A concrete micro-damage core and ultrasonic phased array complementary verification detection method

By generating a three-dimensional ultrasonic image on the concrete surface and forming an acoustic beacon source, combined with sensor array monitoring and spectral feature matching, the uncertainty of the verification position caused by drill bit deflection was solved, and precise complementary verification of ultrasonic detection and drill core was achieved, thus improving the reliability of the detection results.

CN122882610BActive Publication Date: 2026-11-24SICHUAN VOCATIONAL & TECHN COLLEGE OF COMM
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202611404217.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-09-10
Publication Date
2026-11-24
Estimated Expiration
2046-09-10

AI Technical Summary

Technical Problem

In the existing technology, ultrasonic testing and core sampling lack reliable complementary verification methods in concrete defect detection. Drill bit deviation leads to uncertainty in the verification position, making it difficult to ensure that the core sample contains the abnormal area detected by ultrasonic testing.

Method used

An ultrasonic phased array probe is deployed on the concrete surface to generate a three-dimensional ultrasonic image to identify abnormal target areas and delineate the center point, forming an acoustic beacon source. During drilling, signal changes are monitored through a sensor array, and offset feature sequences are recorded to ensure that the drill bit is aligned with the target area. The extracted core samples are then subjected to spectral feature matching and acoustic impedance comparison to achieve accurate verification.

Benefits of technology

It enables real-time tracking of the drill bit's position inside concrete, ensuring consistency between the core sample and ultrasonic testing results, and improving the credibility and accuracy of the verification.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122882610B_ABST
    Figure CN122882610B_ABST
Patent Text Reader

Abstract

The application belongs to the technical field of concrete detection, and specifically discloses a kind of concrete micro-damage core and ultrasonic phased array complementary verification detection method, the center point of abnormal target area is circled to the concrete to be measured by ultrasonic phased array imaging, and the acoustic beacon source is actively formed in the center point of abnormal target area;Drill bit is introduced along the direction of beacon source, the change of beacon source signal is monitored by sensor array during drilling and the offset characteristic sequence is recorded, the real-time tracking of drill bit relative to target area position is realized;After scanning the core sample, the projection position of beacon source on the cross section of core sample is deduced from offset characteristic sequence by matching layer position in frequency spectrum, according to which the sampling is fixed and compared with the corresponding position of ultrasonic image, so that the complementary verification is completed under the clear spatial correspondence, the uncertainty of verification position caused by drill bit deflection is overcome, and the consistency of core verification and ultrasonic detection in physical space is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of concrete testing technology, and specifically discloses a method for complementary verification and testing of concrete using micro-destructive core drilling and ultrasonic phased array. Background Technology

[0002] During service, concrete structures are susceptible to defects such as voids, cracks, and poor bonding due to factors such as loads and environmental erosion. If these defects are not detected in time, they will endanger structural safety. Ultrasonic testing technology, with its advantages of being non-destructive and having strong penetrating power, has become the main method for detecting internal defects in concrete.

[0003] For example, the patent with authorization announcement number CN110333293B discloses a method for exciting and detecting concrete defects using a square grid phased ultrasonic array. By selecting a square area on the concrete surface, an ultrasonic phased array arranged in a square grid is set up. The middle probe array element is used as the emission source and the outer ring probe array elements are used as the receiver. The array element plane is used to perform phased focusing imaging on each discrete point of the defect to obtain the image and depth direction position information of each point of the defect.

[0004] Although the above-mentioned method can locate internal defects in concrete by ultrasonic imaging, the results are affected by various factors such as the heterogeneity of concrete and the distribution of aggregates. There may be a deviation between the imaging and the actual state of the defects, making it difficult to directly verify the location results physically.

[0005] In engineering practice, core sampling is usually used for verification. Core sampling can directly obtain physical samples and visually observe the appearance of the core sample, which is a direct testing method.

[0006] Existing technologies already include detection methods that combine ultrasonic testing with core drilling. For example, patent application CN121577752A discloses a device and method for detecting internal defects in cement concrete based on ultrasonic technology. The device includes a model processing terminal, a scanner, an ultrasonic testing instrument, and a core drilling machine. The scanner collects data and performs grid division. The ultrasonic testing instrument is used to detect defects inside the concrete, and the core drilling machine is used to extract core samples from the defects. The solution also includes a positioning bracket, which controls the ultrasonic testing instrument and the core drilling machine to perform detection at different sampling points via a positioning platform.

[0007] This scheme achieves a certain degree of seamless integration between the two detection methods. However, the defect location of ultrasonic testing is based on the imaging coordinate system, while core sampling is based on the physical coordinates on site. The spatial correspondence between the two depends on surface markings and macroscopic alignment. In actual drilling, the drill bit is prone to deflection. The existing scheme lacks a real-time tracking method for the relative position of the drill bit and the target area, resulting in a lack of reliable verification basis for whether the core truly contains the abnormal area determined by ultrasonic testing, and the credibility of complementary verification is insufficient. Summary of the Invention

[0008] To solve the above-mentioned technical problems, or at least partially solve them, the present invention provides a method for complementary verification and testing of concrete micro-destruction core drilling and ultrasonic phased array.

[0009] The objective of this invention can be achieved through the following technical solutions: A method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array includes the following steps: An ultrasonic phased array probe is deployed on the concrete surface to be tested, ultrasonic phased array data is acquired and a three-dimensional ultrasonic image is generated, and acoustic anomaly target areas are identified and the core center point is delineated. Switch the ultrasonic phased array probe to continuous wave mode to form an acoustic beacon source at the core center point; The drill bit is guided along the direction aligned with the acoustic beacon source for drilling and coring. Throughout the drilling process, the signal changes of the acoustic beacon source are continuously monitored and recorded by the sensor array to form an offset feature sequence that varies with the drilling depth. Drilling is stopped and core samples are retrieved when the drill bit has passed the depth of the acoustic beacon source, based on the offset feature sequence. A ring scan was performed layer by layer along the axial direction of the core sample. The layer where the spectral characteristics matched the acoustic beacon source was labeled as the beacon interception depth. The arrival time difference and amplitude difference were indexed from the offset feature sequence using the beacon interception depth to determine the projection position of the acoustic beacon source on the cross section of the core sample. The sample was cut off with the projection position as the center for strength testing, and the acoustic impedance characteristics at the corresponding position in the three-dimensional ultrasonic image were compared to complete the complementary verification.

[0010] Combining all the above technical solutions, the positive effects of this invention are as follows: This invention uses ultrasonic phased array imaging to delineate the center point of the abnormal target area in the concrete under test, and actively forms an acoustic beacon source at the center point. The drill bit is guided along the direction of the beacon source. Throughout the drilling process, the sensor array monitors the changes in the beacon source signal and records the offset feature sequence, realizing real-time tracking of the drill bit's position relative to the target area. After the core sample is removed and scanned, the projection position of the beacon source on the cross-section of the core sample is deduced from the offset feature sequence using spectral matching. Based on this, the sample is sampled at a fixed point and compared with the corresponding position in the ultrasonic image. This allows complementary verification to be completed under a clear spatial correspondence, overcoming the uncertainty of the verification position caused by drill bit deflection and improving the consistency between core verification and ultrasonic detection in physical space. Attached Figure Description

[0011] The present invention will be further described with reference to the accompanying drawings, but the embodiments in the drawings do not constitute any limitation on the present invention. For those skilled in the art, other drawings can be obtained based on the following drawings without creative effort.

[0012] Figure 1 This is a diagram illustrating the method steps of the present invention; Figure 2 This is a flowchart illustrating the implementation process of identifying acoustically anomalous target areas and delineating the core center point in this invention. Figure 3 This is a flowchart of the process for determining whether to stop drilling in this invention. Detailed Implementation

[0013] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0014] This invention proposes a complementary verification and testing method using micro-destructive core drilling of concrete and ultrasonic phased array, see reference. Figure 1 As shown, it includes the following steps: Step 1: Deploy ultrasonic phased array probes on the concrete surface to be tested, acquire ultrasonic phased array data and generate three-dimensional ultrasonic images, identify acoustically abnormal target areas and delineate the core center point. This step aims to obtain the three-dimensional spatial distribution information of the acoustic structure inside the concrete to be tested, providing a data foundation for the subsequent identification and localization of abnormal target areas.

[0015] Specifically, the ultrasonic phased array probe array is first tightly coupled to the concrete surface to be tested to ensure good acoustic coupling between each array element and the concrete. The probe array consists of multiple array elements arranged according to a certain geometric pattern, and each array element can independently transmit and receive ultrasonic signals.

[0016] During the test, each array element is driven to emit broadband ultrasonic pulses in turn by a rotating excitation method. In this process, only a single array element is excited to emit sound waves each time, while all array elements are synchronously in the receiving state to record the echo signals from the interfaces of various media inside the concrete after the transmission. Each time a single element excitation and full element reception are completed, a complete set of echo time series under the excitation-reception combination is obtained. After traversing all array elements as excitation sources, all collected echo time series together constitute the full matrix echo dataset of the ultrasonic phased array. After data acquisition, the area inside the concrete to be imaged is spatially discretized and divided into a three-dimensional grid with regular dimensions. Each grid cell is called a grid point, and the spatial coordinates of the grid point are the location to be imaged. For each grid point, process all excitation-receiver combinations one by one according to the following steps: (1) For a certain excitation array element-receiver array element combination, the first propagation time of the ultrasonic wave from the excitation array element to the grid point is calculated based on the spatial coordinates of the excitation array element and the grid point coordinates. At the same time, the second propagation time of the scattered echo generated at the grid point to the receiving array element is calculated based on the grid point coordinates and the spatial coordinates of the receiving array element. The two are added together to obtain the total arrival time of the echo corresponding to the grid point under this combination.

[0017] (2) Locate and extract the amplitude at the corresponding moment in the echo time series of the corresponding excitation-receiver combination based on the total arrival time of the echo; After completing the traversal of all excitation-reception combinations, the amplitudes of the grid points extracted from all combinations are coherently superimposed, and the composite amplitude is used as the final imaging amplitude of the grid points.

[0018] During the superposition process, the signal originating from the actual defect location satisfies the in-phase superposition condition due to the consistent propagation path of the sound waves, and its amplitude is enhanced. Meanwhile, the noise signal is weakened by the random phase distribution, thereby improving the signal-to-noise ratio of the defect signal.

[0019] Repeat the above amplitude calculation process for all grid points within the three-dimensional imaging area. After obtaining the imaging amplitude of each grid point, arrange them according to spatial coordinates to construct a three-dimensional ultrasound image.

[0020] Furthermore, after the three-dimensional ultrasound images are constructed, it is necessary to identify areas with abnormal acoustic parameters from the images and quantify their spatial locations to determine the spatial reference points for subsequent verification operations.

[0021] See Figure 2 In a preferred embodiment, the process of identifying acoustically anomalous target areas and delineating the core center point is as follows: The imaging amplitude of each grid point in the 3D ultrasound image is traversed, and grid points with imaging amplitudes higher than a preset background threshold are marked as candidate anomalies. The preset background threshold can be selected by selecting multiple local windows evenly distributed across the entire image in the 3D ultrasound image, with each window avoiding the image boundary region. The maximum amplitude of the grid points in each window is calculated, and then the average value of all the maximum values ​​of the windows is calculated. The average value is used as the background threshold. This is because the defect area usually only occupies a small volume proportion in the image, and the probability of the window covering the defect area is low. Therefore, the obtained average maximum amplitude value still mainly reflects the upper limit of the background amplitude of normal concrete.

[0022] Based on this, spatial neighborhood connectivity analysis is performed on all candidate anomalies, spatially adjacent candidate anomalies are merged into the same continuous region, and the corresponding region is identified as the acoustic anomaly target area. After the abnormal target area is identified, the spatial coordinates of all grid points occupied by the target area are obtained. The arithmetic mean of the row direction coordinates, column direction coordinates and depth direction coordinates of all grid points are calculated. The geometric center position is taken as the core center point of the acoustic abnormal target area. The core center point is the spatial guidance reference for the subsequent acoustic beacon source formation and core drilling. Its physical significance is that it transforms the abnormal position determined in the ultrasonic image domain into specific spatial coordinates that can be tracked in the core drilling process, and establishes a unified geometric reference for ultrasonic detection and core drilling verification.

[0023] Step 2: Switch the ultrasonic phased array probe to continuous wave mode to form an acoustic beacon source at the core center point; After obtaining the spatial coordinates of the core center point of the acoustic anomaly target area in Step 1, the anomaly location determined in the ultrasonic image domain is obtained. However, the coordinates are only an abstract spatial location in the imaging system. During subsequent core drilling, once the drill bit enters the concrete, its relative position to the target area cannot be directly determined through external observation. Whether the drill bit is deviating or still advancing towards the target area lacks real-time judgment. To solve this problem, a spatial positioning reference needs to be actively established at the coordinate location, which can be continuously sensed by the drill bit throughout the drilling process.

[0024] In a preferred embodiment, the acoustic beacon source is formed as follows: Switching the ultrasonic phased array probe from pulse transmission mode to continuous wave transmission mode, with the core center point as the focusing point, reconfiguring the initial phase of each array element, so that the continuous wave sound beams emitted by each array element reach the same phase superposition state at the core center point, forming a continuous focused sound field with highly concentrated spatial energy, and the focused sound field generates concentrated sound radiation force at the core center point. Considering that concrete is a heterogeneous medium, the actual sound path of the sound waves emitted by each array element may differ during the propagation to the focal point. In order to achieve effective in-phase superposition, before adjusting the initial phase of each array element, the sound velocity distribution on the concrete surface to be tested is pre-scanned by the phased array probe array to obtain the sound velocity distribution data in each direction within the detection area. Based on the sound velocity distribution obtained from the pre-scan, the actual sound path between each array element and the focal point is corrected, and the required transmission delay for each array element is recalculated. The initial transmission phase of each array element is configured with the corrected delay value so that the continuous wave sound beams emitted by each array element are superimposed in phase at the core center point. Under the action of the sound radiation force of the continuously focused sound field, the concrete medium at the core center point generates steady-state forced vibration with the same frequency as the excitation signal. Once the steady-state forced vibration is formed, it continuously radiates secondary sound waves to the surrounding medium. The secondary acoustic radiation source is spatially fixed at the core center point, and its radiation characteristics have a deterministic correspondence with the excitation conditions, thus forming an acoustic beacon source that can be tracked and located during subsequent drilling and coring processes.

[0025] During coring, the sensor array uses the following signal enhancement method to detect the beacon source: Each sensing zone collects the received feedback signal multiple times. The signals collected multiple times are aligned according to the collection time and then averaged in phase to suppress random noise. Based on this, the carrier frequency of the excitation signal is used as the reference frequency, and the averaged signal is subjected to narrowband filtering to extract the amplitude of the frequency components as the effective signal.

[0026] It should be noted that in this method, the sensor array tracks the beacon source by utilizing the relative differences in signals generated by the presence or absence of the beacon source and its relative orientation changes. The relative differences in signals generated between different zones due to their different spatial orientations serve as the basis for judging drill bit deviation. During drilling and coring, feed can be paused when beacon source signal acquisition is required to avoid periods of strong noise.

[0027] The physical location of the acoustic beacon source obtained in this way strictly coincides with the core center point of the abnormal target area determined in the ultrasonic image, providing a spatial reference that can be continuously sensed by the sensor array for the initial determination of the drill bit guide direction and the real-time tracking of the drill bit's position relative to the target area throughout the drilling process.

[0028] Step 3: Guide the drill bit along the direction aligned with the acoustic beacon source for drilling and coring. Throughout the drilling process, continuously monitor and record the signal changes of the acoustic beacon source through a sensor array to form an offset feature sequence that varies with drilling depth. After establishing an acoustic beacon source at the core center point, the beacon source is spatially fixed at the center of the abnormal target area and can serve as a reference for sensing the relative position of the drill bit during the drilling and coring process. However, during the actual drilling process, the drill bit is affected by factors such as uneven hardness of aggregates inside the concrete and obstruction by reinforcing bars, and its advancing direction will inevitably deviate from the initial alignment direction. Moreover, the deviation accumulates with the increase of drilling depth and cannot be directly observed from the outside.

[0029] To achieve real-time tracking of the drill bit's position relative to the target area, a sensing device capable of sensing the spatial orientation of the beacon source needs to be deployed at the front end of the drill bit's guide path, and signal changes need to be continuously collected throughout the drilling process to obtain the offset information of the drill bit relative to the beacon source at each drilling depth.

[0030] As one possible implementation of the present invention, the offset feature sequence is formed in the following manner: A ring-shaped partitioned sensor array is coaxially deployed at the front end of the drill bit guide path. The sensor array contains multiple sensor partitions distributed at equal angles along the circumference. Each partition can independently emit detection pulses towards the acoustic beacon source and receive the echo signal. The function of the ring-shaped partitioned sensor array is to utilize the geometric feature that the partitions are spatially distributed in different orientations. When there is a deviation between the drill bit's central axis and the beacon source position, the distance and azimuth angle of each partition relative to the beacon source will be different. The arrival time and amplitude of the received echo signal will show differences corresponding to the direction and amount of deviation. By analyzing the differences, the relative spatial relationship between the drill bit and the beacon source can be deduced. During drilling, signal acquisition is triggered at fixed depth intervals. During each acquisition, each section emits a probe pulse towards the acoustic beacon source and receives the echo signal. The arrival time and amplitude of the echo signal received by each section are recorded. To avoid inaccurate judgment of relative offset due to synchronous changes in absolute measurements caused by beacon source signal fluctuations, a fixed section is used as a reference. The arrival time difference and amplitude difference between the reference section and the other sections are calculated. The arrival time difference of each section represents the signal arrival sequence of the beacon source relative to the reference section at different spatial orientations, and its sign and relative magnitude reflect the direction of the beacon source's deviation from the center of the sensor array. The amplitude difference represents the signal energy attenuation distribution of the beacon source relative to the reference section at different spatial orientations. The combination of both can be used to determine the relative offset direction and amount between the drill bit and the beacon source.

[0031] In practice, the sensor array is evenly distributed in the circumferential direction. Any fixed-numbered partition is selected as the reference partition. Subsequent acquisitions are calculated based on this partition. Once the reference partition is determined, the arrival time difference and amplitude difference of the reference partition itself are both zero. However, this does not affect the subsequent calculation of the orientation angle and deviation. This is because the orientation angle and deviation are synthesized from the differences of each partition. The zero value of a single reference partition only indicates that the difference in that orientation is zero. Together with the differences of the other partitions, it constitutes a complete deviation vector. Therefore, the zero value of the reference partition will not have any impact on the final result. The current drilling depth, the calculated arrival time difference and amplitude difference of each zone are encoded together into a set of offset feature parameters. The offset feature parameters are arranged continuously in ascending order of drilling depth to form an offset feature sequence. The sequence completely records the continuous change trajectory of the spatial offset of the drill bit center axis relative to the acoustic beacon source with the drilling depth from the start of drill bit feeding to the current depth. This provides a data basis for subsequent determination of whether the drill bit has passed the depth where the beacon source is located.

[0032] Step 4: Stop drilling when the drill bit has passed the depth of the acoustic beacon source based on the offset feature sequence, and take out the core sample; During the drilling process, the feed is not continuous indefinitely. Drilling needs to be stopped in time when the drill bit tip reaches and passes through the depth of the acoustic beacon source to ensure that the extracted core sample contains the layer where the abnormal target area is located, while avoiding excessive drilling that could cause the target layer in the core sample to be missing.

[0033] See Figure 3 In one optional implementation, the process for determining whether to stop drilling is as follows: Step 41: Extract multiple consecutive sets of offset feature parameters from the end of the offset feature sequence as a decision window; Step 42: Calculate the difference in arrival time between two adjacent groups within the decision window as the first difference sequence, which is used to characterize the trend of arrival time difference with drilling depth. At the same time, calculate the difference in amplitude between two adjacent groups as the second difference sequence, which is used to characterize the trend of amplitude difference with drilling depth. Step 43: Compare the positive and negative signs of each value in the first difference sequence one by one along the increasing drilling depth direction. When the drill bit tip has not yet approached the beacon source, the beacon source is located in front of the drill bit. The echo signals received by each section show a monotonically changing trend as drilling progresses. At this time, the positive and negative signs of each value in the first difference sequence remain consistent. As the drill bit continues to advance, when the drill bit tip approaches and begins to cross the depth where the beacon source is located, the position of the beacon source relative to the drill bit tip tip changes from front to back. The changing trend of the echo signal reverses during this process. The reversal is manifested in the positive and negative signs of the first difference sequence changing from being consistent to flipping. This indicates that the drill bit tip has reached the vicinity of the depth where the beacon source is located. Record the drilling depth corresponding to the arrival time difference at the flipping point as the first candidate depth. Step 44: Compare the signs of each value in the second difference sequence along the increasing drilling depth direction. When the drill bit tip has not yet approached the beacon source, the amplitude difference of each zone continues to decrease as the drill bit advances. At this time, all values ​​in the second difference sequence are negative and the negative signs remain consistent. As the drill bit continues to advance, when the drill bit tip reaches and crosses the depth where the beacon source is located, the amplitude difference of each zone reaches the minimum value and then begins to increase. The turning point is that the negative values ​​in the second difference sequence change to positive values, indicating that the drill bit tip has crossed the plane where the beacon source is located. Record the drilling depth corresponding to the amplitude difference at the sign change position as the second candidate depth. Step 45: Of the two candidate depths mentioned above, the first candidate depth represents the depth at which the drill bit tip reaches the beacon source, and the second candidate depth represents the distance after the drill bit tip passes through the plane where the beacon source is located. Both are related to the drill bit passing through the beacon source. When the distance between the first candidate depth and the second candidate depth in the drilling depth axis is less than a predetermined distance threshold, it indicates that the two are adjacent in the depth direction. The smaller of the two drilling depths is taken as the determination value for determining that the drill bit has passed through the depth where the acoustic beacon source is located, so as to ensure that drilling stops immediately after the drill bit tip just passes through the plane where the beacon source is located, and to avoid the destruction or loss of the target layer in the core sample due to continued advancement.

[0034] The aforementioned predetermined spacing threshold is based on the drill bit diameter and is set between 0.8 and 1.2 times the drill bit diameter. This range can cover the signal spacing variation under different drill bit diameters and avoid misjudgment due to a threshold that is too narrow or missed judgment due to a threshold that is too wide. For example, if the drill bit diameter is 80 mm, the predetermined spacing threshold is 90 mm.

[0035] As an application example, during a drilling operation, the following offset feature sequence data was collected: Table 1. Offset Feature Sequence and Difference Calculation Results

[0036] As shown in the table, in the first difference sequence, the sign remains -2 (negative) before 110mm and turns to +1 (sign flip) at 120mm. The drilling depth of 120mm corresponding to the flip position is recorded as the first candidate depth. In the second difference sequence, the sign remains -1 (negative) at 110mm and turns to +3 (negative to positive) at 120mm. The corresponding amplitude difference value of 7 is at a trough, and the drilling depth of 110mm is recorded as the second candidate depth. The distance between the first candidate depth of 120mm and the second candidate depth of 110mm is 10mm, which is less than the predetermined distance threshold. The smaller of the two, 110mm, is taken as the drilling stop determination depth.

[0037] Step 5: Perform a ring scan of the core sample layer by layer along the axial direction. The layer where the spectral characteristics match the acoustic beacon source is marked as the beacon interception depth. The arrival time difference and amplitude difference are indexed from the offset feature sequence using the beacon interception depth to determine the projection position of the acoustic beacon source on the cross section of the core sample. After the core sample is extracted, it needs to be tested to obtain the true physical properties of the abnormal target area and compared with the acoustic features of the corresponding location in the ultrasound image. To ensure that the comparison is based on a precise spatial correspondence, the actual position corresponding to the abnormal target area in the ultrasound image needs to be accurately located on the core sample. Since the drill bit is deflected during the core extraction process, the center point of the target area determined in the ultrasound image may not necessarily be located on the geometric center axis of the core sample, but may deviate from the axis by a certain direction and distance. Therefore, it is necessary to calibrate the beacon interception depth on the core sample and combine it with the offset feature sequence recorded during the drilling process to deduce the projection position of the beacon source on the cross-section of the core sample. Then, based on the projection position, point detection is performed to ensure that the detected sample position corresponds strictly to the abnormal target area determined by ultrasound in physical terms.

[0038] The following description is based on specific examples; First, core sample scanning and beacon interception depth calibration are performed, as follows: The removed core sample is fixed on the rotating platform, so that the axis of the core sample coincides with the axis of rotation of the rotating platform. The rotating platform can drive the core sample to rotate precisely around its own axis. The scanning probe is fixed to the side of the core sample and points into the core sample. During the scanning process, the scanning probe is moved layer by layer from one end of the core sample to the other. When it reaches a layer, the rotating platform is activated to rotate the core sample around the axis once. During the rotation, the scanning probe continuously emits sound waves into the core sample and receives transmitted or reflected echo signals, thereby obtaining complete annular scanning data of the layers. The dominant frequency and harmonic distribution of the scan signals at each layer are extracted as the spectral characteristics of the layer. The spectral characteristics of each layer are compared with the steady-state forced vibration spectral characteristics of the acoustic beacon source in turn. Multiple layers with consistent and continuous adjacent spectral characteristics are selected, and the axial midpoint of the continuous layers is taken as the beacon interception depth.

[0039] The reason for the above calibration is that the acoustic beacon source has a certain spatial scale in the axial direction of the core sample, rather than being an infinitely thin plane. When the drill bit passes through the beacon source, it will leave spectral feature traces on multiple consecutive layers within the thickness range of the beacon source. Therefore, taking the axial midpoint of consecutive adjacent matching layers as the depth of the beacon source center can eliminate the positioning error caused by the thickness of the beacon source itself, and make the calibrated depth correspond to the depth position of the core center point of the target area in the ultrasound image.

[0040] Secondly, determine the projection position of the beacon source.

[0041] After the beacon interception depth calibration is completed, it is necessary to further determine the specific direction and distance of the beacon source from the core sample's central axis within the depth cross-section. Assume the annular partitioned sensing array contains N sensing partitions distributed at equal angles along the circumference. The spatial azimuth angle of each partition is known. Using the beacon interception depth as the index, a set of offset feature parameters corresponding to the offset feature sequence is extracted as the target group. The target group records the arrival time difference of each partition. , … and amplitude difference , … ; Extract the arrival time difference from the target group, and let the spatial azimuth of each sensing zone be . , ... , The arrival time difference of each region is projected onto mutually orthogonal X-axis and Y-axis directions according to its spatial azimuth angle. The algebraic sum of the projections in the X and Y directions is calculated to obtain the composite component of the arrival time difference in the X and Y directions. and , , ,by and The arctangent function of the ratio is used to calculate the direction angle of the beacon source from the center axis of the core sample. .

[0042] Extract the amplitude difference from the target group, and project the amplitude difference of each partition onto the X-axis and Y-axis directions according to its spatial azimuth angle. Calculate the algebraic sum of the projections in the X and Y directions to obtain the composite components of the amplitude difference in the X and Y directions. and , , ,by and The square root of the sum of the squares is used to calculate the deviation of the beacon source from the center axis of the core sample. .

[0043] Obtain the direction angle and deviation Then, starting from the center point of the cross section where the beacon intercepts the depth (i.e., the intersection of the core sample's central axis and the depth plane), along the direction angle... Distance of movement in the indicated direction The point reached is the projection position of the acoustic beacon source on the cross-section, and the projection position is the actual physical position corresponding to the core center point of the abnormal target area in the ultrasound image inside the core sample.

[0044] Step 6: Take a sample centered on the projected position for strength testing, and compare it with the acoustic impedance characteristics at the corresponding position in the 3D ultrasound image to complete the complementary verification.

[0045] After obtaining the projected position of the beacon source on the core sample cross-section, direct testing of the projected position is required to obtain the actual mechanical property data of the target area, which is used to verify the accuracy of the ultrasound testing results. Strength is a key mechanical property index in concrete quality evaluation, and the point load strength test can be performed on small-sized samples without preparing standard large-sized specimens, making it suitable for strength testing of local areas of core samples. Therefore, strength testing is selected as the verification method.

[0046] The strength testing process is as follows: On the surface of the core sample, centered on the projected position, cuts are made at a certain distance above and below the beacon interception depth along the axial direction of the core sample to extract a thin sheet-shaped core sample segment between the two cut surfaces. The cutting spacing is determined based on the core sample diameter and point load test requirements, typically ranging from 0.5 to 1.0 times the core sample diameter, to ensure the thin sheet has sufficient bearing surface and meets the loading space requirements of the test equipment.

[0047] Apply a point load to the thin sheet-shaped core sample segment until failure, record the load value at failure, and convert it to a local strength value based on the geometric parameters of the loading indenter and the sample size, which serves as the actual local strength value of the concrete at the projected position.

[0048] Further, the complementary verification is as follows: The imaging amplitude of each grid point in the 3D ultrasound image reflects the acoustic characteristics of the concrete at the corresponding position, but the amplitude itself is not a mechanical property index, so it needs to be converted into a physical quantity that can be compared with the mechanical test results in the same dimension. Using the analysis software supporting the ultrasound phased array testing system, based on the imaging amplitude of the 3D ultrasound image and the built-in acoustic impedance-strength conversion model of the system, the acoustic impedance inversion strength values of each spatial position of the concrete to be tested are automatically output. When the difference between the local strength value and the acoustic impedance inversion strength value is within the preset tolerance range, the ultrasound testing result of the acoustic abnormal target area is judged to have passed the core drilling verification. If the difference between the two exceeds the preset tolerance range, the ultrasound testing result of the abnormal target area is judged to have failed the core drilling verification, the ultrasound phased array testing parameters need to be recalibrated, and the area needs to be re-scanned by ultrasound and re-evaluated for anomalies.

[0049] The preset tolerance range mentioned above is set as follows: According to the standard for test methods of physical and mechanical properties of concrete, the maximum allowable deviation between the compressive strength value of a single core sample and the average strength value of specimens in the same group is generally no more than 15%. Based on this, taking the acoustic impedance inversion strength value at the corresponding spatial coordinate position in the 3D ultrasound image as the reference value, ±15% of the reference value is set as the preset tolerance range.

[0050] The above embodiments can be implemented, in whole or in part, by software, hardware, firmware, or any other combination thereof. When implemented using software, the above embodiments can be implemented, in whole or in part, in the form of a computer program product.

[0051] Those skilled in the art will recognize that the modules and algorithm steps of the various examples described in conjunction with the embodiments disclosed herein can be implemented in electronic hardware, or a combination of computer software and electronic hardware. Whether these functions are implemented in hardware or software depends on the specific application and design constraints of the technical solution. Those skilled in the art can use different methods to implement the described functions for each specific application, but such implementation should not be considered beyond the scope of this application.

[0052] The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.

Claims

1. A method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array, characterized in that, include: An ultrasonic phased array probe is deployed on the concrete surface to be tested, ultrasonic phased array data is acquired and a three-dimensional ultrasonic image is generated, and acoustic anomaly target areas are identified and the core center point is delineated. Switch the ultrasonic phased array probe to continuous wave mode to form an acoustic beacon source at the core center point; The drill bit is guided along the direction aligned with the acoustic beacon source for drilling and coring. Throughout the drilling process, the signal changes of the acoustic beacon source are continuously monitored and recorded by the sensor array to form an offset feature sequence that varies with the drilling depth. Drilling is stopped and core samples are retrieved when the drill bit has passed the depth of the acoustic beacon source, based on the offset feature sequence. A ring scan was performed layer by layer along the axial direction of the core sample. The layer where the spectral characteristics matched the acoustic beacon source was labeled as the beacon interception depth. The arrival time difference and amplitude difference were indexed from the offset feature sequence using the beacon interception depth to determine the projection position of the acoustic beacon source on the cross section of the core sample. The sample was cut off with the projection position as the center for strength testing, and the acoustic impedance characteristics at the corresponding position in the three-dimensional ultrasonic image were compared to complete the complementary verification. The acoustic beacon source is formed according to the following process: Switch the ultrasonic phased array probe from pulse mode to continuous wave mode, use the core center point as the focusing point, and adjust the initial phase of each array element to make the continuous wave sound beams superimpose in phase at the core center point to form a continuous focused sound field. The concrete medium at the core center point generates steady-state forced vibration at the same frequency as the excitation signal under the action of the acoustic radiation force of the continuously focused sound field. The steady-state forced vibration radiates secondary sound waves to the surrounding medium, and the secondary sound wave radiation source serves as an acoustic beacon source. The beacon interception depth is determined according to the following procedure: The removed core sample is fixed on the rotating platform, so that the axis of the core sample coincides with the axis of rotation of the rotating platform. The scanning probe is coupled to the side wall of the core sample and pointed into the core sample. The scanning probe is moved layer by layer from one end of the core sample to the other. When it reaches a layer, the rotating platform is activated to rotate the core sample around the axis once. During the rotation, the scanning probe continuously collects the transmitted or reflected sound wave signals of the layer and extracts the main frequency and harmonic distribution of the layer signal as the spectral characteristics of the layer. The spectral characteristics of each layer are compared with the steady-state forced vibration spectral characteristics of the acoustic beacon source in turn. Multiple layers with consistent and continuous spectral characteristics are selected, and the axial midpoint of the continuous layers is taken as the beacon interception depth.

2. The method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array as described in claim 1, characterized in that: The generated three-dimensional ultrasound image content is as follows: An ultrasonic phased array probe array is coupled to the concrete surface to be tested. Each array element is excited in turn to emit ultrasonic pulses. During each excitation, all array elements synchronously receive the echo signal, and the echo time sequence under each excitation-reception combination is recorded. For each grid point inside the concrete to be tested, the first propagation time of the sound wave emitted by each excitation array element to the grid point and the second propagation time of the echo scattered from the grid point to each receiving array element are calculated. The two are added together to obtain the total arrival time of the echo. Based on the total arrival time of the echo, locate and extract the echo amplitude at that moment in the corresponding echo time series. Algebraically superimpose the echo amplitudes of the grid points extracted under all excitation-reception combinations, and use the superimposed amplitude as the imaging amplitude of the grid point. A three-dimensional ultrasound image is constructed based on the imaging amplitude of all grid points.

3. The method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array as described in claim 2, characterized in that: The identification of acoustically anomalous target areas and the delineation of the core center point are as follows: Traverse all grid points of the three-dimensional ultrasound image and extract continuous grid regions with superimposed amplitudes higher than the preset background threshold as acoustic abnormality target areas. Obtain the spatial boundary coordinates of the target area, calculate the geometric center position of all grid points occupied by the target area, and use the geometric center position as the core center point of the acoustic anomaly target area.

4. The method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array as described in claim 1, characterized in that: The offset feature sequence is formed in the following manner: A ring-shaped partitioned sensor array is deployed at the front end of the drill bit guide path. The sensor array contains multiple sensor partitions distributed at equal angles along the circumference. Each partition emits a detection pulse toward the acoustic beacon source and receives the feedback signal. During the drilling process, acquisition is triggered at fixed depth intervals. Each acquisition obtains the arrival time and amplitude of the backhaul signal of each zone at the current drilling depth. Using a selected fixed zone as a reference, the arrival time difference and amplitude difference of the other zones relative to the reference zone are calculated. The current drilling depth value, arrival time difference, and amplitude difference are collectively encoded into a set of offset feature parameters. The offset feature parameters are then arranged sequentially in ascending order of drilling depth to form an offset feature sequence.

5. The method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array as described in claim 4, characterized in that: The decision to stop drilling is made as follows: Multiple consecutive sets of offset feature parameters are truncated from the end of the offset feature sequence to form a decision window; The difference in arrival time between two adjacent groups within the decision window is calculated as the first difference sequence, and the difference in amplitude between two adjacent groups is calculated as the second difference sequence. The signs of each value in the first difference sequence are compared sequentially along the increasing drilling depth direction. When the signs of the first difference sequence change from being consistent to being flipped, the drilling depth corresponding to the arrival time difference at the flipping point is recorded as the first candidate depth. The sign of each value in the second difference sequence is compared bit by bit along the increasing direction of drilling depth. When the sign of the second difference sequence changes from being negative to being positive, the drilling depth corresponding to the amplitude difference at the sign change position is recorded as the second candidate depth. When the distance between the first candidate depth and the second candidate depth along the drilling depth axis is less than a predetermined distance threshold, the smaller of the two drilling depths is taken as the depth at which the drill bit has passed the acoustic beacon source, and a stop drilling command is issued.

6. The method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array as described in claim 4, characterized in that: The determination of the projection position of the acoustic beacon source on the cross-section of the core sample is as follows: The target group is a set of offset feature parameters recorded at the corresponding depth in the offset feature sequence based on the beacon interception depth. The arrival time difference in the target group is extracted and decomposed into two mutually orthogonal horizontal components according to the circumferential azimuth of each sensing zone. The direction angle of the acoustic beacon source deviating from the central axis of the core sample is calculated by the ratio of these two components. The amplitude difference in the target group is extracted and decomposed into two mutually orthogonal horizontal components according to the circumferential azimuth of each sensing zone. The deviation of the acoustic beacon source from the center axis of the core sample is calculated using the combined amplitude of these two components. Starting from the center point of the cross section where the beacon interception depth is located, move the distance of the deviation along the directional angle direction, and mark the arrival point as the projection position of the acoustic beacon source on the core sample cross section.

7. The method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array as described in claim 1, characterized in that: The process of taking a sample centered on the projected position for strength testing is as follows: With the projection position as the center, cut along the core sample axial direction at a distance above and below the beacon interception depth, and take out the thin sheet-like core sample segment between the two cut surfaces. A point load is applied to the thin-sheet core sample until failure, and the load value at failure is recorded as the local strength value of the concrete at the projected location.

8. The method for complementary verification and testing of concrete micro-destructive core drilling and ultrasonic phased array as described in claim 7, characterized in that: The complementarity verification process is as follows: The local intensity value is compared with the acoustic impedance inversion intensity value at the same spatial coordinate position in the three-dimensional ultrasound image. If the difference between the two is within the preset tolerance range, the ultrasound detection result of the acoustically abnormal target area is determined to have passed the core drilling verification.

Citation Information

Patent Citations

  • A method for excitation and detection of concrete defects using a square grid phased ultrasonic array

    CN110333293B

  • Cement concrete internal defect detection device and method based on ultrasonic technology

    CN121577752A

  • A building site electromechanical energy-saving linkage regulation and control system and method

    CN122902377A