embodiments do not limit the scope of this application. It should also be understood that, for ease of description, the dimensions of the various parts shown in the drawings are not drawn to actual scale. Techniques, methods, and devices known to those skilled in the art may not be discussed in detail, but where appropriate, such techniques, methods, and devices should be considered part of the specification. In all examples shown and discussed herein, any specific values should be interpreted as merely exemplary and not as limitations. Therefore, other examples of exemplary embodiments may have different values. It should be noted that similar reference numerals and letters in the following drawings denote similar items; therefore, once an item is defined in one drawing, it need not be further discussed in subsequent drawings.
[0025] In the description of this application, it should be understood that the orientation or positional relationship indicated by directional terms such as "front, back, up, down, left, right", "horizontal, vertical, horizontal" and "top, bottom" is usually based on the orientation or positional relationship shown in the accompanying drawings, and is only for the convenience of describing this application and simplifying the description. Unless otherwise stated, these directional terms do not indicate or imply that the device or element referred to must have a specific orientation or be constructed and operated in a specific orientation, and therefore should not be construed as a limitation on the scope of protection of this application; the directional terms "inner" and "outer" refer to the inner and outer contours relative to the outline of each component itself.
[0026] For ease of description, spatial relative terms such as "above," "on top of," "on the upper surface of," "above," etc., are used herein to describe the spatial positional relationship of a device or feature as shown in the figures to other devices or features. It should be understood that spatial relative terms are intended to encompass different orientations in use or operation beyond the orientation of the device as described in the figures. For example, if the device in the figures were inverted, a device described as "above" or "on top of" other devices or structures would subsequently be positioned as "below" or "under" other devices or structures. Thus, the exemplary term "above" can include both "above" and "below." The device may also be positioned in other different ways (rotated 90 degrees or in other orientations), and the spatial relative descriptions used herein will be interpreted accordingly.
[0027] Furthermore, it should be noted that the use of terms such as "first" and "second" to define components is merely for the purpose of distinguishing the corresponding components. Unless otherwise stated, these terms have no special meaning and therefore should not be construed as limiting the scope of protection of this application. In addition, although the terminology used in this application is selected from commonly known and used terms, some terms mentioned in this application's specification may have been chosen by the applicant according to his or her judgment, and their detailed meanings are explained in the relevant sections of this description. Moreover, this application should be understood not only through the actual terms used, but also through the meaning implied by each term.
[0028] Flowcharts are used in this application to illustrate the operations performed by the system according to embodiments of this application. It should be understood that the preceding or following operations are not necessarily performed in exact order. Instead, various steps can be processed in reverse order or simultaneously. Furthermore, other operations may be added to these processes, or one or more steps may be removed from these processes.
[0029] Reference Figure 1 One embodiment of this application proposes a safety assessment method 100 for delayed hydrogen-induced crack initiation (hereinafter referred to as safety assessment method 100). This safety assessment method 100 is applied to defective components of a nuclear reactor, wherein the defective component has a real notch. In this embodiment, the material of the defective component includes a zirconium alloy, thereby employing safety assessment method 100 to assess the possibility that the defective component may be damaged by DHC initiation, leading to safety problems. It should be noted that this application does not limit the object of assessment to include zirconium alloys; in some embodiments, the defective component may include titanium alloys, niobium alloys, or vanadium alloys.
[0030] Continue to refer to Figure 1The safety assessment method 100 includes the following steps. Step S1 is to obtain multiple test samples corresponding to the defective component. The test samples include simulated notches corresponding to actual notches. Further reference... Figure 2 Step S1 includes the following sub-steps. Step S11 is to obtain an initial sample corresponding to the defective component. In this embodiment, the defective component is a pressure tube, and correspondingly, a strip sample is cut along the axial direction on the pressure tube as the initial sample. It should be noted that this application does not limit the specific type of defective component; in some embodiments, the defective component can be a support component in a nuclear reactor. In addition, this application does not limit the method of obtaining the initial sample; in some embodiments, a strip sample is cut along the circumferential direction on the pressure tube as the initial sample. Step S12 is to perform hydrogenation treatment on the initial sample to obtain a hydrogenated sample. In this embodiment, firstly, a layer of zirconium hydride (ZrH2) is deposited on the surface of the initial sample using an electrochemical method, and then annealed under vacuum conditions to uniformly diffuse the hydrogen content in the sample to the target level, so as to simulate the actual hydride distribution after the defective component corresponding to the zirconium alloy is used in a nuclear reactor. The holding temperature range in the annealing treatment includes 350°C to 400°C, and the holding time ranges from 2 hours to 4 hours. In this embodiment, the target level ranges from 50 wppm to 150 wppm. Step S13 involves setting a simulated notch on the hydrogenated sample based on the actual notch to obtain the test sample. It should be noted that the relevant techniques use the basic assumption of an infinitely sharp crack tip, with the DHC initiation stress intensity factor threshold value K as the reference. IH For performance indicators, DHC crack initiation is analyzed. However, in actual nuclear reactor operation, DHC crack initiation often occurs at blunt defects on the zirconium alloy surface caused by scratches, wear, etc. Therefore, the evaluation results obtained by the above-mentioned related technologies differ from the actual situation. In this embodiment, a simulated notch corresponds to a blunt defect, so that the test sample can accurately simulate the real blunt notch that exists in the defective component in actual use. Specifically, in this embodiment, the root of the simulated notch has a geometric radius, thereby forming a blunt defect. The geometric radius ranges from 24μm to 36μm. For example, in step S13, according to the actual damage form of the defective component, such as scratches, wear, etc., a V-shaped diamond cutting wheel is used to process the inner or outer wall of the hydrogenated sample to form a V-shaped notch with a root radius of 30μm as a simulated notch.
[0031] Continue to refer to Figure 1 Step S2 involves determining the baseline function and probability density function corresponding to the defective component based on multiple test samples. The baseline function reflects the mapping relationship between different peak stresses and their corresponding temperature cycle numbers, while the probability density function reflects the probability density between the same peak stress and multiple different temperature cycle numbers. Further reference... Figure 3Step S2 includes the following sub-steps. Step S211 is to apply a different constant load to each test sample. In this embodiment, one end of the test sample is fixed and a constant load is applied to the other end, thereby forming a cantilever beam stress state for the test sample. It should be noted that this application does not limit the specific way of applying the constant load to the test sample. In some embodiments, the test sample is placed in a three-point bending stress state to apply a constant load to the test sample. Step S212 is to determine the peak stress corresponding to the constant load for each test sample. In this embodiment, the root peak stress of the simulated notch in the test sample is determined by the finite element method, and the root peak stress is taken as the peak stress of the test sample under the corresponding constant load. Step S213 is to determine the number of temperature cycles corresponding to the delayed hydrogen-induced crack initiation of each test sample based on multiple temperature cycles. In this embodiment, temperature cycling is used to simulate the periodic temperature changes of defective components during operation in a nuclear reactor. For example, Figure 4 This is a schematic diagram of the temperature curves corresponding to three consecutive temperature cycles experienced by the defective component. For example... Figure 4 As shown, the horizontal axis represents time, in hours (h). The vertical axis represents temperature, in degrees Celsius (°C). Figure 4In each temperature cycle, the ambient temperature of the defective component is increased from room temperature (corresponding to the room temperature line) to above the temperature corresponding to the TSSD (Terminal Solid Solubility for Dissolution) temperature line and maintained at this maximum temperature for a period of time. Then, the temperature is decreased from this maximum temperature to the test temperature corresponding to the test temperature line and maintained at this test temperature for a period of time. Finally, the temperature is decreased from the test temperature to room temperature, thus completing one real temperature cycle. In the above real temperature cycle, the maximum temperature can be 5°C to 10°C higher than the temperature corresponding to the TSSD temperature line. Furthermore, maintaining the maximum temperature for a certain period allows the hydride to dissolve. Correspondingly, maintaining the test temperature for a certain period allows the hydride sufficient time and temperature conditions for the DHC cracking-related reaction to occur. Therefore, in this embodiment, the temperature cycle setting parameters for the test sample are determined based on the lower limit temperature and upper limit temperature of the real temperature cycle corresponding to the defective component, as well as the real temperature change rate. These setting parameters include the simulated lower limit temperature, the simulated upper limit temperature, and the simulated temperature change rate. In this embodiment, the total number of temperature cycles experienced by the test sample is continuously updated. When the test sample happens to experience DHC initiation cracking, the total number of temperature cycles is the temperature cycle count. Thus, the number of temperature cycles required for delayed hydrogen-induced cracking initiation at the corresponding peak stress is determined. Step S214 involves determining a benchmark function based on the peak stresses corresponding to multiple test samples and the number of temperature cycles corresponding to each peak stress. In this embodiment, each peak stress and its corresponding number of temperature cycles are treated as a data point, and the benchmark function is determined by curve fitting based on multiple data points. The expression for the benchmark function is: In the formula Peak stress, The value represents the number of temperature cycles. It is understood that this embodiment does not limit the specific form of the reference function; in some embodiments, the function form is a logarithmic function, and in others, it is a power function.
[0032] Continue to refer to Figure 5Step S2 includes the following sub-steps: Step S221 is to apply the same constant load to each test sample. Step S222 is to determine the peak stress corresponding to the constant load. It is understood that since the same constant load is applied to each test sample, each test sample corresponds to the same peak stress in step S222. Step S223 is to determine the number of temperature cycles corresponding to the delayed hydrogen-induced crack initiation of each test sample based on multiple temperature cycles. It is understood that temperature cycles and the number of temperature cycles have been explained in detail above and will not be repeated here. Step S224 is to determine the probability density function based on the peak stress and the number of temperature cycles corresponding to multiple test samples. In this embodiment, the probability density function is determined based on a Gaussian normal distribution, and the expression of the probability density function in this embodiment is: , In the formula Based on the aforementioned benchmark function and peak stress A set number of temperature cycles, Standard deviation, To achieve peak stress Number of temperature cycles The probability density is calculated. The standard deviation is determined based on the number of temperature cycles for each test sample. In this embodiment, the input to the benchmark function is the number of temperature cycles, and the corresponding output is the peak stress. Based on this, It is the inverse function of the benchmark function, that is, the function The input is the peak stress, and the corresponding output is the number of temperature cycles. Therefore, Peak stress The corresponding number of temperature cycles. In other words, this embodiment determines the baseline correspondence between each peak stress and the number of temperature cycles based on a baseline function. It can be understood that in some embodiments, the input to the baseline function is the peak stress, and the corresponding output is the number of temperature cycles. This serves as the baseline function.
[0033] Continue to refer to Figure 1 Step S3 involves acquiring the initiation stress threshold, characteristic peak stress, and stress data within the target service life of the defective component. In this embodiment, the stress data includes multiple peak stresses corresponding to multiple temperature cycles. Furthermore, the stress data in this embodiment includes peak stresses corresponding to multiple time points; thus, multiple peak stresses corresponding to each temperature cycle can be determined based on the start and end times of each temperature cycle. It should be noted that this application does not limit the method of acquiring stress data. In some embodiments, stress data can be acquired through real experiments, and in some embodiments, stress data can be acquired through finite element numerical simulation. In this embodiment, the initiation stress threshold is the critical stress at which the material of the defective component undergoes hydride redirection.
[0034] Continue to refer to Figure 1 Step S4 involves determining the total number of overload cycles for the defective component based on stress data and the effective stress threshold. Further reference... Figure 6 Step S4 includes the following sub-steps. Step S41: For each temperature cycle corresponding to the stress data, if the peak stress of the temperature cycle is greater than the effective stress threshold, then the temperature cycle is considered an effective temperature cycle. It should be noted that zirconium alloys can generate hydride redirection within a certain temperature range, which may then trigger delayed hydrogen-induced cracking. Therefore, in this embodiment, the peak stress in each temperature cycle is judged according to the effective stress threshold, thereby selecting the temperature cycles that generate hydride redirection as effective temperature cycles that can trigger delayed hydrogen-induced cracking. Step S42: The total number of effective temperature cycles is taken as the total number of overload cycles. It can be understood that since the stress data corresponds to the target service life of the defective component, the total number of overload cycles can reflect the total number of temperature cycles in which hydride redirection occurs in the defective component within the target service life.
[0035] Continue to refer to Figure 1 Step S5 involves determining the crack initiation probability of the defective component based on the characteristic peak stress, total number of overload cycles, benchmark function, and probability density function. Further reference... Figure 7 Step S5 includes the following sub-steps. Step S51 is to determine the average number of temperature cycles based on the characteristic peak stress and the reference function. It is understood that in this embodiment, the reference function reflects the unique number of temperature cycles corresponding to each different peak stress. Therefore, by substituting the characteristic peak stress into the reference function, the number of temperature cycles corresponding to that characteristic peak stress can be determined, and this number of temperature cycles is used as the average number of temperature cycles. In this embodiment, the characteristic peak stress is the maximum value of the peak stress of the defective component during the target service life. Step S52 is to determine the crack initiation probability based on the average number of temperature cycles, the total number of overloads, and the probability density function. The expression for calculating the crack initiation probability in this embodiment is: , In the formula This represents the probability of crack initiation. Let be the cumulative distribution function corresponding to the probability density function. Total number of overload cycles This represents the average number of temperature cycles. The standard deviation is given. Understandably, in this embodiment, the maximum peak stress, i.e., the characteristic peak stress, is used to determine the reference temperature cycle number for DHC crack initiation in the defective component. Then, the probability of DHC crack initiation under the total overload cycles is determined through the cumulative distribution function, thus obtaining a conservative probability value for DHC crack initiation in the defective component. It should be noted that this application does not limit the method of taking the characteristic peak stress. In some embodiments, the characteristic peak stress can be 80% of the maximum peak stress of the defective component during the target service life, thereby ensuring that the corresponding crack initiation probability is not overly conservative.
[0036] It should be noted that this application does not limit the specific form of the probability density function; in some embodiments, the expression of the probability density function can be: In the formula For Weibull modulus, Based on the aforementioned benchmark function and peak stress The determined number of temperature cycles, To achieve peak stress Number of temperature cycles The probability density of crack initiation. Correspondingly, the expression for calculating the crack initiation probability can be: In the formula This represents the probability of crack initiation. Total number of overload cycles This represents the average number of temperature cycles.
[0037] In this embodiment, the safety assessment method 100 also determines the safety assessment result based on the crack initiation probability. Specifically, refer to... Figure 8 The safety assessment method 100 in this embodiment further includes the following steps. Step S6 is to determine the safety assessment result as safe if the crack initiation probability is less than or equal to a risk probability threshold. In this embodiment, the risk probability threshold is determined according to nuclear safety specifications or nuclear safety design requirements. For example, the risk probability threshold can be 10. -6 Step S7 is to determine the safety assessment result as having a risk if the crack initiation probability is greater than the risk probability threshold. Understandably, if the safety assessment result indicates a risk, adjustments are made to the defective component to improve its reliability in the nuclear reactor, thereby improving the reactor's safety. These adjustments include one or more of the following: adjusting the structural design of the defective component, adjusting the corresponding operating parameters of the defective component, and adjusting the material of the defective component.
[0038] During the determination of the peak stress at which DHC cracks initiate, the inventors discovered that as the number of temperature cycles increases, the length of the hydride at the root of the true notch corresponding to the blunt defect gradually increases until cracking occurs. Furthermore, the length of the hydride at crack initiation is related to the material dispersion and has no definite critical value. Therefore, to describe the true value of the peak stress corresponding to DHC crack initiation, it is necessary to simplify the initiation process of DHC at the true notch into an accumulative, probabilistic cyclic damage problem. Thus, in this embodiment, a baseline relationship, or baseline function, between the peak stress at which DHC cracks initiate and the number of temperature cycles was determined based on multiple test samples. Based on this, by setting a characteristic peak stress and the total number of overloads, the complex service stress-time history relationship of the defective component is simplified into a quantifiable crack initiation probability. In other words, this embodiment establishes a baseline relationship between the peak stress of the defective component under cyclic loading and the number of temperature cycles, and incorporates the statistical dispersion of the crack initiation resistance of the defective component into a probabilistic framework. By comparing the effective number of overloads (i.e., the total number of overloads) under service conditions, the crack initiation probability of the defective component for DHC crack initiation is quantitatively evaluated.
[0039] The safety assessment method 100 of this embodiment is based on the role of stress in DHC crack initiation. Specifically, in the relevant evaluation criteria based on stress intensity factors, the cause of DHC crack initiation is attributed to the brittle fracture of hydrides at the crack tip. However, the inventors discovered that in actual DHC occurrence, when the stress peak value exceeds a critical value, hydride redirection occurs first, followed by brittle fracture of hydrides. In other words, only when hydrides are redirected will they precipitate and grow in a direction unfavorable to crack initiation; otherwise, no cumulative effect occurs. Therefore, in this embodiment, the stress criterion is used as the DHC crack initiation mechanism, i.e., an initiation stress threshold is set, thereby making the calculated crack initiation probability more conservative. In addition, this embodiment simulates the DHC initiation process of defective components under real service conditions through characteristic peak stress, thus not relying on the assumptions of infinitely sharp cracks and constant loads in related technologies, and thus obtaining a crack initiation probability that is more in line with reality.
[0040] The safety assessment method 100 of this embodiment, compared with the method of comparing the peak stress at which a single crack is initiated in related technologies, makes full use of material properties and load history. Specifically, this embodiment organically combines material resistance and environmental load through two key data points: a benchmark function and the total number of overload cycles, thereby making the assessment results more comprehensive and accurate. Compared with related existing methods, it fully considers the relationship between the peak stress at which DHC cracks and the number of temperature cycles. Therefore, the safety assessment method 100 of this embodiment can be based on mature DHC testing technology and finite element analysis, making it easy to implement under laboratory conditions, and the crack initiation probability can be directly linked to the acceptable risk threshold, i.e., the risk probability threshold, thus facilitating engineering applications and standard setting.
[0041] An embodiment of this application also proposes a method such as Figure 9 The safety assessment system 200 for delayed hydrogen-induced crack initiation (hereinafter referred to as safety assessment system 200) is shown. Figure 9 The security assessment system 200 may include an internal communication bus 21, a processor 22, a read-only memory (ROM) 23, a random access memory (RAM) 24, and a communication port 25. When applied to a personal computer, the security assessment system 200 may also include a hard disk 26.
[0042] The internal communication bus 21 enables data communication between components of the security assessment system 200. The processor 22 can perform judgments and issue prompts. In some embodiments, the processor 22 may consist of one or more processors. The communication port 25 enables data communication between the security assessment system 200 and external systems. In some embodiments, the security assessment system 200 can send and receive information and data from a network via the communication port 25.
[0043] The security assessment system 200 may also include different types of program storage units and data storage units, such as a hard disk 26, read-only memory (ROM) 23, and random access memory (RAM) 24, capable of storing various data files used for computer processing and / or communication, as well as possible program instructions executed by the processor 22. The processor executes these instructions to implement the main part of the method. The results of the processor processing are transmitted to the user equipment via a communication port and displayed on the user interface.
[0044] In addition, this application also proposes a computer-readable medium storing computer program code, which, when executed by a processor, implements the aforementioned safety assessment method for delayed hydrogen-induced crack initiation.
[0045] The basic concepts have been described above. Obviously, for those skilled in the art, the above disclosure is merely illustrative and does not constitute a limitation of this application. Although not explicitly stated herein, those skilled in the art may make various modifications, improvements, and corrections to this application. Such modifications, improvements, and corrections are suggested in this application, and therefore remain within the spirit and scope of the exemplary embodiments of this application.
[0046] Furthermore, this application uses specific terms to describe embodiments of the application. For example, "an embodiment," "one embodiment," and / or "some embodiments" refer to a particular feature, structure, or characteristic related to at least one embodiment of the application. Therefore, it should be emphasized and noted that "an embodiment," "one embodiment," or "an alternative embodiment" mentioned twice or more in different locations in this specification do not necessarily refer to the same embodiment. In addition, certain features, structures, or characteristics in one or more embodiments of the application can be appropriately combined.
[0047] Similarly, it should be noted that, in order to simplify the description of the present application and thus aid in the understanding of one or more embodiments, the foregoing description of the embodiments of the present application sometimes combines multiple features into a single embodiment, drawing, or description thereof. However, this disclosure method does not imply that the subject matter of the present application requires more features than those mentioned in the claims. In fact, the embodiments contain fewer features than all the features of the single embodiments disclosed above.
[0048] In some embodiments, numbers describing the quantity of components and attributes are used. It should be understood that such numbers used in the description of embodiments are modified in some examples with the terms "approximately," "approximately," or "generally." Unless otherwise stated, "approximately," "approximately," or "generally" indicates that the numbers are allowed to vary by ±20%. Accordingly, in some embodiments, the numerical parameters used in the specification and claims are approximate values, which may be changed depending on the characteristics required by individual embodiments. In some embodiments, numerical parameters should take into account specified significant digits and employ a general method of digit reservation. Although the numerical ranges and parameters used to confirm their breadth of scope in some embodiments of this application are approximate values, in specific embodiments, such values are set as precisely as feasible.
[0049] Some aspects of this application can be executed entirely by hardware, entirely by software (including firmware, resident software, microcode, etc.), or by a combination of hardware and software. The aforementioned hardware or software may be referred to as a "data block," "module," "engine," "unit," "component," or "system." The processor may be one or more application-specific integrated circuits (ASICs), digital signal processors (DSPs), digital signal processing devices (DAPDs), programmable logic devices (PLDs), field-programmable gate arrays (FPGAs), processors, controllers, microcontrollers, microprocessors, or combinations thereof. Furthermore, aspects of this application may manifest as computer products residing in one or more computer-readable media, including computer-readable program code. For example, computer-readable media may include, but are not limited to, magnetic storage devices (e.g., hard disks, floppy disks, magnetic tapes, etc.), optical discs (e.g., compressed CDs, digital multifunction DVDs, etc.), smart cards, and flash memory devices (e.g., cards, sticks, key drives, etc.).
[0050] A computer-readable medium may contain a propagated data signal containing computer program code, for example, on baseband or as part of a carrier wave. This propagated signal may take various forms, including electromagnetic, optical, and so on, or suitable combinations thereof. A computer-readable medium can be any computer-readable medium other than a computer-readable storage medium, which can be connected to an instruction execution system, apparatus, or device to enable communication, propagation, or transmission of a program for use. The program code located on the computer-readable medium can be propagated through any suitable medium, including radio, cable, fiber optic cable, radio frequency signals, or similar media, or any combination of the above media.
[0051] Although this application has been described with reference to specific embodiments, those skilled in the art should recognize that the above embodiments are only used to illustrate this application, and various equivalent changes or substitutions can be made without departing from the spirit of this application. Therefore, any changes or modifications to the above embodiments within the essential spirit of this application will fall within the scope of the claims of this application.
Claims
1. A safety assessment method for delayed hydrogen-induced crack initiation, characterized in that, A defective component applied to a nuclear reactor, the defective component having a real notch, the safety assessment method comprising: Obtain multiple test samples corresponding to the defective component, wherein the test samples include simulated notches corresponding to the actual notches; Based on multiple test samples, a baseline function and a probability density function corresponding to the defective component are determined. The baseline function is used to reflect the mapping relationship between different peak stresses and the corresponding number of temperature cycles, and the probability density function is used to reflect the probability density between the same peak stress and multiple different number of temperature cycles. Obtain the stress threshold, characteristic peak stress, and stress data of the defective component within the target service life; Based on the stress data and the effective stress threshold, the total number of overloads of the defective component is determined; The crack initiation probability of the defective component is determined based on the characteristic peak stress, the total number of overload cycles, the baseline function, and the probability density function. Wherein, the effective stress threshold is the critical stress at which the material of the defective component undergoes hydride redirection, and the characteristic peak stress is the maximum value of the peak stress of the defective component during the target service cycle.
2. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 1, characterized in that, The stress data includes multiple peak stresses corresponding to multiple temperature cycles. The step of determining the total number of overload cycles of the defective component based on the stress data and the effective stress threshold further includes: For each temperature cycle corresponding to the stress data, if the peak stress corresponding to the temperature cycle is greater than the effective stress threshold, then the temperature cycle is regarded as an effective temperature cycle. The total number of effective temperature cycles is taken as the total number of overload cycles.
3. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 1, characterized in that, The step of determining the crack initiation probability of the defective component based on the characteristic peak stress, the total number of overload cycles, the benchmark function, and the probability density function further includes: The average number of temperature cycles is determined based on the characteristic peak stress and the reference function. The crack initiation probability is determined based on the average number of temperature cycles, the total number of overload cycles, and the probability density function.
4. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 1, characterized in that, The expression for the probability density function is: , In the formula Based on the aforementioned benchmark function and peak stress The determined number of temperature cycles, Standard deviation, To achieve peak stress Number of temperature cycles The probability density.
5. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 4, characterized in that, The formula for calculating the crack initiation probability is: , In the formula The crack initiation probability is [the value of the crack]. The cumulative distribution function corresponding to the probability density function. The total number of overloads, This represents the average number of temperature cycles. The standard deviation is denoted as .
6. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 1, characterized in that, The expression for the probability density function is: , In the formula For Weibull modulus, Based on the aforementioned benchmark function and peak stress The determined number of temperature cycles, To achieve peak stress Number of temperature cycles The probability density.
7. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 6, characterized in that, The formula for calculating the crack initiation probability is: , In the formula The crack initiation probability is [the value of the crack]. The total number of overloads, This represents the average number of temperature cycles.
8. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 1, characterized in that, The step of obtaining multiple test samples corresponding to the defective component further includes: Obtain the initial sample corresponding to the defective component; The initial sample was subjected to hydrogenation treatment to obtain a hydrogenated sample; The simulated notch is set on the hydrogenated sample according to the actual notch to obtain the test sample.
9. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 1, characterized in that, The step of determining the benchmark function and probability density function corresponding to the defective component based on multiple test samples further includes: A different constant load was applied to each of the test samples; For each of the test samples, determine the peak stress corresponding to the constant load; For each of the test samples, the number of temperature cycles corresponding to the occurrence of delayed hydrogen-induced crack initiation is determined based on multiple temperature cycles. The benchmark function is determined based on the peak stress corresponding to the multiple test samples and the number of temperature cycles corresponding to each peak stress.
10. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 1, characterized in that, The step of determining the benchmark function and probability density function corresponding to the defective component based on multiple test samples further includes: The same constant load was applied to each of the test samples; Determine the peak stress corresponding to the constant load; For each of the test samples, the number of temperature cycles corresponding to the occurrence of delayed hydrogen-induced crack initiation is determined based on multiple temperature cycles. The probability density function is determined based on the peak stress and the number of temperature cycles corresponding to the multiple test samples.
11. The safety assessment method for delayed hydrogen-induced crack initiation as described in claim 1, characterized in that, The security assessment method also includes: If the crack initiation probability is less than or equal to the risk probability threshold, the safety assessment result is determined to be safe. If the crack initiation probability is greater than the risk probability threshold, then the safety assessment result is determined to be risky.
12. A safety assessment system for delayed hydrogen-induced crack initiation, characterized in that, include: Memory is used to store instructions that can be executed by the processor; as well as A processor for executing the instructions to implement the safety assessment method for delayed hydrogen-induced crack initiation as described in any one of claims 1-11.
13. A computer-readable medium storing computer program code, characterized in that, The computer program code, when executed by a processor, implements the safety assessment method for delayed hydrogen-induced crack initiation as described in any one of claims 1-11.
Citation Information
Patent Citations
Zirconium alloy pressure pipe material corrosion hydrogen charging system and method
CN115950811A
Method for evaluating fracture toughness of metal material in hydrogen environment
CN121994595A