Six-dimensional force sensor based on 3D printing and preparation method thereof

By integrating piezoresistive and piezoelectric sensing layers onto a metallic elastomer skeleton, the problem of insufficient material performance in existing six-dimensional force sensors is solved, enabling high-precision static force and high-frequency dynamic force measurement, expanding the measurement range and improving the stability of the sensor.

CN122900751BActive Publication Date: 2026-11-24CRINM (GUANGDONG) INST FOR ADVANCED MATERIALS & TECH +1
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202611393098.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2026-09-09
Publication Date
2026-11-24
Estimated Expiration
2046-09-09

AI Technical Summary

Technical Problem

Existing 3D printed six-dimensional force sensors mostly use polymer-based materials, which have low elastic modulus and poor creep resistance, limiting their application in high-load scenarios. Moreover, the sensing principle is mostly optical measurement, without integrating piezoresistive or piezoelectric materials.

Method used

Piezoresistive and piezoelectric sensing layers are integrated on a metal elastomer skeleton using 3D printing technology. Piezoresistive and piezoelectric material inks are printed in a preset area, and combined with a conductive interconnect layer and an insulating isolation layer to form a piezoresistive-piezoelectric hybrid six-dimensional force sensor. The whole sensor is then annealed and packaged.

Benefits of technology

It achieves high-precision measurement of static force and high-frequency response of dynamic force, expands the measurement range of the six-dimensional force sensor, reduces quality loss caused by process deviation and human intervention, and improves the stability and measurement capability of the sensor.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122900751B_ABST
    Figure CN122900751B_ABST
Patent Text Reader

Abstract

This invention discloses a six-dimensional force sensor based on 3D printing and its fabrication method, belonging to the field of sensor technology. The invention involves printing a metal elastomer skeleton according to a preset elastomer structure model, wherein the preset elastomer structure model is a three-dimensional structural model corresponding to the metal elastomer skeleton; printing piezoresistive material ink in a predetermined printing area to obtain a piezoresistive sensing layer, and printing piezoelectric material ink in the associated area of ​​the piezoresistive sensing layer to obtain a piezoelectric sensing layer; printing conductive ink at the electrode leads of the piezoresistive sensing layer and the electrode leads of the piezoelectric sensing layer to obtain a conductive interconnect layer, and printing insulating material to obtain an insulating isolation layer; annealing and encapsulating the printed object to obtain the piezoresistive-piezoelectric hybrid six-dimensional force sensor, achieving the hybrid integration of piezoresistive and piezoelectric sensing layers within the same rigid metal six-dimensional force sensor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of sensor technology, and in particular to a six-dimensional force sensor based on 3D printing and its fabrication method. Background Technology

[0002] A six-dimensional force sensor is a sensor capable of simultaneously detecting forces and torques in three spatial directions. It is a core sensing device for achieving precise force-sensing interaction in robots and has wide applications in industrial robots, collaborative robots, humanoid robots, and precision assembly. In recent years, existing 3D-printed six-dimensional force sensors have mostly used polymer-based materials as elastomers. However, their low elastic modulus and poor creep resistance limit their application in high-load scenarios. Although some research has introduced metal 3D printing into the elastomer manufacturing of six-dimensional force sensors, their sensing principles are mostly optical measurements, rather than the integration of piezoresistive or piezoelectric materials.

[0003] The above content is only used to help understand the technical solution of the present invention and does not represent an admission that the above content is prior art. Summary of the Invention

[0004] The main objective of this invention is to provide a 3D-printed six-dimensional force sensor and its fabrication method, aiming to achieve the hybrid integration of piezoresistive and piezoelectric sensing layers within the same rigid metal six-dimensional force sensor. To achieve this objective, this invention provides a method for fabricating a 3D-printed piezoresistive-piezoelectric hybrid six-dimensional force sensor, comprising the following steps: Print the metal elastomer skeleton according to the preset elastomer structure model, wherein the preset elastomer structure model is the three-dimensional structure model corresponding to the metal elastomer skeleton; Piezoresistive material ink is printed in a predetermined printing area to obtain a piezoresistive sensing layer, and piezoelectric material ink is printed in an associated area of ​​the piezoresistive sensing layer to obtain a piezoelectric sensing layer, wherein the associated area includes: an area on the metal elastomer skeleton that is intersected or adjacent to the piezoresistive sensing layer. Conductive ink is printed at the electrode leads of the piezoresistive sensing layer and the electrode leads of the piezoelectric sensing layer to obtain a conductive interconnect layer, and insulating material is printed to obtain an insulating isolation layer. The conductive interconnect layer is used to connect the electrode leads to the signal output pads of the six-dimensional force sensor. The printed object is annealed and packaged to obtain the piezoresistive-piezoelectric hybrid six-dimensional force sensor.

[0005] Optionally, the step of printing the metal elastomer skeleton according to the preset elastomer structure model includes: A pre-set metal material is melted layer by layer using a laser powder bed melting process under a protective atmosphere to form the metal elastomer skeleton. The pre-set metal material includes, but is not limited to, stainless steel powder, titanium alloy powder or maraging steel powder. The protective atmosphere is nitrogen or argon. During the formation of the metal elastomer skeleton, the temperature of the printed substrate is controlled within a first temperature range. After the metal elastomer skeleton is formed, the printing substrate is controlled to cool down to a preset printing temperature at a preset cooling rate, wherein the preset cooling rate is 2℃ / min to 5℃ / min, the preset printing temperature meets the printing temperature requirements of the piezoresistive material ink, and a heat insulation structure is provided between the printing substrate and the worktable for printing the piezoresistive material ink.

[0006] Optionally, before the step of printing piezoresistive material ink in the predetermined printing area to obtain the piezoresistive sensing layer, the method further includes: The predetermined printing area is subjected to surface activation treatment, wherein the predetermined printing area is the high strain region corresponding to the elastic beam of the metal elastomer skeleton; The surface activation process includes: controlling an oxygen plasma treatment device to perform oxygen plasma activation treatment on the predetermined printing area, wherein the processing time of the oxygen plasma activation treatment is 30 seconds to 120 seconds; determining the contact angle of the predetermined printing area after the oxygen plasma activation treatment; and completing the surface activation treatment when the contact angle is lower than a preset contact angle threshold.

[0007] Optionally, after the step of annealing and encapsulating the printed object to obtain the piezoresistive-piezoelectric hybrid six-dimensional force sensor, the method further includes: Obtain a calibration sample set, wherein each calibration sample in the calibration sample set includes: a piezoresistive signal corresponding to each piezoresistive sensing unit, a piezoelectric signal corresponding to each piezoelectric sensing unit, temperature data and time window feature data of the piezoresistive-piezoelectric hybrid six-dimensional force sensor, and a corresponding six-dimensional force standard value, wherein the time window feature data is the feature data of the piezoresistive signal and the piezoelectric signal within a preset time window; An extended feature vector is constructed for each calibration sample based on the piezoresistive signal, the piezoelectric signal, the temperature data, and the time window feature data in each calibration sample. The preset neural network is trained based on multiple extended feature vectors and the corresponding six-dimensional force standard values ​​to obtain a decoupled mapping model, wherein the decoupled mapping model is used to determine the six-dimensional force standard values ​​based on the output signals of the piezoresistive sensing layer and the piezoelectric sensing layer.

[0008] Optionally, the piezoresistive signal and the piezoelectric signal are acquired according to the following steps: The piezoresistive sensing layer is connected to a Wheatstone bridge circuit excited by a constant voltage source, and the output signal of the Wheatstone bridge circuit is differentially amplified and low-pass filtered to obtain the piezoresistive signal. The piezoelectric sensing layer is connected to a charge amplifier, and the output signal of the charge amplifier is bandpass filtered to obtain the piezoelectric signal. The piezoresistive signal and the piezoelectric signal are respectively converted from analog to digital, wherein the piezoresistive signal is a DC voltage signal reflecting quasi-static force, and the piezoelectric signal is an AC voltage signal reflecting dynamic force.

[0009] Optionally, the step of printing piezoresistive material ink in a predetermined printing area to obtain a piezoresistive sensing layer includes: A piezoresistive material ink is defined, wherein the piezoresistive material ink includes, but is not limited to: conductive filler, polydimethylsiloxane prepolymer and curing agent, wherein the conductive filler includes, but is not limited to, graphene nanosheets or multi-walled carbon nanotubes; The piezoresistive material ink is printed into a preset sensing pattern in the predetermined printing area using a direct writing process. The preset sensing pattern includes: an axial piezoresistive strip arranged along the axis of the elastic beam, and a shear piezoresistive strip arranged at 45° to the axis of the elastic beam. The printed preset sensing pattern is cured to obtain the piezoresistive sensing layer.

[0010] Optionally, the preset elastomer structure model includes any of the following: The three-beam structure model includes: a central loading platform, an outer fixing ring, and three radial main beams evenly distributed at 120° angles to each other; The cross-beam structure model includes: a central bearing platform, an outer fixing ring, and four orthogonally distributed elastic beams; The Stewart parallel structure model includes: an upper platform, a lower platform, and six elastic pillars with flexible hinges at both ends. The six elastic pillars are arranged in parallel between the upper platform and the lower platform. The metal elastomer skeleton is a one-piece structure formed in one piece.

[0011] Furthermore, to achieve the above objectives, the present invention also provides a piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing, characterized in that the 3D-printed piezoresistive-piezoelectric hybrid six-dimensional force sensor comprises: a metal elastomer skeleton, a piezoresistive sensing layer, a piezoelectric sensing layer, a conductive interconnect layer, and an insulating isolation layer, wherein: The piezoresistive sensing layer and the piezoelectric sensing layer are arranged in the high-strain region corresponding to the elastic beam of the metal elastomer skeleton. The conductive interconnect layer connects the electrode leads of the piezoresistive sensing layer and the electrode leads of the piezoelectric sensing layer; The insulating isolation layer is disposed at the intersection of the conductive interconnect layers; The metal elastomer skeleton, the piezoresistive sensing layer, the piezoelectric sensing layer, the conductive interconnect layer, and the insulating isolation layer are formed into an integral structure using the above-described fabrication method for a piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing.

[0012] Furthermore, to achieve the above objectives, the present invention also provides a fabrication apparatus for a piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing. The apparatus comprises: a memory, a processor, and a fabrication program for the piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing, stored in the memory and executable on the processor. The fabrication program for the piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing is configured to implement the steps of the aforementioned fabrication method for the piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing.

[0013] Furthermore, to achieve the above objectives, the present invention also provides a storage medium storing a fabrication program for a piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing. When the fabrication program for the piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing is executed by a processor, the steps of the fabrication method for the piezoresistive-piezoelectric hybrid six-dimensional force sensor based on 3D printing described in any of the above claims are implemented.

[0014] This invention proposes a method for fabricating a six-dimensional force sensor based on 3D printing. The method involves printing a metal elastomer skeleton according to a pre-defined elastomer structure model, printing piezoresistive material ink in a predetermined printing area to obtain a piezoresistive sensing layer, printing piezoelectric material ink in a related area to obtain a piezoelectric sensing layer, then printing conductive ink at the electrode leads to obtain a conductive interconnect layer, and finally printing insulating material to obtain an insulating isolation layer. The printed object is then annealed and encapsulated. This method integrates the metal elastomer skeleton, piezoresistive sensing layer, piezoelectric sensing layer, conductive interconnect layer, and insulating isolation layer into a single multi-material 3D printing process, eliminating the need for traditional discrete processes such as patching, wire bonding, and multiple alignments. This reduces quality control issues caused by manual intervention and process deviations. Furthermore, by integrating piezoresistive and piezoelectric sensing layers on the same rigid metal elastomer, it achieves both high-precision measurement of static forces and high-frequency response of dynamic forces, significantly expanding the measurement range of the six-dimensional force sensor. Attached Figure Description

[0015] Figure 1 This is a schematic diagram of the structure of the fabrication equipment for a 3D-printed six-dimensional force sensor, which is part of the hardware operating environment involved in the embodiments of the present invention. Figure 2This is a schematic flowchart of the first embodiment of the fabrication method of the six-dimensional force sensor based on 3D printing of the present invention; Figure 3 This is a schematic flowchart of the second embodiment of the fabrication method of the six-dimensional force sensor based on 3D printing of the present invention; Appendix Figure 4 This is a top view of the elastomer structure of the present invention; Appendix Figure 5 This is a top view of the structure of an elastomer; Appendix Figure 6 A schematic diagram of the Stewart parallel structure elastic body; Appendix Figure 7 This is a schematic diagram of the sensor unit layout in a single support column.

[0016] The realization of the objective, functional features and advantages of the present invention will be further explained in conjunction with the embodiments and with reference to the accompanying drawings. Detailed Implementation

[0017] It should be understood that the specific embodiments described herein are merely illustrative of the invention and are not intended to limit the invention.

[0018] Reference Figure 1 , Figure 1 This is a schematic diagram of the fabrication equipment for a 3D-printed six-dimensional force sensor, which is part of the hardware operating environment involved in the embodiments of the present invention.

[0019] like Figure 1 As shown, the fabrication device for the 3D-printed six-dimensional force sensor may include: a processor 1001, such as a central processing unit (CPU), a communication bus 1002, an interactive device 1003, a network interface 1004, and a memory 1005. The communication bus 1002 is used to enable communication between these components. The interactive device 1003 may include a display screen and an input unit such as a keyboard. The interactive device 1003 may also be connected to the communication bus via standard wired or wireless interfaces. The network interface 1004 may optionally include standard wired or wireless interfaces (such as a Wi-Fi interface). The memory 1005 may be a high-speed random access memory (RAM) or a stable non-volatile memory (NVM), such as a disk drive. Alternatively, the memory 1005 may be a storage device independent of the aforementioned processor 1001.

[0020] Those skilled in the art will understand that Figure 1 The structure shown does not constitute a limitation on the fabrication equipment for a 3D-printed six-dimensional force sensor, and may include more or fewer parts than shown, or combine certain parts, or have different part arrangements.

[0021] like Figure 1 As shown, the memory 1005, which serves as a storage medium, may include an operating system, a data storage module, a network communication module, a user interface module, and a fabrication program for a 3D-printed six-dimensional force sensor.

[0022] exist Figure 1 In the fabrication device for a 3D-printed six-dimensional force sensor shown, the network interface 1004 is mainly used for data communication with other devices; the interactive device 1003 is mainly used for data interaction with the user; the processor 1001 and memory 1005 in the fabrication device for a 3D-printed six-dimensional force sensor of the present invention can be set in the fabrication device for a 3D-printed six-dimensional force sensor. The fabrication device for a 3D-printed six-dimensional force sensor calls the fabrication program for a 3D-printed six-dimensional force sensor stored in the memory 1005 through the processor 1001, and executes the fabrication method for a 3D-printed six-dimensional force sensor provided in the embodiment of the present invention.

[0023] This invention provides a method for fabricating a six-dimensional force sensor based on 3D printing, referring to... Figure 2 , Figure 2 This is a schematic flowchart of the first embodiment of a method for fabricating a six-dimensional force sensor based on 3D printing according to the present invention.

[0024] In this embodiment, the method for fabricating the six-dimensional force sensor based on 3D printing includes: Step S1: Print the metal elastomer skeleton according to the preset elastomer structure model, wherein the preset elastomer structure model is the three-dimensional structure model corresponding to the metal elastomer skeleton. In this embodiment, the preset elastomer structure model is a three-dimensional structural model corresponding to the metal elastomer skeleton, i.e., a pre-established CAD model of the metal elastomer skeleton. Its structural form can be selected from three classic configurations: a three-beam structure, a cross-beam structure, and a Stewart parallel structure. This embodiment uses metal material to print the elastomer skeleton, ensuring the overall stiffness and range of the sensor. Optionally, the preset elastomer structure model may also include a lattice-based lightweight structure located in the non-core force transmission region. The lattice unit is, for example, a body-centered cubic configuration or a three-period minimal surface configuration, with a relative density of 15% to 30% and a lattice wall thickness of 0.2 mm to 0.5 mm. This allows for a 40% to 55% weight reduction of the metal elastomer skeleton while maintaining overall stiffness. Furthermore, the lattice pores can serve as channels for the penetration and filling of piezoresistive and piezoelectric inks, enhancing the interfacial bonding strength between dissimilar materials.

[0025] Step S2: Print piezoresistive material ink in a predetermined printing area to obtain a piezoresistive sensing layer, and print piezoelectric material ink in an associated area of ​​the piezoresistive sensing layer to obtain a piezoelectric sensing layer, wherein the associated area includes: an area on the metal elastomer skeleton that is intersected or adjacent to the piezoresistive sensing layer. In this embodiment, the predetermined printing area is the high-strain region corresponding to the elastic beam of the metal elastomer skeleton. Specifically, the piezoresistive sensing layer is printed with piezoresistive material ink and can measure static and quasi-static forces; the piezoelectric sensing layer is printed with piezoelectric material ink and has significant advantages in sensitivity and dynamic response, used to measure dynamic and alternating forces; the associated region is the area on the metal elastomer skeleton that is interspersed or adjacent to the piezoresistive sensing layer, that is, the piezoelectric sensing layer and the piezoresistive sensing layer are interspersed or adjacent to each other in the high-strain concentration region of the elastic beam. Optionally, after the piezoelectric sensing layer is printed, it undergoes polarization treatment, for example, by corona discharge or contact polarization, with a polarization electric field strength of 30kV / cm to 80kV / cm, a polarization temperature of 80℃ to 100℃, and a polarization time of 30 minutes to 90 minutes, so that the piezoelectric coefficient d33 is not less than 12pC / N. By integrating the two sensing principles of piezoresistive and piezoelectric in situ, it is possible to achieve both high-precision measurement of static forces and high-frequency response of dynamic forces, thus overcoming the problem of limited measurement range of a single sensing mechanism.

[0026] Step S3: Print conductive ink at the electrode leads of the piezoresistive sensing layer and the electrode leads of the piezoelectric sensing layer to obtain a conductive interconnect layer, and print insulating material to obtain an insulating isolation layer. The conductive interconnect layer is used to connect the electrode leads to the signal output pads of the six-dimensional force sensor. In this embodiment, the conductive ink is, for example, silver nanowire ink or conductive carbon paste, with a printed linewidth of 100μm to 200μm and a layer thickness of 5μm to 15μm. The conductive interconnect layer connects the electrode leads of each piezoresistive and piezoelectric sensing unit to the signal output pads on the outer edge of the six-dimensional force sensor, forming a complete signal acquisition circuit network. The insulating material is, for example, UV-curable acrylate or epoxy resin, with a dielectric strength of not less than 15kV / mm after curing. The insulating isolation layer is printed at the intersections of the conductive traces and between the sensing units to achieve electrical isolation. This allows for in-situ formation of interconnect and isolation structures within the sensor, eliminating the need for additional wire bonding processes.

[0027] Step S4: Anneal and encapsulate the printed object to obtain the piezoresistive-piezoelectric hybrid six-dimensional force sensor.

[0028] In this embodiment, the annealing process involves subjecting the printed object to a low-temperature annealing at 100°C to 120°C for 2 to 4 hours to alleviate residual stress between the printed layers. The encapsulation process involves installing the annealed sensor core into a housing and extending signal wiring. This results in the piezoresistive-piezoelectric hybrid six-dimensional force sensor, where the metal elastomer framework and functional layers are integrated into a single structure. This low-temperature annealing eliminates residual stress between layers, ensuring the long-term stability of the sensor.

[0029] In this embodiment, a metal elastomer skeleton is printed according to a preset elastomer structure model. A piezoresistive sensing layer is obtained by printing piezoresistive material ink in a predetermined printing area, and a piezoelectric sensing layer is obtained by printing piezoelectric material ink in an associated area. Then, conductive ink is printed at the electrode lead-out end to obtain a conductive interconnect layer, and insulating material is printed to obtain an insulating isolation layer. Finally, the printed object is annealed and packaged. This allows the metal elastomer skeleton, piezoresistive sensing layer, piezoelectric sensing layer, conductive interconnect layer, and insulating isolation layer to be integrated into a single multi-material 3D printing process. This eliminates the need for traditional discrete processes such as patching, wire bonding, and multiple alignments, reducing quality control issues caused by manual intervention and process deviations. Furthermore, by integrating sensing layers based on both piezoresistive and piezoelectric principles onto the same rigid metal elastomer, the measurement range of the six-dimensional force sensor is significantly broadened, achieving both high-precision measurement of static forces and high-frequency response of dynamic forces.

[0030] Furthermore, based on the first embodiment, a second embodiment of the fabrication of the six-dimensional force sensor based on 3D printing of the present invention is proposed. In this embodiment, reference is made to... Figure 3 The step of printing the metal elastomer skeleton according to the preset elastomer structure model includes: Step S11: Under a protective atmosphere, a laser powder bed melting process is used to melt the preset metal material layer by layer to form the metal elastomer skeleton; The preset metal material includes: stainless steel powder, titanium alloy powder or maraging steel powder, and the protective atmosphere is nitrogen or argon. In this embodiment, the laser powder bed fusion process, also known as the L-PBF process, uses a fiber laser to melt metal powder layer by layer under a protective atmosphere. The preferred metal material is 17-4PH stainless steel powder, Ti6Al4V titanium alloy powder, or 18Ni300 maraging steel powder. The protective atmosphere is nitrogen or argon, and the oxygen content in the printing chamber is controlled below 1000 ppm to ensure molding quality. Specifically, the printing parameters are, for example, laser power of 200W to 500W, scanning speed of 300mm / s to 1500mm / s, and layer thickness of 30μm to 50μm. By integrally molding the metal elastomer skeleton through the laser powder bed fusion process, a high-stiffness, high-precision metal elastomer can be obtained, overcoming the defects of low elastic modulus and poor creep resistance of polymer elastomers.

[0031] Step S12: During the formation of the metal elastomer skeleton, the temperature of the printed substrate is controlled within a first temperature range. In this embodiment, the first temperature range is the temperature range that the printing substrate needs to maintain when printing the metal elastomer skeleton, for example, room temperature to 200°C. By controlling the temperature of the printing substrate within the first temperature range during the formation of the metal elastomer skeleton, the thermal stress during the metal melting process can be reduced, ensuring the molding accuracy and density of the metal elastomer skeleton.

[0032] Step S13: After the metal elastomer skeleton is formed, the printing substrate is controlled to cool down to the preset printing temperature at a preset cooling rate.

[0033] In this embodiment, the preset printing temperature is the temperature that meets the printing temperature requirements of the piezoresistive material ink, for example, 25±5℃; the preset cooling rate is 2℃ / min to 5℃ / min, that is, after the metal elastomer skeleton is formed, the printing substrate is controlled to be gradually cooled to the preset printing temperature at a rate of 2℃ / min to 5℃ / min, realizing the temperature transition from the high-temperature metal printing process to the low-temperature polymer printing process. The heat insulation structure is set between the printing substrate printing the metal elastomer skeleton and the worktable printing the piezoresistive material ink, for example, a heat insulation structure combining a ceramic heat insulation layer, circulating water cooling and local air cooling is used, and its temperature difference isolation capability can reach more than 500℃. Through the combination of gradient cooling and heat insulation structure, the process temperature conflict between the high-temperature process of metal powder bed melting and the low-temperature printing of piezoresistive material ink can be resolved, ensuring that the two dissimilar materials are formed sequentially in one printing process without thermal interference.

[0034] In this embodiment, a metal elastomer skeleton is formed by melting a preset metal material layer by layer under a protective atmosphere using a laser powder bed melting process. During the formation process, the temperature of the printing substrate is controlled within a first temperature range, and after the skeleton is formed, the printing substrate is controlled to cool down to a preset printing temperature at a preset cooling rate. This ensures the molding quality of the metal elastomer skeleton. Furthermore, the process temperature conflict between the high-temperature metal printing process and the low-temperature printing of piezoresistive ink is resolved through gradient cooling and a heat insulation structure, allowing the two dissimilar materials to be formed sequentially in a single printing process without thermal interference.

[0035] Furthermore, based on the first or second embodiment, a third embodiment of the fabrication of the six-dimensional force sensor based on 3D printing of the present invention is proposed. In this embodiment, before the step of printing piezoresistive material ink in the predetermined printing area to obtain the piezoresistive sensing layer, the method further includes: The predetermined printing area is subjected to surface activation treatment, wherein the predetermined printing area is the high strain region corresponding to the elastic beam of the metal elastomer skeleton; In this embodiment, the predetermined printing area is the high-strain region corresponding to the elastic beam of the metal elastomer skeleton, that is, the surface region where the strain of the elastic beam is concentrated under load. It should be noted that the surface energy of the metal formed by laser powder bed melting is low, and polymer-based inks such as piezoresistive inks have poor wettability and insufficient interfacial bonding strength on the untreated metal surface. Therefore, surface activation treatment is required before printing to provide good interfacial conditions for subsequent sensor layer printing.

[0036] The surface activation process includes: controlling an oxygen plasma treatment device to perform oxygen plasma activation treatment on the predetermined printing area, wherein the processing time of the oxygen plasma activation treatment is 30 seconds to 120 seconds; determining the contact angle of the predetermined printing area after the oxygen plasma activation treatment; and completing the surface activation treatment when the contact angle is lower than a preset contact angle threshold.

[0037] In this embodiment, the surface activation treatment employs oxygen plasma activation: an oxygen plasma treatment device is controlled to perform oxygen plasma activation treatment on the predetermined printing area, with a treatment power of, for example, 50W to 300W, and a treatment duration of 30 seconds to 120 seconds (e.g., 60 seconds). Subsequently, the contact angle of the predetermined printing area after oxygen plasma activation treatment is determined. When the contact angle is lower than a preset contact angle threshold (e.g., below 20°), the surface activation treatment is completed, and the process switches to the printing step of the piezoresistive ink. By using the contact angle as the quantitative criterion for activation completion, the interfacial bonding strength between the metal surface and the polymer-based sensing material can be guaranteed, preventing the sensing layer from delaminating under cyclic loading.

[0038] In this embodiment, by performing surface activation treatment on the predetermined printing area before printing the piezoresistive material ink, and using oxygen plasma activation treatment with the contact angle being lower than a preset contact angle threshold as the criterion for activation completion, the interfacial bonding strength between the metal elastomer skeleton and polymer-based functional materials such as the piezoresistive material ink can be significantly improved, avoiding delamination of the sensing layer under cyclic load and ensuring the long-term reliability of the sensor.

[0039] Furthermore, based on any of the above embodiments, a fourth embodiment of the fabrication of the six-dimensional force sensor based on 3D printing is proposed. In this embodiment, after the step of annealing and encapsulating the printed object to obtain the piezoresistive-piezoelectric hybrid six-dimensional force sensor, the method further includes: Obtain a calibration sample set, wherein each calibration sample in the calibration sample set includes: a piezoresistive signal corresponding to each piezoresistive sensing unit, a piezoelectric signal corresponding to each piezoelectric sensing unit, temperature data and time window feature data of the piezoresistive-piezoelectric hybrid six-dimensional force sensor, and a corresponding six-dimensional force standard value, wherein the time window feature data is the feature data of the piezoresistive signal and the piezoelectric signal within a preset time window; In this embodiment, the calibration sample set is acquired through a high-precision six-axis joint calibration platform, for example, acquiring 1000 to 2000 calibration samples, covering different force / torque combinations and different temperature conditions. Each calibration sample includes: a piezoresistive signal corresponding to each piezoresistive sensing unit, a piezoelectric signal corresponding to each piezoelectric sensing unit, temperature data and time window feature data of the piezoresistive-piezoelectric hybrid six-dimensional force sensor, and a six-dimensional force standard value corresponding to the calibration sample; wherein, the temperature data is used for temperature drift compensation, and the time window feature data is the feature data of the piezoresistive signal and the piezoelectric signal within a preset time window, used for dynamic characteristic analysis. This provides supervised data covering multiple operating conditions for training the decoupled mapping model.

[0040] An extended feature vector is constructed for each calibration sample based on the piezoresistive signal, the piezoelectric signal, the temperature data, and the time window feature data in each calibration sample. In this embodiment, the piezoresistive signal, the piezoelectric signal, the temperature data, and the time window feature data in each calibration sample are concatenated to construct an extended feature vector corresponding to each calibration sample, as shown in the following formula:

[0041] Where X is the extended feature vector. to Let m be the piezoresistive signals corresponding to the m piezoresistive sensing units. to Let m be the piezoelectric signal corresponding to n piezoelectric sensing units, and m and n be the number of piezoresistive sensing units and piezoelectric sensing units, respectively, with the sum of m and n not less than 36. Let T be the temperature data and t be the time window feature data. By incorporating the temperature data and time window feature data into the feature vector, the decoupled mapping model obtained through subsequent training can simultaneously possess temperature drift compensation capability and dynamic characteristic characterization capability.

[0042] The preset neural network is trained based on multiple extended feature vectors and the corresponding six-dimensional force standard values ​​to obtain a decoupled mapping model, wherein the decoupled mapping model is used to determine the six-dimensional force standard values ​​based on the output signals of the piezoresistive sensing layer and the piezoelectric sensing layer.

[0043] In this embodiment, the pre-defined neural network is trained using multiple extended feature vectors as inputs and the corresponding six-dimensional force standard values ​​as supervision labels to obtain the decoupling mapping model. The pre-defined neural network is, for example, a 3- to 4-layer BP neural network, or a random forest regression model. The decoupling mapping model is used to determine the six-dimensional force standard values ​​based on the output signals of the piezoresistive sensing layer and the piezoelectric sensing layer, and its mapping relationship is shown in the following formula.

[0044]

[0045] In formula (2), , , These are the force components in three directions of space. , , These are the torque components in three spatial directions. The decoupling mapping model obtained through training is represented by X, which is the extended feature vector. Specifically, the decoupling mapping relationship for the three-beam structure model and the cross-beam structure model is 12 inputs × 6 outputs, while the decoupling mapping relationship for the Stewart parallel structure model is 24 inputs × 6 outputs. Due to the high measurement redundancy of the Stewart parallel structure, its decoupling accuracy is superior. By replacing the traditional linear mapping matrix with a nonlinear mapping model for decoupling, inter-dimensional coupling and temperature drift can be effectively reduced, thereby improving the comprehensive decoupling accuracy of the six-dimensional forces.

[0046] In this embodiment, by acquiring a calibration sample set containing piezoresistive signals, piezoelectric signals, temperature data, time window feature data, and corresponding six-dimensional force standard values, an extended feature vector is constructed and a preset neural network is trained to obtain a decoupling mapping model. This model can establish a nonlinear mapping relationship from the dual-modal output signal to the six-dimensional force, and use temperature data and time window feature data to compensate for temperature drift and characterize dynamic characteristics, effectively reducing inter-dimensional coupling. Compared with the linear mapping matrix decoupling method, it significantly improves the decoupling accuracy of the six-dimensional force.

[0047] Furthermore, the piezoresistive signal and the piezoelectric signal are acquired according to the following steps: The piezoresistive sensing layer is connected to a Wheatstone bridge circuit excited by a constant voltage source, and the output signal of the Wheatstone bridge circuit is differentially amplified and low-pass filtered to obtain the piezoresistive signal. In this embodiment, the piezoresistive sensing layer is connected to a Wheatstone bridge circuit excited by a constant voltage source. The Wheatstone bridge circuit converts the resistance change of the piezoresistive sensing unit into a voltage output. The output signal of the Wheatstone bridge circuit is differentially amplified and low-pass filtered to suppress high-frequency noise, thus obtaining the piezoresistive signal. This results in a stable, low-noise quasi-static force measurement signal.

[0048] The piezoelectric sensing layer is connected to a charge amplifier, and the output signal of the charge amplifier is bandpass filtered to obtain the piezoelectric signal. In this embodiment, the piezoelectric sensing layer is connected to a charge amplifier with high input impedance. The charge amplifier converts the charge signal output by the piezoelectric sensing unit into a voltage signal. The output signal of the charge amplifier is then bandpass filtered to obtain the piezoelectric signal. This preserves the effective frequency components of the dynamic force and suppresses low-frequency drift and high-frequency interference.

[0049] The piezoresistive signal and the piezoelectric signal are respectively converted from analog to digital, wherein the piezoresistive signal is a DC voltage signal reflecting quasi-static force, and the piezoelectric signal is an AC voltage signal reflecting dynamic force.

[0050] In this embodiment, the piezoresistive signal and the piezoelectric signal are respectively subjected to analog-to-digital conversion, for example, sampling using a 16-bit to 24-bit analog-to-digital converter. The piezoresistive signal is a DC voltage signal reflecting quasi-static force, and the piezoelectric signal is an AC voltage signal reflecting dynamic force. Optionally, a frequency-domain weighted fusion strategy can be adopted for subsequent signal fusion: in the quasi-static range, generally below 10Hz, the piezoresistive signal dominates; in the dynamic range, generally above 1Hz, the piezoelectric signal dominates; and in the transition frequency band from 1Hz to 10Hz, an adaptive complementary filter is used to achieve a smooth transition. This enables the dual-mode signals to complement each other across the entire frequency band, significantly outperforming a single sensing mechanism.

[0051] In this embodiment, a piezoresistive signal is obtained by connecting the piezoresistive sensing layer to a Wheatstone bridge circuit excited by a constant voltage source and then performing differential amplification and low-pass filtering. A piezoelectric signal is obtained by connecting the piezoelectric sensing layer to a charge amplifier and then performing band-pass filtering. The two signals are then converted from analog to digital, thereby obtaining a DC voltage signal reflecting quasi-static force and an AC voltage signal reflecting dynamic force, respectively, providing high-quality acquisition data for the fusion and decoupling of dual-mode signals.

[0052] Furthermore, based on any of the above embodiments, a fifth embodiment of the fabrication of a six-dimensional force sensor based on 3D printing is proposed. In this embodiment, the step of printing piezoresistive material ink in a predetermined printing area to obtain a piezoresistive sensing layer includes: A piezoresistive material ink is defined, wherein the piezoresistive material ink comprises: a conductive filler, a polydimethylsiloxane prepolymer, and a curing agent, wherein the conductive filler is a graphene nanosheet or a multi-walled carbon nanotube; In this embodiment, the piezoresistive ink comprises a conductive filler, a polydimethylsiloxane (PDMS) prepolymer, and a curing agent. The conductive filler is graphene nanosheets or multi-walled carbon nanotubes; wherein the graphene nanosheets have a diameter of, for example, 2 μm to 10 μm and no more than 5 layers. Specifically, the conductive filler is uniformly dispersed in a mixture of the PDMS prepolymer and the curing agent, and an organic solvent is added to adjust the viscosity to 1.0 Pa·s to 10.0 Pa·s to meet the jetting requirements of Direct Ink Writing (DIW). This allows the piezoresistive ink to possess both printability and piezoresistive sensitivity.

[0053] The piezoresistive material ink is printed into a preset sensing pattern in the predetermined printing area using a direct writing process. The preset sensing pattern includes an axial piezoresistive strip arranged along the axis of the elastic beam.

[0054] In this embodiment, the direct-write forming process, also known as the DIW process, uses a dispensing needle with a 15μm to 50μm aperture to print the piezoresistive material ink into a preset sensing pattern on a predetermined printing area. The printing layer thickness is 30μm to 100μm, and the line width is 150μm to 300μm. The preset sensing pattern includes axial piezoresistive strips arranged along the axis of the elastic beam; wherein, the axial piezoresistive strips are used to sense bending strain, corresponding to the measurement of vertical and horizontal force components. Specifically, the number of piezoresistive sensing units depends on the number of elastic beams: a three-beam structure has 24 piezoresistive sensing units, a cross-beam structure has 24 piezoresistive sensing units, and a Stewart parallel structure has 24 piezoresistive sensing units.

[0055] The printed preset sensing pattern is cured to obtain the piezoresistive sensing layer.

[0056] In this embodiment, the printed preset sensing pattern is cured, for example by holding at 80°C for 1 to 2 hours, or by ultraviolet light curing, to obtain the piezoresistive sensing layer. This allows the piezoresistive material ink to be shaped into a stable piezoresistive sensing layer, ensuring the stability of its piezoresistive characteristics.

[0057] In this embodiment, by determining a piezoresistive material ink containing conductive filler, polydimethylsiloxane prepolymer and curing agent, a pre-defined sensing pattern including axial piezoresistive strips and shear piezoresistive strips is printed in a predetermined printing area using a direct writing molding process. The pre-defined sensing pattern is then cured, thereby enabling the in-situ formation of a piezoresistive sensing layer in the high-strain region of the metal elastomer skeleton. This allows the axial piezoresistive strips to sense bending strain and the shear piezoresistive strips to sense shear strain, providing a sensing pattern that matches the strain direction for the decoupled measurement of each component of the six-dimensional force.

[0058] Furthermore, based on any of the above embodiments, a sixth embodiment of the fabrication of the six-dimensional force sensor based on 3D printing of the present invention is proposed. In this embodiment, the preset elastomer structure model includes any of the following: The three-beam structure model includes: a central loading platform, an outer fixing ring, and three radial main beams evenly distributed at 120° angles to each other; In this embodiment, the three-beam structure model includes a central loading platform, an outer fixing ring, and three radial main beams / side beams evenly distributed at 120° angles to each other. The three radial main beams / side beams are completely symmetrical in the circumferential direction and have good isotropic mechanical properties. Its strain response characteristics are as follows: under the action of a vertical force Fz, the three radial main beams simultaneously bend upwards or downwards, generating radial tensile or compressive strain in the same direction; under the action of a horizontal force... / The strain amplitudes of the three radial main beams / side beams are decomposed into components along the directions of each radial side beam. These strain amplitudes are distributed according to the cosθ law. The magnitude and direction of the horizontal force can be reconstructed through vector synthesis of the three-channel signals. Torque... This causes bending deformation in the three radial side beams; torque / The two radial main beams perpendicular to it bend in opposite directions, and decoupling is achieved through differential measurement. For example, a six-dimensional force sensor with a three-beam structure has 24 piezoresistive sensing units and 12 piezoelectric sensing units. The sensor has an outer diameter of Φ30mm, a total height of 12mm, and a weight of about 18g, with an overall accuracy of 0.2%FS. Therefore, it can be used in applications with strict space and weight requirements, such as humanoid robot finger joints and lightweight collaborative robot end effects.

[0059] The cross-beam structure model includes: a central bearing platform, an outer fixing ring, and four orthogonally distributed elastic beams; In this embodiment, the cross-beam structure model includes a central support platform, an outer fixing ring, and four orthogonally distributed elastic beams, which are orthogonally distributed along the X and Y axes. Its strain response characteristics are as follows: under the action of a vertical force Fz, all four elastic beams bend simultaneously, generating radial strain in the same direction; a horizontal force Fx causes one elastic beam in the X direction to be under tension and the other under compression. Make the two elastic beams in the Y direction opposite in direction; torque This causes all four elastic beams to bend and deform; torque / The two elastic beams in the Y and X directions are respectively subjected to bending strains in opposite directions. For example, a six-dimensional force sensor with a cross-beam structure has 24 piezoresistive sensing units and 12 piezoelectric sensing units. The sensor has an outer diameter of Φ50mm, a thickness of 15mm, and weighs approximately 45g, with an overall accuracy of 0.3%FS. The cross-beam structure has good symmetry and is relatively easy to decouple, making it suitable for general force control applications such as industrial robots and collaborative robots.

[0060] The Stewart parallel structure model includes: an upper platform, a lower platform, and six elastic pillars with flexible hinges at both ends. The six elastic pillars are arranged in parallel between the upper platform and the lower platform. The metal elastomer skeleton is a one-piece structure formed in one piece.

[0061] In this embodiment, the Stewart parallel structure model includes an upper platform, a lower platform, and six elastic supports with flexible hinges at both ends. The six elastic supports are arranged in parallel between the upper and lower platforms, meaning that the two ends of each elastic support are evenly distributed on the upper and lower platforms, respectively. Each of the six elastic supports bears its own load independently. The metal elastomer skeleton is a one-piece structure without any assembly parts. Specifically, each elastic support has one piezoresistive sensing unit and one piezoelectric sensing unit at each end, totaling 24 piezoresistive sensing units and 12 piezoelectric sensing units. By decoupling the strain signals from the six elastic supports in parallel, high-precision six-dimensional force output can be obtained. For example, a six-dimensional force sensor with a Stewart parallel structure has an outer diameter of Φ70mm, a height of 32mm, a weight of approximately 65g, a comprehensive accuracy of 0.1%FS, inter-dimensional coupling not exceeding 0.5%FS, and a natural frequency not lower than 2kHz. Stewart parallel structures offer extremely high stiffness, precision, and repeatability, making them suitable for applications with the highest requirements for stiffness and precision, such as aerospace, precision assembly, and humanoid robot ankle joints.

[0062] In this embodiment, by setting the preset elastomer structure model as any one of the three-beam structure model, cross-beam structure model, or Stewart parallel structure model, a six-dimensional force sensor with compact and lightweight structure, easy decoupling, or high stiffness and accuracy can be obtained respectively, so as to adapt to different application scenarios such as humanoid robot finger joints, general industrial robots, and aerospace precision assembly. Moreover, all three structures can be integrally formed by a one-time multi-material 3D printing process.

[0063] Furthermore, this invention also proposes a six-dimensional force sensor based on 3D printing, with appended... Figure 4 This is a top-view schematic diagram of the elastic body structure in the six-dimensional force sensor of this invention. (Attached) Figure 5 This is a top view schematic diagram of the elastic body structure. (Attached) Figure 6 This is a schematic diagram of the Stewart parallel structure elastic body. (Attached) Figure 7 This is a schematic diagram of the sensor unit layout in a single support column. The 3D-printed six-dimensional force sensor includes: a metal elastomer skeleton, a piezoresistive sensing layer, a piezoelectric sensing layer, a conductive interconnect layer, and an insulating layer. The piezoresistive and piezoelectric sensing layers are located in the high-strain regions corresponding to the elastic beams of the metal elastomer skeleton. The conductive interconnect layer connects the electrode leads of the piezoresistive and piezoelectric sensing layers. The insulating layer is located at the intersections of the conductive interconnect layers. The metal elastomer skeleton, the piezoresistive sensing layer, the piezoelectric sensing layer, the conductive interconnect layer, and the insulating layer are an integral structure formed by performing the aforementioned 3D-printed six-dimensional force sensor fabrication method.

[0064] Furthermore, this invention also proposes a fabrication apparatus for a 3D-printed six-dimensional force sensor. The apparatus includes a memory, a processor, and a fabrication program for the 3D-printed six-dimensional force sensor stored in the memory and executable on the processor. The fabrication program for the 3D-printed six-dimensional force sensor is configured to implement the steps of the fabrication method for the 3D-printed six-dimensional force sensor described above.

[0065] Furthermore, this embodiment of the invention also proposes a storage medium storing a fabrication program for a 3D-printed six-dimensional force sensor. When the fabrication program for the 3D-printed six-dimensional force sensor is executed by a processor, it implements the steps of the fabrication method for the 3D-printed six-dimensional force sensor described above.

[0066] It should be noted that, in this document, the terms "comprising," "including," or any other variations thereof are intended to cover non-exclusive inclusion, such that a process, method, article, or system that comprises a list of elements includes not only those elements but also other elements not expressly listed, or elements inherent to such a process, method, article, or system. Unless otherwise specified, an element defined by the phrase "comprising one..." does not exclude the presence of other identical elements in the process, method, article, or system that includes that element.

[0067] The sequence numbers of the above embodiments of the present invention are for descriptive purposes only and do not represent the superiority or inferiority of the embodiments.

[0068] Through the above description of the embodiments, those skilled in the art can clearly understand that the methods of the above embodiments can be implemented by means of software plus necessary general-purpose hardware platforms. Of course, they can also be implemented by hardware, but in many cases the former is a better implementation method. Based on this understanding, the technical solution of the present invention, or the part that contributes to the prior art, can be embodied in the form of a software product. This computer software product is stored in a storage medium (such as ROM / RAM, magnetic disk, optical disk) as described above, and includes several instructions to cause a terminal device (which may be a mobile phone, computer, server, or network device, etc.) to execute the methods described in the various embodiments of the present invention.

[0069] The above are merely preferred embodiments of the present invention and do not limit the scope of the patent. Any equivalent structural or procedural transformations made based on the description and drawings of the present invention, or direct or indirect applications in other related technical fields, are similarly included within the scope of patent protection of the present invention.

Claims

1. A method for fabricating a six-dimensional force sensor based on 3D printing, characterized in that, The method for fabricating the 3D-printed six-dimensional force sensor includes the following steps: Print the metal elastomer skeleton according to the preset elastomer structure model, wherein the preset elastomer structure model is the three-dimensional structure model corresponding to the metal elastomer skeleton; Piezoresistive material ink is printed in a predetermined printing area to obtain a piezoresistive sensing layer, and piezoelectric material ink is printed in an associated area of ​​the piezoresistive sensing layer to obtain a piezoelectric sensing layer, wherein the associated area includes: an area on the metal elastomer skeleton that is intersected or adjacent to the piezoresistive sensing layer. Conductive ink is printed at the electrode leads of the piezoresistive sensing layer and the electrode leads of the piezoelectric sensing layer to obtain a conductive interconnect layer, and insulating material is printed to obtain an insulating isolation layer. The conductive interconnect layer is used to connect the electrode leads to the signal output pads of the six-dimensional force sensor. The printed object is annealed and encapsulated to obtain the piezoresistive-piezoelectric hybrid six-dimensional force sensor. The step of printing the metal elastomer skeleton according to the preset elastomer structure model includes: A pre-set metal material is melted layer by layer using a laser powder bed melting process under a protective atmosphere to form the metal elastomer skeleton. The pre-set metal material includes, but is not limited to, stainless steel powder, titanium alloy powder or maraging steel powder. The protective atmosphere is nitrogen or argon. During the formation of the metal elastomer skeleton, the temperature of the printed substrate is controlled within a first temperature range. After the metal elastomer skeleton is formed, the printing substrate is controlled to cool down to a preset printing temperature at a preset cooling rate, wherein the preset cooling rate is 2℃ / min to 5℃ / min, the preset printing temperature meets the printing temperature requirements of the piezoresistive material ink, and a heat insulation structure is provided between the printing substrate and the worktable for printing the piezoresistive material ink. The step of printing piezoresistive material ink in a predetermined printing area to obtain a piezoresistive sensing layer, and printing piezoelectric material ink in the associated area of ​​the piezoresistive sensing layer to obtain a piezoelectric sensing layer further includes: performing polarization treatment on the piezoelectric sensing layer after the printing of the piezoelectric sensing layer is completed.

2. The method for fabricating a six-dimensional force sensor based on 3D printing as described in claim 1, characterized in that, Before the step of printing piezoresistive material ink in the predetermined printing area to obtain the piezoresistive sensing layer, the method further includes: The predetermined printing area is subjected to surface activation treatment, wherein the predetermined printing area is the high strain region corresponding to the elastic beam of the metal elastomer skeleton; The surface activation process includes: controlling an oxygen plasma treatment device to perform oxygen plasma activation treatment on the predetermined printing area, wherein the processing time of the oxygen plasma activation treatment is 30 seconds to 120 seconds; determining the contact angle of the predetermined printing area after the oxygen plasma activation treatment; and completing the surface activation treatment when the contact angle is lower than a preset contact angle threshold.

3. The method for fabricating a six-dimensional force sensor based on 3D printing as described in claim 1, characterized in that, After the step of annealing and encapsulating the printed object to obtain the piezoresistive-piezoelectric hybrid six-dimensional force sensor, the method further includes: Obtain a calibration sample set, wherein each calibration sample in the calibration sample set includes: a piezoresistive signal corresponding to each piezoresistive sensing unit, a piezoelectric signal corresponding to each piezoelectric sensing unit, temperature data and time window feature data of the piezoresistive-piezoelectric hybrid six-dimensional force sensor, and a corresponding six-dimensional force standard value, wherein the time window feature data is the feature data of the piezoresistive signal and the piezoelectric signal within a preset time window; An extended feature vector is constructed for each calibration sample based on the piezoresistive signal, the piezoelectric signal, the temperature data, and the time window feature data in each calibration sample. The preset neural network is trained based on multiple extended feature vectors and the corresponding six-dimensional force standard values ​​to obtain a decoupled mapping model, wherein the decoupled mapping model is used to determine the six-dimensional force standard values ​​based on the output signals of the piezoresistive sensing layer and the piezoelectric sensing layer.

4. The method for fabricating a six-dimensional force sensor based on 3D printing as described in claim 3, characterized in that, The piezoresistive signal and the piezoelectric signal are acquired according to the following steps: The piezoresistive sensing layer is connected to a Wheatstone bridge circuit excited by a constant voltage source, and the output signal of the Wheatstone bridge circuit is differentially amplified and low-pass filtered to obtain the piezoresistive signal. The piezoelectric sensing layer is connected to a charge amplifier, and the output signal of the charge amplifier is bandpass filtered to obtain the piezoelectric signal. The piezoresistive signal and the piezoelectric signal are respectively converted from analog to digital, wherein the piezoresistive signal is a DC voltage signal reflecting quasi-static force, and the piezoelectric signal is an AC voltage signal reflecting dynamic force.

5. The method for fabricating a six-dimensional force sensor based on 3D printing as described in claim 1, characterized in that, The step of printing piezoresistive material ink in a predetermined printing area to obtain a piezoresistive sensing layer includes: A piezoresistive material ink is defined, wherein the composition of the piezoresistive material ink includes, but is not limited to: conductive filler, polydimethylsiloxane prepolymer and curing agent, wherein the conductive filler includes, but is not limited to, graphene nanosheets or multi-walled carbon nanotubes. The piezoresistive material ink is printed into a preset sensing pattern in the predetermined printing area using a direct writing process. The preset sensing pattern is an axial piezoresistive strip arranged along the axis of the elastic beam. The printed preset sensing pattern is cured to obtain the piezoresistive sensing layer.

6. The method for fabricating a six-dimensional force sensor based on 3D printing as described in any one of claims 1 to 5, characterized in that, The preset elastomer structure model includes any of the following: The three-beam structure model includes: a central loading platform, an outer fixing ring, and three radial main beams evenly distributed at 120° angles to each other; The cross-beam structure model includes: a central bearing platform, an outer fixing ring, and four orthogonally distributed elastic beams; The Stewart parallel structure model includes: an upper platform, a lower platform, and six elastic pillars with flexible hinges at both ends. The six elastic pillars are arranged in parallel between the upper platform and the lower platform. The metal elastomer skeleton is a one-piece structure formed in one piece.

7. A six-dimensional force sensor based on 3D printing, characterized in that, The 3D-printed six-dimensional force sensor comprises: a metal elastomer skeleton, a piezoresistive sensing layer, a piezoelectric sensing layer, a conductive interconnect layer, and an insulating layer, wherein: The piezoresistive sensing layer and the piezoelectric sensing layer are arranged in the high-strain region corresponding to the elastic beam of the metal elastomer skeleton. The conductive interconnect layer connects the electrode leads of the piezoresistive sensing layer and the electrode leads of the piezoelectric sensing layer; The insulating isolation layer is disposed at the intersection of the conductive interconnect layers; The metal elastomer skeleton, the piezoresistive sensing layer, the piezoelectric sensing layer, the conductive interconnect layer, and the insulating isolation layer are an integral structure formed by the fabrication method of the six-dimensional force sensor based on 3D printing as described in claim 1.

8. A fabrication apparatus for a six-dimensional force sensor based on 3D printing, characterized in that, The device includes: a memory, a processor, and a fabrication program for a 3D-printed six-dimensional force sensor stored in the memory and executable on the processor, the fabrication program for the 3D-printed six-dimensional force sensor being configured to implement the steps of the fabrication method for a 3D-printed six-dimensional force sensor as described in any one of claims 1 to 6.

9. A storage medium, characterized in that, The storage medium stores a fabrication program for a 3D-printed six-dimensional force sensor, which, when executed by a processor, implements the steps of the fabrication method for a 3D-printed six-dimensional force sensor as described in any one of claims 1 to 6.

Citation Information

Patent Citations

  • 3D printing method and system for complicated parts based on curved surface layering

    CN107187056A

  • Manufacturing apparatus for physical sensor using 3D printing and the physical sensor

    KR1020180049495A

  • Hybrid strain sensor combining a piezoelectric gauge and a resistive gauge

    WO2025214740A1