Preparation method of nano-thiazole zinc with controllable particle size
By controlling the turbulence intensity and flow ratio using a four-channel vortex reactor, the problem of uneven particle size of nano-thiazole zinc was solved, enabling continuous production with controllable particle size, improving antibacterial activity and formulation stability, and making it suitable for agricultural applications that reduce dosage and increase efficacy.
Patent Information
- Application Number
- CN202611312759.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-27
- Publication Date
- 2026-11-20
AI Technical Summary
In existing technologies, the particle size control of nano-thiazole zinc is not precise, making it difficult to achieve a uniform and controllable particle size distribution. This affects the experimental requirements for its antibacterial ability at different particle sizes and the precise manufacturing for industrial production.
A four-channel vortex reactor was used to control the turbulence intensity during fluid mixing. By adopting a process control strategy of fixing the flow rate ratio and proportionally increasing the total flow rate, continuous preparation of nano-thiazole zinc was achieved, ensuring controllable particle size and stability.
This method achieves a narrower particle size distribution for nano-thiazole zinc particles, improving the stability of the formulation, enhancing its bioactivity against target pathogens, reducing the dosage and lowering environmental risks.
Smart Images

Figure FT_1 
Figure FT_2 
Figure SMS_1
Abstract
Description
Technical Field
[0001] This invention relates to the field of nanopesticide preparation, specifically to a method for preparing nano-thiazole zinc with controllable particle size. Background Technology
[0002] Compared to traditional pesticides, developing nanopesticides is an important way to reduce pesticide use while increasing efficiency. Thiazole zinc, an organozinc coordination fungicide, can enhance its biotoxicity against target pathogens when nano-sized, reducing field application and environmental risks.
[0003] Among the currently disclosed nano-thiazolium zinc preparation technologies, there is no technology for precise control of the particle size of nano-thiazolium zinc. CN107417640A (2017) discloses a chemical synthesis method for nano-thiazolium zinc, which involves mixing thiadiazole and an alkali in a solvent to prepare a thiadiazole salt solution, then dissolving the zinc salt and additives in water (or adding the additives to the thiadiazole salt solution before adding the zinc salt solution), mixing them thoroughly to form a suspension, and finally separating and drying the suspension to obtain powdered nano-thiazolium zinc with a particle size of 1~1000 nm. CN114073250A (2022) uses a physical-mechanical sand milling method, mixing thiazolium zinc, surfactants, thickeners, preservatives, and other additives with water, then feeding the mixture into a sand mill, using sand milling media (such as zirconia beads) with a diameter of 0.1 mm~0.6 mm for circulating sand milling or multi-stage sand milling until the particle size reaches the nanoscale (D). 90 =400~1100nm), after filtering to remove the medium, a suspension is obtained. WO2025093024A1 discloses a method for preparing thiamethoxam / pyraclostrobin nanoemulsion dispersions using a water dilution and mixing process. This method employs a two- or three-component model, where "component A," containing water-soluble thiadiazole salt, water-soluble polymeric adjuvant, and pyraclostrobin nanoemulsion, and "component B," containing zinc salt, are separately diluted with water. Then, under pre-stirring conditions with a stirring speed not less than the effective stirring speed, the diluted component B is added to the diluted component A, directly generating the nanoemulsion dispersion through ionic reaction, resulting in active ingredient particles below 100 nm.
[0004] Despite continuous advancements in existing processes for developing nano-thiazolium zinc, achieving precise control over particle size remains a technological bottleneck. Constructing a nano-dispersion system with uniform and controllable particle size distribution not only meets the experimental needs of exploring antibacterial activity at different particle sizes but also provides crucial control parameters for subsequent industrial-scale precision manufacturing. Therefore, developing a method for the continuous production of nano-thiazolium zinc with controllable particle size is of great significance. Summary of the Invention
[0005] To address the shortcomings of existing technologies, this invention provides a method for preparing nano-thiazole zinc with controllable particle size.
[0006] This invention enables the continuous preparation of nano-sized thiazole zinc particles of varying sizes by controlling the turbulence intensity during fluid mixing within a four-channel vortex reactor. Under the premise of controllable and continuous preparation, the prepared nano-thiazole zinc particles exhibit a narrow particle size distribution, further improving the stability of the nano-thiazole zinc formulation.
[0007] The technical solution of the present invention is as follows: A method for preparing nano-thiazole zinc with controllable particle size, comprising: (1) Dissolve zinc thiazide in dimethyl sulfoxide to prepare an organic phase solution (abbreviated as: O); The dissolution temperature is 50~110 °C, preferably 80~90 °C; The concentration of thiazolium zinc in the organic phase solution is 5-50 mg / mL, preferably 20-25 mg / mL; (2) Dissolve the dispersant MF in deionized water to prepare an aqueous solution (abbreviated as: A); The mass fraction of dispersant MF in the aqueous solution is 0.1-1%, preferably 0.3-0.5%; (3) A four-channel vortex reactor is used. The four inlet channels of the reactor are numbered 1, 2, 3 and 4 in a counterclockwise / clockwise direction. At room temperature (25±2 °C), the organic phase solution is divided into two streams as streams 1 and 3, and the aqueous phase solution is divided into two streams as streams 2 and 4 and pumped into the reactor at the same time. The four streams are mixed in the mixing chamber and then discharged from the reactor outlet to continuously produce a suspension containing nano-thiazole zinc. The flow rate ratio of the aqueous phase solution to the organic phase solution is 1:1 to 10:1 (preferably 3:1 to 5:1), and the total flow rate is 10 to 200 mL / min (preferably 80 to 128 mL / min); the liquid holdup in the reactor mixing chamber is 0.3 mL. The resulting suspension containing nano-thiazole zinc was centrifuged (10,000 rpm, 8 minutes), the precipitate was collected, washed with deionized water, and dried under vacuum at 50 °C to obtain nano-thiazole zinc. Stable thiazole zinc nanoformulations can be prepared by mixing nano-thiazole zinc with adjuvants and using a high-shear method.
[0008] In this invention, the full name of thiazolyl zinc is 2-amino-5-mercapto-1,3,4-thiadiazole zinc, and its structural formula is as follows:
[0009] This invention discloses and utilizes the mixing intensity (determined by Reynolds number) within a four-channel vortex reactor (MIVM). Thing The kinetic relationship between characterization and particle size and polydispersity coefficient.
[0010] In a four-channel vortex reactor, to ensure a uniform micro-mixing environment for the fluid and achieve controllable nanoprecipitation, the Reynolds number within the reactor ( Thing The concentration needs to be controlled above 1600. In this invention, the mixing intensity in the reactor is not a simple monotonic linear relationship with the nanoparticle size and polydispersity index (PDI), but is controlled by the fluid control strategy.
[0011] Specifically, in the preparation of nano-thiazole zinc using a MIVM reactor based on transient nanoprecipitation (FNP) technology, two fluid feed control paths are typically employed to increase the Reynolds number of the system and enhance mixing intensity: The first approach is to keep the organic phase feed flow rate constant and gradually increase the flow rate of the aqueous solution to increase the total flow rate of the system. The second approach is to keep the feed flow rate ratio of the organic phase to the aqueous phase constant and proportionally increase the total pump flow rate of the two-phase streams.
[0012] This invention employs a process control strategy of "fixed flow rate ratio and proportional scale-up". By fixing the mixing ratio of the organic phase (O) and the aqueous phase (A), the total flow rate is simultaneously and linearly increased to improve the Reynolds number, thereby achieving a match between the micro-mixing rate and the dispersant interface adsorption rate. This overcomes the problem of kinetic mismatch under high mixing intensity, and achieves nano-sized thiazolium zinc particles while ensuring a narrow particle size distribution.
[0013] In this invention, the degree of turbulence within the four-channel vortex reactor is determined by the Reynolds number (…). Thing The evaluation is conducted using the following formula:
[0014] In the formula, Thing —Total Reynolds number of the system; i —Specific flow strand number (in this invention) N =4); V i —Linear velocity (m / s) of the i-th feed stream; Q i —Volume flow rate of the i-th feed stream (m³) 3 / s); D —Diameter (m) of the central mixing chamber of the four-channel vortex reactor, which is fixed at 6mm in this embodiment of the invention; S i —Cross-sectional area of the i-th fluid inlet channel (m 2 In the MIVM reactor used in this invention, the cross-sectional area of each channel is 1.65 × 10⁻⁶.-6 m 2 ; n i —The kinematic viscosity (m) of the corresponding fluid at the experimental temperature (e.g., 25 °C). 2 / s). In the system of this invention, the kinematic viscosity of water is 8.93 × 10⁻⁶. -7 m 2 The kinematic viscosity of dimethyl sulfoxide (DMSO) is 1.817 × 10⁻⁶ / s. -6 m 2 / s.
[0015] The innovation and beneficial effects of this invention are as follows: This invention develops a continuous method for preparing nano-thiazolium zinc based on transient nanoprecipitation (FNP) technology. By controlling the flow rate and mixing intensity within the reactor's mixing chamber, the particle size of the nano-thiazolium zinc can be controlled. This process effectively overcomes the limitations of existing technologies and provides a feasible technical approach for the low-cost, continuous production of nano-thiazolium zinc.
[0016] This invention employs a "proportional scale-up" flow control mode, demonstrating excellent feasibility for industrial scale-up. By identifying an optimal two-phase mixing ratio, the kinetic mismatch between micro-mixing and dispersant adsorption in highly turbulent systems is resolved. Furthermore, a control scheme employing a fixed mixing ratio and proportionally scaled-up total flow rate overcomes the problem of uneven particle size distribution during fluid scale-up, ensuring the stability of the continuous preparation process for nano-thiazole zinc.
[0017] The nano-thiazole zinc prepared in this invention effectively enhances the bioactivity of target pathogens. The nano-thiazole zinc prepared based on FNP technology effectively enhances the antibacterial activity against three typical bacterial pathogens. This achievement responds to the agricultural application orientation of "reduced dosage and increased efficiency," ensuring high antibacterial activity while reducing application dosage and lowering environmental risks. Attached Figure Description
[0018] Figure 1 : Schematic diagram of the apparatus for preparing nano-thiazole zinc suspension using a four-channel vortex reactor according to the present invention.
[0019] Figure 2 Scanning electron microscope (SEM) image of nano-sized thiazole zinc prepared in Example 13. Detailed Implementation
[0020] The present invention will be further described below with reference to the accompanying drawings and specific embodiments, but the scope of protection of the present invention is not limited thereto.
[0021] In the following embodiments, Raw material: thiazolyl zinc: purity 98.8%, micron-sized particles; Dispersant MF: Shandong Yousuo Chemical Technology Co., Ltd.; Stabilizer SP-SC3: Jiangsu Qingyu Chemical Technology Co., Ltd.; Dispersant SP-2728: Jiangsu Qingyu Chemical Technology Co., Ltd.; Thickener XG: Zibo Zhongxuan Biochemical Co., Ltd.; Aluminum magnesium silicate SF-04: Suzhou Sinoma Mineral Materials Co., Ltd.; Defoamer S-29: Nanjing Jierun Technology Co., Ltd.; Antifreeze agent ethylene glycol: Sinopharm Chemical Reagent Co., Ltd.
[0022] The four-channel vortex reactor was manufactured by Maikoufulo Microfluidics Technology (Changzhou) Co., Ltd. The device structure is as follows: Figure 1 As shown, the four-channel vortex reactor has four channels (corresponding to streams 1, 2, 3, and 4), each connected to a high-pressure pump (pump 1, 2, 3, and 4) via 8 mm diameter Teflon tubing. After thorough mixing within the mixing chamber, the four streams exit through the outlet, and the suspension flows into a collector. The modular components include: a mixer base and cover, PTFE gaskets, sealing strips, and fixing screws. The mixing chamber has a diameter of 6 mm, a liquid holdup of 0.3 mL, and the cross-sectional area of each of the four inlet channels is 1.65 mm². 2 rectangle.
[0023] The particle size of nano-thiazole zinc was analyzed using a nanoparticle size analyzer (model BeNano 180 Zeta, manufactured by Dandong Better Instruments Co., Ltd.). The average particle size and polydispersity index (PDI) were obtained through three sets of parallel tests.
[0024] I. Preparation Examples
[0025] Example 1: Weigh 10.12 g of zinc thiazole, add 500 mL of dimethyl sulfoxide, stir at 90 °C for three hours to dissolve, and cool at room temperature to obtain an organic phase solution (O); weigh 1.50 g of dispersant MF, dissolve in 500 mL of deionized water to obtain an aqueous phase solution (A); divide the organic phase solution (O) into two streams, 1 and 3, and pump them into the reactor at a flow rate of 6 mL / min (i.e., the total flow rate of the organic phase is 12 mL / min), and simultaneously divide the aqueous phase solution (A) into two streams, 2 and 4, and pump them into the reactor at a flow rate of 12 mL / min (i.e., the total flow rate of the aqueous phase is 24 mL / min). At this time, the contents of the reactor... Thing =2029, after thorough mixing of the streams, a nano-thiazole zinc suspension was continuously prepared. The suspension was centrifuged, washed, and vacuum dried to obtain nano-thiazole zinc with an average particle size of 142 nm and a PDI of 0.21.
[0026] Example 2: Weigh 12.65 g of zinc thiazole, add 500 mL of dimethyl sulfoxide, stir at 90 °C for three hours to dissolve, and cool at room temperature to obtain an organic phase solution (O); weigh 1.75 g of dispersant MF, dissolve in 500 mL of deionized water to obtain an aqueous phase solution (A); divide the organic phase solution (O) into two streams, 1 and 3, and pump them into the reactor at a flow rate of 6 mL / min (i.e., the total flow rate of the organic phase is 12 mL / min), and simultaneously divide the aqueous phase solution (A) into two streams, 2 and 4, and pump them into the reactor at a flow rate of 12 mL / min (i.e., the total flow rate of the aqueous phase is 24 mL / min). At this time, the contents of the reactor... Thing =2029, after thorough mixing, a nano-thiazole zinc suspension was continuously prepared. The suspension was centrifuged, washed, and vacuum dried to obtain nano-thiazole zinc. The average particle size was 141 nm, and the PDI was 0.22.
[0027] Example 3: Weigh 15.18 g of zinc thiazole, add 500 mL of dimethyl sulfoxide, stir at 90 °C for three hours to dissolve, and cool at room temperature to obtain an organic phase solution (O); weigh 2.00 g of dispersant MF, dissolve in 500 mL of deionized water to obtain an aqueous phase solution (A); divide the organic phase solution (O) into two streams, 1 and 3, and pump them into the reactor at a flow rate of 6 mL / min (i.e., the total flow rate of the organic phase is 12 mL / min), and simultaneously divide the aqueous phase solution (A) into two streams, 2 and 4, and pump them into the reactor at a flow rate of 12 mL / min (i.e., the total flow rate of the aqueous phase is 24 mL / min). At this time, the contents of the reactor... Thing =2029, after thorough mixing, a nano-thiazole zinc suspension was continuously prepared. The suspension was centrifuged, washed, and vacuum dried to obtain nano-thiazole zinc. The average particle size was 386 nm, and the PDI was 0.470.
[0028] The preparation conditions and product characteristic parameters of other embodiments are shown in Tables 1 and 2.
[0029] Table 1 shows the results of increasing the mixing intensity by only increasing the aqueous phase (A) flow rate (24~96 mL / min) while keeping other conditions unchanged in Example 2. Thing When ), the particle size and dispersibility index (PDI) of nano-thiazole zinc.
[0030] Table 1
[0031] Table 2 shows the results of enhancing mixing intensity by "same-year amplification" of total flow rate under the condition that other conditions remain unchanged in Example 2. (A:O = 3:1~5:1) Thing When ), the particle size and dispersibility index (PDI) of nano-thiazole zinc are determined.
[0032] Table 2
[0033] Example 20: 10 g of the nano-thiazole zinc prepared in Example 6 was weighed and mixed with 1 g of stabilizer SP-SC3, 2 g of dispersant SP-2728, 1.5 g of ethylene glycol, 0.1 g of thickener XG, 1.0 g of aluminum magnesium silicate SF-04, 0.1 g of defoamer S-29, and 34.3 mL of water. The mixture was then poured into a high-speed shear press and stirred at 10,000 rpm for 10 minutes to obtain a 20% thiazole zinc nano-suspension. The average particle size of the obtained 20% thiazole zinc suspension was determined using a nanoparticle size analyzer to be 246 nm, PDI=0.37, and the particle number was SC-246.
[0034] Example 21: 10 g of the nano-thiazole zinc prepared in Example 7 was weighed and mixed with 1 g of stabilizer SP-SC3, 2 g of dispersant SP-2728, 1.5 g of ethylene glycol, 0.1 g of thickener XG, 1.0 g of aluminum magnesium silicate SF-04, 0.1 g of defoamer S-29, and 34.3 mL of water. The mixture was then poured into a high-speed shear press and stirred at 10,000 rpm for 10 minutes to obtain a 20% thiazole zinc nano-suspension. The average particle size of the obtained 20% thiazole zinc suspension was determined using a nanoparticle size analyzer to be 130 nm, PDI=0.29, and the designation SC-130.
[0035] Example 22: 10 g of the nano-thiazole zinc prepared in Example 8 was weighed and mixed with 1 g of stabilizer SP-SC3, 2 g of dispersant SP-2728, 1.5 g of ethylene glycol, 0.1 g of thickener XG, 1.0 g of aluminum magnesium silicate SF-04, 0.1 g of defoamer S-29, and 34.3 mL of water. The mixture was then poured into a high-speed shear press and stirred at 10,000 rpm for 10 minutes to obtain a 20% thiazole zinc nano-suspension. The average particle size of the obtained 20% thiazole zinc suspension was determined to be 95 nm using a nanoparticle size analyzer, with a PDI of 0.24, and was designated SC-95.
[0036] II. Antibacterial Activity Test of 20% Thiazole Zinc Nano Suspension
[0037] 1. Activation of the tested strains
[0038] The tested strain was *Ralstonia solanacearum*, the pathogen of bacterial wilt of tomato (… Ralstonia solanacearum , Rs. ), Cucumber bacterial angular leaf spot ( Pseudomonas syringaepv. Lachrymander , Psl ) and the soft rot pathogen of cabbage ( Pectobacterium carotovorum subsp. of carrots , PCC All of them were cryopreserved using ultra-low temperature glycerol.
[0039] For activation testing, single colonies of each strain were picked from cryopreservation tubes and inoculated into suitable liquid culture media (CPG medium for *Ralstonia solanacearum*, and NB medium for the others), and incubated in a constant-temperature shaker at 28°C and 180 rpm in the dark. When the bacterial culture reached the logarithmic growth phase, the absorbance (OD) at 600 nm was measured using a UV spectrophotometer. 600 ), and uniformly diluted each target bacterial suspension with sterile fresh culture medium to adjust it to the initial absorbance (OD). 600 =1.0), to be used as a standard test bacterial solution.
[0040] 2. Preparation of drug-containing tablets
[0041] Three different particle sizes of 20% thiamethoxam zinc nano-suspensions (SC-95, SC-130, SC-246) prepared in Examples 20, 21, and 22 were formulated into five concentration gradients. Commercially available micron-sized thiamethoxam zinc suspensions were also formulated into five concentration gradients as control groups. Six mL of the drug solution was added to 54 mL of melted culture medium and mixed thoroughly. The mixture was then poured evenly into four 9 cm petri dishes and cooled to solidify. A blank control group (equal volumes of culture medium + bacterial suspension + sterile water) without the drug was simultaneously set up during the test to monitor the normal growth of the pathogen, and a pure culture medium blank control group was set up to eliminate the baseline influence of transmittance.
[0042] 3. Testing and Evaluation
[0043] Using the turbidimetric method, according to the NY / T 1156.16-2008 standard, a standard test bacterial solution was transferred and diluted 10 μL with sterile water. 4 The bacterial culture was diluted 10 times and 0.1 mL of the diluted solution was inoculated onto each drug-containing plate. After incubation at 28 °C for 24–48 hours, 10 mL of sterile water was added, and the bacterial growth on each plate was scraped off. The optical density of the resulting bacterial suspension was measured at 600 nm using a UV spectrophotometer. The growth inhibition rate for each experiment was calculated using the following formula:
[0044] In the formula, P —Inhibition rate; —The increase in turbidity in the blank control group; —Increase in turbidity in the drug-treated group; All the above tests were performed with 5 independent and parallel biological replicates. After obtaining the apparent growth inhibition rate at each concentration gradient, a log-odds model analysis was conducted. The specific fitting process was as follows: the logarithm of the concentration of the thiazolyl zinc active ingredient (…) was used to calculate the growth inhibition rate. ) as independent variable X The corresponding percentage inhibition rate is converted into a probability value and used as the dependent variable. Y The least squares method was used to construct the toxicity regression equation ( By calculating the correlation coefficient ( R ) Verify the goodness of linear fit of the model and let the regression equation Y =5, and by reverse calculation, the half-maximal effective concentration (EC50) of each formulation system against the four target pathogens can be obtained. 50 ).
[0045] The specific experimental results are shown in Table 3, which contains the antibacterial activity test results of nano-thiazole zinc suspension against three pathogens.
[0046] Table 3
[0047] As shown in Table 3, the antibacterial activity test data indicate that the three thiazole zinc nano-suspensions with different particle sizes prepared in this invention can achieve an inhibition rate of over 99% against three common pathogens, which is superior to the micron-sized formulation. Against tomato bacterial wilt, the three nano-thiazole zinc suspensions showed approximately 32.5-40.7% higher bioactivity against the pathogen compared to the micron-sized thiazole zinc formulation; against Chinese cabbage soft rot, the three nano-thiazole zinc suspensions showed 75-87.5% higher bioactivity compared to the micron-sized thiazole zinc formulation; and against cucumber fine angular rot, the bioactivity was 27.6-32.8% higher than the micron-sized thiazole zinc formulation.
Claims
1. A method for preparing nano-thiazole zinc with controllable particle size, characterized in that, The method includes: (1) Dissolve zinc thiazide in dimethyl sulfoxide to prepare an organic phase solution; (2) Dissolve the dispersant MF in deionized water to prepare an aqueous solution; (3) A four-channel vortex reactor is used. The four inlet channels of the reactor are numbered 1, 2, 3 and 4 in a counterclockwise / clockwise direction. At room temperature, the organic phase solution is divided into two streams as streams 1 and 3, and the aqueous phase solution is divided into two streams as streams 2 and 4 and pumped into the reactor at the same time. The four streams are mixed in the mixing chamber and then discharged from the reactor outlet to continuously produce a suspension containing nano-thiazole zinc. The full name of thiazolyl zinc is 2-amino-5-mercapto-1,3,4-thiadiazole zinc, and its structural formula is as follows: 。 2. The method for preparing nano-thiazole zinc with controllable particle size as described in claim 1, characterized in that, In step (1), the dissolution temperature is 50~110 °C.
3. The method for preparing nano-thiazole zinc with controllable particle size as described in claim 1, characterized in that, Step (1) The concentration of thiazolium zinc in the organic phase solution is 5~50 mg / mL.
4. The method for preparing nano-thiazole zinc with controllable particle size as described in claim 3, characterized in that, The concentration of thiazolium zinc in the organic phase solution is 20-25 mg / mL.
5. The method for preparing nano-thiazole zinc with controllable particle size as described in claim 1, characterized in that, Step (2) The mass fraction of dispersant MF in the aqueous solution is 0.1~1%.
6. The method for preparing nano-thiazole zinc with controllable particle size as described in claim 5, characterized in that, The mass fraction of dispersant MF in the aqueous solution is 0.3~0.5%.
7. The method for preparing nano-thiazole zinc with controllable particle size as described in claim 1, characterized in that, In step (3), the flow rate ratio of the aqueous phase solution to the organic phase solution is 1:1 to 10:1, and the total flow rate is 10 to 200 mL / min; the liquid holding capacity of the reactor mixing chamber is 0.3 mL.
8. The method for preparing nano-thiazole zinc with controllable particle size as described in claim 7, characterized in that, The flow rate ratio of the aqueous phase solution to the organic phase solution is 3:1 to 5:1, and the total flow rate is 80 to 128 mL / min; the liquid holdup in the mixing chamber of the reactor is 0.3 mL.
Citation Information
Patent Citations
Preparation method for nano zinc thiazole
CN107417640A
Zinc thiazole / pyraclostrobin suspended nano-emulsion dispersion
WO2025093024A1