A ceramic body coating heating system
Patent Information
- Application Number
- CN202611377965.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-07
- Publication Date
- 2026-10-27
AI Technical Summary
[0006]本发明的目的在于克服上述技术不足,提供一种陶瓷体镀膜加热系统,解决了现有技术中陶瓷体镀膜需多次进出炉换面,导致耗时长且膜层质量不均的问题
[0017]与现有技术相比,本发明提供的一种陶瓷体镀膜加热系统,通过第一喷淋件可转动地安装于移动件,放置件安装于第一喷淋件,驱动件安装于移动件并与第一喷淋件传动连接,驱动件配置为驱动第一喷淋件、放置件同步转动,放置件上沿周向设有多个安装区,各个安装区被配置为平行且间隔地承载多个陶瓷体,第一喷淋件被设置为朝向安装区的内侧喷射反应液,喷液机构包括第二喷淋件,第二喷淋件安装于炉体一侧,第二喷淋件被配置为经由炉体侧壁的条形孔朝向各个安装区的外侧喷射反应液;通过第一喷淋件和第二喷淋件相配合,第一喷淋件朝安装区的内侧喷射反应液,第二喷淋件朝安装区的外侧喷射反应液,通过内外结合的立体喷射方式,反应液可从不同方向同时作用于陶瓷体表面,确保所有陶瓷体的各个方位均被均匀、完整地覆盖,避免漏喷,从而实现全方位无死角的膜层沉积。
Smart Images

Figure CN122979870A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of ceramic body production technology, and more specifically to a ceramic body coating heating system. Background Technology
[0002] In the manufacturing process of ceramic insulators, chemical vapor deposition is the core technology for forming high-quality functional films. This process typically requires tin tetrachloride as a precursor, which is then deposited on the ceramic surface through a pyrolysis reaction at high temperature to form a dense and uniform tin dioxide film.
[0003] To meet the needs of industrial production, existing technologies often employ a hanging cage to support multiple ceramic bodies and send them into a high-temperature furnace for continuous or semi-continuous heat treatment.
[0004] However, existing sidewall spraying processes have significant technical limitations when processing ceramic bodies with complex geometries (such as cylinders) or requiring all-around coating. Because the spraying assembly is typically fixed at a specific location on the furnace sidewall, the atomized chemical solution, limited by its linear propagation characteristics, often only covers the side of the ceramic body facing the spray nozzle. For cylindrical ceramic bodies, the side facing away from the spray nozzle is prone to forming a "shadow zone," resulting in missing or severely insufficient film thickness.
[0005] The existing production process is forced to adopt a cumbersome "double-furnace entry" process, which involves spraying a coating onto one side of the ceramic body, then removing the cage from the high-temperature furnace, allowing it to cool, or flipping and adjusting the ceramic body using a robotic arm, before moving it back into the high-temperature zone of the furnace for a second spraying. This segmented processing mode has significant drawbacks: First, frequent furnace entry and exit operations disrupt the continuity of the heat treatment process, significantly lengthening the production cycle and severely restricting capacity; second, it is difficult to accurately reproduce the temperature field environment during the first furnace entry process when the ceramic body is removed and re-entered, and temperature fluctuations can easily lead to differences in the crystal quality, adhesion, and photoelectric properties of the two deposited films, forming obvious "joints" or performance gaps; finally, repeated heating and cooling cycles also greatly increase energy consumption and equipment wear. Summary of the Invention
[0006] The purpose of this invention is to overcome the above-mentioned technical deficiencies and provide a ceramic body coating heating system that solves the problem that the ceramic body coating process in the prior art requires multiple furnace entry and exit for surface changes, resulting in long processing time and uneven film quality.
[0007] To achieve the above-mentioned technical objectives, the present invention adopts the following technical solution: This invention provides a ceramic body coating heating system, comprising: The furnace body has a cavity defined inside and is open at one end. The side wall of the furnace body is provided with a strip-shaped hole communicating with the cavity. A conveying mechanism includes a movable component, a first spray component, a placement component, and a driving component. The first spray component is rotatably mounted on the movable component, the placement component is mounted on the first spray component, and the driving component is mounted on the movable component and drivenly connected to the first spray component. The driving component is configured to drive the first spray component and the placement component to rotate synchronously. The placement component has multiple mounting areas along its circumference, and each mounting area is configured to carry multiple ceramic bodies in parallel and at intervals. The first spray component is configured to spray reaction liquid toward the inner side of the mounting area. The movable component is configured to drive the placement component to move into or out of the cavity through an opening. The liquid spraying mechanism includes a second spray element mounted on one side of the furnace body, the second spray element being configured to spray the reaction liquid outwards toward each of the mounting areas via strip-shaped holes.
[0008] In some embodiments, the first spray member includes a rotating shaft and a plurality of spray heads. The rotating shaft is rotatably mounted on a movable member. A liquid guiding cavity is provided in the rotating shaft along the axial direction and the end is open. The plurality of spray heads are arranged at intervals along the circumference of the rotating shaft and communicate with the liquid guiding cavity. The plurality of spray heads extend along the axial direction of the rotating shaft.
[0009] In some embodiments, the placement member includes a frame, a plurality of support portions and a locking portion. The frame is mounted on a rotating shaft and has a plurality of mounting areas along its circumference. A limiting channel with an insertion port is provided at one end of each mounting area. The support portions are configured to support a plurality of ceramic bodies in parallel and at intervals, and the support portions can move into or out of the limiting channel via the insertion ports. The locking portion is configured to be detachably connected to the frame to close or open the plurality of insertion ports.
[0010] In some embodiments, the supporting part includes a square frame, the square frame includes two horizontal bars and two vertical bars connected between the two horizontal bars, wherein one horizontal bar is provided with a plurality of through holes spaced apart, and the other horizontal bar is provided with a plurality of clearance grooves spaced apart, and each clearance groove is coaxially aligned with each of the through holes.
[0011] In some embodiments, the locking part is a baffle and a plurality of locking bolts; The baffle has multiple connecting holes, and the locking bolt passes through the connecting holes and is screwed into the threaded holes on the frame to fix the baffle to the frame.
[0012] In some embodiments, the spraying mechanism further includes a moving component and two clamping modules. The moving component is mounted on one side of the furnace body and has a reciprocating translational end. The two clamping modules are mounted opposite to each other on the translational end. The clamping module includes a support part, a blocking part, and a locking bolt. The support part is installed on the translation end and has a groove. The locking bolt is screwed to the blocking part. The blocking part is connected to the support part. The blocking part has a first state and a second state. In the first state, the blocking part opens the groove and forms a bayonet. In the second state, the blocking part closes the groove and forms a locking space. One end of the locking bolt can extend into the locking space and abut against the second spray element that passes through the locking space.
[0013] In some embodiments, the first liquid storage container is detachably mounted on the translation end, and a branch pipe connected to the second spray member extends downward to the bottom of the first liquid storage container, wherein the second spray member is connected to the air supply member.
[0014] In some embodiments, a limiting module is also installed on the translation end and between the two clamping modules. The limiting module defines a cavity, and the top of the cavity has an opening. The lower end of the first liquid storage container passes through the opening and is accommodated in the cavity. The outer wall contour of the first liquid storage container is adapted to the inner wall contour of the cavity, and the outer diameter of the first liquid storage container matches the inner diameter of the cavity.
[0015] In some embodiments, a limiting bolt is also screwed onto the limiting module, one end of which can extend into the cavity and abut against the outer wall of the first liquid storage container.
[0016] In some embodiments, the first air supply component is an air compressor.
[0017] Compared with the prior art, the present invention provides a ceramic body coating heating system, in which a first spraying component is rotatably mounted on a moving component, a placement component is mounted on the first spraying component, and a driving component is mounted on the moving component and connected to the first spraying component for transmission. The driving component is configured to drive the first spraying component and the placement component to rotate synchronously. The placement component has multiple installation areas along its circumference, and each installation area is configured to support multiple ceramic bodies in parallel and at intervals. The first spraying component is configured to spray reaction liquid toward the inner side of the installation area. The spraying mechanism includes a second spraying component, which is mounted on one side of the furnace body and configured to spray reaction liquid toward the outer side of each installation area through strip-shaped holes in the side wall of the furnace body. By cooperating with the first spraying component and the second spraying component, the first spraying component sprays reaction liquid toward the inner side of the installation area, and the second spraying component sprays reaction liquid toward the outer side of the installation area. Through the three-dimensional spraying method combining the inner and outer sides, the reaction liquid can act on the surface of the ceramic body from different directions simultaneously, ensuring that all aspects of all ceramic bodies are uniformly and completely covered, avoiding missed spraying, thereby achieving all-round film deposition without dead angles. Attached Figure Description
[0018] Figure 1 This is a schematic diagram of the structure of a ceramic body coating heating system provided by the present invention; Figure 2 This is a schematic diagram showing the connection between the liquid spraying mechanism and the furnace body provided by the present invention; Figure 3 yes Figure 2 Enlarged view of region A in the middle; Figure 4 This is a schematic diagram of the connection between the first spray component and the placement component provided by the present invention; Figure 5 This is a partial structural schematic diagram of the conveying mechanism provided by the present invention; Figure 6 This is a schematic diagram of the structure of the first spray component provided by the present invention; Figure 7 This is a schematic diagram of the structure of the support portion provided by the present invention; Figure 8 This is a schematic diagram of the structure of the moving part provided by the present invention; Figure 9 This is a schematic diagram of the clamping module provided by the present invention. Detailed Implementation
[0019] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative and not intended to limit the invention.
[0020] To address the technical problem in existing ceramic coating technologies that require multiple furnace passes for surface changes, resulting in long processing times and uneven film quality, this invention provides a ceramic coating heating system. A second spray element 31 sprays a reaction liquid onto the outer side of the installation area from the outside of the furnace body 1. Simultaneously, a first spray element 22 sprays the reaction liquid from the inside of the furnace body 1 towards the inner side of the installation area. This combined internal and external three-dimensional spraying method allows the reaction liquid to act on the ceramic surface from different directions simultaneously, ensuring that all aspects of the ceramic are uniformly and completely covered.
[0021] Please see Figures 1-9 , Figures 1-9A ceramic body coating heating system provided in one embodiment of the present invention includes a furnace body 1, a conveying mechanism 2, and a spraying mechanism 3. The furnace body 1 defines a cavity 1a with one end open. The side wall of the furnace body 1 has a strip-shaped hole 1b communicating with the cavity 1a. The conveying mechanism 2 includes a moving component 21, a first spray component 22, a placement component 23, and a driving component 24. The first spray component 22 is rotatably mounted on the moving component 21, the placement component 23 is mounted on the first spray component 22, and the driving component 24 is mounted on the moving component 21 and is drively connected to the first spray component 22. The first spray member 22 and the placement member 23 are configured to rotate synchronously. The placement member 23 has multiple installation areas along the circumferential direction. Each installation area is configured to support multiple ceramic bodies in parallel and at intervals. The first spray member 22 is configured to spray the reaction liquid toward the inner side of the installation area. The moving member 21 is configured to drive the placement member 23 to move into or out of the cavity 1a through the opening. The spraying mechanism 3 includes a second spray member 31, which is installed on one side of the furnace body 1. The second spray member 31 is configured to spray the reaction liquid toward the outer side of each installation area through the strip hole 1b.
[0022] In one embodiment, the furnace body 1 is constructed as a high-temperature furnace body, and its interior is lined with a layer of refractory bricks. It should be noted that this application does not strictly limit the specific physical structure of the furnace body, and it can adopt any applicable structure known to those skilled in the art.
[0023] Specifically, two sliding wheels are provided on opposite sides of the bottom of the movable part 21, and two guide rails are installed at intervals on one side of the furnace body. The sliding wheels on opposite sides of the movable part slide in cooperation with the corresponding guide rails. It can be understood that when the movable part 21 moves along the length of the guide rail, it can drive the placement part 23 to enter and exit the cavity 1a through the opening.
[0024] Based on the above scheme, the movable part 21 is provided with a heat insulation cotton layer, and a cover plate is provided on one side of the heat insulation cotton layer. When the placement part 23 is moved into the cavity 1a, the heat insulation cotton layer seals the opening, and the cover plate abuts against the outer wall of the furnace body.
[0025] In one embodiment, the first spray member 22 includes a rotating shaft 221 and a plurality of spray heads 222. The rotating shaft 221 is rotatably mounted on the moving member 21. A liquid guiding cavity is provided in the rotating shaft 221 along the axial direction and the end is open. The plurality of spray heads 222 are arranged circumferentially along the rotating shaft 221 and communicate with the liquid guiding cavity. The plurality of spray heads 222 extend along the axial direction of the rotating shaft 221. Specifically, when the placement member 23 is moved into the cavity 1a and the placement member 23 rotates with the rotating shaft 221, the plurality of mounting areas on the placement member 23 can correspond one by one with the strip hole.
[0026] Specifically, the nozzle 222 includes a conduit and multiple nozzles. One end of the multiple conduits is connected to the rotating shaft 221 and is in fluid communication with the liquid guiding chamber. The multiple nozzles are installed on the conduits at intervals, and all of the multiple nozzles face the inside of the installation area.
[0027] Specifically, to ensure that the conduit and multiple nozzles extending into the combustion furnace are not burned, the conduit and multiple nozzles are made of high-temperature resistant materials; preferably, the conduit is made of stainless steel; the nozzles are made of high-temperature resistant ceramic materials, including but not limited to alumina ceramics, silicon carbide ceramics or silicon nitride ceramics.
[0028] In one embodiment, the placement member 23 includes a frame 231, multiple support portions 232, and a locking portion 233. The frame 231 is mounted on a rotating shaft 221. The frame 231 has multiple mounting areas along its circumference, and each mounting area has a limiting channel 231a with an insertion end. The support portions 232 are configured to support multiple ceramic bodies in parallel and at intervals, and the support portions 232 can move into or out of the limiting channel 231a through the insertion. The locking portion 233 is configured to be detachably connected to the frame 231 to close or open the multiple insertions. Specifically, the placement member 23 is also made of a high-temperature resistant material.
[0029] It is understood that the frame 231 includes four fixed rods 2311 and a cross-shaped connecting plate 2312. The cross-shaped connecting plate is fixedly connected to the rotating shaft and to the four fixed rods. A sliding groove is provided on the side of the two fixed rods that are close to each other, and a limiting channel 231a is formed between the two sliding grooves for the bearing part 232 to pass through.
[0030] In one embodiment, the support portion 232 includes a square frame, which includes two horizontal bars and two vertical bars connected between the two horizontal bars. One horizontal bar is provided with a plurality of through holes 232a at intervals, and the other horizontal bar is provided with a plurality of clearance grooves 232b at intervals, and each clearance groove 232b is coaxially aligned with each through hole 232a.
[0031] Specifically, the ceramic body is cylindrical in shape. One end of the ceramic body is inserted through the perforation 232a and extends into the relief groove 232b, so that multiple ceramic bodies can be supported in the square frame at intervals and parallel. The square frame can be slidably inserted into the limiting channel 231a from the insertion port at one end of the limiting channel 231a.
[0032] In one embodiment, the locking part 233 consists of a baffle 2331 and multiple locking bolts 2332. The baffle 2331 has multiple connecting holes, and the locking bolts 2332 pass through the connecting holes and are screwed into the threaded holes on the frame 231 to fix the baffle 2331 to the frame 231. Specifically, each of the four fixing rods has a threaded hole at its end. The baffle 2331 is a square baffle, and the baffle 2331 is connected to the four fixing rods respectively by the four locking bolts 2332, so that the insertion port at one end of the four limiting channels 231a can be closed.
[0033] It should be noted that a rotary joint 211 is fixedly provided on the movable part 21, and the movable end of the rotary joint 211 is connected to the end of the rotating shaft 221 and communicates with the liquid guiding cavity. The fixed end of the rotary joint 211 is connected to the infusion tube 212, and the infusion tube 212 is in fluid communication with the second air supply part 213. The movable part 21 is detachably installed with a second liquid storage container 214, and the liquid distribution tube on the infusion tube 212 extends downward and is inserted into the second liquid storage container 214.
[0034] Specifically, a sleeve is installed on the movable part 21, and the bottom of the second liquid storage container can be inserted into the sleeve from top to bottom.
[0035] In one embodiment, the drive member 24 includes a drive motor, a drive sprocket, a driven sprocket, and a chain. The drive motor is mounted on the moving member 21. The output end of the drive motor is equipped with the drive sprocket. The driven sprocket is fixed on the rotating shaft. The chain is wound between the drive sprocket and the driven sprocket.
[0036] It should be noted that, in one embodiment, the spraying mechanism 3 further includes a moving part 32 and two clamping modules 33. The moving part 32 is installed on one side of the furnace body 1 and has a reciprocating translational end 320. The two clamping modules 33 are installed opposite to each other on the translational end. The clamping module 33 includes a support part 331, a blocking part 332 and a locking bolt 333. The support part 331 is installed on the translational end and has a groove. The locking bolt 333 is screwed to the blocking part 332. The blocking part 332 is connected to the support part 331. The blocking part 332 has a first state and a second state. In the first state, the blocking part 332 opens the groove and forms a bayonet. In the second state, the blocking part 332 closes the groove and forms a locking space. One end of the locking bolt 2332 can extend into the locking space and abut against the second spraying part 31 that passes through the locking space.
[0037] Specifically, the support part 331 is provided with two connecting slots, and the blocking part 332 is provided with connecting protrusions that slide in cooperation with the two connecting slots.
[0038] Specifically, the moving part 32 is not limited to a specific structure. Specifically, the moving part 32 includes a mounting base 321, a driving pulley 322, a driven pulley 323, a conveyor belt 324, and a power source 325. The driving pulley 322 and the driven pulley 323 are rotatably mounted on the mounting base 321, and the conveyor belt 324 is connected between the driving pulley 322 and the driven pulley 323. The power source 323 is mounted on the mounting base 321, and its output end is connected to the driving pulley 322 for transmission. Its translation end 320 is slidably connected to the mounting base 321 and fixedly connected to the conveyor belt 324.
[0039] The power source is a drive motor, which is electrically connected to a controller (programmable PLC). It can be understood that an incremental encoder is installed on the output shaft of the drive motor. The controller controls the drive motor to rotate forward or backward a predetermined number of times, thereby realizing the reciprocating movement of the translation end in a preset direction.
[0040] In this specific embodiment, the spraying mechanism 3 further includes a first liquid storage container 34 and a first air supply component 35; the first liquid storage container 34 is detachably installed on the translation end, and the branch pipe connected to the second spray component 31 extends downward to the bottom of the first liquid storage container 34, wherein the second spray component 31 is connected to the air supply component.
[0041] It should be noted that both the first liquid storage container 34 and the second liquid storage container are liquid storage bottles with the bottle openings open, allowing external airflow to enter the liquid storage bottles through the bottle openings.
[0042] Furthermore, a limiting module 36 is also installed on the translation end and between the two clamping modules 33. The limiting module 36 defines a cavity, and the top of the cavity has an opening. The lower end of the first liquid storage container 34 passes through the opening and is accommodated in the cavity. The outer wall contour of the first liquid storage container 34 is adapted to the inner wall contour of the cavity, and the outer diameter of the first liquid storage container 34 matches the inner diameter of the cavity 1a.
[0043] Understandably, a limiting bolt is also screwed onto the limiting module 36, one end of which can extend into the cavity and abut against the outer wall of the first liquid storage container 34.
[0044] It should be noted that both the first liquid storage container 34 and the second liquid storage container contain tin tetrachloride solution; and both the first air supply component 35 and the second air supply component are air compressors.
[0045] It should be noted that the inner diameter of the second spray element is 1.5-3 times the inner diameter of the branch pipe; preferably, the inner diameter of the second spray element is 2.5 times the inner diameter of the branch pipe; the inner diameter of the infusion tube is 1.5-3 times the inner diameter of the dispensing tube; preferably, the inner diameter of the infusion tube is 2.5 times the inner diameter of the dispensing tube.
[0046] Specifically, the high-pressure airflow flows at high speed within the second spray element. When it passes the connection between the branch pipe and the second spray element, the static pressure at the connection point will decrease significantly due to the extremely high gas velocity, according to Bernoulli's principle, thus creating a local negative pressure zone at the branch pipe opening. At this time, the lower end of the branch pipe is inserted into the bottom of the first liquid storage container. The liquid surface in the first liquid storage container is subjected to normal atmospheric pressure. Since the negative pressure at the branch pipe opening is much smaller than the pressure on the liquid surface in the first liquid storage container, this pressure difference will force the liquid in the first liquid storage container to flow upward along the branch pipe and be "drawn" into the second spray element. After the reaction liquid is drawn into the second spray element, it will mix with the high-speed high-pressure airflow to form a gas-liquid two-phase flow, and finally be carried by the high-pressure airflow and sprayed out through the second spray element.
[0047] The principle by which the second gas supply component transports the reaction liquid in the second liquid storage container to the infusion pipe is the same as the principle by which the first gas supply component 35 transports the reaction liquid in the first liquid storage container to the second spray component, and will not be elaborated further here.
[0048] To better understand this invention, the following is combined with... Figures 1 to 9 The technical solution of the present invention will be described in detail below: The drive motor drives the translation end to reciprocate in a preset direction, which in turn drives the second spray element 31 to reciprocate between the two ends of the strip hole. High-pressure airflow is delivered to the second spray element 31 via the first air supply element 35. Under the action of the air pressure difference, the reaction liquid in the first liquid storage container 34 is drawn into the second spray element 31. The reaction liquid mixes with the gas in the second spray element 31 and is then sprayed out, enabling the spraying of reaction liquid to each installation area one by one, ensuring that the ceramic surface inside the furnace body 1 can receive the reaction liquid evenly. Simultaneously, the second air supply... The component delivers high-pressure gas flow to the infusion pipe. Under the action of the pressure difference, the reaction liquid in the second liquid storage container is drawn into the liquid guiding chamber of the rotating shaft. After the reaction liquid mixes with the gas in the liquid guiding chamber, it is sprayed out through multiple nozzles, which can spray the reaction liquid on the inner side of multiple installation areas at the same time. When the spraying of reaction liquid into the furnace body is stopped, the locking bolt 2332 can be rotated to release the fixing restriction on the second spray component 31. The second spray component 31 can be moved out of the furnace body, and ceramic fiber cotton cloth is inserted into the strip hole to seal the strip hole.
[0049] The specific embodiments of the present invention described above do not constitute a limitation on the scope of protection of the present invention. Any other corresponding changes and modifications made in accordance with the technical concept of the present invention should be included within the scope of protection of the claims of the present invention.
Claims
1. A ceramic body coating heating system, characterized in that, include: The furnace body has a cavity defined inside and is open at one end. The side wall of the furnace body is provided with a strip-shaped hole communicating with the cavity. A conveying mechanism includes a movable component, a first spray component, a placement component, and a driving component. The first spray component is rotatably mounted on the movable component, the placement component is mounted on the first spray component, and the driving component is mounted on the movable component and drivenly connected to the first spray component. The driving component is configured to drive the first spray component and the placement component to rotate synchronously. The placement component has multiple mounting areas along its circumference, and each mounting area is configured to carry multiple ceramic bodies in parallel and at intervals. The first spray component is configured to spray reaction liquid toward the inner side of the mounting area. The movable component is configured to drive the placement component to move into or out of the cavity through an opening. The liquid spraying mechanism includes a second spray element mounted on one side of the furnace body, the second spray element being configured to spray the reaction liquid outwards toward each of the mounting areas via strip-shaped holes.
2. The ceramic body coating heating system according to claim 1, characterized in that, The first spraying component includes a rotating shaft and a plurality of spray heads. The rotating shaft is rotatably mounted on a moving component. A liquid guiding cavity is provided inside the rotating shaft along the axial direction and the end is open. The plurality of spray heads are arranged at intervals along the circumference of the rotating shaft and communicate with the liquid guiding cavity. The plurality of spray heads extend along the axial direction of the rotating shaft.
3. The ceramic body coating heating system according to claim 2, characterized in that, The placement component includes a frame, multiple support parts, and a locking part. The frame is mounted on a rotating shaft. The frame has multiple mounting areas along its circumference, and a limiting channel with an insertion port at one end is provided corresponding to each mounting area. The support parts are configured to support multiple ceramic bodies in parallel and at intervals, and the support parts can move into or out of the limiting channel through the insertion port. The locking part is configured to be detachably connected to the frame to close or open the multiple insertion ports.
4. The ceramic body coating heating system according to claim 3, characterized in that, The supporting part includes a square frame, which includes two horizontal bars and two vertical bars connected between the two horizontal bars. One of the horizontal bars is provided with a plurality of through holes at intervals, and the other horizontal bar is provided with a plurality of clearance grooves at intervals, and each clearance groove is coaxially aligned with each of the through holes.
5. The ceramic body coating heating system according to claim 4, characterized in that, The locking part consists of a baffle and multiple locking bolts; The baffle has multiple connecting holes, and the locking bolt passes through the connecting holes and is screwed into the threaded holes on the frame to fix the baffle to the frame.
6. The ceramic body coating heating system according to claim 1, characterized in that, The liquid spraying mechanism also includes a moving component and two clamping modules. The moving component is installed on one side of the furnace body and has a reciprocating translational end. The two clamping modules are installed opposite to each other on the translational end. The clamping module includes a support part, a blocking part, and a locking bolt. The support part is installed on the translation end and has a groove. The locking bolt is screwed to the blocking part. The blocking part is connected to the support part. The blocking part has a first state and a second state. In the first state, the blocking part opens the groove and forms a bayonet. In the second state, the blocking part closes the groove and forms a locking space. One end of the locking bolt can extend into the locking space and abut against the second spray element that passes through the locking space.
7. A ceramic body coating heating system according to claim 6, characterized in that, The liquid spraying mechanism further includes a first liquid storage container and a first air supply component; The first liquid storage container is detachably installed on the translation end, and the branch pipe connected to the second spray component extends downward to the bottom of the first liquid storage container, wherein the second spray component is connected to the air supply component.
8. A ceramic body coating heating system according to claim 7, characterized in that, A limiting module is also installed on the translation end and between the two clamping modules. The limiting module defines a cavity, and the top of the cavity has an opening. The lower end of the first liquid storage container passes through the opening and is accommodated in the cavity. The outer wall contour of the first liquid storage container is adapted to the inner wall contour of the cavity, and the outer diameter of the first liquid storage container matches the inner diameter of the cavity.
9. A ceramic body coating heating system according to claim 8, characterized in that, The limiting module is also screwed with a limiting bolt, one end of which can extend into the cavity and abut against the outer wall of the first liquid storage container.
10. A ceramic body coating heating system according to claim 7, characterized in that, The first air supply component is an air compressor.