Camera blue glass and camera module
Patent Information
- Application Number
- CN202610836325.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-06-10
- Publication Date
- 2026-10-27
AI Technical Summary
这种渗透会影响半透油墨的透光效果,并增加扩散油墨渗透形成的光斑问题,从而影响产品的外观和性能
本发明的创新之处在于在蓝玻璃的半透油墨和扩散油墨之间增加了一层固态双面光学胶。这种固态双面光学胶可以有效地阻止半透油墨和扩散油墨之间的相互渗透,同时保持半透油墨的透光性能。通过这种设计,可以显著减少扩散油墨渗透形成的光斑,提高半透油墨的透光效果,从而保证产品的外观和性能。还可以延长蓝玻璃的使用寿命,减少因油墨渗透导致的维修或更换需求。同时可以简化生产过程,减少因油墨渗透导致的废品率,提高生产效率。
Smart Images

Figure CN122984099A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of camera technology, and more specifically, to a camera blue glass and camera module. Background Technology
[0002] In traditional camera blue glass designs, a semi-transparent ink and a diffusing ink are typically stacked on the back of the blue glass. Over time, these two inks may interpenetrate. This interpenetration affects the light transmission of the semi-transparent ink and increases the light spot problem caused by the diffusing ink, thus impacting the product's appearance and performance. Summary of the Invention
[0003] The technical problem to be solved by this invention is how to avoid penetration between semi-transparent ink and diffusion ink, thereby avoiding affecting the light transmission effect of semi-transparent ink and preventing the light spot problem caused by diffusion ink penetration, thus ensuring the appearance and performance of the product.
[0004] The technical problem to be solved by the present invention is achieved through the following technical solution: To address the aforementioned technical problems, this invention provides a blue glass for a camera, comprising a blue glass body, a semi-transparent ink, a solid double-sided optical adhesive, and a diffusion ink, which are sequentially stacked from top to bottom. The semi-transparent ink is disposed at the edge of the lower surface of the blue glass body. The solid double-sided optical adhesive completely covers the semi-transparent ink, and the diffusion ink completely covers the solid double-sided optical adhesive. The thickness of the semi-transparent ink is 4μm-5μm, the thickness of the solid double-sided optical adhesive is 10μm-15μm, and the thickness of the diffusion ink is 6μm-7μm.
[0005] This invention provides a camera module, which includes a lens base and a camera blue glass as described above disposed on the lens base. The lens base includes a side wall of a lower base. A circuit board is disposed at the bottom of the side wall of the lower base perpendicular to the side wall of the lower base. An inner groove is formed on the lower surface of the side wall of the lower base, which surrounds the side wall of the lower base. An adhesive layer is disposed in the inner groove. The circuit board is bonded to the side wall of the lower base through the adhesive layer.
[0006] In a preferred embodiment of the camera module provided by the present invention, at least one exhaust groove is provided on the inner groove.
[0007] In a preferred embodiment of the camera module provided by the present invention, the lower base has four side walls, which are connected in pairs.
[0008] In a preferred embodiment of the camera module provided by the present invention, each of the lower bases has three exhaust slots on its side wall.
[0009] In a preferred embodiment of the camera module provided by the present invention, the adhesive layer is AA glue.
[0010] In a preferred embodiment of the camera module provided by the present invention, the circuit board includes a body and a connecting portion connected to the body, and two mutually staggered reinforcing plates are provided on both sides of the connecting portion.
[0011] In a preferred embodiment of the camera module provided by the present invention, the two reinforcing plates have different widths.
[0012] In a preferred embodiment of the camera module provided by the present invention, the two reinforcing plates have equal widths but their center points are offset from each other.
[0013] In a preferred embodiment of the camera module provided by the present invention, the reinforcing plate is made of FR4, PI or stainless steel.
[0014] The present invention has the following beneficial effects: The innovation of this invention lies in adding a layer of solid double-sided optical adhesive between the semi-transparent ink and the diffusion ink in the blue glass. This solid double-sided optical adhesive effectively prevents the interpenetration between the semi-transparent ink and the diffusion ink while maintaining the light transmittance of the semi-transparent ink. This design significantly reduces light spots caused by diffusion ink penetration, improves the light transmittance of the semi-transparent ink, and thus ensures the product's appearance and performance. It also extends the service life of the blue glass, reducing the need for repair or replacement due to ink penetration. Furthermore, it simplifies the production process, reduces the scrap rate caused by ink penetration, and improves production efficiency. Attached Figure Description
[0015] To more clearly illustrate the solutions in this application, the accompanying drawings used in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are some embodiments of this application. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0016] Figure 1 This is a schematic diagram of the structure of a blue glass for a camera provided by the present invention.
[0017] Figure 2 for Figure 1 A cross-sectional view at point AA.
[0018] Figure 3 This invention provides a schematic diagram of the structure of a camera module.
[0019] Figure 4 for Figure 3 A bottom view of the lens base.
[0020] Figure 5 for Figure 3 A schematic diagram of the improved structure of the circuit board.
[0021] Explanation of icon numbers: 1. Blue glass body; 2. Semi-transparent ink; 3. Solid double-sided optical adhesive; 4. Diffusion ink; Lens base 5; side wall of lower base 6; circuit board 7; inner groove 61; adhesive layer 8; venting groove 72; reinforcing plate 9. Detailed Implementation
[0022] To enable those skilled in the art to better understand the present invention, the technical solutions of the present invention will be clearly and completely described below with reference to the accompanying drawings of the embodiments of the present invention. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort should fall within the scope of protection of the present invention.
[0023] In the description of this invention, it should be understood that the terms "center," "longitudinal," "lateral," "length," "width," "thickness," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," "outer," "clockwise," "counterclockwise," "axial," "radial," and "circumferential" indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing this invention and simplifying the description, and are not intended to indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on this invention.
[0024] Furthermore, the terms "first," "second," and "third" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first," "second," or "third" may explicitly or implicitly include at least one of that feature. In the description of this invention, "a plurality of" means at least two, such as two, three, etc., unless otherwise explicitly specified.
[0025] To enable those skilled in the art to better understand the present application, the technical solutions in the embodiments of the present application will be clearly and completely described below with reference to the accompanying drawings. The present invention will be described in detail below with reference to the accompanying drawings and embodiments, examples of which are shown in the drawings, wherein the same or similar reference numerals denote the same or similar elements or elements having the same or similar functions throughout. The embodiments described below with reference to the accompanying drawings are exemplary and intended to explain the present invention, and should not be construed as limiting the present invention.
[0026] Please see Figure 1 The present invention provides a camera blue glass, which includes a blue glass body 1, a semi-transparent ink 2, a solid double-sided optical adhesive 3, and a diffusion ink 4, which are stacked sequentially from top to bottom. The semi-transparent ink 2 is disposed on the edge of the lower surface of the blue glass body 1. The solid double-sided optical adhesive 3 completely covers the semi-transparent ink 2, and the diffusion ink 4 completely covers the solid double-sided optical adhesive 3. The thickness of the semi-transparent ink 2 is 4μm-5μm, the thickness of the solid double-sided optical adhesive 3 is 10μm-15μm, and the thickness of the diffusion ink 4 is 6μm-7μm.
[0027] The innovation of this invention lies in adding a layer of solid double-sided optical adhesive 3 between the semi-transparent ink 2 and the diffusion ink 4 of the blue glass. This solid double-sided optical adhesive 3 can effectively prevent the interpenetration between the semi-transparent ink 2 and the diffusion ink 4, while maintaining the light transmittance of the semi-transparent ink 2. This design significantly reduces the light spots formed by the diffusion ink 4 penetrating, improving the light transmittance of the semi-transparent ink 2, thereby ensuring the appearance and performance of the product. It can also extend the service life of the blue glass, reducing the need for repair or replacement due to ink penetration. Simultaneously, it simplifies the production process, reduces the scrap rate due to ink penetration, and improves production efficiency.
[0028] Please see Figures 2 to 5This invention provides a camera module comprising a lens base 5 and a camera blue glass as described above, disposed on the lens base 5. The lens base 5 includes a side wall 6 of a lower base. A circuit board 7, perpendicularly disposed to the bottom of the side wall 6, is provided. An inner groove 61, surrounding the side wall 6, is formed on the lower surface of the side wall 6. An adhesive layer 8 is provided in the inner groove 61. The circuit board 7 is bonded to the side wall 6 of the lower base via the adhesive layer 8. In this embodiment, the adhesive layer 8 is glue. When applying the glue, care should be taken not to exceed the lower surface of the side wall 6, while ensuring the glue fills the inner groove 61. This ensures sufficient bonding area between the glue and the side wall after curing, without generating tensile force that could deform the circuit board 7. Because the inner groove 61 is coated with glue, and the glue will not overflow, the tensile force generated after curing is concentrated in the direction perpendicular to the circuit board 7, which will not cause the circuit board 7 to deform. This avoids changes in the flatness of the circuit board 7 with optical sensor caused by the oblique tensile force generated after the glue shrinks. In turn, it avoids changes in the position of the lens and optical sensor, and prevents the clarity of the central area of the image captured by the camera module from not being fixed in the clearest position, thereby improving product yield, reducing product cost, and improving product competitiveness.
[0029] Furthermore, at least one venting groove 72 is provided on the inner groove 61. When the side wall 6 of the lower base is pressed onto the adhesive, the air in the inner groove 61 can be expelled, allowing the adhesive to fill the space of the inner groove 61 smoothly and preventing the formation of air bubbles.
[0030] Furthermore, the lower base has four side walls 6, which are connected in pairs.
[0031] Furthermore, each lower base has three exhaust slots 72 on its side wall 6 to allow air to escape.
[0032] Furthermore, the adhesive layer 8 is AA glue.
[0033] Furthermore, two staggered reinforcing plates 9 are provided on both sides of the circuit board 7. In traditional circuit board 7 designs, reinforcing plates 9 are usually not provided or are placed in the same position with the same width. This causes the pressure applied when inserting or removing the circuit board 7 to be concentrated on the same straight line, resulting in micro-breaks in the circuit board 7. The circuit board 7 provided by this invention has two reinforcing plates 9 located on both sides of the connection and staggered from each other. When the circuit board 7 is pulled out, the pressure applied to the circuit board 7 by the two reinforcing plates 9 is not on the same line segment, and the stress will not be concentrated on the same straight line when bending. This avoids stress concentration and the problem of easy micro-breaks in the circuit at the interface end, thereby improving product yield.
[0034] Furthermore, the two staggered reinforcing plates 9 referred to in this invention can be located at two different positions; alternatively, they can have the same center point but different widths. The key is to ensure that the stress from bending the two reinforcing plates 9 is not concentrated on the same straight line. This avoids stress concentration and the problem of minor breaks in the wiring at the interface, thus improving product yield. In this embodiment, the reinforcing plates 9 include a first reinforcing plate 9 and a second reinforcing plate 9. Each reinforcing plate 9 has a different width, and their center points are on the same horizontal line, so that the edges of the reinforcing plates 9 are staggered and not concentrated on the same straight line.
[0035] Furthermore, the reinforcing plate 9 is made of FR4, PI, or stainless steel. In other embodiments, if the circuit board 7 generates a large amount of heat, a heat dissipation material with better heat dissipation effect, such as aluminum foil reinforcing plate 9, can also be used.
[0036] Furthermore, the outer surfaces of both the first reinforcing plate 9 and the second reinforcing plate 9 are provided with a surface treatment layer to increase surface roughness, so as to improve the friction between the operator and the first reinforcing plate 9 and the second reinforcing plate 9, making the circuit board 7 easier to pull out.
[0037] Furthermore, the surface treatment layer has diamond knurling on the outer surfaces of both the first reinforcing plate 9 and the second reinforcing plate 9, so that the circuit board 7 can be pulled out more easily, reducing the risk of circuit breakage of the circuit board 7.
[0038] In this invention, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," and "fixing," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection, an electrical connection, or a connection that allows communication between them; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components, unless otherwise explicitly limited. Those skilled in the art can understand the specific meaning of the above terms in this invention according to the specific circumstances.
[0039] Obviously, the embodiments described above are only some embodiments of this application, not all embodiments. The accompanying drawings show preferred embodiments of this application, but do not limit the patent scope of this application. This application can be implemented in many different forms; rather, the purpose of providing these embodiments is to provide a more thorough and comprehensive understanding of the disclosure of this application. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions described in the foregoing specific embodiments, or make equivalent substitutions for some of the technical features. Any equivalent structures made using the content of this application's specification and drawings, directly or indirectly applied to other related technical fields, are similarly within the scope of patent protection of this application.
Claims
1. A blue glass for a camera, characterized in that, It comprises a blue glass body, a semi-transparent ink, a solid double-sided optical adhesive, and a diffusion ink, which are stacked sequentially from top to bottom. The semi-transparent ink is disposed on the edge of the lower surface of the blue glass body. The solid double-sided optical adhesive completely covers the semi-transparent ink, and the diffusion ink completely covers the solid double-sided optical adhesive. The thickness of the semi-transparent ink is 4μm-5μm, the thickness of the solid double-sided optical adhesive is 10μm-15μm, and the thickness of the diffusion ink is 6μm-7μm.
2. A camera module, characterized in that, It includes a lens base and a camera blue glass as described in claim 1 disposed on the lens base. The lens base includes a side wall of a lower base. A circuit board is provided at the bottom of the side wall of the lower base and is perpendicular to the side wall of the lower base. An inner groove is formed on the lower surface of the side wall of the lower base and is arranged around the side wall of the lower base. An adhesive layer is provided in the inner groove. The circuit board is bonded to the side wall of the lower base through the adhesive layer.
3. The camera module according to claim 2, characterized in that, At least one exhaust groove is provided on the inner groove.
4. The camera module according to claim 3, characterized in that, The lower base has four side walls, which are connected in pairs.
5. The camera module according to claim 4, characterized in that, Each of the lower bases has three venting slots on its side wall.
6. The camera module according to claim 2, characterized in that, The adhesive layer is AA glue.
7. The camera module according to claim 2, characterized in that, The circuit board includes a body and a connecting part connected to the body, and two staggered reinforcing plates are provided on both sides of the connecting part.
8. The camera module according to claim 7, characterized in that, The two reinforcing plates have different widths.
9. The camera module according to claim 7, characterized in that, The two reinforcing plates have the same width but their center points are offset from each other.
10. The camera module according to claim 7, characterized in that, The reinforcing plate is made of FR4, PI, or stainless steel.